Defluorination, carbon removal and denitrification coupled recycling method and system for industrial strong brine
By employing two-stage chemical precipitation, electrocoagulation precipitation, and resin adsorption for fluoride removal, combined with primary active oxygen mineralization and sulfur autotrophic denitrification, the problem of efficient separation of pollutants and inorganic salts in industrial concentrated brine has been solved, achieving efficient resource utilization and low-cost treatment.
Patent Information
- Application Number
- CN202511088865.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-08-05
- Publication Date
- 2025-11-21
AI Technical Summary
Existing technologies are unable to efficiently separate pollutants and inorganic salts from concentrated industrial brine, resulting in high membrane system fouling rates, difficulty in ensuring the purity of crystalline salts, and a lack of efficient integrated solutions for hardening, fluoride removal, carbon removal, and nitrogen removal, leading to high treatment costs, large reagent consumption, large sludge production, and complex operation and maintenance.
The process employs two-stage chemical precipitation, electrocoagulation precipitation, and resin adsorption for fluoride removal, combined with primary active oxygen mineralization and sulfur autotrophic denitrification. Through nanofiltration salt separation, multi-stage active oxygen mineralization, electrodialysis concentration, and evaporation crystallization, it achieves efficient separation and resource utilization of pollutants and inorganic salts.
It achieves efficient separation and resource recovery of pollutants and target salts, reduces membrane fouling rate, improves the purity of crystalline salt, reduces pollutant emissions, and reduces operating costs through waste liquid recycling.
Smart Images

Figure CN120987496A_ABST
Abstract
Description
TECHNICAL FIELD
[0001] The present application relates to the technical field of wastewater resource utilization, and particularly relates to a resource utilization method and system for removing fluorine, carbon and nitrogen from industrial concentrated salt water. BACKGROUND
[0002] The power, petrochemical, steel, non-ferrous, papermaking, printing and dyeing, pesticide, pharmaceutical and other industries produce hundreds of millions of tons of high-salinity and refractory organic wastewater (industrial concentrated salt water) every year. Such wastewater has the characteristics of extremely high pollutant concentration (such as COD often exceeding 10,000 mg / L, containing phenol cyanide, polycyclic aromatic hydrocarbons, fluorides, heavy metals, etc.), complex composition, strong volatility, high salt content (5% to 20%, mainly Na + , Cl - , SO4 2- ), etc. These characteristics result in low efficiency of conventional biochemical treatment, difficulty in deep mineralization, and if direct evaporation and salt separation are used, a large amount of hazardous waste of mixed salt will be produced, which has high disposal cost and a risk of secondary pollution, seriously restricting the level of wastewater resource utilization. For example, the steel industry needs to break through the core technologies of coking wastewater deep treatment and reuse, cold rolling wastewater deep treatment and reuse, high-salinity wastewater elemental separation, wastewater zero discharge and resource utilization, the non-ferrous industry needs to break through the core technologies of non-ferrous smelting heavy metal wastewater deep treatment and reuse, high-salinity wastewater recovery and resource utilization in hydrometallurgy, heavy metal smelting waste acid wastewater resource utilization and treatment, and the petrochemical industry needs to break through the core technologies of coal chemical high-salinity wastewater elemental separation, high-salinity organic wastewater desalination and concentration evaporation, membrane method for low-cost industrial wastewater resource utilization, etc.
[0003] Industrial concentrated brine generated by various industries has complex composition, low biochemical stability, large amount of reagent consumption, and reverse osmosis membrane system fouling. To solve the above problems, relevant personnel take multi-stage AO microorganism strengthening, PACT gradient coupling reuse, ozone catalytic oxidation, membrane composite fouling prevention and cleaning as the core to carry out efficient wastewater treatment and reuse. However, for the high demand of fluorine-containing and refractory organic high-salt wastewater resource, microorganisms, physical and chemical technologies are numerous but not strongly coupled. The existing high fluorine-containing and refractory organic high-salt wastewater mainly uses three-alkali method, double-alkali method and resin method to remove fluorine, and hard silicon carbon combined with nanofiltration-reverse osmosis desalting and crystallization process. Although a certain degree of salt recovery can be achieved, there are still significant challenges. The core problem is that the pre-separation of organic matter, fluoride ions, total hardness, nitrate and other pollutants in concentrated water and target inorganic salt (such as NaCl and Na2SO4) cannot be efficiently and completely achieved, resulting in high fouling rate of the subsequent membrane system (such as nanofiltration and reverse osmosis), difficulty in ensuring the purity of crystalline salt (sodium chloride / sodium sulfate), and difficulty in controlling the impurity salt rate. In addition, the existing technical system often has poor coupling of various unit technologies such as microorganisms and physical and chemical technologies, and there are problems such as long process chain, large amount of reagent consumption (such as carbon source), high treatment cost, high greenhouse gas emission, large amount of sludge production, and complex operation and maintenance. Especially for high fluorine-containing and refractory organic high-salt wastewater, there is a lack of system solution that efficiently integrates and optimizes hardness removal, fluorine removal, carbon (mineralized organic matter) removal, and denitrification.
[0004] Therefore, a solution is needed to efficiently separate pollutants and inorganic salt from industrial concentrated brine, reduce membrane fouling, ensure the purity of crystalline salt, control the impurity salt rate, and ultimately achieve efficient resource utilization of crystalline salt and water in industrial concentrated brine, while significantly reducing pollutant emissions. SUMMARY
[0005] Therefore, the present application provides an industrial concentrated brine fluorine removal, carbon removal and denitrification coupled resource utilization method and system, which solves the problem of how to utilize the resources of crystalline salt and water in industrial concentrated brine and reduce pollutant emissions.
[0006] To achieve the above technical purposes, the present application adopts the following technical solutions: In a first aspect, the present application provides an industrial concentrated brine fluorine removal, carbon removal and denitrification coupled resource utilization method, comprising the following steps: S1. The industrial concentrated brine is sequentially subjected to two-stage chemical precipitation, electrocoagulation precipitation and resin adsorption to remove fluorine to obtain active oxygen pretreated water; S2. The active oxygen pretreated water is subjected to one-stage active oxygen mineralization and chemical precipitation treatment to obtain decarburized nitrated water; S3. The decarburized nitrated water is subjected to sulfur autotrophic denitrification to remove nitrogen, and after filtration, denitrified water is obtained; S4. The denitrified water is subjected to nanofiltration desalting to obtain nanofiltration water and nanofiltration concentrated water; S5. The nanofiltration water and the nanofiltration concentrated water are subjected to secondary active oxygen mineralization, concentration and crystallization, respectively, to obtain sodium chloride and sodium sulfate, respectively; The waste liquid generated in step S5 is reused for the primary active oxygen mineralization treatment, and the clean water is combined and discharged as the reuse water.
