Method for correcting humidification deformation of earth and rockfill dam based on field actual measurement of moisture content and density of rockfill material

Through on-site triaxial wetting deformation tests on the moisture content and density of rockfill materials, a correction formula was established, which solved the accuracy problem of wetting deformation prediction of earth-rock dams and achieved high-precision, low-cost deformation prediction and control, which is suitable for the design of large-scale dam projects.

CN120740534AActive Publication Date: 2025-10-03POWERCHINA HUADONG ENG CORP LTD +1
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202510943218.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-07-09
Publication Date
2025-10-03
Estimated Expiration
2045-07-09

AI Technical Summary

Technical Problem

Existing technologies make it difficult to accurately predict the wetting deformation of earth-rockfill dams, especially when considering the changes in moisture content and density of on-site rockfill materials. This leads to design deviations and may cause safety risks such as dam body deformation and cracks.

Method used

Through on-site triaxial wetting deformation tests on the moisture content and density of rockfill materials, a correction formula was established. Combined with the conventional wetting model, the correction coefficients of moisture content and density were considered to achieve accurate prediction of wetting deformation.

Benefits of technology

It improves the accuracy of wetting deformation prediction, reduces test costs, has good engineering practicality, can be directly used in earth-rock dam engineering practice, and provides reliable deformation prediction and compaction quality control.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120740534A_ABST
    Figure CN120740534A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of geotechnical engineering, provides a method for correcting humidifying deformation of an earth and rockfill dam based on field actual measurement of moisture content and density of rockfill materials, and aims to accurately reflect actual rules of humidifying deformation of the rockfill materials and improve safety and reliability of design and operation of the earth and rockfill dam. The method comprises the following steps: firstly, selecting a typical rockfill material on site for scale reduction, and systematically carrying out humidification deformation tests under different initial water contents and densities to obtain a rule that the humidification deformation characteristics of the rockfill material change along with the dry density and the water contents; then, on the basis of a conventional humidification model, a correction coefficient is introduced, and a humidification deformation correction formula under water content and density control is established; and finally, substituting the field actually measured moisture content and density data into the correction formula to obtain a correction coefficient, thereby realizing accurate prediction of the humidification deformation of different dam body areas. The method has the advantages of high accuracy, low test cost and good field adaptability, and is suitable for design and evaluation of various large dam body projects such as pumped storage.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of geotechnical engineering and relates to a method for correcting wetting deformation of an earth-rock dam based on on-site measured moisture content and density of rockfill materials. Background Art

[0002] With the rapid development of renewable energy sources in my country (such as wind and photovoltaic power generation), the demand for grid regulation capabilities and energy storage systems is growing. Pumped-storage power stations, due to their low construction and operating costs, long service life, and mature technology, have become the mainstream large-scale energy storage method. Currently, pumped-storage power stations are widely deployed across my country, and installed capacity continues to grow. In the design and construction of pumped-storage power stations, earth-rock dams are typically used as the water storage structures for the upper and lower reservoirs.

[0003] Wetting deformation of rockfill materials refers to the deformation that occurs when they transition from a dry state to a wet state. During the construction and operation of earth-rockfill dams, the materials inevitably undergo wetting due to factors such as rainfall, flooding, and reservoir impoundment. In severe cases, this can cause deformation, cracks, and even leakage in the dam body, threatening the safety of the entire pumped-storage power station. Therefore, accurately predicting and rationally controlling wetting deformation of rockfill materials is a crucial step in design and construction.

[0004] Currently, research on the wetting deformation characteristics of rockfill materials relies primarily on laboratory wetting tests, using common methods such as the "double-line method" and the "single-line method." The single-line method is widely considered more effective because it better reflects the actual deformation process under water immersion. However, the single-line method only captures wetting deformation data under a single stress state. Comprehensively studying the wetting deformation of rockfill materials under different stress states and physical properties (density, moisture content, etc.) requires extensive repeated testing, which is extremely costly and labor-intensive. Furthermore, during the actual construction of earth-rockfill dams, the density and initial moisture content of rockfill materials fluctuate due to differences in construction techniques, equipment efficiency, and climatic conditions. The moisture content of dam materials also changes over time. Using wetting deformation parameters derived from traditional laboratory wetting tests based on single-density dry specimens to guide earth-rockfill dam design often results in errors. On the one hand, wetting deformation may be overestimated, leading to overcompaction after construction adjustments; on the other hand, wetting deformation may be underestimated, resulting in a lack of countermeasures and causing excessive local deformation, cracks, and other engineering risks.

