A method for controlling the narrow slit at the edge of hot-rolled black sheet steel coils.

By optimizing slab thickness, vertical roll side pressure, heating temperature, and roughing descaling passes in the continuous casting and hot rolling processes, the problem of narrow slits at the edge of hot-rolled black skin of low-carbon steel was solved, and high yield production was achieved.

CN123102738APending Publication Date: 2026-11-17BAOSTEEL DESHENG STAINLESS STEEL
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611430149.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-15
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing technologies are insufficient to effectively eliminate edge slit defects in hot-rolled black steel coils of low-carbon steel, leading to yield loss and product downgrading, which in turn affects customer satisfaction.

Method used

By controlling the slab thickness in the continuous casting process, adjusting the side pressure of the vertical rolls, the heating temperature, and the number of descaling passes in the hot rolling process, and optimizing the exit temperature of the rough rolling mill, combined with the distribution of the side pressure of the vertical rolls, the intermediate slab temperature is ensured to be suitable, thus avoiding stress concentration at the edges and the generation of microcracks.

Benefits of technology

It significantly reduced the slit retention rate of hot-rolled black steel coils of low carbon steel to less than 1%, basically eliminating slit defects and greatly improving the yield rate of the production line.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123102738A_ABST
    Figure CN123102738A_ABST
Patent Text Reader

Abstract

This invention discloses a method for controlling the edge slits of hot-rolled black steel coils, comprising: 1) continuous casting process control: controlling the thickness of the steel slab in the continuous casting process to 220-235mm; 2) in the heating sub-process of the hot rolling process, controlling the slab exit temperature at 1220±20℃; in the hot rolling roughing sub-process, controlling the side pressure of the vertical rolls to +25mm-+50mm, with the side pressure distribution for each pass as follows: 10%-16% for the first pass, 27%-33% for the second pass, 40%-45% for the third pass, and 10%-15% for the fourth pass; controlling the number of descaling passes in the roughing process to four to six, and controlling the exit temperature of the roughing process to 1050±20℃. By coordinating the continuous casting and hot rolling processes, the slit retention rate of hot-rolled black steel coils can be reduced to less than 1%, or even to 0%, essentially eliminating slit defects and greatly improving the yield of the production line.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of stainless steel smelting, and more particularly to a method for controlling the narrow slit at the edge of hot-rolled black steel sheets. Background Technology

[0002] After the slab is heated in the hot rolling furnace, a defect of a certain depth will form at the edge during the rough rolling stage. This defect is inherited by the finished black strip coil, forming a slit defect, which has a significant adverse impact on the product quality of downstream customers. Taking the applicant's 1780 hot rolling production line as an example, this production line is configured with two vertical rolling mills, E1 and E2, to achieve width control. Cold rolling customers have reported that the Q195 and SPHD low carbon steel produced by this production line in 2024 has a slit defect. This type of defect is deep and has a large distance from the edge of the strip, causing frequent customer complaints. This not only leads to a loss of yield in the cold rolling process, but in severe cases, it can also cause product downgrading or even scrapping. The prevailing industry view is that the mechanism of edge slot formation is that after the slab undergoes rough rolling and side pressing, cracks or folds appear on the edges of the intermediate slab, which then form black line-like slots after subsequent flat rolling. For example, the article "Edge Quality Control of 304 Stainless Steel Hot-Rolled Strip" in the 5th issue of *World Steel* in 2014 states that the "slot" defect is caused by the side compression lines transferring to the upper and lower surfaces of the strip due to metal flow during rough rolling, and is a defect that is difficult to completely avoid in hot rolling production. The article suggests shifting the vertical roll reduction to subsequent passes to improve the slot defect with a smaller vertical roll reduction. However, actual production has shown that even after adopting the above process adjustment methods, the slot defect remains prominent.

[0003] Therefore, how to eliminate the narrow gaps at the edges of hot-rolled black steel coils has become a key research topic for improving the yield rate of production lines. Summary of the Invention

[0004] The purpose of this invention is to provide a method for controlling the narrow slit at the edge of hot-rolled black steel sheets.

[0005] The technical solution to achieve the purpose of this invention is: a method for controlling the narrow slit at the edge of hot-rolled black sheet of low-carbon steel, which includes: 1) continuous casting process control: controlling the thickness of the steel slab in the continuous casting process to 220mm~235mm; 2) Hot rolling process control: 2.1) Control of the heating sub-process in the heating furnace: The temperature of the slab exiting the furnace shall be controlled at 1220±20℃; 2.2) Control of hot rolling roughing process: The hot rolling roughing process includes vertical roll side pressing operation and roughing descaling operation. The vertical roll side pressing operation is controlled at +25mm to +50mm, and the side pressing distribution of each pass is 10% to 16% for the first pass, 27% to 33% for the second pass, 40% to 45% for the third pass, and 10% to 25% for the fourth pass. The roughing descaling operation is controlled to have four to six passes, and the water pressure of each pass is the conventional parameters for roughing descaling. The roughing mill exit temperature is controlled at 1050±20℃.

