Heating film and its preparation method, battery module, battery pack and electrical equipment
By using a photocurable coating and a conductive adhesive layer to connect the heating film, the problems of poor durability and complex preparation of the heating film under high temperature and high humidity environments are solved, thereby improving durability, simplifying the preparation process, and reducing costs.
Patent Information
- Application Number
- CN202411140680.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-19
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2044-08-19
AI Technical Summary
Existing heating films have poor durability in high temperature and high humidity environments, and their manufacturing process is complex and costly.
A photocurable coating is used as an insulating layer, which is formed on the metal layer and the heating layer by spraying or inkjet printing. Conductive adhesive layer is used to connect the wires, which simplifies the manufacturing process, reduces the number of parts, and improves the resistance to high temperature and humidity.
It improves the heating film's resistance to high temperature and humidity, simplifies the preparation process, reduces production costs, and extends its service life.
Smart Images

Figure CN119789252B_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of heating film technology, and in particular to a heating film and its preparation method, a battery module, a battery pack and electrical equipment. Background Technology
[0002] Given that batteries may fail to charge or have low charge / discharge efficiency when operating in low-temperature environments, related technologies typically incorporate devices for heating the batteries. These devices generally employ heating films, with positive temperature coefficient (PTC) heating films (hereinafter referred to as heating films) being widely used due to their advantages such as flexibility, high heating rate, and self-regulating temperature.
[0003] However, the heating films in related technologies have poor resistance to high temperatures and humidity. Summary of the Invention
[0004] In order to overcome the above-mentioned defects in related technologies, the purpose of this application is to provide a heating film and its preparation method, a battery module, a battery pack and electrical equipment. This application is beneficial to improving the heating film's resistance to high temperature and high humidity.
[0005] On one hand, this application provides a heating film, including a first insulating layer, a metal layer, a heating layer, and a second insulating layer. The first insulating layer is formed on a first side of the metal layer, and the heating layer is formed on a second side of the metal layer. The heating layer is electrically connected to the metal layer. The first side and the second side are opposite sides in the thickness direction of the metal layer. The second insulating layer is formed on the side of the heating layer away from the metal layer. The metal layer is also connected to a wire.
[0006] Both the first insulating layer and the second insulating layer are photocurable coatings.
[0007] In one possible implementation, the photocurable coating comprises a polyurethane-modified acrylate layer or a silicone-modified acrylate layer.
[0008] In one possible implementation, a third insulating layer is further included, the third insulating layer being located between the metal layer and the heating layer; the third insulating layer is provided with a trench, the trench being connected to the metal layer to expose a portion of the metal layer, and the heating layer being electrically connected to the metal layer through the trench.
[0009] In one possible implementation, the third insulating layer comprises a polyurethane-modified acrylate layer or a silicone-modified acrylate layer.
[0010] In one possible implementation, the thicknesses of the first insulating layer, the second insulating layer, and the third insulating layer are all 80–150 μm.
[0011] In one possible implementation, the dielectric strength of the first insulating layer, the second insulating layer, and the third insulating layer is all greater than or equal to 10 kV / mm.
[0012] In one possible implementation, the surface resistivity of the first insulating layer, the second insulating layer, and the third insulating layer are all greater than or equal to 1*10⁻⁶. 12 Ω·cm.
[0013] In one possible implementation, the water vapor permeability of the first, second, and third insulating layers is all less than or equal to 1 g / m³. 2 / day.
[0014] In one possible implementation, the metal layer includes an aluminum foil layer, a rolled copper layer, or an electrolytic copper layer.
[0015] In one possible implementation, the thickness of the metal layer is 20–80 μm, and the volume resistivity of the metal layer is ≤0.001 Ω·cm.
[0016] In one possible implementation, the sum of the thicknesses of the metal layer, the first insulating layer, and the third insulating layer is 100–180 μm.
[0017] In one possible implementation, the heating layer includes a positive temperature coefficient heating layer.
[0018] In one possible implementation, the positive temperature coefficient heating layer comprises a polymer matrix and a conductive filler, wherein the polymer matrix comprises polyethylene, polypropylene, or polyvinyl chloride, and the conductive filler comprises carbon black, graphite, copper powder, silver powder, tin oxide, or zinc oxide.
[0019] In one possible implementation, the metal layer is electrically connected to the wire via a conductive adhesive layer, and a fourth insulating layer is further provided at the connection point between the metal layer and the wire.
[0020] In one possible implementation, the conductive adhesive layer comprises a two-component epoxy resin conductive adhesive layer or a two-component acrylate conductive adhesive layer, wherein the volume resistivity of the conductive adhesive layer is ≤0.001Ω·cm, and the contact resistance between the conductive adhesive layer and the metal layer or the wire is ≤0.05Ω.
