Process for production of N-methylmorpholine with low hasen color number

By using formaldehyde-methanol solution and hydrogen recirculation under a heterogeneous hydrogenation catalyst, the problems of numerous byproducts and high yellowness in the production of N-methylmorpholine in the prior art have been solved, and the production of colorless N-methylmorpholine with high selectivity and high purity has been achieved.

CN121693494APending Publication Date: 2026-03-17BASF SE
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202480050625.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-08-03
Filing Date
2024-08-02
Publication Date
2026-03-17

AI Technical Summary

Technical Problem

Existing techniques for preparing N-methylmorpholine suffer from the problem of large amounts of the byproduct N-formylmorpholine and high yellowness, making it difficult to obtain a colorless product with high selectivity and purity.

Method used

Formaldehyde-methanol solution was used as the raw material for the reductive amination reaction, and the reaction was carried out in the presence of a heterogeneous hydrogenation catalyst with continuous feeding. The use of hydrogen and recycled gas was combined to control the reaction temperature and selectively form N-methylmorpholine.

Benefits of technology

The production of N-methylmorpholine with high selectivity and high purity has been achieved. The product is basically colorless, which reduces the formation of by-products and improves production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

A process for the preparation of N-methylmorpholine comprising continuously feeding morpholine, a formaldehyde solution and hydrogen to at least one reactor containing a heterogeneous hydrogenation catalyst comprising cobalt and copper, and subjecting the morpholine and formaldehyde to reductive amination to obtain N-methylmorpholine wherein the fed formaldehyde solution is a formaldehyde methanol solution.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The present invention relates to a process for the preparation of N-methylmorpholine and N-methylmorpholine oxide.

[0002] N-methylmorpholine (4-methylmorpholine; 4-methyltetrahydro-1,4-oxazine; NMM) is for example used as catalyst in the production of polyurethanes. N-methylmorpholine is also a starting material for the production of N-methylmorpholine oxide which is an important solvent for cellulose.

[0003] It can be prepared by reductive amination of morpholine (MO) with formaldehyde in the presence of hydrogen.

[0004] N-methylmorpholine oxide (N-methylmorpholine N-oxide; NMMO) is for example used as solvent for cellulose. Aqueous solutions of N-methylmorpholine N-oxide are used technically as solubilizer in the production of Lyocell fibers, wherein pulp is dissolved in a solution of N-methylmorpholine N-oxide and water and spun from this solution.

[0005] N-methylmorpholine oxide can be obtained by oxidation of N-methylmorpholine.

[0006] The reductive amination of formaldehyde with morpholine can be carried out in batch mode or in continuous mode.

[0007] DE 179 93 380 relates to the preparation of secondary and tertiary amines by reaction of primary or secondary amines with formaldehyde, followed by hydrogenation of the resulting N-hydroxymethylamine in the presence of a hydrogenation catalyst containing cobalt and manganese and / or chromium at elevated temperature and under pressure. Example 3 of this document discloses the preparation of N-methylmorpholine from morpholine and formaldehyde. Accordingly, 855 parts of morpholine are reacted with 1140 parts of a 30 wt% formaldehyde solution in water under stirring at 500°C in a stirred vessel, 50 parts of the obtained reaction solution per hour are metered to the top of a vertical high-pressure tube which is equipped with a catalyst containing 14.4 wt% of cobalt, 1 wt% of chromium and 0.36 wt% of phosphorus pentoxide on aluminum oxide. The temperature of 150°C is maintained during the reaction, the pressure is kept at 250 bar g by forced hydrogen admission. The outflow from the high-pressure tube is fractionated. N-methylmorpholine having a boiling point of 114°C is obtained in a yield of 90% of theory.

[0008] DE 197 31 745 relates to a continuous process for the preparation of alkylamines by reacting an amine and an aliphatic aldehyde in the presence of free hydrogen on a fixed-bed catalyst. Formaldehyde is preferably used as aldehyde. The document discloses diethylenetriamine, dipropylenetriamine, morpholine, piperidine, pyrrolidine, piperazine, 1 -methyl-piperazine and piperazine as suitable amines. The amine can be employed without the addition of a solvent or in the form of a solution. An alcohol is preferably not used as a solvent. It is preferred that no alcohol is present at all in the reaction system. The amine is particularly preferably used as an aqueous solution. For example, piperazine is used as a 30 to 80% by weight solution in water. The aldehyde is likewise preferably used as an aqueous solution. In this case, the water content of the aldehyde solution is 50% to 90%, in particular 65% to 75%, of the total weight of the solution.

