An optical chip structure and its fabrication method
By designing high and low resistance regions and ridge waveguide structures in the optical chip structure, the problems of time-varying bias point and reduced transmittance of electro-optic modulators are solved, achieving efficient transmission and low loss of optical signals.
Patent Information
- Application Number
- CN202510463936.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2025-04-14
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2045-04-14
AI Technical Summary
Existing electro-optic modulators suffer from time-varying bias points due to the photorefractive effect and photovoltaic effect of lithium niobate or lithium tantalate crystals, while the transmittance and light loss issues are difficult to balance.
Design an optical chip structure including a supporting substrate, an isolation layer, and a photoelectric thin film layer. The photoelectric thin film layer is divided into a first region with high resistance and a second region with low resistance. A ridge waveguide structure is formed on the thin film layer. The resistivity and oxygen content are adjusted by patterning process to optimize charge conduction and light propagation.
This effectively prevents the bias point of the electro-optic modulator from changing over time, maintains the transmittance of the thin film, reduces the loss of the optical signal, and improves the transmission efficiency and stability of the optical signal.
Smart Images

Figure CN120386109B_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of semiconductor technology, and in particular to an optical chip structure and its fabrication method. Background Technology
[0002] Electro-optic modulators are modulators primarily based on the electro-optic effect of electro-optic materials. When a voltage is applied to an electro-optic material such as lithium niobate crystal or lithium tantalate crystal, the refractive index of the electro-optic material changes, thereby altering the characteristics of the light wave passing through the material. Utilizing the electro-optic effect, it is possible to modulate parameters such as the phase, amplitude, intensity, and polarization state of an optical signal.
[0003] When incident light irradiates a thin film made of electro-optic materials such as lithium niobate crystal or lithium tantalate crystal, charges are generated on the surface of the film due to the photorefractive effect or photovoltaic effect of these materials. The high resistance of these electro-optic materials makes charge conduction difficult, and the non-uniform distribution of these charges within and at the interfaces of the single-crystal film creates a non-uniform electric field. This results in inconsistent refractive index changes in different regions of the film, causing changes in the phase and intensity of the light signal as it passes through the film. Consequently, the bias point of the electro-optic modulator changes over time. To address this issue, existing technologies employ reduction reactions on the thin films made of electro-optic materials such as lithium niobate crystal or lithium tantalate crystal to reduce the oxygen content in the crystal and thus lower the resistivity of the film. However, this reduces the transmittance of the film, increasing the light loss of the crystal and limiting its applications. Summary of the Invention
[0004] To address the aforementioned problems in the prior art, this application provides an optical chip structure that avoids the time-varying bias point of the electro-optic modulator caused by the photorefractive effect or photovoltaic effect of electro-optic materials such as lithium niobate crystals or lithium tantalate crystals. Simultaneously, it ensures the transmittance of the thin film and reduces the optical loss of the optical chip structure. The specific technical solution is as follows:
[0005] On one hand, this application provides an optical chip structure, including:
[0006] Support substrate;
[0007] A first isolation layer located on one side surface of the supporting substrate;
[0008] A photoelectric thin film layer is located on the surface of the first isolation layer away from the supporting substrate. The photoelectric thin film layer is provided with at least one first region and a second region. The first region is formed with a ridge waveguide structure, and the resistance of the first region is higher than that of the second region.
[0009] In a possible implementation, the ridge waveguide structure includes a substrate region and a ridge waveguide region, the ridge waveguide region protruding from one side surface of the substrate region, and the substrate region and the ridge waveguide region satisfy at least one of the following characteristics:
[0010] The ridge waveguide region protrudes from one side surface of the substrate region at a height ranging from 50 to 600 nm.
[0011] The width of the ridge waveguide region ranges from 0.5 to 5 μm;
[0012] The thickness of the substrate region ranges from 50 to 600 nm.
[0013] In a possible implementation, the first region and the second region satisfy at least one of the following characteristics:
[0014] The area of the first region accounts for 1%-20% of the total area of the photoelectric thin film layer;
[0015] The area of the second region accounts for 80%-99% of the total area of the photoelectric thin film layer;
[0016] The resistivity range of the first region is 3×10⁻⁶. 10 ~3×10 18 Ω·cm;
[0017] The resistivity range of the second region is 1×10⁻⁶. 9 ~3×10 11 Ω·cm;
[0018] The oxygen content in the first region is higher than that in the second region.
[0019] In a possible implementation, the optical chip structure may further include a second isolation layer located on the side of the supporting substrate away from the first isolation layer.
[0020] In a possible implementation, the first isolation layer and the second isolation layer satisfy at least one of the following characteristics:
[0021] The first isolation layer and the second isolation layer have the same thickness;
[0022] The first isolation layer is made of the same material as the second isolation layer.
[0023] In a possible implementation, the optical chip structure may further include a first defect layer located between the first isolation layer and the supporting substrate.
[0024] In a possible implementation, the optical chip structure may further include a second defect layer located on the surface of the supporting substrate away from the first defect layer.
[0025] In a possible implementation, the structure satisfies at least one of the following characteristics:
[0026] The thickness of the first defect layer ranges from 300 to 10000 μm;
[0027] The material of the first defect layer includes at least one of polycrystalline silicon, ion-implanted polycrystalline silicon, amorphous silicon, and monocrystalline silicon;
[0028] The first defect layer and the second defect layer have the same thickness;
[0029] The first defect layer and the second defect layer are made of the same material.
[0030] In a possible implementation, the structure satisfies at least one of the following characteristics:
[0031] The thickness of the first isolation layer ranges from 1 to 50 μm;
[0032] The thickness of the second region ranges from 50 to 600 nm;
[0033] The thickness of the supporting substrate ranges from 300 to 1000 μm;
[0034] The curvature of the supporting substrate ranges from -30 to 30 μm.
