Display module, display device, and method for manufacturing display module

By using a curable material to create an electromagnetic shielding structure in the flexible circuit board and bonding area, the problem of traditional materials being unable to fully cover the surface in extremely narrow or zero-bezel designs is solved, achieving efficient electromagnetic shielding and reliability.

CN123072289APending Publication Date: 2026-11-10BOE TECHNOLOGY GROUP CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611301374.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-25
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

In ultra-narrow bezel or zero-bezel designs, traditional copper foil or conductive cloth cannot completely cover the flexible circuit board and bonding area, resulting in reduced electromagnetic shielding effect and poor contact conductivity reliability.

Method used

An electromagnetic shielding structure made of curable materials is formed by spraying or coating processes to create insulating and conductive layers on the flexible circuit board and bonding area, covering the flexible circuit board and bonding area, and extending into the bending area to form a continuous shielding structure.

Benefits of technology

With extremely narrow or zero bezels, complete coverage of the flexible circuit board and bonding area is achieved, improving electromagnetic shielding effect and reliability, and avoiding problems such as poor contact or disconnection.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123072289A_ABST
    Figure CN123072289A_ABST
Patent Text Reader

Abstract

This invention provides a display module, a display device, and a method for manufacturing the display module. The display module includes a display panel and a flexible circuit board. The display panel includes a display area, a bending area, and a bonding area connected in sequence. The bending area is bent such that the bonding area bends to the backlight side of the display area. The flexible circuit board is bonded to the bonding area and is located on the backlight side of the display area. The display module also includes an electromagnetic shielding structure that covers the flexible circuit board and the bonding area. The electromagnetic shielding structure is made of a curable material. The display module provided by this disclosure uses a curable material for its electromagnetic shielding structure, which can be precisely applied through dispensing, spraying, or coating processes. Even in spaces with extremely narrow bezels or zero bezels, it can still cover the flexible circuit board, the bonding area, and even the bending area, improving the shielding effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of display product manufacturing technology, and in particular to a display module, a display device, and a method for manufacturing a display module. Background Technology

[0002] In current mid-to-high-end OLED panel module manufacturing processes, back-side electromagnetic interference (EMI) shielding has become a standard feature in reliability design. Because OLED pixel driving uses a high-current, high-frequency scanning method, the back of the panel radiates broadband noise. If not suppressed, this noise can interfere with adjacent modules such as touchscreens, cameras, and antennas, and may also exceed electromagnetic compatibility (EMC) standards during FCC / CE certification processes. In traditional solutions, copper foil and conductive cloth have quickly become the preferred choice for panel manufacturers due to their high conductivity, flexibility, and ease of die-cutting. Applying copper foil / conductive cloth to the metal support or heat-dissipating copper foil on the back of the OLED module forms a three-layer stacked structure: heat dissipation layer → shielding layer → structural component. This structure satisfies EMC requirements while keeping the thickness increment within 0.05 mm, making it a common design paradigm for flagship smartphones, smart wearables, and automotive OLEDs.

[0003] However, as full-screen displays approach the limit of zero bezels (ultra-narrow bezels), the available wrap-around area for OLED modules is compressed to less than 0.3 mm, leaving no physical space for traditional full-surface lamination solutions using copper foil or conductive cloth. Due to the limited lamination area, copper foil or conductive cloth can no longer form a complete Faraday cage structure, resulting in a significant decrease in electromagnetic shielding effectiveness. Furthermore, the reliability of contact and conductivity between the copper foil and the exposed copper grounding area on the flexible printed circuit board (FPC) is difficult to guarantee, easily leading to poor contact or disconnection, further affecting shielding effectiveness. Summary of the Invention

[0004] To address the aforementioned technical problems, this invention provides a display module, a display device, and a method for manufacturing the display module, solving the problem that traditional copper foil or conductive cloth cannot completely cover the screen, resulting in incomplete shielding.

[0005] To achieve the above objectives, the technical solution adopted in the embodiments of the present invention is: a display module, including a display panel and a flexible circuit board;

[0006] The display panel includes a display area, a bending area, and a bonding area connected in sequence, wherein the bending area bends so that the bonding area bends to the backlight side of the display area;

[0007] The flexible circuit board is bonded to the bonding area, and the flexible circuit board is located on the backlight side of the display area;

[0008] The display module also includes an electromagnetic shielding structure, which covers the flexible circuit board and the bonding area.

[0009] The electromagnetic shielding structure is made of a curable material.

[0010] In some embodiments, the electromagnetic shielding structure includes a stacked insulating layer and a first conductive layer;

[0011] A driver chip is disposed on the side of the bonding area away from the display area, and the insulating layer at least covers the driver chip;

[0012] The first conductive layer is located on the side of the insulating layer away from the flexible circuit board, and the first conductive layer is electrically connected to the exposed copper area on the flexible circuit board.

[0013] In some embodiments, the conductive layer is made of conductive adhesive, conductive paint, or conductive silver paste;

[0014] The insulating layer is made of a curable material.

