Intelligent control method for ultra-low speed die casting of aluminum die casting parts for new energy vehicles

By analyzing the mold structure and acquiring real-time data in aluminum die castings for new energy vehicles, and dynamically adjusting the injection speed, the problem of coordinating venting and filling in the filling flow path of large aluminum die castings was solved, thereby improving the stability and filling capacity of the die casting process.

CN123102964APending Publication Date: 2026-11-17TIANJIN SHENGJINTE AUTO PARTS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611452713.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-18
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

During the filling process of large aluminum die-casting parts for new energy vehicles, the uneven propulsion speed of the aluminum liquid front is caused by multiple filling flow paths, different wall thickness areas, and long flow paths. Existing ultra-low speed die-casting methods are difficult to coordinate the discharge of residual gas in the exhaust path with the filling requirements of the far-end thin-walled area.

Method used

By analyzing the mold structure data, setting the detection and venting positions, collecting injection process data in real time, dynamically adjusting the injection speed, and generating a target injection speed, the residual gas discharge in the venting path and the filling requirements of the far-end thin-walled area are balanced.

Benefits of technology

It improves the coordination of filling and venting in the ultra-low speed die casting process of large aluminum die casting parts for new energy vehicles, reduces the possibility of the aluminum liquid front reaching the venting position too early, and enhances the stability of the die casting process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123102964A_ABST
    Figure CN123102964A_ABST
Patent Text Reader

Abstract

This invention discloses an intelligent control method for ultra-low speed die casting of aluminum die castings for new energy vehicles, relating to the field of non-ferrous metal die casting technology. The method includes: determining multiple filling flow paths based on the mold structure of the die casting, and determining the lower limit and upper limit of the injection speed for each filling flow path by combining the arrival time of the molten aluminum, injection operation data and venting pressure, and dynamically generating a target injection speed for injection control, thereby achieving coordination between filling capacity and venting requirements and improving the real-time performance and adaptability of ultra-low speed filling control for large aluminum die castings.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of non-ferrous metal die casting technology, specifically relating to an intelligent control method for ultra-low speed die casting of aluminum die castings for new energy vehicles. Background Technology

[0002] With the development of lightweight and structural integration in new energy vehicles, large aluminum die castings are gradually being used in the manufacture of body structural parts, battery pack housings, and shock absorber towers. Die casting technology is widely used in non-ferrous metal casting in aerospace, automobiles, and high-speed rail. Existing ultra-low speed die casting methods typically inject molten aluminum into a pressure chamber and control the injection mechanism to push the molten aluminum according to a pre-set injection speed and stroke. The molten aluminum then passes through the runner and ingate into the mold cavity. The molten aluminum solidifies under pressure through pressurization and holding. By reducing the flow rate of molten aluminum during the filling stage, the degree of tumbling, spraying, and turbulence of molten aluminum in the pressure chamber and cavity can be reduced, thus reducing the probability of gas entrapment into the molten aluminum.

[0003] However, large aluminum die-cast parts for new energy vehicles typically have multiple filling flow paths, regions with varying wall thicknesses, and long aluminum liquid flow paths. These different flow paths differ in flow distance, cross-section, flow resistance, and heat exchange conditions with the mold, causing varying degrees of temperature drop and flow resistance changes in the continuous flow of the aluminum liquid. Consequently, the aluminum liquid front in each flow path exhibits different actual propulsion velocities. Existing technologies typically control the overall filling process according to preset injection parameters. While increasing the injection speed can improve the filling capacity of thin-walled regions at the far end, it may cause some aluminum liquid fronts to be affected before the corresponding residual gas is fully utilized. When the gas is discharged, it reaches the confluence area or exhaust connection area in advance, sealing the exhaust path between the unfilled area and the exhaust outlet, causing residual gas to stagnate. Although reducing the injection speed can prolong the effective connection time of the exhaust path, it may cause the aluminum liquid at the far end to cool down significantly before reaching the end of the filling process and lose its effective filling capacity, resulting in cold shut or insufficient filling. Therefore, how to dynamically coordinate the injection speed according to the actual filling progress of each filling flow path to balance the residual gas discharge requirements before the exhaust path is closed and the filling requirements of the far thin-walled area before the aluminum liquid loses its effective flow capacity has become a technical problem that still needs to be solved in the existing ultra-low speed die casting method. Summary of the Invention

[0004] The purpose of this invention is to solve the problems mentioned above, and to propose an intelligent control method for ultra-low speed die casting of aluminum die castings for new energy vehicles.

[0005] In a first aspect of this invention, a smart control method for ultra-low speed die casting of aluminum die castings for new energy vehicles is first proposed, the method comprising: Analyze the mold structure data of the die-casting mold to determine the multiple filling flow paths formed after the aluminum liquid enters the mold cavity. Set multiple detection positions in the filling flow paths and mark the corresponding venting positions and target filling positions. Real-time acquisition of working data during the injection process, and acquisition of detection signals by sensors set at the detection position, with the trigger time of the detection signal as the arrival time of the molten aluminum; Based on the arrival time of molten aluminum between adjacent detection positions, the first flow path distance between adjacent detection positions, and working data, the filling characteristic parameters of the filling flow path are determined. Based on the filling characteristic parameters and the second flow path distance from the detection position to the target filling position, the first injection speed of the filling flow path is determined, and the maximum value of the first injection speed among multiple filling flow paths is selected as the lower limit of the injection speed. The remaining venting time is determined based on the venting pressure of the filling flow path. Combined with the filling characteristic parameters and the distance of the third flow path from the filling detection position to the venting position, the second injection speed of the filling flow path is determined. The minimum value of the second injection speed among multiple filling flow paths is selected as the upper limit of the injection speed. Based on the lower limit and upper limit of the injection velocity, a target injection velocity is generated, and injection control is performed according to the target injection velocity.

[0006] Optionally, determining the filling characteristic parameters of the filling flow path based on the arrival time of the molten aluminum between adjacent detection positions, the first flow path distance between adjacent detection positions, and working data includes: Along the direction of aluminum melt flow, adjacent detection positions in the filling flow path are sequentially recorded as the first detection position, the second detection position, and the third detection position; The filling flow path between the first detection position and the second detection position is designated as the first detection section, and the filling flow path between the second detection position and the third detection position is designated as the second detection section. Based on the arrival time of the molten aluminum in the first and second detection sections, the distance of the first flow path, and the working data, the filling characteristic parameters of the filling flow path are determined.