[0007] Preferably, the primary active oxygen mineralization adopts a multi-channel parallel electrochemical oxidation process.
[0008] Preferably, the specific operation of step S1 is as follows: S11. The industrial concentrated brine is subjected to primary fluoride and hardness removal treatment through two-stage chemical precipitation to obtain precipitated purified water; S12. The precipitated purified water is subjected to secondary fluoride and hardness removal treatment through electric flocculation precipitation, multi-medium filtration and resin adsorption fluoride removal in sequence to obtain active oxygen pretreated water.
[0009] Preferably, the specific operation of step S5 is as follows: The nanofiltration water is subjected to secondary active oxygen mineralization, electrodialysis concentration and evaporation crystallization to obtain sodium chloride; The nanofiltration concentrated water is subjected to secondary active oxygen mineralization, evaporation concentration, freeze crystallization and melt recrystallization to obtain sodium sulfate; The mother liquor after evaporation crystallization and freeze crystallization is subjected to miscellaneous salt crystallization to obtain miscellaneous salt and miscellaneous salt liquid, and the miscellaneous salt liquid and the freeze waste liquid generated in the freeze crystallization are reused as waste liquid for the primary active oxygen mineralization treatment; The water produced by the electrodialysis concentration, the evaporation crystallization, the evaporation concentration and the melt recrystallization is discharged as clean water and combined as reuse water.
[0010] Preferably, the system further comprises the step of collecting the precipitate generated in the two-stage chemical precipitation, the electric flocculation precipitation and the primary active oxygen mineralization for preparing a sludge-based environmental functional material.
[0011] Preferably, in step S1, the two-stage chemical precipitation comprises the following steps: adding lime, soda ash and coagulant PAC to the industrial concentrated brine, and then adding flocculant PAM to perform primary chemical precipitation to obtain primary effluent; adding fluoride removal agent and coagulant PAC to the primary effluent, and then adding flocculant PAM to perform secondary chemical precipitation to obtain precipitated purified water.
[0012] Preferably, the step of the primary active oxygen mineralization is as follows: taking an electrode basket filled with a transition metal-based composite material loaded on active coke / activated carbon as a working unit, and taking a graphite rod as a cathode and an anode to perform electrochemical oxidation.
[0013] In a second aspect, the application provides an industrial concentrated brine fluoride and carbon removal and denitrification coupled resource system, comprising: A multi-stage fluoride and hardness removal unit is configured to sequentially perform two-stage chemical precipitation, electric flocculation precipitation and resin adsorption fluoride removal on the industrial concentrated brine to output active oxygen pretreated water; The active oxygen mineralization unit is used to perform primary active oxygen mineralization and chemical precipitation treatment on the active oxygen pretreated water, and output decarbonized nitrified water. The denitrification filtration unit is used to perform sulfur autotrophic denitrification and filtration on decarbonated nitrified water, and output denitrified water. The salt separation unit is used to perform nanofiltration salt separation on denitrified water and output nanofiltration permeate and nanofiltration concentrate. The crystallization unit includes parallel sodium chloride crystallization components and sodium sulfate crystallization components. The sodium chloride crystallization components are used for secondary active oxygen mineralization, electrodialysis concentration and evaporation crystallization of nanofiltration permeate. The sodium sulfate crystallization components are used for secondary active oxygen mineralization, evaporation concentration, freeze crystallization and melt recrystallization of nanofiltration concentrate. The waste liquid of the crystallization unit is returned to the primary active oxygen mineralization unit, and the clean permeate is combined as reclaimed water and discharged.
[0014] Preferably, the primary active oxygen mineralization component of the active oxygen mineralization unit includes multiple primary active oxygen mineralization pools connected in parallel.
[0015] Preferably, the crystallization unit further includes a mixed salt crystallization unit, which is used to collect the mother liquor from freeze crystallization and evaporation crystallization for mixed salt crystallization, and input the generated waste liquid into the primary active oxygen mineralization unit. The beneficial effects of this application are as follows: This application combines hardening removal, fluoride removal, carbon removal, nitrogen removal, wastewater reuse, and salt separation and crystallization into a process combination, achieving efficient separation and resource recovery of pollutants and target salts. By placing the electrochemical-based primary activated oxygen mineralization after the targeted deep fluoride and hardening removal steps, electrode corrosion is minimized, while residual ammonia nitrogen in wastewater is efficiently converted into nitrate nitrogen, completing the carbon removal and nitrification steps. By placing the sulfur autotrophic denitrification process downstream of the activated oxygen mineralization unit, efficient nitrogen removal is achieved through microbial autotrophic metabolism using the nitrate nitrogen generated in the previous step without the need for an external organic carbon source. This approach avoids the problems of long denitrification process pathways and carbon source constraints associated with traditional denitrification methods. This system addresses issues such as high reagent dosage, high treatment costs, high greenhouse gas emissions, large sludge volume, and difficult operation and maintenance. Simultaneously, it ensures the denitrification system is not inhibited by high COD concentrations, achieving efficient and thorough pre-separation of concentrated organic matter, fluoride ions, total hardness, nitrates, etc., from inorganic by-product salts. Further secondary activated oxygen mineralization treatment of the concentrated water and permeate generated by the nanofiltration desalination system effectively solves the problem of pollution concentration ratio. Furthermore, by using series electrodialysis concentration and evaporation crystallization for sodium chloride recovery, and evaporation concentration, freeze crystallization, and melt recrystallization for sodium sulfate purification, the impurity salt rate is controlled, improving the purity of the final salt product and reducing operating costs.