[0015] In some embodiments, the first conductive layer covers the flexible circuit board and the bonding area, and the first conductive layer extends in a first direction to at least cover a portion of the bending area, the first direction being parallel to the light-emitting surface of the display area.

[0016] In some embodiments, the flexible circuit board includes a substrate layer, a second conductive layer and a first cover film are sequentially stacked on a first surface of the substrate layer, and a third conductive layer and a second cover film are sequentially stacked on a second surface of the substrate layer.

[0017] The second conductive layer is bonded to the bonding area, and the electromagnetic shielding structure is located on the side of the second cover film away from the base layer.

[0018] In some embodiments, a cover plate is also included on the light-emitting side of the display panel, the display panel includes a border area located around the display area, and the display module further includes an edge sealing structure located in the border area;

[0019] The edge sealing structure includes a first retaining wall, a second retaining wall, and a filling layer. The first retaining wall is located on the side of the cover plate closer to the display panel, the second retaining wall is located on the side of the display panel away from the cover plate, and the filling layer fills the space formed by the first retaining wall, the second retaining wall, the display panel, and the cover plate.

[0020] The orthographic projection of the edge sealing structure onto the cover plate completely covers the orthographic projection of the bending area onto the cover plate.

[0021] In some embodiments, the electromagnetic shielding structure extends in a first direction to cover a portion of the sealing structure.

[0022] In some embodiments, the first retaining wall, the second retaining wall, and the filling layer are all made of a curable adhesive, and the adhesive used for the first retaining wall and the second retaining wall has a higher tackiness than the adhesive used for the filling layer.

[0023] This disclosure also provides a method for manufacturing a display module, used to manufacture the above-mentioned display module, the method comprising the following steps:

[0024] A display panel and a flexible circuit board are provided for bonding connection. The display panel includes a display area, a bending area, and a bonding area connected in sequence. The bending area is bent such that the bonding area bends to the backlight side of the display area. The flexible circuit board is bonded to the bonding area and is located on the backlight side of the display area.

[0025] An electromagnetic shielding structure is formed on the flexible circuit board and the bonding area using a spraying or coating process.

[0026] In some embodiments, the electromagnetic shielding structure includes a stacked insulating layer and a first conductive layer; a driver chip is disposed on the side of the bonding area away from the display area;

[0027] The process of forming an electromagnetic shielding structure on the flexible circuit board and the bonding area using a spraying or coating process specifically includes:

[0028] The insulating layer is formed by dispensing, spraying, or coating processes and then cured, with the insulating layer covering the driver chip.

[0029] The first conductive layer is formed by dispensing, spraying, or coating processes and then cured. The first conductive layer covers the flexible circuit board and the bonding area.

[0030] In some embodiments, the display module further includes a cover plate located on the light-emitting side of the display panel, the display panel including a border area located around the display area; the display module further includes an edge sealing structure located in the border area;

[0031] The following steps are included before the electromagnetic shielding structure is formed:

[0032] The first retaining wall and the second retaining wall are formed in the border area;

[0033] The filling layer is filled within the space formed by the first retaining wall, the second retaining wall, the display panel, and the cover plate.

[0034] The beneficial effects of the present invention are: the display module provided by this disclosure has an electromagnetic shielding structure made of curable material, which can be precisely constructed through dispensing, spraying or coating processes. Even in the space conditions of extremely narrow bezels or even zero bezels, it can still cover flexible circuit boards, bonding areas and even bending areas, thereby improving the shielding effect. Attached Figure Description

[0035] Figure 1 A schematic diagram illustrating the display module in an embodiment of this disclosure;

[0036] Figure 2 A schematic diagram illustrating the display module in an embodiment of this disclosure;

[0037] Figure 3 This diagram illustrates the edge-sealing structure in an embodiment of the present disclosure.

[0038] Figure 4 A schematic diagram illustrating the display module in an embodiment of this disclosure;

[0039] Figure 5 A schematic diagram illustrating the display module in an embodiment of this disclosure;

[0040] Figure 6 This is a schematic diagram illustrating the manufacturing process of the display module in an embodiment of the present disclosure;

[0041] Figure 7 This is a schematic diagram illustrating the manufacturing process of the display module in an embodiment of this disclosure. Detailed Implementation

[0042] To make the objectives, technical solutions, and advantages of the embodiments of this disclosure clearer, the technical solutions of the embodiments of this disclosure will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some, not all, of the embodiments of this disclosure. All other embodiments obtained by those skilled in the art based on the described embodiments of this disclosure without creative effort are within the scope of protection of this disclosure.

[0043] Unless otherwise defined, the technical or scientific terms used in this disclosure shall have the ordinary meaning understood by one of ordinary skill in the art to which this disclosure pertains. The terms “first,” “second,” and similar terms used in this disclosure do not indicate any order, quantity, or importance, but are merely used to distinguish different components. Similarly, the terms “an,” “a,” or “the,” and similar terms do not indicate a quantity limitation, but rather indicate the presence of at least one. The terms “including,” “comprising,” or “containing,” and similar terms mean that the element or object preceding the word encompasses the elements or objects listed following the word and their equivalents, without excluding other elements or objects. The terms “connected,” “linked,” or similar terms are not limited to physical or mechanical connections, but can include electrical connections, whether direct or indirect. The terms “upper,” “lower,” “left,” and “right,” etc., are used only to indicate relative positional relationships, and these relative positional relationships may change accordingly when the absolute position of the described objects changes.

