Production of a medium-energy proton cyclotron accelerator 68 Ge capsule target and its preparation method

By employing a stepped structure design with a niobium-clad thick shell and a copper heat dissipation target support, along with low-temperature solid-state packaging technology, the sealing reliability and cooling issues of capsule targets in medium-energy proton cyclotron accelerators have been resolved, enabling the efficient generation and safe production of 68Ge.

CN123072802APending Publication Date: 2026-11-10STATE POWER INVESTMENT NUCLIDES TONGCHUANG (CHONGQING) TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611275519.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-21
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

Existing capsule targets in medium-energy proton cyclotron accelerators suffer from insufficient sealing reliability, significant thermal resistance due to large differences in thermal expansion coefficients, and loosening problems caused by cooling water backflow pressure, which limit the production efficiency and safety of 68Ge.

Method used

The target employs a stepped structure design with a niobium-clad thick shell and a copper heat dissipation target support. Combined with low-temperature solid-state packaging and low-heat-input pulsed laser welding technology, it achieves high-strength sealing and effective cooling of the target. It integrates vacuum sealing, cooling water connection and anti-loosening functions, and achieves metallurgical bonding of dissimilar metals through diffusion welding and vacuum brazing.

Benefits of technology

It improves the production efficiency of 68Ge, ensures rapid recovery of the high vacuum environment and the sealing of the cooling system, reduces proton energy loss, enhances the safety redundancy of automated target changing and production line uptime, and avoids metal melting and spatter in the welding heat-affected zone.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123072802A_ABST
    Figure CN123072802A_ABST
Patent Text Reader

Abstract

This invention discloses a method for producing a medium-energy proton cyclotron accelerator. 68 This invention relates to a capsule target and its preparation method for Ge, which pertains to nuclear technology applications and medical isotope production. The capsule target includes a capsule body and a copper heat-dissipating target holder. The capsule body comprises a niobium cladding film, a niobium cladding shell, and a metallic gallium target encapsulated within both. The niobium cladding film is located on the proton incident side, and the niobium cladding shell surrounds the sides and back of the metallic gallium target. The copper heat-dissipating target holder is stepped, divided into an upper and lower section. The upper section has a groove facing the capsule target body for placing the capsule target, and a cooling channel on the side away from the groove. The lower section has a step on its outer periphery, with a vacuum sealing ring at the step. The step protrusion is used for guide insertion and compression sealing with the flange of the target station vacuum chamber. A spring plunger is located on the lower outer periphery, with a spring top ball at the top for engaging with the target gripper groove. This invention solves the technical problems of insufficient sealing reliability and limited heat dissipation capacity of existing liquid gallium targets.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the fields of nuclear technology applications and medical isotope production technology, specifically to a medium-energy proton cyclotron accelerator production... 68 Ge capsule targets and their preparation methods. Background Technology

[0002] Positron emission tomography (PET) is currently the core imaging technology for clinical tumor diagnosis, staging, and efficacy evaluation, and it also plays an irreplaceable role in the diagnosis of cardiovascular and neurological diseases. 68 Ge is one of the most widely used radionuclides in PET imaging. It can label a variety of targeted drugs to achieve precise molecular imaging diagnosis, and the global annual demand is growing rapidly at a rate of more than 20%. 68 Ga mainly comes from 68 Ge / 68 Ga generator, in which 68 Ge serves as the parent nucleus, continuously generating new nuclei through electron capture decay. 68 Ga. Prepared in one step 68 Ge / 68 The Ga generator can meet approximately one year of clinical needs, eliminating the need for on-site accelerator production and offering significant clinical convenience and economic value. Currently, medium-energy proton cyclotron accelerators irradiate natural gallium targets ( 69 Ga(p,2n) 68 Ge nuclear reactors are a global production 68 The mainstream technology route for Ge.

[0003] Capsule-type targets, due to their excellent sealing performance and high safety, have become the mainstream technology in the production of liquid target materials for irradiation and are widely used in the production processes of various medical isotopes. 68 The following key technical problems need to be overcome in the large-scale, industrialized production of Ge: Firstly, gallium is liquid at room temperature and is highly volatile and prone to leakage under irradiation thermal cycling. It also readily forms brittle intermetallic compounds with niobium cladding. Current capsule targets mostly employ vacuum electron beam welding for sealing, which involves high heat input. During welding, gallium is prone to localized melting and spattering, resulting in high weld porosity and insufficient sealing reliability. Other solutions utilize solid precursors such as gallium phosphate to avoid liquid encapsulation, but these have long fabrication cycles, limiting their effectiveness. 68 Ge's productivity efficiency.

