Alloy vacuum induction melting rapid hardening equipment

By setting swinged mold cylinders in the alloy vacuum sensor melting equipment and the use of water vapor to take away the exhaust gas and calories, the problem of insufficient exhaust gas treatment and long coolant in the equipment, and achieve efficient metal ingot production.

CN119334141AActive Publication Date: 2025-01-21GALLIANZ(ANHUI)NEW MATERIALS CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202411892966.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-12-20
Publication Date
2025-01-21
Estimated Expiration
2044-12-20

AI Technical Summary

Technical Problem

The existing alloy vacuum induction smelting equipment lacks the waste gas treatment structure, which leads to bubbles inside the metal ingot and has a long cooling time, which reduces production efficiency.

Method used

Design a alloy vacuum sensor melting speed coagulation device. By setting the mold cylinder to a structure that can be swinged in a certain range, the contact area of ​​the metal fuse and the mold cylinder can be increased, and the cooling water and high temperature metal fuse are used. The water vapor generated by the reaction takes away the exhaust gas and heat to achieve rapid cooling.

Benefits of technology

It effectively avoids the bubble phenomenon inside the metal ingot, improves the production quality of the ingot, shortens the cooling time, and improves production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119334141A_ABST
    Figure CN119334141A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of vacuum melting, in particular to alloy vacuum induction melting and rapid hardening equipment which comprises a supporting part, a melting chamber, a melting assembly, a slag filtering assembly, a cooling assembly, a slag filtering cylinder and a slag skimming assembly. The contact area between molten metal and the mold barrel in the cooling process is increased, the cooling efficiency of the molten metal is improved, meanwhile, waste gas generated in the melting process of metal materials can be taken away by means of the mode that cooling water makes direct contact with the outer wall of the mold barrel and steam generated by the reaction of the cooling water and the high-temperature molten metal, and the cooling efficiency of the mold barrel is improved. The bubble phenomenon is avoided, heat of molten metal can be taken away rapidly, and the purpose of rapid cooling is achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of vacuum melting, in particular to alloy vacuum induction melting and rapid solidification equipment. Background Art

[0002] Alloy vacuum induction melting is a kind of equipment that uses induction heating to heat alloy raw materials under vacuum or protective atmosphere to achieve rapid melting. It is widely used in the production of various alloy materials.

[0003] At present, the existing alloy vacuum induction melting equipment lacks a waste gas treatment structure during actual melting, and the metal material will produce certain waste gas during the melting process, and these waste gases will be mixed in the molten metal during the cooling process, resulting in bubbles inside the metal ingot, and ultimately causing the ingot to fail to meet the subsequent forging process; at the same time, after the molten metal is transferred to the inside of the mold barrel, the mold barrel is mostly fixed, and the contact area between the molten metal and the mold barrel is limited during the cooling process, which makes the cooling time longer and reduces the production efficiency of the metal ingot. Summary of the invention

[0004] In view of the shortcomings of the prior art, the present invention provides an alloy vacuum induction melting and rapid solidification equipment. By configuring the traditional fixed mold barrel to be able to swing back and forth within a certain range, the contact area between the molten metal and the mold barrel during the cooling process is increased, thereby improving the cooling efficiency of the molten metal. At the same time, by directly contacting the outer wall of the mold barrel with cooling water, the water vapor generated by the reaction of cooling water and high-temperature molten metal can not only take away the waste gas generated during the melting process of the metal material and avoid the bubble phenomenon, but also quickly take away the heat of the molten metal, thereby achieving the purpose of rapid cooling.

[0005] The technical solution adopted by the present invention to solve the above technical problems is: an alloy vacuum induction melting and rapid solidification equipment, including a support part and a melting chamber fixedly installed on the upper end of the support part, a melting assembly is arranged in the middle of the inner side of the melting chamber, a slag filter assembly is arranged on the side of the melting assembly, a cooling assembly is arranged below the side of the slag filter assembly away from the melting assembly, the cooling assembly and the inner wall of the melting chamber are slidably matched, a slag filter cylinder is arranged below the side of the melting assembly away from the slag filter assembly, the lower end of the slag filter cylinder is fixedly connected to the bottom of the melting chamber, a slag scraping assembly is arranged above the slag filter cylinder at a position corresponding to the melting assembly, and the slag scraping assembly is installed in the melting chamber On the side wall; the cooling assembly includes a mold barrel, a mold barrel is arranged below the side of the filter residue assembly away from the smelting assembly, the lower end of the mold barrel is in sliding contact with the bottom of the smelting chamber through a guide unit, a lining plate is symmetrically installed on the upper end of the side wall of the mold barrel, a pulley is rotatably installed on the end of the lining plate away from the mold barrel, the pulley and the side wall of the smelting chamber are slidably matched, a cooling unit is sleeved on the outer side near the upper end of the mold barrel, the upper end of the side of the cooling unit is opposite to the lower end of one of the lining plates, the lower end of the cooling unit passes through the smelting chamber and extends to the outside of the smelting chamber, a side skirt is fixedly installed on the lower end of the outer wall of the mold barrel, and a receiving groove is formed between the side skirt and the side wall of the mold barrel.