[0044] The features such as "parallel," "perpendicular," and "identical" used in the embodiments of this disclosure include features in the strict sense of "parallel," "perpendicular," and "identical," as well as cases where "approximately parallel," "approximately perpendicular," and "approximately identical" include certain tolerances. Taking into account the measurement and the tolerances associated with the measurement of a specific quantity (e.g., limitations of the measurement system), they represent the acceptable deviation range for a specific value as determined by a person skilled in the art. For example, "approximately" can mean within one or more standard deviations, or within 3% or 5% of said value.

[0045] Furthermore, throughout this document, unless otherwise defined, the terms “substantially,” “essentially,” “approximately,” and “about” are used to describe and explain small variations. When used with an event or situation, these terms can cover situations where the event or situation occurs precisely or approximately. For example, when used with a numerical value, these terms can include a range of variation of the value less than or equal to 10%, such as less than or equal to ±5%, less than or equal to ±4%, less than or equal to ±3%, less than or equal to ±2%, less than or equal to ±1%, less than or equal to ±0.5%, less than or equal to ±0.1%, or less than or equal to ±0.05%. The term “substantially coplanar” can refer to two surfaces arranged along the same plane within a micrometer range, such as within 40 μm, 30 μm, 20 μm, 10 μm, or 1 μm.

[0046] refer to Figures 1-5 As shown, this embodiment of the present disclosure provides a display module, including a display panel and a flexible circuit board 2;

[0047] The display panel includes a display area 12, a bending area 11, and a bonding area 13 connected in sequence. The bending area 11 is bent so that the bonding area 13 is bent to the backlight side of the display area 12.

[0048] The flexible circuit board 2 is bonded to the bonding area 13, and the flexible circuit board 2 is located on the backlight side of the display area 12;

[0049] The display module also includes an electromagnetic shielding structure, which covers the flexible circuit board 2 and the bonding area 13.

[0050] The electromagnetic shielding structure is made of a curable material.

[0051] Specifically, the display area 12 of the display panel is a normal light-emitting display area 12, and the bending area 11 is a transition area connecting the display area 12 and the bonding area 13. The bending area 11 is bent to fold the bonding area 13 to the backlight side of the display area 12. The flexible circuit board 2 is electrically bonded to the bonding area 13 through bonding processes such as COF (Chip On Film) or COP (Chip On Plastic) and is arranged on the backlight side of the display area 12. Figure 1 This is a schematic diagram showing the flexible circuit board 2 and the bonding area 13 after bonding. The electromagnetic shielding structure is formed by applying a curable material (such as conductive adhesive, conductive paint, or conductive silver paste) through dispensing, spraying, or coating processes, covering the surfaces of the flexible circuit board 2 and the bonding area 13. In this embodiment, the traditional copper foil / conductive cloth is replaced with an electromagnetic shielding structure made of a curable material. Curable materials have excellent rheological properties, and the coating range and thickness can be precisely controlled through high-precision dispensing or spraying equipment. Even in spaces with extremely narrow or even zero borders, it can still completely cover the flexible circuit board 2 and the bonding area 13. Compared with copper foil / conductive cloth, curable materials do not have problems such as die-cutting allowance, alignment tolerance, and bonding bubbles, resulting in higher shielding coverage integrity.

[0052] The curable material has good adhesion to the surface of the display panel and flexible circuit board 2. It can still be tightly attached after bending with the bending area 11, and it is not easy to fall off or lift up. The shielding structure has high reliability, especially in the bending state, it can still maintain the integrity of the shielding.

[0053] For example, the curing method of the curable material includes one or more combinations of UV curing, heat curing, moisture curing, or two-component reaction curing.

[0054] For example, the overall thickness of the electromagnetic shielding structure can be set according to actual needs, for example, it can be 0.1mm ± 0.01mm.

[0055] refer to Figure 4 and Figure 5 In some exemplary embodiments, the electromagnetic shielding structure includes an insulating layer 4 and a first conductive layer 5 stacked together;

[0056] A driver chip 101 is disposed on the side of the bonding area 13 away from the display area 12, and the insulating layer 4 at least covers the driver chip 101;

[0057] The first conductive layer 5 is located on the side of the insulating layer 4 away from the flexible circuit board 2, and the first conductive layer 5 is electrically connected to the exposed copper area 21 on the flexible circuit board 2.