[0009] When using an aqueous formaldehyde solution in the preparation of N-methylmorpholine from morpholine and formaldehyde, a significant amount of N-formylmorpholine is formed as a by-product. Furthermore, the product N-methylmorpholine obtained is characterized by a rather high yellowness.

[0010] It is an object of the present invention to provide an efficient process for the preparation of N-methylmorpholine from morpholine and formaldehyde by reductive amination, wherein N-methylmorpholine is formed with very high selectivity and a substantially pure and colorless crude product is obtained. SUMMARY

[0011] This problem is solved by a process for the preparation of N-methylmorpholine (NMM), comprising continuously feeding morpholine (MO), a formaldehyde solution and hydrogen to at least one reactor containing a heterogeneous hydrogenation catalyst, and subjecting the morpholine and the formaldehyde to reductive amination to obtain N-methylmorpholine, wherein the formaldehyde solution is a formaldehyde methanol solution. DETAILED DESCRIPTION

[0012] The reductive amination can be carried out in one or more reactors. A preferred reactor is a tubular reactor.

[0013] A key feature of the present invention is that the continuously fed formaldehyde solution is a formaldehyde methanol solution. The term "formaldehyde methanol solution" means that formaldehyde is employed in a solution comprising methanol and preferably also water.

[0014] In such a solution, the formaldehyde can exist in different forms. For example, an amount, typically the major part, of the formaldehyde is present as a hemiacetal (resulting from formaldehyde and methanol, also called hemimethylic alcohol or 1-methoxy-methanol) or as a polyformaldehyde having the formula HO-[CH2O] n CH3 (wherein n is an integer typically in the range of 2 to 10). The weight percentages ("wt.-%") specified herein refer to the "theoretical" amounts of formaldehyde, methanol and water, thus neglecting any possible reactions between formaldehyde, methanol and water.

[0015] Preferably, the formaldehyde-methanol solution comprises 30 to 70 wt.% formaldehyde, 20 to 50 wt.% methanol, and 5 to 25 wt.% water. wt.% is based on the total mass of the formaldehyde-methanol solution.

[0016] More preferably, the formaldehyde methanol solution contains 35 to 65 wt.% formaldehyde, 25 to 45 wt.% methanol, and 5 to 20 wt.% water.

[0017] Even more preferably, the formaldehyde methanol solution contains 40 to 60 wt.% formaldehyde, 30 to 45 wt.% methanol, and 5 to 15 wt.% water.

[0018] In a preferred embodiment, the amounts of formaldehyde, methanol, and water in the formaldehyde-methanol solution are ≥ 90 wt.-%, preferably ≥ 95 wt.-%, more preferably ≥ 98 wt.-%, even more preferably ≥ 99 wt.-%, and particularly preferably ≥ 99.5 wt.-%.

[0019] Typically, the reaction temperature is in the range of 30°C to 300°C, preferably 30°C to 250°C, and more preferably 30°C to 200°C. The reaction temperature is even more preferably 60°C to 150°C, particularly preferably 80°C to 130°C, and even more particularly preferably 90°C to 130°C.

[0020] Unless otherwise expressly stated, all pressures in this application refer to absolute pressures.

[0021] The reaction pressure is typically in the range of 50 to 300 bar, preferably 50 to 250 bar, more preferably 50 to 200 bar, even more preferably 60 to 150 bar, particularly preferably 80 to 150 bar, and even more particularly preferably 90 to 140 bar.

[0022] The liquid hourly space velocity (LHSV) on heterogeneous hydrogenation catalysts is typically from 0.05 to 1, preferably from 0.1 to 0.9, more preferably from 0.2 to 0.8, and even more preferably from 0.3 to 0.7 kg morpholine / (L cat Within the range of h). LHSV refers to the volume (bed volume) of the heterogeneous hydrogenation catalyst per hour (h) (in liters) (abbreviated as L). cat. The amount of morpholine in the feed (in kg).

[0023] When the reaction is carried out in the presence of hydrogen, the reactor is preferably pressurized with hydrogen or a mixture of hydrogen and an inert gas (such as nitrogen) to achieve the above pressure. In a preferred embodiment, pure hydrogen is used. Any oxygen should be removed from the reactor before introducing hydrogen, for example, by first feeding an inert gas.

[0024] The amount of hydrogen gas is typically between 100 and 3000 NL / (L) cat. • h), preferably 200 to 2500, more preferably 500 to 2000 NL / (L cat. • h), or even more preferably 700 to 1800 NL / (L cat. • h), particularly preferred 1000 to 1700 NL / (L cat. • h), and more particularly preferred 1200 to 1600 NL / (L cat. Within the range of h).