[0006] Preferably, a feed pipe is installed in the middle of the upper end of the smelting chamber, a vacuum pipe is provided on one side of the feed pipe, a vacuum release valve is installed on the side of the feed pipe away from the vacuum pipe, and a cavity door is provided on the side wall of the end of the smelting chamber.

[0007] Preferably, the smelting component includes an electrode assembly, which is rotatably mounted in the middle of the side wall of the smelting chamber, one end of the electrode assembly extends to the outside of the smelting chamber and is connected to the power supply through a wire, the other end of the electrode assembly extends to the inside of the smelting chamber and is cooperatively connected to an induction coil, a smelting crucible is arranged on the inside of the induction coil, and the outer wall of the smelting crucible and the induction coil are in contact, a connecting frame is fixedly mounted on the side wall of the smelting crucible away from the electrode assembly, one end of the connecting frame away from the smelting crucible extends to the outside of the smelting chamber and is connected to the output shaft of the drive motor, and the drive motor is fixedly mounted on the side wall of the smelting chamber through a motor base.

[0008] Preferably, the filter residue assembly includes an arc groove, which is symmetrically provided on the inner wall of the smelting chamber and located on one side of the smelting assembly. A support plate is slidably installed inside the arc groove through an extrusion spring, and the proximal end of the support plate is detachably connected to a ceramic filter.

[0009] Preferably, a guide plate is fixedly installed on the lower edge of the side wall of the ceramic filter away from the smelting component, and an arc-shaped anti-overflow strip is fixedly installed on the outer edge of the lower half of the side wall of the ceramic filter close to the smelting component.

[0010] Preferably, the smelting crucible and the ceramic filter are both made of high temperature resistant graphite material.

[0011] Preferably, the guide unit includes an arc-shaped limit bar, which is symmetrically installed on the inner wall of the smelting chamber below the mold barrel, and a slideway is formed between the two arc-shaped limit bars. The mold barrel is equipped with a plurality of rollers through a roller frame plate, and the lower ends of the rollers are located on the inner side of the slideway and in sliding contact with the bottom of the smelting chamber.

[0012] Preferably, the cooling unit comprises a high-pressure water pipe, wherein a high-pressure water pipe is provided through the side wall of the smelting chamber below a liner plate, a retaining ring is fixedly installed on the inner side of the high-pressure water pipe near the upper end, a top cap is cooperated with the upper end of the retaining ring, a transverse support pipe is installed on the upper end of the side wall of the high-pressure water pipe, the end of the transverse support pipe away from the high-pressure water pipe is connected to an annular water reservoir, and water spray valves are evenly installed on the inner wall of the annular water reservoir along its circumference.

[0013] Preferably, the top cap is a hollow structure with a spherical upper end and an overflow hole is provided on the side wall of the top cap near the lower end.

[0014] Preferably, the slag scraping assembly includes an electric push rod, which is arranged on the side wall of the smelting chamber away from the chamber door, and the electric push rod is slidably matched with the side wall of the smelting chamber away from the chamber door through the push rod base, and a lever is fixedly connected to the middle part of the lower end of the push rod base, the telescopic end of the electric push rod extends to the interior of the smelting chamber and is fixedly connected to an electromagnet block, a transverse axis is fixedly connected to the middle part of the side wall of the electromagnet block, an insulation cylinder is arranged on the outside of the transverse axis, the end of the transverse axis away from the electromagnet block extends to the inside of the insulation cylinder and a transition rod is evenly hinged along its circumference, the insulation cylinder opening faces the smelting assembly, and the side wall of the end of the insulation cylinder close to the smelting assembly is evenly hinged with slag scraping teeth along its circumference through a torsion spring, and the middle part of the side wall of the slag scraping teeth is hinged to the end of the transition rod away from the transverse axis.