[0005] In summary, wetting deformation is a critical issue in earth-rockfill dam construction, affecting the entire process from construction to water storage and even long-term operation. To improve prediction accuracy and practicality, a correction method for wetting deformation that considers the moisture content and density of the on-site rockfill material is urgently needed, thereby providing more reliable technical support for the design and construction of earth-rockfill dams. Summary of the Invention

[0006] To address the challenges of existing technologies, this paper proposes a method for correcting the wetting deformation of earth-rockfill dams based on field-measured rockfill moisture content and density. This method considers the impact of the actual rockfill moisture content and density on wetting deformation, resolving the difficulty of accurately predicting wetting deformation in earth-rockfill dams under existing technical conditions. By combining high accuracy, low testing costs, and excellent field applicability, it is suitable for the engineering design and assessment of various large-scale dams, including those for pumped storage hydropower plants.

[0007] In order to achieve the above object, the technical solution adopted by the present invention is:

[0008] A correction method for the wetting deformation of earth-rockfill dams based on the on-site measured moisture content and density of rockfill materials. First, typical on-site rockfill materials are selected for scale reduction. By systematically conducting wetting deformation tests at different initial moisture contents and densities, the law of how the wetting deformation characteristics of the rockfill materials change with dry density and moisture content is obtained. Then, based on the conventional wetting model, a correction coefficient is introduced to establish a correction formula for wetting deformation under moisture content and density control. Finally, the on-site measured moisture content and density data are substituted into the correction formula to obtain the correction coefficient, thereby achieving accurate prediction of the wetting deformation amount of different dam body areas. Specifically, the following steps are included:

[0009] Step 1: Select rockfill from the main rockfill partition of the rockfill dam body and scale it down using the similar gradation method according to the Geotechnical Test Methods Standard GB / T50123-2019. The maximum particle size after scaling is 60 mm. The specific gravity and natural moisture content of the scaled rockfill are measured in an indoor laboratory.

[0010] The methods for determining the specific gravity and natural moisture content of the rockfill materials are carried out by the floating weighing method and the drying method respectively according to the "Geotechnical Test Method Standard GB / T 50123-2019".

[0011] Step 2: For the rockfill material with a maximum particle size of 60 mm obtained in the first step, triaxial wetting deformation tests were carried out at different densities and moisture contents to obtain the wetting deformation characteristics of the rockfill material and the law of change of the wetting deformation characteristics of the rockfill material with dry density and moisture content.

[0012] Furthermore, in the second step, triaxial wetting tests were conducted on the rockfill material. Sample preparation and testing procedures were conducted in accordance with the triaxial wetting deformation test section of the "Test Procedure for Coarse-Grained Soils" (T / CHES 29-1019). The specimens were cylindrical, 300 mm in diameter and 700 mm in height. During the test, the wetting shear strain and wetting volumetric strain of the rockfill material were recorded.

[0013] Furthermore, in the second step, when designing triaxial wetting deformation tests for rockfill materials at different densities and initial moisture contents under different working conditions, orthogonal design can be omitted to reduce the testing workload. It is recommended that two main working conditions be used: Working Condition 1 controls the initial moisture content of the specimens to 0% and conducts triaxial wetting deformation tests for rockfill materials at low, medium (design fill density), and high density gradients, with at least 3-5 density gradients. Working Condition 2 controls the test density to the design fill density and conducts triaxial wetting deformation tests for rockfill materials at low, medium, and high density gradients, with at least 3-5 moisture content gradients.