[0007] Optionally, the filling characteristic parameters for determining the filling flow path include: Calculate the first propulsion velocity between the first detection position and the second detection position; The injection velocity data within the first leading edge passage time is obtained from the working data, and the first average injection velocity corresponding to the first detection section is determined based on the injection velocity data. Calculate the second propulsion velocity between the second and third detection positions; The injection velocity data within the second leading edge passage time is obtained from the working data, and the second average injection velocity corresponding to the second detection section is determined based on the injection velocity data. The first average injection velocity, the first propulsion velocity, the second average injection velocity, and the second propulsion velocity are mapped to obtain the flow path response parameters. The first propulsion speed, the second propulsion speed, and the flow path response parameters are used as the filling characteristic parameters of the filling flow path.

[0008] Optionally, determining the first injection velocity of the filling flow path based on the filling characteristic parameters and the second flow path distance from the detection position to the target filling position includes: Based on the mold structure data, the length of the flow path between the third detection position and the target filling position is taken as the second flow path distance; The equivalent acceleration of the filling flow path is determined based on the first propulsion speed, the second propulsion speed, the passage time of the first leading edge, and the passage time of the second leading edge. Based on the second propulsion speed, the second leading edge passage time, and the equivalent acceleration, the current propulsion speed of the aluminum liquid is predicted, and based on the current propulsion speed, the equivalent acceleration, and the second flow path distance, the predicted remaining filling time of the aluminum liquid from the third detection position to the target filling position is predicted. Determine the baseline remaining filling time based on the current propulsion speed and the distance to the second flow path; When the predicted remaining filling time is greater than the baseline remaining filling time, the target propulsion speed is determined based on the baseline remaining filling time, the equivalent acceleration, and the second flow path distance. When the predicted remaining filling time is less than or equal to the baseline remaining filling time, the current propulsion speed is used as the target propulsion speed. The first injection velocity of the filling flow path is determined based on the target propulsion speed and flow path response parameters.

[0009] Optionally, determining the second injection velocity of the filling flow path includes: Based on the mold structure data, the length of the flow path along the filling flow path between the third detection position and the corresponding venting position is taken as the third flow path distance; The remaining venting time of the filling flow path is obtained, and the ratio between the distance of the third flow path and the remaining venting time is used as the critical propulsion speed. Based on the critical propulsion speed and flow path response parameters, the second injection speed of the corresponding filling flow path is determined.

[0010] Optionally, determining the remaining venting time based on the venting pressure of the filling flow path includes: Collect exhaust pressure data from the filling flow path; Extract the exhaust pressure value sequence from the exhaust pressure data, input the exhaust pressure value sequence into a preset vacuum exhaust model for fitting, and obtain a pressure change model; Obtain the target exhaust pressure of the filling flow path, input the target exhaust pressure into the pressure change model, calculate the time interval corresponding to the change to the target exhaust pressure, and use the time interval as the remaining exhaust time of the corresponding filling flow path.

[0011] Optionally, generating the target injection velocity based on the lower limit and upper limit of the injection velocity includes: Obtain the current injection velocity from the working data; If the current injection velocity is less than the lower limit of the injection velocity, the lower limit of the injection velocity is determined as the target injection velocity; If the current injection speed is between the lower limit and the upper limit of the injection speed, the current injection speed is determined as the target injection speed; If the current injection velocity is greater than the upper limit of the injection velocity, the upper limit of the injection velocity is determined as the target injection velocity.

[0012] Optionally, it also includes: When the lower limit of the injection speed is greater than the upper limit of the injection speed, the upper limit of the injection speed is determined as the first stage target injection speed, and injection control is performed according to the first stage target injection speed. During the injection control process, the exhaust pressure data of the filling flow path is collected in real time, and the exhaust pressure of the filling flow path is determined based on the exhaust pressure data. If the exhaust pressure meets the preset exhaust conditions, the third injection speed of the filling flow path is determined based on the working data and the filling characteristic parameters of the corresponding filling flow path. The maximum value of the third injection velocity among multiple filling flow paths is selected as the target injection velocity for the second stage, and injection control is performed according to the target injection velocity for the second stage.

[0013] The beneficial effects of this invention are: 1. This invention, by jointly analyzing the advancing trend of the aluminum melt front, the remaining filling distance, and the venting pressure and remaining venting time, determines the lower limit of the injection speed that meets the filling requirements of the far-end thin-walled region and the upper limit of the injection speed that meets the venting requirements. It unifies the filling capacity requirements and venting constraints in large non-ferrous metal castings for automobiles into speed boundaries that can be directly used for injection control, thereby improving the coordination between filling and venting under long flow paths, thin walls, and multi-branch cavity conditions.

[0014] 2. This invention compares the current injection speed with the real-time updated upper and lower limits of the injection speed and dynamically generates a target injection speed accordingly. This allows the injection control to be dynamically adjusted according to the actual advancement state and exhaust progress of each filling flow path of the large non-ferrous metal casting for automobiles. While meeting the filling requirements of the far-end area, it reduces the possibility of the aluminum liquid front reaching the exhaust position too early, thereby improving the stability of the ultra-low speed die casting process of large aluminum die castings for new energy vehicles. Attached Figure Description

[0015] The invention will now be further described with reference to the accompanying drawings.

[0016] Figure 1 A flowchart of an intelligent control method for ultra-low speed die casting of aluminum die casting parts for new energy vehicles provided in an embodiment of the present invention; Figure 2 A flowchart of another intelligent control method for ultra-low speed die casting of aluminum die casting parts for new energy vehicles provided in an embodiment of the present invention. Detailed Implementation

[0017] The technical solutions of the present invention will be clearly and completely described below with reference to the accompanying drawings of the embodiments of the present invention. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments.

[0018] It should be noted that all formula calculations in the scheme are purely numerical calculations.

[0019] Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0020] This invention provides an intelligent control method for ultra-low speed die casting of aluminum die castings for new energy vehicles. See [link to relevant documentation]. Figure 1 .

[0021] S101, analyze the mold structure data of the die-casting mold, determine the multiple filling flow paths formed after the aluminum liquid enters the mold cavity, set multiple detection positions in the filling flow paths, and mark the corresponding venting positions and target filling positions.

[0022] To ensure clarity and conciseness in the description of the following embodiments, a brief introduction to the relevant terms is given first.

[0023] Mold structure data: refers to a set of data used to describe information such as mold cavity space, gating system, venting system and core structure.

[0024] The flow path of the mold filling is the flow path formed by the aluminum liquid entering the mold cavity through the inner gate and advancing along the continuous space of the cavity to the corresponding downstream area. It is used to characterize the main advancing direction and positional connection relationship of the aluminum liquid front in the cavity.