[0006] Through years of production line practice, the inventors discovered that simply controlling the side pressure of the vertical rolls cannot eliminate the narrow gaps at the edges of hot-rolled black steel coils. It is necessary to comprehensively consider the thickness of the steel slab and various stages of the hot rolling process. 1. This invention adjusts the side pressure of the vertical rolls for low-carbon steel from +5mm to +25mm to +50mm. The increased side pressure helps to close the looseness, micro-cracks, and vibration marks at the corners of the continuously cast slab. At the same time, the literature "Quality Control of Edges of Hot-Rolled Steel Strip of 304 Stainless Steel" teaches that the reduction of the vertical rolls in each pass should be shifted to the next pass. Through statistical analysis of a large amount of field production data, the inventors found that increasing the side pressure of the vertical rolls in each pass (currently, the conventional side pressure in each pass is about 5%) and using the vertical rolls to trim the edges of the slab in the previous pass at higher temperatures results in a flat and slightly convex regular cross-section on the sides of the intermediate slab, without local protrusions or depressions. During horizontal rolling, the edge is subjected to uniform stress, avoiding local overpressure that induces new folds. It can also release the casting stress and rolling stress at the edge in advance during the high-temperature rough rolling stage. When rolling in the next pass after the vertical roll side pressure, the edge is less likely to generate micro-cracks and folds due to stress concentration, thereby inhibiting the formation of slits. 2. Through statistical analysis of a large amount of on-site production data, the inventors summarized the correlation between defects and process parameters and found that the existing slab thickness is generally 190-205mm. By increasing the slab thickness to 220-235mm, the temperature drop during the rough rolling process of the slab was reduced and the narrow gap was improved. If the slab thickness is further increased, the heating time and rough rolling load will be increased, which is detrimental to production. 3. The temperature of the intermediate billet during the roughing rolling process is also crucial for controlling the slits in carbon steel, and the main factor affecting the temperature of the intermediate billet is the hot rolling roughing process. The inventors discovered that excessively high intermediate billet temperatures during rough rolling (exiting at temperatures exceeding 1070°C) significantly increase the risk of iron oxide scale defects in low-carbon steel, affecting the surface quality control of the finished product. Conversely, excessively low intermediate billet temperatures (exiting at temperatures below 1030°C) result in high deformation resistance, poor plasticity, difficulty in pressing edges and corners during side pressing, and a tendency to generate hard micro-cracks. These cracks propagate into linear black lines along the edges, hindering metal flow. Furthermore, bulges and sharp corners generated during side pressing at low intermediate billet temperatures cannot smoothly transition, leading to edge biting, folding, and narrow slits during flat rolling. In the hot rolling process, the slab is heated to a certain temperature in the furnace before being rolled in the rough rolling mill. The temperature drop during rough rolling is primarily due to descaling water and air cooling. The furnace exit temperature is the initial temperature of the slab after rough rolling. The descaling water generally affects the temperature drop per pass. The temperature is approximately 5-10℃. Air cooling is mainly related to the total rolling time and ambient temperature of the roughing mill. Since the total rolling time and ambient temperature of the roughing mill do not vary much overall, the actual furnace exit temperature and the control of the descaling water in the roughing mill directly affect the temperature conditions during the roughing mill rolling process. The roughing mill exit temperature is the exit temperature of the intermediate billet in the last pass of the roughing mill. Therefore, the control of the furnace exit temperature, the control of the descaling pass, and the control of the roughing mill exit temperature are all to provide good temperature conditions for the side pressure of the intermediate billet. To ensure that the temperature of the intermediate billet is suitable, this invention controls the side pressure of the vertical rolls at +25mm to +50mm. The side pressure distribution for each pass is 10% to 16% for the first pass, 27% to 33% for the second pass, 40% to 45% for the third pass, and 10% to 15% for the fourth pass. The descaling passes are controlled at four to six, and the roughing mill exit temperature is controlled at 1050±20℃.

[0007] In summary, by coordinating adjustments to the continuous casting and hot rolling processes, the slit retention rate of hot-rolled black steel coils can be reduced to less than 1%, or even to 0%, essentially eliminating slit defects and significantly improving the yield rate of the production line. Attached Figure Description

[0008] Figure 1 This is a photograph of the white sheet roll obtained by conventional small side pressure control and pickling of low carbon steel SPHD in Comparative Example 1 of the present invention. Figure 2 This is a photograph of the white sheet roll obtained by the method for controlling the narrow slits at the edge of the hot-rolled black sheet roll of low carbon steel SPHD in Embodiment 1 of the present invention and after pickling. Figure 3 This is a photograph of the white sheet roll obtained by the low carbon steel SPHD after being treated with the method of controlling the narrow slits on the edge of the hot-rolled black sheet roll of low carbon steel and pickled in Embodiment 2 of the present invention. Figure 4This is a photograph of the white sheet obtained by the low carbon steel SPHD after being treated with the method for controlling the narrow slits at the edge of the hot-rolled black sheet of low carbon steel and then pickled, according to Example 3 of the present invention. Figure 5 This is a photograph of the white sheet obtained by the low carbon steel SPHD after being treated with the method for controlling the narrow slits at the edge of the hot-rolled black sheet of low carbon steel and then pickled, according to Example 4 of the present invention. Figure 6 This is a photograph of the white sheet obtained after the low-carbon steel SPHD in Embodiment 5 of the present invention is processed by the method for controlling the narrow slits at the edge of the hot-rolled black sheet of low-carbon steel and then pickled. Detailed Implementation