[0004] Secondly, in order to improve 68For Ge-based targets to withstand higher proton beams per unit time, the heat dissipation requirements are extremely high. Niobium cladding is often used as a target cladding layer due to its resistance to proton irradiation, while copper is used as the target substrate due to its exceptional thermal conductivity. The large difference in their coefficients of thermal expansion results in significant thermal resistance at the interface of conventional mechanical clamping or brazing connections, which becomes a bottleneck restricting the upper limit of the beam current withstand capability of the target.

[0005] Third, industrial-grade production lines require frequent target replacements to achieve continuous power supply. The target is connected to the target holder inside the vacuum chamber of the target station via a gripper in the target replacement mechanism. The bottom of the target holder usually needs to be connected to a cooling water inlet. When the cooling water enters the target, it generates upward back pressure. In a high-activity environment, the target may become loose, which will directly cause a shutdown accident. Summary of the Invention

[0006] To address the problems existing in the prior art, this invention provides a method for producing a medium-energy proton cyclotron accelerator. 68 The capsule target and its preparation method for Ge can minimize the energy loss of protons in the shell while ensuring the structural strength and sealing reliability of the target, thereby improving... 68 Ge generation efficiency.

[0007] The technical solution of the present invention is as follows: In a first aspect of the invention, a method for producing a medium-energy proton cyclotron accelerator is provided. 68 Ge's capsule target includes a capsule target body and a copper heat dissipation target holder; The capsule target includes a niobium cladding film, a niobium cladding shell, and a gallium metal target encapsulated inside both. The niobium cladding film is located on the proton incident side, and the niobium cladding shell surrounds the side and back sides of the gallium metal target. The edge of the niobium cladding shell is provided with a stepped structure for limiting the niobium cladding film. The copper heat dissipation target support has a stepped structure, including an upper target support and a lower target support. The upper target support has a groove on the side facing the capsule target body, which is used to place the capsule target body. A cooling channel is provided on the other side of the upper target support opposite to the groove. The lower target support has a step on its outer periphery, and a vacuum sealing ring is provided at the step. The raised part of the step is used to guide and insert into the flange of the target station vacuum chamber and press and seal it. A spring plunger is provided on the outer periphery of the lower target support, and a spring top ball is provided at the top of the spring plunger for engaging with the target gripper groove.

[0008] In some embodiments of the present invention, the thickness of the niobium cladding film is less than the thickness of the niobium cladding shell.

[0009] In some embodiments of the present invention, the cooling channel is in the shape of a longitudinal cuboid.

[0010] In some embodiments of the present invention, the lower target support is provided with a female cooling water pipe inlet. The inlet side of the female cooling water pipe inlet is chamfered and widened to facilitate guiding and fitting with the male inlet on the target gripper. The inner wall of the female cooling water pipe inlet is machined with a cooling water sealing ring groove, and a cooling water sealing ring is built in to prevent cooling water leakage.

[0011] In some embodiments of the present invention, two spring plungers are symmetrically arranged in the width direction of the copper heat dissipation target support.

[0012] In some embodiments of the present invention, the metal gallium target is naturally abundant gallium, which is encapsulated in a solid state within a niobium cladding cavity.

[0013] In a second aspect of the invention, a method for producing a medium-energy proton cyclotron accelerator is provided. 68 The method for preparing a capsule target for Ge includes the following steps: S1. Take an oxygen-free copper block as the upper half blank of the copper heat dissipation target support, and mill a groove on the side of the capsule target body to match the shape of the niobium cladding thick shell. S2. Embed the niobium plate into the groove, and use diffusion welding process to weld the niobium plate to the upper half of the copper heat dissipation target support as a whole. Then, mill a longitudinal rectangular cooling channel on the cooling channel side of the upper half, and mill the niobium plate on the capsule target side to form a niobium-clad thick shell. S3. Complete capsule target encapsulation in a low-temperature environment: Liquid gallium metal is frozen into solid by liquid nitrogen, pressed and cut into gallium sheets that match the inner cavity of the niobium shell, and then placed into the inner cavity of the thick niobium shell. The niobium shell film is covered and the step structure is used for positioning. Pulsed laser welding is used to seal the joint between the film and the thick shell. S4. Mill the lower half of the copper heat dissipation target support to form the cooling water channel, spring plunger mounting hole and target station docking step; S5. After pre-placing the brazing filler metal on the mating surfaces of the upper and lower parts of the copper heat dissipation target holder, vacuum brazing is used to weld the upper and lower parts into an integral target holder. S6. Install the vacuum sealing O-ring, cooling water sealing O-ring, and spring plunger respectively to complete the target preparation.