[0021] In one possible implementation, the fourth insulating layer comprises a polyurethane-modified acrylate layer or a silicone-modified acrylate layer.
[0022] On the other hand, this application provides a method for preparing a heating film, comprising:
[0023] Provide a metal layer;
[0024] A first insulating layer is formed on a first side of the metal layer;
[0025] A heating layer is formed on the second side of the metal layer, and the heating layer is electrically connected to the metal layer; wherein the first side and the second side are opposite sides in the thickness direction of the metal layer;
[0026] A second insulating layer is formed on the side of the heating layer opposite to the metal layer;
[0027] Electrically connect the wire to the metal layer;
[0028] Both the first insulating layer and the second insulating layer are photocurable coatings.
[0029] In one possible implementation, the photocurable coating comprises a polyurethane-modified acrylate layer or a silicone-modified acrylate layer.
[0030] In one possible implementation, the first insulating layer is formed on the first side of the metal layer by spraying or inkjet printing insulating material and then curing it by light.
[0031] And / or, the second insulating layer is formed on the side of the heating layer opposite to the metal layer by spraying or inkjet printing insulating material and then curing it by light.
[0032] One possible implementation also includes:
[0033] A third insulating layer is formed on the second side of the metal layer, the third insulating layer being located between the metal layer and the heating layer; wherein the third insulating layer has a trench formed therein, the trench communicating with the metal layer to expose a portion of the metal layer, and the heating layer being electrically connected to the metal layer through the trench.
[0034] In one possible implementation, the third insulating layer comprises a polyurethane-modified acrylate layer or a silicone-modified acrylate layer.
[0035] In one possible implementation, forming a third insulating layer on the second side of the metal layer includes:
[0036] A shielding layer is covered on the second side of the metal layer;
[0037] An insulating material is sprayed onto the metal layer covered by the shielding layer and then cured by light.
[0038] Remove the shielding layer to form the third insulating layer.
[0039] In one possible implementation, the fabrication of the heat-generating layer on the second side of the metal layer includes:
[0040] A heating layer paste is printed on the side of the third insulating layer opposite to the metal layer.
[0041] The printed heating layer paste is baked and cured to form the heating layer.
[0042] In one possible implementation, the heating layer includes a positive temperature coefficient heating layer.
[0043] In one possible implementation, the positive temperature coefficient heating layer comprises a polymer matrix and a conductive filler, wherein the polymer matrix comprises polyethylene, polypropylene, or polyvinyl chloride, and the conductive filler comprises carbon black, graphite, copper powder, silver powder, tin oxide, or zinc oxide.
[0044] In one possible implementation, the baking temperature of the heating layer slurry is 80-150°C; the baking time of the heating layer slurry is 15-30 minutes.
[0045] In one possible implementation, the second insulating layer is formed on the side of the heating layer opposite to the third insulating layer by spraying or inkjet printing insulating material and then curing it by light.
[0046] In one possible implementation, electrically connecting the wire to the metal layer includes:
[0047] A conductive adhesive layer is applied to the metal layer at the location where the wire is connected, and the wire is then bonded to the conductive adhesive layer.
[0048] A fourth insulating layer is applied at the bonding location between the metal layer and the wire.
[0049] In one possible implementation, the conductive adhesive layer comprises a two-component epoxy resin conductive adhesive layer or a two-component acrylate conductive adhesive layer, wherein the volume resistivity of the conductive adhesive layer is ≤0.001Ω·cm, and the contact resistance between the conductive adhesive layer and the metal layer or the wire is ≤0.05Ω.
[0050] In one possible implementation, the fourth insulating layer comprises a polyurethane-modified acrylate layer or a silicone-modified acrylate layer.
[0051] In another aspect, this application provides a battery module including any of the heating films described above.
[0052] In another aspect, this application provides a battery pack including at least one battery module as described above.
[0053] In another aspect, this application provides an electrical device including the battery pack described above.