[0015] Beneficial effects of the present invention:

[0016] (1) The cooling unit provided in the cooling assembly of the present invention can utilize water pressure to drive the mold barrel to swing back and forth, and the guide unit, lining plate and pulley can cooperate with each other to ensure the stability of the mold barrel. During the reciprocating swinging process, the molten metal will shake, thereby increasing the contact area with the mold barrel. The cooling water sprayed by the cooling unit can achieve the purpose of rapid cooling. At the same time, the water vapor generated by the cooling water when it meets the high temperature can rapidly increase the pressure inside the smelting chamber, thereby taking away the waste gas generated during the melting process of the metal material after the vacuum valve is opened, avoiding the occurrence of bubbles inside the metal ingot and improving its production quality.

[0017] (2) The slag filter assembly provided in the present invention can filter out the slag inside the mold barrel during the process of pouring the molten metal into the mold barrel. When used in conjunction with the slag scraping assembly, the slag inside the mold barrel can be quickly scraped out and collected and processed in a centralized manner. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] The present invention is further described below in conjunction with the accompanying drawings and embodiments.

[0019] Figure 1 is a first three-dimensional structural schematic diagram of the present invention; Figure 2 is a second three-dimensional structural schematic diagram of the present invention; Figure 3 The present invention Figure 1 Schematic diagram of the three-dimensional structure after removing the cavity door; Figure 4 The present invention Figure 3 Schematic diagram of the internal structure; Figure 5 It is a schematic diagram of the three-dimensional connection structure between the support part, the smelting chamber and the slag filter assembly in the present invention; Figure 6 The present invention Figure 5 A schematic diagram of the enlarged structure at point A; Figure 7 It is a schematic diagram of the three-dimensional connection structure between the support part, the smelting chamber, the slag filter assembly and the cooling assembly in the present invention; Figure 8 The present invention Figure 7 A schematic diagram of the enlarged structure at B; Fig. 9 The present invention Figure 7 A schematic diagram of the enlarged structure at C; Fig.10 It is a schematic diagram of the three-dimensional connection structure of the cooling unit in the present invention; Fig.11 The present invention Fig.10 A schematic diagram of the structure at D of FIG. Fig.12 It is a schematic diagram of the three-dimensional connection structure between the smelting chamber and the slag removal assembly in the present invention; Fig.13 The present invention Fig.12 Enlarged structural diagram at E.

[0020] In the figure: 1. Support part; 2. Melting chamber; 21. Feeding pipe; 22. Vacuuming pipe; 23. Vacuum release valve; 24. Chamber door; 3. Melting assembly; 31. Electrode assembly; 32. Induction coil; 33. Melting crucible; 34. Connecting frame; 35. Driving motor; 4. Filter residue assembly; 41. Arc groove; 42. Support plate; 43. Extrusion spring; 44. Ceramic filter; 441. Guide plate; 442. Arc overflow prevention strip; 5. Cooling assembly; 51. Mold cylinder; 52. guide unit; 521. arc-shaped limit strip; 522. roller; 523. roller frame plate; 53. Lining plate; 54. Pulley; 55. Cooling unit; 551. High-pressure water pipe; 552. Top cap; 5521. Overflow hole; 553. Retaining ring; 554. Transverse support pipe; 555. Annular water reservoir; 56. Side skirt; 6. Filter cartridge; 7. Slag scraping assembly; 71. Electric push rod; 72. Magnet block; 73. Horizontal axis; 74. Heat insulation cylinder; 75. Transition rod; 76. Slag scraping teeth; 77. Push rod. DETAILED DESCRIPTION

[0021] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further explained below in conjunction with specific implementation methods.

[0022] Embodiment 1:

[0023] See also Figures 1 to 6 An alloy vacuum induction melting and rapid solidification equipment comprises a support part 1 and a smelting chamber 2 fixedly installed on the upper end of the support part 1, a smelting assembly 3 is arranged in the middle of the inner side of the smelting chamber 2, a slag filter assembly 4 is arranged on the side of the smelting assembly 3, a cooling assembly 5 is arranged below the side of the slag filter assembly 4 away from the smelting assembly 3, and the cooling assembly 5 is slidably matched with the inner wall of the smelting chamber 2.

[0024] A feed pipe 21 is installed in the middle of the upper end of the smelting chamber 2, a vacuum pipe 22 is installed on one side of the feed pipe 21, a vacuum release valve 23 is installed on the side of the feed pipe 21 away from the vacuum pipe 22, and a chamber door 24 is installed on the side wall of the end of the smelting chamber 2.

