A copper faucet casting equipment and method
By using a micro-motion mechanism and a hammering unit in a graded and coordinated process in a copper faucet casting molding equipment, the problem of decreased flow and filling performance of low-lead copper molten metal was solved, achieving efficient bubble removal and improving casting quality and production efficiency.
Patent Information
- Application Number
- CN202611581952.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-13
- Publication Date
- 2026-11-17
AI Technical Summary
In the existing technology, the flow and filling performance of low-lead copper melt is reduced, which makes it difficult for copper faucets to completely remove tiny air bubbles inside the cavity in complex internal cavities, thin-walled flow channels and dead corners, forming pores and pinhole defects, affecting product quality and production yield.
Using copper faucet casting equipment, a micro-motion mechanism and an external tapping unit are set in the mold to achieve graded and coordinated processing. First, the micro-motion mechanism peels off and gathers micro-bubbles on the wall surface, and then the tapping unit causes the bubbles to float up and be discharged. Combined with internal turbulence and external vibration, a directional driving and exhaust effect is formed.
It effectively reduces internal porosity and pinhole defects in castings, improves the casting quality and yield of copper faucets, and avoids new defects such as churning of copper liquid and solidification shell.
Smart Images

Figure CN123102928A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of casting and molding technology, and in particular to a casting and molding equipment and method for copper faucets. Background Technology
[0002] In the mass production of copper faucets, gravity casting is the mainstream process for blank forming. With the implementation of global standards for low-lead drinking water contact materials, low-lead copper alloys have become the core raw material for plumbing and sanitary ware products. Due to the significant reduction in the proportion of lead, the flow and filling performance of low-lead copper melt has decreased significantly. When filling complex inner cavities, thin-walled channels, corners, and dead corners of the faucet, the air inside the cavity cannot be completely expelled, easily forming a large number of diffuse microbubbles that adhere to the inner wall of the cavity. The traditional method of relying on the parting surface venting groove and the top riser for natural venting is difficult to effectively remove the microbubbles adhering to the wall, ultimately leading to defects such as pores and pinholes inside the casting. This not only reduces the structural strength and sealing reliability of the product, but also significantly increases the production scrap rate, becoming the main technical bottleneck for the large-scale mass production of low-lead copper faucets.
[0003] In current production, external mold tapping and overall frame vibration are commonly used to assist in venting. However, these solutions generally use continuous vibration with a single parameter throughout the entire process, which can only cause indiscriminate disturbance to the copper liquid inside the cavity. They cannot achieve graded and coordinated treatment of the aggregation, growth, and directional expulsion of diffuse microbubbles attached to the wall surface. The improvement effect on micro pinhole defects is very limited. If the vibration amplitude and frequency are blindly increased in order to improve the venting effect, it is very easy to cause problems such as copper liquid churning and air entrapment, and damage to the initial solidified shell, which may induce new casting quality defects. Summary of the Invention
[0004] The purpose of this invention is to provide a copper faucet casting equipment and method, which solves the problem that existing technologies use external mold hammering and overall frame vibration to assist in venting. However, such solutions generally use continuous vibration with a single parameter throughout the entire process, which can only generate indiscriminate disturbance to the copper liquid inside the cavity. They cannot achieve graded and coordinated treatment of the aggregation, growth, and directional expulsion of diffuse microbubbles attached to the wall surface, and the improvement effect on micro-pinhole defects is very limited.
[0005] To achieve the above objectives, the present invention provides a copper faucet casting equipment, including a mold, a top cover, and a casting assembly, wherein the top cover is disposed above the mold; The casting assembly includes a feed pipe, an internal contact block, multiple micro-motion mechanisms, an inlet sealing plate, and multiple striking units. The feed pipe is connected to the top cover. The mold has an inlet. The feed pipe is located above the inlet. The internal contact block and multiple micro-motion mechanisms are sequentially located inside the mold. The inlet sealing plate is located inside the top cover. The multiple striking units are sequentially distributed outside the top cover.
[0006] The micro-motion mechanism includes a micro-motion cylinder and a micro-motion sealing block. The micro-motion cylinder is disposed inside the mold, and the output end of the micro-motion cylinder is fixedly connected to the micro-motion sealing block. The micro-motion sealing block is slidably connected to the mold.