[0054] This application provides a heating film and its preparation method, a battery module, a battery pack, and an electrical device. The heating film includes a first insulating layer, a metal layer, a heating layer, and a second insulating layer. The first insulating layer is formed on a first side of the metal layer, and the heating layer is formed on a second side of the metal layer, electrically connected to the metal layer. The first and second sides are opposite sides in the thickness direction of the metal layer. The second insulating layer is formed on the side of the heating layer away from the metal layer, and the metal layer is also connected to a wire. Both the first and second insulating layers are photocurable coatings. This application improves the heating film's resistance to high temperatures and humidity by forming a first insulating layer on the first side of the metal layer and a second insulating layer on one side of the heating layer, and by selecting both the first and second insulating layers as photocurable coatings. Since the water vapor transmission rate of the photocurable coating is low, this improves the heating film's resistance to high temperatures and humidity. Attached Figure Description
[0055] To more clearly illustrate the technical solutions in the embodiments or related technologies of this application, the accompanying drawings used in the description of the embodiments or related technologies will be briefly introduced below. Obviously, the accompanying drawings described below are some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0056] Figure 1 This is a simplified structural diagram of the heating film in related technologies;
[0057] Figure 2 A simplified structural diagram of a heating film provided in one embodiment of this application;
[0058] Figure 3 This is a flowchart illustrating the preparation process of a heating film provided in one embodiment of this application.
[0059] Figure label:
[0060] 11-Bottom Layer;
[0061] 12-Surface layer;
[0062] 13-PTC heating layer;
[0063] 14-Current-carrying strip;
[0064] 15 - Second adhesive layer;
[0065] 16-Conductive wire;
[0066] 100 - Metal layer;
[0067] 200 - Third insulation layer;
[0068] 300-Heating layer;
[0069] 400 - Second insulation layer;
[0070] 500 - Wire. Detailed Implementation
[0071] To make the objectives, technical solutions, and advantages of the embodiments of this application clearer, the technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are some embodiments of this application, but not all embodiments.
[0072] Based on the embodiments in this application, all other embodiments obtained by those skilled in the art without inventive effort are within the scope of protection of this application. Unless otherwise specified, the following embodiments and features can be combined with each other.
[0073] As described in the background section, the heating films in the related technologies have problems such as poor resistance to high temperature and humidity and complex preparation processes. Figure 1 This is a simplified structural diagram of the heating film in related technologies. Please refer to... Figure 1 In the related technology, the heating film includes a bottom layer 11 and a top layer 12 disposed opposite to each other. A PTC heating layer 13 and a current-carrying strip 14 are also provided between the bottom layer 11 and the top layer 12. Both the bottom layer 11 and the top layer 12 can be polyimide film (PI) layers or polyethylene terephthalate film (PET) layers. The bottom layer 11 is bonded to the first side of the current-carrying strip 14 and the first side of the PTC heating layer 13 through a first adhesive layer (not shown in the figure), and the top layer 12 is bonded to the second side of the PTC heating layer 13 through a second adhesive layer 15. The current-carrying strip 14 is electrically connected to a conductive wire 16, which is connected to an external power supply device.
[0074] Since both the bottom layer 11 and the top layer 12 are polyimide film layers or polyethylene terephthalate film layers, and their thickness is generally less than or equal to 150 μm, their water vapor permeability is generally greater than 50 g / m². 2 / day, the PTC heating layer 13 is easily aged by the infiltrated moisture under high temperature conditions, and the heating film has poor resistance to high temperature and high humidity.
[0075] Furthermore, since both the bottom layer 11 and the top layer 12 are polyimide film layers or polyethylene terephthalate film layers, corresponding first and second adhesive layers 15 are required to bond them together with the PTC heating layer 13 and the current-carrying strip 14. The first and second adhesive layers 15 are typically made of hot melt adhesive, which requires heating to bond adjacent layers together. Therefore, the manufacturing process is relatively complex, increasing the difficulty of quality control for the heating film and resulting in a lower yield.
[0076] The current-carrying strip 14 is generally formed by printing a specific pattern of silver paste onto the surface of the surface layer 12, followed by baking and curing. The baking temperature is 80–150°C, and the baking time is 5–30 minutes. The preparation process of the current-carrying strip 14 is complex and time-consuming.
[0077] When installing the current-carrying strip 14 and the conductive wire 16, the outer film at the connection point of the conductive wire 16 needs to be removed first using a laser. Then, rivets are driven into the connection point of the conductive wire 16, and solder wire is heated and melted to weld the conductive wire 16 to the rivets. An insulating material also needs to be hot-pressed onto the welded conductive wire 16 for insulation protection. The insulating material is generally composed of silicone rubber and hot-melt adhesive film. The hot-pressing conditions are generally a temperature of 160–200℃, a pressure of 0.1–0.25 MPa, and a hot-pressing time of 95–105 seconds. The installation process is complex, time-consuming, and labor-intensive. Furthermore, the insulating material requires heat curing, which consumes a significant amount of energy, increasing the production cost of the heating film.
