Automatic welding method and welding system for air conditioner pipeline

By obtaining and adjusting welding parameters in real time, the problems of unstable welding strength and low reliability in the prior art are solved, and higher welding quality and reliability are achieved.

CN120079973AActive Publication Date: 2025-06-03FOSHAN SHUANGYI ELECTRICAL TECH IND CO LTD

Patent Information

Application Number
CN202510559992.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-04-30
Publication Date
2025-06-03
Estimated Expiration
2045-04-30

AI Technical Summary

Technical Problem

The prior art cannot adjust the welding process according to the real-time state changes of copper pipes and stainless steel pipes during welding, resulting in unstable welding strength and low reliability.

Method used

The automatic welding method is adopted to obtain the physical parameters and environmental parameters of the pipeline to be welded, and the welding parameters are adjusted in real time, including parameters in the arc starting, self-adjustment and arc closing stages to adapt to the state changes of copper pipes and stainless steel pipes.

Benefits of technology

It effectively overcomes the thermal conductivity difference between copper and stainless steel, reduces the probability of defects such as pore cracks, and improves the reliability of automatic welding.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120079973A_ABST
    Figure CN120079973A_ABST
Patent Text Reader

Abstract

The invention relates to an automatic welding method and system for an air conditioner pipeline, and the method comprises the steps: arcing stage welding: determining arcing welding parameters according to first physical parameters and first environmental parameters, and carrying out arcing stage welding; the self-adjusting stage welding comprises the steps that an adjusting strategy is determined according to the second physical parameters, the welding parameters are adjusted in real time according to the adjusting strategy, and self-adjusting stage welding is conducted; the arc suppression stage welding comprises the steps that arc suppression welding parameters are determined according to the welding parameters of the self-adjusting stage, and arc suppression stage welding is carried out. In the welding process, relevant parameters are collected in real time, welding parameters of automatic welding are adjusted in real time according to the relevant parameters, heat conduction difference between copper and stainless steel can be effectively overcome by collecting relevant parameters of a molten pool, current, voltage and the like in real time and dynamically adjusting welding energy input, the probability of occurrence of defects such as air holes and cracks is reduced, and welding quality is improved. And the reliability of automatic welding is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of automatic welding, and in particular to an automatic welding method and welding system for air-conditioning pipelines. Background Art

[0002] Copper pipes, aluminum pipes, and iron pipes are commonly used in air-conditioning and heat exchanger pipelines. These materials not only have high procurement costs but also poor corrosion resistance and pressure resistance. Currently, there is also a solution to use stainless steel to replace copper products and manufacture composite pipes through welding, but the welding method is relatively simple and not mature enough.

[0003] For example, Chinese Patent Publication No. CN114110284A discloses a stainless-steel air-conditioning pipeline, which includes a welded stainless-steel pipe body (the material includes SUS304 / 304L, SUS436 / 436J1L, SUS409 / 409L). A copper connecting pipe and a stainless-steel connecting pipe are welded above the welded stainless-steel pipe body, or copper connecting pipes and stainless-steel connecting pipes are welded at both ends respectively. It can be applied in various pipelines, and the use amount of copper pipes can be reduced to the greatest extent. It can be applied to stainless-steel gas (water) collecting pipes, mufflers, filters, three-way pipes, and U-shaped pipes, with a wide range of applications. The stainless-steel pipe has good corrosion resistance, strong pressure resistance and tensile strength. The manufacturing cost can be reduced to the greatest extent, and the service life of the product can be improved. A unique welding technology is adopted to ensure that the metal filler metal forms good wettability and spreadability, increase the strength and sealing performance of the weld, with beautiful weld formation, no leakage, strong corrosion resistance and high pressure resistance of the product, effectively reducing the use amount of copper pipes on the air-conditioning pipeline, greatly reducing the manufacturing cost, with high social and economic benefits and strong practicability. Thus, it can be seen that the existing technology replaces copper with stainless steel and welds to produce composite pipes through welding technology. However, its welding process or procedure only simply sets relevant physical parameters or electrical parameters, and welding is carried out according to the set parameters during the whole welding process, without considering that the states of the copper pipe and the stainless-steel pipe change during the welding process, and the same or preset parameters cannot adapt to the state changes of the copper pipe and the stainless-steel pipe and the whole welding process flow, resulting in defects such as cracks and pores in the welding, and low reliability. Summary of the Invention

[0004] Therefore, the present invention provides an automatic welding method and welding system for air-conditioning pipelines to overcome the problem in the prior art that the welding process flow cannot be adjusted according to the real-time state changes of the copper pipe and the stainless-steel pipe during the welding process, resulting in unstable welding strength and low reliability.

[0005] To achieve the above object, the present invention provides an automatic welding method for air-conditioning pipelines, including: Obtain the first physical parameters and the first environmental parameters of the copper pipe to be welded and the stainless steel pipe to be welded. Among them, the first physical parameters include the thickness of the welded part of the stainless steel pipe, the thickness of the welded part of the copper pipe, and the wire diameter, and the first environmental parameters include air humidity, air temperature, and the concentration of acidic gases in the air; Determine the arc starting welding parameters according to the first physical parameters and the first environmental parameters, and perform welding in the arc starting stage according to the arc starting welding parameters; After the welding in the arc starting stage is completed, perform welding in the self-adjusting stage, Obtain the second physical parameters of the molten pool in real time. Among them, the second physical parameters include the surface temperature of each position of the molten pool; Determine the characteristics of the welding molten pool according to the second physical parameters, and judge whether to adjust the welding parameters in real time based on the molten pool parameters corresponding to the characteristics of the welding molten pool. Perform welding in the self-adjusting stage according to the welding parameters adjusted in real time. Among them, the characteristics of the welding molten pool include the first boundary of the molten pool close to the copper pipe side and the second boundary of the molten pool close to the stainless steel pipe side, and the molten pool parameters include the molten pool surface area and the molten pool surface temperature; After the welding in the self-adjusting stage is completed, enter the arc extinguishing stage for welding. Determine the arc extinguishing welding parameters according to the welding parameters in the self-adjusting stage, and perform welding in the arc extinguishing stage according to the arc extinguishing welding parameters.

[0006] Further, the process of determining the arc starting welding parameters according to the first physical parameters and the first environmental parameters includes: Determine the arc starting voltage according to the thickness of the welded part of the stainless steel pipe and the thickness of the welded part of the copper pipe, determine the arc starting current according to the wire diameter, determine the arc starting length according to the arc starting voltage and the arc starting current, and determine the initial wire feeding speed according to the arc starting current; Determine the nozzle diameter of the shielding gas according to the arc starting current, the arc starting voltage, and the arc starting length; Determine the initial shielding gas flow rate according to the air humidity, the air temperature, the concentration of acidic gases in the air, and the nozzle diameter.

[0007] Further, the process of determining the arc starting voltage according to the thickness of the welded part of the stainless steel pipe and the thickness of the welded part of the copper pipe includes: Determine the average thickness of the welded part according to the thickness of the welded part of the stainless steel pipe and the thickness of the welded part of the copper pipe; Determine the welding proportional coefficient according to the average thickness; Determine the arc starting voltage according to the welding proportional coefficient and the base voltage.

[0008] Further, the process of determining the arc starting current according to the wire diameter includes: Determine the distribution coefficient according to the thickness of the welded part of the stainless steel pipe and the thickness of the welded part of the copper pipe, and determine the arc starting current according to the current coefficient per unit thickness, the distribution coefficient, and the wire diameter.

[0009] Further, the process of determining the initial protective gas flow rate according to the air humidity, air temperature, and concentration of acidic gas in the air includes: Determine the basic flow rate of the protective gas according to the welding speed and nozzle diameter, determine the humidity correction value, temperature correction value, and acidic gas correction value according to the air humidity, air temperature, and concentration of acidic gas in the air respectively, and determine the initial protective gas flow rate according to the basic flow rate, humidity correction value, temperature correction value, and acidic gas correction value.