[0014] Furthermore, in the second step, the density control index is determined according to the properties of the rockfill material. If the rockfill material is blasting material, the porosity or porosity ratio is used for control, and if the rockfill material is gravel, the compaction degree is used for control. The moisture content is mass moisture content.

[0015] Furthermore, in the second step, the law of the change of the wet deformation characteristics of rockfill materials with dry density and moisture content is mainly the wet shear strain , Wetting volume strain , with the stress level , confining pressure (kPa), porosity n (%), water content (%) change pattern.

[0016] Step 3: Establish a correction formula based on the conventional wetting model that takes into account moisture content and density to describe the variation of the wetting deformation characteristics of rockfill materials with dry density and moisture content.

[0017] Furthermore, the form of the correction formula based on the conventional wetting model considering moisture content and density is recommended as follows, wherein formula (1) is the corrected wetting shear strain model, formula (2) is the corrected wetting volume strain model, and formula (3) is the calculation formula for the correction coefficient:

[0018] (1)

[0019] (2)

[0020] (3)

[0021] in, is the wetting shear strain, is the stress level; is the undetermined coefficient in the wetting shear strain model; is the undetermined index of the wetting shear strain model; K is the correction coefficient obtained from the experiment; is the humidification volume strain; is the wetting dilatancy ratio. Based on the wetting dilatancy ratio, the wetting volume change can be calculated through the wetting shear strain. Therefore, when making corrections, only the correction coefficient K of the wetting shear strain needs to be considered. is the wetting dilatancy ratio of rockfill The undetermined coefficient of is the stress ratio when the wetting dilatancy ratio is 0; p' is the average effective principal stress; p a is one atmosphere (101.2 kPa), used to make stress units dimensionless; m is the wetting dilatancy ratio The undetermined stress index; is the stress ratio, that is, the ratio of the deviatoric stress q to the average principal stress p; is the fitting index of the correction coefficient; is the effective water absorption rate (i.e., the moisture content above which no wetting deformation occurs even when the moisture content increases), obtained by fitting the data; is the designed porosity of the fill, i.e. the benchmark porosity for the wetting test study; is the moisture content of the rockfill material to be corrected for wetting deformation; Density of rockfill material to be corrected for wetting deformation.

[0022] Step 4: Based on the wetting deformation characteristics of the rockfill material obtained from the triaxial wetting deformation test of the rockfill material in Step 2, the parameters of the correction formula considering moisture content and density established based on the conventional wetting model in Step 3 are fitted. Then, the actual moisture content and density of the rockfill material of the earth-rockfill dam that needs to be corrected for wetting deformation are substituted into Formula (3) to obtain the correction coefficient K. The correction of the wetting deformation of the earth-rockfill dam based on the moisture content and density of the rockfill material measured on site can be completed using Formulas (1) and (2).

[0023] Furthermore, in step 4, the process of fitting parameters based on the modified formula considering moisture content and density of the conventional wetting model is as follows:

[0024] Step 4.1, based on the working condition 1 in the second step, the initial moisture content of the sample is controlled to be 0%, the density is the fill design density, the simplification coefficient K=1, and the modified model is degraded to the conventional wetting model. The parameters in formula (1) are fitted by the nonlinear regression function of the statistical analysis software SSPS. 、 , the parameters in formula (2) 、 , m;

[0025] Step 4.2: Based on the fitting results of step 4.1, according to the working condition 1 in step 2, the initial moisture content of the sample is controlled to 0%, and the wet deformation test of rockfill materials with different densities is carried out. The nonlinear regression function of the statistical analysis software SSPS is used to fit the parameters in formula (3): ;

[0026] Step 4.3, based on the working condition 2 in the second step, the test density is controlled to be the filling design density, including the triaxial wetting deformation test of rockfill materials with low, medium and high levels and at least 3-5 moisture content gradients and the parameter fitting results of steps 2) and 3), and the nonlinear regression function of the statistical analysis software SSPS is used to fit the parameters in formula (3) .

