Composition with latex based on 2-octyl acrylate / methyl methacrylate and photoinitiator

By using a combination of polymer particles of 2-octyl acrylate, methyl methacrylate, and olefinic unsaturated acid monomers with a low concentration of photoinitiator, the brittleness and lifespan damage issues of coatings when improving DPUR were solved, achieving high stain resistance and time stability.

CN123076649APending Publication Date: 2026-11-10ROHM & HAAS CO
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202580022129.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2024-03-19
Filing Date
2025-02-28
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

In existing waterborne exterior architectural coatings, the increase in the glass transition temperature (Tg) of the latex when improving stain resistance (DPUR) leads to brittleness, swelling, and shrinkage of the coating, and the amount of UV-active photoinitiators required to improve DPUR also impairs the coating's lifespan.

Method used

A water-based dispersion is formed using polymer particles containing 2-octyl acrylate, methyl methacrylate and olefinic unsaturated acid monomers, with a Tg in the range of -20°C to 20°C, and combined with 0.02% to 4% by weight of photoinitiator, for use in paint compositions.

Benefits of technology

With low concentrations of photoinitiator, the coating exhibits high stain resistance and time stability, avoiding the adverse effects of premature degradation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

The present invention relates to a composition comprising: a) an aqueous dispersion of polymer particles comprising structural units of 2-octyl acrylate, methyl methacrylate and an ethylenically unsaturated acid monomer; and b) a photoinitiator. The composition of the present invention can be used for example in architectural coating formulations, especially exterior architectural paint formulations.
Need to check novelty before this filing date? Find Prior Art

Description

Background Technology

[0001] This invention relates to compositions comprising a latex based on 2-octyl acrylate / methyl methacrylate and a photoinitiator. The aqueous dispersion of polymer particles (latex) present in waterborne exterior architectural coating formulations comprises polymers typically having structural units of butyl acrylate, methyl methacrylate, and methacrylic acid, as well as auxiliary special acrylic monomers (such as urea methacrylate). It is desired that coatings produced from these formulations withstand exposure to commonly occurring environmental stresses (such as UV exposure to sunlight, seasonal temperature changes, precipitation, and contaminants) while maintaining an acceptable aesthetic appearance. A commonly used aesthetic measure is the stain resistance (DPUR) of the coating when exposed to contaminants. DPUR is largely influenced by the surface hardness of the coating; therefore, it can be measured by adjusting the glass transition temperature (T) of the latex. g Increasing the temperature above 25°C can improve DPUR. Unfortunately, latex T... g Increased levels of T often lead to brittleness, swelling, and shrinkage in coatings due to seasonal changes, especially in wood substrates. g The DPUR of coated products prepared from latex formulations at temperatures below 15°C can be improved to acceptable levels by including an effective amount of a UV-active photoinitiator (such as benzophenone). However, the amount of photoinitiator required to achieve acceptable DPUR often impairs the effective life of the coating, as manifested by loss of gloss, loss of tone, binder chalking, and surface cracking. Therefore, the development of coatings with moderately low T g The latex will be advantageous, as it provides the benefits of good DPUR performance without the adverse effects of premature degradation of the coating when exposed to outdoor conditions. Summary of the Invention

[0002] This invention addresses a need in the art by providing a composition comprising: a) an aqueous dispersion of polymer particles comprising structural units of 2-octyl acrylate, methyl methacrylate, and an olefinically unsaturated acid monomer; and b) a photoinitiator, wherein the Tg of the polymer particles is as measured by differential scanning calorimetry. g Within a temperature range of -20°C to 20°C, wherein the concentration of the photoinitiator is in the range of 0.02 wt% to 4 wt% based on the weight of the polymer particles and the photoinitiator. The compositions of the present invention can be used in paint compositions, particularly exterior paint compositions forming coatings with high stain resistance and improved integrity over time. Detailed Implementation

[0003] This invention is a composition comprising: a) an aqueous dispersion of polymer particles comprising structural units of 2-octyl acrylate, methyl methacrylate, and an olefinically unsaturated acid monomer; and b) a photoinitiator, wherein the Tg of the polymer particles is as measured by differential scanning calorimetry. g Within the range of -20°C to 20°C, the concentration of the photoinitiator is in the range of 0.02 wt% to 4 wt% based on the weight of the polymer particles and the photoinitiator.