[0025] The smelting assembly 3 includes an electrode assembly 31, which is rotatably installed in the middle of the side wall of the smelting chamber 2. One end of the electrode assembly 31 extends to the outside of the smelting chamber 2 and is connected to the power supply through a wire. The other end of the electrode assembly 31 extends to the inside of the smelting chamber 2 and is matched with an induction coil 32. A smelting crucible 33 is arranged inside the induction coil 32, and the outer wall of the smelting crucible 33 and the induction coil 32 are in contact. A connecting frame 34 is fixedly installed on the side wall of the smelting crucible 33 away from the electrode assembly 31. One end of the connecting frame 34 away from the smelting crucible 33 extends to the outside of the smelting chamber 2 and is connected to the output shaft of the driving motor 35. The driving motor 35 is fixedly installed on the side wall of the smelting chamber 2 through a motor base.

[0026] The filter residue assembly 4 includes an arc groove 41, and the arc groove 41 is symmetrically opened on the inner wall of the smelting chamber 2 and located on one side of the smelting assembly 3. A support plate 42 is slidably installed inside the arc groove 41 through an extrusion spring 43, and a ceramic filter screen 44 is detachably connected to the proximal end of the support plate 42. The smelting crucible 33 and the ceramic filter screen 44 are both made of high-temperature resistant graphite material.

[0027] A guide plate 441 is fixedly installed on the lower edge of the side wall of the ceramic filter 44 away from the smelting component 3, and an arc-shaped anti-overflow strip 442 is fixedly installed on the outer edge of the lower half of the side wall of the ceramic filter 44 close to the smelting component 3.

[0028] In specific operation, the feed tube 21 is first opened manually, and then two or more metal materials are added into the smelting crucible 33 from the feed tube 21, and then the end cover at the upper end of the feed tube 21 is closed, and the vacuum tube 22 is connected to the external exhaust device, and the inside of the smelting chamber 2 is evacuated by the external exhaust device, and the external power supply is started, and the electrode assembly 31 is powered by the external power supply, so as to drive the induction coil 32 to heat and melt the metal material inside the smelting crucible 33. During the heating process, the inside of the smelting chamber 2 can be observed manually through the observation window provided on the chamber door 24; when the metal material inside the smelting crucible 33 is melted into molten metal, the drive motor 35 is started, and the drive motor 35 drives the connection The frame 34 and the melting crucible 33 are rotated 90 degrees toward the chamber door 24, so that the molten metal inside the melting crucible 33 is poured into the cooling assembly 5. During this process, the melting crucible 33 will continuously squeeze the ceramic filter 44 and drive the support plate 42 to move in the arc groove 41, thereby driving the squeezing spring 43 to compress. Subsequently, the molten metal inside the melting crucible 33 will be filtered by the ceramic filter 44 and then flow downward through the guide plate 441 into the cooling assembly 5. The ceramic filter 44 can filter the slag in the molten metal in the melting crucible 33, and the arc-shaped anti-overflow strip 442 can prevent the molten metal from overflowing and falling during the pouring process, causing waste. After the pouring is completed, the connecting frame 34 and the melting crucible 33 are reset by the driving motor 35.

[0029] See also Figures 1 to 4 as well as Figures 7 to 11 The cooling assembly 5 includes a mold barrel 51. The mold barrel 51 is arranged below the side of the filter residue assembly 4 away from the smelting assembly 3. The lower end of the mold barrel 51 is in sliding contact with the bottom of the smelting chamber 2 through a guide unit 52. The upper end of the side wall of the mold barrel 51 is symmetrically installed with a lining plate 53. The end of the lining plate 53 away from the mold barrel 51 is rotatably installed with a pulley 54. The pulley 54 and the side wall of the smelting chamber 2 are slidably matched. A cooling unit 55 is sleeved on the outer side of the mold barrel 51 near the upper end. The upper end of the side of the cooling unit 55 is directly opposite to the lower end of one of the lining plates 53. The lower end of the cooling unit 55 passes through the smelting chamber 2 and extends to the outside of the smelting chamber 2. A side skirt 56 is fixedly installed at the lower end of the outer wall of the mold barrel 51, and a receiving groove is formed between the side skirt 56 and the side wall of the mold barrel 51.