[0016] This application collects sludge generated during defluorination, hardening, and primary oxygen mineralization to prepare sludge-based environmental functional materials. By reusing the wastewater generated during concentration and crystallization into primary oxygen mineralization treatment, and combining the clean water into reclaimed water for discharge, this application achieves waste treatment and resource utilization. Attached Figure Description
[0017] Figure 1 This is a schematic diagram of the system in this application. Detailed Implementation
[0018] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to embodiments. It should be understood that the specific embodiments described herein are merely illustrative and not intended to limit the invention.
[0019] This application provides a resource recovery method for the coupled removal of fluoride, carbon, and nitrogen from industrial concentrated brine, comprising the following steps: S1. Industrial concentrated brine is subjected to two-stage chemical precipitation, electrocoagulation precipitation and resin adsorption to remove fluoride, to obtain oxygen-pretreated water. S2. The pretreated water is subjected to primary oxygen mineralization and chemical precipitation to obtain decarbonized nitrified water; S3. The decarbonized nitrified water is subjected to sulfur autotrophic denitrification to remove nitrogen, and after filtration, denitrified water is obtained; S4. Perform nanofiltration to separate the denitrified water and obtain nanofiltration permeate and nanofiltration concentrate; S5. Nanofiltration permeate and nanofiltration concentrate are subjected to two-stage active oxygen mineralization, concentration and crystallization to obtain sodium chloride and sodium sulfate respectively. The waste liquid generated in step S5 is recycled to the primary active oxygen mineralization treatment, and the clean water is combined into recycled water for discharge.
[0020] The resource utilization method of coupled defluorination, decarbonization and denitrification of industrial concentrated brine in this application efficiently separates pollutants from inorganic salts, resulting in high purity of crystalline salts, less polluted water discharge, and low membrane fouling rate. This realizes the resource utilization of crystalline salts and water in industrial concentrated brine and reduces the amount of pollutant emissions.
[0021] In step S1, the Ca content is reduced through two-stage chemical precipitation. 2+ Mg 2+ The concentration of fluoride ions and organic matter is then reduced, followed by electrocoagulation precipitation to form large amounts of aluminum hydroxide and iron hydroxide. Fluorides, calcium and magnesium ions, and organic matter are further removed using sweeping flocculation, charged colloids of hydrolysis products, microbubble flotation scraping, and PAC / PAM coagulation sedimentation. Afterward, resin adsorption is used for deep defluorination to obtain oxygenated pretreated water, preventing the inability to perform primary oxygenation mineralization using conventional methods such as calcium ion defluorination. The electrocoagulation precipitation mainly involves the following reactions: Anode reaction: Fe→Fe 2+ +2e - 4Fe 2+ +O₂ + 10H₂O → 4Fe(OH)₃↓ + 8H₂O + Fe 2+ +2OH - →Fe(OH)2↓ Al→Al 3+ +3e - 2H2O-4e - →O2+4H + Cathode reaction: 2H2O+2e - →H2+2OH - 2Al + 6H₂O + 2OH⁻ - →3Al(OH)4 - +3H2 3Al(OH)4 - →Al(OH)3↓+OH - ; In step S2, the pretreated water undergoes primary oxygen mineralization, which efficiently oxidizes and degrades COD and ammonia nitrogen, greatly improving the mineralization rate. Ammonia nitrogen is converted into nitrate nitrogen, resulting in decarbonized nitrified water. In step S3, the decarbonized nitrified water undergoes sulfur autotrophic denitrification and is then subjected to multi-stage filtration to remove nitrate, suspended solids, colloids, organic matter, PAC, and PAM, resulting in denitrified water. In step S4, the denitrified water enters a nanofiltration membrane separation system to achieve efficient separation of divalent salts such as sodium sulfate and monovalent salts such as sodium chloride. In step S5, the nanofiltration concentrate and the nanofiltration concentrate generate corresponding crystalline salts, enabling the recycling of wastewater and the discharge of clean permeate.
[0022] This application combines hardening removal, fluoride removal, carbon removal, nitrogen removal, wastewater reuse, and salt separation and crystallization into a process combination, achieving efficient separation and resource recovery of pollutants and target salts. By placing the electrochemical-based primary activated oxygen mineralization after the targeted deep fluoride and hardening removal steps, electrode corrosion is minimized, while residual ammonia nitrogen in wastewater is efficiently converted into nitrate nitrogen, completing the carbon removal and nitrification steps. By placing the sulfur autotrophic denitrification process downstream of the activated oxygen mineralization unit, efficient nitrogen removal is achieved through microbial autotrophic metabolism using the nitrate nitrogen generated in the previous step without the need for an external organic carbon source. This approach avoids the problems of long denitrification process pathways and carbon source constraints associated with traditional denitrification methods. This system addresses issues such as high reagent dosage, high treatment costs, high greenhouse gas emissions, large sludge volume, and difficult operation and maintenance. Simultaneously, it ensures the denitrification system is not inhibited by high COD concentrations, achieving efficient and thorough pre-separation of concentrated organic matter, fluoride ions, total hardness, nitrates, etc., from inorganic by-product salts. Further secondary activated oxygen mineralization treatment of the concentrated water and permeate generated by the nanofiltration desalination system effectively solves the problem of pollution concentration ratio. Furthermore, by using series electrodialysis concentration and evaporation crystallization for sodium chloride recovery, and evaporation concentration, freeze crystallization, and melt recrystallization for sodium sulfate purification, the impurity salt rate is controlled, improving the purity of the final salt product and reducing operating costs.
[0023] In addition, this application collects sludge generated during defluorination, hardening and primary oxygen mineralization to prepare sludge-based environmental functional materials, and reuses the waste liquid generated during concentration and crystallization to primary oxygen mineralization treatment, and combines the clean water into recycled water for discharge, thus realizing waste treatment and resource utilization.
[0024] In some embodiments, primary active oxygen mineralization employs a multi-channel parallel electrochemical oxidation process.
[0025] In this embodiment, setting up a multi-channel primary active oxygen mineralization treatment branch according to the sewage flow rate is beneficial to improving efficiency and mineralization rate.
[0026] In some embodiments, step S1 specifically involves the following steps: S11. Industrial concentrated brine is subjected to a first-stage defluorination and hardness removal treatment through two-stage chemical precipitation to obtain purified precipitated water; S12. The precipitated purified water is sequentially passed through electrocoagulation sedimentation, multi-media filtration and resin adsorption for defluorination, and then subjected to two-stage defluorination and hardening treatment to obtain oxygen-pretreated water.