[0025] The amount of hydrogen is expressed in liters as the volume (bed volume) of the heterogeneous hydrogenation catalyst (abbreviated as L). cat Based on .) and hours (h).

[0026] NL stands for Standard Liter, which is the liter of hydrogen (molecular hydrogen) under standard conditions (STP). Standard conditions should be understood as follows:

[0027] Standard pressure = 1.01325 bar.

[0028] Standard temperature = 0°C.

[0029] In a preferred embodiment, the method according to the invention is operated in a recirculating gas mode. This means separating the low-volatility components (particularly hydrogen) from the obtained NMM and recycling them back into the reaction. The separation is typically carried out in a high-pressure separator (the reactor effluent is fed into this high-pressure separator). The high-pressure separator is a device (e.g., a vessel) operating at a pressure slightly below the reaction pressure. The recirculating gas preferably contains at least 10% by volume, particularly 50 to 100% by volume, and very particularly 80 to 100% by volume of H2. The recirculating gas flow rate is preferably between 40 and 1500 m³ / h. 3 (Under operating pressure) / [catalyst m] 3 In the range of [(bed volume)·h], especially in the range of 100 to 700 m³ 3 (Under operating pressure) / [catalyst m] 3 Within the range of [(bed volume)·h].

[0030] In a preferred embodiment, NMM is partially recycled to the reductive amination of MO and formaldehyde. The recycling of NMM to the reaction helps control the temperature distribution in the one or more reactors. The more NMM is recycled, the lower the temperature rise in the one or more reactors. This recycling typically occurs after low-volatility components (particularly hydrogen) have been separated from the NMM. This separation can be carried out in a high-pressure separator as described above.

[0031] The weight ratio of the recirculated NMM to the combined amount of formaldehyde-methanol solution and MO fed into the one or more reactors can range from 1:1 to 10:1, preferably from 2:1 to 8:1. The weight ratio is calculated based on the mass flow rate of the respective streams containing the NMM, MO, and formaldehyde-methanol solution. It should be noted that such streams may also contain other components. For example, the formaldehyde-methanol solution stream may contain water (as further specified below), which also contributes to the mass flow rate. Similarly, the NMM stream may contain certain byproducts (as specified above) that contribute to the mass flow rate. The same applies to any impurities that may be contained in the MO.

[0032] It should be noted that the NMM obtained according to the method of the invention typically does not contain any starting materials (formaldehyde and / or MO). In the case of recycled NMM containing small amounts of starting materials, any such amount does not contribute to the formaldehyde to MO molar ratio as defined according to the invention (i.e., the molar ratio is based solely on fresh formaldehyde and MO). Generally, the formaldehyde to morpholine molar ratio in the feed into the reactor is in the range of 0.8:1 to 1.5:1, preferably 0.9:1 to 1.2:1.

[0033] The NMM obtained according to the present invention is contained in the reactor effluent discharged from the one or more reactors.

[0034] In addition to NMM, the reactor effluent also contains hydrogen, methanol, water, and byproducts. Water is formed during the reaction and may be further contained in a formaldehyde-methanol solution. Preferably, this reactor effluent is subjected to purification including the following steps:

[0035] (i) subjecting the reactor effluent to degassing (preferably in a high-pressure separator) to obtain a degassed stream;

[0036] (ii) subject the degassed stream of step (i) to a distillation step to remove methanol and obtain a stream containing NMM and lean methanol.

[0037] The degassing in step (i) is specifically for the purpose of removing hydrogen. Step (ii) is typically performed in a column.

[0038] Regarding the economics of purifying crude NMM, using methanol-formaldehyde is superior to using an aqueous formaldehyde solution. This can be attributed to the following: methanol has a lower boiling point than water, therefore less energy is required to remove methanol by distillation.

[0039] The aqueous NMM mixture thus obtained can be used in the production of NMMO as taught herein. The NMM obtained from step (ii) can also be subjected to a further distillation step to obtain a mixture of NMM and water. Such distillation is described in European Patent Application 23200776.5.

[0040] The method according to the invention is carried out in the presence of a heterogeneous hydrogenation catalyst. The term "heterogeneous catalyst" refers to a solid catalyst, preferably in particulate form, which is contacted with a liquid reaction mixture comprising the starting material and any intermediates already obtained and NMM.