[0025] Detection position: refers to a pre-set spatial location along the filling flow path used to detect whether the leading edge of the molten aluminum has reached the corresponding position. A sensor is set at the detection position to respond to the arrival status of the molten aluminum, and the arrival time of the molten aluminum is determined based on the detection signal generated by the sensor. Exhaust position: refers to the position in the filling flow path corresponding to the cavity exhaust groove, vacuum exhaust channel or other exhaust structure. After the aluminum liquid advances to this position, it will affect the gas communication relationship between the corresponding unfilled area and the exhaust structure. It is used to characterize the position where the exhaust path may be blocked by the aluminum liquid.

[0026] Target filling position: refers to the target position reached by the molten aluminum in the filling flow path.

[0027] In one possible implementation, mold structure data such as a three-dimensional model of the die-casting mold, gating system design data, and mold assembly data are acquired, and the cavity geometry, ingate location, main runner and sub-runner structure, cavity wall thickness distribution, reinforcing ribs and core structure, venting groove location, and vacuum venting channel location are extracted from them to generate a three-dimensional model of the cavity.

[0028] Using the connection point between the ingate and the cavity as the starting point for filling, a connectivity analysis is performed on the 3D model of the cavity. Specifically, the cavity space is divided into multiple adjacent grid cells. A cavity connectivity graph is established based on the connectivity relationships between adjacent grid cells. Using the grid cell corresponding to the ingate as the starting node, a continuous path is searched along the cavity connectivity relationships towards cavity regions with gradually increasing distance from the ingate. For branch paths formed from the same ingate to different cavity regions, the corresponding filling flow paths are determined. For cases where multiple ingates supply liquid to different regions, corresponding filling flow paths are established. For cases where different filling flow paths converge downstream, the corresponding confluence position and flow path connection relationship are recorded. Through the above processing, the 3D model of the cavity used for automotive non-ferrous metal die casting is converted into an equivalent flow path determined based on the cavity space connectivity relationships, and the equivalent flow path is used as the filling flow path for molten aluminum in the cavity of automotive non-ferrous metal castings.

[0029] After determining the filling flow path, at least three detection positions are set along the aluminum liquid flow direction on each flow path, based on the length of each flow path and the cavity structure. Detection positions are preferentially set at locations where the cavity cross-section changes, flow path turning points, transitions between thick-walled and thin-walled regions, before and after reinforcing rib areas, and in the middle of long flow paths. Adjacent detection positions should be continuous and not located in cavity sections with major branching or confluence structures. For filling flow paths with long flow paths or multiple significant structural change areas, additional detection positions can be added beyond the three. For multiple filling flow paths sharing a common upstream region, detection positions within the common flow region can be shared by different flow paths, with subsequent detection positions set after each flow path branches. The position of each detection position in the mold is recorded, and each detection position is associated with its corresponding filling flow path. It should be noted that the above-mentioned detection position settings can be configured by those skilled in the art according to actual applications and are not limited here.

[0030] In the 3D model of the mold cavity, identify the areas where the cavity connects to the venting groove or vacuum venting channel. Determine the venting connection positions as the aluminum liquid advances downstream along each filling flow path, and mark these venting connection positions as the venting positions of the corresponding filling flow paths. When different filling flow paths correspond to different venting channels, mark the venting positions separately; when multiple filling flow paths correspond to the same venting channel, record the connection positions of each filling flow path to the venting channel.

[0031] The target filling position for each filling flow path is determined based on the 3D model of the cavity. The target filling position can be selected from the far end of the corresponding filling flow path, the end of the thin-walled area, the end of the reinforcing rib, the confluence area, or the final filling area determined based on the mold design data and trial molding data. The position of the target filling position in the mold is recorded.

[0032] After completing the above processing, the correspondence between the filling flow path, detection position, venting position, and target filling position is generated using the filling flow path identifier, and the order of each position along the filling flow path is recorded. For the flow path distance between each position, the equivalent center path of the corresponding filling flow path can be extracted based on the 3D model of the cavity, and the path length can be calculated along the equivalent center path; alternatively, continuous mesh paths between corresponding positions can be searched in the cavity connectivity graph and the path lengths can be accumulated.

[0033] S102 collects working data in real time during the injection process and obtains detection signals through sensors set at the detection position, using the trigger time of the detection signal as the arrival time of the molten aluminum.

[0034] To ensure clarity and conciseness in the description of the following embodiments, a brief introduction to the relevant terms is given first.

[0035] Working data: refers to the data collected in real time during the injection process to characterize the operating status of the injection mechanism, including process parameters such as actual injection speed, injection position, injection stroke, injection pressure, and corresponding sampling time.

[0036] In one implementation method, the working data of the injection mechanism is acquired in real time. The working data includes the actual injection speed and injection position of the injection plunger, as well as the corresponding sampling time. It may also include existing process data from the die-casting machine's operation, such as injection stroke and injection pressure. This data can be directly read from the die-casting machine's injection controller, displacement detection device, and pressure detection device, and the actual injection speed, injection position, and other working parameters corresponding to each sampling time are combined to form the working data.

[0037] Simultaneously, sensors positioned at each detection location acquire the corresponding detection signal. The sensors employ detection elements capable of responding to local physical state changes that occur when the molten aluminum front reaches the detection location. Pressure sensors can be used; when the molten aluminum front has not yet reached the detection location, the sensor's detection value is in the corresponding background state; when the molten aluminum front reaches the detection location and contacts the corresponding cavity wall or measuring component, the local cavity pressure changes, and the pressure sensor converts this pressure change into an electrical signal, generating the corresponding detection signal.

[0038] In one embodiment, temperature, conductivity, or other sensors capable of distinguishing the state of the molten aluminum before and after its arrival can also be used. For example, after the molten aluminum reaches the detection position, it causes changes in local temperature, conductivity, or other detectable physical quantities, which are then converted into electrical signals by a corresponding sensor. It should be noted that those skilled in the art can select sensors according to the actual application, and no limitation is made here.

[0039] Next, when a sensor located at any detection position generates a detection signal, the corresponding detection position is determined based on the sensor's acquisition channel that generated the signal. Specifically, a correspondence between sensor acquisition channels and detection positions is pre-established, and each detection position is configured with a unique location identifier. When a certain acquisition channel generates a detection signal, the corresponding location identifier is queried based on that acquisition channel to determine the detection position corresponding to this detection signal.

[0040] Working data and data acquisition from each sensor channel are recorded using a unified time base. At the start of the current injection cycle, a unified injection cycle start time is established, and working data and various detection signals are recorded according to the same system clock. When a detection signal is detected, the corresponding trigger timestamp is read and used as the arrival time of the molten aluminum front at the corresponding detection position.