[0007] The striking unit includes a striking support plate, a striking drive motor, and a striking block. The striking support plate is disposed above the top cover, and the striking drive motor is disposed on the striking support plate. The output end of the striking drive motor is fixedly connected to the striking block.
[0008] The casting assembly further includes an internal lifting cylinder and an inlet sealing unit. The internal lifting cylinder is located above the top cover, and its output end passes through the top cover and is fixedly connected to the internal contact block. The inlet sealing unit is located inside the top cover and above the mold.
[0009] The inlet sealing unit includes a lifting electric slide rail and a transverse electric slide rail. The lifting electric slide rail is located inside the top cover. The output end of the lifting electric slide rail is fixedly connected to the transverse electric slide rail. The output end of the transverse electric slide rail is fixedly connected to the inlet sealing plate. The inlet sealing plate is adapted to the feed port.
[0010] The casting assembly further includes a movable sealing unit and multiple side-opening cylinders. The movable sealing unit is disposed on the top cover, and the multiple side-opening cylinders are sequentially disposed on both sides of the mold.
[0011] The movable sealing unit includes a metal sealing ring, two inflatable sealing mechanisms, multiple sealing locking mechanisms, a movable sealing strip, and multiple reset mechanisms. The metal sealing ring is located below the top cover. The mold has an annular groove, and the metal sealing ring is adapted to the annular groove. The two inflatable sealing mechanisms are respectively located on the outer and inner sides of the metal sealing ring. The multiple sealing locking mechanisms are sequentially located inside the metal sealing ring. The two ends of the movable sealing strip are fixedly connected to the inner walls of the metal sealing ring and the top cover, respectively. The multiple reset mechanisms are sequentially located inside the top cover.
[0012] The inflatable sealing mechanism includes an air pump and an inflatable sealing bag. The air pump is located on one side of the metal sealing ring, and the output end of the air pump is connected to the inflatable sealing bag. The inflatable sealing bag is located on one side of the metal sealing ring. The sealing and locking mechanism includes a limiting block, a telescopic rod, a spring, and a first electromagnet. The metal sealing ring has a groove, the mold has a limiting groove, the limiting block is adapted to the groove, the two ends of the telescopic rod and the spring are fixedly connected to the inner wall of the groove and the limiting block, respectively, the spring is sleeved on the outside of the telescopic rod, and the first electromagnet is disposed on the inner wall of the groove. The first electromagnet attracts the limiting block.
[0013] The reset mechanism includes a reset cylinder and a second electromagnet. The reset cylinder is located inside the top cover, and its output end is fixedly connected to the second electromagnet. The second electromagnet attracts the metal sealing ring.
[0014] The present invention also provides a method for casting and molding a copper faucet, using the copper faucet casting and molding equipment described above, comprising the following steps: The mold is driven to close, the top cover moves down to close, the metal sealing ring is embedded in the annular groove and positioned and locked by the sealing locking mechanism, and the inflatable sealing bag is inflated and expands to stick to the groove wall, thus completing the double sealing of the parting surface. The molten copper is injected into the mold cavity through the feed pipe and the inlet. Multiple micro-motion mechanisms drive the micro-motion sealing block to reciprocate, peeling off the micro-bubbles attached to the cavity wall and causing them to converge towards the center. At the same time, the internal contact block reciprocates to disturb the molten copper, guiding the bubbles to gather towards the top. The inlet sealing plate moves to close the feed port, and multiple tapping units tap the top cover according to set parameters, causing the gathered bubbles to grow, float up, and be discharged from the cavity. After the casting is left to solidify and form, the air-filled sealing bag is deflated, the seal is released, the reset mechanism drives the metal sealing ring to retract and reset, and the top cover rises to separate from the mold. The mold is opened, and the formed copper faucet casting is removed, completing the single-cycle casting process.