[0041] Any heterogeneous catalyst with sufficient hydrogenation activity can be used to manufacture the NMM according to the invention. It can be a supported or unsupported catalyst. Unsupported catalysts are preferred.

[0042] Preferably, the heterogeneous hydrogenation catalyst contains no or substantially no palladium. The amount of palladium is preferably less than 0.5 wt.-%, more preferably less than 0.05 wt.-%, and even more preferably less than 0.01 wt.-%, based on the total weight of the heterogeneous hydrogenation catalyst.

[0043] The heterogeneous hydrogenation catalyst is installed in the reactor (preferably as a fixed bed).

[0044] Heterogeneous hydrogenation catalysts contain cobalt and copper.

[0045] Preferably, the heterogeneous hydrogenation catalyst comprises cobalt, copper, and manganese; more preferably, cobalt, copper, manganese, and molybdenum; and particularly preferably, cobalt, copper, manganese, molybdenum, and phosphorus.

[0046] Heterogeneous hydrogenation catalysts can be prepared, for example, by precipitation or impregnation methods. Suitable heterogeneous hydrogenation catalysts and corresponding methods for their production are taught, for example, in EP 2043996 B1, WO 2011 / 067200 A1, WO 2011 / 067199 A1 and EP 2780109 B1 (all by BASF).

[0047] In general, heterogeneous hydrogenation catalysts include:

[0048] 5 to 90 wt.-%, preferably 10 to 60 wt.-%, of cobalt.

[0049] 1 to 40 wt.-%, preferably 2 to 30 wt.-%, of copper.

[0050] 0 to 30 wt.% manganese

[0051] 0 to 30 wt.% molybdenum, and

[0052] 0 to 30 wt.% phosphorus.

[0053] In a highly preferred embodiment, the heterogeneous hydrogenation catalyst comprises, based on the total weight of the heterogeneous hydrogenation catalyst:

[0054] 5 to 90 wt.-%, especially 10 to 60 wt.-%, cobalt

[0055] 1 to 40 wt.-%, especially 2 to 30 wt.-%, of copper

[0056] 0.1 to 30 wt.% of manganese, especially 1 to 10 wt.%

[0057] 0.1 to 30 wt.-%, especially 1 to 10 wt.-%, and

[0058] 0.05 to 30 wt.% in particular 0.1 to 5 wt.% of phosphorus.

[0059] The preparation of such catalysts is taught, for example, in DE 2321101 (BASF). Accordingly, the catalyst is obtained by precipitation followed by calcination. The catalyst thus obtained is activated by reduction in a stream of hydrogen. It should be noted that any “wt.-%” specified herein with respect to the composition of heterogeneous hydrogenation catalysts refers to heterogeneous hydrogenation catalysts after any final heat treatment (e.g., calcination) and before reduction with hydrogen.

[0060] As can be deduced from the nature of the preparation method, the corresponding metal is at least partially present in oxidized form. However, the presence of a certain amount of such metal in elemental form is not excluded. For example, in the preparation process, a certain amount of the corresponding metal in elemental form may be applied in addition to the use of the corresponding metal nitrite. Generally, any corresponding metal present in oxidized form at concentrations greater than 90 wt.-%, preferably greater than 95 wt.-%, more preferably greater than 99 wt.-% (or even greater than 99.5 wt.-%). Phosphorus is generally present in essentially oxidized form. Typically, elemental phosphorus is not applied in catalyst preparation, but only phosphorus (especially phosphoric acid) in oxidized form is applied. Furthermore, the formation of elemental phosphorus is unlikely to occur during precipitation or calcination. Therefore, it is preferable that the corresponding phosphorus is present in oxidized form at concentrations greater than 99 wt.-%, more preferably greater than 99.5 wt.-%, and even more preferably greater than 99.9 wt.-%.

[0061] The heterogeneous hydrogenation catalyst preferably also contains oxygen. In a preferred embodiment, the heterogeneous hydrogenation catalyst contains oxygen, and the cumulative amounts of oxygen, cobalt, copper, manganese, molybdenum, phosphorus, and cobalt are based on the total weight of the heterogeneous hydrogenation catalyst as ≥ 80 wt.-%, preferably ≥ 90 wt.-%, more preferably ≥ 95 wt.-%, even more preferably ≥ 97 wt.-%, particularly preferably ≥ 98 wt.-%.

[0062] The present invention further relates to a method for preparing N-methylmorpholine oxide (NMMO), the method comprising the following steps:

[0063] (i) The preparation of N-methylmorpholine according to the method of the present invention as described above, and

[0064] (ii) subject the N-methylmorpholine obtained in step (i) to an oxidation reaction to obtain N-methylmorpholine oxide.