[0014] In some embodiments of the present invention, the process conditions for diffusion welding in step S2 are: a vacuum degree of not less than 5 × 10⁻⁶. -3 The welding temperature is 800℃~900℃, the applied pressure is 10~20 MPa, and the holding time is 30~60 min.

[0015] In some embodiments of the present invention, the pulsed laser welding in step S3 adopts a low heat input mode, the width of the welding heat-affected zone is no more than 0.5 mm, and the solid metal gallium in the inner cavity of the niobium cladding does not melt during the welding process.

[0016] In some embodiments of the present invention, the vacuum brazing in step S5 is performed at 10... -2 The process is carried out under a Pa-level vacuum environment, and the airtightness leakage rate of the mating surface between the upper and lower parts of the copper heat sink support after brazing is no greater than 1×10⁻⁶. -9 Pa·m 3 / s.

[0017] One or more technical solutions of the present invention have the following beneficial effects: (1) The capsule target of the present invention utilizes the stepped structure of the edge of the niobium-clad thick shell to precisely position the niobium-clad thin film. The niobium-clad thin film minimizes proton energy loss while ensuring structural strength. The sides and back use niobium-clad thick shells with sufficient structural thickness to completely encapsulate the irradiated liquid gallium, effectively preventing gallium leakage and avoiding its corrosion of downstream structural components. At the same time, the niobium-clad thick shell can completely deposit the remaining proton beam after penetrating the target material, maximizing 68Ge yield while preventing deformation of the underlying structural components due to excessive irradiation. This structure minimizes proton energy loss in the shell while ensuring the structural strength and sealing reliability of the target, thereby improving… 68 Ge generation efficiency.

[0018] (2) This invention integrates four functions—vacuum sealing, target cooling, cooling water connection, and anti-loosening—into a single stepped target holder structure: the stepped protrusion and vacuum flange guide insertion ensure rapid recovery of the high vacuum environment in front of the target; the longitudinal rectangular cooling channel fits snugly against the capsule target side, minimizing the heat conduction path; the bottom cooling water inlet is chamfered and flared to smoothly connect with the male part of the gripper; the elastic engagement of the spring plunger ball and the gripper groove specifically counteracts the upward backflow pressure generated when the cooling water is introduced. The entire interface design allows for blind insertion, locking, and unlocking of the target without manual intervention, significantly improving the safety redundancy and production line uptime of automated target changing.

[0019] (3) The preparation method of the capsule target of the present invention achieves metallurgical bonding of two dissimilar metals by diffusion welding of the niobium-clad thick shell and the upper part of the oxygen-free copper target holder, fundamentally eliminating the contact thermal resistance of conventional mechanical pressing or brazing interface; the capsule target uses the stepped structure of the edge of the niobium-clad thick shell to accurately position the niobium-clad thin film, and completes the sealing by combining low temperature solid pressing and low heat input pulse laser welding process, effectively avoiding local melting and splashing of metal gallium in the welding heat-affected zone.

[0020] (4) This invention addresses the engineering challenge of not being able to perform subsequent operations on the internal flow channels of oxygen-free copper using conventional tools. It adopts a reverse process path of "milling the upper half of the flow channel first, then diffusion welding the niobium plate, and finally vacuum brazing the upper and lower target supports." This not only avoids the problem of the cooling flow channel being inaccessible after overall welding, but also ensures the airtightness of the target support mating surface through vacuum brazing. In addition, the low-temperature packaging process (liquid nitrogen freezing of solid gallium, pressing, cutting, and packaging) effectively solves the technical problem of the difficulty in precisely manipulating liquid gallium. Attached Figure Description

[0021] Figure 1 A front view of the capsule target for producing 68Ge using the medium-energy proton cyclotron accelerator of this invention; Figure 2 for Figure 1 A magnified view of a section at point A in the middle; Figure 3 This is a schematic diagram of the capsule target body side of the upper target holder of the present invention; Figure 4 This is a schematic diagram of the cooling channel side of the upper target holder of the present invention.