[0041] S103, based on the arrival time of the molten aluminum between adjacent detection positions, the distance of the first flow path, and the working data, determine the filling characteristic parameters of the filling flow path.

[0042] To ensure clarity and conciseness in the description of the following embodiments, a brief introduction to the relevant terms is given first.

[0043] First flow path distance: refers to the length of the flow path between adjacent detection positions in the filling flow path, determined along the actual direction of aluminum liquid propulsion. It is used to characterize the flow distance that the leading edge of the aluminum liquid needs to travel in the corresponding detection section.

[0044] Filling characteristic parameters: refers to the set of parameters used to characterize the advancing state of the aluminum liquid front in the filling flow path and the response relationship between the injection speed and the advancing speed of the aluminum liquid front.

[0045] In one implementation, after obtaining the arrival time of the molten aluminum at at least three detection positions in the filling flow path and the working data during the injection process, three consecutive adjacent detection positions are selected from the same filling flow path according to the flow direction of the molten aluminum in the filling flow path, and are sequentially recorded as the first detection position, the second detection position, and the third detection position. The filling flow path between the first detection position and the second detection position is designated as the first detection section, and the filling flow path between the second detection position and the third detection position is designated as the second detection section. For filling flow paths with more than three detection positions, after a detection signal is generated at a new downstream detection position, the detection position and its two upstream adjacent detection positions can be selected to re-divide the two detection sections, so that the subsequently determined filling characteristic parameters can correspond to the flow path region currently traversed by the leading edge of the molten aluminum.

[0046] Based on the arrival times of the molten aluminum recorded in S102, the arrival times of the molten aluminum front at the first, second, and third detection positions are obtained respectively. The difference between the arrival times of the molten aluminum at the second and first detection positions is taken as the first front passage time, and the difference between the arrival times of the molten aluminum at the third and second detection positions is taken as the second front passage time. Thus, the actual time consumed by the molten aluminum front in the two consecutive detection sections before and after its passage can be obtained.

[0047] In one implementation, the equivalent center path of the corresponding filling flow path is extracted from the three-dimensional model of the cavity. Specifically, the center of the cross-section of the continuous cavity region corresponding to the filling flow path can be extracted, and the center points of the cross-sections obtained continuously along the aluminum liquid propulsion direction can be connected sequentially to form an equivalent center line. The first detection position, the second detection position, and the third detection position are then projected onto this equivalent center line. The lengths of the curved paths between the first detection position and the second detection position, and between the second detection position and the third detection position, are calculated along the equivalent center line to obtain the distance between the first segment and the second segment.

[0048] The first propulsion speed for the first detection segment is obtained by dividing the distance of the first section by the time it takes for the first leading edge to pass through; similarly, the second propulsion speed for the second detection segment is obtained by dividing the distance of the second section by the time it takes for the aluminum liquid leading edge to pass through the second leading edge. The calculation principle is based on determining the average propulsion speed of the corresponding segment using the actual time required for the aluminum liquid leading edge to traverse a known flow path distance. Therefore, the obtained propulsion speed reflects the actual motion state of the aluminum liquid leading edge in the actual cavity, rather than the theoretical flow rate directly calculated from the injection plunger speed. By comparing the propulsion speeds of the two detection segments, the change in the propulsion capability of the aluminum liquid leading edge after passing through the current flow path region can be further reflected.

[0049] Furthermore, based on the passage times of the first and second leading edges, injection velocity data within corresponding time ranges are extracted from the working data obtained in S102. Specifically, the injection velocity data within the time range corresponding to the first and second detection positions is used as the injection velocity data for the first detection segment, and the injection velocity data within the time range corresponding to the second and third detection positions is used as the injection velocity data for the second detection segment. Since the working data and detection signals are recorded using a unified time reference, the actual injection velocity data can be time-matched according to the arrival time of the molten aluminum.

[0050] For the first detection section, the average of multiple injection velocity values ​​collected within the first leading edge's passage time is calculated to obtain the first average injection velocity. For the second detection section, the average of multiple injection velocity values ​​collected within the second leading edge's passage time is calculated to obtain the second average injection velocity. The reason for using averaging is that the plunger velocity may fluctuate within a small range during the actual injection process, and the velocity value at a single sampling moment cannot stably represent the actual injection state within the entire detection section. By averaging multiple velocity sampling values ​​within the corresponding time range, the injection velocity corresponding to the passage process of the aluminum molten front in that section can be obtained.

[0051] This establishes a correspondence between the first average injection speed and the first propulsion speed in the first detection section, and a correspondence between the second average injection speed and the second propulsion speed in the second detection section. The former reflects the actual average speed of the injection mechanism in the first detection section and the actual propulsion response generated by the aluminum liquid front, while the latter reflects the actual average speed of the injection mechanism in the second detection section and the corresponding aluminum liquid front propulsion response. By correlating the actual input state of the injection mechanism with the actual movement state of the aluminum liquid front within the same time range, the deviation caused by evaluating the filling state solely based on the equipment's set injection speed can be reduced.

[0052] In one possible implementation, the injection velocity of the injection plunger is used as the input, and the propulsion velocity of the aluminum liquid front within the same time interval is used as the output, to establish a local proportional response relationship between the injection velocity and the propulsion velocity of the aluminum liquid front: ,in, Indicates the propulsion speed of the leading edge of the molten aluminum; This indicates the injection velocity of the injection plunger; This represents the flow path response parameters corresponding to the filling flow path. Since the aluminum melt front advance velocity and the injection plunger velocity use the same velocity dimension, the flow path response parameters... It is a dimensionless parameter.

[0053] Substituting the obtained first average injection velocity and first propulsion velocity, as well as the second average injection velocity and second propulsion velocity, into the above response relationship, the predicted propulsion velocities corresponding to the first and second detection sections are obtained, respectively. The flow path response parameters are determined using the least squares method, i.e., the following is established:

[0054] in, This represents the sum of squared prediction errors. Indicates the first propulsion speed; Indicates the second propulsion speed; Indicates the first average injection velocity; This indicates the second average injection velocity.

[0055] By minimizing the sum of squared prediction errors, the flow path response parameters can be obtained: Substituting the actual first average injection velocity and the actual measured first propulsion velocity in the first detection section, and the actual second average injection velocity and the actual measured second propulsion velocity in the second detection section into the above formula, the flow path response parameters of the current filling flow path can be calculated. The flow path response parameters represent the equivalent response degree of the motion of the injection plunger converted into the propulsion motion of the aluminum liquid front in the current filling stage.