[0078] In view of this, the embodiments of this application aim to provide a heating film and its preparation method, a battery module, a battery pack and an electrical device. By forming a first insulating layer on the first side of the metal layer and a second insulating layer on one side of the heating layer, and both the first insulating layer and the second insulating layer are selected as photocurable coatings, the high temperature and high humidity resistance of the heating film is improved because the water vapor transmission rate of the photocurable coating is low.
[0079] The embodiments of this application will now be described in detail with reference to the accompanying drawings, so that those skilled in the art can gain a more detailed understanding of the contents of this application.
[0080] Figure 2 This is a simplified structural diagram of a heating film provided in one embodiment of this application.
[0081] Please refer to Figure 2This embodiment provides a heating film, including a first insulating layer (not shown in the figure), a metal layer 100, a heating layer 300, and a second insulating layer 400. The first insulating layer is formed on a first side of the metal layer 100. Exemplarily, the first insulating layer can be formed on the metal layer 100 by spraying or inkjet printing. The heating layer 300 is formed on a second side of the metal layer 100 and is electrically connected to the metal layer 100. The first side and the second side are opposite sides in the thickness direction of the metal layer 100. Exemplarily, the heating layer 300 can be made of PTC material, and the heating layer 300 can be formed on the metal layer 100 by processes such as printing and baking. The second insulating layer 400 is formed on the side of the heating layer 300 facing away from the metal layer 100. Exemplarily, the second insulating layer 400 can also be formed on the heating layer 300 by spraying or inkjet printing. The metal layer 100 is also connected to a wire 500, which is used to connect an external power source to supply power to the metal layer 100. When the metal layer 100 is powered on, the heating layer 300 connected to it will heat up, thereby achieving the purpose of heating.
[0082] In this embodiment, both the first insulating layer and the second insulating layer 400 are photocurable flexible coatings. Because the photocurable coating has low water vapor permeability, it improves the heating film's resistance to high temperatures and humidity. For example, the photocurable flexible coating can be a polyurethane-modified acrylate layer or a silicone-modified acrylate layer.
[0083] As can be seen from the above description, in this embodiment, a first insulating layer is formed on the first side of the metal layer 100, and a second insulating layer 400 is formed on one side of the heating layer 300. Both the first insulating layer and the second insulating layer 400 are photocurable flexible coatings. Since the water vapor permeability of the photocurable coating is small, the high temperature and high humidity resistance of the heating film is improved.
[0084] Please continue to refer to Figure 2 This embodiment also includes a third insulating layer 200, which is formed on the second side of the metal layer 100 and located between the metal layer 100 and the heating layer 300. The third insulating layer 200 has trenches that communicate with the metal layer 100 to expose a portion of the metal layer 100, and the heating layer 300 is electrically connected to the metal layer 100 through the trenches. Exemplarily, the third insulating layer 200 can also be formed on the metal layer 100 by spraying or inkjet printing; a shielding layer can be used to shield a portion of the metal layer 100 before the third insulating layer 200 is prepared, and then the shielding layer is removed after the third insulating layer 200 is prepared to form the trenches.
[0085] In this embodiment, the third insulating layer 200 exposes part of the metal layer 100 through grooves, so as to act as a current-carrying strip and be electrically connected to the heating layer 300. This helps to reduce the number of components in the heating film and simplify the manufacturing process.
[0086] Optionally, the third insulating layer 200 in this embodiment includes a polyurethane-modified acrylate layer or an organosilicon-modified acrylate layer, thereby giving it a lower water vapor permeability to further prevent external water vapor from corroding the internal heating layer 300.
[0087] Optionally, in this embodiment, the thicknesses of the first insulating layer, the second insulating layer 400, and the third insulating layer 200 can all be selected to be 80-150 μm, thereby ensuring that the first insulating layer, the third insulating layer 200, and the second insulating layer 400 can have good performance.
[0088] The dielectric strength of the first insulating layer, the second insulating layer 400, and the third insulating layer 200 are all greater than or equal to 10KV / mm, thus ensuring that the heating film has good insulation performance and strong voltage withstand capability, enabling the heating film to work stably for a long time.
[0089] The surface resistivity of the first insulating layer, the second insulating layer 400, and the third insulating layer 200 is all greater than or equal to 1*10. 12 The high surface resistivity (Ω·cm) reduces the current carrying capacity of the heating film surface, ensuring its insulation performance; the high surface resistivity also ensures that the heating film has good corrosion resistance and wear resistance, which helps to extend its service life.
[0090] The water vapor transmission rate of the first insulating layer, the second insulating layer 400, and the third insulating layer 200 is all less than or equal to 1 g / m². 2 / day, thereby preventing the heating layer inside the heating film from being corroded and ensuring the stability of the heating film when working in a high temperature and high humidity environment.