[0022] In the figure: 1. Capsule target; 101. Metallic gallium; 102. Niobium cladding film; 103. Niobium cladding thick shell; 104. Stepped structure; 2. Copper heat dissipation target support; 201. Upper target support; 202. Lower target support; 203. Vacuum sealing ring groove; 204. Stepped surface; 205. Vacuum sealing ring; 206. Cooling water sealing ring; 207. Chamfered flare; 208. Spring plunger; 209. Cooling channel; 210. Brazing filler groove; 211. Groove. Detailed Implementation

[0023] It should be noted that the following detailed descriptions are exemplary and intended to provide further illustration of the invention. Unless otherwise specified, all technical and scientific terms used in this invention have the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains.

[0024] It should be noted that the terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit the scope of exemplary embodiments according to the invention. As used herein, unless otherwise expressly indicated by the invention, the singular form is intended to include the plural form as well. Furthermore, it should be understood that when the terms "comprising" and / or "including" are used in this specification, they indicate the presence of features, steps, operations, devices, components, and / or combinations thereof.

[0025] Example 1 In a typical embodiment of the present invention, a method for producing a medium-energy proton cyclotron accelerator is proposed. 68 Ge's capsule target, such as Figures 1 to 4 As shown, it includes a capsule target 1 and a copper heat dissipation target holder 2; The capsule target 1 includes a niobium cladding film 102, a niobium cladding shell 103, and a gallium 101 target material encapsulated inside both. The niobium cladding film 102 is located on the proton incident side and is relatively thin to facilitate efficient proton beam incidence. The niobium cladding shell 103 surrounds the side and back sides of the gallium 101 target material, forming a robust support and sealing structure. The edge of the niobium cladding shell 103 is provided with a stepped structure 104 for limiting the niobium cladding film 102, which is used to accurately position and limit the niobium cladding film 102 to ensure the stability of the film's position during encapsulation and use. The copper heat dissipation target support 2 has a stepped structure, including an upper target support 201 and a lower target support 202. The upper target support 201 has a groove 211 on the side facing the capsule target 1, which is used to place the capsule target 1. On the other side of the upper target support 201 opposite to the groove 211, a cooling channel 209 is provided for circulating cooling medium to remove the heat generated by the target during operation. The lower target support 202 has a stepped surface 204 on its outer periphery. A vacuum sealing ring groove 203 is opened at the stepped surface 204. A vacuum sealing ring 205 is installed in the vacuum sealing ring groove 203. The raised part of the step is used to guide and insert into the flange of the target station vacuum chamber and press and seal it to ensure a high vacuum environment in front of the beam line. A spring plunger 208 is provided on the outer periphery of the lower target support 202. The top of the spring plunger 208 has a spring top ball for engaging with the target gripper groove to ensure stable connection and quick assembly and disassembly of the target during operation.

[0026] In this embodiment, the thickness of the niobium cladding film 102 is less than the thickness of the niobium cladding shell 103. The niobium cladding film 102 minimizes proton energy loss while ensuring structural strength. The sides and back are covered with a niobium shell 103 of sufficient structural thickness, which can completely encapsulate the irradiated liquid gallium 101, effectively preventing gallium leakage and avoiding its corrosion of downstream structural components. Simultaneously, the niobium shell 103 can completely deposit the remaining proton beam after penetrating the target, thus achieving… 68 To maximize Ge production while preventing deformation of the underlying structural components due to excessive irradiation.

[0027] In one specific embodiment of this example, the thickness of the niobium cladding film 102 is 0.1mm to 0.5mm, and the thickness of the niobium cladding shell 103 is greater than 0.5mm. The thickness of the niobium cladding shell can be selected according to actual needs.