[0027] Compared with the prior art, the present invention has the following beneficial effects:

[0028] (1) The present invention establishes a correction formula based on the conventional wetting model that takes into account moisture content and density. This solves the limitation of traditional wetting deformation prediction that fails to consider the actual density and initial moisture content changes of dam construction materials on site, and can significantly improve the prediction accuracy.

[0029] (2) The design method of the triaxial wetting deformation test of rockfill materials proposed in this invention can greatly reduce the workload of sample preparation while ensuring that the law of the variation of the wetting deformation characteristics of rockfill materials with density and moisture content can be obtained, and has good engineering practicality.

[0030] (3) The correction method for wetting deformation of earth-rock dams based on the on-site measured moisture content and density of rockfill materials proposed in this invention can be directly applied to earth-rock dam engineering practice. By substituting the on-site measured moisture content and density, the correction result of wetting deformation that is regionally adapted can be obtained, providing a reliable technical means for dam body zoning deformation prediction and compaction quality control.

[0031] (4) The test process of the method of the present invention strictly complies with the "Geotechnical Test Method Standard GB / T 50123-2019" and the "Coarse-grained Soil Test Procedure T / CHES 29-2019". The parameter determination method is clear and has broad engineering application and promotion value. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] Figure 1 This is a typical asphalt concrete core dam filling zoning map;

[0033] Figure 2 is the gradation curve of rockfill materials;

[0034] Figure 3 is the curve of wet shear strain changing with time;

[0035] Figure 4 is the curve of the variation of the wetted body strain with time;

[0036] Figure 5 The variation of wetting shear strain with stress level under different porosity conditions;

[0037] Figure 6The variation of the strain of the wetted body with the stress level under different porosity conditions;

[0038] Figure 7 is the variation law of wetting shear strain with moisture content;

[0039] Figure 8 The variation law of the humidified body strain with the moisture content;

[0040] Figure 9 This is the fitting effect diagram of wetting shear strain under different porosity conditions;

[0041] Figure 10 This is the fitting effect diagram of the wetting dilatancy ratio;

[0042] Figure 11 is the fitting effect of wetting shear strain;

[0043] Figure 12 is the fitting effect of humidification volume change;

[0044] Figure 13 is the measured porosity frequency distribution histogram of rockfill materials;

[0045] Figure 14 is the frequency distribution histogram of the measured moisture content of rockfill materials;

[0046] Figure 15 Flow chart of the method of the present invention. DETAILED DESCRIPTION

[0047] The following describes the relevant designs of the present invention in detail with reference to the accompanying drawings. Taking an asphalt concrete core dam project as an example, the specific implementation process of the correction method for the wetting deformation of an earth-rock dam based on the on-site measurement of the moisture content and density of the rockfill material is described.

[0048] Step 1: The asphalt concrete core dam project is divided into the following sections: Figure 1 As shown in Figure 1, the dam body consists of upstream rockfill area I, downstream rockfill area I, downstream rockfill area II, a grouting gallery, and a concrete core wall. Considering the wetting deformation behavior of the upstream dam body, the rockfill material from upstream rockfill area I was used as the test material. According to the "Soil Test Method Standard GB / T 50123-2019", the similar gradation method was used for scaling. The dam material gradation curves before and after scaling are shown in the attached figure. Figure 2 The maximum particle size is 60 mm. In an indoor laboratory, the specific gravity and moisture content of the scaled-down rockfill material were measured using the float weighing method and the drying method, respectively. The measured specific gravity of the material was 2.97, and the natural moisture content was 0.3%.

