An automatic feeding steel pipe pole welding equipment
By using Curie temperature-triggered ferromagnetic micro/nanoparticle strips during the welding process, staged control of the molten pool and heat-affected zone was achieved, solving the problems of single control and sensor dependence in existing magnetron welding technology, and improving welding quality and energy utilization.
Patent Information
- Application Number
- CN202611410434.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-11
- Publication Date
- 2026-11-17
AI Technical Summary
Existing magnetron welding technology cannot control the liquid metal in the molten pool and the solid heat-affected zone in stages. It relies on external sensors, which have measurement errors and control delays. The magnetic field energy coverage is uneven and lacks targeting. Furthermore, it does not introduce exogenous functional materials with customized Curie temperatures.
The particle strip is formed by mixing ferromagnetic micro/nano particles with a predetermined Curie temperature with a high-temperature resistant inorganic binder. The magnetic field generator automatically switches the working mode during the welding process. The magnetic property mutation of the particle material is used to control the molten pool and heat-affected zone at different temperature stages, including electromagnetic stirring and magnetostrictive vibration.
It achieves grain refinement of the molten pool, reduction of segregation, and elimination of residual tensile stress during the welding process, thereby improving welding quality and energy utilization, avoiding delays and errors of external sensors, and ensuring that magnetic field energy is targeted to weak points.
Smart Images

Figure CN123103259A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of steel pipe pole welding technology, and specifically to an automatic feeding steel pipe pole welding equipment. Background Technology
[0002] Steel pipe poles are widely used in power transmission towers, building steel structures, petrochemicals and other fields as important structural components and pipeline components. The welding quality of their butt joints directly affects the safety and service life of the structure or pipeline.
[0003] During the welding process, the weld and the adjacent heat-affected zone undergo rapid heating and cooling, which easily leads to grain coarsening, hardening of the structure, and concentration of residual tensile stress. This is the main cause of brittle fracture, stress corrosion cracking, and fatigue failure of steel pipe rods during service.
[0004] Existing magnetic field-assisted welding technology can improve the microstructure of weld joints, refine grains, and reduce segregation through electromagnetic stirring. However, existing magnetic welding technologies generally suffer from the following problems:
[0005] The control mode is singular, applying a constant magnetic field throughout the welding process, which cannot be used to control the different response mechanisms of the molten metal in the molten pool and the solid heat-affected zone in stages.
[0006] Relying on external sensors such as infrared thermometry to actively control magnetic field parameters results in measurement errors and control delays.
[0007] The magnetic field energy covers a large area uniformly, but lacks targeting of the weak link of the fusion line. Furthermore, the Curie temperature is only passively accepted as an inherent property of the parent material, and there is no technical solution to actively introduce exogenous functional materials with customized Curie temperatures to achieve tissue regulation.
[0008] Therefore, those skilled in the art have provided an automated steel pipe pole welding device to solve the problems mentioned in the background art. Summary of the Invention
[0009] To solve the above-mentioned technical problems, the present invention provides an automatic feeding steel pipe pole welding equipment, including a frame, feeding mechanisms disposed at the left and right ends of the frame, and a welding mechanism disposed in the central area of the frame;
[0010] The welding mechanism includes:
[0011] The ring frame is fixedly installed on the machine frame;
[0012] A magnetic welding assembly is rotatably mounted inside a ring frame and is used to weld the butt joint of two steel pipe rods. The magnetic welding assembly is equipped with a magnetic field generator.
[0013] A particle coating assembly is set on both sides of the annular frame and is used to coat the outer circular surface of the end of the steel pipe rod with an annular particle strip before welding.
[0014] The granular band is composed of ferromagnetic micro / nano particles with a predetermined Curie temperature Tc and a high-temperature resistant inorganic binder.
[0015] During the welding process, the magnetic field generator produces a magnetic field in the particle zone. When the temperature of the particle zone exceeds the Curie temperature Tc, the particles lose magnetism, and the magnetic field penetrates the pipe wall and acts on the molten metal in the molten pool to perform electromagnetic stirring. When the temperature drops below the Curie temperature Tc, the particles regain ferromagnetism, and the magnetic field energy is concentrated in the solid heat-affected zone where the particle zone is located, causing the particles to produce magnetostrictive vibrations to microscopically control the solid structure.
[0016] Preferably, the ring frame includes two fixed rings symmetrically distributed on the left and right sides. The two fixed rings are fixedly connected to the frame by a fixed rod. An inner slide rail is provided at one adjacent end of each of the two fixed rings. The magnetic welding assembly is slidably fitted in the inner slide rail. An outer slide rail is provided on the outer end face of each fixed ring. The particle coating assembly is slidably fitted in the outer slide rail.
[0017] Preferably, the magnetic welding assembly includes:
[0018] The slip ring has its left and right edges slidably embedded in the inner slide rails of two fixed rings. The outer circumferential surface of the slip ring is provided with an outer toothed ring, which is used to mesh with the drive assembly to achieve circumferential rotation.
[0019] At least one cylinder is fixedly installed on the inner wall of the slip ring, and the moving end of the cylinder is fixedly connected to a base plate.
[0020] The welding head, fixedly installed on the base plate, is used for welding the butt joint circumferential seam of steel pipe poles.
[0021] Preferably, the magnetic field generator comprises two sets, which are respectively arranged on both sides of the base plate along the axial direction of the steel pipe rod, and correspond to the positions of the particle strips on the outer circular surface of the steel pipe rod ends on the left and right sides;
[0022] Each magnetic field generator set includes:
[0023] The arc-shaped magnetic pole shoe has its concave arc surface located on the radial outer side of the corresponding particle band, with a preset radial gap between them;
[0024] The excitation coil is embedded in a side groove opened in the side wall of the arc-shaped magnetic pole shoe. The excitation coil is electrically connected to an external controllable excitation power supply. A protective cover is provided at the opening of the side groove. The protective cover is made of non-magnetic high-temperature resistant material.