[0030] The guide unit 52 includes an arc-shaped limit bar 521, which is symmetrically installed on the inner wall of the smelting chamber 2 below the mold barrel 51. A slideway is formed between the two arc-shaped limit bars 521. The mold barrel 51 is installed with a plurality of rollers 522 through a roller frame plate 523. The lower ends of the rollers 522 are located on the inner side of the slideway and are in sliding contact with the bottom of the smelting chamber 2.

[0031] The cooling unit 55 includes a high-pressure water pipe 551, wherein the high-pressure water pipe 551 is penetrated on the side wall of the smelting chamber 2 below a liner plate 53, a retaining ring 553 is fixedly installed on the inner side of the high-pressure water pipe 551 near the upper end, and a top cap 552 is installed on the upper end of the retaining ring 553, a transverse support pipe 554 is installed on the upper end of the side wall of the high-pressure water pipe 551, and the end of the transverse support pipe 554 away from the high-pressure water pipe 551 is connected to an annular water reservoir 555, and the inner wall of the annular water reservoir 555 is evenly installed with water spray valves along its circumference.

[0032] The top cap 552 is a hollow structure with a spherical upper end, and an overflow hole 5521 is provided on the side wall of the top cap 552 near the lower end.

[0033] During specific operation, after the molten metal enters the mold barrel 51, high-pressure water is intermittently introduced into the high-pressure water pipe 551 through an external water supply device. The pressure of the high-pressure water will drive the top cap 552 to be ejected upward and drive the lining plate 53 to tilt. Under the action of the pulley 54 and the guide unit 52, the mold barrel 51 can rock back and forth, thereby driving the molten metal inside it to rock, thereby increasing the contact area between the molten metal and the inner wall of the mold barrel 51. When the overflow hole 5521 moves to the same height as the horizontal support pipe 554, the high-pressure water will pass through the horizontal support pipe 554 into the annular water reservoir 555, and then be sprayed onto the outer wall of the mold barrel 51 through the water spray valve, and finally formed between the side skirt 56 and the side wall of the mold barrel 51. The water vapor is collected by the containing groove, thereby quickly cooling the molten metal inside the mold barrel 51. During the cooling process, the water flow sprayed by the water spray valve will quickly vaporize after contacting the outer wall of the mold barrel 51. The vaporized water vapor can increase the internal pressure of the smelting chamber 2. When the pressure reaches the preset value, the vacuum release valve 23 will open. At this time, the water vapor inside the smelting chamber 2 will be quickly discharged through the vacuum release valve 23. During the discharge process, the water vapor can take away the heat of the molten metal and the waste gas generated by the metal material during the melting process, thereby improving the quality of the alloy ingot. After the molten metal inside the mold barrel 51 is cooled into an alloy ingot, the cavity door 24 is manually opened, so that the alloy ingot can be taken out through the existing lifting equipment for subsequent operations.

[0034] Embodiment 2:

[0035] The technical solution is basically the same as that of the first embodiment, see Figure 2 , Figure 4 as well as Fig.12 and Fig.13 The difference is that a slag filter cylinder 6 is installed at the lower part of the smelting component 3 away from the slag filter assembly 4, the lower end of the slag filter cylinder 6 is fixedly connected to the bottom of the smelting chamber 2, and a slag scraping assembly 7 is arranged above the slag filter cylinder 6 at a position corresponding to the smelting component 3, and the slag scraping assembly 7 is installed on the side wall of the smelting chamber 2.

[0036] The slag removal assembly 7 includes an electric push rod 71, which is arranged on the side wall of the smelting chamber 2 away from the chamber door 24. The electric push rod 71 slides with the side wall of the smelting chamber 2 away from the chamber door 24 through a push rod base, and a lever 77 is fixedly connected to the middle part of the lower end of the push rod base. The telescopic end of the electric push rod 71 extends into the interior of the smelting chamber 2 and is fixedly connected to an electromagnet block 72. A transverse axis 73 is fixedly connected to the middle part of the side wall of the electromagnet block 72. An insulating cylinder 74 is arranged on the outside of the transverse axis 73. The end of the transverse axis 73 away from the electromagnet block 72 extends to the interior of the insulating cylinder 74 and a transition rod 75 is evenly hinged along its circumference. The opening of the insulating cylinder 74 faces the smelting assembly 3 and the side wall of the end close to the smelting assembly 3 is evenly hinged with slag removal teeth 76 through a torsion spring along its circumference. The middle part of the side wall of the slag removal tooth 76 is hinged with the end of the transition rod 75 away from the transverse axis 73.