[0028] like Figure 2As shown, the cooling channel 209 is longitudinally rectangular. This channel design increases the heat exchange area and enhances the convective heat transfer effect, enabling it to promptly remove the large amount of heat generated by the capsule target 1 under proton irradiation, ensuring stable target operating temperature. The capsule target 1 is directly welded to the capsule target side of the upper half of the copper heat dissipation target support 2, minimizing the heat conduction path.

[0029] In this embodiment, the lower part of the copper heat dissipation target support 2 is provided with a female cooling water pipe port, and the target gripper is correspondingly provided with a male cooling water pipe port. The inlet side of the female cooling water pipe port is chamfered and widened 207 to facilitate smooth guiding and quick docking with the male port on the target gripper. The inner wall of the female cooling water pipe port is machined with a cooling water sealing ring groove, and a cooling water sealing ring 206 is placed in the groove. The elastic deformation of the O-ring achieves a reliable static seal, effectively preventing cooling water from leaking at the pipe connection and ensuring the sealing and safety of the cooling system operation.

[0030] In this embodiment, two spring plungers 208 are evenly distributed around the circumference of the copper heat dissipation target holder 2. Since the cooling water entering the target generates upward pressure, which could potentially cause the target to detach from the gripper, spring plungers 208 are provided on the copper heat dissipation target holder 2. A spring ball is provided at the top of the spring plunger 208, which can engage with the corresponding groove on the target gripper, achieving a reliable connection between the target and the gripper and preventing loosening. The symmetrical arrangement provides balanced clamping force and positioning accuracy for the connection between the target and the gripper, preventing the target from deflecting or loosening after installation, ensuring accurate positioning and a stable connection within the vacuum chamber, and also facilitating rapid blind insertion operations.

[0031] In this embodiment, the gallium 101 target material is naturally abundant gallium, encapsulated in a solid state within a niobium cladding cavity. Using naturally abundant gallium as the target material is relatively low-cost and readily available; encapsulating it in a solid state avoids problems such as flow and leakage that may occur with liquid metal during irradiation or processing, thus improving the safety, stability, and operability of the target during preparation, transportation, and use.

[0032] In this embodiment, the copper heat dissipation target 2 is made of high thermal conductivity oxygen-free copper and has an overall stepped structure, integrating the following four core functions: (1) Vacuum sealing function: The copper heat dissipation target support 2 has a vacuum sealing ring groove 203 in the middle of the step, and a vacuum sealing ring 205 is provided on the step surface 204. When the target is connected to the vacuum chamber flange of the target station, the raised part of the step plays a guiding and positioning role, and the step plane is in close contact with the flange plane, pressing the vacuum sealing ring 205 to ensure a high vacuum environment in the beamline in front of the target.

[0033] (2) Target cooling function: The upper half of the copper heat dissipation target holder 2 has a longitudinally rectangular cooling channel 209 machined on its cooling channel side. This channel design increases the heat exchange area and enhances the convective heat transfer effect, enabling it to promptly remove the large amount of heat generated by the capsule target 1 under proton irradiation, ensuring stable target operating temperature. The capsule target 1 is directly welded to the capsule target side of the upper half of the copper heat dissipation target holder 2, minimizing the heat conduction path.

[0034] (3) Cooling water sealing function: The bottom of the copper heat dissipation target support 2 is provided with a female cooling water pipe inlet. The inlet side of the female inlet is chamfered and widened by 207 to facilitate guiding and fitting with the male inlet on the target gripper. The inner wall of the female inlet is machined with a cooling water sealing ring groove, and a cooling water sealing ring 206 is built in to prevent cooling water leakage.

[0035] (4) Anti-loosening function: Since the cooling water entering the target generates upward pressure, which could cause the target to detach from the gripper, a spring plunger 208 is designed on the copper heat dissipation target support 2. The top of the spring plunger 208 is provided with a spring ball, which can engage with the corresponding groove on the target gripper to achieve a reliable connection between the target and the gripper and prevent loosening.

[0036] Example 2 In a typical embodiment of the present invention, a method for producing a medium-energy proton cyclotron accelerator is provided. 68 The method for preparing a capsule target for Ge includes the following steps: S1. Take an oxygen-free copper block as the blank for the upper half of the copper heat dissipation target support, and mill a groove on the side of the capsule target body to match the shape of the niobium cladding thick shell; the oxygen-free copper block needs to have sufficient thickness to provide the structural strength required for subsequent diffusion welding and avoid deformation during the welding process.

