A vacuum cutting stage and a vacuum cutting method
By employing a dual-cavity region design and differential adsorption technology, the problems of warping and offset during the cutting of small-sized metal films were solved, resulting in higher cutting stability and yield, and improved film surface consistency.
Patent Information
- Application Number
- CN202611475336.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-21
- Publication Date
- 2026-11-10
AI Technical Summary
Existing single-cavity vacuum cutting stages struggle to stably suppress warping and shifting of cut films when cutting small-sized metal films, while also preventing the films from deforming due to excessive adsorption forces, thus limiting yield improvement.
The design employs a dual-cavity region, which controls the negative pressure difference between the retention region and the removal region separately. The negative pressure difference is adjusted within a preset range through an independent exhaust mechanism, ensuring that the retention region uses a smaller negative pressure for gentle adsorption, while the removal region uses a larger negative pressure for strong adsorption, thus achieving differential adsorption.
It improves the stability of small-sized metal film cutting and positioning and the yield of transfer and patching, reduces the deformation damage of the retained film during the adsorption and cutting process, and improves the consistency and flatness of the film surface after cutting.
Smart Images

Figure CN123060792A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor power device packaging, and more particularly to a vacuum cutting stage and a vacuum cutting method. Background Technology
[0002] Metal films, due to their excellent electrical and thermal conductivity, are widely used in the chip packaging of power devices such as insulated-gate bipolar transistors (IGBTs) and silicon carbide metal-oxide-semiconductor semiconductors (SiMDSs). In automated mass production, arrayed metal films, along with a release liner, are laid flat on a vacuum cutting stage. The stage applies vacuum adsorption to the films, and then individual metal films are cut and separated according to component dimensions. These films are then picked up by vacuum nozzles and transferred for mounting. Currently, mass production lines commonly use single-cavity vacuum adsorption stages. The stage forms a connected adsorption chamber, with a perforated adsorption panel and flexible pad above it. An air extraction device evacuates the entire adsorption surface via a single air path, ensuring that the release liner and metal film are fixed under uniform negative pressure across the entire surface. These stages are primarily developed for transferring relatively large metal films. The films themselves possess a certain weight and rigidity, and uniform pressure adsorption across the entire surface meets the fixing requirements during the cutting process. The related structures and processes are relatively mature.
[0003] As power devices become increasingly miniaturized, the size of individual transfer metal films is constantly decreasing, leading to a reduction in the film's weight and rigidity. Meanwhile, the area of the release liner region that needs to be removed from the periphery of the metal film increases significantly. When the cutting edge severs the film outline, the release liner in the outer removal area tends to retract inwards due to its internal stress. Under the single-cavity, uniform pressure adsorption method, the stage applies roughly the same adsorption force to both the retained metal film area and the outer removal area, making it difficult to create a stronger, continuous constraint on the outer removal area. This retraction stress then propagates inwards, pulling on the very lightweight retained metal film. Once cutting is complete, the film edges are prone to warping, localized arching, and positional shifts, causing the nozzle to misalign or even drop the film. If the overall negative pressure of the single cavity is increased to suppress periphery retraction, the tiny metal film in the retained area will simultaneously bear the same adsorption force, leading to over-adsorption and resulting in stretching lines and localized depressions. The uniform pressure method struggles to balance reliable periphery adhesion with gentle support in the retained area. Therefore, when the existing single-cavity vacuum cutting stage with uniform negative pressure is applied to the cutting of small-sized metal films, it is difficult to stably suppress the warping and displacement of the cut film, and it is also difficult to avoid the deformation of the film due to excessive adsorption force. The yield improvement of small-sized metal film transfer patches is restricted. Summary of the Invention
[0004] To address the shortcomings of existing technologies, this invention discloses a vacuum cutting stage applied to a metal film to be cut. The metal film to be cut includes a retention area and a removal area, comprising: A platform base, comprising a platform base and a support member disposed above the platform base, wherein the platform base and the support member enclose an internal space, and the support surface of the support member is used to place the metal film to be cut. The internal space includes a first cavity region and a second cavity region that are isolated from each other by a first seal. The second cavity region is an annular region, and the first cavity region is located within the area enclosed by the second cavity region. The size of the first cavity region matches the size of the retention region, and the size of the second cavity region matches the size of the removal region, so that when the metal film to be cut is placed on the bearing surface of the carrier, the retention region is aligned with the first cavity region, and the removal region is aligned with the second cavity region. The support member has multiple ventilation holes for applying negative pressure from the first cavity region to the retention region and applying negative pressure from the second cavity region to the removal region. An exhaust mechanism is provided, wherein the exhaust end of the exhaust mechanism extends to the first cavity region and the second cavity region respectively, for extracting gas from the first cavity region and the second cavity region respectively, so as to control the negative pressure in the first cavity region to be less than the negative pressure in the second cavity region.