[0025] Preferably, the particle coating assembly includes:
[0026] The guide rail has one end slidably embedded in the outer slide rail of the fixed ring;
[0027] The pellet storage bin has a ring-shaped hollow structure and is fixedly connected to the other end of the guide rail. Its interior contains slurry used to form pellet belts.
[0028] The outer peripheral surface of the pellet storage bin is provided with an outer toothed ring II, which is used to mesh with the drive assembly to drive the pellet storage bin to rotate.
[0029] Preferably, a plurality of coating heads are arranged circumferentially on the inner ring surface of the granular storage bin, and an adjuster is provided on one side of each coating head;
[0030] The adjuster is used to axially position the end face of the steel pipe before the coating operation begins, and simultaneously adjust the radial and axial distances between the coating head and the outer circumferential surface of the steel pipe.
[0031] Preferably, the regulator includes:
[0032] An electric actuator, the fixed end of which is installed on the inner wall of the granule storage bin, and the movable end which extends and retracts radially and is fixedly connected to a moving plate;
[0033] The L-shaped baffle has one end that is slidably inserted into the movable plate and its extension length is adjustable.
[0034] Limit screws are used to lock the baffle onto the movable plate;
[0035] The nozzle of the coating head is fixedly mounted on the moving plate and moves synchronously with the moving plate.
[0036] Preferably, the coating head further includes a micro pump, the inlet of which is connected to a through hole in the inner wall of the granule storage bin, and the outlet of which is connected to a nozzle via a hose.
[0037] Preferably, the ferromagnetic micro / nano particles are selected from one or more of Mn-Zn ferrite, Ni-Zn ferrite, or rare earth-transition metal alloys, and their Curie temperature Tc is selected in the range of 100℃ to 350℃ according to the material of the steel pipe rod to be welded and the welding process requirements.
[0038] Preferably, the granular band is located on the outer circular surface of the steel pipe rod end at a predetermined axial distance from the welding end face;
[0039] The magnetic field generated by the magnetic field generator is a DC magnetic field or a low-frequency alternating magnetic field.
[0040] The technical effects and advantages of this invention are as follows:
[0041] (1) This invention utilizes the inherent abrupt change in the magnetic properties of particulate materials at the Curie temperature Tc as a control trigger signal to enable the same magnetic field generator to automatically switch operating modes during the welding thermal cycle:
[0042] In the heating stage (T>Tc), the particles are demagnetized, the magnetic field penetrates and acts on the molten pool for electromagnetic stirring, so as to refine the weld grain, and reduce segregation and porosity;
[0043] In the cooling stage (T<Tc), the particles restore ferromagnetism, the magnetic field energy is concentrated in the heat-affected zone, the particles generate magnetostrictive vibration to break coarse grains, eliminate residual tensile stress and induce the precipitation of strengthening phases;
[0044] The entire switching process is triggered by the temperature response of the material itself, no external sensors and control systems are required, and the time sequence is guaranteed by physical laws;
[0045] (2) The particles of the present invention are only coated on the outer circular surface of the pipe end of the steel pipe pole. At high temperature, the particles are demagnetized to release the magnetic field and uniformly cover the molten pool. At low temperature, the particles restore magnetism to recover the magnetic field and concentrate it in the heat-affected zone where the particle band is located, ensuring that the magnetic field energy acts on the fusion line which is the weakest link of the welded joint, with high energy utilization rate. Brief Description of the Drawings
[0046] Figure 1 is a schematic diagram of the three-dimensional structure of the present invention;
[0047] Figure 2 is a front view of the present invention;
[0048] Figure 3 is a side view of the present invention;
[0049] Figure 4 is a schematic structural diagram of the clamping and positioning assembly in the present invention;
[0050] Figure 5 is a partial exploded view of the present invention;
[0051] Figure 6 is in the present invention Figure 5 is a schematic structural diagram of Part A;
[0052] Figure 7 is a schematic structural diagram of the welding mechanism in the present invention;
[0053] Figure 8 is in the present invention Figure 7 is a side view thereof;
[0054] Figure 9 is in the present invention Figure 7 is an exploded view thereof;
[0055] Figure 10 is an exploded view of the magnetic welding assembly in the present invention;
[0056] Figure 11 is an exploded view of the particle coating assembly in the present invention;
[0057] Figure 12 In this invention Figure 11 A schematic diagram of the structure at point B.
[0058] In the picture:
[0059] 1. Frame; 2. Support legs; 3. Feeding mechanism; 4. Steel pipe pole; 5. Mounting slot; 6. Welding mechanism;
[0060] 31. Transfer roller; 32. Clamping and positioning assembly; 321. Frame; 322. Hydraulic rod; 323. Mounting frame; 324. Roller;
[0061] 41. Particle band;
[0062] 61. Ring frame; 62. Magnetic welding assembly; 63. Particle coating assembly; 64. Drive assembly;
[0063] 611. Fixing ring; 612. Fixing rod; 613. Inner slide rail; 614. Outer slide rail;
[0064] 621. Slip ring; 622. External gear ring 1; 623. Detection sensor; 624. Cylinder; 625. Base plate; 626. Welding head; 627. Magnetic field generator;
[0065] 6271. Arc-shaped magnetic pole shoe; 6272. Side groove; 6273. Excitation coil; 6274. Protective cover;
[0066] 631. Guide rail; 632. Granule storage bin; 633. External toothed ring II; 634. Through hole; 635. Coating head; 636. Regulator; 637. Injection hole; 638. Sealing plug;
[0067] 6351, Miniature pump; 6352, Hoses; 6353, Nozzles; 6361, Electric actuators; 6362, Moving plates; 6363, Baffles; 6364, Limit screws;
[0068] 641. Connecting frame; 642. Drive motor; 643. Gear. Detailed Implementation
[0069] The present invention will now be described in further detail with reference to the accompanying drawings and specific embodiments. The embodiments of the present invention are given for illustrative and descriptive purposes only, and are not intended to be exhaustive or to limit the invention to the forms disclosed. Many modifications and variations will be apparent to those skilled in the art. The embodiments were chosen and described to better illustrate the principles and practical application of the invention, and to enable those skilled in the art to understand the invention and design various embodiments with various modifications suitable for a particular purpose.