[0015] This invention discloses a copper faucet casting equipment and method. During operation, the copper faucet casting equipment first closes the mold by placing a top cover over it. Molten copper is then injected into the mold cavity through the feed pipe and inlet. During filling, multiple micro-motion mechanisms perform small reciprocating movements on the inner wall of the cavity, disturbing the molten copper near the wall and causing microbubbles adhering to the inner wall to converge towards the cavity. Simultaneously, an internal contact block agitates the molten copper in the center, guiding the bubbles to gather towards the top. After filling, an inlet sealing plate moves to close the inlet, maintaining a sealed state inside the cavity. Subsequently, multiple striking units strike the outer wall of the top cover at a set frequency, transmitting vibrations to the molten copper inside the cavity, causing the gathered bubbles to continue growing and rise upwards. After the molten copper has completely solidified, the seal is released, and the top cover is separated from the mold, allowing the formed copper faucet casting to be removed. Therefore, a reciprocating micro-motion mechanism is set inside the mold, which works in conjunction with multiple tapping units on the outside of the top cover. First, the internal micro-motion removes and aggregates micro-bubbles on the wall surface, and then the external tapping vibration causes the bubbles to rise and be discharged, forming a graded and coordinated venting effect. This effectively removes micro-bubbles from the wall surface, significantly reduces porosity and pinhole defects inside the casting, improves the casting quality and production yield of copper faucets, and avoids the generation of new defects such as copper liquid churning and air entrapment, and damage to the initial solidification shell, without significantly increasing the vibration amplitude. Attached Figure Description
[0016] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the accompanying drawings used in the description of the embodiments or the prior art will be briefly introduced below.
[0017] Figure 1 This is a schematic diagram of the structure of the copper faucet casting equipment of the present invention.
[0018] Figure 2 This is a cross-sectional view of the copper faucet casting equipment of the present invention.
[0019] Figure 3 This is the invention Figure 1 Enlarged view of the local structure at point A.
[0020] Figure 4 This is the invention Figure 2 Enlarged view of the local structure at point B.
[0021] Figure 5 This is the invention Figure 2 Enlarged view of the local structure at point C.
[0022] Figure 6 This is a diagram of the internal structure of the top cover of the present invention.
[0023] Figure 7 This is a flowchart of the steps of the copper faucet casting method of the present invention.
[0024] 1-Mold, 2-Top cover, 3-Feed pipe, 4-Internal contact block, 5-Inlet sealing plate, 6-Feed port, 7-Micro-motion cylinder, 8-Micro-motion sealing block, 9-Tapping support plate, 10-Tapping drive motor, 11-Tapping block, 12-Internal lifting cylinder, 13-Lifting electric slide rail, 14-Horizontal electric slide rail, 15-Side opening and closing cylinder, 16-Metal sealing ring, 17-Modible sealing strip, 18-Annular groove, 19-Air pump, 20-Inflatable sealing bag, 21-Limiting block, 22-Telescopic rod, 23-Spring, 24-First electromagnet, 25-Groove, 26-Limiting groove, 27-Reset cylinder, 28-Second electromagnet. Detailed Implementation
[0025] The embodiments of the present invention are described in detail below. Examples of the embodiments are shown in the accompanying drawings. The embodiments described below with reference to the accompanying drawings are exemplary and intended to explain the present invention, but should not be construed as limiting the present invention.
[0026] Please see Figures 1 to 6 This invention provides a copper faucet casting equipment, including a mold 1, a top cover 2, and a casting assembly. The top cover 2 is disposed above the mold 1. The casting assembly includes a feed pipe 3, an internal contact block 4, multiple micro-motion mechanisms, an inlet sealing plate 5, and multiple striking units. The feed pipe 3 is connected to the top cover 2. The mold 1 has an inlet 6, and the feed pipe 3 is located above the inlet 6. The internal contact block 4 and the multiple micro-motion mechanisms are sequentially located inside the mold 1. The inlet sealing plate 5 is disposed inside the top cover 2, and the multiple striking units are sequentially distributed outside the top cover 2.
[0027] In this embodiment, the mold 1 and the top cover 2 together constitute the main body of the forming cavity of the casting. The feed pipe 3 is the pouring and feeding channel for molten copper, which can smoothly guide the molten copper into the cavity. The internal contact block 4 is a turbulence component in the middle of the cavity, which can guide the bubbles to float by turbulence in the middle of the molten copper through reciprocating motion. Multiple micro-motion mechanisms are embedded in the inner wall of the cavity, which can peel off the diffuse micro-bubbles attached to the cavity wall through small reciprocating motion. The inlet sealing plate 5 can close the feed port 6 after filling, ensuring the sealed environment inside the cavity. Multiple knocking units are distributed outside the top cover 2, which can cause the bubbles inside the cavity to gather, grow and be discharged upward through knocking vibration. Through the graded exhaust structure of the internal micro-motion turbulence and external knocking vibration, the micro-bubbles attached to the wall can be peeled off first and then directed to float upward, which can effectively solve the problem of limited exhaust effect of single vibration, greatly reduce the defects of air holes and pinholes inside the casting, and improve the casting quality and production yield of copper faucets.