[0037] S2. Embed the niobium plate into the groove and weld the niobium plate to the upper part of the copper heat dissipation target support using diffusion welding. Diffusion welding can achieve metallurgical bonding between niobium and copper, ensuring minimal interfacial thermal resistance and significantly improving heat exchange efficiency. Subsequently, a longitudinal rectangular cooling channel is milled on the upper half of the cooling channel side, and the niobium plate is milled and shaped into a niobium-clad thick shell on the capsule target side. Since the cooling channel is located inside the target support, conventional machining cannot be completed on the entire target support. Therefore, the channel needs to be machined first and then welded to the lower half.

[0038] Among them, niobium plates need to be nickel-plated on the bonding surface before diffusion welding to improve welding performance. The process conditions for diffusion welding are: the vacuum degree of the welding environment is not less than 5×10 -3Pa is applied to effectively prevent metal oxidation at high temperatures; the welding temperature is controlled within the range of 800~900℃ to ensure sufficient atomic diffusion at the copper-niobium interface; at the same time, a pressure of 10Mpa~20Mpa is applied to promote close contact and atomic migration at the interface; the holding time is maintained at 30 min~60 min to ensure that a uniform and firm metallurgical bonding layer is formed at the welding interface.

[0039] S3. Capsule target encapsulation is completed in a low-temperature environment: liquid gallium metal is frozen into a solid state by liquid nitrogen, pressed and cut into gallium sheets that match the inner cavity of the niobium cladding, and then placed into the inner cavity of the thick niobium cladding. The niobium cladding film is covered and the step structure is used for positioning. Pulsed laser welding is used to seal the joint between the film and the thick shell.

[0040] The pulsed laser welding process employs a low-heat-input mode. This mode precisely controls the energy, frequency, and duration of the laser pulse, strictly limiting the width of the heat-affected zone to no more than 0.5 mm. This minimizes the thermal impact on surrounding materials, especially the internal gallium target, ensuring that the solid gallium within the niobium cladding cavity remains solid and does not melt during welding, thus maintaining the initial shape of the target and the integrity of the package. Pulsed laser welding features low heat input and a narrow heat-affected zone, effectively preventing the melting of solid gallium during welding and ensuring package quality. Preferably, the laser pulse energy is 3 J.

[0041] S4. Mill the lower half of the copper heat dissipation target support to form the cooling water channel, spring plunger mounting hole and target station docking step.

[0042] S5. After pre-applying brazing filler metal to the mating surfaces of the upper and lower parts of the copper heat dissipation target holder, vacuum brazing is used to weld the upper and lower parts into an integral target holder.

[0043] Among them, the vacuum brazing process is in 10 -2 The process is performed under a high vacuum environment at the Pa level to completely eliminate the adverse effects of oxidation on the brazing quality. After brazing, the airtightness of the mating surfaces of the upper and lower parts of the copper heat sink holder must be rigorously tested, requiring a leakage rate of no more than 1×10⁻⁶. -9 Pa·m 3 / s, ensuring that the overall structure of the target holder has excellent sealing performance under subsequent high vacuum or cooling water pressure environments, preventing any leakage.

[0044] S6. Install the vacuum sealing O-ring, cooling water sealing O-ring, and spring plunger respectively to complete the target preparation.

[0045] While the specific embodiments of the present invention have been described above in conjunction with the accompanying drawings, this is not intended to limit the scope of protection of the present invention. Those skilled in the art should understand that various modifications or variations that can be made by those skilled in the art without creative effort based on the technical solutions of the present invention are still within the scope of protection of the present invention.

Claims

1. A method for producing a medium-energy proton cyclotron accelerator 68 Ge's capsule target, characterized in that... Includes the capsule target and the copper heat dissipation target holder; The capsule target includes a niobium cladding film, a niobium cladding shell, and a gallium metal target encapsulated inside both. The niobium cladding film is located on the proton incident side, and the niobium cladding shell surrounds the side and back sides of the gallium metal target. The edge of the niobium cladding shell is provided with a stepped structure for limiting the niobium cladding film. The copper heat dissipation target support has a stepped structure, including an upper target support and a lower target support. The upper target support has a groove on the side facing the capsule target body, which is used to place the capsule target body. A cooling channel is provided on the other side of the upper target support opposite to the groove. The lower target support has a step on its outer periphery, and a vacuum sealing ring is provided at the step. The raised part of the step is used to guide and insert into the flange of the target station vacuum chamber and press and seal it. A spring plunger is provided on the outer periphery of the lower target support, and a spring top ball is provided at the top of the spring plunger for engaging with the target gripper groove.