[0005] Preferred options also include: A first negative pressure gauge is installed in the first cavity region to obtain the current negative pressure value in the first cavity region; A second negative pressure gauge is installed in the second cavity region to obtain the current negative pressure value in the second cavity region; The host computer is connected to the first negative pressure gauge, the second negative pressure gauge, and the exhaust mechanism, respectively. It is used to control the exhaust mechanism to extract air from the first cavity area and the second cavity area respectively according to the negative pressure difference between the current negative pressure value in the first cavity area and the current negative pressure value in the second cavity area, so as to keep the negative pressure difference within a preset negative pressure range, and the negative pressure in the first cavity area is less than the negative pressure in the second cavity area.
[0006] Preferably, the internal space includes a first isolation groove and a second isolation groove; It also includes a second seal; The first isolation groove is disposed between the first cavity region and the second cavity region; The second isolation groove is disposed at the outer periphery of the second cavity region; The first sealing element is connected to the first isolation groove to isolate the gas flow between the first cavity region and the second cavity region; The second seal is connected to the second isolation groove to isolate the second cavity area from the external gas flow.
[0007] Preferably, the width of the first isolation groove and the width of the second isolation groove are both 1 mm.
[0008] Preferably, the carrier includes: A vacuum adsorption plate, wherein the vacuum adsorption plate has a plurality of vent holes corresponding to the first cavity region and the second cavity region respectively; A soft pad, the lower surface of which is fixedly connected to the upper surface of the vacuum adsorption plate, the upper surface of which serves as the bearing surface.
[0009] Preferably, the diameter of each vent hole on the vacuum adsorption plate is 0.3mm to 0.5mm, and the spacing between each adjacent vent hole is 4mm.
[0010] Preferably, the thickness of the cushion is 1.0 mm to 1.5 mm.
[0011] Preferably, the annular width of the second cavity region is 4mm to 5mm.
[0012] This invention discloses a vacuum cutting method applied to a metal film to be cut. The metal film to be cut includes a retention area and a removal area. The vacuum cutting stage is used to support the metal film to be cut. The method includes: Step S1: Place the metal film to be cut on the bearing surface of the carrier, with the retained area aligned with the first cavity area and the removed area aligned with the second cavity area; In step S2, the exhaust mechanism extracts gas from the first cavity region and the second cavity region respectively to maintain the negative pressure in the first cavity region being less than the negative pressure in the second cavity region.
[0013] Preferably, a first negative pressure gauge is provided in the first cavity region, a second negative pressure gauge is provided in the second cavity region, and a host computer is provided, which is connected to the first negative pressure gauge, the second negative pressure gauge and the exhaust mechanism respectively; Step S2 includes: Step S21: The host computer obtains the current negative pressure value in the first cavity area through the first negative pressure gauge, and obtains the current negative pressure value in the second cavity area through the second negative pressure gauge; Step S22: The host computer processes and obtains the negative pressure difference between the current negative pressure value in the first cavity area and the current negative pressure value in the second cavity area; In step S23, the host computer controls the exhaust mechanism to extract air from the first cavity area and the second cavity area respectively according to the negative pressure difference, so as to keep the negative pressure difference within a preset negative pressure range, and the negative pressure in the first cavity area is less than the negative pressure in the second cavity area.
[0014] The following beneficial effects can be obtained by using the present invention: 1. By controlling the negative pressure in the first cavity region to be less than that in the second cavity region, and applying negative pressure to the metal film respectively, the stability of small-sized metal film cutting and positioning and the yield of transfer bonding are improved.
[0015] 2. By applying a smaller negative pressure to the retention area through the first cavity area and a larger negative pressure to the removal area through the second cavity area, the deformation damage of the retention film during the adsorption and cutting process is reduced, and the consistency and flatness of the film surface after cutting are improved. Attached Figure Description
[0016] Figure 1 This is an exploded view of the vacuum cutting stage in this invention; Figure 2 This is a top view of the vacuum cutting stage in this invention; Figure 3 This is a side view of the vacuum cutting stage in this invention; Figure 4 This is a schematic diagram of the vacuum cutting method in this invention; Figure 5 This is a schematic diagram of the process of controlling the exhaust mechanism by the host computer in this invention.
