Elastic-plastic graded damping device and preparation method thereof
The elastic-plastic graded shock-absorbing device, which uses the synergistic effect of multiple layers of materials, solves the problem of insufficient energy dissipation capacity of existing shock-absorbing devices in complex vibration environments, achieves lightweighting and improved stability, and is suitable for multiple engineering fields.
Patent Information
- Application Number
- CN202511142304.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-08-15
- Publication Date
- 2025-10-03
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing shock-absorbing devices have insufficient energy dissipation capacity in complex vibration environments and are difficult to meet grading requirements. In addition, the material density is high and the interlayer bonding strength is insufficient, resulting in excessive weight of the device and poor long-term stability.
An elastic-plastic graded shock-absorbing device that uses the synergistic effect of multiple layers of materials, including nickel-titanium alloy, magnesium-aluminum alloy and carbon fiber reinforced epoxy resin composite materials, achieves graded energy dissipation and lightweight design through shape memory effect, plastic deformation and rigid support structure.
It exhibits excellent shock absorption performance in complex vibration environments, reduces the weight of the device, improves structural stability and applicability, and is suitable for aerospace, transportation, and construction fields.
Smart Images

Figure CN120739819A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of shock absorption, in particular to an elastic-plastic graded shock absorption device and a preparation method thereof. Background Art
[0002] Vibration control is a key technology in engineering structures and equipment operation. In particular, in the fields of aerospace, transportation, and construction, vibration significantly impacts equipment accuracy, structural safety, and service life. Currently, mainstream shock absorbers rely primarily on single materials (such as rubber pads) or simple composite structures (such as spring-damper systems). Their single energy dissipation mechanism makes them difficult to adapt to complex vibration environments: Traditional rubber damping materials are prone to hardening and failure under high-frequency vibration, and their recovery after plastic deformation is poor. Metal spring systems cannot achieve graded energy dissipation and are prone to resonance when subjected to impact loads. Existing graded damping structures (such as metal-rubber laminates) lack interlayer bonding strength, which can lead to delamination after long-term use. Furthermore, the high material density leads to excessive weight. In particular, there is a lack of a solution that can simultaneously meet the following requirements: adaptive graded energy dissipation for low, medium, and high-intensity vibrations; reduce the device's weight through a lightweight layered structure; and ensure interlayer bonding strength to maintain long-term stability.
[0003] In response to the above problems, there is an urgent need to develop an elastic-plastic graded shock-absorbing device that can improve the shock-absorbing performance through the synergistic effect of multiple layers of materials without increasing the complexity of the structure, so as to meet the actual needs in different vibration environments. Summary of the Invention
[0004] This invention provides an elastic-plastic graded shock-absorbing device and its preparation method, addressing the problems of existing shock-absorbing devices, such as insufficient energy dissipation capacity in complex vibration environments and mechanical properties that fail to meet graded requirements. Through the synergistic effect of multiple layers of materials, the device exhibits excellent shock-absorbing performance under high-frequency vibration or impact loads. The optimized material selection and preparation process also enhance the overall stability and applicability of the structure.