[0028] Furthermore, the micro-motion mechanism includes a micro-motion cylinder 7 and a micro-motion sealing block 8. The micro-motion cylinder 7 is disposed inside the mold 1, and the output end of the micro-motion cylinder 7 is fixedly connected to the micro-motion sealing block 8. The micro-motion sealing block 8 is slidably connected to the mold 1.
[0029] In this embodiment, the micro-motion cylinder 7 is a power output component for micro-motion, which can output stable reciprocating extension and retraction power. The micro-motion sealing block 8 is the actuator that directly contacts the molten copper. Its outer wall is smoothly attached to the inner wall of the cavity. Driven by the micro-motion cylinder 7, it can perform small-amplitude high-frequency reciprocating sliding along the inner wall of the cavity, generating directional micro-disturbances on the molten copper near the wall surface. This peels off the micro-bubbles that are tightly attached to the inner wall of the cavity and causes them to converge towards the center of the cavity. At the same time, the sliding sealing structure can ensure the sealing of the side wall of the cavity, prevent the molten copper from seeping into the drive structure, and ensure the accuracy of the casting surface and the reliability of the equipment operation.
[0030] Furthermore, the striking unit includes a striking support plate 9, a striking drive motor 10, and a striking block 11. The striking support plate 9 is disposed above the top cover 2, and the striking drive motor 10 is disposed on the striking support plate 9. The output end of the striking drive motor 10 is fixedly connected to the striking block 11.
[0031] In this embodiment, the striking support plate 9 serves as the mounting base for the striking component, fixed above the top cover 2 to provide stable support for the striking action. The striking drive motor 10 is the power source for the striking action, which can precisely control the frequency and amplitude of the striking action to adapt to the venting requirements of different casting stages. The striking block 11 is the striking execution end, which periodically strikes the outer wall of the top cover 2 as the motor output shaft rotates, uniformly transmitting the vibration to the molten copper inside the cavity, causing the gathered microbubbles to continue to grow and rise. Through the striking vibration with controllable parameters, the problem of molten copper churning and entrapment caused by blindly increasing the vibration amplitude can be avoided, ensuring the stability and controllability of the venting process.
[0032] Furthermore, the casting assembly also includes an internal lifting cylinder 12 and an inlet sealing unit. The internal lifting cylinder 12 is disposed above the top cover 2. The output end of the internal lifting cylinder 12 passes through the top cover 2 and is fixedly connected to the internal contact block 4. The inlet sealing unit is disposed inside the top cover 2 and located above the mold 1.
[0033] In this embodiment, the internal lifting cylinder 12 is the lifting drive component of the internal contact block 4, which can drive the internal contact block 4 to reciprocate vertically along the cavity, generating longitudinal turbulence on the copper liquid in the middle of the cavity, guiding the peeled bubbles to gather in the top area of the cavity, forming a coordinated internal and external turbulence and exhaust effect with the micro-motion mechanism on the wall, further improving the bubble gathering efficiency; the inlet sealing unit is the displacement drive component of the inlet sealing plate 5, which can precisely control the position and clamping force of the inlet sealing plate 5 to achieve reliable sealing of the feed port 6, preventing external air from flowing back into the cavity after filling.
[0034] Furthermore, the inlet sealing unit includes a lifting electric slide rail 13 and a transverse electric slide rail 14. The lifting electric slide rail 13 is disposed inside the top cover 2. The output end of the lifting electric slide rail 13 is fixedly connected to the transverse electric slide rail 14. The output end of the transverse electric slide rail 14 is fixedly connected to the inlet sealing plate 5. The inlet sealing plate 5 is adapted to the feed port 6.