[0065] Oxidation step (ii) includes reacting N-methylmorpholine with a stoichiometric amount of aqueous hydrogen peroxide solution in an aqueous medium in the presence of carbon dioxide as a promoter.

[0066] In a preferred embodiment, oxidation step (ii) comprises reacting N-methylmorpholine with a less than stoichiometric amount of aqueous hydrogen peroxide solution in an aqueous medium while applying a vapor space to the aqueous medium having a carbon dioxide partial pressure p(CO2) of less than 0.75 bar absolute, preferably less than 0.20 bar absolute. Although carbon dioxide is an effective promoter for the conversion of tertiary amines to their amine oxides, the applicant has found that amounts of free carbon dioxide exceeding the promoting amount can cause undesirable discoloration.

[0067] In the embodiments, the initial concentration of the tertiary amine in the aqueous medium (i.e., the concentration of the tertiary amine before the addition of hydrogen peroxide) is in the range of 40 to 95 vol.-%, preferably 60 to 85 vol.-%. Any aqueous solution of hydrogen peroxide can be used. For practical considerations, the concentration of hydrogen peroxide in the aqueous solution added to the aqueous medium is in the range of 10 to 70 wt.-%, preferably 29 to 51 wt.-%.

[0068] The following examples are for illustrative purposes only and should not be construed as limiting the invention in any way. Example

[0069] catalyst:

[0070] The catalyst was prepared according to EP 0383132 or DE 2321101 (BASF). Its composition (based on the corresponding oxide) is as follows:

[0071] The catalyst contained 15.2 g of Cu, 2.5 g of Mn, 2.4 g of Mo, 0.9 g of P, and 16.5 g of Co.

[0072] Examples 1 to 11

[0073] Example 1 (for comparison) and Example 2 (according to the present invention)

[0074] In a heated reactor with an inner diameter of 4 mm and a total volume of 60 mL, 2-3 wire mesh rings were loaded into the lower section, followed by alternating loading of 4 mm catalyst "strips" and 3 mm glass beads, and finally 2-3 wire mesh rings. The catalyst was activated at a maximum temperature of 270°C before the reaction. Therefore, the catalyst was heated to 250°C with a hydrogen flow of 90 NL / h. After 12 h at 250°C, the reactor was cooled to 40°C. A pressure of 150 bar was used. Morpholine (MO) was metered into the reactor at 30 g / h. The reactor was maintained at the temperatures and absolute pressures listed in Table 1 below. Additionally, formaldehyde was metered in via a second pump. Aqueous solutions of formaldehyde (FA) containing 35 wt.% and 65 wt.% water (entry 1 in Table 1 below) or a formaldehyde-methanol solution containing 55 wt.% formaldehyde, 35 wt.% methanol, and 10 wt.% water (entry 2 in Table 1 below) were prepared. A recirculation feed process was implemented, which recirculates the crude product feed after the high-pressure separator to the reactor inlet at a MO feed to recirculation feed mass ratio of 2:1 (RLV). Samples were taken from the reaction mixture at different times and analyzed by gas chromatography. For this purpose, an “RTX-5 Amin” GC column was used with the following parameters: RTX-5 Amin ((30 m x 0.32 mm x 1.5 µm) 60°C – 5°C / min – 280°C – 6 min. Flow rate: 1.5 NL / min N2.

[0075] Determine the Hassen color number on a Lico 620 colorimeter (Company HACH).

[0076] The results are presented in Table 1 below.

[0077] Table 1

[0078]

[0079] Comparative example (formaldehyde aqueous solution)

[0080] According to the present invention (formaldehyde methanol solution)

[0081] Examples 3-11

[0082] Examples 3-11 were performed similarly to Example 2. Process parameters, conversion rates, and product selectivity are listed in Table 2 below.

[0083] Table 2

[0084] .

Claims

1. A process for the preparation of N-methylmorpholine, the process comprising: morpholine, a formaldehyde solution and hydrogen are continuously fed to at least one reactor containing a heterogeneous hydrogenation catalyst comprising cobalt and copper, and the morpholine and formaldehyde are subjected to reductive amination to obtain N-methylmorpholine, wherein the fed formaldehyde solution is a formaldehyde methanol solution.