[0017] In the attached image: 1. Platform base; 11. First cavity area; 12. Second cavity area; 2. First exhaust pipe; 3. Second exhaust pipe; 4. First seal; 5. Second seal; 6. Vacuum adsorption plate; 7. Soft pad; 8. Magnetic pressure block. Detailed Implementation
[0018] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0019] It should be noted that, unless otherwise specified, the embodiments and features described in the present invention can be combined with each other.
[0020] The present invention will be further described below with reference to the accompanying drawings and specific embodiments, but this is not intended to limit the scope of the invention.
[0021] This invention discloses a vacuum cutting stage applied to a metal film to be cut, the metal film including a retention area and a removal area, such as... Figure 1 As shown, it includes: The platform base includes a platform base 1 and a support member disposed above the platform base 1. The platform base 1 and the support member enclose an internal space, and the bearing surface of the support member is used to place the metal film to be cut. The internal space includes a first cavity region 11 and a second cavity region 12 that are isolated from each other by a first seal 4; The second cavity region 12 is an annular region, and the first cavity region 11 is located within the area enclosed by the second cavity region 12. The size of the first cavity region 11 matches the size of the retention region, and the size of the second cavity region 12 matches the size of the removal region, so that when the metal film to be cut is placed on the bearing surface of the carrier, the retention region is aligned with the first cavity region 11, and the removal region is aligned with the second cavity region 12. The carrier has multiple vent holes for applying negative pressure from the first cavity region 11 to the retention region and applying negative pressure from the second cavity region 12 to the removal region. The exhaust mechanism has its suction end extending to the first cavity region 11 and the second cavity region 12, respectively, to extract gas from the first cavity region 11 and the second cavity region 12, so as to control the negative pressure in the first cavity region 11 to be less than the negative pressure in the second cavity region 12.
[0022] Specifically, the overall dimensions of the metal film sheet are 96mm × 96mm, with a thickness of approximately 65μm. The effective area of the cut metal film conforms to small-size specifications, ranging from 1.0mm × 1.0mm to 2.5mm × 2.5mm. The release film to be cut is made of PET (Polyethylene Terephthalate) or ETFE (Ethylene Tetrafluoroethylene). During film laying, magnetic clamping blocks 8 can be used to first fix the edges of the entire film sheet to ensure alignment accuracy.
[0023] The stage substrate comprises two parts: a stage base 1 and a support component. The stage base 1 is located below, and the support component is mounted on top of the stage base 1. After the stage base 1 and the support component are aligned, a closed internal space is formed between them. A groove is machined on the side of the stage base 1 facing the support component. After the support component is closed, the groove is sealed, thereby forming a first cavity region 11 and a second cavity region 12 in the internal space. The two cavity regions are isolated from each other by a first sealing component 4, and their gases are not interconnected. The stage base 1 can be made of 6061-T6 aluminum alloy and the surface is treated with hard black antistatic anodizing to balance structural rigidity, lightweight, and the antistatic and cleanliness requirements of the semiconductor packaging environment.
[0024] The second cavity region 12 is an annular region, and the first cavity region 11 is located within the area enclosed by the second cavity region 12. The size of the first cavity region 11 matches the retention area of the metal film, and the size of the second cavity region 12 matches the removal area of the metal film. When the metal film to be cut is placed on the bearing surface of the carrier, the arrayed retention areas are aligned one-to-one with the first cavity regions 11, and the outer annular removal areas are aligned with the annular second cavity regions 12, so that the two cavity regions are respectively facing the two parts of the metal film that need to be treated differently.
[0025] The carrier has multiple vent holes, each located within the coverage area of the first cavity region 11 and the second cavity region 12. The negative pressure in the first cavity region 11 acts on the retention area through the vent holes above it, and the negative pressure in the second cavity region 12 acts on the removal area through the vent holes above it, so that the negative pressures of different magnitudes in the two cavity regions can be transmitted to the corresponding two parts of the metal film respectively.
[0026] The exhaust mechanism has two independent suction ends, namely the first exhaust pipe 2 and the second exhaust pipe 3. The first exhaust pipe 2 extends into the first cavity region 11, and the second exhaust pipe 3 extends into the second cavity region 12, forming two independent air paths for suction and independent adjustment of negative pressure, so that the negative pressure in the first cavity region 11 is less than the negative pressure in the second cavity region 12. The negative pressure is used to characterize the degree of vacuuming. The greater the negative pressure, the lower the pressure relative to the atmosphere in the cavity, and the stronger the adsorption capacity for the membrane. Therefore, the second cavity region 12, which is aligned with the removal region, is evacuated more thoroughly and has a stronger adsorption force, while the first cavity region 11, which is aligned with the retention region, has a relatively mild adsorption force. This creates a state where the outer removal region is locked by strong adsorption, and the central retention region is stably supported by a smaller negative pressure. That is, the effective area is constrained by stronger adsorption on the outer release membrane and supported by weaker adsorption on the metal membrane.