[0037] In this embodiment, the heat insulating tube 74 has magnetic attraction.

[0038] In specific operation, after the melting crucible 33 is reset, the connecting frame 34 and the melting crucible 33 are driven by the driving motor 35 to rotate 90 degrees in the opposite direction, and then the electric push rod 71 is started, and the electric push rod 71 drives the electromagnet block 72, the horizontal shaft 73, the insulation cylinder 74, the transition rod 75 and the slag removal teeth 76 to move into the melting crucible 33. When the slag removal teeth 76 contact the side wall of the melting crucible 33, the electromagnet block 72 is energized, and then the electric push rod 71 continues to push, and the electromagnet block 72 will move toward the insulation cylinder 74, and finally the electromagnet block 72 will move to the insulation cylinder 74. The iron block 72 will be attracted to the end of the insulation tube 74, and the slag scraper teeth 76 will move to a state of contact with the inner wall of the melting crucible 33. Then, the electric push rod 71 will drive the electromagnet block 72, the horizontal axis 73, the insulation tube 74, the transition rod 75 and the slag scraper teeth 76 to move away from the melting crucible 33 as a whole, so that the slag inside the melting crucible 33 is scraped into the slag filter tube 6 by the slag scraper teeth 76. During the slag scraping process, the slag scraper assembly 7 can be driven to rotate as a whole by the manual control lever 77, thereby improving the slag removal efficiency.

[0039] The working principle of the present invention when in use:

[0040] One: first open the feed tube 21 manually, then add two or more metal materials from the feed tube 21 into the smelting crucible 33, then close the end cover at the upper end of the feed tube 21, connect the vacuum tube 22 to the external exhaust device, evacuate the inside of the smelting chamber 2 through the external exhaust device, start the external power supply, and energize the electrode assembly 31 through the external power supply, thereby driving the induction coil 32 to heat and melt the metal material inside the smelting crucible 33. During the heating process, the internal situation of the smelting chamber 2 can be observed manually through the observation window provided on the chamber door 24.

[0041] 2. When the metal material in the melting crucible 33 is melted into molten metal, the driving motor 35 is started, and the connecting frame 34 and the melting crucible 33 are driven by the driving motor 35 to rotate 90 degrees toward the chamber door 24, so that the molten metal in the melting crucible 33 is poured into the mold tube 51. In this process, the melting crucible 33 will continuously squeeze the ceramic filter screen 44 and drive the support plate 42 to move in the arc groove 41, thereby driving the extrusion spring 43 to compress. Subsequently, the molten metal in the melting crucible 33 will be filtered by the ceramic filter screen 44 and then flow downward through the guide plate 441 into the cooling assembly 5. The ceramic filter screen 44 can filter the slag in the molten metal in the melting crucible 33, and the arc-shaped anti-overflow strip 442 can prevent the molten metal from overflowing and falling during the pouring process to cause waste. After the pouring is completed, the connecting frame 34 and the melting crucible 33 are reset by the driving motor 35.

[0042] 3. When the molten metal enters the mold barrel 51, high-pressure water is intermittently introduced into the high-pressure water pipe 551 through an external water supply device. The pressure of the high-pressure water will drive the top cap 552 to be ejected upward and drive the lining plate 53 to tilt. Under the action of the pulley 54 and the guide unit 52, the mold barrel 51 can rock back and forth, thereby driving the molten metal inside it to rock, thereby increasing the contact area between the molten metal and the inner wall of the mold barrel 51. When the overflow hole 5521 moves to the same height as the horizontal support pipe 554, the high-pressure water will pass through the horizontal support pipe 554 into the annular water reservoir 555, and then be sprayed onto the outer wall of the mold barrel 51 through the water spray valve, and finally be contained in the container formed between the side skirt 56 and the side wall of the mold barrel 51. The vacuum trough collects the water, thereby rapidly cooling the molten metal inside the mold barrel 51. During the cooling process, the water sprayed from the water spray valve will quickly vaporize after contacting the outer wall of the mold barrel 51. The vaporized water vapor can increase the internal pressure of the smelting chamber 2. When the pressure reaches the preset value, the vacuum release valve 23 will open. At this time, the water vapor inside the smelting chamber 2 will be quickly discharged through the vacuum release valve 23. During the discharge process, the water vapor can take away the heat of the molten metal and the waste gas generated by the metal material during the melting process, thereby improving the quality of the alloy ingot. After the molten metal inside the mold barrel 51 is cooled into an alloy ingot, the cavity door 24 is manually opened, so that the alloy ingot can be taken out through the existing lifting equipment for subsequent operations.