[0035] In a possible implementation, the structure satisfies at least one of the following characteristics:
[0036] The material of the first insulating layer includes at least one of silicon dioxide, silicon nitride, and aluminum oxide;
[0037] The material of the photoelectric thin film layer includes at least one of lithium niobate, lithium tantalate, and barium titanate.
[0038] The supporting substrate includes at least one of silicon, silicon carbide, sapphire, and quartz.
[0039] In a possible implementation, the structure may further include an electrode structure located on the side surface of the second region away from the first insulating layer.
[0040] On the other hand, this application provides a method for fabricating an optical chip structure, the method comprising:
[0041] Provide a supporting substrate;
[0042] A first isolation layer is formed on one side surface of the supporting substrate;
[0043] A photoelectric thin film layer is formed on the surface of the first isolation layer away from the supporting substrate using a patterning process;
[0044] The optoelectronic thin film layer is provided with at least one first region and a second region, the first region is formed with a ridge waveguide structure, and the resistance of the first region is higher than that of the second region.
[0045] In a possible implementation, forming a photoelectric thin film layer on the surface of the first isolation layer away from the supporting substrate using a patterning process includes:
[0046] A preset photoelectric thin film layer is formed on the surface of the first isolation layer away from the supporting substrate. The preset photoelectric thin film layer includes at least one first initial region and a second initial region. The resistance of the first initial region is higher than that of the second initial region.
[0047] The preset photoelectric thin film layer is patterned and etched to form a ridge waveguide structure in the first initial region to obtain the first region, and the second initial region is thinned to obtain the second region.
[0048] In a possible implementation, a predetermined photoelectric thin film layer is formed on the surface of the first isolation layer away from the supporting substrate, comprising:
[0049] An initial photoelectric thin film layer is formed on the surface of the first isolation layer on the side away from the supporting substrate;
[0050] A patterned blocking layer is formed on the initial photoelectric thin film layer, and the blocking layer blocks the thin film layer region corresponding to the first region in the initial photoelectric thin film layer.
[0051] The initial photoelectric thin film layer with the patterned blocking layer is restored to restore the thin film layer area exposed by the blocking layer, and the blocking layer is removed to form the preset photoelectric thin film layer.
[0052] In a possible implementation, before forming a photoelectric thin film layer on the surface of the first isolation layer away from the supporting substrate using a patterning process, the fabrication method further includes forming a second isolation layer on the supporting substrate away from the first isolation layer.
[0053] In a possible implementation, before forming a photoelectric thin film layer on the surface of the first isolation layer away from the supporting substrate based on a patterning process, the fabrication method further includes forming a first defect layer between the first isolation layer and the supporting substrate.
[0054] In a possible implementation, before forming a photoelectric thin film layer on the surface of the first isolation layer away from the supporting substrate based on a patterning process, the method further includes forming a second defect layer on the surface of the supporting substrate away from the first defect layer.
[0055] Based on the above technical solution, this application has the following beneficial effects: The technical solution of the present invention provides an optical chip structure, which includes a supporting substrate, a first isolation layer located on one side surface of the supporting substrate, and a photoelectric thin film layer located on the side surface of the first isolation layer away from the supporting substrate. The photoelectric thin film layer is provided with at least one first region and a second region. The first region forms a ridge waveguide structure. The resistance of the first region is higher than that of the second region. By providing at least one first region and a second region on the photoelectric thin film layer, wherein the resistance of the first region is higher than that of the second region, the low resistance of the second region can timely conduct the charge generated by the photorefractive effect or photovoltaic effect of the photoelectric thin film layer, avoiding the problem of the bias point of the electro-optic modulator changing with time due to the non-uniform electric field generated in the single crystal thin film and at the single crystal thin film interface. At the same time, the high resistance of the first region ensures the transmittance of the thin film layer, thereby reducing the loss of the optical signal of the structure. Furthermore, the ridge waveguide structure formed in the first region can not only effectively guide and limit the propagation of the optical signal, but also further reduce the loss of the optical signal. Attached Figure Description
[0056] To more clearly illustrate the technical solutions of this application, the accompanying drawings used in the description of the embodiments or prior art will be briefly introduced below. Obviously, the drawings described below are merely some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without any creative effort.
[0057] Figure 1 This is a schematic diagram of the optical chip structure in a specific embodiment of the present invention.
[0058] Figure 2 This is a schematic diagram of the optical chip structure in a specific embodiment of the present invention.
[0059] Figure 3 This is a schematic diagram of the optical chip structure in a specific embodiment of the present invention.
[0060] Figure 4 This is a schematic diagram of the optical chip structure in a specific embodiment of the present invention.
[0061] Figure 5 This is a schematic diagram of the optical chip structure in a specific embodiment of the present invention.
[0062] Figure 6 This is a schematic diagram of the optical chip structure in a specific embodiment of the present invention.
[0063] Figure 7 This is a schematic diagram of the optical chip structure in a specific embodiment of the present invention.
[0064] Figure 8 This is a top view of an optical chip structure without electrodes in a specific embodiment of the present invention.
[0065] Figure 9 This is a top view of the optical chip structure after adding an electrode mechanism in a specific embodiment of the present invention.
[0066] Figure 10 This is a schematic diagram of the fabrication process of the optical chip structure fabrication method of the present invention.
[0067] In the figure: 101-Supporting substrate, 102-First isolation layer, 103-Photoelectric thin film layer, 1031-First region, 1032-Second region, 1033-Base region, 1034-Ridge waveguide region, 104-Second isolation layer, 105-First defect layer, 106-Second defect layer, 107-Electrode structure, 108-Initial photoelectric thin film layer, 109-Blocking layer, 110-Initial photoresist layer, 111-Patterned initial photoresist layer, 112-Patterned blocking layer, 113-Preset photoelectric thin film layer, 1131-First initial region, 1132-Second initial region, 114-Photoresist layer, 115-Patterned photoresist layer. Detailed Implementation
[0068] The technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments. Based on the embodiments of this application, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of this application.