[0005] To achieve the above objectives, the present invention is implemented through the following technical solutions: an elastic-plastic graded shock absorbing device, comprising: The elastic transformation layer is made of nickel-titanium alloy with an atomic ratio of nickel to titanium of 55:45. Its function is to absorb and store some vibration energy under external force through the shape memory effect. Then, when the stress exceeds a critical value, it undergoes superelastic deformation, releasing the stored energy and dissipating it as heat. The elastic transformation layer is prepared using a vacuum induction melting and homogenization annealing process. Nickel and titanium powders are mixed in a certain atomic ratio and then melted into an ingot. After annealing to eliminate internal stress, it is cooled to room temperature and processed into the desired shape. The plastic deformation layer is made of a magnesium-aluminum alloy with a weight ratio of 70:30. After the elastic deformation layer reaches its ultimate stress, it further absorbs residual vibration energy through its own plastic deformation and forms a stress concentration zone in a localized area to disperse external forces. The plastic deformation layer is produced using a powder metallurgy process, where magnesium and aluminum powders are mixed in appropriate proportions, cold-pressed, and then sintered at high temperature to obtain a dense blank. The rigid deformation layer is made of a carbon fiber reinforced epoxy resin composite material. Its function is to provide a stable support structure for the elastic deformation layer and the plastic deformation layer, while preventing external impact forces from being directly transmitted to the underlying equipment. The rigid deformation layer is prepared by stacking carbon fiber cloth impregnated with epoxy resin layer by layer, applying pressure between each layer and curing at high temperature to form a composite material plate. The elastic, plastic and rigid deformation layers are stacked and bonded in sequence using epoxy resin adhesive, and the interlayer bonding surfaces are sandblasted to increase the roughness and ensure bonding strength. A shock-absorbing base is installed under the elastic-plastic graded shock-absorbing device to fix the entire device and disperse the bottom stress.
[0006] Preferably, the preparation method of the plastic property-changing layer is as follows: Raw material preparation: Prepare 70% magnesium powder and 30% aluminum powder by weight, with a particle size range of 20-50μm; Powder mixing: put magnesium powder and aluminum powder into a ball mill and mix them with a ball-to-material ratio of 10:1, a rotation speed of 200-300 rpm, and a mixing time of 2-4 hours; Cold pressing: The mixed powder is placed in a mold and a pressure of 100-200 MPa is applied for cold pressing to obtain a preformed body; High temperature sintering: Place the preform in a sintering furnace, heat to 500-600°C at a heating rate of 10°C / min, keep warm for 1-2 hours, and then cool to room temperature with the furnace.
[0007] Preferably, the method for preparing the rigid property-changing layer is as follows: Layer by layer: Impregnate the carbon fiber cloth with epoxy resin and stack it layer by layer, applying a pressure of 0.5-1MPa between each layer; High temperature curing: The stacked composite panels are heated to 120-150°C and kept warm for 2-4 hours to form composite panels with high strength and stability.
[0008] Preferably, the method of sequentially laminating the elastic property change layer, the plastic property change layer and the rigid property change layer is as follows: Surface treatment: sandblast the bottom surface of the elastic deformation layer, the upper and lower surfaces of the plastic deformation layer, and the top surface of the rigid deformation layer respectively, and control the roughness within Ra1.6-3.2μm; Gluing and laminating: evenly apply epoxy resin adhesive on the upper surface of the plastic deformation layer with a coating thickness of 0.2-0.5mm, align the bottom surface of the elastic deformation layer with the upper surface of the plastic deformation layer, apply a pressure of 5-10MPa, and preliminarily cure at room temperature for 1-2 hours; Secondary gluing and lamination: Apply the same adhesive on the lower surface of the plastic deformation layer with a thickness of 0.2-0.5mm, align the top surface of the rigid deformation layer with the lower surface of the plastic deformation layer, apply a pressure of 5-10MPa, and cure at 60-80℃ for 4-6 hours.
[0009] Preferably, the magnesium powder and aluminum powder are dried before mixing, with the drying temperature being 80-100° C. and the drying time being 2-3 hours.
[0010] Preferably, the epoxy resin adhesive has a weight ratio of epoxy resin matrix to curing agent of 2:1, and a viscosity of 5000-10000 mPa·s.
[0011] Preferably, the thickness of the elastic qualitative change layer is 2-5 mm.
