A Simulation Calculation Method for Magnetic Properties of Transformer Core Based on Equivalent Model
The simulation calculation method for the magnetic properties of transformer cores based on equivalent models solves the problem of accuracy in calculating the no-load loss and no-load current of transformer cores, achieving higher calculation accuracy and shorter calculation time, and is suitable for predicting the no-load performance of transformer cores.
Patent Information
- Application Number
- CN202611204990.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-10
- Publication Date
- 2026-11-10
AI Technical Summary
Existing technologies cannot accurately calculate the no-load loss and no-load current of transformer cores. Traditional methods have significant deviations, especially in the loss verification process of new core structures. Furthermore, existing finite element simulation calculations cannot accurately obtain magnetic performance parameters.
A simulation method for the magnetic properties of transformer cores based on an equivalent model is adopted. By obtaining the structural parameters of the core and the test parameters of the sample, a single-stack periodic model is established, the boundaries of the joint zone, stress zone and uniform zone are determined, and material properties are assigned to them respectively. The equivalent model of the core partition is established for simulation, taking into account the effects of stress and joints.
While ensuring computational accuracy, the model size is reduced, the computation time is shortened, the actual structure is simulated, and the accuracy of the simulation results is improved, with a computational error of less than 10%.
Smart Images

Figure CN123069653A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of transformer core magnetic property calculation technology, and in particular to a method for simulating and calculating the magnetic properties of transformer cores based on an equivalent model. Background Technology
[0002] No-load loss and no-load current are core electrical performance indicators of transformer cores, and the core joint structure and internal material stress are key factors determining no-load performance. Currently, there is no mature and accurate quantitative calculation system for no-load current; while in engineering, the classic formula of process coefficient × silicon steel ratio × core mass is commonly used to calculate core no-load loss. However, the process coefficient is obtained through statistical fitting of measured engineering data, and the calculated results often deviate significantly from the measured data. This problem is even more pronounced in the loss verification process of new core structures.
[0003] To more accurately predict the no-load performance of iron cores, finite element simulation is introduced to construct a computational model that more closely resembles the actual physical process. This compensates for the inherent bias in the statistical fitting of process coefficients in traditional analytical methods, providing more reliable numerical support for the prediction of no-load losses and currents in novel iron core structures. However, existing solutions have significant shortcomings: such as... Figure 1 As shown, due to its structural characteristics, the iron core has three different regions: the joint region, the stress-affected region, and the uniform region. The magnetic properties parameters corresponding to these three regions are different, and conventional testing methods cannot accurately obtain them, resulting in a large deviation between the simulation results calculated by finite element simulation and the measured values. Summary of the Invention
[0004] To address the shortcomings of the prior art, the purpose of this invention is to provide a simulation calculation method for the magnetic properties of transformer cores based on an equivalent model, in order to solve one or more problems in the prior art.
[0005] To achieve the above objectives, the technical solution of the present invention is as follows: A simulation calculation method for the magnetic properties of transformer cores based on an equivalent model includes the following steps: Obtain the core structure parameters and core sample testing parameters; A single-stack periodic model was established based on the core structure parameters; Simulation of a single-stack periodic model was performed to obtain a magnetic flux density distribution map; Determine the boundary data of the joint area based on the magnetic flux density distribution map; Determine the stress zone boundary data based on the test parameters of the iron core sample; Based on the boundary data of the stress zone and the boundary data of the joint zone, the equivalent zone of the joint, the equivalent zone of the stress, and the uniform zone are determined. Determine the material properties corresponding to the joint equivalent region, stress equivalent region, and uniform region respectively; A core partition equivalent model is established based on the core structure parameters, joint equivalent zone, stress equivalent zone, uniform zone, and corresponding material properties. The equivalent model of the core partition is simulated to obtain the predicted no-load loss and no-load current.
[0006] The above technical solution includes a uniform region, a stress equivalent region, and a joint equivalent region. It also considers the impact of stress and joints on no-load performance, and eliminates the need for detailed modeling. This significantly reduces the model size and shortens the calculation time while ensuring calculation accuracy.