[0058] Figure 4 This is a schematic diagram showing the insulating layer 4 formed on the side of the driver chip 101 away from the display panel. Figure 5 This is a schematic diagram illustrating the formation of the first conductive layer 5 on the side of the insulating layer 4 away from the display panel. Specifically, the insulating layer 4 is first formed on the surface of the driver chip 101 using dispensing, spraying, or coating processes, and then cured to form an insulating protective layer. The first conductive layer 5 is then formed on the side of the insulating layer 4 away from the flexible circuit board 2. The first conductive layer 5 completely covers the flexible circuit board 2 and the bonding area 13, and the first conductive layer 5 contacts the exposed copper area 21 on the flexible circuit board 2 to form an electrical connection, thus creating a grounding loop for the electromagnetic shielding structure. In this embodiment, the insulating layer 4 and the first conductive layer 5 are stacked. The insulating layer 4 covers the driver chip 101 to prevent the subsequently formed first conductive layer 5 from contacting the surface of the driver chip 101 and causing a short circuit, ensuring the normal operation of the driver chip 101. The first conductive layer 5 is electrically connected to the exposed copper area 21 on the flexible circuit board 2, enabling the electromagnetic shielding structure to form a complete Faraday cage grounding loop, effectively guiding and discharging electromagnetic noise from the back of the display panel to the ground wire.

[0059] For example, the insulating layer 4 also has thermal conductivity. When the driver chip 101 operates at high brightness, the temperature rises. The insulating layer 4 helps to transfer the heat generated by the driver chip 101 to the flexible circuit board 2 or other components, thus heat dissipating the driver chip 101 and reducing its operating temperature, thereby improving the reliability of the display module.

[0060] For example, the coverage of the insulating layer 4 is not limited to covering only the driver chip 101. For example, it can also cover other devices or areas on the bonding area 13 other than the exposed copper area 21, depending on the design requirements.

[0061] For example, the electrical connection between the first conductive layer 5 and the exposed copper area 21 is not limited to direct contact. For example, a transition layer filled with conductive particles can be provided between the exposed copper area 21 and the first conductive layer 5.

[0062] For example, the insulating layer 4 can be formed using the same molding process as the first conductive layer 5 (e.g., spraying), or it can be formed using a dispensing process to adapt to the local shape of the driver chip 101.

[0063] In some exemplary embodiments, the conductive layer is made of conductive adhesive, conductive paint, or conductive silver paste;

[0064] The insulating layer 4 is made of a curable material, such as a curable adhesive.

[0065] Conductive adhesive, conductive paint, and conductive silver paste are all curable conductive materials with good conductivity, which can ensure the shielding effectiveness of the first conductive layer 5. They also have good fluidity and adhesion, making them suitable for spraying, coating, or dispensing processes. They have a wide process window and high yield.

[0066] The insulating layer 4 is made of a curable adhesive material, which has stable mechanical strength and insulation properties after curing, and can meet the insulation protection and heat dissipation requirements of the driver chip 101.

[0067] In some exemplary embodiments, the first conductive layer 5 covers the flexible circuit board 2 and the bonding area 13, and the first conductive layer 5 extends in a first direction to at least cover a portion of the bending area 11, the first direction being parallel to the light-emitting surface of the display area 12.

[0068] Specifically, the first conductive layer 5 extends along the extension direction (first direction) of the display panel, and its extension range extends beyond the connection position between the bonding area 13 and the bending area 11, covering at least a portion of the bending area 11 near the bonding area 13. The coverage area of ​​the first conductive layer 5 is slightly larger than the outline of the flexible circuit board 2, thereby forming an edge-wrapping coverage of the flexible circuit board 2.

[0069] Since the first conductive layer 5 is a curable material that can be directly molded, it can be continuously covered even in curved transition areas such as the bending area 11. In contrast, copper foil / conductive cloth is prone to creases, warping, and gaps in the bending area 11. This solution has better adaptability in the bending area 11.

[0070] For example, the proportion of the first conductive layer 5 covering the bending area 11 can be adjusted according to the border width and shielding requirements, such as covering the portion of the bending area 11 located on the backlight side of the display panel.

[0071] In some exemplary embodiments, the flexible circuit board 2 includes a substrate layer, a second conductive layer and a first cover film are sequentially stacked on the first surface of the substrate layer, and a third conductive layer and a second cover film are sequentially stacked on the second surface of the substrate layer.

[0072] The second conductive layer is bonded to the bonding region 13, and the electromagnetic shielding structure is located on the side of the second cover film away from the base layer.

[0073] Specifically, the base layer is a flexible substrate (e.g., a polyimide PI film). The second conductive layer is a bonding pad layer (e.g., a gold pad layer) bonded to the bonding region 13. The first cover film is disposed on the side of the second conductive layer away from the base layer to protect the second conductive layer and provide insulation. The third conductive layer is a signal trace layer (e.g., a copper trace layer). The second cover film is disposed on the side of the third conductive layer away from the base layer to protect the third conductive layer and prevent short circuits.