[0010] Further, the process of determining the welding pool characteristics of the welding pool includes: Identify the isotherms on the copper tube side and the isotherms on the stainless steel tube side corresponding to the welding pool respectively, use the isotherm corresponding to the first temperature on the copper tube side as the first boundary of the welding pool, use the isotherm corresponding to the second temperature on the stainless steel tube side as the second boundary of the welding pool, and determine the surface area of the welding pool according to the first boundary and the second boundary of the welding pool. Uniformly set a number of monitoring points between the center of the welding pool and the first boundary and the second boundary of the welding pool and obtain the temperatures of the monitoring points, and determine the surface temperature of the welding pool according to the temperatures of the monitoring points.

[0011] Further, the process of determining whether to adjust the welding parameters in real time based on the welding pool parameters corresponding to the welding pool characteristics includes: Determine whether to adjust the welding current and / or welding speed according to the comparison result between the surface temperature of the welding pool and the preset temperature range; Determine whether to adjust the welding voltage and / or arc length according to the comparison result between the surface area of the welding pool and the preset area range.

[0012] Further, it further includes: adjusting the wire feeding speed according to the welding speed and welding current in the self-adjustment stage, and dynamically adjusting the current protective gas flow rate according to the welding speed, the surface temperature of the welding pool, and the initial protective gas flow rate in the self-adjustment stage.

[0013] Further, the process of determining the arc-extinguishing welding parameters according to the welding parameters in the self-adjustment stage includes: Determine the arc-extinguishing current according to the welding current in the self-adjustment stage, the arc-extinguishing current is positively correlated with the welding current in the self-adjustment stage, determine the arc-extinguishing voltage according to the welding voltage in the self-adjustment stage, and the arc-extinguishing voltage is positively correlated with the welding voltage in the self-adjustment stage.

[0014] On the other hand, the present invention also provides an automatic welding system for air-conditioning pipelines, including: A data acquisition module for acquiring the first physical parameters and first environmental parameters of the copper tube and stainless steel tube to be welded, and for acquiring the second physical parameters of the welding pool in real time; The starting arc welding parameter determination module, which is connected to the data acquisition module, is used to determine the starting arc welding parameters according to the first physical parameter and the first environmental parameter; The self-adjustment strategy analysis module, which is connected to the data acquisition module, is used to determine the characteristics of the welding molten pool according to the second physical parameter, and judge whether it is necessary to adjust the welding parameters in real time based on the pool parameters corresponding to the characteristics of the welding molten pool; The ending arc welding parameter determination module, which is connected to the data acquisition module, is used to determine the ending arc welding parameters according to the welding parameters in the self-adjustment stage; The automatic welding equipment, which is respectively connected to the starting arc welding parameter determination module, the self-adjustment strategy analysis module and the ending arc welding parameter determination module, is used to weld the copper pipe to be welded and the stainless steel pipe to be welded according to the welding parameters in the starting arc stage, the self-adjustment stage and the ending arc stage.

[0015] Compared with the prior art, the beneficial effects of the present invention are as follows. The automatic welding method and welding system for air-conditioning pipelines of the present invention use stainless steel to replace copper and weld and produce composite pipes through automatic welding technology. During the welding process, relevant parameters are collected in real time and the welding parameters of the automatic welding are adjusted in real time according to the relevant parameters. By collecting relevant parameters such as molten pool related parameters, current and voltage in real time and dynamically adjusting the welding energy input, the thermal conductivity difference between copper and stainless steel can be effectively overcome, the occurrence probability of defects such as pores and cracks can be reduced, and the reliability of automatic welding can be improved.

[0016] Furthermore, the present invention matches the gas flow rate through environmental parameters and nozzle diameter, which can effectively isolate moisture and acidic gases in the air, avoid hydrogen embrittlement, nitridation or sulfide pollution of the molten pool, and avoid waste caused by excessive gas supply during the starting arc stage through the matching of nozzle diameter and flow rate, while preventing protection failure due to insufficient flow rate. During the welding process, the flow rate of the shielding gas is dynamically adjusted according to the welding speed and the surface temperature of the molten pool, significantly reducing the porosity and surface oxidation.

[0017] Furthermore, the thermal conductivity of stainless steel and copper differs significantly. The present invention welds stainless steel and copper. Based on the average thickness, the starting arc voltage is corrected by a proportionality coefficient, which can dynamically balance the thermal requirements of stainless steel and copper, avoid insufficient penetration on the copper side due to excessive heat dissipation, and prevent intergranular corrosion caused by overheating on the stainless steel side.

[0018] Furthermore, the present invention adjusts the welding current and / or welding speed based on the surface temperature of the molten pool. The surface temperature of the molten pool directly reflects the heat input. When it is detected that the temperature exceeds the preset range, it indicates that the temperature is too high, and the welding current and / or welding speed are automatically adjusted to reduce the heat input per unit length and avoid burn-through or grain coarsening. When the temperature is too low, reverse adjustment is performed to ensure that the penetration meets the standard.

[0019] Furthermore, based on the adjustment of the welding voltage and / or arc length according to the molten pool surface area, the molten pool surface area reflects the state of arc energy distribution. An overly large surface area indicates that the arc is divergent. Reducing the voltage or shortening the arc can increase the arc energy density, suppressing the excessive spreading of the molten pool. If the surface area is too small, the adjustment is reversed to avoid incomplete fusion defects.

[0020] Furthermore, the method and system of the present invention can obtain the second physical parameters of the molten pool in real time through the data acquisition module. When deformation is caused by the difference in the thermal expansion coefficients of copper and steel, the welding parameters can be automatically compensated to ensure the stability and quality of welding.

[0021] Furthermore, the air-conditioning pipeline of the present invention uses stainless steel instead of copper, significantly reducing the material cost. Combining real-time parameter adjustment reduces the rejection rate of products, and cooperating with automatic welding control realizes the collaborative optimization of cost reduction and efficiency improvement. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 is the overall flowchart of the method of the embodiment of the present invention; Figure 2 is the adjustment flowchart of determining the welding current and / or welding speed according to the molten pool surface temperature and the preset temperature range in the embodiment of the present invention; Figure 3 is the adjustment flowchart of determining the welding voltage and / or arc length according to the molten pool surface area and the preset area range in the embodiment of the present invention; Figure 4 is the adjustment flowchart of determining the welding current and / or welding speed according to the molten pool temperature and the preset temperature range in the embodiment of the present invention; Figure 5 is the adjustment flowchart of determining the welding speed and / or welding current according to the molten pool length and the preset length range in the embodiment of the present invention; Figure 6 is the adjustment flowchart of determining the welding voltage and / or arc length according to the molten pool width and the preset width range in the embodiment of the present invention; Figure 7 is the adjustment flowchart of determining the welding current and / or welding speed according to the molten pool depth and the preset depth range in the embodiment of the present invention; Figure 8 is the schematic diagram of the system structure of the embodiment of the present invention; Figure 9 is the block diagram of the structure of the electronic device of the embodiment of the present invention. DETAILED DESCRIPTION OF THE EMBODIMENTS

[0023] In order to make the objectives and advantages of the present invention clearer and more understandable, the present invention will be further described below in conjunction with embodiments; it should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0024] The preferred embodiments of the present invention will be described below with reference to the accompanying drawings. Those skilled in the art should understand that these embodiments are only used to explain the technical principle of the present invention and do not limit the protection scope of the present invention.

[0025] It should be noted that in the description of the present invention, the terms indicating the direction or positional relationship such as "upper", "lower", "left", "right", "inner", "outer", etc. are based on the direction or positional relationship shown in the drawings. This is only for convenience of description and does not indicate or imply that the device or element must have a specific orientation, be constructed and operated in a specific orientation. Therefore, it should not be construed as a limitation of the present invention.