[0035] In this embodiment, the lifting electric slide rail 13 can drive the horizontal moving electric slide rail 14 and the inlet sealing plate 5 to complete the vertical lifting action as a whole. The horizontal moving electric slide rail 14 can drive the inlet sealing plate 5 to complete the horizontal displacement action. The two cooperate with each other to first move the inlet sealing plate 5 horizontally to directly above the feed port 6, and then press it down vertically to close the feed port 6. The displacement is accurate and the alignment is reliable. After closing, it can effectively isolate the inside of the cavity from the external environment, ensure the sealed environment inside the cavity during the vibration exhaust stage, and avoid air backflow affecting the exhaust effect.
[0036] Furthermore, the casting assembly also includes a movable sealing unit and a plurality of side opening and closing cylinders 15. The movable sealing unit is disposed on the top cover 2, and the plurality of side opening and closing cylinders 15 are sequentially disposed on both sides of the mold 1.
[0037] In this embodiment, the multiple side-opening and closing cylinders 15 are driving components for the mold 1 to separate and close. They are symmetrically arranged on both sides of the mold and can output power synchronously to ensure smooth and synchronous mold closing and separation. The movable sealing unit is a sealing execution component for the parting surface. It is set on the top cover 2 and can move synchronously with the top cover. After mold closing, it can perform multiple sealing treatments on the parting surface of the mold 1 and the top cover 2, further improving the overall sealing performance of the cavity, avoiding air leakage on the parting surface during vibration venting, ensuring that air bubbles are discharged directionally from the top venting path, and improving venting efficiency and effect.
[0038] Furthermore, the movable sealing unit includes a metal sealing ring 16, two inflatable sealing mechanisms, multiple sealing locking mechanisms, a movable sealing strip 17, and multiple reset mechanisms. The metal sealing ring 16 is disposed below the top cover 2. The mold 1 has an annular groove 18. The metal sealing ring 16 and the annular groove 18 are mutually adapted. The two inflatable sealing mechanisms are respectively disposed on the outer and inner sides of the metal sealing ring 16. The multiple sealing locking mechanisms are sequentially disposed inside the metal sealing ring 16. The two ends of the movable sealing strip 17 are respectively fixedly connected to the metal sealing ring 16 and the inner wall of the top cover 2. The multiple reset mechanisms are sequentially disposed inside the top cover 2.
[0039] In this embodiment, the metal sealing ring 16 is a rigid support skeleton for sealing the parting surface, embedded in the annular groove 18 to form a basic hard seal. The movable sealing strip 17 is a flexible connecting sealing component that can adaptively stretch and contract with the rise and fall of the metal sealing ring 16 to fill the gap between the top cover 2 and the metal sealing ring 16. The two inflatable sealing mechanisms are respectively arranged on the inner and outer sides of the sealing ring, and can form a flexible seal to fill tiny gaps through inflation. Multiple sealing locking mechanisms can lock the metal sealing ring 16 embedded in the groove to prevent the sealing ring from shifting during vibration. Multiple reset mechanisms can drive the metal sealing ring 16 to quickly retract and reset when the mold is opened to avoid interfering with the parting and picking action. Through the combination of hard seal, flexible inflatable seal, and locking positioning, the sealing reliability and stability of the parting surface are greatly improved.
[0040] Further, the inflation sealing mechanism includes an air pump 19 and an inflation sealing bag 20. The air pump 19 is disposed on one side of the metal sealing ring 16, and the output end of the air pump 19 is connected to the inflation sealing bag 20. The inflation sealing bag 20 is disposed on one side of the metal sealing ring 16. The sealing locking mechanism includes a limiting block 21, a telescopic rod 22, a spring 23, and a first electromagnet 24. The metal sealing ring 16 has a groove 25, and the mold 1 has a limiting groove 26. The limiting block 21 is adapted to the groove 25. The two ends of the telescopic rod 22 and the spring 23 are respectively fixedly connected to the inner wall of the groove 25 and the limiting block 21. The spring 23 is sleeved on the outside of the telescopic rod 22. The first electromagnet 24 is disposed on the inner wall of the groove 25, and the first electromagnet 24 attracts the limiting block 21.