[0074] The electromagnetic shielding structure is located on the side of the first cover film away from the substrate layer, i.e., on the outermost side of the bonding side of the flexible circuit board 2. This isolates the first conductive layer 5 from the second conductive layer through the first cover film. Even if the first conductive layer 5 covers a large area of ​​the flexible circuit board 2, it will not be connected to the bonding circuit of the bonding area 13, thus preventing a short circuit in the bonding signal. The exposed copper area 21 is the grounded exposed copper area 21 on the flexible circuit board 2, and the first conductive layer 5 is electrically connected to the exposed copper area 21.

[0075] For example, the specific location of the exposed copper area 21 can be determined according to the overall grounding design. For example, it can be set at one end or edge of the flexible circuit board 2 near the bonding area 13 to facilitate a large-area reliable contact with the first conductive layer 5.

[0076] refer to Figures 2-5 In some exemplary embodiments, a cover plate 6 located on the light-emitting side of the display panel is also included. The display panel includes a bezel area located around the display area 12. The display module also includes an edge sealing structure 3 located in the bezel area. (Refer to...) Figure 2 The area marked within the dashed box;

[0077] The edge sealing structure 3 includes a first retaining wall 31, a second retaining wall 32, and a filling layer 33. The first retaining wall 31 is located on the side of the cover plate 6 close to the display panel, the second retaining wall 32 is located on the side of the display panel away from the cover plate 6, and the filling layer 33 fills the space formed by the first retaining wall 31, the second retaining wall 32, the display panel, and the cover plate 6.

[0078] The orthographic projection of the edge sealing structure 3 on the cover plate 6 completely covers the orthographic projection of the bending area 11 on the cover plate 6.

[0079] The edge sealing structure 3 seals the gap between the cover plate 6 and the display panel in the bezel area, providing dustproof, waterproof, and moisture-proof protection, thus improving the environmental reliability of the display module. The orthogonal projection of the edge sealing structure 3 onto the cover plate 6 completely covers the orthogonal projection of the bending area 11 onto the cover plate 6, ensuring that the internal stress borne by the bending area 11 is evenly distributed by the retaining wall and the filling layer 33, guaranteeing the strength of the panel edge, preventing warping and cracking at the bending area 11, and further supporting narrow bezel design.

[0080] For example, the first barrier 31, the second barrier 32, and the filler layer 33 can be formed by dispensing. The first barrier 31 can be dispensed onto the inner edge of the cover plate 6, and the second barrier 32 can be dispensed onto the back edge of the display panel. The cross-sectional shape of the first barrier 31 and / or the second barrier 32 can be rectangular, trapezoidal, or U-shaped, etc., designed according to the flowability and curing shrinkage rate of the adhesive. The material of the cover plate 6 can be, for example, a glass cover plate 6 or a flexible cover plate 6, and is not limited thereto.

[0081] For example, the specific structural form of the edge sealing structure 3 is not limited to the combination of the first barrier wall 31, the second barrier wall 32, and the filling layer 33 described above. The edge sealing structure 3 may also consist only of an annular support pad, that is, the annular support pad completely replaces the first barrier wall 31, the second barrier wall 32, and the filling layer 33, and independently constitutes the edge sealing structure 3. Specifically, the annular support pad is arranged around the outer periphery of the frame area. When cut along the thickness direction of the display panel, the cross-sectional shape of the annular support pad is L-shaped. The annular support pad includes a first support wall and a second support wall that are connected to each other. The first support wall is connected to the side of the cover plate 6 facing the display panel and extends circumferentially along the inner edge of the cover plate 6. The second support wall is connected to the first support wall and covers the frame area of ​​the display panel, extending circumferentially along the backlight side edge of the display panel. In this way, the annular support pad is attached to the inner side of the cover plate 6 through the first support wall and to the frame area of ​​the display panel through the second support wall, directly sealing the gap between the cover plate 6 and the display panel in the frame area, without the need to separately set up a barrier wall and a filling layer 33.

[0082] The annular support pad can be integrally molded using a curable adhesive material or formed using die-cut patches (such as rubber patches, polyurethane patches, or metal patches), and this application does not limit this. If the annular support pad is integrally molded using a curable adhesive material, its molding process can be compatible with the dispensing and coating processes of the electromagnetic shielding structure, sharing existing dispensing and curing equipment, thus reducing equipment investment.

[0083] In some exemplary embodiments, the electromagnetic shielding structure extends in a first direction to cover a portion of the sealing structure 3.

[0084] Specifically, the first conductive layer 5 extends along the first direction to the area where the edge sealing structure 3 is located on the frame area, so that the shielding cage extends from the binding area 13 and the bending area 11 all the way to the edge sealing structure 3 of the frame area, forming a shielding body that is continuously closed on the back and edge of the module. The electromagnetic shielding structure extends to cover part of the edge sealing structure 3, so that the boundary of the Faraday cage extends to the outermost edge of the module, and the shielding cage remains continuously closed at the edge of the module, avoiding the shielding structure from ending at the bending area 11 and leaving a shielding gap in the frame area, thus achieving higher shielding integrity.

[0085] In some exemplary embodiments, the first retaining wall 31, the second retaining wall 32, and the filling layer 33 are all made of a curable adhesive, and the adhesive used in the first retaining wall 31 and the second retaining wall 32 has a higher viscosity than the adhesive used in the filling layer 33.