[0027] In this embodiment, the Ca content is first reduced through a primary defluorination and hardening treatment. 2+ Mg 2+ The concentration of fluoride ions and organic matter is then determined, and the effluent undergoes a secondary defluorination and hardening treatment to remove calcium from the water. 2+ Mg 2+The concentrations of fluoride ions and organic matter are further reduced to levels acceptable for primary oxygen mineralization to avoid electrode corrosion problems during long-term operation of subsequent primary and secondary oxygen mineralization.
[0028] In some embodiments, step S5 specifically involves: nanofiltration permeate undergoing secondary active oxygen mineralization, electrodialysis concentration, and evaporation crystallization to obtain sodium chloride; nanofiltration concentrate undergoing secondary active oxygen mineralization, evaporation concentration, freeze crystallization, and melt recrystallization to obtain sodium sulfate; the mother liquor after evaporation crystallization and freeze crystallization is subjected to mixed salt crystallization to obtain mixed salt and mixed salt solution; the mixed salt solution and the freeze waste liquid generated by freeze crystallization are reused as waste liquid in primary active oxygen mineralization treatment; the permeate from electrodialysis concentration, permeate from evaporation crystallization, permeate from evaporation concentration, and permeate from melt recrystallization are used as clean permeate and combined as reclaimed water for discharge.
[0029] In some embodiments, the method further includes the step of collecting the precipitates generated from two-stage chemical precipitation, electrocoagulation precipitation, and primary active oxygen mineralization for the preparation of sludge-based environmental functional materials.
[0030] In this embodiment, by adding a step to collect sediment, the waste utilization of pollutants can be realized. The sludge-based environmental functional material uses sludge as the formula base, urban domestic sludge with negative raw material costs as an auxiliary ingredient, and biomass such as straw and wood chips as a heat source and to provide a connected pore structure. The solid waste content of the three exceeds 97%.
[0031] In some embodiments, step S1 includes the following steps: adding lime, soda ash and coagulant PAC to industrial concentrated brine, and then adding flocculant PAM to carry out primary chemical precipitation to obtain primary effluent; adding defluoridating agent and coagulant PAC to the primary effluent, and then adding flocculant PAM to carry out secondary chemical precipitation to obtain purified precipitated water.
[0032] In this embodiment, the two-stage coupled (TS) high-density sedimentation tank follows the rule that the lower the final effluent concentration of pollutants, the higher the reagent dosage. It also integrates the advantages of mixing, flocculation, sedimentation, and sludge thickening. The two-stage chemical precipitation treatment helps to save on reagents.
[0033] In some embodiments, the primary activated oxygen mineralization step is as follows: using an electrode basket filled with activated coke / activated carbon-supported transition metal matrix composite material as the working unit, and a graphite rod as the cathode and anode, electrochemical oxidation is performed.
[0034] In this embodiment, the electrode basket has good conductivity and many pores, which is conducive to the deep removal of residual COD and hardness.
[0035] like Figure 1As shown, this application provides a resource recovery system for coupled defluorination, decarbonization, and denitrification of industrial concentrated brine, comprising: a multi-stage defluorination and dehardening unit for sequentially performing two-stage chemical precipitation, electrocoagulation precipitation, and resin adsorption defluorination on industrial concentrated brine, outputting oxygen-pretreated water; an oxygen mineralization unit for performing primary oxygen mineralization and chemical precipitation on the oxygen-pretreated water, outputting decarbonized nitrified water; a denitrification filtration unit for performing sulfur autotrophic denitrification and filtration on the decarbonized nitrified water, outputting denitrified water; a salt separation unit for performing nanofiltration salt separation on the denitrified water, outputting nanofiltration permeate and nanofiltration concentrate; and a crystallization unit comprising parallel sodium chloride crystallization and sodium sulfate crystallization components. The sodium chloride crystallization component is used for secondary oxygen mineralization, electrodialysis concentration, and evaporation crystallization on the nanofiltration permeate; the sodium sulfate crystallization component is used for secondary oxygen mineralization, evaporation concentration, freeze crystallization, and melt recrystallization on the nanofiltration concentrate; the waste liquid from the crystallization unit is returned to the primary oxygen mineralization unit, and the clean permeate is combined as reclaimed water for discharge.
[0036] This application's multi-stage defluoridation and defluoridation unit includes a series-connected equalization tank, a TS high-density sedimentation tank, an integrated electrocoagulation sedimentation machine, a multi-media filter, and a resin defluoridation system. It is used to sequentially treat industrial concentrated brine through two stages of chemical precipitation, electrocoagulation sedimentation, and resin adsorption defluoridation, outputting pre-treated water with activated oxygen. Specifically, a mixture of concentrated wastewater from multiple industries (chlor-alkali, chemical, and steel) in an industrial cluster is pumped into the equalization tank as industrial concentrated brine, and then subjected to sedimentation treatment in a two-stage coupled (TS) high-density sedimentation tank. The influent surface loading of the TS high-density sedimentation tank is set at 7.5~12 m³. 3 / (m 2 (h) The sludge return ratio is controlled at 3-5%. Lime, soda ash, and coagulant PAC are added to the primary mixing tank; flocculant PAM is added to the primary flocculation tank; defluoridating agent and coagulant PAC are added to the secondary mixing tank; and flocculant PAM is added to the secondary flocculation tank, so that Ca... 2+ Mg 2+ The concentrations of fluoride ions and organic matter are significantly reduced. Simultaneously, the TS high-density sedimentation tank and electrocoagulation sedimentation integrated machine are equipped with an output port connected to the sludge-based environmental functional material preparation system, allowing for resource-based treatment of the generated sludge. The electrocoagulation sedimentation integrated machine mainly consists of electrolytic flocculation, microbubble flotation, a scraper, and a sedimentation module. The anode is made of Fe, Al, stainless steel, or graphite, while the cathode is made of Al rods, stainless steel, or graphite. The electrodes are reversed every 5-10 minutes. The resin defluorination system is primarily composed of macroporous cross-linked polystyrene, operating at temperatures below 60°C, with a pH control of 4-9 and a regeneration time of 30-60 minutes.