[0070] Example
[0071] Please see Figures 1-12 In this embodiment, an automatic feeding steel pipe pole welding device is provided, the overall structure of which is as follows: Figure 1 , Figure 2 and Figure 3 As shown, the equipment mainly includes a frame 1, a feeding mechanism 3, a steel pipe rod 4, and a welding mechanism 6;
[0072] The frame 1 has multiple support legs 2 at its bottom to stably support the equipment on the working ground. The frame 1 has a set of feeding mechanisms 3 at each of its left and right ends along its length. The two sets of feeding mechanisms 3 are symmetrically arranged in structure, and their conveying directions can be selectively forward or reversed. Through this bidirectional conveying design, both ends of the equipment can be used as feeding ends. In the welding preparation stage, the two sets of feeding mechanisms 3 simultaneously convey the steel pipe rods 4 to be welded from both ends of the frame 1 to the central area of the frame 1 until the opposite ends of the two steel pipe rods 4 are joined at the welding station.
[0073] The welding mechanism 6 is fixedly installed in the central area of the frame 1 and is matched with the position of the feeding mechanism 3. When the two steel pipe rods 4 are transported to the preset welding station and axially aligned and fitted with the end face, the welding mechanism 6 performs welding operation on the butt joint circumferential seam between the two steel pipe rods 4, thereby fixing the two together as one.
[0074] After the welding process is completed, the feeding mechanism 3 on one side can be switched to reverse operation mode according to the preset discharge direction instruction, and used as a discharge conveying mechanism. At this time, the entire steel pipe rod 4 that has been welded is transported out of the welding station in the opposite direction of the original feeding path under the drive of the feeding mechanism 3 on this side, and transferred to the receiving device of the next process, thereby realizing the continuous automated operation cycle of feeding, welding and discharge.
[0075] Specifically, the structure of the feeding mechanism 3 is as follows: Figure 1 and Figure 4 As shown, it includes a transfer roller 31 and several sets of clamping and positioning components 32 arranged at intervals along the conveying direction;
[0076] The transfer roller 31 is rotatably mounted inside the frame 1. It can adopt a conventional roller conveyor structure in the art, which will not be described in detail here. The transfer roller 31 is used to carry the steel pipe rod 4 and drive it to move longitudinally along the frame 1 to complete the loading and unloading conveying.
[0077] The clamping and positioning assembly 32 is used to limit and guide the radial position of the steel pipe rod 4 during the conveying process, and to apply clamping force to the steel pipe rod 4 during the welding process to achieve circumferential positioning. Each clamping and positioning assembly 32 includes a frame 321. The frame 321 has a gate-shaped structure, spans across the top of the frame 1 and is fixedly installed on the working area of the transmission roller 31. Hydraulic rods 322 are fixedly installed on the inner top wall and the inner side walls of the front and rear sides of the frame 321. The piston rod ends of each hydraulic rod 322 extend toward the central axis of the frame 321.
[0078] Each hydraulic rod 322 has a fixed mounting frame 323 at its movable end. Rollers 324 are rotatably mounted within the mounting frame 323 via a rotating shaft. The rotation axis of the rollers 324 is perpendicular to the axial direction of the steel pipe rod 4, thus ensuring that the rolling direction of the rollers 324 is consistent with the axial movement direction of the steel pipe rod 4. When the steel pipe rod 4 moves forward under the drive of the transmission roller 31, rolling contact is formed between the rollers 324 and the outer circumferential surface of the steel pipe rod 4 to reduce frictional resistance during transport. When the hydraulic rod 322 drives the rollers 324 to press towards the center, multiple rollers 324 in various directions act together on the outer circumferential surface of the steel pipe rod 4, achieving clamping and positioning of the steel pipe rod 4 and ensuring that it does not rotate circumferentially or move axially during welding.
[0079] like Figure 5 and Figure 6 As shown, a downwardly recessed mounting groove 5 is provided at the center of the frame 1. The mounting groove 5 is located between the two sets of feeding mechanisms 3 on the left and right. The welding mechanism 6 is housed in the mounting groove 5, and its working area corresponds vertically to the docking position of the two steel pipe rods 4 to be welded.
[0080] During the welding preparation stage, the steel pipe rods 4 on the left and right sides are driven by their respective feeding mechanisms 3, and their ends to be welded are fed towards each other and gradually approach each other. Through the guiding and limiting effect of the clamping and positioning components 32 in the feeding mechanism 3, the axes of the two steel pipe rods 4 are coaxially aligned and their two end faces are tightly fitted.
[0081] After centering is completed, the welding mechanism 6 is started and welding is carried out along the butt joint of the two steel pipe rods 4 to fix them together as a continuous steel pipe rod 4. After the welding process is completed, the welding mechanism 6 is reset, and the feeding mechanism 3 moves the welded steel pipe rod 4 out of the welding station according to the preset discharge direction and transports it to the receiving device of the next process, thus completing a complete welding operation cycle.
[0082] The specific structure of welding mechanism 6 is as follows: Figure 6 , Figure 7 , Figure 8 and Figure 9As shown, it includes a ring frame 61, a magnetic welding assembly 62, a particle coating assembly 63, and a drive assembly 64.