[0041] In this embodiment, the air pump 19 is the air source power component for the air-sealed system, which can precisely control the inflation volume and air pressure of the air-sealed bag 20. After inflation, the air-sealed bag 20 can adaptively expand and fit tightly against the inner wall of the annular groove 18, filling the tiny gaps left by the hard seal and forming a reliable flexible seal. The limiting block 21 is the locking actuator, and the telescopic rod 22 is the telescopic guide component, ensuring that the telescopic path of the limiting block 21 is smooth and without deviation. The spring 23 is the elastic reset component, which releases thrust under normal conditions to push the limiting block 21 outward and into the limiting groove 26, completing the position locking of the sealing ring. After the first electromagnet 24 is energized, it generates magnetic attraction force to attract the limiting block 21 and retract it into the groove 25, quickly releasing the locking state. Through the structure of elastic engagement and magnetic unlocking, the locking state is stable and reliable, and the unlocking operation is convenient and efficient, which can quickly complete the positioning and release of the sealing ring.
[0042] Furthermore, the reset mechanism includes a reset cylinder 27 and a second electromagnet 28. The reset cylinder 27 is disposed inside the top cover 2. The output end of the reset cylinder 27 is fixedly connected to the second electromagnet 28. The second electromagnet 28 attracts the metal sealing ring 16.
[0043] In this embodiment, the reset cylinder 27 is a vertical drive component for the reset action, which can drive the second electromagnet 28 to complete the lifting action. After the second electromagnet 28 is energized, it can generate a strong magnetic attraction force to attract and fix the metal sealing ring 16. When the mold is opened, it can drive the metal sealing ring 16 to rise smoothly and retract to reset, avoiding the sealing ring from protruding below the top cover and interfering with the parting action. When the mold is closed, it can push the metal sealing ring 16 to accurately embed it into the annular groove 18. The lifting action is precise and controllable, and the reset is stable and reliable.
[0044] When using the copper faucet casting equipment of this embodiment, multiple side-opening cylinders 15 synchronously drive the mold 1 to close, the top cover 2 moves down to cover the top of the mold 1, the reset cylinder 27 pushes the second electromagnet 28 down, causing the metal sealing ring 16 to be embedded into the annular groove 18 of the mold 1; then the first electromagnet 24 is de-energized and loses its magnetic attraction, the spring 23 releases its elastic thrust to push the limiting block 21 outward along the groove 25 and into the limiting groove 26 to lock the position of the metal sealing ring 16, the movable sealing strip 17 stretches and unfolds with the metal sealing ring 16 to fill the gap between the top cover 2 and the metal sealing ring 16; then the air pump 19 starts to fill the air-filled sealing bag 20 with gas of a set pressure, so that the air-filled sealing bag 20 expands and sticks tightly to the inner and outer walls of the annular groove 18 to complete the double sealing of the parting surface. Molten copper is smoothly injected into the cavity of mold 1 through feed pipe 3 and inlet 6. During filling, multiple micro-actuators 7 are activated simultaneously, driving the corresponding micro-actuator sealing blocks 8 to slide back and forth along the inner wall of the cavity at a small amplitude and high frequency. This generates directional micro-disturbances on the molten copper near the wall, peeling off the diffuse micro-bubbles tightly attached to the inner wall of the cavity and causing them to converge towards the center of the cavity. At the same time, the internal lifting cylinder 12 is activated, driving the internal contact block 4 to move back and forth vertically along the cavity, disturbing the molten copper in the center of the cavity and guiding the peeled-off bubbles to converge towards the top area of the cavity. After filling is completed, the lifting electric slide rail 13 and the horizontal moving electric slide rail 14 work together to first drive the inlet sealing plate 5 to move horizontally to directly above the inlet 6, and then press down vertically to seal the inlet 6, ensuring the sealing performance of the upper part of the cavity and preventing external air from flowing back in. Subsequently, multiple striking drive motors 10 are started synchronously, driving the corresponding striking blocks 11 to periodically strike the outer wall of the top cover 2 at a set frequency and amplitude. The vibration is evenly transmitted through the top cover 2 to the molten copper inside the cavity, causing the gathered microbubbles to continue to grow and rise, and be discharged from the cavity through the top exhaust path. During the solidification process of the casting, the inflatable sealing bag 20 continuously maintains the set air pressure to ensure the sealing reliability of the parting surface and prevent external air from seeping into the cavity. After the casting has completely solidified, the air pump 19 extracts the gas from the air-sealed bag 20, causing the bag to shrink and detach from the groove wall. The first electromagnet 24 is energized to generate magnetic attraction, attracting the limiting block 21 to overcome the thrust of the spring 23 and retract into the groove 25, releasing the locking state of the metal sealing ring 16. Subsequently, the reset cylinder 27 drives the second electromagnet 28 to rise, and the metal sealing ring 16 rises and retracts synchronously through magnetic attraction. Then, the top cover 2 rises and separates from the mold 1. Multiple side opening and closing cylinders 15 drive the mold 1 to open, and the formed copper faucet casting can be taken out, completing the single-cycle casting process.