[0004] Polymer particles typically have a z-average particle size in the range of 50 nm to 300 nm, as measured by dynamic light scattering. The glass transition temperature (Tg) of the polymer particles is measured by dynamic scanning calorimetry. g The temperature range is -20°C, preferably -10°C to 20°C, and preferably to 10°C. In a preferred embodiment, the polymer particles comprise at least 90% by weight, more preferably at least 95% by weight, structural units of 2-octyl acrylate and methyl methacrylate. In this embodiment, based on the weight of the polymer particles, the polymer particles preferably comprise 45% by weight, more preferably 50% to 70% by weight, more preferably to 60% by weight, structural units of 2-octyl acrylate; and preferably 29% by weight, more preferably 40% to 54% by weight, more preferably to 48% by weight, structural units of methyl methacrylate; and 0.2% by weight, more preferably 0.5% by weight, and most preferably 1.0% to 5% by weight, and more preferably 3% by weight, of an olefinic unsaturated acid monomer, preferably one or more olefinic unsaturated acid monomers selected from the group consisting of: acrylic acid, methacrylic acid, itaconic acid, and ethyl methacrylate 2-phosphate (PEM).

[0005] In another embodiment, the polymer particles comprise 25% to 42% by weight of ethyl acrylate structural units; 25% to 42% by weight of 2-octyl acrylate structural units; 16% to 40% by weight of methyl methacrylate structural units; and 0.2% to 5% by weight of olefinic unsaturated acid monomer structural units.

[0006] The polymer particles may also contain structural units of one or more auxiliary monomers, such as urea methacrylate, acetyl methacrylate (AAEM), diacetone acrylamide (DAAM), and 2-(dimethylamino) methacrylate (DMAEMA), the concentration of which is typically no more than 15% by weight based on the weight of the polymer particles.

[0007] The term "structural unit" is used herein to describe the residue of the stated monomer after polymerization. For example, the structural unit of methyl methacrylate is shown below:

[0008]

[0009] The dashed lines represent the connection points between the structural units and the polymer backbone.

[0010] Photoinitiators are one or more compounds that generate free radicals through hydrogen atom extraction (i.e., Norish type II chemistry) when exposed to light wavelengths in the 100 nm to 400 nm range, or that undergo homolytic cleavage (i.e., Norish type I chemistry) when exposed to wavelengths in the 100 nm to 400 nm range. Examples of photoinitiators include benzophenone, methyl 2-benzoylbenzoate, 4-methylbenzophenone, 2,2-dimethoxy-2-phenylacetophenone, 4-methoxybenzophenone, 3,4-dimethylbenzophenone, 4-hydroxybenzophenone, 2-ethylanthraquinone, 2-(p-toluyl)benzoic acid, benzoin isobutyl ether, 4-benzoylbiphenyl, p-anetoin, 4-(4-methylphenylthio)benzophenone, 4,4'-dimethylbenzophenone, trimethylbenzophenone, etc. Phenylacetic acid, phenylbis(2,4,6-trimethylbenzoyl)phosphine oxide, ethyl-2,4,6-(trimethylbenzoyl)phosphine oxide, 2,4,6-trimethylbenzophenone, 4-phenylbenzophenone, isopropylthioxanthone, benzoyl ether, benzophenone hydrazone, diphenylacetic acid, benzophenone methacrylate, vinylbenzylmethylbenzoylbenzoate, hydroxymethylacryloyloxypropylmethylbenzoylbenzoate, hydroxymethylacryloyloxypropylbenzophenone, benzophenones substituted with hydroxyl-terminated epoxyalkyl groups as described in US 11760713 B2, and commercially available polymeric benzophenones, examples of which include Omnipol 2702, Omnipol 910, and Omnipol BP photoinitiators.

[0011] Based on the weight of the polymer particles and the photoinitiator, the concentration of the photoinitiator is preferably in the range of 0.05% or 0.1% by weight to 2% or 1% by weight to 0.6% or 0.4% by weight.

[0012] Latex can be advantageously prepared by emulsion polymerization, a process well-known in the art. Latex can be prepared by, for example, single-stage, multi-stage, or dynamite-feed polymerization methods, and can have various particle size distributions.

[0013] The compositions of the present invention can be prepared in a variety of ways, including a) contacting the photoinitiator with the monomer emulsion prior to emulsion polymerization; b) contacting the photoinitiator with an aqueous dispersion of polymer particles; or c) contacting the photoinitiator with a coating or pre-coating containing polymer particles.