[0083] Among them, the ring frame 61 is installed on the frame 1. It is a ring structure and its bottom is placed in the mounting groove 5. The inner surface of the mounting groove 5 is an arc structure and is concentric with the ring frame 61. A magnetic welding component 62 is set at the center of the ring frame 61. The magnetic welding component 62 is slidably connected to the ring frame 61 and can rotate along the inner circumference of the ring frame 61 under the drive of the drive component 64, thereby realizing the full circumferential welding operation of the butt joint circumferential seam of the two steel pipe rods 4.
[0084] A set of particle coating components 63 is provided on each of the left and right sides of the ring frame 61 along its axial direction. The particle coating components 63 are located close to the end face of the steel pipe rod 4 to be welded, and can rotate around the axis of the steel pipe rod 4 under the drive of the drive component 64. Before the welding operation begins, the particle coating components 63 form a ring of particle strips 41 by spraying at a preset distance from the end face of the outer circle of the pipe end of the steel pipe rod 4. The particle strips 41 work together with the magnetic field during the welding process of the magnetic welding component 62 to improve the microstructure of the welded joint and improve the welding quality.
[0085] The drive assembly 64 is connected to the magnetic welding assembly 62 and the particle coating assembly 63 to provide the required rotary drive force for both, ensuring the coordinated operation of welding and coating.
[0086] Specifically, such as Figure 6 As shown, two sets of drive components 64 are respectively provided for the magnetic welding component 62 and the particle coating component 63, symmetrically arranged on both sides of the frame 1. Each drive component 64 includes a connecting frame 641. The bottom of the connecting frame 641 is fixedly installed on the side wall of the frame 1, and the top of the connecting frame 641 is fixedly mounted with a drive motor 642. The output shaft end of the drive motor 642 is fixedly connected to a main shaft, and a gear 643 is coaxially provided on the main shaft. The gear 643 in the drive component 64 corresponding to the magnetic welding component 62 meshes with the transmission teeth of the magnetic welding component 62 to drive the magnetic welding component 62 to rotate circumferentially along the ring frame 61. The gear 643 in the drive component 64 corresponding to the particle coating component 63 meshes with the transmission teeth of the particle coating component 63 to drive the particle coating component 63 to rotate around the axis of the steel pipe rod 4. Thus, the power of the drive motor 642 is transmitted to the corresponding component through the gear 643, realizing independent drive of welding and coating actions.
[0087] like Figure 9 As shown, the ring frame 61 includes two fixed rings 611 that are symmetrically distributed along the axial direction. The two fixed rings 611 are fixedly connected to the frame 1 by fixed rods 612, so that the ring frame 61 is stably installed in the upper area of the mounting groove 5.
[0088] Each of the two fixed rings 611 has an inner slide rail 613 on one of its adjacent end faces, which is used to slide with the magnetic welding assembly 62 and provide circumferential rotation guidance and radial support for the magnetic welding assembly 62.
[0089] Each fixed ring 611 has an outer slide rail 614 on its outer end face away from the other fixed ring 611. The outer slide rail 614 is used to slide with the particle coating component 63 on the corresponding side, so that the particle coating component 63 can rotate stably around the axis of the steel pipe rod 4.
[0090] Through the above-mentioned double-layer slide rail structure design, the magnetic welding component 62 and the particle coating component 63 achieve independent guidance of rotational motion on the same ring frame 61, without interfering with each other, thus ensuring the spatial coordination and motion accuracy of welding and coating operations.
[0091] The specific structure of the magnetic welding assembly 62 is as follows: Figure 10 As shown, it includes a slip ring 621. The left and right edges of the slip ring 621 are slidably embedded in the inner slide rails 613 of the two fixed rings 611, so that it can rotate stably in the circumferential direction under the guidance of the inner slide rails 613. An external toothed ring 622 is provided on the outer circumferential surface of the slip ring 621. The external toothed ring 622 meshes with the corresponding gear 643 in the drive assembly 64. When the drive motor 642 drives the gear 643 to rotate, the gear 643 drives the slip ring 621 to rotate in the circumferential direction in the inner slide rail 613 through the external toothed ring 622.
[0092] At least one cylinder 624 is fixedly installed on the inner wall of the slip ring 621. The piston rod of the cylinder 624 extends inward along the radial direction of the slip ring 621, and its movable end is fixedly connected to the base plate 625. A welding head 626 is fixedly installed on the base plate 625. The welding head 626 points towards the area to be welded on the steel pipe rod 4. When the slip ring 621 rotates, the cylinder 624 and the welding head 626 rotate together. The welding head 626 rotates around the axis of the steel pipe rod 4 for one revolution, which can complete the full circumference welding of the butt joint circumference of the two steel pipe rods 4.
[0093] Furthermore, a set of magnetic field generators 627 are provided on each side of the base plate 625 along the axial direction of the steel pipe rod 4. The two sets of magnetic field generators 627 correspond to the particle strips 41 on the outer circular surface of the pipe ends of the steel pipe rod 4 on the left and right sides, respectively. Each set of magnetic field generators 627 includes an arc-shaped magnetic pole shoe 6271. The concave arc surface of the arc-shaped magnetic pole shoe 6271 is located on the radial outer side of the corresponding particle strip 41, and a preset radial gap, such as 1mm to 3mm, is left between the two to ensure effective magnetic field coupling while avoiding mechanical interference.
[0094] A side groove 6272 is provided on the side wall of the arc-shaped magnetic pole shoe 6271. An excitation coil 6273 is embedded in the side groove 6272. The excitation coil 6273 is electrically connected to a controllable excitation power supply outside the equipment through a wire. A protective cover 6274 is provided at the opening of the side groove 6272. The protective cover 6274 is made of non-magnetic high-temperature resistant material to protect the excitation coil 6273 from damage by welding spatter and fumes, while not affecting the normal penetration of the magnetic field.