[0056] Because the actual injection velocity of the plunger is not directly equivalent to the advance velocity of the molten aluminum front in a specific filling flow path, different filling flow paths for large automotive aluminum die castings have different flow cross-sections, turning structures, and flow resistances. The same injection velocity applied to different filling flow paths may produce different front-edge advance responses. Therefore, by identifying the flow path response parameters online using two sets of actual injection velocities and actual advance velocities, the aforementioned combined flow effects can be reflected in the flow path response parameters.

[0057] After determining the flow path response parameters, the first propulsion speed, the second propulsion speed, and the flow path response parameters are collectively used as the filling characteristic parameters of the current filling flow path. The first and second propulsion speeds reflect the actual propulsion state and changing trend of the aluminum liquid front in two consecutive detection sections, while the flow path response parameters reflect the actual response relationship between the current injection speed and the corresponding frontal propulsion speed of the filling flow path. Subsequently, after determining the target propulsion speed required for the aluminum liquid, the corresponding injection speed can be calculated in reverse based on the aforementioned flow path response relationship, providing a computational basis for determining the actual required injection speed for different filling flow paths.

[0058] S104. Based on the filling characteristic parameters and the second flow path distance from the detection position to the target filling position, determine the first injection speed of the filling flow path, and select the maximum value of the first injection speed among multiple filling flow paths as the lower limit of the injection speed.

[0059] To ensure clarity and conciseness in the description of the following embodiments, a brief introduction to the relevant terms is given first.

[0060] Second flow path distance: refers to the length of the flow path determined by the filling flow path between the current detection position used for filling status judgment and the corresponding target filling position. It is used to characterize the remaining flow distance required for the aluminum liquid front to continue advancing to the target filling position.

[0061] First injection speed: refers to the injection speed determined based on the current filling characteristic parameters of the filling flow path and the distance between the second flow path, which is used to meet the subsequent filling requirements of the corresponding filling flow path, and serves as a candidate speed for determining the lower limit of the injection speed.

[0062] In one possible implementation, after obtaining the first propulsion speed, the second propulsion speed, the first leading edge passage time, the second leading edge passage time, and the flow path response parameters corresponding to the current filling flow path, the equivalent center line along the filling flow path between the third detection position and the corresponding target filling position is obtained according to the cavity three-dimensional model through the processing method of S103 described above, and the path length of the equivalent center line is used as the second flow path distance.

[0063] To determine whether the propulsion capacity of the molten aluminum front decreases after passing through the two detection sections, the local equivalent acceleration of the current filling flow path is determined based on the first and second propulsion velocities. Considering that the first and second propulsion velocities are the average velocities of the molten aluminum front as it passes through the two detection sections, under short-time equivalent uniform acceleration conditions, the average velocities can be equivalent to the instantaneous velocities at the midpoint of the corresponding sections. Therefore, the time interval between the two average velocities is half the sum of the durations of the first and second propulsion fronts. Based on this, the equivalent acceleration can be determined using the following formula:

[0064] in, This represents the equivalent acceleration of the filling flow path. Indicates the duration of passage of the first frontier; This indicates the duration of the second frontier.

[0065] Equivalent acceleration is a short-term equivalent motion parameter generated during the current local filling stage based on the actual advancing speed of two consecutive detection sections. It is mainly used to represent the changing trend of the advancing speed of the molten aluminum front. When the equivalent acceleration is less than zero, it indicates that the molten aluminum front generally decelerates after passing through the current two detection sections; when the equivalent acceleration is close to zero, it indicates that the molten aluminum front basically maintains its current advancing state; when the equivalent acceleration is greater than zero, it indicates that the molten aluminum front generally accelerates.

[0066] Since the second propulsion velocity is the average propulsion velocity over the entire segment from the second detection position to the third detection position, rather than the propulsion velocity of the aluminum liquid front at the instant it reaches the third detection position, the current propulsion velocity of the aluminum liquid front when it reaches the third detection position is further estimated using the second propulsion velocity, the duration of the second front's passage, and the equivalent acceleration. Based on the relationship between the average velocity of a segment and the velocity at the midpoint of the segment in uniformly accelerated motion, it can be expressed as: ,in, This indicates the current propulsion speed of the molten aluminum when it reaches the third detection position.

[0067] Next, taking the third detection position as the current prediction starting point, and maintaining the above equivalent advancement trend for a short period of time, the time required for the aluminum liquid front to advance from the third detection position to the target filling position is predicted based on the current advancement speed, equivalent acceleration, and second flow path distance. This is the prediction of the remaining filling time, obtained according to the displacement relationship: ,in, Indicates the distance of the second flow path; This represents the predicted remaining filling time. The predicted remaining filling time is obtained through the above method.

[0068] Using the above method, the forward propulsion state of the aluminum liquid front, which has already been detected before the third detection position, can be used to predict the continuation of the short-distance filling process after the third detection position. The first and second propulsion velocities reflect the actual movement changes of the aluminum liquid front within two consecutive detection sections. The equivalent acceleration obtained from these two velocities can characterize whether the aluminum liquid front in the current flow path maintains its propulsion, accelerates its propulsion, or gradually decays. Therefore, by using the current propulsion velocity predicted at the third detection position as the initial state, and continuing this equivalent propulsion trend for a short period in the remaining filling section, the time required for the aluminum liquid front to reach the target filling position according to the current movement trend can be deduced by combining the second flow path distance from the third detection position to the target filling position.

[0069] Furthermore, the baseline remaining filling time is determined by using the current advance speed of the molten aluminum front when it reaches the third detection position as a reference. Specifically, assuming that the molten aluminum front can maintain its current advance speed within the subsequent second flow path distance, the ratio between the second flow path distance and the current advance speed is used as the baseline remaining filling time.

[0070] When the predicted remaining filling time is less than or equal to the baseline remaining filling time, it means that continuing to move according to the current propulsion trend will not further extend the time to reach the target filling position relative to the current constant speed state. In this case, there is no need to increase the propulsion speed for the far-end filling, so the current propulsion speed is directly used as the target propulsion speed.

[0071] When the predicted remaining filling time is greater than the baseline remaining filling time, it indicates a significant attenuation trend in the current filling flow path. Continuing to advance according to the current motion state will further prolong the time required for the molten aluminum to reach the target filling position. In this case, the baseline remaining filling time is used as the expected completion time, and the advance speed required for the molten aluminum front to travel the distance of the second flow path within the baseline remaining filling time, while maintaining the current equivalent acceleration, is calculated in reverse; this is the target advance speed. The target propulsion speed can be obtained from the above formula, where, Indicates the target's speed of movement; This indicates the remaining filling time.