[0027] In one embodiment, target negative pressures are set for the two cavity regions, controlling the first cavity region 11 to reach a preset first negative pressure value and the second cavity region 12 to reach a preset second negative pressure value, and ensuring that the first negative pressure value is less than the second negative pressure value. The first negative pressure value of the first cavity region 11 can be -30 kPa to -40 kPa, and the second negative pressure value of the second cavity region 12 can be -40 kPa to -50 kPa. The negative pressure of the second cavity region 12 is 5 kPa to 10 kPa higher than that of the first cavity region 11. In another embodiment, the current negative pressure of the two cavity regions is acquired in real time during the evacuation process, and the corresponding evacuation force is dynamically adjusted so that the negative pressure of the first cavity region 11 is always less than that of the second cavity region 12, and the negative pressure difference between the two is maintained within a preset negative pressure range; for example, the negative pressure difference can be maintained within the aforementioned range of 5 kPa to 10 kPa. The absolute negative pressure of the two cavity regions can fluctuate within a certain range depending on the membrane specifications, membrane laying status, and other working conditions, as long as the negative pressure of the second cavity region 12 is always higher than that of the first cavity region 11.
[0028] Furthermore, in terms of the gas path configuration, each suction end of the exhaust mechanism is connected to the vacuum generating element through its own exhaust pipe. Each gas path is equipped with a pressure regulating valve and an on / off valve. The pressure regulating valve is used to set the negative pressure of the gas path, and the on / off valve is used to control the connection and disconnection of the gas path. The exhaust pipe and the platform base 1 can be connected by a vacuum quick-connect connector with a diameter of about 6mm, which facilitates assembly and disassembly and ensures the interface is sealed.
[0029] In one embodiment, the two air paths are each equipped with independent vacuum generating elements, that is, two air pumps are used to pump air separately. The first air pump is connected to the first cavity region 11 through the first pressure regulating valve, the first on / off valve and the first exhaust pipe 2, and the second air pump is connected to the second cavity region 12 through the second pressure regulating valve, the second on / off valve and the second exhaust pipe 3. The two air paths are independent of each other in terms of pumping power and control. When one path adjusts the negative pressure or stops pumping air, the other path is not affected.
[0030] In another embodiment, the two gas paths share the same vacuum generating element, that is, a single air pump is used as a common vacuum source. The air pump's intake port is divided into two branches after passing through the main pipeline. The two branches are connected to the corresponding cavity areas through their respective pressure regulating valves, on / off valves, and exhaust pipes. The air pump only provides a unified pumping power. The negative pressure of the two cavity areas is independently adjusted by two pressure regulating valves. Setting the second pressure regulating valve to a higher vacuum level than the first pressure regulating valve can also achieve differential adsorption where the negative pressure in the second cavity area 12 is greater than that in the first cavity area 11. This can also reduce the number of vacuum generating elements and facilitate the overall pipeline layout.
[0031] In a preferred embodiment of the present invention, it further includes: A first negative pressure gauge is installed in the first cavity region 11 to obtain the current negative pressure value in the first cavity region 11; The second negative pressure gauge is installed in the second cavity region 12 to obtain the current negative pressure value in the second cavity region 12; The host computer is connected to the first negative pressure gauge, the second negative pressure gauge, and the exhaust mechanism, respectively. It is used to control the exhaust mechanism to draw air from the first cavity region 11 and the second cavity region 12 respectively, based on the negative pressure difference between the current negative pressure value in the first cavity region 11 and the current negative pressure value in the second cavity region 12, so as to keep the negative pressure difference within a preset negative pressure range, and the negative pressure in the first cavity region 11 is less than the negative pressure in the second cavity region 12.
[0032] Specifically, the host computer communicates with the first negative pressure gauge, the second negative pressure gauge, and the two air paths of the exhaust mechanism to receive the current negative pressure fed back by the two negative pressure gauges, calculate the negative pressure difference between them, compare the negative pressure difference with the preset negative pressure range, and then send control commands to the two air paths respectively. By adjusting the air pumping force or the opening degree of the pressure regulating valve and the state of the on / off valve, the air pumping speed of the two cavity areas is changed respectively, thereby stabilizing the negative pressure difference between the two cavity areas within the preset negative pressure range and ensuring that the negative pressure of the first cavity area 11 is always less than that of the second cavity area 12.