[0007] Furthermore, the establishment of a single-stack periodic model based on the core structure parameters includes the following steps: Extract the primary silicon steel parameters from the core structure parameters and remove the through-hole parameters to obtain simplified parameters; A single-stack iron core model was established based on simplified parameters; Periodic boundary conditions are added to the upper and lower surfaces of the single-stack iron core model to form a single-stack periodic model.
[0008] With the above technical solution, the main stage accounts for a high proportion of the mass of the entire iron core. The data obtained by modeling the main stage separately is closest to the overall accuracy. Compared with modeling all stages of the iron core, the simulation time is greatly reduced, but the results will not deviate too much.
[0009] Furthermore, simulations are performed on the single-stack periodic model to obtain the magnetic flux density distribution map, including the following steps: The single-stack periodic model is simulated to obtain the magnetic flux data of the entire stack of iron cores. The simulation data of the top or bottom silicon steel sheet is extracted from the magnetic flux data of the entire stack of iron cores as a magnetic flux density distribution map.
[0010] With the above technical solution, the silicon steel sheets at the top or bottom are more affected by the missing corners. Selecting the top or bottom silicon steel sheets will result in the most obvious change in magnetic flux at the joint, which is more conducive to accurately determining the joint boundary.
[0011] Furthermore, determining the joint area boundary data based on the magnetic flux density distribution map includes the following steps: The magnetic flux density distribution map is divided into n regions at fixed intervals along the width of the iron core sheet; In each region, magnetic flux density values are extracted sequentially from the uniform area towards the centerline of the joint along the rolling direction to obtain the magnetic flux density waveform that varies with distance. The magnetic flux density value of the uniform region is determined as the standard value; Points are sequentially selected along the magnetic flux density waveform, and it is determined whether the change in magnetic flux density between the selected point and the standard value is greater than 0.1T. If it is not greater than, continue to take points along the magnetic flux density waveform; If the value is greater than 1, then the point is the boundary point between the uniform area and the seam area in the corresponding region. After determining the boundary points of n regions, a straight line is obtained by fitting all the boundary points, which is the boundary data of the seam area.
[0012] Furthermore, the establishment of the equivalent model for the iron core partition includes the following steps: A multi-level core model is established based on the core structure parameters. Each level of core has multiple layers of silicon steel sheets. The multiple layers of silicon steel sheets of the same level of core are offset sequentially according to the preset step amount. On the multi-level core model, joint equivalent zone, stress equivalent zone and uniform zone are set, and corresponding material properties are assigned to them to form a core partition equivalent model.
[0013] Using the above technical solution, each layer of silicon steel sheet is modeled according to the step size, which can simulate the missing corner inside the iron core joint and the magnetic concentration phenomenon formed therefrom, which is more in line with the actual physical structure.
[0014] Furthermore, determining the material properties corresponding to the joint equivalent region, stress equivalent region, and uniform region respectively includes the following steps: Obtain typical BP and BH curves of silicon steel materials for current cores, and use them as material properties in the uniform region; The first coefficients of the joint equivalent zone and the uniform zone are obtained through a pre-set first test. The material properties of the joint equivalent zone are calculated based on the material properties of the uniform zone and the first coefficients. The second coefficients of the stress equivalent region and the uniform region are obtained through a pre-set second test. The material properties of the stress equivalent region are calculated based on the material properties of the uniform region and the second coefficients.
[0015] The material property curves of the joint equivalent zone and stress equivalent zone obtained by the above technical solution through the first and second coefficients are closer to the performance curves of silicon steel materials in the actual operation of the iron core.
[0016] Furthermore, the first experiment includes the following steps: The first single-phase iron core was stacked and the BPa and BHa curves of the first single-phase iron core were obtained by testing; The first single-phase iron core was cut and reassembled into a second single-phase iron core with the same joint structure, and the BPb and BHb curves corresponding to the second single-phase iron core were obtained by testing. The cutting process for the first single-phase iron core involves cutting the large trapezoidal silicon steel sheet constituting the first single-phase iron core into multiple smaller trapezoidal silicon steel sheets of the same shape, wherein the number of smaller trapezoidal sheets is m times the number of larger trapezoidal sheets. Based on the proportions of the joint area and the uniform area, and the BP and BH curves of the first single-phase core and the second single-phase core, the BP and BH curves corresponding to the joint area and the uniform area are calculated respectively, and then the first coefficient is determined.