[0095] In addition, two detection sensors 623 are fixedly installed on the inner wall of the slip ring 621. The detection sensors 623 can be photoelectric sensors or proximity sensors. When the steel pipe rods 4 on the left and right sides move to the predetermined docking position at the center of the welding station under the drive of the feeding mechanism 3, the detection sensors 623 detect the arrival signal of the end of the steel pipe rod 4 and feed the signal back to the control system of the equipment (which adopts existing technology and will not be described in detail in this article). The control system then controls the transmission roller 31 to stop conveying and simultaneously activates the clamping and positioning assembly 32 to clamp and limit the steel pipe rod 4, preparing for subsequent welding operations.
[0096] The specific structure of the particle coating component 63 is as follows: Figure 11 and Figure 12 As shown, it includes a guide rail 631. One end of the guide rail 631 is slidably embedded in the outer slide rail 614 of the fixing ring 611 and can slide along the circumference of the outer slide rail 614. The other end of the guide rail 631 is fixedly connected to a granule storage bin 632. The granule storage bin 632 has an annular hollow structure and is used to contain the slurry that forms the granule belt 41. An injection hole 637 is provided on the outer wall of the granule storage bin 632 for replenishing the slurry into the bin. A sealing plug 638 is detachably sealed inside the injection hole 637.
[0097] The outer peripheral surface of the pellet storage bin 632 is provided with an external gear ring 633. The external gear ring 633 meshes with the corresponding gear 643 in the drive assembly 64. When the drive motor 642 starts, the gear 643 drives the pellet storage bin 632 to rotate as a whole through the external gear ring 633, thereby causing the guide rail 631 to slide circumferentially along the outer slide rail 614.
[0098] Several coating heads 635 are arranged circumferentially on the inner ring surface of the granular storage bin 632. Each coating head 635 is provided with an adjuster 636 on one side. The adjuster 636 is used to axially position the end face of the steel pipe rod 4 before the coating operation begins, and at the same time adjust the radial distance between the coating head 635 and the outer circumferential surface of the steel pipe rod 4.
[0099] Specifically, the regulator 636 includes an electric push rod 6361, a movable plate 6362, a baffle 6363, and a limiting screw 6364. The fixed end of the electric push rod 6361 is installed on the inner wall of the granule storage bin 632, and its movable end extends and retracts along the radial direction of the granule storage bin 632 and is fixedly connected to the movable plate 6362. The movable plate 6362 has an insertion groove, and one end of the L-shaped baffle 6363 is slidably inserted into the insertion groove, and its extension length is adjustable. The limiting screw 6364 passes through the side wall of the movable plate 6362 and is used to lock the L-shaped baffle 6363 in the current extension position.
[0100] In the coating preparation stage before welding, the electric actuator 6361 drives the moving plate 6362 and the L-shaped baffle 6363 to extend towards the center of the granule storage bin 632. The bent section of the L-shaped baffle 6363 faces the welding end face of the steel pipe rod 4. When the L-shaped baffle 6363 extends into place, its inner side abuts against the welding end face of the steel pipe rod 4, thereby axially limiting the steel pipe rod 4. At the same time, the radial position of the moving plate 6362 determines the position of the nozzle 6353 in the coating head 635 fixedly connected to it relative to the outer circumferential surface of the steel pipe rod 4. The radial spacing between them can be adjusted by changing the extension length of the L-shaped baffle 6363 within the moving plate 6362. This changes the axial distance between the inner side of the L-shaped baffle 6363 and the nozzle 6353, thereby adjusting the axial distance between the particle strip 41 formed by the nozzle 6353 on the outer circumference of the steel pipe rod 4 and the welding end face. When the extension length increases, the particle strip 41 is farther from the welding end face; when the extension length decreases, the particle strip 41 is closer to the welding end face. Thus, it can flexibly adapt to the requirements of different pipe diameters and different welding processes for the coating position of the particle strip 41.
[0101] The coating head 635 includes a micro pump 6351, a hose 6352, and a nozzle 6353. The inlet of the micro pump 6351 is connected to a through hole 634 on the inner wall of the granule storage bin 632. The granule slurry can enter the micro pump 6351 through the through hole 634. The outlet of the micro pump 6351 is connected to the nozzle 6353 through the hose 6352. The nozzle 6353 is fixedly installed on the moving plate 6362 and moves synchronously with the moving plate 6362. When the granule storage bin 632 rotates and the micro pump 6351 works, the nozzle 6353 sprays the granule slurry evenly onto the outer circular surface of the end of the steel pipe rod 4. Under the axial positioning cooperation of the regulator 636, a uniform annular granule belt 41 is formed at the preset position. It should be noted that in order to accelerate the drying of the granule belt 41 after coating, an infrared heating device can be added, which can be achieved using existing technology.
[0102] The following describes in detail the cooperative working principle of the particle belt 41 and the magnetic welding assembly 62 in this invention, based on the above structure:
[0103] In this invention, the particle band 41 is composed of ferromagnetic micro / nano particles with a predetermined Curie temperature Tc and a high-temperature resistant inorganic binder. The ferromagnetic particles are selected from one or more of Mn-Zn ferrite, Ni-Zn ferrite, or rare earth-transition metal alloys. The Curie temperature of Mn-Zn power ferrite material is about 200-250℃, the Curie temperature of Mn-Zn high conductivity material is about 120-170℃, and the Curie temperature of Ni-Zn ferrite is higher (>300℃). By adjusting the material formula, a customized design with a Curie temperature in the range of 100℃ to 350℃ can be achieved (the specific implementation is not described in detail here; this invention only utilizes its temperature performance). The particle size is 50nm to 5μm.
[0104] Taking the welding of Q345B steel pipe rod 4 as an example, Mn-Zn ferrite micro-nano particles with a Curie temperature Tc of 220℃ and an average particle size of 500nm are selected. They are mixed with sodium silicate and other high-temperature resistant inorganic binders and appropriate solvents to form a slurry, which is then stored in the particle storage silo 632.