2. The method of claim 1, wherein, The heterogeneous hydrogenation catalyst comprises, based on the total weight of the heterogeneous hydrogenation catalyst: cobalt in the range of 5 to 90 wt.-%, copper in the range of 1 to 40 wt.-%, manganese in the range of 0 to 30 wt.-%, molybdenum in the range of 0 to 30 wt.-%, and phosphorus in the range of 0 to 30 wt.-%.

3. The method of claim 1 or 2, wherein, The heterogeneous hydrogenation catalyst comprises cobalt, copper, manganese, molybdenum and phosphorus.

4. The method of any one of claims 1 to 3, wherein, The heterogeneous hydrogenation catalyst comprises, based on the total weight of the heterogeneous hydrogenation catalyst: cobalt in the range of 5 to 90 wt.-%, copper in the range of 1 to 40 wt.-%, manganese in the range of 0.1 to 30 wt.-%, molybdenum in the range of 0.1 to 30 wt.-%, and phosphorus in the range of 0.05 to 30 wt.-%.

5. The method of any one of claims 1 to 4, wherein, The fed formaldehyde methanol solution comprises formaldehyde in the range of 30 to 70 wt.-%, methanol in the range of 20 to 50 wt.-%, and water in the range of 5 to 25 wt.-%.

6. The method of any one of claims 1 or 5, wherein, The molar ratio of formaldehyde to morpholine in the feed to the reactor is in the range of 0.8 : 1 to 1.5 : 1, preferably 0.9 : 1 to 1.2 :

1.

7. The method of any one of claims 1 to 6, wherein, The reductive amination is carried out in liquid phase.

8. The method of any one of claims 1 to 7, wherein, N-methylmorpholine is partially recycled to the reductive amination of morpholine and formaldehyde.

9. The method of claim 8, wherein, The weight ratio of the combined amount of recycled N-methylmorpholine to the morpholine and formaldehyde methanol solution fed to the one or more reactors is in the range of 1 : 1 to 10 : 1, preferably 2 : 1 to 8 :

1.

10. The method of any one of claims 1 to 9, wherein, The reaction temperature is in the range of 30 °C to 300 °C, preferably 30 °C to 250 °C, more preferably 30 °C to 200 °C, even more preferably 60 °C to 150 °C, particularly preferably 80 °C to 130 °C, more particularly preferably 90 °C to 130 °C.

11. The method of any one of claims 1 to 10, wherein, The reaction pressure is in the range of 50 to 300 bar, preferably 50 to 250 bar, more preferably 50 to 200 bar, even more preferably 60 bar to 150 bar, particularly preferably 80 to 150 bar, more particularly preferably 90 to 140 bar.

12. The method of any one of claims 1 to 11, wherein, The liquid hourly space velocity on the heterogeneous hydrogenation catalyst is in the range of 0.05 to 1, preferably 0.1 to 0.9, more preferably 0.2 to 0.8, even more preferably 0.3 to 0.7 kg morpholine / (L kat h) of the heterogeneous hydrogenation catalyst.

13. A process for the preparation of N-methylmorpholine oxide (NMMO) comprising the steps of: (i) preparing N-methylmorpholine according to any one of claims 1 to 12, and (ii) subjecting the N-methylmorpholine obtained in step (i) to an oxidation reaction to obtain N-methyl-morpholine oxide.

14. The method of claim 13, wherein, The oxidation reaction of step (ii) comprises reacting N-methylmorpholine with less than the stoichiometric amount of an aqueous hydrogen peroxide solution in an aqueous medium in the presence of carbon dioxide as a promoter.

15. The method of claim 14, wherein, The oxidation step (ii) comprises reacting N-methylmorpholine with less than stoichiometric amounts of aqueous hydrogen peroxide in an aqueous medium, while applying to the aqueous medium a vapor space having a carbon dioxide partial pressure p(CO2) of less than 0.75 bar abs, preferably less than 0.20 bar abs. The oxidation step (ii) comprises reacting N-methylmorpholine with less than stoichiometric amounts of aqueous hydrogen peroxide in an aqueous medium, while applying to the aqueous medium a vapor space having a carbon dioxide partial pressure p(CO2) of less than 0.75 bar abs, preferably less than 0.20 bar abs.

Citation Information

Patent Citations

  • Alkyl-amine compounds preparation with high conversion and selectivity and minimum residue

    DE19731745C1

  • Cobalt, copper, manganese and molybdenum catalyst - for hydrogenation of carboxylic acids to alcohols

    DE2321101A1

  • Cobalt catalysts

    EP0383132A1

  • Method for producing an amine

    EP2043996B1

  • Process for producing sn-containing catalysts

    EP2780109B1