[0043] Fourth: After the melting crucible 33 is reset, the connecting frame 34 and the melting crucible 33 are driven by the driving motor 35 to rotate 90 degrees in the opposite direction, and then the electric push rod 71 is started, and the electric push rod 71 drives the electromagnet block 72, the horizontal shaft 73, the insulation cylinder 74, the transition rod 75 and the slag removal teeth 76 to move into the melting crucible 33. When the slag removal teeth 76 contact the side wall of the melting crucible 33, the electromagnet block 72 is energized, and then the electric push rod 71 continues to push, and the electromagnetic The iron block 72 will move toward the insulating tube 74, and finally the electromagnet block 72 will be attracted to the end of the insulating tube 74. At the same time, the slag scraper teeth 76 will move to a state of contact with the inner wall of the smelting crucible 33. Then, the electric push rod 71 will drive the electromagnet block 72, the horizontal axis 73, the insulating tube 74, the transition rod 75 and the slag scraper teeth 76 to move as a whole away from the smelting crucible 33, so that the slag inside the smelting crucible 33 is scraped into the slag filter tube 6 by the slag scraper teeth 76.

[0044] The above shows and describes the basic principles, main features and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention. The scope of the present invention is defined by the attached claims and their equivalents.

Claims

1. An alloy vacuum induction melting and rapid solidification device, comprising a support portion (1) and a melting chamber (2) fixedly mounted on the upper end of the support portion (1), characterized in that: A smelting assembly (3) is arranged in the middle of the inner side of the smelting chamber (2), a slag filter assembly (4) is arranged on the side of the smelting assembly (3), a cooling assembly (5) is arranged below the side of the slag filter assembly (4) away from the smelting assembly (3), the cooling assembly (5) and the inner wall of the smelting chamber (2) are slidably matched, a slag filter cylinder (6) is installed below the side of the smelting assembly (3) away from the slag filter assembly (4), the lower end of the slag filter cylinder (6) is fixedly connected to the bottom of the smelting chamber (2), a slag scraping assembly (7) is arranged above the slag filter cylinder (6) at a position corresponding to the smelting assembly (3), and the slag scraping assembly (7) is mounted on the side wall of the smelting chamber (2); The cooling assembly (5) comprises: A mold barrel (51), wherein the mold barrel (51) is disposed below a side of the filter residue assembly (4) away from the smelting assembly (3); A guide unit (52), wherein the lower end of the mold cylinder (51) is in sliding contact with the bottom of the smelting chamber (2) via the guide unit (52); A lining plate (53) is symmetrically mounted on the upper end of the side wall of the mold cylinder (51); The pulley (54) is rotatably mounted on the end of the liner (53) away from the mold cylinder (51), and the pulley (54) and the side wall of the smelting chamber (2) are slidably matched; A cooling unit (55) is sleeved on the outer side of the mold cylinder (51) near the upper end, the upper end of the side of the cooling unit (55) is directly opposite to the lower end of one of the lining plates (53), and the lower end of the cooling unit (55) passes through the smelting chamber (2) and extends to the outside of the smelting chamber (2); A side skirt (56) is fixedly mounted on the lower end of the outer side wall of the mold cylinder (51), and a receiving groove is formed between the side skirt (56) and the side wall of the mold cylinder (51).

2. The alloy vacuum induction melting and rapid solidification equipment according to claim 1, characterized in that: A feed pipe (21) is installed in the middle of the upper end of the smelting chamber (2), a vacuum pipe (22) is provided on one side of the feed pipe (21), a vacuum release valve (23) is installed on the side of the feed pipe (21) away from the vacuum pipe (22), and a chamber door (24) is provided on the side wall of the end of the smelting chamber (2).

3. The alloy vacuum induction melting and rapid solidification equipment according to claim 1, characterized in that: The smelting assembly (3) comprises an electrode assembly (31), wherein the electrode assembly (31) is rotatably mounted in the middle of the side wall of the smelting chamber (2), one end of the electrode assembly (31) extends to the outside of the smelting chamber (2) and is connected to a power source via a wire, the other end of the electrode assembly (31) extends to the inside of the smelting chamber (2) and is cooperatively connected to an induction coil (32), a smelting crucible (33) is arranged inside the induction coil (32), and the outer wall of the smelting crucible (33) and the induction coil (32) are in contact, a connecting frame (34) is fixedly mounted on the side wall of the smelting crucible (33) away from the electrode assembly (31), one end of the connecting frame (34) away from the smelting crucible (33) extends to the outside of the smelting chamber (2) and is connected to the output shaft of a driving motor (35), and the driving motor (35) is fixedly mounted on the side wall of the smelting chamber (2) via a motor base.