[0009] The preferred embodiments of the present invention will be described in detail below. Example 1

[0010] Taking hot-rolled black steel coil of Q195 / SPHD low-carbon steel as an example, a method for controlling the edge slit of hot-rolled black steel coil of low-carbon steel includes: 1) Continuous casting process control: The thickness of the steel slab is controlled at 230mm during the continuous casting process; 2) Hot rolling process control: 2.1) Control of the heating sub-process in the heating furnace: Control the slab exit temperature at 1209℃; 2.2) Control of hot rolling roughing process: The control of the hot rolling roughing process includes the control of the vertical roll side pressure, the control of the roughing descaling passes, and the control of the roughing exit temperature. The vertical roll side pressure is controlled at +30mm, and the side pressure of each pass is distributed as follows: 13% for the first pass, 30% for the second pass, 43% for the third pass, and 14% for the fourth pass. The roughing descaling passes are controlled to be six, and the roughing exit temperature is controlled at 1039℃.

[0011] Examples 2-6 Examples 2-6 use the same control method as Example 1, the difference being the specific process parameters. This invention also provides conventional low-side-pressure control methods as comparative examples 1-3, with specific process parameters shown in Table 1. Table 1

[0012] The slit retention rate (number of low-carbon steel slit-retained coils / number of low-carbon steel production coils) of low-carbon steel Q195 / SPHD after treatment in Examples 1-5 and Comparative Examples 1-4 are shown in Table 2.

[0013] Table 2

[0014] As shown in Table 2, when production is carried out according to Examples 1-5, with the side pressure increased to 25mm-50mm, the slab thickness increased to 230mm, the furnace exit temperature increased to 1200-1240℃, and the roughing mill exit temperature increased to above 1030℃, the slit defect is eliminated. Figures 2-6 The image shows a white sheet roll obtained by pickling the low carbon steel SPHD treated in Examples 1-5. The narrow slits on the edge of the white sheet roll are eliminated, and there are only very shallow indentations, which meet the customer's requirements.

[0015] In contrast, the slab thickness of Comparative Example 1 was only 200mm, and the slit retention rate reached 5.9%. Figure 1 As can be seen, the photograph of the white sheet obtained by conventional small side pressure control and pickling of low carbon steel SPHD in Comparative Example 1 shows obvious slit defects; compared with Comparative Example 1, Comparative Example 2 increases the slab thickness, but the vertical roll side pressure is only 4%, and the slit retention rate reaches 6%; Comparative Example 3 has slightly lower furnace exit temperature and roughing mill exit temperature. Although the vertical roll side pressure and slab thickness are increased, the slit retention rate is still 3.5%; Comparative Example 4 increases the slab thickness to 230mm and increases the vertical roll side pressure. However, the roughing mill exit temperature is low. Although the slit retention rate is still unqualified, the slit retention rate is significantly lower than that of Comparative Example 1, Comparative Example 2 and Comparative Example 4. The slit retention rate is 64% lower than that of Comparative Example 1.

[0016] By comparing Examples 1-5 with Comparative Examples 1-4, and by comparing the comparative examples among themselves, it can be seen that only when the vertical roll side pressure, slab thickness, furnace exit temperature, and roughing mill exit temperature are adjusted simultaneously can the slit defect be eliminated.

[0017] The above description is merely an embodiment of the present invention and does not limit the patent scope of the present invention. Any equivalent process transformations made using the content of the present invention specification, or direct or indirect applications in other related technical fields, are similarly included within the patent protection scope of the present invention.

Claims

1. A method for controlling the narrow slit at the edge of a hot-rolled black sheet steel coil, characterized in that: It includes: 1) Continuous casting process control: In the continuous casting process, the thickness of the steel slab is controlled between 220mm and 235mm; 2) Hot rolling process control: 2.1) Control of the heating sub-process in the heating furnace: The temperature of the slab exiting the furnace shall be controlled at 1220±20℃; 2.2) Control of hot rolling roughing process: The hot rolling roughing process includes vertical roll side pressing operation and roughing descaling operation. The vertical roll side pressing operation is controlled at +25mm to +50mm. The side pressing of each pass is distributed as follows: 10% to 16% for the first pass, 27% to 33% for the second pass, 40% to 45% for the third pass, and 10% to 25% for the fourth pass. The roughing descaling operation is controlled at four to six passes. The roughing exit temperature is controlled at 1050±20℃.