[0105] In the coating preparation stage before welding, the electric actuator 6361 of the regulator 636 drives the moving plate 6362 and the L-shaped baffle 6363 to extend towards the center of the granule storage bin 632. The inner side of the L-shaped baffle 6363 abuts against the welding end face of the steel pipe rod 4 to achieve axial positioning. By adjusting the extension length of the L-shaped baffle 6363 in the moving plate 6362, the axial distance between the granule belt 41 and the welding end face is set to 3-5mm. At the same time, the radial position of the moving plate 6362 determines the radial distance between the nozzle 6353 and the outer circumferential surface of the steel pipe rod 4.
[0106] After positioning, the drive motor 642 drives the granule storage bin 632 to rotate as a whole through the meshing of the gear 643 and the external gear ring 633. The micro pump 6351 works to transport the granule slurry through the through hole 634 and the hose 6352 to the nozzle 6353, and evenly spray it on the outer circular surface of the end of the steel pipe rod 4 to form an annular granule strip 41 with a width of 3-6mm and a thickness of about 0.2-0.5mm. After coating, the slurry is cured by hot air or other heating methods, and the granule strip 41 is firmly attached to the pipe wall.
[0107] After coating is completed, when the steel pipe rods 4 on the left and right sides move to the predetermined position towards the center of the welding station under the drive of the feeding mechanism 3, the detection sensor 623 detects the arrival signal of the ends of the two steel pipe rods 4 and feeds the signal back to the control system of the equipment. The control system adopts the control unit commonly used in conventional welding equipment. Its control logic is well known to those skilled in the art and will not be described in detail here. After receiving the arrival signal, the control system immediately controls the transmission roller 31 to stop conveying and simultaneously starts the extension of each hydraulic rod 322 of the clamping and positioning component 32, driving the corresponding roller 324 to press against the outer circumferential surface of the steel pipe rod 4, thereby clamping and limiting the two steel pipe rods 4 in both the axial and circumferential directions, so that the welding end faces of the two steel pipe rods 4 are fitted and aligned.
[0108] At this time, the magnetic welding assembly 62 is in the welding start position. The arc-shaped magnetic pole shoe 6271 in the magnetic field generator 627 is located on the radial outer side of the corresponding particle belt 41 along with the slip ring 621. Its concave arc surface is opposite to the outer circular surface of the particle belt 41, and there is a preset radial gap between them, such as 1-3mm, to form a uniform radial air gap. The excitation coil 6273 is electrically connected to the external controllable excitation power supply through the wire. Before the welding starts, the controllable excitation power supply passes DC current to the excitation coil 6273 to establish an initial magnetic field in the particle belt 41 area.
[0109] When the welding power supply is started, the welding head 626 starts to arc. The drive motor 642 drives the slip ring 621 to rotate circumferentially in the inner slide rail 613 through the meshing of the gear 643 and the outer gear ring 622. The cylinder 624 and the welding head 626 rotate together. The welding head 626 rotates around the axis of the steel pipe rod 4 and welds the butt joint circumferential seam of the two steel pipe rods 4.
[0110] The heat from the electric arc causes the temperature of the pipe end of the steel pipe rod 4 and the particle band 41 attached thereto to rise sharply. When the temperature of the particle band 41 exceeds its Curie temperature Tc (taking Q345B steel pipe rod as an example, Tc=220℃), the particles undergo a ferromagnetic-paramagnetic transition, and the magnetic permeability drops sharply from hundreds to close to the vacuum magnetic permeability within an extremely narrow temperature range.
[0111] At this point, the particle band 41 transforms from a highly permeable medium into a magnetic circuit break point in the magnetic circuit. The magnetic field is no longer bound and concentrated by the particle band 41, but instead uniformly penetrates the pipe wall and covers the entire weld pool area. Under the action of the external magnetic field, the molten metal in the weld pool is driven by the Lorentz force, generating forced convection and electromagnetic stirring. This stirring effect produces the following results:
[0112] It breaks the growth conditions of coarse columnar crystals, promotes the refinement of weld grains, and transforms columnar crystals into fine equiaxed crystals;
[0113] Accelerates the uniform diffusion of solute elements and reduces component segregation;
[0114] Promotes bubble escape and reduces porosity defects;
[0115] Based on this, the electromagnetic stirring effect of an external magnetic field can improve the microstructure of the welded joint, making the grains finer and more uniform, significantly reducing defects in the welded joint, making the weld surface smoother and improving its mechanical properties.
[0116] As the welding head 626 rotates forward, the weld and heat-affected zone after the arc passes begin to cool naturally. When the temperature of this area drops below the Curie temperature Tc, the particles regain their ferromagnetism, and the magnetic permeability rises sharply back to its original level.
[0117] At this time, the particle strip 41 becomes a high-permeability magnetic path again on the magnetic circuit, and the magnetic field is captured and concentrated by the particle strip 41 again. The magnetic field energy is highly concentrated in the solid heat-affected zone where the particle strip 41 is located. At this stage, the controllable excitation power supply can switch the excitation current to low-frequency AC (e.g., 5Hz) to generate an alternating magnetic field. Under the action of the alternating magnetic field, the ferromagnetic particles generate a magnetostrictive effect—that is, they undergo high-frequency micro-vibrations with the frequency of the alternating magnetic field.
[0118] This micro-vibration propagates from the particle as the center to the surrounding solid tissue, generating localized micro-mechanical impacts, the effects of which include:
[0119] The already formed coarse grains are broken up, further promoting the grain refinement of the heat-affected zone;
[0120] Microscopic plastic deformation can release welding thermal stress, eliminate residual tensile stress, and even introduce beneficial residual compressive stress.
[0121] The particles themselves act as heterogeneous nucleation sites, which, under the induction of a magnetic field, promote the precipitation of fine second phases (such as carbides) in favorable directions, pinning grain boundaries and hindering grain growth;
[0122] Piezomagnetic ferrite materials can generate mechanical vibrations in an alternating field, converting electromagnetic energy into mechanical kinetic energy. This invention utilizes this effect to automatically convert the temperature change (down to Tc) during the welding cooling stage into a trigger signal for mechanical control actions.