[0033] Furthermore, during the pre-extraction stage, the host computer controls the two air paths to simultaneously extract air, ensuring that the first cavity region 11 and the second cavity region 12 reach the same pre-treatment negative pressure and maintain it for the set pre-treatment time. After entering the working stage, the host computer controls the two air paths to form and maintain the aforementioned differential negative pressure. This closed-loop control is particularly suitable for the aforementioned dynamic control method: when the peripheral removal area shows a shrinkage trend due to cutting, or when changes in the film laying state cause fluctuations in the negative pressure of a certain cavity region, the host computer adjusts the extraction force of that path according to the real-time feedback from the negative pressure gauge, so that the negative pressure difference always falls within the preset range, without locking the two cavity regions to a fixed negative pressure value.
[0034] In one embodiment, the first negative pressure value and the second negative pressure value can be preset directly through two pressure regulating valves, and the gas extraction sequence can be controlled by the on / off valve to achieve differential adsorption in a fixed value control manner.
[0035] In a preferred embodiment of the present invention, such as Figure 1 As shown, the internal space includes a first isolation slot and a second isolation slot; It also includes a second seal 5; The first isolation groove is disposed between the first cavity region 11 and the second cavity region 12; The second isolation groove is located on the outer periphery of the second cavity region 12; The first sealing element 4 is connected to the first isolation groove to isolate the gas flow between the first cavity region 11 and the second cavity region 12. The second sealing element 5 is connected to the second isolation groove to isolate the second cavity area 12 from the external gas flow.
[0036] Specifically, the first sealing element 4 and the second sealing element 5 both adopt rubber sealing rings with circular cross sections. After they are matched with the corresponding isolation grooves, the first cavity area 11 and the second cavity area 12 each form an independent sealed air chamber, which neither crosses with each other nor leaks to the outside, providing a sealing basis for maintaining different negative pressures in the two cavity areas.
[0037] In a preferred embodiment of the present invention, the width of the first isolation groove and the width of the second isolation groove are both 1 mm.
[0038] In a preferred embodiment of the present invention, such as Figure 1 As shown, the carrier includes: Vacuum adsorption plate 6, with multiple air vents corresponding to the first cavity region 11 and the second cavity region 12 respectively. The soft pad 7 has its lower surface fixedly connected to the upper surface of the vacuum adsorption plate 6, and the upper surface of the soft pad 7 serves as the bearing surface.
[0039] Specifically, the vacuum adsorption plate 6 is a rigid plate that covers the side of the carrier base 1 facing the membrane. The vacuum adsorption plate 6 has multiple vent holes corresponding to the first cavity region 11 and the second cavity region 12, allowing gas to flow longitudinally along the thickness direction of the vacuum adsorption plate 6, thus transmitting the negative pressure upwards within the two cavity regions. The lower surface of the soft pad 7 is fixedly connected to the upper surface of the vacuum adsorption plate 6, and the upper surface of the soft pad 7 serves as a bearing surface on which the metal membrane to be cut is placed.
[0040] Furthermore, the soft pad 7 can be made of silicone-free, anti-static, micro-permeable foamed silicone. The soft pad 7 body does not have venting grooves or through holes; gas slowly and evenly permeates through the micropores inside the soft pad 7, resulting in gentle dispersion of adsorption force and preventing the metal film from being strongly adsorbed by the venting holes, causing indentations. The absence of silicone precipitation avoids contamination of the subsequent sintering interface by silicon-based substances, and the anti-static properties reduce the impact of static electricity on the micro-films. A matte micro-texture can be formed on the surface of the soft pad 7 to reduce localized adhesion between the film and the supporting surface. The lower surface of the soft pad 7 can be fully adhered to the vacuum adsorption plate 6 using PI (Polyimide) high-temperature resistant double-sided adhesive, and the edges are sealed with PI tape to reduce edge leakage.
[0041] like Figure 1As shown, a magnetic pressure block 8 is also provided to assist in positioning the edge of the flattened metal film, so as to fix the position of the entire film sheet before the negative pressure is established.
[0042] In a preferred embodiment of the present invention, the diameter of each vent hole on the vacuum adsorption plate 6 is 0.3mm to 0.5mm, and the spacing between each adjacent vent hole is 4mm.
[0043] In a preferred embodiment of the present invention, the thickness of the cushion 7 is 1.0 mm to 1.5 mm.
[0044] Specifically, the thickness of the pad 7 is matched with its hardness, which can be Shore A35 to Shore A45. The appropriate thickness and hardness ensure that the pad 7 provides cushioning protection and gently disperses the adsorption force, without being too soft and causing it to sink and deform under negative pressure, or too hard and losing its cushioning and gas equalization functions.