[0012] The present invention provides an elastic-plastic graded shock-absorbing device and a preparation method thereof, which has the following beneficial effects: The present invention adopts nickel-titanium alloy, magnesium-aluminum alloy and carbon fiber reinforced epoxy resin composite materials, and the overall density is significantly lower than that of traditional metal shock-absorbing materials, which reduces the weight of the device and improves the installation flexibility. Through the three-layer collaborative mechanism of "elastic deformation-plastic energy dissipation-rigid support", graded absorption and dissipation of external vibration or impact force is achieved. The elastic deformation layer utilizes the shape memory effect and superelastic properties to absorb the initial vibration energy, the plastic deformation layer further dissipates the residual energy through local plastic deformation, and the rigid deformation layer effectively isolates the external impact force and protects the underlying equipment from damage. In addition, the shock-absorbing base assembled at the bottom of the device can disperse stress and improve the overall stability, making it suitable for complex vibration environments in the fields of aerospace, transportation and construction. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 It is a schematic diagram of the overall structure of the present invention; Figure 2 Schematic diagram of the structure of the elastic property change layer, the plastic property change layer and the rigid property change layer of the present invention; Figure 3 This is a flow chart for preparing the elastic qualitative change layer of the present invention; Figure 4 This is a flow chart for preparing the plastic property-changing layer of the present invention; Figure 5 This is a flow chart for preparing the rigid property change layer of the present invention.
[0014] Among them, 1. Elastic deformation layer; 2. Plastic deformation layer; 3. Rigid deformation layer; 4. Shock-absorbing base. DETAILED DESCRIPTION
[0015] The following will clearly and completely describe the technical solution of the present invention in conjunction with the accompanying drawings. Obviously, the embodiments described are only some embodiments of the present invention, not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of the present invention.
[0016] The elastic-plastic graded shock absorbing device of the present invention is as follows Figure 1 and Figure 2 As shown, the overall structure consists of an elastic transformation layer 1, a plastic transformation layer 2, a rigid transformation layer 3, and a shock-absorbing base 4. Each layer is stacked and bonded together using epoxy resin adhesive to form a coordinated whole. The elastic transformation layer 1 is the topmost layer, its bottom surface tightly attached to the top surface of the plastic transformation layer 2. The bottom surface of the plastic transformation layer 2 is bonded to the top surface of the rigid transformation layer 3. The bottom of the rigid transformation layer 3 is equipped with a shock-absorbing base 4 to stabilize the entire device and distribute stress at the bottom.
[0017] The elastic transformation layer 1 is made of nickel-titanium alloy, with the atomic ratio of nickel to titanium being 55:45. The preparation process is as follows: Figure 3 As shown. First, nickel powder and titanium powder are mixed according to the atomic ratio. During the mixing process, a ball mill is used for homogenization treatment. The ball-to-material ratio is 10:1, the rotation speed is controlled at 200-300rpm, and the mixing time is 2-4 hours. The mixed powder is melted into ingots by vacuum induction melting technology. The vacuum degree is strictly controlled during the melting process to avoid oxidation. After the melting is completed, the ingot is subjected to homogenization annealing treatment. The annealing temperature is set to 800-900℃, the holding time is 2-3 hours, and then it is cooled to room temperature with the furnace to eliminate internal stress. The cooled ingot is machined into a thin sheet with a thickness of 2-5mm as the final form of the elastic transformation layer 1. The bottom surface of the elastic transformation layer 1 is sandblasted, and the roughness is controlled at Ra1.6-3.2μm to improve the bonding strength with the plastic transformation layer 2.
[0018] The plastic deformation layer 2 is made of magnesium-aluminum alloy, with a weight ratio of magnesium to aluminum of 70:30. The preparation process is as follows: Figure 4As shown. First, prepare magnesium powder and aluminum powder with a particle size range of 20-50μm. Before mixing, dry the two powders at 80-100℃ for 2-3 hours to remove moisture. The dried powder is weighed according to weight percentage and placed in a ball mill for mixing. The ball-to-material ratio is 10:1, the rotation speed is 200-300rpm, and the mixing time is 2-4 hours. The mixed powder is placed in a mold and cold-pressed at a pressure of 100-200MPa to obtain a preform. The preform is then placed in a sintering furnace for high-temperature sintering with a heating rate of 10℃ / min, a sintering temperature of 500-600℃, a holding time of 1-2 hours, and then cooled to room temperature with the furnace. The sintered body is processed into the desired shape, and its upper and lower surfaces are sandblasted, and the roughness is also controlled at Ra1.6-3.2μm.