[0026] In addition, it should also be noted that in the description of the present invention, unless otherwise clearly specified and defined, the terms "installation", "connection", "connection" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium, and it can be the communication inside two elements. For those skilled in the art, the specific meanings of the above terms in the present invention can be understood according to specific situations.

[0027] In the welding method of the present invention, the copper pipe to be welded and the stainless steel pipe to be welded are both round pipes. The movement mode of the welding rod is circular movement, and the included angle between the axis of the welding rod and the tangent direction of the weld is 75° - 85°.

[0028] Please refer to Figure 1 As shown, an automatic welding method for air-conditioning pipelines according to an embodiment of the present invention includes: Step S1, obtaining the first physical parameters and the first environmental parameters of the copper pipe to be welded and the stainless steel pipe to be welded. Among them, the first physical parameters include the thickness of the welding part of the stainless steel pipe, the thickness of the welding part of the copper pipe, and the diameter of the welding wire, and the first environmental parameters include air humidity, air temperature, and the concentration of acidic gases in the air; Step S2, determining the arc starting welding parameters according to the first physical parameters and the first environmental parameters, and performing welding in the arc starting stage according to the arc starting welding parameters; Step S3, when the welding in the arc starting stage is completed, perform welding in the self-adjusting stage. Among them, Step S31, obtaining the second physical parameters of the molten pool in real time. Among them, the second physical parameters include the surface temperature of each position of the molten pool; Step S32: Determine the characteristics of the welding molten pool according to the second physical parameter, and judge whether to adjust the welding parameters in real time based on the molten pool parameters corresponding to the characteristics of the welding molten pool. Perform welding in the self-adjustment stage according to the welding parameters adjusted in real time. Among them, the characteristics of the welding molten pool include the first boundary of the molten pool close to the copper pipe side and the second boundary of the molten pool close to the stainless steel pipe side, and the molten pool parameters include the surface area of the molten pool and the surface temperature of the molten pool. Step S4: After the welding in the self-adjustment stage is completed, enter the welding in the arc extinguishing stage. Determine the arc extinguishing welding parameters according to the welding parameters in the self-adjustment stage, and perform welding in the arc extinguishing stage according to the arc extinguishing welding parameters.

[0029] The automatic welding method and welding system for air-conditioning pipelines of the present invention use stainless steel to replace copper and weld and produce composite pipes through automatic welding technology. During the welding process, relevant parameters are collected in real time and the welding parameters of the automatic welding are adjusted in real time according to the relevant parameters. By collecting relevant parameters of the molten pool, such as current and voltage, and dynamically adjusting the welding energy input, the thermal conductivity difference between copper and stainless steel can be effectively overcome, the occurrence probability of defects such as pores and cracks can be reduced, and the reliability of the automatic welding can be improved.

[0030] The air-conditioning pipelines of the present invention use stainless steel to replace copper, which significantly reduces the material cost. Combining real-time parameter adjustment reduces the rejection rate of products, and cooperating with automatic welding control realizes the collaborative optimization of cost reduction and efficiency improvement.

[0031] Specifically, in step S1, the first physical parameters of the copper pipe to be welded and the stainless steel pipe to be welded can be obtained by measuring the dimensions of the copper pipe to be welded, the stainless steel pipe to be welded, and the welding wire. The first environmental parameter can be measured by setting a number of corresponding sensors.

[0032] Specifically, in step S2, the process of determining the starting arc welding parameters according to the first physical parameter and the first environmental parameter includes: Step S21: Determine the starting arc voltage according to the thickness of the welding part of the stainless steel pipe and the thickness of the welding part of the copper pipe, determine the starting arc current according to the diameter of the welding wire, determine the starting arc length according to the starting arc voltage and the starting arc current, and determine the initial wire feeding speed according to the starting arc current. Step S22: Determine the nozzle diameter of the shielding gas according to the starting arc current, the starting arc voltage and the starting arc length. Step S23: Determine the initial shielding gas flow rate according to the air humidity, the air temperature, the concentration of acidic gas in the air and the nozzle diameter.

[0033] Specifically, in step S21, the process of determining the starting arc current according to the diameter of the welding wire includes: determining the distribution coefficient according to the thickness of the welding part of the stainless steel pipe and the thickness of the welding part of the copper pipe, and determining the starting arc current according to the current coefficient per unit thickness, the distribution coefficient and the diameter of the welding wire.

[0034] In one embodiment, the distribution coefficient is determined according to the thickness of the welded joint of the stainless steel pipe and the thickness of the welded joint of the copper pipe. Let the thickness of the welded joint of the stainless steel pipe be , with the unit of mm, and the thickness of the welded joint of the copper pipe be , with the unit of mm. Then the distribution coefficient of the stainless steel pipe is , and the distribution coefficient of the copper pipe is , is the current coefficient per unit thickness of stainless steel (30 - 40 A / mm), is the current coefficient per unit thickness of copper (80 - 150 A / mm). Then the formula for the starting arc current is as follows:

[0035] Among them, is the correction value of the steel pipe, taking 20, is the correction value of the copper pipe, taking 30. The correction value is positive for thin plates and negative for thick plates. For example, if the thickness of the welded joint of the stainless steel pipe is 3 mm and the thickness of the welded joint of the copper pipe is 5 mm, then is 20, is -30, and d is the diameter of the welding wire, with the unit of mm.

[0036] Specifically, in step S21, the process of determining the starting arc voltage according to the thickness of the welded joint of the stainless steel pipe and the thickness of the welded joint of the copper pipe includes: Determine the average thickness of the welded joint according to the thickness of the welded joint of the stainless steel pipe and the thickness of the welded joint of the copper pipe, determine the welding ratio coefficient according to the average thickness, and determine the starting arc voltage according to the welding ratio coefficient and the base voltage.

[0037] In one embodiment, the thickness of the welded joint of the stainless steel pipe is , and the thickness of the welded joint of the copper pipe is , then the average thickness of the welded joint is . Preset the average thickness range, and the two endpoint values of the average thickness range are respectively taken as the minimum value and the maximum value of the thickness data of the qualified air-conditioning pipeline in historical welding. Determine the welding ratio coefficient according to the average thickness of the welded joint and the average thickness range , The value range is 0.05 - 0.15 V / A. Determine the proportionality coefficient according to the position of the average thickness of the welded joint in the average thickness range. For example, if the average thickness of the welded joint is the median of the average thickness range, then the proportionality coefficient takes the median value of the value range of 0.05 - 0.15 V / A, that is, 0.10 V / A. The base voltage C is the no-load voltage of the automatic welding equipment, then the starting arc voltage is the sum of the base voltage C and the product of the proportionality coefficient and the starting arc current.

[0038] It is understandable that there are differences in the thermal conductivity of stainless steel and copper. When welding a stainless steel pipe and a copper pipe in the present invention, based on the average thickness, the starting arc voltage is corrected by a proportionality coefficient, which can dynamically balance the thermal requirements of stainless steel and copper, avoid insufficient penetration on the copper side due to excessive heat dissipation, and prevent intergranular corrosion caused by overheating on the stainless steel side.

[0039] Specifically, in step S21, the starting arc length is determined according to the starting arc voltage and the starting arc current.

[0040] In one embodiment, the starting arc length is calculated according to the following formula:

[0041] where, is the starting arc length, in mm, is the proportionality constant, in A / V, with a value range of 0.1 - 0.3, is the starting arc voltage, in V, is the starting arc current, in A, is the material current coefficient of stainless steel, taking 1.0, is the material current coefficient of copper, taking 1.8, is the humidity correction coefficient, with a value range of 0.05 - 0.15. For humidity-sensitive materials, a higher value is taken. When the welding material is sensitive to humidity (moisture) in the air, the value of the humidity correction coefficient should be selected as the larger value in its value range (0.05 - 0.15) (i.e., close to 0.15), is the relative humidity of the air.