[0014] In another aspect, the present invention is a paint composition comprising water, latex, photoinitiator, dispersant, surfactant, and rheology modifier, and optionally one or more of the following materials: inorganic opaque pigments such as TiO2, organic passivating pigments such as opaque polymers, agglomerators, extenders, and light stabilizers such as hindered amine light stabilizers. The paint composition may have any desired pigment volume concentration (PVC), including PVC in the range of 5 to 70. PVC is defined by the following formula:

[0015]

[0016] The compositions of the present invention can also be, for example, caulking agents, sealants, roofing coatings, or clear coatings for wood or leather. For paint compositions, the volatile organic compound (VOC) content is preferably <50 g / L, or <10 g / L, or 0 g / L, as determined by ASTM D3960-02.

[0017] Another advantage of 2-octyl acrylate is that it is an alkaline pyrolysis product of ricinoleic acid, which is found in castor oil. There is an ongoing need to find bio-based alternatives to fossil fuels; 2-octyl acrylate provides such an alternative. Notably, it has been surprisingly found that coatings prepared from paint formulations containing 2-octyl acrylate-based latex exhibit excellent DPUR at relatively low concentrations of photoinitiators. Example Differential scanning calorimetry for determining glass transition temperature

[0018] Differential scanning calorimetry (DSC) was used to calculate the T of the latex. g The latex sample was dried, placed in an aluminum pan, and rolled up and closed. The pan was placed in a DSC unit (TA Instruments Discovery 2500). The pan was then exposed to a thermal cycle with the following programmed instructions: heating to 150.00°C at 20.00°C / min, holding isothermally for 2.00 min, cooling to -90.00°C at 20.00°C / min, holding isothermally for 2.00 min, and heating to 150.00°C at 20.00°C / min. Thermal data were collected during the second heating cycle. T was measured at the inflection point of the heat flow curve (the change in the second derivative value). g Table 1 illustrates the latexes used in the DPUR study. BA refers to n-butyl acrylate, 2-OA refers to 2-octyl acrylate, MMA refers to methyl methacrylate, MAA refers to methacrylic acid, UMA refers to urea methacrylate, and n-DCC refers to n-dodecyl mercaptan. C1 refers to Comparative Example 1 latex; C2 refers to Comparative Example 2 latex; Ex1 refers to Example 1 latex; and Ex2 refers to Example 2 latex. Table 1 - Description of Latex

[0019] Preparation of paint formulations

[0020] These example latexes and comparative example latexes were used to prepare paints suitable for external applications. Table 2 illustrates the grinding process for each formulation; pbw refers to parts by weight of each component. The components were added in specified amounts to a steel grinding jar and mixed at 2000 rpm for 25 minutes using serrated mixing blades. The ground mixture was then divided equally into four 1L containers. Preparation of each individual paint was completed using a top-mounted mixer equipped with 3-blade paddles. Table 2 - Grinding Parts of Paint Mixtures

[0021]

[0022] TAMOL, TRITON, and DOWSIL are all trademarks of Dow Chemical Company and its affiliates.

[0023] Table 3 illustrates the mixing steps for the paint formulation. Add the components listed in the mixing table to the containers in their specified amounts, mixing at 1000 rpm. Then, dispense a portion (50.0 g) of each paint into nine plastic containers. ROPAQUE, TERGITOL, and ACRYSOL are all trademarks of Dow Chemical Company and its affiliates. Table 3 - Paint Mixing Parts of Paint Mixtures

[0024]

[0025] Solutions of each photoinitiator were prepared by dissolving 6.0 g of photoinitiator in acetone (54.0 g). The DPUR of each of paints 1 to 4 was evaluated with and without a photoinitiator. The photoinitiators were benzophenone (BZ), methyl 2-benzoylbenzoate (M2B), 4-methylbenzophenone (MBP), and 2,2-dimethoxy-2-phenylacetophenone (DMP). Each coating containing a photoinitiator was evaluated at two concentrations: 0.2 wt% and 0.6 wt% of photoinitiator based on the weight of the latex polymer particles. A 0.2 wt% sample was prepared by transferring 0.24 g of photoinitiator solution to 50 g of paints 1 to 4 in the first group while mixing at 500 rpm; a 0.6 wt% sample was prepared by transferring 0.72 g of photoinitiator solution to 4 of paints 1 to 4 in the second group. Each of these samples was applied to a chromate-treated aluminum panel (AL36, supplied by Q-Lab) using a Teflon scraper with a 10-mil gap. The paint samples were allowed to dry for 24 hours in a controlled temperature and humidity chamber (22°C, 50% RH). The panels were then placed in a Q-Lab QUV accelerated weathering tester using a 340nm UVA lamp with a radiation flux density of 0.89 W / m² at 60°C. 2 The panels were exposed to QUV for 72 hours, after which they were removed and prepared for DPUR testing. This was done by mixing Davis Colors 641 brown iron oxide (125g), water (250g), and TAMOL. ™ Prepare a dirt slurry using 731A dispersant (2 mL). Disperse the slurry using a benchtop mixer for 1 minute until smooth. Then, apply the dirt slurry to the lower half of an exposed painted panel and allow it to dry for 4 hours. Then, wash the dirt off the panel by hand using running water and a coarse cotton cloth. Then, allow the panel to dry for 24 hours and measure the color difference (ΔE) between the clean lower half of each panel and the upper half of each panel (without dirt applied, to be used as a reference).