[0045] In a preferred embodiment of the present invention, the annular width of the second cavity region 12 is 4mm to 5mm.
[0046] Specifically, the width of the annular region 12 of the second cavity region is matched with the width of the removal region around the metal film, so that the entire removal region is within the strong adsorption range of the second cavity region 12, continuously locking the outer release film in the circumferential direction, and avoiding the release film retraction stress from being transmitted inward due to insufficient local constraint.
[0047] This invention discloses a vacuum cutting method applied to a metal film to be cut. The metal film to be cut includes a retention area and a removal area. The metal film to be cut is supported by the aforementioned vacuum cutting stage. Figure 4 As shown, it includes: Step S1: Place the metal film to be cut on the bearing surface of the carrier, aligning the retained area with the first cavity area 11 and the removed area with the second cavity area 12. In step S2, the exhaust mechanism extracts gas from the first cavity region 11 and the second cavity region 12 respectively to keep the negative pressure in the first cavity region 11 less than the negative pressure in the second cavity region 12.
[0048] Specifically, when the metal membrane is first laid flat on the supporting surface, there is still a layer of air between the metal membrane and the supporting surface. Furthermore, the metal membrane itself is thin and light. When air is extracted under a large negative pressure difference, the airflow will instantly and forcefully draw downwards, trapping the air under the membrane, forming bubbles, wrinkles, or causing the membrane to shift. Therefore, before establishing the negative pressure difference between the first cavity region and the second cavity region, the exhaust mechanism simultaneously and equally extracts gas from the first cavity region 11 and the second cavity region 12 through two air paths, so that the two cavity regions reach the same preset pretreatment negative pressure, and maintains this pretreatment negative pressure for a preset pretreatment time.
[0049] The pretreatment negative pressure ranges from -15 kPa to -20 kPa, and the pretreatment time ranges from 0.3 s to 0.8 s.
[0050] The pretreatment negative pressure is less than the first negative pressure value of the first cavity region 11 and the second negative pressure value of the second cavity region 12 during cutting. During the pretreatment negative pressure maintenance, gas is uniformly extracted from the micropores in the pad 7, the metal film tends to be laid flat on the bearing surface, and no air bubbles are generated between the metal film and the bearing surface. After pre-extraction and venting are completed, the host computer controls the venting mechanism to further extract gas from the first cavity region 11 and the second cavity region 12 to maintain the negative pressure in the first cavity region 11 less than the negative pressure in the second cavity region 12.
[0051] Cutting is performed after maintaining a lower negative pressure within the first cavity region 11 than within the second cavity region 12. The mounting component is picked up by a vacuum nozzle above the stage and lowered. The cutting blade cuts the metal film piece by piece along the contour of the retained area. The cut size of each piece corresponds to the component size, ranging from 1.0mm × 1.0mm to 2.5mm × 2.5mm. At the cutting position, the metal film unit corresponding to the retained effective area is located above the first cavity region 11 and is stably supported by a smaller negative pressure. The annular release film to be removed around it is located above the second cavity region 12 and is locked in place by a larger negative pressure. After the cutting edge cuts the film outline, the outer release film tends to retract inward due to its internal stress. The second cavity region 12 continuously locks the removal area with stronger adsorption, counteracting this retraction stress and preventing it from pulling on the extremely lightweight metal film unit, causing the corners to curl, arch, or shift in position. The first cavity region 11 supports the metal film unit corresponding to the retention area with a smaller negative pressure, preventing it from being over-adsorbed and causing stretching lines or local depressions. Throughout the cutting process, the venting mechanism maintains the negative pressure in both cavity regions without releasing or interrupting it, ensuring that the second cavity region 12 always locks the removal area until the entire board is cut.
[0052] After cutting, post-cutting processing is performed. After all units on the board are cut, the negative pressure in the two cavity areas is gradually returned to natural atmospheric pressure: first, the first cavity area 11 is de-evacuated and connected to the atmosphere, returning to natural atmospheric pressure. After an interval of 0.5s to 1s, the second cavity area 12 is then returned to natural atmospheric pressure; in one specific embodiment, this interval is 0.8s. By locking the second cavity area 12 (the area to be removed) and releasing it last, the release film and cutting debris are prevented from rebounding instantaneously when both cavity areas lose pressure simultaneously. During depressurization, the evacuation can be cut off by a shut-off valve, and the cavity can be connected to the atmosphere through a pipeline. Alternatively, clean, dry air or inert gas can be introduced into the cavity to allow the gauge pressure inside the cavity to return to natural atmospheric pressure smoothly. After depressurization, the cut and separated silver film units are picked up one by one using a vacuum nozzle, transferred, and mounted onto the corresponding components, completing the transfer and mounting process.