[0069] For the terms defined below, unless a different definition is given elsewhere in the claims or this specification, these definitions shall apply. All numerical values, whether explicitly indicated or not, are defined herein as being modified by the term "about." The term "about" generally refers to a range of numerical values that a person skilled in the art would consider equivalent to the stated values to produce substantially the same properties, functions, results, etc. A range of numerical values indicated by a low value and a high value is defined as including all numerical values included within that range and all subranges included within that range.
[0070] It should be noted that the terms "first," "second," etc., in the specification, claims, and accompanying drawings of this application are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that such data can be interchanged where appropriate so that the embodiments of this application described herein can be implemented in orders other than those illustrated or described herein. Furthermore, the terms "comprising" and "having," and any variations thereof, are intended to cover non-exclusive inclusion.
[0071] On the one hand, the following describes an optical chip structure provided by an embodiment of this application, such as... Figure 1 As shown, it includes:
[0072] Support substrate 101;
[0073] In some embodiments, the support substrate 101 includes at least one of silicon, silicon carbide, sapphire, and quartz. Silicon, sapphire, and quartz all have high optical transmittance, which can ensure the effective transmission of optical signals and reduce light loss, while silicon carbide has a large high breakdown electric field strength, which can operate under high voltage conditions without electrical breakdown and can be used in high voltage devices.
[0074] Specifically, the quartz is either fused quartz or single-crystal quartz.
[0075] In some embodiments, the thickness of the support substrate 101 ranges from 300 to 1000 μm. The thickness of the support substrate 101 can be any value within the above range, and will not be enumerated here. A larger thickness of the support substrate 101 will lead to increased light loss during propagation and may also increase the manufacturing cost, while a smaller thickness of the support substrate 101 will reduce the mechanical strength of the chip.
[0076] In some embodiments, the curvature of the support substrate 101 ranges from -30 to 30 μm. The curvature of the support substrate 101 can be any value within the above range, and will not be enumerated here. By limiting the range of curvature, the manufacturability of the chip structure is ensured, and the increased integration and manufacturing difficulty caused by excessively small curvature of the support substrate 101 is avoided.
[0077] like Figure 1 As shown, the optical chip structure of this application also includes a first isolation layer 102 located on one side surface of the support substrate 101. Adding the first isolation layer 102 to one side surface of the support substrate 101 can prevent mutual interference between the support substrate 101 and the photoelectric thin film layer 103, thereby improving the stability of the electro-optic modulator.
[0078] In some embodiments, the material of the first isolation layer 102 includes at least one of silicon dioxide, silicon nitride, and aluminum oxide; all of the above materials have good insulation and low dielectric constant, which can effectively prevent mutual interference between different layers and reduce the loss of optical signals.
[0079] In some embodiments, the thickness of the first isolation layer 102 ranges from 1 to 50 μm. The thickness of the first isolation layer 102 can be any value within the above range, and will not be enumerated here. By limiting the thickness range of the first isolation layer 102, it is possible to avoid the increase in light propagation loss due to excessive isolation layer thickness, and the difficulty in ensuring isolation effect if the isolation layer thickness is too small. In addition, the isolation layer within the above thickness range can also reduce the microwave loss of the chip structure.
[0080] In some embodiments, such as Figure 3 As shown, the optical chip structure also includes a second isolation layer 104 located on the side of the support substrate 101 away from the first isolation layer 102. By adding the second isolation layer 104, the transmission and loss of optical signals can be further reduced, and the stability of the device can be improved.
[0081] In some embodiments, the first isolation layer 102 and the second isolation layer 104 have the same thickness. Having two isolation layers of the same thickness allows for better stress balance between the supporting substrate 101 and the photoelectric thin film layer 103, resulting in a more uniform stress distribution and improved fabrication yield of the optical chip structure.
[0082] Specifically, the thickness of the second isolation layer 104 ranges from 1 to 50 μm. The thickness of the second isolation layer 104 can be any value within the above range, and will not be enumerated here.
[0083] In some embodiments, the first isolation layer 102 and the second isolation layer 104 are made of the same material. Using the same material ensures that the two isolation layers have the same coefficient of thermal expansion. At different operating temperatures, the same coefficient of thermal expansion can avoid internal stress in the chip structure caused by temperature changes, thus ensuring the performance and stability of the device.
[0084] Specifically, the material of the second insulating layer 104 includes at least one of silicon dioxide, silicon nitride, and aluminum oxide.
[0085] In some embodiments, such as Figure 5 As shown, the optical chip structure also includes a first defect layer 105 located between the first isolation layer 102 and the support substrate 101. The support substrate 101 may generate electrons under the illumination of incident light, and the first defect layer 105 can absorb the electrons generated by the support substrate 101 to reduce the microwave loss of the device.
[0086] In some embodiments, the thickness of the first defect layer 105 ranges from 300 to 10000 μm. The thickness of the first defect layer 105 can be any value within the above range, and will not be enumerated here. The thickness of the first defect layer 105 affects the modulation efficiency, extinction ratio, and bandwidth of the electro-optic modulator. By limiting the above thickness range, the modulation efficiency, extinction ratio, and bandwidth of the electro-optic modulator are guaranteed.
[0087] In some embodiments, the material of the first defect layer 105 includes at least one of polycrystalline silicon, ion-implanted polycrystalline silicon, amorphous silicon, and monocrystalline silicon.