[0026] Use the CIELAB 1976 formula shown below to calculate ΔE.

[0027]

[0028] “L*” is a measure of brightness, indexed from 0 to 100, where 0 is dark (no color) and 100 is bright (pure white). “a*” represents the red / green scale, and “b*” represents the blue / yellow scale. The sum of the squared differences of these values ​​measured by a colorimeter (BYK Spectro-Guide) gives the overall value of the color change, “ΔE”. Table 4 illustrates a summary of the ΔE values ​​from the DPUR results of the tested paints. The subscripts “0.2” and “0.6” refer to the weight percentage of the photoinitiator (PI) based on the weight of the latex solids. Table 4 - ΔE results from the DPUR study

[0029]

[0030] This table illustrates that paints containing 2-OA / MMA latex exhibit comparable ΔE values ​​in DPUR studies without a photoinitiator. However, paints containing 2-OA / MMA latex show a significant reduction in ΔE, where any photoinitiator in the tested photoinitiators is as low as 0.2% by weight. The low photoinitiator content required to achieve excellent DPUR results in more stable coating properties over time.

Claims

1. A composition comprising: a) an aqueous dispersion of polymer particles comprising structural units of 2-octyl acrylate, methyl methacrylate, and an olefinically unsaturated acid monomer; and b) a photoinitiator, wherein the Tg of the polymer particles is as measured by dynamic scanning calorimetry. g Within the range of -20°C to 20°C, wherein the concentration of the photoinitiator is in the range of 0.02% by weight to 4% by weight, based on the weight of the polymer particles and the photoinitiator.

2. The composition of claim 1, wherein, based on the weight of the polymer particles, the polymer particles comprise: 45% to 70% by weight of 2-octyl acrylate structural units; 29% to 54% by weight of methyl methacrylate structural units; and 0.2% to 5% by weight of the olefinic unsaturated acid monomer structural units.

3. The composition according to claim 2, wherein the olefinic unsaturated acid monomer is one or more monomers selected from the group consisting of: acrylic acid, methacrylic acid, itaconic acid, and ethyl 2-phosphate methacrylate; wherein the polymer particles have a T g Within the range of approximately -10°C to 10°C.

4. The composition according to claim 3, wherein the olefinic unsaturated acid monomer is methacrylic acid; and the photoinitiator is one or more compounds selected from the group consisting of: benzophenone, methyl 2-benzoylbenzoate, 4-methylbenzophenone, 2,2-dimethoxy-2-phenylacetophenone, 4-methoxybenzophenone, 3,4-dimethylbenzophenone, 4-hydroxybenzophenone, 2-ethylanthraquinone, 2-(p-toluyl)benzoic acid, benzoin isobutyl ether, 4-benzoylbiphenyl, p-anetoin, 4-(4-methylphenylthio)benzophenone, 4,4'-dimethylbenzophenone The photoinitiator comprises, but is not limited to, triphenylacetic acid, phenylbis(2,4,6-trimethylbenzoyl)phosphine oxide, ethyl-2,4,6-(trimethylbenzoyl)phosphine oxide, 2,4,6-trimethylbenzophenone, 4-phenylbenzophenone, isopropylthioxanthone, benzoyl ether, benzophenone hydrazone, diphenylacetic acid, benzophenone methacrylate, vinylbenzylmethylbenzoylbenzoate, hydroxymethylacryloyloxypropylmethylbenzoylbenzoate, hydroxymethylacryloyloxypropylbenzophenone, benzophenone substituted with hydroxyl-terminated epoxyalkyl groups, and polymeric benzophenone; wherein the concentration of the photoinitiator is in the range of 0.05% by weight to 1% by weight.