[0123] This invention establishes a Curie temperature self-triggering mechanism, specifically referring to: utilizing the inherent Curie temperature of the particulate material as a physical switch, at different stages of the welding thermal cycle, without the need for any external temperature sensor and control system to actively intervene, automatically changing the coupling mode between the particles and the magnetic field, thereby automatically switching the target and mode of action of the magnetic field.
[0124] Specifically, this manifests as follows:
[0125] During the welding heating stage, when the temperature of the particle band 41 is higher than its Curie temperature Tc, the particles become paramagnetic and lose their magnetism. At this time, the magnetic field is no longer bound by the particle band 41, but instead penetrates the pipe wall uniformly and acts on the molten metal in the molten pool. Through electromagnetic stirring, the weld grains are refined and the compositional segregation and porosity defects are reduced.
[0126] During the welding cooling stage, when the temperature drops below the Curie temperature Tc, the particles regain their ferromagnetism. The magnetic field energy is recaptured and concentrated in the solid heat-affected zone where the particle band 41 is located. The particles that regain their magnetism generate magnetostrictive vibrations under the action of the magnetic field, which break the already formed coarse grains, eliminate residual tensile stress, and induce fine second phases to precipitate along favorable directions to strengthen the microstructure.
[0127] This self-triggered mechanism differs from existing technologies in that:
[0128] The trigger signal comes from the magnetic abrupt change in the particulate material itself at the Curie temperature, rather than from external sensor measurement; and the same magnetic field device automatically switches between molten pool stirring mode and solid structure control mode only due to temperature changes.
[0129] Furthermore, the triggering timing is determined by the material's thermal conduction and phase change physical processes, eliminating the delay and error of electronic control systems. Moreover, the particles only exist at the coating location. At high temperatures, the particles lose magnetism, causing the magnetic field to be released and act on the molten pool. At low temperatures, the particles regain magnetism, causing the magnetic field to be recovered and concentrated on the heat-affected zone, resulting in high energy utilization.
[0130] After the welding head 626 rotates once with the slip ring 621, the welding of the entire circumference of the butt joint is completed. The controllable excitation power supply is disconnected, the excitation coil 6273 is de-energized, the magnetic field is removed, the clamping and positioning component 32 is released, and the entire steel pipe rod 4 that has been welded is transported out of the welding station by the feeding mechanism 3 in the opposite direction to enter the next process. The granular strip 41 is permanently retained on the pipe wall as a disposable functional material, which has no adverse effect on the subsequent use of the steel pipe rod 4.
[0131] This invention, through the aforementioned Curie temperature self-triggered mechanism and phased synergistic control, achieves the following technical effects for welding steel pipe rod 4:
[0132] During the welding heating stage (T > Tc), electromagnetic stirring causes forced convection in the molten pool, breaking the growth conditions of coarse columnar crystals and promoting significant grain refinement in the weld, transforming columnar crystals into fine equiaxed crystals. At the same time, electromagnetic stirring accelerates the uniform diffusion of solute elements, reduces component segregation, promotes bubble escape, and effectively reduces the sensitivity to porosity and hot cracking. For the welding of steel pipe rod 4, it reduces internal defects in the weld, improves the strength and toughness matching of the weld itself, and reduces the repair welding rate.
[0133] During the welding cooling stage (T < Tc), the magnetostrictive vibration generated after the particles regain their ferromagnetism applies a high-frequency micro-mechanical impact to the solid heat-affected zone. This impact releases the welding thermal stress through micro-plastic deformation, significantly reducing the residual tensile stress. At the same time, the stress state at the weld toe changes from harmful residual tensile stress to compressive stress that is beneficial to fatigue strength, thereby extending the fatigue life of the steel pipe rod 4 under alternating loads (such as wind vibration).
[0134] The steel pipe rod 4 is prone to stress corrosion cracking under the combined action of corrosive media and residual tensile stress. The present invention eliminates the residual tensile stress in the heat-affected zone and introduces compressive stress during the cooling stage, thereby inhibiting the initiation and propagation conditions of stress corrosion cracks and improving the operational safety of the steel pipe rod 4 in a highly corrosive environment.
[0135] The coarse-grained zone of the weld heat-affected zone becomes the weakest softening link of the joint due to excessive grain growth. During the cooling stage, magnetostrictive vibration breaks up the already formed coarse grains. At the same time, the grains themselves act as heterogeneous nucleation points, promoting the precipitation of fine second phases along favorable directions and pinning grain boundaries under the induction of the magnetic field, hindering the continued growth of grains, eliminating the softening phenomenon in the heat-affected zone, making the hardness and strength distribution of the entire weld joint more uniform, and avoiding the problem of fracture concentration in the near-weld area.
[0136] Uneven thermal shrinkage during welding is the main cause of bending deformation of steel pipe rods. Microscopic vibration during the cooling stage causes thermal stress to be gradually released at high temperature, rather than concentrated shrinkage after complete cooling, thereby reducing residual deformation after welding, ensuring the straightness of steel pipe rod 4, and reducing the amount of subsequent straightening work.
[0137] Obviously, the described embodiments are only a part of the embodiments of the present invention, and not all of them. All other embodiments obtained by those skilled in the art and related fields based on the embodiments of the present invention without inventive effort should fall within the scope of protection of the present invention. Structures, devices, and operating methods not specifically described and explained in the present invention, unless otherwise specified or limited, shall be implemented according to conventional means in the art.