[0091] The metal layer 100 in this embodiment includes an aluminum foil layer, a rolled copper layer, or an electrolytic copper layer, thereby giving the metal layer 100 good moisture resistance and good printing effect, and facilitating the preparation of other film layers on the metal layer 100.
[0092] The thickness of the metal layer 100 can be selected from 20 to 80 μm, and the volume resistivity of the metal layer 100 is ≤0.001 Ω·cm, thereby ensuring that the metal layer 100 has good conductivity.
[0093] In this embodiment, the sum of the thicknesses of the metal layer 100, the first insulating layer, and the third insulating layer 200 can be selected as 100-180 μm, thereby ensuring that the metal layer 100, the first insulating layer, and the third insulating layer 200 have good mechanical properties and durability, and reducing their manufacturing costs while meeting the requirements.
[0094] The heating layer 300 in this embodiment can be made of PTC material, meaning that the heating layer includes a positive temperature coefficient heating layer. Therefore, the heating layer 300 can restrict the flow of current when the temperature rises to a certain level, thus providing protection; and when the temperature drops below a specific temperature, the resistance will return to a lower level.
[0095] The positive temperature coefficient heating layer includes a polymer matrix and conductive fillers, wherein the polymer matrix includes polyethylene, polypropylene or polyvinyl chloride, and the conductive fillers include carbon black, graphite, copper powder, silver powder, tin oxide or zinc oxide.
[0096] For example, in this embodiment, the metal layer 100 and the wire 500 are electrically connected through a conductive adhesive layer, thereby ensuring the conductivity between the metal layer 100 and the wire 500. A fourth insulating layer is also provided at the connection point between the metal layer 100 and the wire 500. It can be understood that the location of the metal layer 100 for connecting the wire can be located at the end of the metal layer 100; the fourth insulating layer covers the connection point between the metal layer 100 and the wire 500 to ensure the insulation of that location.
[0097] In this embodiment, the conductive adhesive layer includes a two-component epoxy resin conductive adhesive layer or a two-component acrylate conductive adhesive layer. The volume resistivity of the conductive adhesive layer is ≤0.001Ω·cm, and the contact resistance between the conductive adhesive layer and the metal layer 100 or the wire 500 is ≤0.05Ω, thereby ensuring good conductivity between the metal layer 100 and the wire 500.
[0098] The fourth insulation layer includes a polyurethane-modified acrylate layer or an organosilicon-modified acrylate layer, which ensures insulation while having a low water vapor permeability to prevent corrosion of the internal heating layer 300.
[0099] Figure 3 This is a flowchart illustrating the preparation process of a heating film provided in one embodiment of this application.
[0100] Please refer to Figure 3 This embodiment also provides a method for preparing a heating film, including:
[0101] Step S110: Provide a metal layer.
[0102] For example, the metal layer can be an aluminum foil layer, a rolled copper layer, or an electrolytic copper layer, thereby giving the metal layer a good printing effect and facilitating the fabrication of other film layers on the metal layer. The thickness of the metal layer can be selected from 20 to 80 μm, and the volume resistivity of the metal layer is ≤0.001 Ω·cm, thereby ensuring that the metal layer has good conductivity.
[0103] Step S120: Prepare a first insulating layer on the first side of the metal layer.
[0104] For example, the first insulating layer may be a photocurable coating, which is formed on the first side of the metal layer by spraying or inkjet printing insulating material and then curing it under light. The first insulating layer includes a polyurethane-modified acrylate layer or a silicone-modified acrylate layer.
[0105] Step S130: A heating layer is prepared on the second side of the metal layer, and the heating layer is electrically connected to the metal layer; wherein, the first side and the second side are opposite sides in the thickness direction of the metal layer.
[0106] For example, the heating layer can be prepared according to the following steps:
[0107] First, the heating layer paste is printed on the second side of the metal layer.
[0108] Then, the printed heating layer paste is baked and cured to form the heating layer.
[0109] The heating layer slurry is a PTC material slurry, and the heating layer includes a positive temperature coefficient heating layer.
[0110] The positive temperature coefficient heating layer includes a polymer matrix and conductive fillers. The polymer matrix includes polyethylene, polypropylene or polyvinyl chloride, and the conductive fillers include carbon black, graphite, copper powder, silver powder, tin oxide or zinc oxide.
[0111] The baking temperature of the heating layer slurry can be 80-150℃; the baking time of the heating layer slurry can be 15-30 minutes.