[0042] Specifically, in step S21, the initial wire feeding speed is determined according to the starting arc current.

[0043] In one embodiment, the initial wire feeding speed is the starting arc current (in A) divided by the wire melting coefficient (in A·min / m). Among them, the wire melting coefficient is usually 2 - 6 A·min / m, depending on the wire material and diameter. In this embodiment, the wire material is preferably a steel wire, with a diameter of 0.001 m, and the wire melting coefficient takes .

[0044] Specifically, after the starting arc voltage and the starting arc current in the starting arc stage are determined, the initial welding speed in the starting arc stage can be determined according to the starting arc voltage and the starting arc current. Specifically, the initial welding speed in the starting arc stage is calculated according to the following formula:

[0045] where, is the initial welding speed in the starting arc stage, P is the comprehensive correction coefficient (determined through process tests, typical range ), is the arcing current, is the arcing voltage, is the average thermal conductivity of the material, taking the average value of the thermal conductivities of stainless steel and copper, h is the average thickness of the material, in mm, taking the average thickness at the welding joint. The thickness of the welding joint of the stainless steel pipe is and the thickness of the welding joint of the copper pipe is , then the average thickness of the welding joint is .

[0046] Specifically, in step S22, the process of determining the nozzle diameter of the shielding gas according to the arcing current, arcing voltage and arcing length includes: The arcing current and arcing voltage determine the initial heat input during welding. The nozzle diameter determines the coverage range of the shielding gas. The higher the heat input, the larger the coverage range required, and the nozzle diameter needs to be increased. The larger the arcing length, the smaller the required coverage range of the shielding gas, and thus the nozzle diameter can be reduced. Therefore, the nozzle diameter is positively correlated with the heat input, that is, the product of the arcing current and the arcing voltage, and negatively correlated with the arcing length.

[0047] In one embodiment, the nozzle diameter is the product of the arcing voltage and the arcing current multiplied by the comprehensive process coefficient and then divided by the arcing length. The comprehensive process coefficient needs to be calibrated through experiments, and the recommended initial value is 0.02 - 0.05 ).

[0048] Among them, the comprehensive process coefficient can be calibrated through multi-variable orthogonal experiments. Design multiple combinations of arcing voltage, arcing current and arcing length, such as a 3×3×3 orthogonal experiment table, and fit the average value and confidence interval of the comprehensive process coefficient through a large amount of experimental data to eliminate the single-variable error.

[0049] Specifically, in step S23, the process of determining the initial shielding gas flow rate according to the air humidity, air temperature, concentration of acidic gases in the air and the nozzle diameter includes: Determine the basic flow rate of the shielding gas according to the welding speed and the nozzle diameter, determine the humidity correction value, temperature correction value and acidic gas correction value according to the air humidity, air temperature and concentration of acidic gases in the air respectively, and determine the initial shielding gas flow rate according to the basic flow rate, humidity correction value, temperature correction value and acidic gas correction value.

[0050] In one embodiment, the initial shielding gas flow rate Q is as follows:

[0051] Among them, is the automatic welding correction coefficient, in mm, taking 0.8, is the nozzle diameter, in mm, is the initial welding speed, with the unit of mm / s, is the humidity correction value, is the temperature correction value, is the acid gas correction value, is the air humidity, is the difference between the air temperature and the standard temperature (25 °C), is the concentration of acid gas.

[0052] More specifically, for the humidity correction value , a humidity critical threshold is set. When , the humidity correction is started, = 0.02.

[0053] For the temperature correction value , piecewise correction is implemented. When , takes 0.1. When , takes 0. When 15 °C , takes 0.05.

[0054] For the acid gas correction value , piecewise correction is implemented. When 5 ppm, takes 0.1. When 5 20 ppm, takes 0.3. When , takes 0.5.

[0055] It can be understood that the above humidity correction value, temperature correction value, and acid gas correction value are also used to eliminate the dimensions of humidity, temperature, and acid gas concentration.

[0056] The present invention matches the gas flow rate through environmental parameters and nozzle diameter, can effectively isolate moisture and acid gas in the air, avoid hydrogen embrittlement, nitridation, or sulfide pollution of the molten pool. By matching the nozzle diameter and flow rate, it avoids waste caused by excessive gas supply during the arc starting stage, and at the same time prevents protection failure due to insufficient flow rate. During the welding process, the protective gas flow rate is dynamically adjusted according to the welding speed and the surface temperature of the molten pool, significantly reducing the porosity and surface oxidation.

[0057] Specifically, in step S32, determining the characteristics of the welding molten pool of the molten pool includes: Use an infrared thermal imager to photograph the molten pool, respectively identify the isotherms corresponding to the copper tube side and the stainless steel tube side of the molten pool, take the isotherm corresponding to the first temperature on the copper tube side as the first boundary of the molten pool, take the isotherm corresponding to the second temperature on the stainless steel tube side as the second boundary of the molten pool, and determine the surface area of the molten pool according to the first boundary and the second boundary of the molten pool. Uniformly set a number of monitoring points between the center of the molten pool and the first boundary and the second boundary of the molten pool and obtain the temperatures of the monitoring points, and determine the surface temperature of the molten pool according to the temperatures of the monitoring points.

[0058] Specifically, the first temperature is the melting point of the copper tube, and the melting point of copper, about 1083 °C, can be taken. The second temperature is the melting point of the stainless steel tube, and the melting point of stainless steel, about 1450 °C, is taken. The first boundary and the second boundary are the boundaries on both sides of the molten pool. The front and rear boundaries of the molten pool are the third boundary and the fourth boundary respectively. The third boundary is the solidification boundary of the welding wire (the isotherm corresponding to the third temperature is used as the third boundary of the molten pool, and the third temperature usually takes the melting point of the welding wire), and the fourth boundary is the current welding position. The area enclosed by the first boundary and the second boundary of the molten pool and the closed area composed of the third boundary and the fourth boundary is determined as the surface of the molten pool. After determining the surface of the molten pool, the specific surface area of the molten pool can be obtained based on machine vision.

[0059] It can be understood that since the two sides of the welding in the present invention are different metals and there are differences in their physical properties, therefore, in identifying the size of the molten pool area, the corresponding temperature identification boundary is adopted to distinguish the welding influence area from the molten pool area, so that the range of the molten pool boundary can be accurately obtained, the identification accuracy of the molten pool size is improved, and thus the adjustment accuracy of adjusting the welding parameters based on the molten pool characteristics in the present invention is improved.

[0060] When welding dissimilar metals, such as copper and stainless steel in this application, the difference in the thermal conductivity of copper and stainless steel is large. The traditional optical method is easily interfered by thermal deformation and it is difficult to uniformly calibrate the molten pool boundary. The method of dividing temperature thresholds can independently adapt to different material characteristics. The present invention delimits the molten pool boundary through the isotherm corresponding to the melting point, avoids misjudging the heat affected zone as the molten pool, and can independently calibrate the true melting range on both material sides.

[0061] The accurate calibration of the molten pool boundary in the present invention is the premise for determining whether the interface of dissimilar metals is fully melted. And the accurate control of the molten pool surface area can avoid incomplete fusion or excessive penetration. Real-time monitoring of the molten pool surface area and temperature gradient can quantify the thermal state of the molten pool and avoid brittle phases (grain coarsening) or microcracks (deformation or burn-through, the molten pool fails to cover the welding path, resulting in incomplete fusion or weld discontinuity) caused by uneven temperature. By setting the molten pool boundary through the temperature threshold method, the identification accuracy of the molten pool characteristics in dissimilar metal welding is significantly improved, and then the dynamic optimization of welding parameters is realized, and the welding quality is improved.