[0037] The activated oxygen mineralization unit includes a primary activated oxygen mineralization tank group and a high-density sedimentation tank. The inlet of the primary activated oxygen mineralization tank group is connected to the outlet of the resin defluoridation system, used for primary activated oxygen mineralization and chemical precipitation treatment of the activated oxygen pretreated water, outputting decarbonized nitrified water. The high-density sedimentation tank adds PAM at a concentration of 0.8~1.2 ppm, and PAC is determined according to water quality, ranging from 20~1000 ppm. The processing rate of a single mineralization tank in the primary activated oxygen mineralization tank group is 7.5~30 t / h, and the volumetric current density is 150~250 A / m³. 3 The activated oxygen mineralization tank is equipped with an output port connected to the sludge-based environmental functional material preparation system, which then processes the generated sludge-based environmental functional material preparation system for resource utilization.
[0038] The denitrification and filtration unit includes a sulfur autotrophic denitrification reactor and a filtration assembly. The inlet of the sulfur autotrophic denitrification reactor is connected to the outlet of the high-density sedimentation tank. It is used for sulfur autotrophic denitrification and filtration of the decarbonization nitrification water, outputting denitrified water. The pH of the sulfur autotrophic denitrification reaction is controlled at 6.5~8.2, and the denitrification load is 0.8 kgN / (m³). 3 •d) and above; the filtration components include a self-cleaning filter, a multi-media filter, and an ultrafiltration unit connected in sequence; the decarbonized nitrified water undergoes extreme denitrification in a sulfur autotrophic denitrification reactor, followed by a self-cleaning filter, a multi-media filter, and an ultrafiltration unit to progressively improve and remove nitrates, suspended solids, colloids, organic matter, PAC, PAM, and ions, and then enters a nanofiltration membrane separation system to achieve efficient separation of divalent salts such as sodium sulfate and monovalent salts such as sodium chloride.
[0039] The salt separation unit includes a nanofiltration salt separation system, whose inlet is connected to the outlet of the filter assembly. It performs nanofiltration salt separation on the denitrified water, separating monovalent salts and divalent salts, and outputs nanofiltration permeate and nanofiltration concentrate. The nanofiltration salt separation system controls the recovery rate to 80%±5%, and the membrane housing adopts a 6-core configuration with a capacity of 450~600 Psi.
[0040] The crystallization unit includes a mixed salt crystallization unit, a parallel sodium chloride crystallization assembly (for treating nanofiltration permeate), and a sodium sulfate crystallization assembly (for treating nanofiltration concentrate). Because the salt concentration of nanofiltration permeate is relatively low and direct evaporation crystallization is costly, the sodium chloride crystallization assembly comprises a two-stage activated oxygen mineralization tank, an electrodialysis concentration unit, and an evaporator crystallizer connected in sequence, used to treat nanofiltration permeate to obtain sodium chloride. The sodium sulfate crystallization assembly comprises a two-stage activated oxygen mineralization tank, a triple-effect pre-concentration unit, a freeze crystallization unit, and a melt recrystallization unit connected in sequence, used to treat nanofiltration concentrate and dry it into industrial-grade sodium sulfate product. The mother liquor outlet from the evaporation crystallization unit is connected to the mixed salt crystallization unit, and the cold... The mother liquor outlet of the frozen crystallization unit is connected to the mixed salt crystallization unit. After the mother liquor from the frozen crystallization and evaporation crystallization undergoes mixed salt crystallization, a mixed salt solution is obtained. The outlet of the mixed salt crystallization unit is connected to the primary active oxygen mineralization unit, and the mixed salt solution is returned to the primary active oxygen deep mineralization system for purification. The frozen waste liquid outlet of the frozen crystallization unit is connected to the primary active oxygen mineralization unit, and the frozen waste liquid is returned to the primary active oxygen deep mineralization system for purification. The electrodialysis concentration unit, evaporation crystallization unit, triple-effect pre-concentration unit, and melt recrystallization unit are all equipped with outlets for discharging clean permeable water. The permeable water obtained from the triple-effect pre-concentration unit and the melt recrystallization unit is reused.
[0041] Among them, the electrodialysis unit concentrates salt solutions such as sodium chloride (below 5%) to 15-20%, with a maximum operating current of 200A and a maximum power of 50-150 kW; the triple-effect pre-concentration unit has a sodium sulfate concentration of over 20%, a freezing crystallization control temperature range of -5℃ to 5℃, and a residence time of over 4 hours; the sludge-based environmental functional material preparation system has a daily processing capacity of no less than 10t / d, a material water storage coefficient of 55-90%, and a waste heat recovery rate of over 35%.
[0042] In some embodiments, the primary active oxygen mineralization component of the active oxygen mineralization unit includes a plurality of primary active oxygen mineralization pools connected in parallel.
[0043] In this embodiment, the activated oxygen mineralization unit is equipped with n (n≥1, the value is determined according to the sewage flow rate) groups of primary activated oxygen deep mineralization tanks. The type is plastic basket electrode, and both the anode and cathode are graphite rods. The basket is filled with activated coke, coal-based activated carbon or other types of granular activated carbon-based flow-collecting composite materials with good conductivity and well-developed pore structure. Then, it enters the high-density sedimentation tank, and PAC, PAM, hardening agent, etc. are added to achieve deep removal of residual COD and hardness. After the n groups of primary activated oxygen deep mineralization tanks are connected in parallel, a primary activated oxygen mineralization component is obtained. The inlet of the primary activated oxygen mineralization component is connected to the outlet of the resin defluorination system, and the outlet of the primary activated oxygen mineralization component is connected to the inlet of the high-density sedimentation tank.
[0044] In some embodiments, the crystallization unit further includes a mixed salt crystallization unit for collecting the mother liquor from freeze crystallization and evaporation crystallization to crystallize mixed salts, and inputting the generated waste liquid into the primary active oxygen mineralization unit.
[0045] In this embodiment, by adding a mixed salt crystallization unit as an intermediary to collect the mother liquor from freeze crystallization and evaporation crystallization, the amount of mixed salt is further increased, and the content of mixed salt in the waste liquid is reduced to reduce the damage to the primary active oxygen mineralization unit.
[0046] The following specific embodiments further illustrate this solution.