[0072] Finally, based on the flow path response parameters obtained from the aforementioned embodiments, the target feed speed is converted into an injection speed that the die-casting machine can execute. The first injection speed corresponding to the filling flow path can be expressed as: ,in, This indicates the first injection velocity corresponding to the filling flow path.

[0073] Therefore, when a long flow path or a thin-walled flow path at the far end has shown obvious decline in the leading edge, the corresponding first injection speed can be increased according to its actual decline and the remaining flow path distance; while for a filling flow path with normal leading edge advance, the injection speed corresponding to the current advance state is maintained.

[0074] The first injection velocity of multiple filling flow paths is obtained in the above manner. The first injection velocities of multiple filling flow paths are compared and the maximum value is taken as the lower limit of the injection velocity.

[0075] This embodiment, through the above implementation method, can determine the leading edge advancement state and its changing trend of each filling flow path online based on the arrival time of the aluminum liquid and the injection operation data obtained in real time during the current injection cycle, and calculate the corresponding first injection speed in a timely manner in combination with the remaining flow path distance, so that the lower limit of the injection speed can be dynamically updated with the actual filling state, thereby improving the real-time performance and adaptability of multi-flow path filling control for large automotive aluminum die castings.

[0076] S105, determine the remaining venting time based on the venting pressure of the filling flow path, and determine the second injection speed of the filling flow path by combining the filling characteristic parameters and the distance of the third flow path from the filling detection position to the venting position. Select the minimum value of the second injection speed among multiple filling flow paths as the upper limit of the injection speed.

[0077] To ensure clarity and conciseness in the description of the following embodiments, a brief introduction to the relevant terms is given first.

[0078] Remaining venting time: refers to the estimated time required for the venting pressure of the corresponding filling flow path to change from the current value to the target venting pressure under the current venting state.

[0079] The third flow path distance refers to the length of the flow path determined along the filling flow path between the current detection position used to determine the filling status and the corresponding exhaust position. It is used to characterize the remaining flow distance that the aluminum liquid front needs to travel to continue advancing to the exhaust position.

[0080] Second injection speed: determined based on the remaining venting time of the filling flow path, the distance of the third flow path, and the flow path response parameters, it is the critical injection speed used to advance the aluminum liquid front towards the venting position under the condition of meeting the current venting time requirement, and serves as a candidate speed for determining the upper limit of the injection speed.

[0081] In one implementation, based on the correspondence between the filling flow path and the exhaust position determined in S101, the exhaust groove, vacuum exhaust channel, or vacuum branch connected to the exhaust position of each filling flow path is determined, and the exhaust channel is used as the exhaust pressure detection object for the corresponding filling flow path. After vacuum exhaust is started, the exhaust pressure data is collected in real time by a pressure sensor installed in the exhaust channel or vacuum branch, and the sampling time corresponding to each exhaust pressure value is recorded to form an exhaust pressure value sequence for the corresponding filling flow path.

[0082] In this embodiment, the preset vacuum exhaust model adopts the exponential pressure decay model during the vacuum system evacuation process: ,in, Indicates time The corresponding exhaust pressure; Indicates the start time of the fitted time period The corresponding exhaust pressure; It represents the equivalent steady pressure that the exhaust pressure approaches when the current pumping capacity and gas inflow conditions remain unchanged. This represents the pressure decay parameter, used to characterize the rate at which the current exhaust pressure decreases.

[0083] The exhaust pressure value sequence is input into a preset vacuum exhaust model for fitting to determine the corresponding... and Thus, a pressure change model corresponding to the current exhaust process is obtained.

[0084] The target venting pressure is obtained from the vacuum die-casting process parameters corresponding to the product to be die-cast. It should be noted that the target venting pressure is a process parameter pre-determined for the specific product to be die-cast and the die-casting mold during the non-ferrous metal casting process. During the mold trial and process development stages, multiple sets of trial molds are conducted by adjusting the vacuum venting conditions. Based on the quality test results of the trial castings, such as porosity, airtightness, or mechanical properties, the venting pressure that can meet the quality requirements of the castings and that the vacuum system can stably achieve is determined.

[0085] Starting from the current exhaust pressure, the target exhaust pressure is substituted into the fitted pressure change model to solve for the time interval corresponding to the current exhaust pressure dropping to the target exhaust pressure, and this time interval is used as the remaining exhaust time of the corresponding filling flow path.

[0086] In one possible implementation, after obtaining the flow path response parameters of the current filling flow path and the corresponding remaining venting time, the equivalent center line along the filling flow path between the third detection position and the corresponding venting position is obtained from the three-dimensional model of the cavity through the processing method of S103 described above, and the path length of the equivalent center line is used as the third flow path distance.

[0087] To ensure that the leading edge of the molten aluminum has a propulsion time that matches the remaining venting time before reaching the corresponding venting position, the ratio between the third flow path distance and the remaining venting time is used as the critical propulsion speed. This ratio reflects the speed at which the leading edge of the molten aluminum advances to the venting position within the remaining venting time.

[0088] Based on the aforementioned determined flow path response parameters, the critical feed rate is converted into an injection rate that the die-casting machine can execute, i.e., the second injection rate: ,in, This indicates the second injection velocity corresponding to the filling flow path. Indicates the distance of the third flow path. This indicates the remaining venting time for the corresponding filling flow path.

[0089] When the remaining venting time of the corresponding filling flow path is zero, it means that the venting pressure at the venting position has reached the target venting pressure. At this time, the filling flow path will no longer perform the above steps and calculate the second injection speed.

[0090] After calculating the second injection velocity corresponding to multiple filling flow paths in the above manner, the smallest second injection velocity is selected as the current upper limit of the injection velocity, so that the injection velocity can meet the exhaust constraints in the current multiple filling flow paths, reducing the possibility that some aluminum liquid front reaches the exhaust position in advance before the corresponding residual gas is fully discharged and affects the connection of the exhaust passage.

[0091] This embodiment correlates the remaining flow distance of the molten aluminum front from the corresponding venting position with the remaining venting time required for the current venting pressure to reach the target venting pressure. This yields the critical propulsion speed allowed for each filling flow path under the current venting state, which is then converted into a corresponding second injection speed based on flow path response parameters. Consequently, the upper limit of the injection speed can dynamically change with the actual position of the molten aluminum front and the venting progress. By selecting the smallest second injection speed among multiple filling flow paths, the overall injection process satisfies the current venting constraints, reducing the possibility of the molten aluminum front reaching the venting position prematurely and affecting the effective connectivity of the venting passage.