5. The composition according to claim 3, wherein the olefinic unsaturated acid monomer is methacrylic acid; the photoinitiator is one or more compounds selected from the group consisting of: benzophenone, methyl 2-benzoylbenzoate, 4-methylbenzophenone, and 2,2-dimethoxy-2-phenylacetophenone; wherein the concentration of the photoinitiator is in the range of 0.05% by weight to 0.6% by weight.

6. The composition according to claim 5, wherein the photoinitiator is methyl 2-benzoylbenzoate.

7. The composition according to claim 5, wherein the photoinitiator is 4-methylbenzophenone.

8. The composition of claim 1, wherein the polymer particles comprise 25% to 42% by weight of ethyl acrylate structural units; 25% to 42% by weight of 2-octyl acrylate structural units; 16% to 40% by weight of methyl methacrylate structural units; and 0.2% to 5% by weight of the olefinic unsaturated acid monomer structural units.

9. A paint composition comprising: a) an aqueous dispersion of polymer particles comprising structural units of 2-octyl acrylate, methyl methacrylate, and an olefinically unsaturated acid monomer; b) a photoinitiator; c) a dispersant; d) a surfactant; and e) a rheology modifier; wherein the Tg of the polymer particles, as measured by dynamic scanning calorimetry, is... g Within the range of -20°C to 20°C, wherein the concentration of the photoinitiator is in the range of 0.02% by weight to 4% by weight, based on the weight of the polymer particles and the photoinitiator.

10. The paint composition of claim 9, wherein, based on the weight of the polymer particles, the polymer particles comprise: 45% to 70% by weight of 2-octyl acrylate structural units; 29% to 54% by weight of methyl methacrylate structural units; and 0.2% to 5% by weight of the olefinic unsaturated acid monomer structural units, wherein the olefinic unsaturated acid monomer is one or more monomers selected from the group consisting of: acrylic acid, methacrylic acid, itaconic acid, and ethyl 2-phosphate methacrylate; and wherein the T of the polymer particles... g Within the range of approximately -10°C to 10°C.

11. The paint composition according to claim 10, wherein the olefinic unsaturated acid monomer is methacrylic acid; and the photoinitiator is one or more compounds selected from the group consisting of: benzophenone, methyl 2-benzoylbenzoate, 4-methylbenzophenone, 2,2-dimethoxy-2-phenylacetophenone, 4-methoxybenzophenone, 3,4-dimethylbenzophenone, 4-hydroxybenzophenone, 2-ethylanthraquinone, 2-(p-toluyl)benzoic acid, benzoin isobutyl ether, 4-benzoylbiphenyl, p-anetoin, 4-(4-methylphenylthio)benzophenone, 4,4'-dimethylbenzophenone, triphenylacetic acid, The composition comprises phenyl bis(2,4,6-trimethylbenzoyl)phosphine oxide, ethyl-2,4,6-(trimethylbenzoyl)phosphine oxide, 2,4,6-trimethylbenzophenone, 4-phenylbenzophenone, isopropylthioxanthone, benzoyl ether, benzophenone hydrazone, diphenylacetic acid, benzophenone methacrylate, vinylbenzylmethylbenzoylbenzoate, hydroxymethylacryloyloxypropylmethylbenzoylbenzoate, hydroxymethylacryloyloxypropylbenzophenone, benzophenone substituted with hydroxyl-terminated epoxyalkyl groups, and polymeric benzophenone; wherein the concentration of the photoinitiator is in the range of 0.05% by weight to 1% by weight; and wherein the composition further comprises TiO2.

12. The paint composition according to claim 10, wherein the olefinic unsaturated acid monomer is methacrylic acid; the photoinitiator is one or more compounds selected from the group consisting of benzophenone, methyl 2-benzoylbenzoate, 4-methylbenzophenone, and 2,2-dimethoxy-2-phenylacetophenone; wherein the concentration of the photoinitiator is in the range of 0.05% by weight to 0.6% by weight; and wherein the composition further comprises TiO2.

13. The paint composition according to claim 12, wherein the photoinitiator is methyl 2-benzoylbenzoate.

14. The paint composition according to claim 12, wherein the photoinitiator is 4-methylbenzophenone.

Citation Information

Patent Citations

  • Benzophenone derivative

    US11760713B2