[0112] Step S140: Prepare a second insulating layer on the side of the heating layer away from the metal layer.
[0113] For example, the second insulating layer can also be a photocurable coating, which is formed on the side of the heating layer away from the third insulating layer by spraying or inkjet printing insulating material and then curing it under light. The second insulating layer includes a polyurethane-modified acrylate layer or an organosilicon-modified acrylate layer.
[0114] Step S150: Electrically connect the wire to the metal layer.
[0115] For example, electrically connecting a wire to a metal layer can be performed according to the following steps:
[0116] First, a conductive adhesive layer is applied to the metal layer where the wires are to be connected, and then the wires are bonded to the conductive adhesive layer. It is understood that the locations on the metal layer where the wires are to be connected can be at the ends of the metal layer.
[0117] Then, a fourth insulating layer is applied at the bonding position between the metal layer and the wire. The fourth insulating layer can also be a photocurable coating. The fourth insulating layer is formed at the bonding position between the metal layer and the wire by spraying or inkjet printing insulating material and then curing it under light.
[0118] The conductive adhesive layer comprises a two-component epoxy resin conductive adhesive layer or a two-component acrylate conductive adhesive layer, wherein the volume resistivity of the conductive adhesive layer is ≤0.001Ω·cm, and the contact resistance between the conductive adhesive layer and the metal layer or wire is ≤0.05Ω. The fourth insulating layer comprises a polyurethane-modified acrylate layer or an organosilicon-modified acrylate layer.
[0119] The method in this embodiment further includes forming a third insulating layer on the second side of the metal layer, the third insulating layer being located between the metal layer and the heating layer. The third insulating layer has trenches that communicate with the metal layer to expose a portion of the metal layer, and the heating layer is electrically connected to the metal layer through the trenches.
[0120] For example, the third insulating layer can also be a photocurable coating, or it can be formed on the second side of the metal layer by spraying or inkjet printing insulating material and then curing it under light. The third insulating layer includes a polyurethane-modified acrylate layer or a silicone-modified acrylate layer.
[0121] Specifically, the preparation of the third insulating layer can be carried out according to the following steps:
[0122] First, a shielding layer is placed on the second side of the metal layer. This shielding layer can partially cover the metal layer to prevent insulating material from adhering to it.
[0123] Then, an insulating material is sprayed onto the metal layer covered with the shielding layer and cured by light, thereby forming an insulating layer on the second side of the metal layer.
[0124] Finally, the shielding layer is removed, and the area shielded by the shielding layer forms a trench that connects to the metal layer, thus forming a third insulating layer.
[0125] In this embodiment, the first insulating layer, the second insulating layer, the third insulating layer, and the fourth insulating layer are all polyurethane-modified acrylate layers or silicone-modified acrylate layers, thereby ensuring that the heating film has a low water vapor permeability and enhancing the heating film's resistance to high temperature and high humidity.
[0126] The metal layer can concentrate the heat and infrared radiation emitted by the heating layer to the second insulating layer, while also achieving a uniform heat distribution and insulation effect. The metal layer has good ductility; compared to the current-carrying strips prepared with silver paste in related technologies, the metal layer in this embodiment has better bending resistance. Furthermore, since there is no need to specially prepare current-carrying strips, it helps to reduce the number of components in the heating film and simplifies the manufacturing process.
[0127] In this embodiment, the first, second, third, and fourth insulating layers can all be formed by spraying insulating material and then curing it under light to create a photocurable flexible coating. Compared to related technologies, this eliminates the need for a backing layer to be heated and cured before connecting adjacent film layers, making it more energy-efficient and avoiding direct damage or hidden internal damage to the heating layer during heating and curing. Furthermore, since no backing layer is required, thermal resistance is reduced, improving heat transfer efficiency.
[0128] In this embodiment, the metal layer and the wire are bonded together with a conductive adhesive layer. This maintains the reliability of the electrical connection between the two and allows for conductive bonding at room temperature. The fabrication process does not require high-temperature curing, simplifying the construction process. Furthermore, it can achieve electrical connections between different types of electrode materials, such as copper, aluminum, and carbon fiber. The method of bonding the metal layer and the wire with a conductive adhesive layer also facilitates subsequent maintenance.
[0129] This embodiment also provides a battery module, including the heating film described above.
[0130] It is understandable that by installing the aforementioned heating film inside the battery module, the normal heating of the battery module can be ensured while improving the heating film's resistance to high temperature and humidity, thereby helping to extend the performance and lifespan of the battery module.
[0131] This embodiment also provides a battery pack, including the above-mentioned battery module.