[0088] In some embodiments, such as Figure 6 As shown, the optical chip structure also includes a second defect layer 106 located on the surface of the support substrate 101 away from the first defect layer 105. By adding the second defect layer 106, the microwave loss of the device is further reduced.
[0089] In some embodiments, the first defect layer 105 and the second defect layer 106 have the same thickness.
[0090] Specifically, the thickness of the second defect layer 106 is 300–10000 μm. The thickness of the second defect layer 106 can be any value within the above range, and will not be enumerated here.
[0091] In some embodiments, the first defect layer 105 and the second defect layer 106 are made of the same material.
[0092] Specifically, the material of the second defect layer 106 includes at least one of polycrystalline silicon, ion-implanted polycrystalline silicon, amorphous silicon, and monocrystalline silicon. By defining the first defect layer 105 and the second defect layer 106 as having the same material and thickness, a more uniform electric field distribution can be provided, which helps to improve the efficiency of the electro-optic modulator and also provides a smoother light transmission path, thereby reducing insertion loss.
[0093] like Figure 1-2 As shown, the optical chip structure of this application includes a photoelectric thin film layer 103 located on the side of the first isolation layer 102 away from the support substrate 101. The photoelectric thin film layer 103 is provided with at least one first region 1031 and a second region 1032. The first region 1031 is formed with a ridge waveguide structure, and the resistance of the first region 1031 is higher than the resistance of the second region 1032.
[0094] In some embodiments, the photoelectric thin film layer 103 is made of at least one of lithium niobate, lithium tantalate, and barium titanate. These materials exhibit excellent photoelectric effects and are suitable for fabricating electro-optic modulators.
[0095] In some embodiments, the area of the first region 1031 accounts for 1%-20% of the total area of the photoelectric thin film layer 103. This arrangement ensures that the chip structure has good light transmittance and avoids the problem that a small area of the first region 1031 may lead to reduced light transmittance of the chip structure and increased light loss of the crystal.
[0096] In some embodiments, the resistivity of the first region 1031 is in the range of 3 × 10⁻⁶. 10 ~3×10 18 Ω·cm. By limiting the resistivity of the first region 1031, the energy loss of the optical signal during transmission can be effectively reduced, thereby improving the transmission efficiency of the optical signal.
[0097] In some embodiments, the area of the second region 1032 accounts for 80%-99% of the total area of the optoelectronic thin film layer 103. This arrangement ensures that the chip structure can conduct the charge generated by the photorefractive effect or photovoltaic effect of the optoelectronic thin film layer 103 in a timely manner, avoiding the problem of the bias point of the electro-optic modulator changing over time due to the non-uniform electric field generated in and at the single crystal thin film interface.
[0098] In some embodiments, the resistivity of the second region 1032 is in the range of 1×10⁻⁶. 9 ~3×10 11 Ω·cm. By setting an appropriate resistivity, it is possible to avoid excessive resistivity, which would make it difficult for the chip structure to conduct the charge generated on the optoelectronic thin film layer 103, resulting in a non-uniform electric field within and at the interface of the single crystal thin film, and consequently causing the bias point of the electro-optic modulator to change over time.
[0099] In some embodiments, the thickness of the second region 1032 ranges from 50 to 600 nm. The thickness of the second region 1032 can be any value within the above range, and will not be enumerated here. When the thickness of the second region 1032 is smaller, its resistivity will increase accordingly, but its transmittance will also increase. In order to ensure that the second region 1032 has a low resistance while ensuring a certain transmittance, the above thickness range is limited.
[0100] In some embodiments, the oxygen content in the first region 1031 is higher than the oxygen content in the second region 1032. The higher the oxygen content in the photoelectric thin film layer 103, the higher its resistivity and transmittance. Therefore, the oxygen content in the first region 1031 is set to be higher than the oxygen content in the second region 1032.
[0101] In some embodiments, such as Figure 2As shown, the ridge waveguide structure includes a substrate region 1033 and a ridge waveguide region 1034. The ridge waveguide region 1034 protrudes from one side surface of the substrate region 1033, and the protrusion height of the ridge waveguide region 1034 protruding from the side surface of the substrate region 1033 ranges from 50 to 600 nm. The protrusion height of the ridge waveguide region 1034 can be any value within the above range, and is not enumerated here. The waveguide structure is used to guide and define the region of light propagation. By defining the above-mentioned protrusion height, the propagation path of the optical signal is optimized, the propagation loss of light is reduced, and the coupling efficiency of light is improved.
[0102] In some embodiments, the width of the ridge waveguide region 1034 ranges from 0.5 to 5 μm. The width of the ridge waveguide region 1034 can be any value within this range, and will not be enumerated here. By limiting the width as described above, the problem of increased optical loss due to an excessively narrow waveguide region is avoided, while the problem of reduced modulation efficiency of the electro-optic modulator due to an excessively wide waveguide region is also avoided.
[0103] In some embodiments, the thickness of the substrate region 1033 ranges from 50 to 600 nm. The thickness of the substrate region 1033 can be any value within the above range, and will not be enumerated here. By limiting the thickness range of the substrate region 1033, the transmittance of the first region 1031 can be improved, while the light loss of the first region 1031 can be reduced.
[0104] For example, Figure 8 This is a top view of the optical chip structure of an embodiment of this application, as shown below. Figure 8 As shown, the first region 1031 and the second region 1032 of the photoelectric thin film layer 103 are adjacent to each other, and the first region 1031 and the second region 1032 are arranged alternately.
[0105] In some embodiments, such as Figure 4 and Figure 7 As shown, the structure also includes an electrode structure 107 located on the side surface of the second region 1032 away from the first isolation layer 102. Forming the electrode structure 107 in the second region 1032 not only enables the detection and processing of optical signals, but also effectively controls the propagation and modulation of optical signals, improving the performance and efficiency of the modulator.