[0019] The rigid deformation layer 3 is made of carbon fiber reinforced epoxy resin composite material, and its preparation process is as follows: Figure 5 As shown. First, the carbon fiber cloth is impregnated with epoxy resin. During the impregnation process, ensure that the resin evenly covers the fiber surface to avoid residual bubbles. The impregnated carbon fiber cloth is stacked layer by layer, and a pressure of 0.5-1MPa is applied between each layer to ensure close bonding between the layers. The stacked composite material plate is placed in a high-temperature curing furnace and heated to 120-150°C for 2-4 hours, and then naturally cooled to room temperature. The cured composite material plate has high strength and stability, and its top surface is sandblasted with a roughness controlled at Ra1.6-3.2μm.
[0020] The lamination process for the elastic, plastic, and rigid layers 3 is as follows: First, an epoxy resin adhesive is evenly applied to the upper surface of the plastic layer 2. The adhesive has a weight ratio of epoxy resin matrix to curing agent of 2:1, a viscosity of 5000-10000 mPa·s, and a coating thickness of 0.2-0.5 mm. The bottom surface of the elastic layer 1 is aligned with the upper surface of the plastic layer 2, and a pressure of 5-10 MPa is applied. The adhesive is initially cured at room temperature for 1-2 hours. Subsequently, the same adhesive is applied to the lower surface of the plastic layer 2 to a thickness of 0.2-0.5 mm. The top surface of the rigid layer 3 is aligned with the lower surface of the plastic layer 2, and a pressure of 5-10 MPa is applied. The adhesive is cured at 60-80°C for 4-6 hours. The interlayer bonding surfaces are sandblasted to increase the roughness and ensure bonding strength.
[0021] The shock-absorbing base 4 is connected to the bottom of the rigid deformation layer 3 via bolts or other fixing methods. Its function is to fix the device, disperse the stress at the bottom, and absorb the residual vibration energy transmitted by the rigid deformation layer 3. The design of the shock-absorbing base 4 can be adjusted according to the actual application scenario. For example, a lightweight design can be adopted in the aerospace field, while the bottom friction coefficient can be increased to improve stability in the construction field.
[0022] The working principle of this device is as follows: when external vibration or impact force acts on the elastic transformation layer 1, the shape memory effect of nickel-titanium alloy first absorbs and stores part of the vibration energy. As the external force increases, the elastic transformation layer 1 undergoes superelastic deformation, converting the stored energy into heat energy dissipation. When the stress exceeds the limit value of the elastic transformation layer 1, the plastic transformation layer 2 begins to play a role, further absorbing the residual vibration energy through local plastic deformation, and forming a stress concentration area in the local area to disperse the external force. The rigid transformation layer 3 provides a stable support structure for the elastic transformation layer 1 and the plastic transformation layer 2 throughout the process, while preventing external impact force from being directly transmitted to the underlying equipment. The shock-absorbing base 4 improves the overall stability by dispersing the bottom stress.
[0023] This device is suitable for use in complex vibration environments in the aerospace, transportation, and construction sectors. For example, in aerospace, it can be used to reduce vibration and protect internal aircraft equipment, reducing the device's weight while increasing installation flexibility. In transportation, it can be applied to vehicle suspension systems to effectively absorb vibrations caused by uneven road surfaces. In construction, it can be used in the seismic design of high-rise buildings, protecting their structural safety through graded absorption and dissipation of seismic energy.
[0024] While embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions, and variations may be made to these embodiments without departing from the principles and spirit of the invention, and that the scope of the invention is defined by the appended claims and their equivalents.