[0062] Specifically, the average value of the temperatures at several monitoring points is used as the molten pool surface temperature data.

[0063] Specifically, the process of determining whether to adjust the welding parameters in real time based on the molten pool parameters corresponding to the welding molten pool characteristics includes: Determining the adjustment of the welding current and / or the welding speed according to the comparison result between the molten pool surface temperature and the preset temperature range; Determining the adjustment of the welding voltage and / or the arc length according to the comparison result between the molten pool surface area and the preset area range.

[0064] Please refer to Figure 2 , in one embodiment, determining the adjustment of the welding current and / or the welding speed according to the molten pool surface temperature and the preset temperature range includes: If the molten pool surface temperature is greater than the maximum value of the preset temperature range, the welding current is reduced by 5% - 10% each time based on the existing welding current and / or the welding speed is increased by 10 - 20 cm / min each time based on the existing welding speed until the molten pool surface temperature drops within the preset temperature range; If the molten pool surface temperature is less than the minimum value of the preset temperature range, the welding current is increased by 5% - 10% each time based on the existing welding current and / or the welding speed is reduced by 10 - 20 cm / min each time based on the existing welding speed until the molten pool surface temperature rises within the preset temperature range.

[0065] If the molten pool surface temperature is within the preset temperature range, the current welding current and welding speed are maintained.

[0066] As an implementation method, the preset temperature range is determined according to the average temperature of the molten pool during the welding process without welding defects such as cracks and pores in the historical automatic welding of air-conditioning pipelines. During the welding process of each copper pipe to be welded and stainless steel pipe to be welded, the second physical parameters of the molten pool include: the molten pool surface temperature and the molten pool surface area are both detected, recorded and saved in real time. After the first N automatic weldings are completed, the finished products are inspected. For the n qualified finished products (n ≤ N) (without welding defects such as cracks and pores), the average value of the molten pool surface temperatures during the welding processes of the n finished products is taken to form a temperature set. The maximum value in the temperature set is taken as the upper limit value of the preset temperature range, and the minimum value in the set is taken as the lower limit value of the preset temperature range. According to this preset temperature range, the (N + 1)-th automatic welding is carried out. After the welding is completed, if the finished product is qualified (without welding defects such as cracks and pores), the average value of the molten pool surface temperature during this welding process is added to the above temperature set for update, and then the preset temperature range is re-determined.

[0067] The present invention adjusts the welding current and / or welding speed based on the temperature of the molten pool surface. The temperature of the molten pool surface directly reflects the heat input. When it is detected that the temperature exceeds the preset range, it indicates that the temperature is too high, and the welding current and / or welding speed are automatically adjusted to reduce the heat input per unit length and avoid burn-through or grain coarsening. When the temperature is too low, reverse adjustment is performed to ensure that the penetration meets the standard.

[0068] It can be understood that whether to adjust the welding current and / or welding speed is determined according to the comparison result between the temperature of the molten pool surface and the preset temperature range. Adjusting the welding current and / or welding speed can both achieve the adjustment and control of the temperature of the molten pool surface. One welding parameter of the welding current and the welding speed can be adjusted only, or both the welding current and the welding speed can be adjusted.

[0069] In one embodiment, the adjustment of the welding voltage and / or the arc length according to the surface area of the molten pool and the preset area range includes: If the surface area of the molten pool is greater than the maximum value of the preset area range, the welding voltage is reduced in steps of 2 - 3V based on the existing welding voltage, and / or the arc length is shortened in steps of 0.1 - 0.2mm until the surface area of the molten pool drops within the preset area range; If the surface area of the molten pool is less than the minimum value of the preset area range, the welding voltage is increased in steps of 2 - 3V based on the existing welding voltage, and / or the arc length is extended in steps of 0.1 - 0.2mm until the surface area of the molten pool rises within the preset area range.

[0070] If the surface area of the molten pool is within the preset area range, the current welding voltage and arc length are maintained.

[0071] As an implementation method, the preset area range is determined according to the average surface area of the molten pool during the welding process without welding defects such as cracks and pores in the historical automatic welding of air-conditioning pipelines. During the welding process of the copper pipe to be welded and the stainless-steel pipe to be welded each time, the second physical parameters of the molten pool include: the temperature of the molten pool surface and the surface area of the molten pool are both detected, recorded, and saved in real time. After the first N automatic weldings are completed, the finished products are inspected. For the n qualified finished products (n ≤ N) (without welding defects such as cracks and pores), the average value of the surface areas of the molten pool during the welding of the n finished products is taken to form a surface area set. The maximum value in the surface area set is taken as the upper limit value of the preset area range, and the minimum value in the set is taken as the lower limit value of the preset area range. According to this preset area range, the (N + 1)-th automatic welding is performed. After the welding is completed, if the finished product is qualified (without welding defects such as cracks and pores), the average value of the surface area of the molten pool during this welding process is added to the above surface area set for update, and then the preset area range is re-determined.

[0072] The present invention adjusts the welding voltage and / or the arc length based on the surface area of the molten pool. The surface area of the molten pool reflects the state of the arc energy distribution. An overly large surface area indicates that the arc is divergent. By reducing the voltage or shortening the arc, the arc energy density is increased, and the excessive spreading of the molten pool is inhibited. If the surface area is too small, the adjustment is reversed to avoid the lack of fusion defect.

[0073] It can be understood that whether to adjust the welding voltage and / or the arc length is determined according to the comparison result between the surface area of the molten pool and the preset area range. Adjusting the welding voltage and / or the arc length can both achieve the adjustment and control of the surface temperature of the molten pool. One of the welding parameters, namely the welding voltage and the arc length, can be adjusted, or both the welding voltage and the arc length can be adjusted.

[0074] The present invention also provides another implementation manner. The second physical parameters of the molten pool include: the temperature of the molten pool (the surface temperature of the molten pool), the length of the molten pool (determined according to the third boundary and the fourth boundary, taking the average value of the distance between the third boundary and the fourth boundary), the width of the molten pool (determined according to the first boundary and the second boundary, taking the average value of the distance between the first boundary and the second boundary), and the depth of the molten pool (the maximum value of the thickness of the molten pool); The determination of the adjustment strategy according to the second physical parameter includes: Determining the adjustment of the welding current and / or the welding speed according to the temperature of the molten pool and the preset temperature range; Determining the adjustment of the welding speed and / or the welding current according to the length of the molten pool and the preset length range; Determining the adjustment of the welding voltage and / or the arc length according to the width of the molten pool and the preset width range; Determining the adjustment of the welding current and / or the welding speed according to the depth of the molten pool and the preset depth range.

[0075] It can be understood that for the second physical parameter, that is, the temperature of the molten pool, the length of the molten pool, the width of the molten pool, and the depth of the molten pool, the temperature of the molten pool can be directly measured or indirectly measured by an infrared pyrometer, a thermal imager, a spectrometer, etc. For the geometric parameters of the molten pool, after using the infrared thermal imager to photograph the molten pool and determining the first boundary, the second boundary, the third boundary, and the fourth boundary, the length and width of the molten pool can be determined, or they can also be directly measured or indirectly measured by means such as the cooperation of a high-speed camera and a filter system, a coaxial vision system, and ultrasonic detection.

[0076] The temperature of the molten pool is a key parameter in the welding process, which directly affects the weld formation, the metallurgical reaction, and the welding quality. The temperature of the molten pool is approximately linearly and positively correlated with the welding current and inversely proportional to the welding speed. Therefore, the present invention monitors the temperature of the molten pool in real time during the welding process and adjusts the temperature of the molten pool in a timely manner by controlling the welding current and the welding speed.