[0017] The above technical solution allows for the calculation of the first coefficient corresponding to the joint area based on the same material, thus avoiding deviations caused by material fluctuations.
[0018] Furthermore, the second test includes the following steps: The global stress influence coefficient at the mesoscale is obtained by measuring silicon steel sheets using a magnetic domain observation device. The magnetic properties of the material before and after longitudinal shearing are obtained by using an online longitudinal shearing measurement device, and the local stress influence coefficient at the macroscopic scale is calculated. The global stress influence coefficient is corrected by the local stress influence coefficient to obtain the second coefficient.
[0019] With the above technical solution, data at the mesoscale can be directly obtained through magnetic domain observation equipment, while data at the macroscale can only be detected locally by selecting a few magnetic density points through longitudinal shearing online measurement equipment. Therefore, correcting macroscopic data with mesoscale data can improve the accuracy of coefficients and shorten the detection time.
[0020] Compared with the prior art, the beneficial technical effects of the present invention are as follows: 1. The model includes a uniform region, a stress equivalent region, and a joint equivalent region. It considers the impact of stress and joints on no-load performance, and does not require detailed modeling. This significantly reduces the model size and shortens the calculation time while ensuring calculation accuracy.
[0021] 2. It closely matches the actual engineering structure, and models the structure in layers according to the number of steps and the step amount to simulate the phenomena of missing corners in stacked structures and magnetic concentrating; but it does not lead to a significant increase in the overall computational load. Attached Figure Description
[0022] Figure 1 A schematic diagram of the partitioning of the transformer core is shown.
[0023] Figure 2 A flowchart of the simulation calculation method for the magnetic properties of transformer cores based on an equivalent model, provided by an embodiment of the present invention, is shown.
[0024] Figure 3 The magnetic flux density distribution diagram of the single-stack iron core model provided in the embodiment of the present invention is shown.
[0025] Figure 4 The simulated and experimental values of transformer core no-load loss provided by the embodiments of the present invention are shown.
[0026] Figure 5 The simulated and experimental values of the transformer core no-load current provided in the embodiments of the present invention are shown. Detailed Implementation
[0027] A simulation calculation method for the magnetic properties of transformer cores based on an equivalent model, see [link to relevant documentation]. Figure 2 This includes the following steps: S100: Obtain the core structure parameters and core sample test parameters.
[0028] S200. Establish a single-stack periodic model based on the core structure parameters.
[0029] S300. Simulate the single-stack periodic model to obtain the magnetic flux density distribution map.
[0030] S400. Determine the boundary data of the joint area based on the magnetic flux density distribution map.
[0031] S500. Determine the stress zone boundary data based on the core sample test parameters.
[0032] S600. Based on the stress zone boundary data and the joint zone boundary data, determine the joint equivalent zone, stress equivalent zone, and uniform zone.
[0033] S700, determine the material properties corresponding to the joint equivalent zone, stress equivalent zone and uniform zone respectively.
[0034] S800. Based on the core structure parameters, joint equivalent zone, stress equivalent zone, uniform zone, and corresponding material properties, establish a core partition equivalent model.
[0035] S900, simulate the equivalent model of the core partition to obtain the predicted no-load loss and no-load current.
[0036] In step S100, the core structure parameters include the core window height, center distance, sheet width, number of stages, thickness of each stage, step size, number of steps, and diameter of the through hole.
[0037] The core sample testing parameters are obtained by observing the sheared silicon steel sheet sample with a magnetic domain observation device to obtain magnetic domain distribution data from the sheared edge to the interior region of the sample.
[0038] In step S200, a single-stack periodic model is established based on the core structure parameters, specifically including the following steps: S210. Extract the main silicon steel parameters from the core structure parameters and remove the through-hole parameters to obtain simplified parameters.