[0132] Specifically, one or more battery modules can be installed in the battery pack as needed. Because the battery pack uses the aforementioned battery modules, its working stability is better, which helps to improve its charging and discharging performance and extend the service life of the battery pack.
[0133] This embodiment also provides an electrical device, including the battery pack described above.
[0134] Specifically, the electrical equipment includes vehicles (such as new energy vehicles), aircraft, ships, computers, energy storage cabinets, etc. Because the electrical equipment uses the aforementioned battery packs, the equipment has good operational stability, which helps to improve its charging and discharging performance and extend its service life.
[0135] In the description of this application, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "upper", "lower", "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", "outer", "clockwise", "counterclockwise", "axial", "radial", "circumferential", etc., indicating the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this application.
[0136] In this application, unless otherwise expressly specified and limited, the terms "installation," "connection," "joining," "fixing," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two components or the interaction between two components. Those skilled in the art can understand the specific meaning of the above terms in this application according to the specific circumstances.
[0137] It should be noted that in the description of this application, the terms "first" and "second" are used only for convenience in describing different components and should not be construed as indicating or implying a sequential relationship, relative importance, or implicitly specifying the number of technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include at least one of those features.
[0138] The embodiments or implementation methods in this application are described in a progressive manner. Each embodiment focuses on the differences from other embodiments, and the same or similar parts between the embodiments can be referred to each other.
[0139] In the description of this application, the terms "one embodiment," "some embodiments," "illustrative embodiment," "example," "specific example," or "some examples," etc., refer to specific features, structures, materials, or characteristics described in connection with an embodiment or example that are included in at least one embodiment or example of this application. In this application, the illustrative expressions of the above terms do not necessarily refer to the same embodiment or example. Furthermore, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in one or more embodiments or examples.
[0140] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of this application, and are not intended to limit them. Although this application has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some or all of the technical features therein. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of this application.
Claims
1. A heating film, characterized in that, The device includes a first insulating layer, a metal layer (100), a heating layer (300), a second insulating layer (400), and a third insulating layer (200). The first insulating layer is formed on a first side of the metal layer (100), and the heating layer (300) is formed on a second side of the metal layer (100). The heating layer (300) is electrically connected to the metal layer (100). The first side and the second side are opposite sides of the thickness direction of the metal layer (100). The second insulating layer (400) is formed on the side of the heating layer (300) away from the metal layer (100). The metal layer (100) is also connected to a wire (500). The third insulating layer (200) is located between the metal layer (100) and the heating layer (300); the third insulating layer (200) is provided with a groove, the groove is connected to the metal layer (100) to expose part of the metal layer (100), and the heating layer (300) is electrically connected to the metal layer (100) through the groove; Wherein, the first insulating layer and the second insulating layer (400) are both photocurable coatings, and the photocurable coatings include polyurethane modified acrylate layers or silicone modified acrylate layers.
2. The heating film according to claim 1, characterized in that, The third insulating layer (200) includes a polyurethane-modified acrylate layer or an organosilicon-modified acrylate layer.
3. The heating film according to claim 1, characterized in that, The thickness of the first insulating layer, the second insulating layer (400) and the third insulating layer (200) are all 80~150μm.
4. The heating film according to claim 1, characterized in that, The dielectric strength of the first insulating layer, the second insulating layer (400) and the third insulating layer (200) is greater than or equal to 10KV / mm.
5. The heating film according to claim 1, characterized in that, The surface resistivity of the first insulating layer, the second insulating layer (400), and the third insulating layer (200) is all greater than or equal to 1*10. 12 Ω·cm.
6. The heating film according to claim 1, characterized in that, The water vapor permeability of the first insulating layer, the second insulating layer (400) and the third insulating layer (200) is less than or equal to 1 g / m² / day.
7. The heating film according to claim 1, characterized in that, The metal layer (100) includes an aluminum foil layer, a rolled copper layer, or an electrolytic copper layer.
8. The heating film according to claim 6, characterized in that, The thickness of the metal layer (100) is 20~80μm, and the volume resistivity of the metal layer (100) is ≤0.001Ω·cm.
9. The heating film according to claim 1, characterized in that, The sum of the thicknesses of the metal layer (100), the first insulating layer, and the third insulating layer (200) is 100~180μm.
10. The heating film according to claim 1, characterized in that, The heating layer (300) includes a positive temperature coefficient heating layer.
11. The heating film according to claim 10, characterized in that, The positive temperature coefficient heating layer includes a polymer matrix and a conductive filler. The polymer matrix includes polyethylene, polypropylene, or polyvinyl chloride, and the conductive filler includes carbon black, graphite, copper powder, silver powder, tin oxide, or zinc oxide.