[0077] Please refer to Figure 4, in one embodiment, determining the adjustment of the welding current and / or welding speed according to the molten pool temperature and a preset temperature range includes: If the molten pool temperature is greater than the upper limit value of the preset temperature range, the welding current is reduced by 5% - 10% each time based on the existing welding current and / or the welding speed is increased by 10 - 20 cm / min each time based on the existing welding speed until the molten pool temperature drops within the preset temperature range; If the molten pool temperature is less than the lower limit value of the preset temperature range, the welding current is increased by 5% - 10% each time based on the existing welding current and / or the welding speed is reduced by 10 - 20 cm / min each time based on the existing welding speed until the molten pool temperature rises within the preset temperature range.

[0078] As an implementation method, the preset temperature range is determined according to the average temperature of the molten pool during the welding process without welding defects such as cracks and pores in the historical automatic welding of air-conditioning pipelines. During the welding process of each copper pipe to be welded and stainless steel pipe to be welded, the second physical parameters of the molten pool, including the molten pool temperature, molten pool length, molten pool width, and molten pool depth, are detected, recorded, and saved in real time. After the first N automatic weldings are completed, the finished products are inspected. For the n qualified finished products (n ≤ N) (without welding defects such as cracks and pores), the average value of the molten pool temperatures during the welding processes of the n finished products is taken to form a temperature set. The maximum value in the temperature set is taken as the upper limit value of the preset temperature range, and the minimum value in the set is taken as the lower limit value of the preset temperature range. According to this preset temperature range, the (N + 1)-th automatic welding is performed. After the welding is completed, if the finished product is qualified (without welding defects such as cracks and pores), the average value of the molten pool temperature during this welding process is added to the above temperature set for updating, and then the preset temperature range is re-determined.

[0079] The molten pool extends beyond the weld groove range, resulting in an enlarged heat-affected zone, which may cause deformation or burn-through (for thin pipes). The molten pool fails to cover the welding path, resulting in incomplete fusion or discontinuous welds. The molten pool length is directly related to the welding speed. The faster the speed, the shorter the molten pool; conversely, the longer it is. Therefore, the present invention monitors the molten pool length during the welding process in real time and adjusts the molten pool length in a timely manner by controlling the welding speed.

[0080] Please refer to Figure 5 , in one embodiment, determining the adjustment of the welding speed and / or welding current according to the molten pool length and a preset length range includes: If the length of the molten pool is greater than the upper limit of the preset length range, the welding speed is increased by an increment of 5 - 10 cm / min each time on the basis of the existing welding speed until the length of the molten pool drops within the preset length range. During the process of increasing the welding speed, if the depth of the molten pool is less than the lower limit of the preset depth range, the welding current is increased by 5 - 10 A for every 10 cm / min increase in the welding speed until the depth of the molten pool rises within the preset depth range; If the length of the molten pool is less than the lower limit of the preset length range, the welding speed is decreased by an increment of 5 - 10 cm / min each time on the basis of the existing welding speed until the length of the molten pool rises within the preset length range. During the process of decreasing the welding speed, if the depth of the molten pool is greater than the upper limit of the preset depth range, the welding current is decreased by 5 - 10 A for every 10 cm / min decrease in the welding speed until the depth of the molten pool drops within the preset depth range.

[0081] As an implementation manner, the preset length range is determined according to the average length of the molten pool during the welding process without welding defects such as cracks and pores in the historical automatic welding of air-conditioning pipelines. During the welding process of each copper pipe to be welded and stainless steel pipe to be welded, the second physical parameters of the molten pool include: the molten pool temperature, molten pool length, molten pool width, and molten pool depth are all detected, recorded, and saved in real time. After the first N automatic weldings are completed, the finished products are inspected. For the n qualified finished products (n ≤ N) (without welding defects such as cracks and pores), the average value of the molten pool lengths during the welding of the n finished products is taken to form a length set. The maximum value in the length set is taken as the upper limit of the preset length range, and the minimum value in the set is taken as the lower limit of the preset length range. According to this preset length range, the (N + 1)-th automatic welding is carried out. After the welding is completed, if the finished product is qualified in quality inspection (without welding defects such as cracks and pores), the average value of the molten pool length during this welding process is added to the above length set for updating, and then the preset length range is re-determined.

[0082] If the width of the molten pool is too wide, it indicates that too much heat diffuses laterally, the weld surface is sunken, and the grains in the heat-affected zone are coarsened. If it is too narrow, there will be poor fusion, the weld formation is narrow and high, and it is easy to produce undercut or slag inclusion. The width of the molten pool is determined by the arc energy distribution and is directly affected by the welding voltage and arc length. Therefore, the present invention monitors the width of the molten pool during the welding process in real time and adjusts the width of the molten pool by controlling the welding voltage and arc length.

[0083] Please refer to Figure 6 , in an embodiment, the adjustment of the welding voltage and / or arc length according to the width of the molten pool and the preset width range includes: If the width of the molten pool is greater than the maximum value of the preset width range, the welding voltage is reduced in steps of 2 - 3V based on the existing welding voltage, and / or the arc length is shortened in steps of 0.1 - 0.2mm until the width of the molten pool drops within the preset width range; If the width of the molten pool is less than the minimum value of the preset width range, the welding voltage is increased in steps of 2 - 3V based on the existing welding voltage, and / or the arc length is extended in steps of 0.1 - 0.2mm until the width of the molten pool rises within the preset width range.

[0084] As an implementation manner, the preset width range is determined according to the diameter of the welding wire. The lower limit value of the preset width range is × the diameter of the welding wire, and the upper limit value of the preset width range is × the diameter of the welding wire.

[0085] In one embodiment, = 2, = 3.

[0086] The depth of the molten pool is an important index of welding quality, directly affecting the penetration, mechanical properties and defect control of the weld seam. The depth of the molten pool is approximately linearly and positively correlated with the current and inversely proportional to the welding speed. Therefore, the present invention monitors the depth of the molten pool in real time during the welding process and adjusts the width of the molten pool in time by controlling the welding current and the welding speed.

[0087] Please refer to Figure 7 , in one embodiment, determining the adjustment of the welding current and / or the welding speed according to the depth of the molten pool and the preset depth range includes: If the depth of the molten pool is greater than the maximum value of the preset depth range, the welding current is reduced in steps of 10 - 20A based on the existing welding current, and / or the welding speed is increased by 10% - 20% until the depth of the molten pool drops within the preset depth range; If the depth of the molten pool is less than the minimum value of the preset depth range, the welding current is increased in steps of 10 - 20A based on the existing welding current, and / or the welding speed is reduced by 10% - 20% until the depth of the molten pool rises within the preset depth range.

[0088] As an implementation manner, the preset depth interval is determined according to the average depth of the molten pool during the welding process without welding defects such as cracks and pores in the historical automatic welding process of the air-conditioning pipeline. During the welding process of the copper pipe to be welded and the stainless-steel pipe to be welded each time, the second physical parameters of the molten pool include: the molten pool temperature, the molten pool length, the molten pool width, and the molten pool depth, which are all detected, recorded, and saved in real time. After the automatic welding of the first N times is completed, the finished products are inspected. For the n qualified finished products (n ≤ N) (without welding defects such as cracks and pores), the average value of the molten pool depth during the welding process of the n finished products is taken to form a depth set. The maximum value in the depth set is taken as the upper limit value of the preset depth interval, and the minimum value in the set is taken as the lower limit value of the preset depth interval. According to this preset depth interval, the (N + 1)-th automatic welding is carried out. After the welding is completed, if the finished product passes the quality inspection (without welding defects such as cracks and pores), the average value of the molten pool depth during this welding process is added to the above depth set for updating, and then the preset depth interval is determined again.

[0089] Specifically, it further includes: adjusting the wire feeding speed according to the welding speed and the welding current during the self-adjustment stage.