[0039] S220. Establish a single-stack iron core model based on simplified parameters.
[0040] S230. Add periodic boundary conditions to the upper and lower surfaces of the single-stack iron core model to form a single-stack periodic model.
[0041] Since the perforation affects the stress of the core, its magnetic domain distribution data is also recorded in the core sample testing parameters. This step is mainly to prepare for the subsequent determination of the joint area, so it is necessary to eliminate the interference of the perforation, that is, to establish a single-stack periodic model without the perforation. The principal stage parameter is selected during modeling because the principal stage accounts for the largest proportion in the entire core, and its simulation results are closest to the overall core model compared to other stages.
[0042] In step S300, the single-stack periodic model is simulated to obtain the magnetic flux density distribution map, which specifically includes the following steps: S310. Simulate the single-stack periodic model to obtain the magnetic flux data of the entire stack of iron cores; S320. Extract the simulation data of the top or bottom silicon steel sheet from the magnetic flux data of the entire stack of iron cores as a magnetic flux density distribution map.
[0043] When simulating a single-stack periodic model, the simulation software generates magnetic flux data for the entire stack of iron cores. However, this data is too large for determining the subsequent joint area. Considering that the joint structure of iron cores of the same level is consistent, to reduce redundant calculations, only the simulation data of the top or bottom silicon steel sheet is selected.
[0044] Magnetic flux density distribution diagram as follows Figure 3 As shown, the magnetic flux density distribution in the uniform region is uniform and consistent with the design magnetic flux density value of the iron core. However, due to the change in magnetic circuit length and the phenomenon of magnetic flux passing through the plates, the magnetic flux density in the joint-affected area accumulates, with the magnetic flux density increasing at the inner corner.
[0045] In step S400, the boundary data of the joint area is determined based on the magnetic flux density distribution map, including the following steps: S410. Divide the magnetic flux density distribution map into n regions at fixed intervals along the width of the core sheet. S420. In each region, extract the magnetic flux density value sequentially from the uniform area to the joint centerline along the rolling direction to obtain the magnetic flux density waveform that varies with distance. S430. Determine the magnetic flux density value of the uniform region as the standard value; S440. Take points sequentially along the magnetic flux density waveform, and determine whether the change in magnetic flux density between the selected point and the standard value is greater than 0.1T. S450, if not greater than, continue to take points along the magnetic flux density waveform; S460. If it is greater than 0, then the point is the boundary point between the uniform area and the joint area in the corresponding region. S470. After determining the boundary points of n regions, fit all the boundary points to obtain a straight line, which is the boundary data of the seam area.
[0046] The rolling direction of the silicon steel core sheet is its length direction. Since the magnetic flux density waveform is taken from the uniform region towards the centerline of the joint, the initial position of the waveform must be in the uniform region, and the ending position of the waveform must be in the joint region. Therefore, in step S430, the magnetic flux density value at the initial position of the waveform can be directly used as the standard value, or the average value of all magnetic flux density values within a preset range from the initial position of the waveform can be used as the standard value.
[0047] In step S420, the centerline of each region in its width direction is used as the extraction position of the magnetic flux density waveform. In step S440, points are then sequentially extracted from the uniform region towards the seam centerline along the rolling direction at preset intervals in the magnetic flux density waveform.
[0048] In step S470, all boundary points need to be fitted into a straight line. The more boundary points there are, the closer the fitted line is to the actual joint boundary; however, the more boundary points there are, the more loop judgment logic is required for the corresponding magnetic flux density value. To balance accuracy and calculation speed, in this embodiment, the number of regions n must be greater than or equal to 10, and the corresponding fixed interval is between 5-10 mm.
[0049] In step S500, the magnetic domain morphology in the stress-affected region is irregular, while the magnetic domain shape in the uniform region is regular. The magnetic domain distribution data of the core sample is directly displayed in the core sample testing parameters. Therefore, determining the stress zone boundary data based on the core sample testing parameters means finding the boundary between the irregular domains and the regular strip-shaped domains, which is the boundary between the stress zone and the uniform region.