[0053] In a preferred embodiment of the present invention, after performing step S1, a first negative pressure gauge is set in the first cavity region, a second negative pressure gauge is set in the second cavity region, and a host computer is set up, which is connected to the first negative pressure gauge, the second negative pressure gauge and the exhaust mechanism respectively. like Figure 5 As shown, step S2 includes: Step S21: The host computer obtains the current negative pressure value in the first cavity area through the first negative pressure gauge, and obtains the current negative pressure value in the second cavity area through the second negative pressure gauge; Step S22: The host computer processes and obtains the negative pressure difference between the current negative pressure value in the first cavity area and the current negative pressure value in the second cavity area; In step S23, the host computer controls the exhaust mechanism to extract air from the first cavity area and the second cavity area respectively according to the negative pressure difference, so as to keep the negative pressure difference within the preset negative pressure range, and the negative pressure in the first cavity area is less than the negative pressure in the second cavity area.
[0054] An embodiment is provided here to enable those skilled in the art to better understand the vacuum cutting platform and the corresponding cutting method in this invention.
[0055] The platform base 1 is made of 6061-T6 aluminum alloy and undergoes hard black antistatic anodizing. A first, non-communicating cavity region 11 and a ring-shaped second cavity region 12 are machined on the platform base 1, separated by a 1mm wide first isolation groove. The ring-shaped second cavity region 12 has a width of 4.5mm and is continuous circumferentially without any breaks. Ventilation holes with a diameter of 0.4mm and a center-to-center spacing of 4mm are matrix-cut on the vacuum adsorption plate 6. No holes are cut at the corresponding positions of the first isolation groove. A soft pad 7 is fully laid on top of the vacuum adsorption plate 6. The soft pad 7 is made of 1.2mm thick, Shore A40 hardness, non-silicone-leaching, antistatic, micro-permeable foamed silicone with a matte, micro-textured surface and no venting grooves. The soft pad 7 is bonded with PI high-temperature resistant double-sided adhesive and sealed with PI tape around its edges. Two independent vacuum quick-connectors with a diameter of 6mm are set on the outside of the platform. They are connected to the first cavity area 11 and the second cavity area 12 through the first exhaust pipe 2 and the second exhaust pipe 3, respectively. The two air paths are independently pressure-regulated and independently switched on and off. The first sealing element 4 and the second sealing element 5 are respectively set on the periphery of the first cavity area 11 and the second cavity area 12. After the vacuum adsorption plate 6 is closed, two independent sealed air chambers are formed.
[0056] During operation, the entire ETFE release film carrying the silver or copper film is laid flat on the soft pad 7, aligning the retention area with the first cavity area 11 and the removal area with the second cavity area 12. First, the exhaust mechanism simultaneously draws air through two channels, bringing the first cavity area 11 and the second cavity area 12 to a pretreatment negative pressure of -18 kPa and maintaining it for 0.5 seconds. The gas is slowly extracted through the micropores and vents of the soft pad 7, and the interlayer air between the silver film to be cut and the carrier is orderly discharged. Then, the two negative pressures are adjusted to bring the first cavity area 11 to -35 kPa and the second cavity area 12 to -45 kPa. The negative pressure in the second cavity area 12 is 10 kPa higher than that in the first cavity area 11, creating a state where the removal area is locked by a stronger negative pressure, and the retention area is stably supported by a smaller negative pressure. The components are then picked up by a vacuum nozzle above the stage and lowered. The silver film is cut piece by piece and the transfer is completed. In Example 1, the cutting size is 1.0mm × 1.0mm, and in Example 2, the cutting size is 2.5mm × 2.5mm. During the cutting process, the exhaust mechanism maintains the negative pressure of the first cavity area 11 and the second cavity area 12 without releasing it, so that the second cavity area 12 is always locked in the removal area. After the whole board is cut, the negative pressure of the first cavity area 11 is first raised to the natural air pressure, and after an interval of 0.8s, the negative pressure of the second cavity area 12 is raised to the natural air pressure.
[0057] The above description is merely a preferred embodiment of the present invention and does not limit the implementation and protection scope of the present invention. Those skilled in the art should realize that any equivalent substitutions and obvious changes made based on the description and illustrations of the present invention should be included within the protection scope of the present invention.