[0092] S106 generates a target injection velocity based on the lower limit and upper limit of the injection velocity, and performs injection control according to the target injection velocity.

[0093] In one possible implementation, after obtaining the lower limit and upper limit of the injection speed according to the aforementioned processing, when the lower limit of the injection speed is less than or equal to the upper limit of the injection speed, a target injection speed is determined based on the current actual operating state of the die-casting machine, and the injection mechanism is controlled according to the target injection speed. The lower limit of the injection speed is used to ensure the subsequent filling requirements in the current multiple filling flow paths, and the upper limit of the injection speed is used to meet the venting time constraints in the current multiple filling flow paths. The two together form the allowable injection speed range for the current injection stage.

[0094] Specifically, the current injection speed is obtained from the real-time collected working data. The current injection speed can be directly taken from the actual injection speed feedback value output by the die-casting machine controller.

[0095] The current injection speed is compared with both the lower and upper limits of the injection speed. If the current injection speed is less than the lower limit, it means that if the current injection speed continues, at least one filling flow path's leading edge cannot meet its current subsequent filling requirements. Therefore, the lower limit of the injection speed is set as the target injection speed, causing the injection mechanism to increase the injection speed to the minimum speed required for the current filling state.

[0096] If the current injection speed is between the lower limit and the upper limit of the injection speed, it means that the current injection speed meets the filling speed requirements of each filling flow path and does not exceed the upper limit of the speed allowed by the current venting state. At this time, there is no need to make additional adjustments to the injection speed. The current injection speed is directly determined as the target injection speed to maintain the current injection state and avoid unnecessary speed changes while meeting the filling and venting requirements.

[0097] If the current injection speed is greater than the upper limit of the injection speed, it means that if the injection continues at the current speed, at least one of the aluminum liquid fronts of the filling flow path may reach the venting position prematurely before the corresponding venting pressure reaches the target venting pressure. Therefore, the upper limit of the injection speed is set as the target injection speed, so that the injection mechanism reduces the injection speed to the range allowed by the current venting constraint.

[0098] After determining the target injection speed, it is sent to the injection controller of the die-casting machine as the speed setpoint for the current injection stage. The injection controller can employ a closed-loop speed control method. Based on the deviation between the actual speed feedback value of the injection plunger and the target injection speed, it controls the servo valve, proportional flow valve, or servo hydraulic drive mechanism to adjust the hydraulic flow entering the injection cylinder, thereby adjusting the injection speed of the injection plunger towards the target injection speed. Once the injection speed reaches the target injection speed, the controller continues to perform closed-loop adjustment of the injection mechanism based on real-time speed feedback to maintain the injection speed following the target injection speed.

[0099] As the injection process continues, with the aluminum melt front reaching a new detection position and the vacuum exhaust pressure continuously changing, the arrival time of the aluminum melt, working data, and exhaust pressure data can be re-acquired using the aforementioned method. The filling characteristic parameters, remaining exhaust time, lower limit of injection speed, and upper limit of injection speed for each filling flow path can then be updated. The updated upper and lower limits of injection speed are then compared with the current injection speed to redetermine the target injection speed, allowing it to be dynamically adjusted according to the current filling progress and exhaust status.

[0100] In one possible implementation, when the lower limit of the injection speed is greater than the upper limit of the injection speed, it indicates that the minimum injection speed corresponding to the current filling requirement has exceeded the maximum injection speed allowed under venting conditions, and there is currently no injection speed range that simultaneously satisfies both requirements. In this case, the current venting requirement is prioritized, the upper limit of the injection speed is determined as the first-stage target injection speed, and injection is performed according to the first-stage target injection speed, allowing the aluminum melt front to continue advancing while providing time for residual gas to be discharged.

[0101] During the first stage of injection, pressure data of the exhaust channels connected to the corresponding exhaust positions of each filling flow path are continuously collected, and the current exhaust pressure is obtained in the manner described above. When the corresponding exhaust pressure reaches the target exhaust pressure of the filling flow path, it is determined that the filling flow path meets the preset exhaust conditions, indicating that the current exhaust requirements have been completed, and it is no longer necessary to use the remaining exhaust time to impose an upper limit constraint on the injection speed of the filling flow path.

[0102] Once the exhaust conditions are met, the injection speed, injection position, and corresponding sampling time are obtained based on the current working data. Combined with the previously determined flow path response parameters and equivalent acceleration, the current propulsion state of the corresponding filling flow path is re-evaluated.

[0103] Specifically, the equivalent advance speed of the current aluminum liquid front can be determined based on the current actual injection speed and flow path response parameters. Combined with the current remaining filling distance and the remaining filling time prediction method in S104, the target advance speed that meets the subsequent filling requirements of the filling flow path is re-determined. Then, the target advance speed is converted into the injection speed on the die-casting machine side using the flow path response parameters, and this injection speed is used as the third injection speed for the corresponding filling flow path. Therefore, the third injection speed is re-determined based on the actual operating state after the first stage of low-speed injection, rather than directly using the lower limit of the injection speed calculated before the start of the first stage.

[0104] The third injection velocity corresponding to each of the multiple filling flow paths that still need to be filled is determined according to the above method, and the maximum value among them is selected as the target injection velocity for the second stage. Since the maximum third injection velocity corresponds to the flow path with the highest requirement for subsequent filling capacity among the current multiple filling flow paths, using this velocity as the target injection velocity for the second stage can prioritize meeting the subsequent filling needs of long flow paths or thin-walled areas at the far end.

[0105] The second-stage target injection speed is sent to the die-casting machine injection controller, and the speed is adjusted in a closed loop through a servo valve, proportional flow valve or servo hydraulic mechanism to switch the injection speed from the first-stage target injection speed to the second-stage target injection speed, and continue to complete the subsequent filling.

[0106] This invention divides the complex cavity of large aluminum die-casting parts used in automobile and other non-ferrous metal castings into multiple filling flow paths with clearly defined detection, venting, and target filling positions. It utilizes the arrival time of the molten aluminum and injection operation data during the current injection cycle to obtain the actual leading edge advancement state and flow path response relationship of each filling flow path online. Based on this, on the one hand, a lower limit of the injection speed to meet subsequent filling requirements is determined according to the advancing trend of the molten aluminum front and the remaining filling distance; on the other hand, an upper limit of the injection speed is determined by combining the actual venting pressure, remaining venting time, and the remaining flow path distance to the venting position. This unifies the requirements for remote filling and venting path maintenance into speed constraints executable by the die-casting machine. The target injection speed is dynamically adjusted according to the real-time updated upper and lower limits, enabling injection control to adapt to changes in the actual filling progress and venting state of multiple filling flow paths, thus improving the real-time performance and adaptability of ultra-low speed filling control for large non-ferrous metal castings such as those for new energy vehicles.