[0106] For example, Figure 9 This is a top view of the optical chip structure of an embodiment of this application, as shown below. Figure 9 As shown, an electrode structure 107 is provided on each of the second regions 1032 of the photoelectric thin film layer 103, and the electrode structures 107 are arranged at intervals.
[0107] On the other hand, the following describes a method for fabricating an optical chip structure according to an embodiment of this application. This method is used to fabricate the optical chip structure as described in the above embodiments, and the method includes:
[0108] S1: Provides a support substrate 101;
[0109] In some embodiments, the support substrate 101 includes at least one of silicon, silicon carbide, sapphire, and quartz. Silicon, sapphire, and quartz all have high optical transmittance, which can ensure the effective transmission of optical signals and reduce light loss, while silicon carbide has a large high breakdown electric field strength, which can operate under high voltage conditions without electrical breakdown and can be used in high voltage devices.
[0110] Specifically, the quartz is either fused quartz or single-crystal quartz.
[0111] In some embodiments, the thickness of the support substrate 101 ranges from 300 to 1000 μm. The thickness of the support substrate 101 can be any value within this range, and will not be enumerated here. This arrangement ensures the mechanical strength of the chip structure while avoiding the problem of increased light loss during propagation caused by a larger thickness of the support substrate 101.
[0112] In some embodiments, the curvature of the support substrate 101 ranges from -30 to 30 μm. The curvature of the support substrate 101 can be any value within this range, and will not be enumerated here. By limiting the curvature range of the support substrate 101, the manufacturability of the chip structure is ensured.
[0113] S2: A first isolation layer 102 is formed on one side surface of the support substrate 101; by adding the isolation layer, the interaction between the support substrate 101 and the photoelectric thin film layer 103 is avoided.
[0114] Specifically, a first isolation layer 102 is formed on one side surface of the support substrate 101 using physical vapor deposition or chemical vapor deposition.
[0115] In some embodiments, the material of the first insulating layer 102 includes at least one of silicon dioxide, silicon nitride, and aluminum oxide. These materials have good insulation and low dielectric constant, effectively preventing mutual interference between different layers while reducing optical signal loss.
[0116] In some embodiments, the thickness of the first isolation layer 102 ranges from 1 to 50 μm. The thickness of the first isolation layer 102 can be any value within this range, and will not be enumerated here. By setting the thickness within the above range, not only can the microwave loss of the chip structure be reduced, but also the interaction between different layers can be avoided.
[0117] In some embodiments, before forming the photoelectric thin film layer 103 on the surface of the first isolation layer 102 away from the support substrate 101 using a patterning process, the fabrication method further includes forming a second isolation layer 104 on the side of the support substrate 101 away from the first isolation layer 102. By forming the second isolation layer 104, the transmission and loss of optical signals can be further reduced.
[0118] Specifically, the second isolation layer 104 can be formed on the side of the substrate away from the first isolation layer 102 by physical vapor deposition or chemical vapor deposition.
[0119] In some embodiments, the first isolation layer 102 and the second isolation layer 104 have the same thickness.
[0120] In some embodiments, the first isolation layer 102 and the second isolation layer 104 are made of the same material. Using the same material and thickness for both the first isolation layer 102 and the second isolation layer 104 ensures the performance and stability of the chip structure.
[0121] Specifically, the material of the second insulating layer 104 includes at least one of silicon dioxide, silicon nitride, and aluminum oxide.
[0122] Specifically, the thickness of the second isolation layer 104 ranges from 1 to 50 μm. The thickness of the second isolation layer 104 can be any value within the above range, and will not be enumerated here.
[0123] In some embodiments, such as Figure 10 As shown, before forming the photoelectric thin film layer 103 on the surface of the first isolation layer 102 away from the supporting substrate 101 using a patterning process, the fabrication method further includes forming a first defect layer 105 between the first isolation layer 102 and the supporting substrate 101. The structure obtained in this embodiment is as follows: Figure 10 In the optical chip structure a, the supporting substrate 101 may generate electrons under the irradiation of incident light, and the first defect layer 105 can absorb the electrons generated by the supporting substrate 101 to reduce the microwave loss of the device.
[0124] Specifically, a first defect layer 105 is formed between the first isolation layer 102 and the support substrate 101 by means of vapor deposition or ion implantation. This application does not specify the formation method of the first defect layer 105, but only requires that the first defect layer 105 be formed between the first isolation layer 102 and the support substrate 101.
[0125] Specifically, vapor deposition can include physical vapor deposition or chemical vapor deposition.
[0126] In some embodiments, the thickness of the first defect layer 105 ranges from 300 to 10000 μm. The thickness of the first defect layer 105 can be any value within the above range, and will not be enumerated here. The thickness of the defect layer affects the propagation path and speed of light, thereby affecting the propagation efficiency of light and the transmission quality of signals. Furthermore, an excessively thick defect layer may increase light scattering, leading to attenuation and distortion of the optical signal.
[0127] In some embodiments, the material of the first defect layer 105 includes at least one of polycrystalline silicon, ion-implanted polycrystalline silicon, amorphous silicon, and monocrystalline silicon.
[0128] In some embodiments, before forming the photoelectric thin film layer 103 on the surface of the first isolation layer 102 away from the support substrate 101 using a patterning process, the method further includes forming a second defect layer 106 on the surface of the support substrate 101 away from the first defect layer 105. By adding the second defect layer 106, the microwave loss of the device is further reduced.
[0129] Specifically, a second defect layer 106 is formed on the surface of the support substrate 101 away from the first defect layer 105 by means of vapor deposition or ion implantation. This application does not specify the formation method of the second defect layer 106, it is only necessary to form the second defect layer 106 on the surface of the support substrate 101 away from the first defect layer 105.
[0130] Specifically, vapor deposition can be physical vapor deposition or chemical vapor deposition.
