Preparation method of coal rock polished section

By pre-wetting the coal particles, the problem of low flatness of the light sheet in the traditional coal rock sheet preparation method is solved, and a higher quality coal rock sheet preparation is achieved, which is suitable for modern instrument analysis.

CN119643245APending Publication Date: 2025-03-18GUIZHOU UNIV
4 Cites 0 Cited by

Patent Information

Application Number
CN202411798646.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-12-09
Publication Date
2025-03-18

AI Technical Summary

Technical Problem

Traditional coal rock light sheet preparation methods lead to a large number of bubbles inside the light sheet, many potholes on the surface, and low flatness, which limits its application and analysis accuracy in modern instrument analysis.

Method used

Before the coal particles are mixed with the binder, pre-wetting treatment is carried out, and the coal particles are fully wetted with water or dextrin solution to eliminate the gas film on the surface of the coal particles, thereby avoiding the generation of internal bubbles.

Benefits of technology

Through pre-wetting treatment, the flatness and finish of the coal rock light sheet is significantly improved, the surface pits are eliminated, the microscopic composition boundaries are clear, and the quality and analysis accuracy of the light sheet are improved.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a preparation method of a coal rock polished section, which comprises the following steps: before mixing a coal sample which is crushed to a qualified particle size with an adhesive, carrying out pre-wetting treatment on the coal sample by using water or a dextrin solution, stirring to fully wet coal particles, carrying out suction filtration, drying in the shade, mixing the coal particles with the adhesive, putting the mixture into a mold, drying under a room temperature condition, and carrying out sintering to obtain the coal rock polished section. And grinding and polishing to prepare the coal rock polished section. Compared with a national standard method, the polished section prepared after the coal particles are pretreated through the pre-wetting method is more stable in quality, potholes are not formed in the polished surface, flatness is better, surface roughness is smaller, maceral boundaries are clearer, the method is high in operability, and coal rock properties cannot be affected. Water or a dextrin solution is used for pretreatment so as to eliminate air films on the surfaces of the coal particles, enhance the wettability of the surfaces of the coal particles and fundamentally avoid bubbles and pits in the polished section.