[0047] Example 1 A resource recovery method for coupled defluorination, decarbonization, and denitrification of industrial concentrated brine includes the following steps: S1. Add lime, soda ash, and coagulant PAC to industrial concentrated brine, followed by flocculant PAM for primary chemical precipitation to obtain primary effluent; add defluoridating agent and coagulant PAC to the primary effluent, followed by flocculant PAM for secondary chemical precipitation to obtain purified precipitated water; pass the purified precipitated water sequentially through electrocoagulation sedimentation (electrode reversed every 5 minutes), multi-media filtration, and resin adsorption defluorination (operating temperature 60℃, pH 4, regeneration time 30 minutes) for secondary defluorination and hardness removal to obtain activated oxygen pretreated water; S2. A multi-channel parallel electrochemical oxidation process is adopted, using an electrode basket filled with activated coke / activated carbon supported by a transition metal matrix composite as the working unit, and graphite rods as the cathode and anode (the size of a single electrode basket is 0.116m). 3 The effective volume is 1.51m³. 3 Volume current density 249 A / m 3 (Total current 375A, operating voltage 9.8V), after mineralization, PAC (20 ppm) and PAM (0.8 ppm) are added for chemical precipitation to obtain decarbonized nitrified water; S3. The decarbonized nitrified water is subjected to sulfur autotrophic denitrification (pH 7.4, denitrification load 1.2 kgN / (m³)). 3 ·d), and then through self-cleaning filtration, multi-media filtration and ultrafiltration for step-by-step quality improvement, denitrified water is obtained; S4. Perform nanofiltration to separate salts from the denitrified water (recovery rate 80%±5%, operating pressure 450 Psi) to obtain nanofiltration permeate (containing monovalent salts) and nanofiltration concentrate (containing divalent salts). S5. Nanofiltration permeate undergoes two-stage activated oxygen mineralization (single electrode basket size is 0.116m). 3 The effective volume is 1.51m³. 3 Volume current density 150 A / m 3The process involves several steps: 1) Electrodialysis concentration (concentrating a 5% salt solution to 15%) and evaporation crystallization to obtain sodium chloride; 2) Nanofiltration concentrate undergoing secondary active oxygen mineralization, triple-effect pre-concentration (sodium sulfate concentration ≥20%), freeze crystallization (-5℃, residence time 4h), and melt recrystallization to obtain sodium sulfate; 3) The mother liquor from evaporation crystallization and freeze crystallization is subjected to mixed salt crystallization to obtain mixed salt and mixed salt solution; 4) The mixed salt solution and freeze-crystallized wastewater are recycled to primary active oxygen mineralization treatment; 5) Electrodialysis concentrate, evaporation crystallization concentrate, evaporation concentrate, and melt recrystallization concentrate are treated as clean water and combined as recycled water for discharge; 6) The precipitates from two-stage chemical precipitation, electrocoagulation precipitation, and primary active oxygen mineralization are collected and used in conjunction with municipal sludge and biomass (straw / wood chips) to prepare sludge-based environmental functional materials (solid waste content ≥97%, water storage coefficient 55~90%).
[0048] Example 2 A resource recovery method for coupled defluorination, decarbonization, and denitrification of industrial concentrated brine includes the following steps: S1. Add lime, soda ash, and coagulant PAC to industrial concentrated brine, followed by flocculant PAM for primary chemical precipitation to obtain primary effluent; add defluoridating agent and coagulant PAC to the primary effluent, followed by flocculant PAM for secondary chemical precipitation to obtain purified precipitated water; pass the purified precipitated water sequentially through electrocoagulation sedimentation (electrode reversal every 10 minutes), multi-media filtration, and resin adsorption defluorination (operating temperature 50℃, pH 9, regeneration time 60 minutes) for secondary defluorination and hardness removal to obtain activated oxygen pretreated water; S2. A multi-channel parallel electrochemical oxidation process is adopted, using an electrode basket filled with activated coke / activated carbon supported by a transition metal matrix composite as the working unit, and graphite rods as the cathode and anode (the size of a single electrode basket is 0.116m). 3 The effective volume is 1.51m³. 3 Volume current density 249 A / m 3 (Total current 375A, operating voltage 9.8V), after mineralization, PAC (1000 ppm) and PAM (1.2 ppm) are added for chemical precipitation to obtain decarbonized nitrified water; S3. The decarbonized nitrified water is subjected to sulfur autotrophic denitrification (pH 7.4, denitrification load 1.7 kgN / (m³)). 3 ·d), and then through self-cleaning filtration, multi-media filtration and ultrafiltration for step-by-step quality improvement, denitrified water is obtained; S4. Perform nanofiltration to separate salts from the denitrified water (recovery rate 80%±5%, operating pressure 600 Psi) to obtain nanofiltration permeate (containing monovalent salts) and nanofiltration concentrate (containing divalent salts). S5. Nanofiltration permeate undergoes two-stage activated oxygen mineralization (single electrode basket size is 0.116m).3 The effective volume is 1.51m³. 3 Volume current density 150 A / m 3 The process involves several steps: 1) Electrodialysis concentration (concentrating a 5% salt solution to 20%) and evaporation crystallization to obtain sodium chloride. 2) Nanofiltration concentrate undergoes secondary active oxygen mineralization, triple-effect pre-concentration (sodium sulfate concentration ≥20%), freeze crystallization (-5℃, residence time 6h), and melt recrystallization to obtain sodium sulfate. 3) The mother liquor from evaporation crystallization and freeze crystallization is subjected to mixed salt crystallization to obtain mixed salt and mixed salt solution. The mixed salt solution and the freeze-crystallized wastewater are recycled to primary active oxygen mineralization treatment. 4) Electrodialysis concentrate, evaporation crystallization concentrate, evaporation concentrate, and melt recrystallization concentrate are treated as clean water and combined as recycled water for discharge. 5) The precipitates from two stages of chemical precipitation, electrocoagulation precipitation, and primary active oxygen mineralization are collected and used in conjunction with municipal sludge and biomass (straw / wood chips) to prepare sludge-based environmental functional materials (solid waste content ≥97%, water storage coefficient 55~90%).