[0131] In some embodiments, the first defect layer 105 and the second defect layer 106 have the same thickness.
[0132] Specifically, the thickness of the second defect layer 106 is 300–10000 μm. The thickness of the second defect layer 106 can be any value within the above range, and will not be enumerated here.
[0133] In some embodiments, the first defect layer 105 and the second defect layer 106 are made of the same material.
[0134] Specifically, the material of the second defect layer 106 includes at least one of polycrystalline silicon, ion-implanted polycrystalline silicon, amorphous silicon, and monocrystalline silicon.
[0135] S3: A photoelectric thin film layer 103 is formed on the surface of the first isolation layer 102 away from the supporting substrate 101 using a patterning process. The photoelectric thin film layer 103 has at least one first region 1031 and a second region 1032. The first region 1031 has a ridge waveguide structure, and the resistance of the first region 1031 is higher than that of the second region 1032. The optical chip structure prepared by the above method allows for timely conduction of the charge generated by the photorefractive effect or photovoltaic effect of the photoelectric thin film layer due to the photorefractive effect. This avoids the problem of the bias point of the electro-optic modulator changing over time due to the non-uniform electric field generated within and at the interface of the single-crystal thin film. Simultaneously, the high resistance of the first region ensures the transmittance of the thin film layer, reducing the loss of the optical signal. Furthermore, the ridge waveguide structure formed in the first region not only effectively guides and restricts the propagation of the optical signal but also further reduces the loss of the optical signal.
[0136] In some embodiments, the photoelectric thin film layer 103 is made of at least one of lithium niobate, lithium tantalate, and barium titanate. These materials exhibit excellent photoelectric effects and are suitable for fabricating electro-optic modulators.
[0137] In some embodiments, such as Figure 10 As shown, a photoelectric thin film layer 103 is formed on the surface of the first isolation layer 102 away from the supporting substrate 101 using a patterning process, including:
[0138] A preset photoelectric thin film layer 113 is formed on the surface of the first isolation layer 102 away from the support substrate 101. The preset photoelectric thin film layer 113 includes at least one first initial region 1131 and a second initial region 1132. The resistance of the first initial region 1131 is higher than the resistance of the second initial region 1132.
[0139] A patterned etching process is performed on the preset optoelectronic thin film layer 113 to form a ridge waveguide structure in the first initial region 1131, resulting in the first region 1031. The second initial region 1132 is then thinned to obtain the second region 1032. A reduction process is used to form the first initial region 1131 and the second initial region 1132 on the optoelectronic thin film layer 103. The resistance of the first initial region 1131 is higher than that of the second initial region 1132, allowing the second initial region 1132 to conduct the charge generated on the thin film layer in a timely manner. Simultaneously, the first initial region 1131 maintains a certain transmittance, reducing light loss. After the patterned etching process on the preset optoelectronic thin film layer 113, a ridge waveguide structure is formed in the first initial region 1131, effectively guiding the transmission of optical signals. Thinning the second initial region 1132 further improves its transmittance and reduces light loss.
[0140] In some embodiments, the area of the first region 1031 accounts for 1%-20% of the total area of the photoelectric thin film layer 103. This arrangement ensures that the chip structure has good light transmittance and avoids the problem that a small area of the first region 1031 may lead to reduced light transmittance of the chip structure and increased light loss of the crystal.
[0141] In some embodiments, the resistivity of the first region 1031 is in the range of 3 × 10⁻⁶. 10 ~3×10 18 Ω·cm. By limiting the resistivity of the first region 1031, the energy loss of the optical signal during transmission can be effectively reduced, thereby improving the transmission efficiency of the optical signal.
[0142] In some embodiments, the area of the second region 1032 accounts for 80%-99% of the total area of the optoelectronic thin film layer 103. This arrangement ensures that the chip structure can conduct the charge generated by the photorefractive effect or photovoltaic effect of the optoelectronic thin film layer 103 in a timely manner, avoiding the problem of the bias point of the electro-optic modulator changing over time due to the non-uniform electric field generated in and at the single crystal thin film interface.
[0143] In some embodiments, the resistivity of the second region 1032 is in the range of 1×10⁻⁶. 9 ~3×10 11 Ω·cm. By setting an appropriate resistivity, it is possible to avoid excessive resistivity, which would make it difficult for the chip structure to conduct the charge generated on the optoelectronic thin film layer 103, resulting in a non-uniform electric field within and at the interface of the single crystal thin film, and consequently causing the bias point of the electro-optic modulator to change over time.
[0144] In some embodiments, the thickness of the second region 1032 ranges from 50 to 600 nm. The thickness of the second region 1032 can be any value within the above range, and will not be enumerated here. When the thickness of the second region 1032 is smaller, its resistivity will increase accordingly, but its transmittance will also increase. In order to ensure that the second region 1032 has a low resistance while ensuring a certain transmittance, the above thickness range is limited.
[0145] In some embodiments, the oxygen content in the first region 1031 is higher than the oxygen content in the second region 1032. The higher the oxygen content in the photoelectric thin film layer 103, the higher its resistivity and transmittance. Therefore, the oxygen content in the first region 1031 is set to be higher than the oxygen content in the second region 1032.
[0146] In some embodiments, the ridge waveguide structure includes a substrate region 1033 and a ridge waveguide region 1034. The ridge waveguide region 1034 protrudes from one side surface of the substrate region 1033, and the protrusion height of the ridge waveguide region 1034 protruding from one side surface of the substrate region 1033 ranges from 50 to 600 nm. The protrusion height of the ridge waveguide region 1034 can be any value within the above range, and will not be enumerated here.