[0050] In step S700, the material properties corresponding to the joint equivalent region, stress equivalent region, and uniform region are determined respectively, specifically including the following steps: S710. Obtain the typical BP and BH curves of the silicon steel material of the current core, and use them as material properties in the uniform region. S720. Obtain the first coefficients of the joint equivalent zone and the uniform zone through a preset first test, and calculate the material properties of the joint equivalent zone based on the material properties of the uniform zone and the first coefficients. S730. Obtain the second coefficients of the stress equivalent region and the uniform region through a preset second test, and calculate the material properties of the stress equivalent region based on the material properties of the uniform region and the second coefficients.
[0051] Typical BP and BH curves for silicon steel materials are provided by the supplier or obtained by testing the corresponding silicon steel materials using a single-piece tester or Epstein square.
[0052] By conducting pre-set experiments, the relationship between the material properties in the joint zone and the uniform zone, as well as the relationship between the material properties in the stress zone and the uniform zone, are determined. Then, two specific virtual materials equivalent to the material properties in the joint zone and the stress zone are generated in the simulation software for use in the subsequent establishment of the core partition equivalent model.
[0053] It should be noted that there is no specific order between steps S700 and S600, and step S700 can be conducted independently. However, the subsequent step S800 can only begin after steps S500 and S600 have been completed.
[0054] In one embodiment, the first trial includes the following steps: S721. Stack the first single-phase iron core and test to obtain the BPa and BHa curves of the first single-phase iron core; S722. The first single-phase iron core is cut and reassembled into a second single-phase iron core with the same joint structure, and the BPb and BHb curves corresponding to the second single-phase iron core are obtained by testing. S723. Based on the proportions of the joint area and the uniform area, the BPa and BHa curves, and the BPb and BHb curves, calculate the BP and BH curves corresponding to the joint area and the uniform area respectively, and then determine the first coefficient.
[0055] The first and second single-phase cores have identical structures, differing only in sheet length. The volume ratio of the uniform region and the joint region within the core can be determined based on the boundary of the joint-affected area. Two linear equations in two variables are then established to derive the BP and BH curves corresponding to the joint region and the uniform region, respectively. Finally, the first coefficient can be obtained based on the ratio of the BP and BH curves corresponding to the joint region and the uniform region.
[0056] The equation is as follows:
[0057] After solving, we get:
[0058] Where c and d represent the volume percentages of the joint area and uniform area of the first single-phase core, respectively; e and f represent the volume percentages of the joint area and uniform area of the second single-phase core, respectively; X j and X u X represents the unit loss or magnetic field strength of the joint region and the uniform region corresponding to a certain magnetic flux density, respectively; a and X b These are the unit losses or magnetic field strengths of the first and second single-phase iron cores corresponding to a certain magnetic flux density, which can be directly obtained from the measured BPa or BHa curves, BPb or BHb curves.
[0059] In addition, the first single-phase core must be consistent with the core to be simulated in terms of joint structure.
[0060] The cutting process for the first single-phase core involves cutting the large trapezoidal silicon steel sheet constituting the first single-phase core into multiple smaller trapezoidal silicon steel sheets of the same shape, with the number of smaller trapezoidal sheets being m times the number of larger trapezoidal sheets. Correspondingly, the thickness of the second single-phase core is m times that of the first single-phase core.
[0061] In one embodiment, the second trial includes the following steps: S731. Obtain the global stress influence coefficient at the mesoscopic scale by measuring silicon steel sheets using a magnetic domain observation device; S732. Obtain material magnetic property data before and after longitudinal shearing using an online longitudinal shearing measurement device and calculate the local stress influence coefficient at the macroscopic scale. S733. The global stress influence coefficient is corrected by the local stress influence coefficient to obtain the second coefficient.
[0062] In this embodiment, the online longitudinal shearing measurement device is an online iron loss measuring instrument.
[0063] The local stress influence coefficient is obtained by comparing the material's magnetic properties before longitudinal cutting (i.e., the material's magnetic properties in the uniform region unaffected by stress) with the material's magnetic properties after longitudinal cutting (i.e., the material's magnetic properties in the stress region after stress influence).