[0049] Example 3 A resource recovery method for coupled defluorination, decarbonization, and denitrification of industrial concentrated brine includes the following steps: S1. Add lime, soda ash, and coagulant PAC to industrial concentrated brine, followed by flocculant PAM for primary chemical precipitation to obtain primary effluent; add defluoridating agent and coagulant PAC to the primary effluent, followed by flocculant PAM for secondary chemical precipitation to obtain purified precipitated water; pass the purified precipitated water sequentially through electrocoagulation sedimentation (electrode reversed every 8 minutes), multi-media filtration, and resin adsorption defluorination (operating temperature 40℃, pH 6, regeneration time 40 minutes) for secondary defluorination and hardness removal to obtain oxygenated pretreated water; S2. A multi-channel parallel electrochemical oxidation process is adopted, using an electrode basket filled with activated coke / activated carbon supported by a transition metal matrix composite as the working unit, and graphite rods as the cathode and anode (the size of a single electrode basket is 0.116m). 3 The effective volume is 1.51m³. 3 Volume current density 249 A / m 3 (Total current 375A, operating voltage 9.8V), after mineralization, PAC (500 ppm) and PAM (1.0 ppm) are added for chemical precipitation to obtain decarbonized nitrified water; S3. The decarbonized nitrified water is subjected to sulfur autotrophic denitrification (pH 7.4, denitrification load 2.0 kgN / (m³)). 3 ·d), and then through self-cleaning filtration, multi-media filtration and ultrafiltration for step-by-step quality improvement, denitrified water is obtained; S4. Perform nanofiltration to separate salts from the denitrified water (recovery rate 80%±5%, operating pressure 500 Psi) to obtain nanofiltration permeate (containing monovalent salts) and nanofiltration concentrate (containing divalent salts). S5. Nanofiltration permeate undergoes two-stage activated oxygen mineralization (single electrode basket size is 0.116m). 3 The effective volume is 1.51m³. 3 Volume current density 150 A / m 3 The process involves several steps: 1) Electrodialysis concentration (concentrating a 5% salt solution to 18%) and evaporation crystallization to obtain sodium chloride; 2) Nanofiltration concentrate undergoing secondary active oxygen mineralization, triple-effect pre-concentration (sodium sulfate concentration ≥20%), freeze crystallization (0℃, residence time 8h), and melt recrystallization to obtain sodium sulfate; 3) The mother liquor from evaporation crystallization and freeze crystallization is subjected to mixed salt crystallization to obtain mixed salt and mixed salt solution; 4) The mixed salt solution and freeze-crystallized wastewater are recycled to primary active oxygen mineralization treatment; 5) Electrodialysis concentrate, evaporation crystallization concentrate, evaporation concentrate, and melt recrystallization concentrate are treated as clean water and combined as recycled water for discharge; 6) The precipitates from two-stage chemical precipitation, electrocoagulation precipitation, and primary active oxygen mineralization are collected and used in conjunction with municipal sludge and biomass (straw / wood chips) to prepare sludge-based environmental functional materials (solid waste content ≥97%, water storage coefficient 55~90%).
[0050] Example 4 A resource recovery system for coupled defluorination, carbon removal, and nitrogen removal of industrial concentrated brine includes: Multi-stage defluorination and hardening removal units, including a series-connected equalization tank and a TS high-density sedimentation tank (surface loading 7.5~12 m³). 3 / (m 2 •h), sludge return ratio 3~5%), electrocoagulation sedimentation integrated machine, multi-media filter, macroporous cross-linked polystyrene resin defluorination system, TS high-density sedimentation tank, sludge discharge outlet of electrocoagulation sedimentation integrated machine connected to sludge-based environmental functional material preparation system; The activated oxygen mineralization unit includes a primary activated oxygen mineralization tank group and a high-density sedimentation tank; n groups of primary activated oxygen deep mineralization tanks are connected in parallel to obtain a primary activated oxygen mineralization component. The inlet of the primary activated oxygen mineralization component is connected to the outlet of the resin defluorination system, and the outlet of the primary activated oxygen mineralization component is connected to the inlet of the high-density sedimentation tank. The inlet of the primary activated oxygen mineralization tank group is connected to the outlet of the resin defluorination system. The output port of the activated oxygen mineralization unit is connected to the sludge-based environmental functional material preparation system, and the generated sludge-based environmental functional material preparation system is used for resource recovery.
[0051] The denitrification filtration unit includes a sulfur autotrophic denitrification reactor and a filtration assembly connected in series. The inlet of the sulfur autotrophic denitrification reactor is connected to the outlet of the high-density sedimentation tank and is used to perform sulfur autotrophic denitrification and filtration on the decarbonized nitrification water to output denitrified water. The filtration assembly includes a self-cleaning filter, a multi-media filter and an ultrafiltration unit connected in sequence. The salt separation unit includes a nanofiltration salt separation system, whose inlet is connected to the outlet of the filter assembly to perform nanofiltration salt separation on the denitrified water, separating monovalent salts and divalent salts, and outputting nanofiltration permeate and nanofiltration concentrate. The crystallization unit includes a mixed salt crystallization unit, a sodium chloride crystallization assembly, and a sodium sulfate crystallization assembly connected in parallel. The sodium chloride crystallization assembly includes a secondary activated oxygen mineralization tank, an electrodialysis concentration unit, and an evaporator crystallizer connected in sequence, used to treat nanofiltration permeate to obtain sodium chloride. The sodium sulfate crystallization assembly includes a secondary activated oxygen mineralization tank, a triple-effect pre-concentration unit, a freeze crystallization unit, and a melt recrystallization unit connected in sequence, used to treat nanofiltration concentrate to obtain sodium sulfate. The mother liquor outlet of the evaporator crystallization unit is connected to the mixed salt crystallization unit, and the mother liquor outlet of the freeze crystallization unit is connected to the mixed salt crystallization unit. After the mother liquor from freeze crystallization and evaporator crystallization undergoes mixed salt crystallization, a mixed salt solution is obtained. The outlet of the mixed salt crystallization unit is connected to the primary activated oxygen mineralization unit for reuse of the mixed salt solution. The freeze waste liquid outlet of the freeze crystallization unit is connected to the primary activated oxygen mineralization unit for reuse of the freeze waste liquid. The electrodialysis concentration unit, the evaporator crystallization unit, the triple-effect pre-concentration unit, and the melt recrystallization unit are all equipped with outlets for discharging clean permeate.
[0052] The above are merely preferred embodiments of the present invention, but the scope of protection of the present invention is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in the present invention should be included within the scope of protection of the present invention.