[0090] In one embodiment, adjusting the wire feeding speed according to the welding speed and the welding current includes: adjusting the wire feeding speed according to the collaborative adjustment formula of the welding speed and the welding current. The formula is as follows:

[0091] Wherein, is the wire feeding speed, is the welding current, with the unit of A, is the wire melting coefficient, is the cross-sectional area of the weld, with the unit of , is the wire diameter, with the unit of mm, is the welding speed, with the unit of mm / s, is the material density, is the deposition efficiency. For steel wires, , , with the unit of g / min, .

[0092] As an implementation manner, the data parameters involved in the above wire feeding speed calculation formula of the present invention are all converted through data format conversion to eliminate the dimension difference. For example, the data with different dimensions are converted into data under the same dimension through standardization.

[0093] Specifically, it further includes: dynamically adjusting the current shielding gas flow according to the welding speed, the surface temperature of the molten pool, and the initial shielding gas flow during the self-adjustment stage.

[0094] In one embodiment, the dynamic adjustment of the current shielding gas flow rate according to the welding speed, the molten pool surface temperature, and the initial shielding gas flow rate includes: integrating the welding speed and the temperature effect, constructing a dynamic adjustment formula, and dynamically adjusting the shielding gas flow rate according to the dynamic adjustment formula. The dynamic adjustment formula is as follows:

[0095] Wherein, is the shielding gas flow rate, with the unit of L / min, Q is the initial shielding gas flow rate, with the unit of L / min, is the reference welding speed, with the range of 300 mm / min to 1000 mm / min, is the welding speed, with the unit of mm / min, is the molten pool surface temperature, with the unit of °C, is the standard temperature (taking 50% of the higher melting point of the welding material, i.e., 50% of the melting point of stainless steel), with the unit of °C, is the speed sensitivity coefficient, taking 0.5 to 1.5, is the temperature sensitivity coefficient, taking 0.2 to 0.5.

[0096] Specifically, the process of determining the arc-extinguishing welding parameters according to the welding parameters in the self-adjustment stage includes: Determining the arc-extinguishing current according to the welding current in the self-adjustment stage, the arc-extinguishing current is positively correlated with the welding current in the self-adjustment stage, determining the arc-extinguishing voltage according to the welding voltage in the self-adjustment stage, and the arc-extinguishing voltage is positively correlated with the welding voltage in the self-adjustment stage.

[0097] In one embodiment, the arc-extinguishing current = the average value of the welding current in the adjustment stage , and the arc-extinguishing voltage = the average value of the welding voltage in the adjustment stage .

[0098] As an implementation manner, the division methods of the arc-starting stage, the self-adjustment stage, and the arc-extinguishing stage are: the arc-starting stage is within the range of 0.1 s to 0.5 s after the start of welding, the arc-extinguishing stage is entered when the distance from the weld end is 2 mm to 5 mm, and the self-adjustment stage is between the arc-starting stage and the arc-extinguishing stage.

[0099] Please refer to Figure 8 . On the other hand, the present invention also provides an automatic welding system for air-conditioning pipelines, including: A data acquisition module, used to acquire the first physical parameters and the first environmental parameters of the copper pipe and the stainless steel pipe to be welded, and to acquire the second physical parameters of the molten pool in real time; An arc-starting welding parameter determination module, which is connected to the data acquisition module and is used to determine the arc-starting welding parameters according to the first physical parameters and the first environmental parameters; A self - adjustment strategy analysis module, which is connected to the data acquisition module, is used to determine the characteristics of the welding molten pool according to the second physical parameter, and judge whether it is necessary to adjust the welding parameters in real time based on the molten pool parameters corresponding to the welding molten pool characteristics; An arc - extinguishing welding parameter determination module, which is connected to the data acquisition module, is used to determine the arc - extinguishing welding parameters according to the welding parameters in the self - adjustment stage; An automatic welding device, which is respectively connected to the starting - arc welding parameter determination module, the self - adjustment strategy analysis module and the arc - extinguishing welding parameter determination module, is used to weld the copper pipe to be welded and the stainless - steel pipe to be welded according to the welding parameters in the starting - arc stage, the self - adjustment stage and the arc - extinguishing stage.

[0100] It should be understood that since the settings of the above - mentioned various modules are only for explaining the functional units of the system of the present disclosure, the physical devices corresponding to these modules can be the processor itself, or a part of the software in the processor, a part of the hardware, or a part of the combination of software and hardware. Therefore, the number of each module in the figure is only illustrative.

[0101] Various embodiments of the systems and techniques described above in this article can be implemented in digital electronic circuit systems, integrated circuit systems, field - programmable gate arrays (FPGAs), application - specific integrated circuits (ASICs), application - specific standard products (ASSPs), systems - on - a - chip (SOCs), complex programmable logic devices (CPLDs), computer hardware, firmware, software, and / or combinations thereof. These various embodiments can include: implemented in one or more computer programs, the one or more computer programs can be executed and / or interpreted on a programmable system including at least one programmable processor, the programmable processor can be a dedicated or general - purpose programmable processor, can receive data and instructions from a storage system, at least one input device, and at least one output device, and transmit the data and instructions to the storage system, the at least one input device, and the at least one output device.

[0102] To solve the above - mentioned technical problems, an embodiment of the present invention further provides an electronic device, including a memory, a processor, and a computer program stored on the memory and executable on the processor. When the processor executes the program, it implements the steps of a method for automatic welding of air - conditioning pipelines as described above.

[0103] Such as Figure 9As shown, the computer / electronic device includes a memory, a processor, and a network interface that are communicatively connected to each other via a system bus. It should be noted that only a computer device with components such as a memory, a processor, a network interface, and an operating system is shown in the figure. However, it should be understood that it is not required to implement all the shown components, and more or fewer components can be implemented alternatively. Among them, those skilled in the art of this technology can understand that the computer / electronic device here is a device that can automatically perform numerical calculations and / or information processing according to pre-set or stored instructions, and its hardware includes but is not limited to microprocessors, application specific integrated circuits (ASICs), field-programmable gate arrays (FPGAs), digital signal processors (DSPs), embedded devices, etc.

[0104] The computer / electronic device can be a computing device such as a desktop computer, a notebook, a palm computer, and a cloud server. The computer / electronic device can interact with the user through means such as a keyboard, a mouse, a remote control, a touchpad, or a voice control device.

[0105] There can be one or more memories, and at least one type of readable storage medium is included. The readable storage medium includes flash memory, hard disk, multimedia card, card-type memory (such as SD or DX memory, etc.), random access memory (RAM), static random access memory (SRAM), read-only memory (ROM), electrically erasable programmable read-only memory (EEPROM), programmable read-only memory (PROM), magnetic memory, magnetic disk, optical disc, etc. In some embodiments, the memory can be an internal storage unit of the computer device, such as the hard disk or memory of the computer device. In other embodiments, the memory can also be an external storage device of the computer device, such as a plug-in hard disk, a smart media card (SMC), a secure digital (SD) card, a flash card, etc., equipped on the computer device. Of course, the memory can also include both the internal storage unit and the external storage device of the computer device. In this embodiment, the memory is usually used to store the operating system and various application software installed on the computer device, such as the program code for an automatic welding method for air-conditioning pipelines. In addition, the memory can also be used to temporarily store various data that have been output or will be output.

[0106] The processor may be a central processing unit (CPU), a controller, a microcontroller, a microprocessor, or other data processing chips in some embodiments. The processor is generally used to control the overall operation of the computer device. In this embodiment, the processor is used to run the program code stored in the memory or process data, such as running a program code for an automatic welding method of air-conditioning pipelines.

[0107] The network interface may include a wireless network interface and / or a wired network interface, which is generally used to establish a communication connection between the computer device and other electronic devices.