[0045] Please see Figure 7 The present invention also provides a method for casting and molding a copper faucet, using the aforementioned copper faucet casting and molding equipment, comprising the following steps: S1: Drive the mold 1 to close, the top cover 2 moves down to close, the metal sealing ring 16 is embedded in the annular groove 18 and positioned and locked by the sealing locking mechanism, the inflatable sealing bag 20 is inflated and expands to stick to the groove wall, and the parting surface is double sealed. S2: The copper liquid is injected into the cavity of the mold 1 through the feed pipe 3 and the inlet 6. Multiple micro-motion mechanisms drive the micro-motion sealing block 8 to reciprocate, peel off the micro bubbles attached to the cavity wall and make them converge towards the center. At the same time, the internal contact block 4 reciprocates up and down to disturb the copper liquid and guide the bubbles to gather towards the top. S3: The inlet sealing plate 5 moves to close the inlet port 6, and multiple tapping units tap the top cover 2 according to set parameters, causing the gathered bubbles to grow, float up and be discharged from the cavity; S4: After the casting is left to solidify and form, the air-filled sealing bag 20 is deflated, the sealing lock is released, the reset mechanism drives the metal sealing ring 16 to retract and reset, and the top cover 2 rises and separates from the mold 1; S5: Drive the mold 1 to open, take out the formed copper faucet casting, and complete the single-cycle casting process.
[0046] In this process, the mold 1 is driven to close, the top cover 2 moves down to close, the metal sealing ring 16 is embedded in the annular groove 18 and positioned and locked by the sealing locking mechanism, and the inflatable sealing bag 20 is inflated and expands to stick to the groove wall, completing the double sealing of the parting surface; the copper liquid is injected into the cavity of the mold 1 through the feed pipe 3 and the inlet 6, and multiple micro-motion mechanisms drive the micro-motion sealing block 8 to reciprocate, peeling off the micro-bubbles attached to the cavity wall and causing them to converge towards the center, while the internal contact block 4 reciprocates to disturb the copper liquid, guiding the bubbles to gather at the top; the inlet sealing plate 5 moves to close the inlet 6, and multiple tapping units tap the top cover 2 according to set parameters, causing the gathered bubbles to grow, float up and be discharged from the cavity. After the casting is left to stand and solidify, the inflatable sealing bag 20 is deflated, releasing the sealing lock, and the reset mechanism drives the metal sealing ring 16 to retract and reset, and the top cover 2 rises to separate from the mold 1; the mold 1 is driven to open, and the formed copper faucet casting is taken out, completing the single-cycle casting operation.
[0047] The above-disclosed embodiments are merely one or more preferred embodiments of this application and should not be construed as limiting the scope of this application. Those skilled in the art can understand that all or part of the processes for implementing the above embodiments and equivalent changes made in accordance with the claims of this application still fall within the scope of this application.
Claims
1. A copper faucet casting and molding equipment, comprising a mold and a top cover, wherein the top cover is disposed above the mold, characterized in that, It also includes casting components; The casting assembly includes a feed pipe, an internal contact block, multiple micro-motion mechanisms, an inlet sealing plate, and multiple striking units. The feed pipe is connected to the top cover. The mold has an inlet. The feed pipe is located above the inlet. The internal contact block and multiple micro-motion mechanisms are sequentially located inside the mold. The inlet sealing plate is located inside the top cover. The multiple striking units are sequentially distributed outside the top cover.
2. The copper faucet casting equipment as described in claim 1, characterized in that, The micro-motion mechanism includes a micro-motion cylinder and a micro-motion sealing block. The micro-motion cylinder is disposed inside the mold, and the output end of the micro-motion cylinder is fixedly connected to the micro-motion sealing block. The micro-motion sealing block is slidably connected to the mold.