Claims
1. A resource recovery method for coupled defluorination, decarbonization, and denitrification of industrial concentrated brine, characterized in that, Includes the following steps: S1. Industrial concentrated brine is subjected to two-stage chemical precipitation, electrocoagulation precipitation and resin adsorption to remove fluoride, to obtain oxygen-pretreated water. S2. The pretreated oxygen water is subjected to primary oxygen mineralization and chemical precipitation treatment to obtain decarbonized nitrified water; S3. The decarbonized nitrified water is subjected to sulfur autotrophic denitrification to remove nitrogen, and after filtration, denitrified water is obtained; S4. Perform nanofiltration desalination on the denitrified water to obtain nanofiltration permeate and nanofiltration concentrate; S5. The nanofiltration permeate and the nanofiltration concentrate are respectively subjected to two-stage active oxygen mineralization, concentration and crystallization to obtain sodium chloride and sodium sulfate respectively. The waste liquid generated in step S5 is reused in the primary active oxygen mineralization treatment, and the clean water is combined into reclaimed water for discharge.
2. The resource recovery method for coupled defluorination, decarbonization, and denitrification of industrial concentrated brine according to claim 1, characterized in that, The primary active oxygen mineralization employs a multi-channel parallel electrochemical oxidation process.
3. The resource recovery method for coupled defluorination, decarbonization, and denitrification of industrial concentrated brine according to claim 1, characterized in that, The specific operation of step S1 is as follows: S11. Industrial concentrated brine is subjected to a first-stage defluorination and hardness removal treatment through two-stage chemical precipitation to obtain purified precipitated water; S12. The precipitated purified water is sequentially passed through electrocoagulation sedimentation, multi-media filtration and resin adsorption for defluorination, and then subjected to two-stage defluorination and hardening treatment to obtain oxygen-pretreated water.
4. The resource recovery method for coupled defluorination, decarbonization, and denitrification of industrial concentrated brine according to claim 1, characterized in that, The specific operation of step S5 is as follows: The nanofiltration permeate is subjected to two-stage activated oxygen mineralization, electrodialysis concentration, and evaporation crystallization to obtain sodium chloride; The nanofiltration concentrate is subjected to two-stage active oxygen mineralization, evaporation concentration, freeze crystallization, and melt recrystallization to obtain sodium sulfate; The mother liquor after evaporation crystallization and freeze crystallization is subjected to mixed salt crystallization to obtain mixed salt and mixed salt solution. The mixed salt solution and the freeze waste liquid generated by freeze crystallization are recycled as waste liquid to the primary active oxygen mineralization treatment. The electrodialysis concentrate, evaporation crystallization, evaporation concentrate, and melt recrystallization products are treated as clean water and combined as recycled water for discharge.
5. The resource recovery method for coupled defluorination, decarbonization, and denitrification of industrial concentrated brine according to claim 1, characterized in that, The method also includes the step of collecting the precipitates produced by the two-stage chemical precipitation, electrocoagulation precipitation, and the first-stage active oxygen mineralization for the preparation of sludge-based environmental functional materials.
6. The resource recovery method for coupled defluorination, decarbonization, and denitrification of industrial concentrated brine according to claim 3, characterized in that, In step S1, the two-stage chemical precipitation includes the following steps: adding lime, soda ash and coagulant PAC to industrial concentrated brine, and then adding flocculant PAM to carry out primary chemical precipitation to obtain primary effluent; adding defluoridating agent and coagulant PAC to the primary effluent, and then adding flocculant PAM to carry out secondary chemical precipitation to obtain purified precipitated water.
7. The resource recovery method for coupled defluorination, decarbonization, and denitrification of industrial concentrated brine according to claim 3, characterized in that, The first-stage activated oxygen mineralization process involves using an electrode basket filled with activated coke / activated carbon-supported transition metal matrix composite material as the working unit, and a graphite rod as the cathode and anode, to perform electrochemical oxidation.
8. A resource recovery system for coupled defluorination, decarbonization, and denitrification of industrial concentrated brine for performing the method as described in any one of claims 1-7, characterized in that, include: The multi-stage defluoridation and hardening unit is used to sequentially perform two-stage chemical precipitation, electrocoagulation precipitation and resin adsorption defluoridation on industrial concentrated brine, and output oxygen-pretreated water. The active oxygen mineralization unit is used to perform primary active oxygen mineralization and chemical precipitation treatment on the active oxygen pretreated water, and output decarbonized nitrified water. The denitrification filtration unit is used to perform sulfur autotrophic denitrification and filtration on the decarbonized nitrification water, and output denitrified water. The salt separation unit is used to perform nanofiltration salt separation on the denitrified water and output nanofiltration permeate and nanofiltration concentrate. The crystallization unit includes a sodium chloride crystallization component and a sodium sulfate crystallization component connected in parallel. The sodium chloride crystallization component is used for secondary active oxygen mineralization, electrodialysis concentration, and evaporation crystallization of nanofiltration permeate. The sodium sulfate crystallization component is used for secondary active oxygen mineralization, evaporation concentration, freeze crystallization, and melt recrystallization of nanofiltration concentrate. The waste liquid of the crystallization unit is returned to the primary active oxygen mineralization unit, and the clean permeate is combined as reclaimed water and discharged.
9. The resource recovery system for coupled defluorination, decarbonization, and denitrification of industrial concentrated brine according to claim 8, characterized in that, The primary oxygen mineralization component of the active oxygen mineralization unit includes multiple primary oxygen mineralization pools connected in parallel.
10. The resource recovery system for coupled defluorination, decarbonization, and denitrification of industrial concentrated brine according to claim 8, characterized in that, The crystallization unit also includes a mixed salt crystallization unit, which is used to collect the mother liquor from freeze crystallization and evaporation crystallization for mixed salt crystallization, and input the generated waste liquid into the primary active oxygen mineralization unit.
Citation Information
Patent Citations
Method and system for treating salt-containing wastewater
CN113072228A
Salt-containing organic wastewater recycling and zero discharge process
CN113636702A
Electrochemical advanced treatment device and process for perfluorinated compound wastewater
CN114180763A
Resource utilization method for high-salinity wastewater in coal chemical industry
CN116535031A
Sulfate purification process and system for high-salinity wastewater
CN119528389A