[0107] The foregoing has described one embodiment of the present invention in detail, but this content is merely a preferred embodiment and should not be considered as limiting the scope of the present invention. All equivalent variations and modifications made within the scope of the claims of this invention should still fall within the scope of the claims of this invention.

Claims

1. An intelligent control method for ultra-low speed die casting of aluminum die castings for new energy vehicles, characterized in that, The method includes: Analyze the mold structure data of the die-casting mold to determine the multiple filling flow paths formed after the aluminum liquid enters the mold cavity. Set multiple detection positions in the filling flow paths and mark the corresponding venting positions and target filling positions. Real-time acquisition of working data during the injection process, and acquisition of detection signals by sensors set at the detection position, with the trigger time of the detection signal as the arrival time of the molten aluminum; Based on the arrival time of molten aluminum between adjacent detection positions, the first flow path distance between adjacent detection positions, and working data, the filling characteristic parameters of the filling flow path are determined. Based on the filling characteristic parameters and the second flow path distance from the detection position to the target filling position, the first injection speed of the filling flow path is determined, and the maximum value of the first injection speed among multiple filling flow paths is selected as the lower limit of the injection speed. The remaining venting time is determined based on the venting pressure of the filling flow path. Combined with the filling characteristic parameters and the distance of the third flow path from the filling detection position to the venting position, the second injection speed of the filling flow path is determined. The minimum value of the second injection speed among multiple filling flow paths is selected as the upper limit of the injection speed. Based on the lower limit and upper limit of the injection velocity, a target injection velocity is generated, and injection control is performed according to the target injection velocity.

2. The method according to claim 1, characterized in that, The process of determining the filling characteristic parameters of the filling flow path based on the arrival time of the molten aluminum between adjacent detection positions, the first flow path distance between adjacent detection positions, and working data includes: Along the direction of aluminum melt flow, adjacent detection positions in the filling flow path are sequentially recorded as the first detection position, the second detection position, and the third detection position; Based on the arrival times of the molten aluminum at the first, second, and third detection positions, the first flow path distance between adjacent detection positions, and the working data, the filling characteristic parameters of the filling flow path are determined.

3. The method according to claim 2, characterized in that, The filling characteristic parameters for determining the filling flow path include: Calculate the first propulsion velocity between the first detection position and the second detection position; The injection velocity data within the first leading edge passage time is obtained from the working data, and the first average injection velocity corresponding to the first detection section is determined based on the injection velocity data. Calculate the second propulsion velocity between the second and third detection positions; The injection velocity data within the second leading edge passage time is obtained from the working data, and the second average injection velocity corresponding to the second detection section is determined based on the injection velocity data. The first average injection velocity, the first propulsion velocity, the second average injection velocity, and the second propulsion velocity are mapped to obtain the flow path response parameters. The first propulsion speed, the second propulsion speed, and the flow path response parameters are used as the filling characteristic parameters of the filling flow path.

4. The method according to claim 3, characterized in that, The step of determining the first injection velocity of the filling flow path based on the filling characteristic parameters and the second flow path distance from the detection position to the target filling position includes: Based on the mold structure data, the length of the flow path between the third detection position and the target filling position is taken as the second flow path distance; The equivalent acceleration of the filling flow path is determined based on the first propulsion speed, the second propulsion speed, the passage time of the first leading edge, and the passage time of the second leading edge. Based on the second propulsion speed, the second leading edge passage time, and the equivalent acceleration, the current propulsion speed of the aluminum liquid is predicted, and based on the current propulsion speed, the equivalent acceleration, and the second flow path distance, the predicted remaining filling time of the aluminum liquid from the third detection position to the target filling position is predicted. Determine the baseline remaining filling time based on the current propulsion speed and the distance to the second flow path; When the predicted remaining filling time is greater than the baseline remaining filling time, the target propulsion speed is determined based on the baseline remaining filling time, the equivalent acceleration, and the second flow path distance. When the predicted remaining filling time is less than or equal to the baseline remaining filling time, the current propulsion speed is used as the target propulsion speed. The first injection velocity of the filling flow path is determined based on the target propulsion speed and flow path response parameters.

5. The method according to claim 4, characterized in that, The second injection velocity for determining the filling flow path includes: Based on the mold structure data, the length of the flow path along the filling flow path between the third detection position and the corresponding venting position is taken as the third flow path distance; The remaining venting time of the filling flow path is obtained, and the ratio between the distance of the third flow path and the remaining venting time is used as the critical propulsion speed. Based on the critical propulsion speed and flow path response parameters, the second injection speed of the corresponding filling flow path is determined.

6. The method according to claim 1, characterized in that, Determining the remaining venting time based on the venting pressure of the filling flow path includes: Collect exhaust pressure data from the filling flow path; Extract the exhaust pressure value sequence from the exhaust pressure data, input the exhaust pressure value sequence into a preset vacuum exhaust model for fitting, and obtain a pressure change model; Obtain the target exhaust pressure of the filling flow path, input the target exhaust pressure into the pressure change model, calculate the time interval corresponding to the change to the target exhaust pressure, and use the time interval as the remaining exhaust time of the corresponding filling flow path.

7. The method according to claim 1, characterized in that, The generation of target recoil velocity based on the lower limit and upper limit of recoil velocity includes: Obtain the current injection velocity from the working data; If the current injection velocity is less than the lower limit of the injection velocity, the lower limit of the injection velocity is determined as the target injection velocity; If the current injection speed is between the lower limit and the upper limit of the injection speed, the current injection speed is determined as the target injection speed; If the current injection velocity is greater than the upper limit of the injection velocity, the upper limit of the injection velocity is determined as the target injection velocity.

8. The method according to claim 7, characterized in that, Also includes: When the lower limit of the injection speed is greater than the upper limit of the injection speed, the upper limit of the injection speed is determined as the first stage target injection speed, and injection control is performed according to the first stage target injection speed. During the injection control process, the exhaust pressure data of the filling flow path is collected in real time, and the exhaust pressure of the filling flow path is determined based on the exhaust pressure data. If the exhaust pressure meets the preset exhaust conditions, the third injection speed of the filling flow path is determined based on the working data and the filling characteristic parameters of the corresponding filling flow path. The maximum value of the third injection velocity among multiple filling flow paths is selected as the target injection velocity for the second stage, and injection control is performed according to the target injection velocity for the second stage.