12. The heating film according to claim 1, characterized in that, The metal layer (100) and the wire (500) are electrically connected through a conductive adhesive layer, and a fourth insulating layer is also provided at the connection position between the metal layer (100) and the wire (500).
13. The heating film according to claim 12, characterized in that, The conductive adhesive layer includes a two-component epoxy resin conductive adhesive layer or a two-component acrylate conductive adhesive layer, the volume resistivity of the conductive adhesive layer is ≤0.001Ω·cm, and the contact resistance between the conductive adhesive layer and the metal layer (100) or the wire (500) is ≤0.05Ω.
14. The heating film according to claim 12, characterized in that, The fourth insulating layer includes a polyurethane-modified acrylate layer or an organosilicon-modified acrylate layer.
15. A method for preparing a heating film, characterized in that, include: Provide a metal layer; A first insulating layer is formed on a first side of the metal layer; A heating layer is formed on the second side of the metal layer, and the heating layer is electrically connected to the metal layer; wherein the first side and the second side are opposite sides in the thickness direction of the metal layer; A second insulating layer is formed on the side of the heating layer opposite to the metal layer; Electrically connect the wire to the metal layer; A third insulating layer is formed on the second side of the metal layer, the third insulating layer being located between the metal layer and the heating layer; wherein, the third insulating layer has a trench formed therein, the trench communicating with the metal layer to expose a portion of the metal layer, and the heating layer being electrically connected to the metal layer through the trench; Wherein, both the first insulating layer and the second insulating layer are photocurable coatings, and the photocurable coatings include polyurethane-modified acrylate layers or silicone-modified acrylate layers.
16. The method for preparing the heating film according to claim 15, characterized in that, The first insulating layer is formed on the first side of the metal layer by spraying or inkjet printing insulating material and then curing it by light. And / or, the second insulating layer is formed on the side of the heating layer opposite to the metal layer by spraying or inkjet printing insulating material and then curing it by light.
17. The method for preparing the heating film according to claim 16, characterized in that, The third insulating layer includes a polyurethane-modified acrylate layer or a silicone-modified acrylate layer.
18. The method for preparing the heating film according to claim 16, characterized in that, The step of forming a third insulating layer on the second side of the metal layer includes: A shielding layer is covered on the second side of the metal layer; An insulating material is sprayed onto the metal layer covered by the shielding layer and then cured by light. Remove the shielding layer to form the third insulating layer.
19. The method for preparing the heating film according to claim 16, characterized in that, The step of preparing a heat-generating layer on the second side of the metal layer includes: A heating layer paste is printed on the side of the third insulating layer opposite to the metal layer. The printed heating layer paste is baked and cured to form the heating layer.
20. The method for preparing the heating film according to claim 19, characterized in that, The heating layer includes a positive temperature coefficient heating layer.
21. The method for preparing the heating film according to claim 20, characterized in that, The positive temperature coefficient heating layer includes a polymer matrix and a conductive filler. The polymer matrix includes polyethylene, polypropylene, or polyvinyl chloride, and the conductive filler includes carbon black, graphite, copper powder, silver powder, tin oxide, or zinc oxide.
22. The method for preparing the heating film according to claim 19, characterized in that, The baking temperature of the heating layer slurry is 80-150℃; the baking time of the heating layer slurry is 15-30 minutes.
23. The method for preparing the heating film according to claim 15, characterized in that, The step of electrically connecting the wire to the metal layer includes: A conductive adhesive layer is applied to the metal layer at the location where the wire is connected, and the wire is then bonded to the conductive adhesive layer. A fourth insulating layer is applied at the bonding location between the metal layer and the wire.
24. The method for preparing the heating film according to claim 23, characterized in that, The conductive adhesive layer comprises a two-component epoxy resin conductive adhesive layer or a two-component acrylate conductive adhesive layer, wherein the volume resistivity of the conductive adhesive layer is ≤0.001Ω·cm, and the contact resistance between the conductive adhesive layer and the metal layer or the wire is ≤0.05Ω.
25. The method for preparing the heating film according to claim 23, characterized in that, The fourth insulating layer is a polyurethane-modified acrylate layer or an organosilicon-modified acrylate layer.
26. A battery module, characterized in that, Includes the heating film as described in any one of claims 1-14.
27. A battery pack, characterized in that, It includes at least one battery module as described in claim 26.
28. An electrical appliance, characterized in that, Includes the battery pack as described in claim 27.
Citation Information
Patent Citations
Organic PTC heating film
CN213718245U
Manufacture of mirror with heater
JP2000127911A