Claims
1. A vacuum cutting stage, applied to a metal film to be cut, the metal film to be cut including a retention area and a removal area, characterized in that, include: A platform base, comprising a platform base and a support member disposed above the platform base, wherein the platform base and the support member enclose an internal space, and the support surface of the support member is used to place the metal film to be cut. The internal space includes a first cavity region and a second cavity region that are isolated from each other by a first seal. The second cavity region is an annular region, and the first cavity region is located within the area enclosed by the second cavity region. The size of the first cavity region matches the size of the retention region, and the size of the second cavity region matches the size of the removal region, so that when the metal film to be cut is placed on the bearing surface of the carrier, the retention region is aligned with the first cavity region, and the removal region is aligned with the second cavity region. The support member has multiple ventilation holes for applying negative pressure from the first cavity region to the retention region and applying negative pressure from the second cavity region to the removal region. An exhaust mechanism is provided, wherein the exhaust end of the exhaust mechanism extends to the first cavity region and the second cavity region respectively, for extracting gas from the first cavity region and the second cavity region respectively, so as to control the negative pressure in the first cavity region to be less than the negative pressure in the second cavity region.
2. The vacuum cutting stage according to claim 1, characterized in that, Also includes: A first negative pressure gauge is installed in the first cavity region to obtain the current negative pressure value in the first cavity region; A second negative pressure gauge is installed in the second cavity region to obtain the current negative pressure value in the second cavity region; The host computer is connected to the first negative pressure gauge, the second negative pressure gauge, and the exhaust mechanism, respectively. It is used to control the exhaust mechanism to extract air from the first cavity area and the second cavity area respectively according to the negative pressure difference between the current negative pressure value in the first cavity area and the current negative pressure value in the second cavity area, so as to keep the negative pressure difference within a preset negative pressure range, and the negative pressure in the first cavity area is less than the negative pressure in the second cavity area.
3. The vacuum cutting stage according to claim 1, characterized in that, The internal space includes a first isolation slot and a second isolation slot; It also includes a second seal; The first isolation groove is disposed between the first cavity region and the second cavity region; The second isolation groove is disposed at the outer periphery of the second cavity region; The first sealing element is connected to the first isolation groove to isolate the gas flow between the first cavity region and the second cavity region; The second seal is connected to the second isolation groove to isolate the second cavity area from the external gas flow.
4. The vacuum cutting stage according to claim 3, characterized in that, The width of the first isolation groove and the width of the second isolation groove are both 1 mm.
5. The vacuum cutting stage according to claim 1, characterized in that, The carrier includes: A vacuum adsorption plate, wherein the vacuum adsorption plate has a plurality of air vents corresponding to the first cavity region and the second cavity region respectively; A soft pad, the lower surface of which is fixedly connected to the upper surface of the vacuum adsorption plate, the upper surface of which serves as the bearing surface.
6. The vacuum cutting stage according to claim 5, characterized in that, The diameter of each vent hole on the vacuum adsorption plate is 0.3mm to 0.5mm, and the distance between each adjacent vent hole is 4mm.
7. The vacuum cutting stage according to claim 5, characterized in that, The thickness of the cushion is 1.0mm to 1.5mm.
8. The vacuum cutting stage according to claim 1, characterized in that, The annular width of the second cavity region is 4mm to 5mm.
9. A vacuum cutting method applied to a metal film to be cut, the metal film to be cut comprising a retention area and a removal area, characterized in that, The method of using a vacuum cutting stage as described in any one of claims 1-8 to support the metal film to be cut includes: Step S1: Place the metal film to be cut on the bearing surface of the carrier, with the retained area aligned with the first cavity area and the removed area aligned with the second cavity area; In step S2, the exhaust mechanism extracts gas from the first cavity region and the second cavity region respectively to maintain the negative pressure in the first cavity region being less than the negative pressure in the second cavity region.
10. The vacuum cutting method according to claim 9, characterized in that, A first negative pressure gauge is installed in the first cavity region, a second negative pressure gauge is installed in the second cavity region, and a host computer is installed, which is connected to the first negative pressure gauge, the second negative pressure gauge and the exhaust mechanism respectively; Step S2 includes: Step S21: The host computer obtains the current negative pressure value in the first cavity area through the first negative pressure gauge, and obtains the current negative pressure value in the second cavity area through the second negative pressure gauge; Step S22: The host computer processes and obtains the negative pressure difference between the current negative pressure value in the first cavity area and the current negative pressure value in the second cavity area; In step S23, the host computer controls the exhaust mechanism to extract air from the first cavity area and the second cavity area respectively according to the negative pressure difference, so as to keep the negative pressure difference within a preset negative pressure range, and the negative pressure in the first cavity area is less than the negative pressure in the second cavity area.