2. Production of a medium-energy proton cyclotron accelerator as described in claim 1 68 Ge's capsule target, characterized in that... The thickness of the niobium cladding film is less than the thickness of the niobium cladding shell.

3. Production of a medium-energy proton cyclotron accelerator as described in claim 1 68 Ge's capsule target, characterized in that... The cooling channel is in the shape of a longitudinal cuboid.

4. Production of a medium-energy proton cyclotron accelerator as described in claim 1 68 Ge's capsule target, characterized in that... The lower target support is provided with a female cooling water pipe inlet. The inlet side of the female cooling water pipe inlet is chamfered and flared to facilitate the guide and fit with the male inlet on the target gripper. The inner wall of the female cooling water pipe inlet is machined with a cooling water sealing ring groove, and a built-in cooling water sealing ring is used to prevent cooling water leakage.

5. Production of a medium-energy proton cyclotron accelerator as described in claim 1 68 Ge's capsule target, characterized in that... Two spring plungers are symmetrically arranged in the width direction of the copper heat dissipation target holder.

6. Production of a medium-energy proton cyclotron accelerator as described in claim 1 68 Ge's capsule target, characterized in that... The gallium target is made of naturally abundant gallium and is encapsulated in a solid state within a niobium-clad cavity.

7. A method for producing a medium-energy proton cyclotron accelerator as described in any one of claims 1-6 68 The method for preparing a capsule target for Ge is characterized in that, Includes the following steps: S1. Take an oxygen-free copper block as the upper half blank of the copper heat dissipation target support, and mill a groove on the side of the capsule target body to match the shape of the niobium cladding thick shell. S2. Embed the niobium plate into the groove, and use diffusion welding process to weld the niobium plate to the upper half of the copper heat dissipation target support as a whole. Then, mill a longitudinal rectangular cooling channel on the cooling channel side of the upper half, and mill the niobium plate on the capsule target side to form a niobium-clad thick shell. S3. Complete capsule target encapsulation in a low-temperature environment: Liquid gallium metal is frozen into solid by liquid nitrogen, pressed and cut into gallium sheets that match the inner cavity of the niobium shell, and then placed into the inner cavity of the thick niobium shell. The niobium shell film is covered and the step structure is used for positioning. Pulsed laser welding is used to seal the joint between the film and the thick shell. S4. Mill the lower half of the copper heat dissipation target support to form the cooling water channel, spring plunger mounting hole and target station docking step; S5. After pre-placing the brazing filler metal on the mating surfaces of the upper and lower parts of the copper heat dissipation target holder, vacuum brazing is used to weld the upper and lower parts into an integral target holder. S6. Install the vacuum sealing O-ring, cooling water sealing O-ring, and spring plunger respectively to complete the target preparation.

8. Production of a medium-energy proton cyclotron accelerator as described in claim 7 68 The method for preparing a capsule target for Ge is characterized in that, The process conditions for diffusion welding in step S2 are: vacuum degree not less than 5 × 10⁻⁶. -3 The welding temperature is 800℃~900℃, the applied pressure is 10~20 MPa, and the holding time is 30~60 min.

9. Production of a medium-energy proton cyclotron accelerator as described in claim 7 68 The method for preparing a capsule target for Ge is characterized in that, In step S3, the pulsed laser welding adopts a low heat input mode, the width of the welding heat-affected zone is no more than 0.5 mm, and the solid metal gallium inside the niobium cladding cavity does not melt during the welding process.

10. The method for preparing a capsule target for producing 68Ge in a medium-energy proton cyclotron accelerator as described in claim 7, characterized in that, The vacuum brazing in step S5 is performed at 10 -2 The process is carried out under a Pa-level vacuum environment, and the airtightness leakage rate of the mating surface between the upper and lower parts of the copper heat sink support after brazing is no greater than 1×10⁻⁶. -9 Pa·m 3 / s.