[0147] In some embodiments, the width of the ridge waveguide region 1034 ranges from 0.5 to 5 μm. The width of the ridge waveguide region 1034 can be any value within this range, and will not be enumerated here. By limiting the width as described above, the problem of increased optical loss due to an excessively narrow waveguide region is avoided, while the problem of reduced modulation efficiency of the electro-optic modulator due to an excessively wide waveguide region is also avoided.
[0148] In some embodiments, the thickness of the substrate region 1033 ranges from 50 to 600 nm. The thickness of the substrate region 1033 can be any value within the above range, and will not be enumerated here. By limiting the thickness range of the substrate region 1033, the transmittance of the first region 1031 can be improved, while the light loss of the first region 1031 can be reduced.
[0149] In some embodiments, such as Figure 10 As shown, a preset photoelectric thin film layer 113 is formed on the surface of the first isolation layer 102 away from the supporting substrate 101, including:
[0150] An initial photoelectric thin film layer 108 is formed on the surface of the first isolation layer 102 on the side away from the supporting substrate 101;
[0151] A patterned blocking layer 112 is formed on the initial photoelectric thin film layer 108 to obtain an optical chip structure f. The blocking layer 109 blocks the thin film layer region corresponding to the first region 1031 in the initial photoelectric thin film layer 108.
[0152] The initial photoelectric thin film layer 108 with a patterned blocking layer 112 is reduced to restore the thin film layer region exposed by the blocking layer 109, resulting in an optical chip structure g. The blocking layer 109 is then removed to form a preset photoelectric thin film layer 113, resulting in an optical chip structure h. By forming a patterned blocking layer 112 on the initial photoelectric thin film layer 108, the photoelectric thin film layer with the patterned blocking layer can be reduced at a higher temperature, thereby restoring the thin film layer region exposed by the blocking layer 109, which is the second initial region 1132. Simultaneously, the thin film layer region not blocked by the blocking layer 109 is not restored; this region is the first initial region 1131.
[0153] Specifically, the reduction treatment can be carried out by hydrogen annealing or carbon annealing. The annealing temperature used in hydrogen annealing is 300-1000℃ and the annealing time is 3-50h. The annealing temperature used in carbon annealing is 300-1000℃ and the annealing time is 3-50h.
[0154] Specifically, the barrier layer 109 can be removed by wet etching.
[0155] In some embodiments, such as Figure 10 As shown, a patterned blocking layer 112 is formed on the initial photoelectric thin film layer 108, including:
[0156] A barrier layer 109 is formed on the initial photoelectric thin film layer 108 to obtain the optical chip structure b;
[0157] A patterned initial photoresist layer 111 is formed on an initial photoelectric thin film layer 108 having a barrier layer 109 to obtain an optical chip structure d;
[0158] Using a patterned initial photoresist layer 111 as a mask, the initial photoelectric thin film layer 108 with a barrier layer 109 is etched to transfer the pattern of the initial photoresist layer 111 to the barrier layer 109, resulting in optical chip structure e. The initial photoresist layer 111 is then removed to form a patterned barrier layer 112 on the initial photoelectric thin film layer 108, resulting in optical chip structure f. The reason for depositing the barrier layer 109 on the initial photoelectric thin film layer 108 before reduction is that photoresist is difficult to withstand high temperatures and is not suitable for subsequent reduction processes. Specifically, the barrier layer 109 can be etched using either dry etching or wet etching.
[0159] Specifically, the barrier layer 109 can be formed on the initial photoelectric thin film layer 108 by vapor deposition.
[0160] Specifically, the material of the barrier layer 109 can be SiO2, SiN, polycrystalline silicon, diamond-like film, etc.
[0161] In some embodiments, forming a patterned initial photoresist layer 110 on an initial photoelectric thin film layer 108 having a barrier layer 109 includes: coating photoresist on the initial photoelectric thin film layer 108 having a barrier layer 109 and performing a heat treatment to form an initial photoresist layer 110 on the initial photoelectric thin film layer 108 to obtain an optical chip structure c; exposing and developing the initial photoresist layer 110 to form a patterned initial photoresist layer 111 on the initial photoelectric thin film layer 108 having a barrier layer 109 to obtain an optical chip structure d.
[0162] In some embodiments, such as Figure 10As shown, the preset photoelectric thin film layer 113 is subjected to patterning etching, including:
[0163] A patterned photoresist layer 115 is formed on a preset optoelectronic thin film layer 113 to obtain an optical chip structure j;
[0164] Using a patterned photoresist layer 115 as a mask, a preset photoelectric thin film layer 113 is etched to form a ridge waveguide structure in a first initial region 1131, resulting in a first region 1031. The second initial region 1132 is then thinned to obtain a second region 1032, resulting in an optical chip structure k. The patterned photoresist layer 115 is then removed to obtain a photoelectric thin film layer 103 and an optical chip structure l. Specifically, the preset photoelectric thin film layer 113 can be etched using either dry etching or wet etching; preferably, dry etching is used.
[0165] Specifically, the patterned photoresist layer 115 can be removed using either dry etching or wet etching. Preferably, the patterned photoresist layer 115 is removed using wet etching.
[0166] In some embodiments, forming a patterned photoresist layer 115 on a preset photoelectric thin film layer 113 includes: coating the preset photoelectric thin film layer 113 with photoresist and performing a heat treatment to form a photoresist layer 114 on the preset photoelectric thin film layer 113 to obtain an optical chip structure i; and exposing and developing the photoresist layer 114 to form a patterned photoresist layer 115 on the preset photoelectric thin film layer 113 to obtain an optical chip structure j.
[0167] In some embodiments, after forming a photoelectric thin film layer 103 on the surface of the first isolation layer 102 away from the support substrate 101 based on a patterning process, the fabrication method further includes forming an electrode structure 107 on the surface of the second region 1032 away from the first isolation layer 102.