3. The copper faucet casting equipment as described in claim 2, characterized in that, The striking unit includes a striking support plate, a striking drive motor, and a striking block. The striking support plate is disposed above the top cover, and the striking drive motor is disposed on the striking support plate. The output end of the striking drive motor is fixedly connected to the striking block.
4. The copper faucet casting and molding equipment as described in claim 3, characterized in that, The casting assembly also includes an internal lifting cylinder and an inlet sealing unit. The internal lifting cylinder is located above the top cover, and its output end passes through the top cover and is fixedly connected to the internal contact block. The inlet sealing unit is located inside the top cover and above the mold.
5. The copper faucet casting equipment as described in claim 4, characterized in that, The inlet sealing unit includes a lifting electric slide rail and a transverse electric slide rail. The lifting electric slide rail is located inside the top cover. The output end of the lifting electric slide rail is fixedly connected to the transverse electric slide rail. The output end of the transverse electric slide rail is fixedly connected to the inlet sealing plate. The inlet sealing plate is adapted to the feed port.
6. The copper faucet casting and molding equipment as described in claim 5, characterized in that, The casting assembly also includes a movable sealing unit and multiple side-opening cylinders. The movable sealing unit is disposed on the top cover, and the multiple side-opening cylinders are sequentially disposed on both sides of the mold.
7. The copper faucet casting and molding equipment as described in claim 6, characterized in that, The movable sealing unit includes a metal sealing ring, two inflatable sealing mechanisms, multiple sealing locking mechanisms, a movable sealing strip, and multiple reset mechanisms. The metal sealing ring is located below the top cover. The mold has an annular groove, and the metal sealing ring is adapted to the annular groove. The two inflatable sealing mechanisms are respectively located on the outer and inner sides of the metal sealing ring. The multiple sealing locking mechanisms are sequentially located inside the metal sealing ring. The two ends of the movable sealing strip are fixedly connected to the inner walls of the metal sealing ring and the top cover, respectively. The multiple reset mechanisms are sequentially located inside the top cover.
8. The copper faucet casting and molding equipment as described in claim 7, characterized in that, The inflation sealing mechanism includes an air pump and an inflation sealing bag. The air pump is located on one side of the metal sealing ring, and the output end of the air pump is connected to the inflation sealing bag. The inflation sealing bag is located on one side of the metal sealing ring. The sealing and locking mechanism includes a limiting block, a telescopic rod, a spring, and a first electromagnet. The metal sealing ring has a groove, the mold has a limiting groove, the limiting block is adapted to the groove, the two ends of the telescopic rod and the spring are fixedly connected to the inner wall of the groove and the limiting block, respectively, the spring is sleeved on the outside of the telescopic rod, and the first electromagnet is disposed on the inner wall of the groove. The first electromagnet attracts the limiting block.
9. The copper faucet casting and molding equipment as described in claim 8, characterized in that, The reset mechanism includes a reset cylinder and a second electromagnet. The reset cylinder is located inside the top cover, and its output end is fixedly connected to the second electromagnet. The second electromagnet attracts the metal sealing ring.
10. A method for casting and molding a copper faucet, using the copper faucet casting and molding equipment as described in claim 9, characterized in that, Includes the following steps: The mold is driven to close, the top cover moves down to close, the metal sealing ring is embedded in the annular groove and positioned and locked by the sealing locking mechanism, and the inflatable sealing bag is inflated and expands to stick to the groove wall, thus completing the double sealing of the parting surface. The molten copper is injected into the mold cavity through the feed pipe and the inlet. Multiple micro-motion mechanisms drive the micro-motion sealing block to reciprocate, peeling off the micro-bubbles attached to the cavity wall and causing them to converge towards the center. At the same time, the internal contact block reciprocates to disturb the molten copper, guiding the bubbles to gather towards the top. The inlet sealing plate moves to close the feed port, and multiple tapping units tap the top cover according to set parameters, causing the gathered bubbles to grow, float up, and be discharged from the cavity. After the casting is left to solidify and form, the air-filled sealing bag is deflated, the seal is released, the reset mechanism drives the metal sealing ring to retract and reset, and the top cover rises to separate from the mold. The mold is opened, and the formed copper faucet casting is removed, completing the single-cycle casting process.