[0049] Step 2: For the rockfill material with a maximum particle size of 60 mm obtained in step 1, triaxial wet deformation tests were carried out under different density and moisture content control. The tests used three confining pressure gradients, namely 500 kPa, 1500 kPa, and 2500 kPa. Stress level S l The values ​​are 0.2, 0.5, and 0.8. To reduce the test workload, based on the design porosity of 19% and the design fill moisture content of 1.9% in the upstream rockfill zone I, operating condition 1 is used to control the initial moisture content of the sample to 0%, and the rockfill porosity is set to 18%, 19%, and 20% respectively; operating condition 2 is used to control the test density to the fill design density of 19%, and the initial mass moisture content w is set to 1.2%, 1.9%, and 2.6% respectively. The detailed test plan is shown in Table 1 below:

[0050] Table 1

[0051]

[0052] Specimen preparation and test procedures were conducted in accordance with the triaxial wetting deformation test section of the "Test Procedure for Coarse-Grained Soils, T / CHES 29-1019." The specimens were cylindrical, 300 mm in diameter and 700 mm in height. Following preparation, a preset confining pressure was applied according to the test design. Consolidation was considered complete when the volume-versus-time curve approached the horizontal line. Axial stress was then applied to the appropriate stress level. The wetting shear strain and wetting volumetric strain of the rockfill specimens were immediately recorded. A stability criterion was a change in axial strain of less than 0.01% within 30 minutes. After stabilization of dry specimens or specimens with a certain moisture content, saturation was performed with a 2-meter head differential while maintaining the confining pressure and axial stress constant. The wetting deformation stability criterion also employed a change in axial strain of less than 0.01% within 30 minutes. The test was considered complete when deformation stabilized.

[0053] Finally, the curves of the wetting volume change and wetting shear strain obtained in step 2 over time are shown in the attached figure. Figure 3 、 Figure 4 The obtained wet deformation characteristics of rockfill materials vary with dry density and moisture content. Figure 5 、 Figure 6 , attached Figure 7 、 Figure 8 shown.

[0054] Step 3: Establish a correction formula based on the conventional wetting model that takes into account moisture content and density to describe the variation of the wetting deformation characteristics of rockfill materials with dry density and moisture content:

[0055] (1)

[0056] (2)

[0057] (3)

[0058] in, is the wetting shear strain, is the stress level; is the undetermined coefficient in the wetting shear strain model; is the undetermined index of the wetting shear strain model; K is the correction coefficient obtained from the experiment; is the humidified volume strain, is the wetting dilatancy ratio. Based on the wetting dilatancy ratio, the wetting volume change can be calculated through the wetting shear strain. Therefore, when making corrections, only the correction coefficient K of the wetting shear strain needs to be considered. is the wetting dilatancy ratio of rockfill The undetermined coefficient of is the stress ratio when the wetting dilatancy ratio is 0; p' is the average effective principal stress; p a is one atmosphere (101.2 kPa), used to make stress units dimensionless; m is the wetting dilatancy ratio The undetermined stress index; is the stress ratio, that is, the ratio of the deviatoric stress q to the average principal stress p; is the fitting parameter of the correction coefficient; is the effective water absorption rate (i.e., the moisture content above which no wetting deformation occurs even when the moisture content increases), obtained by fitting the data; is the designed porosity of the fill, i.e. the benchmark porosity for the wetting test study; is the moisture content of the rockfill material for which wetting deformation correction is to be predicted; The density of the rockfill material for which wetting deformation correction is to be predicted.

[0059] Step 4: Based on the wetting deformation characteristics of the rockfill material obtained from the triaxial wetting deformation test in Step 2, fit the formula parameters of the correction formula based on the conventional wetting model established in Step 3 that takes into account moisture content and density. The fitting process is as follows:

[0060] 1) Based on the working condition 1 in step 2, the initial moisture content of the sample is controlled to be 0%, the density is the fill design porosity of 19%, the simplification coefficient K=1, and the modified model is degraded to the conventional wetting model. The parameters in formula (1) are fitted by the nonlinear regression function of the statistical analysis software SSPS. 、 , the parameters in formula (2) 、 , m;

[0061] 2) Based on the fitting result of a, according to the working condition 1 in step 2, the initial moisture content of the sample is controlled to be 0%, and the initial density is 18%, 19%, and 21% for the wet deformation test of rockfill materials. The nonlinear regression function of the statistical analysis software SSPS is used to fit the parameters in formula (3): Among them, the shear strain fitting effect of the wetting test with different porosity is shown in the attached Figure 9 The dilatancy ratio fitting results of different wetting tests are shown in the appendix. Figure 10 As shown;