4. The alloy vacuum induction melting and rapid solidification equipment according to claim 3 is characterized in that: The filter residue assembly (4) comprises an arc groove (41), and the arc groove (41) is symmetrically provided on the inner wall of the smelting chamber (2) and located on one side of the smelting assembly (3). A support plate (42) is slidably installed inside the arc groove (41) via a compression spring (43), and a ceramic filter screen (44) is detachably connected to the proximal end of the support plate (42).

5. The alloy vacuum induction melting and rapid solidification equipment according to claim 4, characterized in that: A guide plate (441) is fixedly mounted on the lower edge of the side wall of the ceramic filter (44) away from the smelting assembly (3), and an arc-shaped anti-overflow strip (442) is fixedly mounted on the outer edge of the lower half of the side wall of the ceramic filter (44) close to the smelting assembly (3).

6. The alloy vacuum induction melting and rapid solidification equipment according to claim 5, characterized in that: The smelting crucible (33) and the ceramic filter (44) are both made of high-temperature resistant graphite material.

7. The alloy vacuum induction melting and rapid solidification equipment according to claim 1, characterized in that: The guide unit (52) comprises an arc-shaped limit strip (521), and the arc-shaped limit strips (521) are symmetrically mounted on the inner wall of the smelting chamber (2) below the mold barrel (51), and a slideway is formed between the two arc-shaped limit strips (521). The mold barrel (51) is mounted with a plurality of rollers (522) via a roller frame plate (523), and the lower ends of the rollers (522) are located inside the slideway and in sliding contact with the bottom of the smelting chamber (2).

8. The alloy vacuum induction melting and rapid solidification equipment according to claim 1, characterized in that: The cooling unit (55) comprises a high-pressure water pipe (551), wherein a high-pressure water pipe (551) is provided through a side wall of the smelting chamber (2) below a liner plate (53), a retaining ring (553) is fixedly installed on the inner side of the high-pressure water pipe (551) near the upper end, a top cap (552) is installed on the upper end of the retaining ring (553), a transverse support pipe (554) is installed on the upper end of the side wall of the high-pressure water pipe (551), and an annular water reservoir (555) is connected to the end of the transverse support pipe (554) away from the high-pressure water pipe (551).

9. The alloy vacuum induction melting and rapid solidification equipment according to claim 8, characterized in that: The top cap (552) is a hollow structure with a spherical upper end, and an overflow hole (5521) is provided on the side wall of the top cap (552) near the lower end.

10. The alloy vacuum induction melting and rapid solidification equipment according to claim 2, characterized in that: The slag removal assembly (7) comprises an electric push rod (71), which is arranged on a side wall of the smelting chamber (2) away from the chamber door (24), the electric push rod (71) is slidably matched with the side wall of the smelting chamber (2) away from the chamber door (24) through a push rod base, and a lever (77) is fixedly connected to the middle of the lower end of the push rod base, the telescopic end of the electric push rod (71) extends into the interior of the smelting chamber (2) and is fixedly connected to an electromagnet block (72), and a transverse shaft (73) is fixedly connected to the middle of the side wall of the electromagnet block (72). ), an insulating cylinder (74) is arranged outside the transverse axis (73), an end of the transverse axis (73) away from the electromagnet block (72) extends into the interior of the insulating cylinder (74) and is evenly hinged with a transition rod (75) along its circumference, the opening of the insulating cylinder (74) faces the smelting assembly (3), and a slag scraper (76) is evenly hinged with a side wall of the end of the insulating cylinder (74) close to the smelting assembly (3) along its circumference through a torsion spring, and the middle part of the side wall of the slag scraper (76) is hingedly matched with the end of the transition rod (75) away from the transverse axis (73).

Citation Information

Patent Citations

  • Smelting system

    CN113091456A

  • Smelting equipment for air conditioner refrigeration copper pipe machining

    CN113959224A

  • Vacuum melting and blanking device

    CN201440033U

  • Water cooling copper crucible

    CN207050439U

  • Device for pulling out nozzle in ladle incorporating molten metal

    JP1998058123A