[0086] Specifically, the dispensing precision is high, allowing dispensing to be applied to the outermost cover plate 6 of the module and bending area 11. The first retaining wall 31 and the second retaining wall 32 are formed by dispensing high-viscosity adhesive. The high-viscosity adhesive can be layered to the required retaining wall thickness without easily collapsing, ensuring the strength of the panel edges and achieving a narrow frame. The filler layer 33 uses a very low-viscosity adhesive, filling the space between the walls formed by the high-viscosity adhesive (i.e., the first retaining wall 31 and the second retaining wall 32). The low-viscosity adhesive remains stable under the constraint of the retaining walls and does not overflow.

[0087] It should be noted that, Figures 2-5 The edge sealing structure 3 is provided in all display modules, but it is not an essential component of the display module. In embodiments where the display module does not have a narrow bezel design requirement, the edge sealing structure 3 can be omitted. That is, no edge sealing structure is provided between the cover plate 6 and the display panel in the bezel area. In this case, the display module relies solely on the bending structure of the bending area 11 to achieve the bonding connection between the bonding area 13 and the flexible circuit board 2. Correspondingly, if the edge sealing structure 3 is omitted, the electromagnetic shielding structure does not need to extend to cover the edge sealing structure; its coverage area is limited to the flexible circuit board 2 and the bonding area 13.

[0088] refer to Figure 3 For example, an ink layer 7 is provided on the side of the cover plate 6 near the display panel, and the first barrier 31 is provided on the side of the ink layer 7 away from the cover plate 6. That is, the first barrier 31 is dotted onto the surface of the ink layer 7. The ink layer 7 is arranged circumferentially along the border area to cover the non-display area of ​​the border area, thereby improving the appearance of the border of the display module.

[0089] This disclosure also provides a method for manufacturing a display module, used to manufacture the above-mentioned display module, the method comprising the following steps:

[0090] Step S1: Provide the display panel and flexible circuit board 2 for bonding connection;

[0091] The display panel includes a display area 12, a bending area 11, and a bonding area 13 connected in sequence. The bending area 11 is bent so that the bonding area 13 is bent to the backlight side of the display area 12. The flexible circuit board 2 is bonded to the bonding area 13 and is located on the backlight side of the display area 12.

[0092] Step S2: An electromagnetic shielding structure is formed on the flexible circuit board 2 and the bonding area 13 by spraying or coating processes.

[0093] The formed area of ​​the electromagnetic shielding structure covers the surfaces of the flexible circuit board 2 and the bonding area 13, and extends along the first direction to cover part of the bending area 11. Its coverage area is larger than the outer contour of the flexible circuit board 2. The cured electromagnetic shielding structure is electrically connected to the exposed copper area 21 on the flexible circuit board 2, thereby reliably grounding the shielding structure.

[0094] refer to Figure 6 In some exemplary embodiments, the electromagnetic shielding structure includes an insulating layer 4 and a first conductive layer 5 stacked together; a driver chip 101 is disposed on the side of the bonding area 13 away from the display area 12;

[0095] The process of forming an electromagnetic shielding structure on the flexible circuit board 2 and the bonding area 13 using a spraying or coating process specifically includes:

[0096] Step S21: The insulating layer 4 is formed by dispensing, spraying or coating processes and then cured. The insulating layer 4 covers the driver chip 101.

[0097] Specifically, the curable adhesive is applied to the bonding area 13 through dispensing, spraying, or coating processes, so that the insulating layer 4 covers the driver chip 101, that is, the driver chip 101 is completely covered by the insulating layer 4. After the insulating layer 4 is formed, it is cured by ultraviolet light irradiation, heating, or placing it in a curing oven, so that the insulating layer 4 changes from a liquid or semi-solid state to a solid state.

[0098] It should be noted that the coverage of the insulating layer 4 is not limited to covering only the driver chip 101. For example, it can also cover other chips (such as touch ICs) or areas on the bonding area 13 other than the exposed copper area 21 to expand the insulation protection range.

[0099] Step S22: The first conductive layer 5 is formed by dispensing, spraying or coating processes and then cured. The first conductive layer 5 covers the flexible circuit board 2 and the bonding area 13.

[0100] Specifically, a curable conductive material (such as conductive adhesive, conductive paint, or conductive silver paste) is formed on the surface of the flexible circuit board 2 and the bonding area 13 through dispensing, spraying, or coating processes, so that the first conductive layer 5 covers the flexible circuit board 2 and the bonding area 13, and extends to cover the insulating layer 4. After the first conductive layer 5 is formed, it is cured by ultraviolet light irradiation, heating, or placing it in a curing oven, so that the first conductive layer 5 changes from a liquid or semi-solid state to a solid state.

[0101] The cured first conductive layer 5 is electrically connected to the exposed copper area 21 on the flexible circuit board 2, so that the electromagnetic shielding structure is reliably grounded.