[0168] The foregoing description has fully disclosed the specific embodiments of this application. It should be noted that any modifications made by those skilled in the art to the specific embodiments of this application do not depart from the scope of the claims. Accordingly, the scope of the claims of this application is not limited to the foregoing specific embodiments.
Claims
1. An optical chip structure, characterized by include: Support substrate; A first isolation layer located on one side surface of the supporting substrate; A photoelectric thin film layer is located on the surface of the first isolation layer away from the supporting substrate. The photoelectric thin film layer is provided with at least one first region and a second region. The first region is formed with a ridge waveguide structure. The first region and the second region are located in the same layer of the photoelectric thin film layer. The material of the first region and the material of the second region are the same. The area of the first region is smaller than the area of the second region. The resistance of the first region is higher than the resistance of the second region. The oxygen content of the first region is higher than the oxygen content of the second region.
2. The optical chip structure of claim 1, wherein, The ridge waveguide structure includes a substrate region and a ridge waveguide region, the ridge waveguide region protruding from one side surface of the substrate region, and the substrate region and the ridge waveguide region satisfy at least one of the following characteristics: The ridge waveguide region protrudes from one side surface of the substrate region at a height ranging from 50 to 600 nm. The width of the ridge waveguide region ranges from 0.5 to 5 μm; The thickness of the substrate region ranges from 50 to 600 nm.
3. The optical chip structure of claim 1, wherein, The first region and the second region satisfy at least one of the following characteristics: The area of the first region accounts for 1%-20% of the total area of the photoelectric thin film layer; The area of the second region accounts for 80%-99% of the total area of the photoelectric thin film layer; The resistivity range of the first region is 3×10⁻⁶. 10 ~3×10 18 Ω•cm; The second region has a resistivity in the range of 1 x 10 9 3 x 10 11 Ω-cm.
4. The optical chip structure of claim 1, wherein, The optical chip structure also includes a second isolation layer located on the side of the supporting substrate away from the first isolation layer.
5. The optical chip structure of claim 4, wherein, The first isolation layer and the second isolation layer satisfy at least one of the following characteristics: The first isolation layer and the second isolation layer have the same thickness; The first isolation layer is made of the same material as the second isolation layer.
6. The optical chip structure of claim 1, wherein, The optical chip structure also includes a first defect layer located between the first isolation layer and the supporting substrate.
7. The optical chip structure of claim 6, wherein, The optical chip structure also includes a second defect layer located on the surface of the supporting substrate away from the first defect layer.
8. The optical chip structure of claim 7, wherein, The structure satisfies at least one of the following characteristics: The thickness of the first defect layer ranges from 300 to 10000 μm; The material of the first defect layer includes at least one of polycrystalline silicon, ion-implanted polycrystalline silicon, amorphous silicon, and monocrystalline silicon; The first defect layer and the second defect layer have the same thickness; The first defect layer and the second defect layer are made of the same material.
9. The optical chip structure according to any one of claims 1-8, characterized in that, The structure satisfies at least one of the following characteristics: The thickness of the first isolation layer ranges from 1 to 50 μm; The thickness of the second region ranges from 50 to 600 nm; The thickness of the supporting substrate ranges from 300 to 1000 μm; The curvature of the supporting substrate ranges from -30 to 30 μm.
10. The optical chip structure according to any of claims 1-8, characterized in that, The structure satisfies at least one of the following characteristics: The material of the first insulating layer includes at least one of silicon dioxide, silicon nitride, and aluminum oxide; The material of the photoelectric thin film layer includes at least one of lithium niobate, lithium tantalate, and barium titanate. The supporting substrate includes at least one of silicon, silicon carbide, sapphire, and quartz.
11. The optical chip structure according to any of claims 1 to 8, characterized in that The structure also includes an electrode structure located on the side surface of the second region away from the first isolation layer.
12. A method of fabricating an optical chip structure, characterized by, The preparation method includes: Provide a supporting substrate; A first isolation layer is formed on one side surface of the supporting substrate; A photoelectric thin film layer is formed on the surface of the first isolation layer away from the supporting substrate using a patterning process; The optoelectronic thin film layer has at least one first region and a second region. The first region has a ridge waveguide structure. The first region and the second region are located in the same layer of the optoelectronic thin film layer. The materials of the first region and the second region are the same. The area of the first region is smaller than the area of the second region. The resistance of the first region is higher than the resistance of the second region. The oxygen content of the first region is higher than the oxygen content of the second region.
13. The method of claim 12, wherein, The formation of a photoelectric thin film layer on the surface of the first isolation layer away from the supporting substrate based on a patterning process includes: A preset photoelectric thin film layer is formed on the surface of the first isolation layer away from the supporting substrate. The preset photoelectric thin film layer includes at least one first initial region and a second initial region. The resistance of the first initial region is higher than that of the second initial region. The preset photoelectric thin film layer is patterned and etched to form a ridge waveguide structure in the first initial region to obtain the first region, and the second initial region is thinned to obtain the second region.
14. The method of claim 13, wherein, A predetermined photoelectric thin film layer is formed on the surface of the first isolation layer away from the supporting substrate, including: An initial photoelectric thin film layer is formed on the surface of the first isolation layer on the side away from the supporting substrate; A patterned blocking layer is formed on the initial photoelectric thin film layer, and the blocking layer blocks the thin film layer region corresponding to the first region in the initial photoelectric thin film layer. The initial photoelectric thin film layer with the patterned blocking layer is restored to restore the thin film layer area exposed by the blocking layer, and the blocking layer is removed to form the preset photoelectric thin film layer.
Citation Information
Patent Citations
Heterostructure and preparation method thereof
CN116564802A
Composite film for high-performance electro-optical modulator and preparation method thereof
CN118311792A
Photoelectric material modulator and manufacturing method thereof
CN118466056A