[0064] The global stress influence coefficient is the ratio of the performance of any uniform region to the average performance of the stress region from a mesoscopic perspective.
[0065] The global stress influence coefficient obtained at the mesoscale is affected by size and only represents the results of the test area. The local stress influence coefficient, however, is the average value of the test results for the entire roll of silicon steel. Therefore, the final second coefficient needs to be corrected for the global stress influence coefficient using the local stress influence coefficient, so that the second coefficient can more accurately represent the entire roll of silicon steel.
[0066] In step S800, an equivalent model of the iron core partition is established, which specifically includes the following steps: S810. Establish a multi-level core model based on the core structure parameters. For each level of core, establish multiple layers of silicon steel sheets. The multiple layers of silicon steel sheets of the same level of core are offset sequentially according to the preset step amount. S820. Set up a joint equivalent zone, a stress equivalent zone, and a uniform zone on the multi-level core model, and assign corresponding material properties to each zone to form a core partition equivalent model.
[0067] Multi-stage core models can be built by establishing only symmetrical models based on symmetry, which can save equipment resources and calculation time in simulation calculations; when the high and low voltage sides are asymmetrical, 1 / 4 models of the high voltage side and 1 / 4 models of the low voltage side are built respectively; when the high and low voltage sides are symmetrical, only 1 / 4 models of the high voltage side or 1 / 4 models of the low voltage side are built.
[0068] Furthermore, by using step offsets to create missing corners that more closely resemble the actual structure, the data simulated by the core partition equivalent model is closer to the actual measured values.
[0069] See Figure 4 , Figure 5 The simulation results were verified by conducting experiments on multiple transformer cores. The results show that the average calculation error of no-load loss in the unpartitioned simulation model is 21%, and the average calculation error of no-load current is 36%; the calculation error of no-load loss in the partitioned equivalent simulation model is less than 6%, and the calculation error of no-load current is less than 10%, indicating that its calculation accuracy meets the requirements of engineering design.
[0070] Furthermore, for a conventional three-phase three-column transformer core, the calculation time for a single-piece simulation model containing only 5 stacks of silicon steel sheets is more than 6 hours; while the partitioned equivalent simulation model, even if the entire core model is built, only takes 5-15 minutes to calculate, which can save calculation time while ensuring the accuracy of the model calculation.
[0071] The technical features of the above embodiments can be combined in any way. For the sake of brevity, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0072] The embodiments described above are merely illustrative of several implementations of the present invention, and while the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the invention patent. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of the present invention, and these all fall within the protection scope of the present invention. Therefore, the protection scope of this invention patent should be determined by the appended claims.
Claims
1. A simulation calculation method for the magnetic properties of transformer cores based on an equivalent model, characterized in that, Includes the following steps: Obtain the core structure parameters and core sample testing parameters; A single-stack periodic model was established based on the core structure parameters; Simulation of a single-stack periodic model was performed to obtain a magnetic flux density distribution map; Determine the boundary data of the joint area based on the magnetic flux density distribution map; Determine the stress zone boundary data based on the test parameters of the iron core sample; Based on the boundary data of the stress zone and the boundary data of the joint zone, the equivalent zone of the joint, the equivalent zone of the stress, and the uniform zone are determined. Determine the material properties corresponding to the joint equivalent region, stress equivalent region, and uniform region respectively; A core partition equivalent model is established based on the core structure parameters, joint equivalent zone, stress equivalent zone, uniform zone, and corresponding material properties. The equivalent model of the core partition is simulated to obtain the predicted no-load loss and no-load current.
2. The method for simulating and calculating the magnetic properties of a transformer core based on an equivalent model as described in claim 1, characterized in that: The establishment of a single-stack period model based on the core structure parameters includes the following steps: Extract the primary silicon steel parameters from the core structure parameters and remove the through-hole parameters to obtain simplified parameters; A single-stack iron core model was established based on simplified parameters; Periodic boundary conditions are added to the upper and lower surfaces of the single-stack iron core model to form a single-stack periodic model.