[0102] The layering process, which first forms the insulating layer 4 and then the first conductive layer 5, ensures that the insulating layer 4 is located between the driver chip 101 and the first conductive layer 5, thus providing insulation isolation for the driver chip 101. When the first conductive layer 5 covers a large area of ​​the flexible circuit board 2 and the bonding area 13, it will not short-circuit with the pads or metal traces on the surface of the driver chip 101. This avoids the process limitations of traditional copper foil / conductive cloth solutions that require precise avoidance of IC areas, resulting in a large process tolerance and high yield.

[0103] The insulating layer 4 serves a dual purpose of protecting and dissipating heat for the driver chip 101: on the one hand, it prevents the driver chip 101 from being scratched, and on the other hand, it conducts the heat generated by the driver chip 101 to the flexible circuit board 2 or other components when working at high brightness, thereby reducing the operating temperature of the driver chip 101 and improving the reliability of the module.

[0104] The spraying or coating process can continuously cover curved transition areas such as the bending area 11. The shielding structure is less prone to creases, warping, and gaps when bent, and is superior to copper foil / conductive cloth bonding methods in terms of bending adaptability.

[0105] refer to Figure 7 In some exemplary embodiments, the display module further includes a cover plate 6 located on the light-emitting side of the display panel, and the display panel includes a frame area located around the display area 12; the display module further includes an edge sealing structure 3 located in the frame area;

[0106] The following steps are included before the electromagnetic shielding structure is formed:

[0107] S101: The first retaining wall 31 and the second retaining wall 32 are formed in the border area;

[0108] Specifically, a highly viscous, curable adhesive is applied via a dispensing process to the side of the cover plate 6 closest to the display panel (forming a first barrier 31) and the side of the display panel furthest from the cover plate 6 (forming a second barrier 32). The first barrier 31 extends circumferentially along the inner edge of the cover plate 6, and the second barrier 32 extends circumferentially along the outer edge of the frame area of ​​the display panel. After dispensing, the first barrier 31 and the second barrier 32 are cured to set their shape and maintain circumferential continuity.

[0109] S102: The filling layer 33 is filled into the space formed by the first retaining wall 31, the second retaining wall 32, the display panel and the cover plate 6.

[0110] Specifically, a low-viscosity filler material is injected or dotted into the space formed by the first retaining wall 31, the second retaining wall 32, the display panel, and the cover plate 6, and the filler layer 33 fills the space. The filler layer 33 is then cured to seal and fix the cover plate 6 and the display panel at the edge area. The orthographic projection of the edge sealing structure 3 on the cover plate 6 completely covers the orthographic projection of the bending area 11 on the cover plate 6.

[0111] Before forming the electromagnetic shielding structure, the edge sealing structure 3 is formed first, so that the edge sealing structure 3 seals and fixes the gap between the cover plate 6 and the display panel in the frame area. When the electromagnetic shielding structure is sprayed / coated subsequently, the overall structure of the module is already stable, and the forming of the shielding structure will not be affected by the displacement of the cover plate 6 or the change of the gap in the frame area, resulting in high forming accuracy and yield.

[0112] The process sequence of sealing the edges first and then shielding allows the electromagnetic shielding structure to extend and cover part of the sealing structure 3 (e.g., the surface of the filling layer 33). The shielding cage extends from the binding area 13 and the bending area 11 all the way to the edge sealing structure 3 of the frame area, forming a continuous and closed Faraday cage on the back and edge of the module, resulting in high shielding integrity.

[0113] The retaining wall uses a combination of high-viscosity adhesive and low-viscosity adhesive for the filling layer 33, which balances the shape retention of the retaining wall with the filling density of the filling layer 33 (the high-viscosity adhesive is layered without collapsing, while the low-viscosity adhesive has good fluidity and fills the wall fully with few air bubbles), resulting in high-quality edge sealing.

[0114] For example, this disclosure also provides a display device including the display module described above.

[0115] The display device includes, but is not limited to, components such as: a radio frequency unit, a network module, an audio output unit, an input unit, a sensor, a display unit, a user input unit, an interface unit, a memory, a processor, and a power supply. Those skilled in the art will understand that the above-described structure of the display device does not constitute a limitation on the display device; the display device may include more or fewer of the aforementioned components, or combine certain components, or arrange different components. In embodiments of the present invention, the display device includes, but is not limited to, a monitor, a mobile phone, a tablet computer, a television set, a wearable electronic device, a navigation display device, etc.

[0116] The display device can be any product or component with display function, such as a television, monitor, digital photo frame, mobile phone, or tablet computer. The display device also includes a flexible circuit board, a printed circuit board, and a backplate.

[0117] Furthermore, embodiments of this disclosure provide an electronic device including a memory, a processor, and one or more programs stored in the memory and executable on the processor, wherein when the one or more programs are executed by the processor, the electronic device performs the method described above.

[0118] In one embodiment, this disclosure also provides a computer-readable storage medium having a computer program stored thereon, which, when executed by a processor, implements the steps in the above method embodiments.