Claims
1. An automatic feeding steel pipe pole welding device, comprising a frame (1), feeding mechanisms (3) disposed at the left and right ends of the frame (1), and a welding mechanism (6) disposed in the central area of the frame (1), characterized in that: The welding mechanism (6) includes: The ring frame (61) is fixedly installed on the frame (1); A magnetic welding assembly (62) is rotatably mounted in a ring frame (61) for welding the butt joint of two steel pipe rods (4). A magnetic field generator (627) is provided on the magnetic welding assembly (62). The particle coating assembly (63) is disposed on both sides of the annular frame (61) and is used to coat the outer circular surface of the end of the steel pipe rod (4) with an annular particle strip (41) before welding. Among them, the particle band (41) is composed of ferromagnetic micro-nano particles with a predetermined Curie temperature Tc and a high-temperature resistant inorganic binder; During the welding process, the magnetic field generator (627) generates a magnetic field in the particle zone (41). When the temperature of the particle zone (41) exceeds the Curie temperature Tc, the particles lose magnetism and the magnetic field penetrates the pipe wall to act on the molten metal in the molten pool for electromagnetic stirring. When the temperature drops below the Curie temperature Tc, the particles regain ferromagnetism and the magnetic field energy is concentrated in the solid heat-affected zone where the particle zone (41) is located, causing the particles to generate magnetostrictive vibrations to micro-control the solid structure.
2. The automatic feeding steel pipe pole welding equipment according to claim 1, characterized in that, The ring frame (61) includes two fixed rings (611) symmetrically distributed on the left and right. The two fixed rings (611) are fixedly connected to the frame (1) by a fixed rod (612). An inner slide rail (613) is provided at one adjacent end of each of the two fixed rings (611). The magnetic welding assembly (62) is slidably fitted in the inner slide rail (613). An outer slide rail (614) is provided on the outer end face of each fixed ring (611). The particle coating assembly (63) is slidably fitted in the outer slide rail (614).
3. The automatic feeding steel pipe pole welding equipment according to claim 2, characterized in that, The magnetic welding assembly (62) includes: The slip ring (621) has its left and right edges slidably embedded in the inner slide rails (613) of the two fixed rings (611). The outer circumferential surface of the slip ring (621) is provided with an outer toothed ring (622), which is used to mesh with the drive assembly (64) to achieve circumferential rotation. At least one cylinder (624) is fixedly installed on the inner wall of the slip ring (621), and the movable end of the cylinder (624) is fixedly connected to the base plate (625). The welding head (626) is fixedly installed on the base plate (625) and is used to weld the butt joint of the steel pipe rod (4).
4. The automatic feeding steel pipe pole welding equipment according to claim 3, characterized in that, The magnetic field generator (627) includes two sets, which are respectively set on both sides of the base plate (625) along the axial direction of the steel pipe rod (4) and correspond to the positions of the particle band (41) on the outer circular surface of the pipe end of the steel pipe rod (4) on the left and right sides. Each magnetic field generator (627) includes: The arc-shaped magnetic pole shoe (6271) has its concave arc surface located on the radial outer side of the corresponding particle band (41), with a preset radial gap between them; The excitation coil (6273) is embedded in the side groove (6272) opened on the side wall of the arc-shaped magnetic pole shoe (6271). The excitation coil (6273) is electrically connected to an external controllable excitation power supply. A protective cover (6274) is provided at the opening of the side groove (6272). The protective cover (6274) is made of non-magnetic high-temperature resistant material.
5. The automatic feeding steel pipe pole welding equipment according to claim 2, characterized in that, The particle coating assembly (63) includes: The guide rail (631) has one end slidably embedded in the outer slide rail (614) of the fixing ring (611); The pellet storage bin (632) has a ring-shaped hollow structure and is fixedly connected to the other end of the guide rail (631). Its interior contains slurry for forming the pellet belt (41). The outer peripheral surface of the pellet storage bin (632) is provided with an outer toothed ring II (633), which is used to mesh with the drive assembly (64) to drive the pellet storage bin (632) to rotate.
6. The automatic feeding steel pipe pole welding equipment according to claim 5, characterized in that, The inner ring surface of the granular storage bin (632) is provided with a number of coating heads (635) spaced circumferentially, and each coating head (635) is provided with an adjuster (636) on one side. The adjuster (636) is used to axially position the end face of the steel pipe rod (4) before the coating operation begins, and simultaneously adjust the radial and axial distances between the coating head (635) and the outer circumferential surface of the steel pipe rod (4).
7. The automatic feeding steel pipe pole welding equipment according to claim 6, characterized in that, The regulator (636) includes: An electric actuator (6361) has its fixed end installed on the inner wall of the granule storage bin (632), and its movable end extends and retracts radially and is fixedly connected to a movable plate (6362). The L-shaped baffle (6363) has one end slidably inserted into the movable plate (6362) and its extension length is adjustable; The limiting screw (6364) is used to lock the baffle (6363) onto the movable plate (6362); The nozzle (6353) of the coating head (635) is fixedly mounted on the moving plate (6362) and moves synchronously with the moving plate (6362).
8. The automatic feeding steel pipe pole welding equipment according to claim 7, characterized in that, The coating head (635) further includes a micro pump (6351), whose inlet is connected to a through hole (634) on the inner wall of the granule storage bin (632), and whose outlet is connected to a nozzle (6353) via a hose (6352).
9. The automatic feeding steel pipe pole welding equipment according to claim 1, characterized in that, The ferromagnetic micro-nano particles are selected from one or more of Mn-Zn ferrite, Ni-Zn ferrite or rare earth-transition metal alloy, and their Curie temperature Tc is selected in the range of 100℃ to 350℃ according to the material of the steel pipe rod (4) to be welded and the welding process requirements.
10. The automatic feeding steel pipe pole welding equipment according to claim 1, characterized in that, The particle band (41) is located on the outer circular surface of the end of the steel pipe rod (4) at a preset axial distance from the welding end face; The magnetic field generated by the magnetic field generator (627) is a DC magnetic field or a low-frequency alternating magnetic field.