3. The method for simulating and calculating the magnetic properties of a transformer core based on an equivalent model as described in claim 2, characterized in that: To obtain the magnetic flux density distribution map, a simulation of a single-stack periodic model is performed, including the following steps: The single-stack periodic model is simulated to obtain the magnetic flux data of the entire stack of iron cores. The simulation data of the top or bottom silicon steel sheet is extracted from the magnetic flux data of the entire stack of iron cores as a magnetic flux density distribution map.
4. The method for simulating and calculating the magnetic properties of a transformer core based on an equivalent model as described in claim 1, characterized in that, Determining the boundary data of the joint area based on the magnetic flux density distribution map includes the following steps: The magnetic flux density distribution map is divided into n regions at fixed intervals along the width of the iron core sheet; In each region, magnetic flux density values are extracted sequentially from the uniform area towards the centerline of the joint along the rolling direction to obtain the magnetic flux density waveform that varies with distance. The magnetic flux density value of the uniform region is determined as the standard value; Points are sequentially selected along the magnetic flux density waveform, and it is determined whether the change in magnetic flux density between the selected point and the standard value is greater than 0.1T. If it is not greater than, continue to take points along the magnetic flux density waveform; If the value is greater than 1, then the point is the boundary point between the uniform area and the seam area in the corresponding region. After determining the boundary points of n regions, a straight line is obtained by fitting all the boundary points, which is the boundary data of the seam area.
5. The method for simulating and calculating the magnetic properties of a transformer core based on an equivalent model as described in claim 1, characterized in that, The establishment of the equivalent model for the iron core partition includes the following steps: A multi-level core model is established based on the core structure parameters. Each level of core has multiple layers of silicon steel sheets. The multiple layers of silicon steel sheets of the same level of core are offset sequentially according to the preset step amount. On the multi-level core model, joint equivalent zone, stress equivalent zone and uniform zone are set, and corresponding material properties are assigned to them to form a core partition equivalent model.
6. The method for simulating and calculating the magnetic properties of a transformer core based on an equivalent model as described in claim 1, characterized in that, The determination of the material properties corresponding to the joint equivalent region, stress equivalent region, and uniform region includes the following steps: Obtain typical BP and BH curves of silicon steel materials for current cores, and use them as material properties in the uniform region; The first coefficients of the joint equivalent zone and the uniform zone are obtained through a pre-set first test. The material properties of the joint equivalent zone are calculated based on the material properties of the uniform zone and the first coefficients. The second coefficients of the stress equivalent region and the uniform region are obtained through a pre-set second test. The material properties of the stress equivalent region are calculated based on the material properties of the uniform region and the second coefficients.
7. The method for simulating and calculating the magnetic properties of a transformer core based on an equivalent model as described in claim 6, characterized in that, The first test includes the following steps: The first single-phase iron core was stacked and the BPa and BHa curves of the first single-phase iron core were obtained by testing; The first single-phase iron core was cut and reassembled into a second single-phase iron core with a consistent joint structure, and the BPb and BHb curves corresponding to the second single-phase iron core were obtained by testing. The cutting process for the first single-phase iron core involves cutting the large trapezoidal silicon steel sheet constituting the first single-phase iron core into multiple smaller trapezoidal silicon steel sheets of the same shape, wherein the number of smaller trapezoidal sheets is m times the number of larger trapezoidal sheets. Based on the proportions of the joint area and the uniform area, and the BP and BH curves of the first single-phase core and the second single-phase core, the BP and BH curves corresponding to the joint area and the uniform area are calculated respectively, and then the first coefficient is determined.
8. The method for simulating and calculating the magnetic properties of a transformer core based on an equivalent model as described in claim 6, characterized in that, The second test includes the following steps: The global stress influence coefficient at the mesoscale is obtained by measuring silicon steel sheets using a magnetic domain observation device. The magnetic properties of the material before and after longitudinal shearing are obtained by using an online longitudinal shearing measurement device, and the local stress influence coefficient at the macroscopic scale is calculated. The global stress influence coefficient is corrected by the local stress influence coefficient to obtain the second coefficient.