[0119] The aforementioned computer-readable storage medium, since the computer program stored in its memory is executed by the processor to implement the steps in the above-described method embodiments, can similarly bring about the beneficial effects of the above-described silicon wafer placement and removal method, which will not be elaborated here.

[0120] Those skilled in the art will understand that all or part of the processes in the methods of the above embodiments can be implemented by a computer program instructing related hardware. The computer program can be stored in a non-volatile computer-readable storage medium, and when executed, it can include the processes of the embodiments of the methods described above. Any references to memory, storage, databases, or other media used in the embodiments provided in this application can include at least one of non-volatile and volatile memory. Non-volatile memory can include read-only memory (ROM), magnetic tape, floppy disk, flash memory, or optical storage, etc. Volatile memory can include random access memory (RAM) or external cache memory. By way of illustration and not limitation, RAM can be in various forms, such as static random access memory (SRAM) or dynamic random access memory (DRAM), etc.

[0121] The following points need to be explained:

[0122] (1) The accompanying drawings of the embodiments of this disclosure only involve the structures involved in the embodiments of this disclosure. Other structures can be referred to the general design.

[0123] (2) For clarity, the thickness of layers or regions is enlarged or reduced in the drawings used to describe embodiments of the present disclosure, i.e., these drawings are not drawn to scale. It will be understood that when an element such as a layer, film, region or substrate is referred to as being “above” or “below” another element, the element may be “directly” located “above” or “below” the other element or there may be intermediate elements.

[0124] (3) Where there is no conflict, the embodiments of this disclosure and the features in the embodiments can be combined with each other to obtain new embodiments.

[0125] It is understood that the above embodiments are merely exemplary implementations used to illustrate the principles of the present invention, and the present invention is not limited thereto. For those skilled in the art, various modifications and improvements can be made without departing from the spirit and essence of the present invention, and these modifications and improvements are also considered to be within the scope of protection of the present invention.

Claims

1. A display module, characterized in that, Including display panels and flexible circuit boards; The display panel includes a display area, a bending area, and a bonding area connected in sequence, wherein the bending area bends so that the bonding area bends to the backlight side of the display area; The flexible circuit board is bonded to the bonding area, and the flexible circuit board is located on the backlight side of the display area; The display module also includes an electromagnetic shielding structure, which covers the flexible circuit board and the bonding area. The electromagnetic shielding structure is made of a curable material.

2. The display module according to claim 1, characterized in that, The electromagnetic shielding structure includes a stacked insulating layer and a first conductive layer; A driver chip is disposed on the side of the bonding area away from the display area, and the insulating layer at least covers the driver chip; The first conductive layer is located on the side of the insulating layer away from the flexible circuit board, and the first conductive layer is electrically connected to the exposed copper area on the flexible circuit board.

3. The display module according to claim 2, characterized in that, The conductive layer is made of conductive adhesive, conductive paint, or conductive silver paste. The insulating layer is made of a curable material.

4. The display module according to claim 2, characterized in that, The first conductive layer covers the flexible circuit board and the bonding area, and extends in a first direction to at least cover a portion of the bending area, the first direction being parallel to the light-emitting surface of the display area.

5. The display module according to claim 2, characterized in that, The flexible circuit board includes a substrate layer, a second conductive layer and a first cover film are sequentially stacked on the first surface of the substrate layer, and a third conductive layer and a second cover film are sequentially stacked on the second surface of the substrate layer. The second conductive layer is bonded to the bonding area, and the electromagnetic shielding structure is located on the side of the second cover film away from the base layer.

6. The display module according to claim 1, characterized in that, It also includes a cover plate located on the light-emitting side of the display panel, the display panel including a border area located around the display area, and the display module including an edge sealing structure located in the border area; The edge sealing structure includes a first retaining wall, a second retaining wall, and a filling layer. The first retaining wall is located on the side of the cover plate closer to the display panel, the second retaining wall is located on the side of the display panel away from the cover plate, and the filling layer fills the space formed by the first retaining wall, the second retaining wall, the display panel, and the cover plate. The orthographic projection of the edge sealing structure onto the cover plate completely covers the orthographic projection of the bending area onto the cover plate.

7. The display module according to claim 6, characterized in that, The electromagnetic shielding structure extends in the first direction to cover the edge sealing structure.

8. The display module according to claim 6, characterized in that, The first retaining wall, the second retaining wall, and the filling layer are all made of curable adhesive material, and the adhesive material used in the first retaining wall and the second retaining wall has a higher viscosity than the adhesive material used in the filling layer.

9. A display device, characterized in that, Includes the display module as described in any one of claims 1-8.

10. A method for manufacturing a display module, characterized in that, The manufacturing method for producing the display module according to any one of claims 1-8 includes the following steps: A display panel and a flexible circuit board are provided for bonding connection. The display panel includes a display area, a bending area, and a bonding area connected in sequence. The bending area is bent such that the bonding area bends to the backlight side of the display area. The flexible circuit board is bonded to the bonding area and is located on the backlight side of the display area. An electromagnetic shielding structure is formed on the flexible circuit board and the bonding area using a spraying or coating process.