[0108] The present invention also provides another implementation manner, that is, to provide a readable storage medium, on which a computer program is stored, and when the computer program is executed by a processor, the steps of an automatic welding method for air-conditioning pipelines as described above are implemented.

[0109] So far, the technical solutions of the present invention have been described in conjunction with the preferred embodiments shown in the drawings. However, it is easy for those skilled in the art to understand that the protection scope of the present invention is obviously not limited to these specific embodiments. Without departing from the principle of the present invention, those skilled in the art can make equivalent changes or substitutions to the relevant technical features, and the technical solutions after these changes or substitutions will fall within the protection scope of the present invention.

[0110] The above are only the preferred embodiments of the present invention and are not used to limit the present invention; for those skilled in the art, the present invention can have various changes and modifications. Any modification, equivalent substitution, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A method for automatic welding of air conditioning pipelines, characterized in that: include: Obtaining first physical parameters and first environmental parameters of the copper pipe to be welded and the stainless steel pipe to be welded, wherein the first physical parameters include the thickness of the stainless steel pipe at the welding point, the thickness of the copper pipe at the welding point, and the diameter of the welding wire, and the first environmental parameters include air humidity, air temperature, and acid gas concentration in the air; Determine arc starting welding parameters according to the first physical parameter and the first environmental parameter, and perform arc starting stage welding according to the arc starting welding parameters; After the arc starting stage welding is completed, the self-adjustment stage welding is carried out. Acquire a second physical parameter of the molten pool in real time, wherein the second physical parameter includes a surface temperature at each position of the molten pool; Determine the welding molten pool characteristics according to the second physical parameter, and determine whether to adjust the welding parameters in real time based on the molten pool parameters corresponding to the welding molten pool characteristics, and perform self-adjustment stage welding according to the welding parameters adjusted in real time, wherein the welding molten pool characteristics include a first molten pool boundary close to the copper tube side and a second molten pool boundary close to the stainless steel tube side, and the molten pool parameters include a molten pool surface area and a molten pool surface temperature; When the self-adjustment stage welding is completed, the arc closure stage welding begins. The arc closure welding parameters are determined according to the welding parameters of the self-adjustment stage, and the arc closure stage welding is performed according to the arc closure welding parameters.

2. The automatic welding method for air conditioning pipelines according to claim 1, characterized in that: The process of determining arc welding parameters according to the first physical parameter and the first environmental parameter comprises: Determine the arc starting voltage according to the thickness of the stainless steel pipe welding part and the thickness of the copper pipe welding part, determine the arc starting current according to the welding wire diameter, determine the arc starting length according to the arc starting voltage and arc starting current, and determine the initial wire feeding speed according to the arc starting current; Determine the nozzle diameter of the protective gas according to the arc starting current, arc starting voltage and arc starting length; The initial protective gas flow rate is determined according to air humidity, air temperature, acid gas concentration in the air and the nozzle diameter.

3. The automatic welding method for air conditioning pipelines according to claim 2 is characterized in that: The process of determining the arc starting voltage according to the thickness of the stainless steel pipe welding part and the thickness of the copper pipe welding part comprises: Determine the average thickness of the weld according to the thickness of the stainless steel pipe weld and the thickness of the copper pipe weld; determining a welding proportional coefficient according to the average thickness; The arc starting voltage is determined according to the welding proportional coefficient and the basic voltage.

4. The automatic welding method for air conditioning pipelines according to claim 2 is characterized in that: The process of determining the arc starting current according to the welding wire diameter includes: determining the distribution coefficient according to the thickness of the stainless steel pipe welding point and the thickness of the copper pipe welding point, and determining the arc starting current according to the current coefficient per unit thickness, the distribution coefficient and the welding wire diameter.

5. The automatic welding method for air conditioning pipelines according to claim 2 is characterized in that: The process of determining the initial protective gas flow rate according to air humidity, air temperature, and acid gas concentration in the air includes: The basic flow rate of the shielding gas is determined according to the welding speed and the nozzle diameter. The humidity correction value, temperature correction value and acid gas correction value are determined according to the air humidity, air temperature and the acid gas concentration in the air respectively. The initial shielding gas flow rate is determined according to the basic flow rate, humidity correction value, temperature correction value and acid gas correction value.

6. The automatic welding method for air conditioning pipelines according to claim 1, characterized in that: The process of determining the weld pool characteristics of the weld pool includes: Respectively identify the isotherms on the copper tube side and the isotherms on the stainless steel tube side corresponding to the molten pool, use the isotherms corresponding to the first temperature on the copper tube side as the first boundary of the molten pool, use the isotherms corresponding to the second temperature on the stainless steel tube side as the second boundary of the molten pool, and determine the surface area of ​​the molten pool according to the first boundary of the molten pool and the second boundary of the molten pool; A plurality of monitoring points are evenly arranged between the center of the molten pool and the first boundary and the second boundary of the molten pool, and the temperatures of the plurality of monitoring points are obtained, and the surface temperature of the molten pool is determined according to the temperatures of the plurality of monitoring points.

7. The automatic welding method for air conditioning pipelines according to claim 6, characterized in that: The process of judging whether to adjust the welding parameters in real time based on the molten pool parameters corresponding to the welding molten pool characteristics includes: Determining whether to adjust the welding current and / or welding speed according to the comparison result between the surface temperature of the molten pool and the preset temperature range; Whether to adjust the welding voltage and / or arc length is determined based on the comparison result between the surface area of ​​the molten pool and the preset area interval.

8. The automatic welding method for air conditioning pipelines according to claim 2, characterized in that: Also includes: In the self-adjustment stage, the wire feeding speed is adjusted according to the welding speed and the welding current, and the current shielding gas flow rate is dynamically adjusted according to the welding speed, the surface temperature of the molten pool and the initial shielding gas flow rate.

9. The automatic welding method for air conditioning pipelines according to claim 1, characterized in that: The process of determining arc-ending welding parameters according to the welding parameters in the self-adjustment stage includes: The arc ending current is determined according to the welding current in the self-adjusting stage, and the arc ending current is positively correlated with the welding current in the self-adjusting stage. The arc ending voltage is determined according to the welding voltage in the self-adjusting stage, and the arc ending voltage is positively correlated with the welding voltage in the self-adjusting stage.

10. An automatic welding system for air conditioning pipelines, characterized in that: include: A data acquisition module, used to acquire a first physical parameter and a first environmental parameter of the copper pipe and the stainless steel pipe to be welded, and to acquire a second physical parameter of the molten pool in real time; An arc-starting welding parameter determination module, connected to the data acquisition module, for determining arc-starting welding parameters according to the first physical parameter and the first environmental parameter; a self-adjustment strategy analysis module, which is connected to the data acquisition module and is used to determine the characteristics of the welding pool according to the second physical parameter, and determine whether to adjust the welding parameters in real time based on the molten pool parameters corresponding to the characteristics of the welding pool; A module for determining arc-ending welding parameters, which is connected to the data acquisition module and is used to determine arc-ending welding parameters according to the welding parameters in the self-adjustment stage; The automatic welding equipment is respectively connected to the arc starting welding parameter determination module, the self-adjustment strategy analysis module and the arc ending welding parameter determination module, and is used to weld the copper pipe to be welded and the stainless steel pipe to be welded according to the welding parameters in the arc starting stage, the self-adjustment stage and the arc ending stage.

Citation Information

Patent Citations

  • Stainless steel air conditioner pipeline

    CN114110284A

  • Welding parameter self-adaptive adjusting method based on molten pool state analysis

    CN116258649A

  • Method and system for adjusting wire feeding speed of wire feeder

    CN119368874A

  • Arc welding adaptive process control system

    US4613743A

  • Duplex stainless steel welded joint and method for manufacturing same

    WO2020203931A1

Cited By

  • Hand-held laser welding head power control method and system based on molten pool temperature

    CN121209652A