Claims
1. An elastic-plastic graded shock-absorbing device, characterized in that: include: An elastic qualitative change layer (1), wherein the elastic qualitative change layer (1) is made of nickel-titanium alloy, and the atomic ratio of nickel to titanium is 55:45; A plastic deformation layer (2), wherein the plastic deformation layer (2) is made of a magnesium-aluminum alloy, and the weight ratio of magnesium to aluminum is 70:30; A rigid property-changing layer (3), wherein the rigid property-changing layer (3) is made of a carbon fiber reinforced epoxy resin composite material; A shock-absorbing base (4), the shock-absorbing base (4) being connected to the bottom of the rigid property-changing layer (3); The elastic property change layer (1), the plastic property change layer (2) and the rigid property change layer (3) are sequentially laminated and bonded together using an epoxy resin adhesive.
2. A method for preparing an elastic-plastic material, characterized in that: The method for preparing the elastic qualitative change layer (1) comprises the following steps: S1 nickel powder and titanium powder according to the atomic ratio of 55:45 mixed, melted into an ingot in a vacuum induction furnace; S2 after the smelting of the alloy ingot homogenization annealing treatment, the annealing temperature is 800-900 ℃, the holding time is 2-3 hours; S3. After cooling to room temperature, process into the desired shape.
3. The method for preparing an elastic-plastic material according to claim 2, characterized in that: The method for preparing the plastic property-changing layer (2) comprises the following steps: S1. Raw material preparation: Prepare 70% magnesium powder and 30% aluminum powder by weight, with a particle size range of 20-50μm; S2 powder mixing: magnesium powder and aluminum powder were mixed in a ball mill with a ball-to-material ratio of 10:1, a speed of 200-300rpm, and a mixing time of 2-4 hours; S3 cold pressing: The mixed powder is loaded into a mold and cold pressed under a pressure of 100-200MPa to obtain a preform; S4. High-temperature sintering: Place the preform in a sintering furnace and heat it to 500-600°C at a heating rate of 10°C / min. Keep it at this temperature for 1-2 hours and then cool it to room temperature.
4. The method for preparing an elastic-plastic material according to claim 2, characterized in that: The method for preparing the rigid property-changing layer (3) comprises the following steps: S1. Impregnate carbon fiber cloth with epoxy resin and stack them layer by layer, applying a pressure of 0.5-1MPa between each layer; S2. Heat to 120-150°C and cure for 2-4 hours to form a composite material plate.
5. The method for preparing an elastic-plastic material according to claim 2, characterized in that: The method of sequentially laminating the elastic transformation layer (1), the plastic transformation layer (2) and the rigid transformation layer (3) is as follows: S1. Surface treatment: sandblasting the bottom surface of the elastic deformation layer (1), the upper and lower surfaces of the plastic deformation layer (2), and the top surface of the rigid deformation layer (3), respectively, with the roughness controlled within Ra1.6-3.2μm; S2. Glue bonding: evenly coat the upper surface of the plastic deformation layer (2) with an epoxy resin adhesive to a thickness of 0.2-0.5 mm, align the bottom surface of the elastic deformation layer (1) with the upper surface of the plastic deformation layer (2), apply a pressure of 5-10 MPa, and initially cure at room temperature for 1-2 hours; S3. Secondary gluing and laminating: Apply the same adhesive to the lower surface of the plastic deformation layer (2) with a thickness of 0.2-0.5 mm, align the top surface of the rigid deformation layer (3) with the lower surface of the plastic deformation layer (2), apply a pressure of 5-10 MPa, and cure at 60-80°C for 4-6 hours.
6. The method for preparing an elastic-plastic material according to claim 3, characterized in that: The magnesium powder and aluminum powder are dried before mixing, with the drying temperature being 80-100° C. and the drying time being 2-3 hours.
7. The method for preparing an elastic-plastic material according to claim 5, characterized in that: The epoxy resin adhesive has a weight ratio of epoxy resin matrix to curing agent of 2:1 and a viscosity of 5000-10000 mPa·s.
8. The method for preparing an elastic-plastic material according to claim 2, characterized in that: The thickness of the elastic qualitative change layer (1) is 2-5 mm.