[0062] 3) Based on the working condition 2 in step 2, the control test density is 19% of the filling design density, the initial moisture content is 1.2%1.9.2.6 and the corresponding working condition 1 control test density is 19% of the filling design density, the initial moisture content is 0% of the rockfill triaxial wet deformation test and the parameter fitting results of 2) and 3), the parameters in formula (3) are fitted by the nonlinear regression function of the statistical analysis software SSPS. The fitting results of the humidification test with different moisture contents are shown in the attached Figure 11 、 Figure 12 shown.

[0063] Finally, the parameters of the wetting deformation correction model of the rockfill material in this engineering example are shown in Table 2:

[0064] Table 2

[0065]

[0066] The cumulative distribution histogram of moisture content and density of rockfill materials measured on site is shown in the attached figure. Figure 13 、 Figure 14 As shown in Figure 3, the actual moisture content and density of the rockfill material of the earth-rock dam that needs to be corrected for wetting deformation are substituted into formula (3) to obtain the correction coefficient K. For example, if the porosity at the site is 19.5% and the mass moisture content is 1%, then the wetting deformation correction coefficient K of this area is calculated as 0.63 by substituting it into formula (3). Then, formulas (1) and (2) can be used to complete the correction of the wetting deformation of the earth-rock dam based on the moisture content and density of the rockfill material measured on site.

[0067] The above-described embodiments merely express the implementation methods of the present invention, but should not be understood as limiting the scope of the present invention. It should be pointed out that those skilled in the art can make several modifications and improvements without departing from the concept of the present invention, which all fall within the scope of protection of the present invention.

Claims

1. A method for correcting the wetting deformation of earth-rockfill dams based on the moisture content and density of rockfill materials measured on site, characterized in that: The correction method comprises the following steps: Step 1: Select the rockfill materials from the main rockfill partition of the rockfill dam body, scale them down using the similar gradation method, and measure the specific gravity and natural moisture content of the scaled rockfill materials; Step 2: Conduct triaxial wetting deformation tests on the scaled rockfill materials at different densities and moisture contents to obtain the wetting deformation characteristics of the rockfill materials and the law of how the wetting deformation characteristics of the rockfill materials change with dry density and moisture content; Step 3: Establish a correction formula based on the conventional wetting model that takes into account moisture content and density to describe how the wetting deformation characteristics of rockfill materials change with dry density and moisture content; The correction formula includes a corrected wetting shear strain model, a corrected wetting volume strain model, and a calculation formula for a correction coefficient; Step 4: Based on the wetting deformation characteristics of the rockfill material obtained from the triaxial wetting deformation test in Step 2, the parameters of the correction formula established in Step 3 are fitted. Furthermore, the actual moisture content and density of the rockfill material for the earth-rockfill dam requiring wetting deformation correction are substituted into the correction coefficient calculation formula in Step 3 to obtain the correction coefficient K. The corrected wetting shear strain model and corrected wetting volume strain model from Step 3 are then used to correct the wetting deformation of the earth-rockfill dam based on the field-measured moisture content and density of the rockfill material, achieving accurate prediction of the wetting deformation in different dam body regions.

2. The method for correcting the wetting deformation of earth-rockfill dams based on on-site measurement of the moisture content and density of rockfill materials according to claim 1, characterized in that: In the first step, the maximum particle size after scaling is 60 mm.

3. The method for correcting the wetting deformation of earth-rockfill dams based on on-site measurements of the moisture content and density of rockfill materials according to claim 1, characterized in that: In the second step, when designing the triaxial wetting deformation test of rockfill materials with different densities and initial moisture contents under different working conditions, orthogonal design is not performed to reduce the test workload.

4. The method for correcting the wetting deformation of earth-rockfill dams based on on-site measurements of the moisture content and density of rockfill materials according to claim 1, characterized in that: In the second step, different working conditions include two main working conditions: Working condition 1 is to control the initial moisture content of the sample to 0%, and design low, medium and high levels and at least 3-5 density gradients for triaxial wetting deformation test of rockfill materials; Working condition 2 is to control the test density to the fill design density, and design low, medium and high levels and at least 3-5 moisture content gradients for triaxial wetting deformation test of rockfill materials.

5. The method for correcting the wetting deformation of earth-rockfill dams based on on-site measurement of the moisture content and density of rockfill materials according to claim 1, characterized in that: In the second step: the density index is determined according to the properties of the rockfill material. If the rockfill material is blasting material, the porosity or porosity ratio is used to control it; if the rockfill material is gravel, the compaction degree is used to control it; the moisture content is the mass moisture content.

6. The method for correcting the wetting deformation of earth-rockfill dams based on on-site measurements of the moisture content and density of rockfill materials according to claim 1, characterized in that: In the second step: the law of the change of the wet deformation characteristics of the rockfill material with dry density and moisture content is mainly the wet shear strain , Wetting Volume Strain , with the stress level , confining pressure (kPa), porosity n (%), water content (%) change pattern.

7. The method for correcting the wetting deformation of earth-rockfill dams based on on-site measurements of the moisture content and density of rockfill materials according to claim 4, characterized in that: In the third step, the corrected wetting shear strain model is shown in formula (1), the corrected wetting volume strain model is shown in formula (2), and the calculation formula of the correction coefficient is shown in formula (3); specifically: (1), (2), (3), in, is the wetting shear strain; is the stress level; is the undetermined coefficient in the wetting shear strain model; is the undetermined index of the wetting shear strain model; K is the correction coefficient obtained from the experiment; is the humidification volume strain; is the wetting dilatancy ratio; is the wetting dilatancy ratio of rockfill The undetermined coefficient of is the stress ratio when the wetting dilatancy ratio is 0; p' is the average effective principal stress; p a is atmospheric pressure; m is the humidification dilatancy ratio The undetermined stress index; is the stress ratio, that is, the ratio of the deviatoric stress q to the average principal stress p; is the fitting index of the correction coefficient; is the effective water absorption rate; is the designed porosity of the fill; is the moisture content of the rockfill material to be corrected for wetting deformation; Density of rockfill material to be corrected for wetting deformation.

8. The method for correcting the wetting deformation of earth-rockfill dams based on on-site measurements of the moisture content and density of rockfill materials according to claim 7, characterized in that: In the fourth step, the process of fitting parameters based on the modified formula taking into account moisture content and density based on the conventional humidification model is as follows: Step 4.1: Based on the working condition 1 in the second step, the initial moisture content of the sample is controlled to be 0%, the density is the fill design density, the simplification coefficient K=1, and the modified model is degraded to the conventional wetting model. The parameters in the fitting formula (1) are 、 , the parameters in formula (2) 、 , m; Step 4.2: Based on the fitting results of step 4.1, according to the working condition 1 in the second step, the initial moisture content of the sample is controlled to 0%, and the wet deformation test of rockfill materials with different densities is carried out, and the parameters in formula (3) are fitted. ; Step 4.3, based on the working condition 2 in the second step, the test density is controlled to be the filling design density, including the triaxial wetting deformation test of rockfill materials with low, medium and high levels and at least 3-5 moisture content gradients and the parameter fitting results of steps 4.2 and 4.3, and the parameters in formula (3) are fitted. .

Citation Information

Patent Citations

  • Test method for multi-stage dynamic loading accumulative deformation of subgrade soil under humidification

    CN110702541A

  • Humidification deformation three-parameter hyperbolic calculation model of built-in rigid wall body of earth and rockfill dam and calculation method of pull-down force of rigid wall body

    CN113191010A

  • Method for determining humidifying strain of rockfill material based on particle softening coefficient

    CN113484162A

  • Method for calculating and predicting core wall pore water pressure during construction period of high-core-wall earth and rockfill dam

    CN114970258A

  • High-soil core-wall rock-fill dam rock-fill investigation method for sand slate rock-fill material source

    CN117008211A