A gas-liquid separation RTM molding process for high-transmittance composite materials
By setting up independent gas and liquid pathways in the RTM process and adopting a graded dispensing strategy of gas leading edge propulsion and resin trailing edge follow-up, the problems of air entrainment and flow front convergence in the traditional RTM process are solved, achieving high light transmittance and optical uniformity of high-transmittance composite materials and improving the yield.
Patent Information
- Application Number
- CN202611531309.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-30
- Publication Date
- 2026-11-17
AI Technical Summary
In the traditional RTM process for preparing high-transmittance composite materials, the resin tends to carry air from the mold cavity into the resin flow front during the resin propulsion process, resulting in the formation of microbubbles inside the product. This affects the transmittance and optical uniformity. Furthermore, the convergence of the resin flow front causes thickness deviation and optical distortion, making it difficult to ensure the consistency of overall transmittance and resulting in a low yield.
The gas-liquid separation RTM molding process is adopted. By setting independent gas and liquid channels in the mold, the gas channel is used to create a vacuum and inject resin in stages. Combined with the strategy of gas leading edge advancement and resin trailing edge follow-up, gas-liquid separation and stable pressure gradient control are achieved, eliminating the problems of microbubbles and flow front convergence.
Composite material products with high light transmittance and high optical uniformity are obtained, resulting in high light transmittance, good optical uniformity, low defect rate, and improved yield.
Smart Images

Figure CN123104113A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of composite material molding technology, specifically to a gas-liquid separation RTM molding process for high-transmittance composite materials. Background Technology
[0002] RTM (Resin Transfer Molding) is a closed-mold molding process. Its basic principle is as follows: fiber reinforcement is pre-laid in a closed mold, liquid resin is injected into the mold cavity through an injection device to impregnate the fiber reinforcement, and then cured at a certain temperature to obtain composite material products. This process has been widely used in aerospace, automotive, rail transportation, wind turbine blades, building lighting, sports equipment and other fields due to its advantages of low volatility, low pressure molding, high fiber content and good surface quality. However, when preparing high-transmittance composite material products, the traditional RTM process uses a single resin injection port design. During the resin propulsion process, air in the mold cavity is easily entrained into the resin flow front, resulting in the formation of microbubbles inside the product. This seriously affects the transmittance and optical uniformity. Furthermore, when using single-point or multi-point simultaneous injection, the resin flow front converges in the center of the mold cavity or in certain areas, causing thickness deviation and optical distortion in those areas. It is difficult to ensure the consistency of overall transmittance, resulting in a low yield. Summary of the Invention
[0003] This invention provides a gas-liquid separation RTM molding process for high-transmittance composite materials, which can effectively solve the problems mentioned in the background art. Traditional RTM processes use a single resin injection port design, which easily traps air from the mold cavity into the resin flow front during resin propulsion, resulting in the formation of microbubbles inside the product. This seriously affects the transmittance and optical uniformity. Furthermore, when using single-point or multi-point simultaneous injection, the resin flow front converges in the center of the mold cavity or in certain areas, causing thickness deviation and optical distortion in those areas. It is difficult to ensure the consistency of overall transmittance, resulting in a low yield.
[0004] To achieve the above objectives, the present invention provides the following technical solution: a gas-liquid separation RTM molding process for high-transmittance composite materials, comprising the following process flow: Step S1, mold preparation and gas-liquid channel design; Step S2: Fiber preform laying and gas-liquid medium integration; Step S3: Mold closing and mold airtightness test; Step S4: Vacuum pre-evacuation and gas passage pre-pressurization; Step S5, resin preparation and liquid channel pretreatment; Step S6, gas-liquid separation graded dispensing; Step S7, stepped heating and curing; Step S8: Demolding and post-processing of the product.
[0005] According to the above technical solution, in step S1, a molding die with independent gas and liquid passages is designed and processed according to the shape, size and light transmittance requirements of the product to be processed. Among them, the gas passage is laid out along the mold closing surface or the pre-set guiding medium inside the preform to remove air from the mold cavity before injection and to provide a stable gas pressure gradient during the injection process. The liquid passage is uniformly laid out along the thickness or width of the product to transport resin to the fiber preform.
[0006] According to the above technical solution, the gas passage adopts a microporous structure or a drainage mesh structure and is arranged on at least one side of the preform; The liquid passage adopts a trough-type, flow channel-type, or porous medium-type structure, and is laid out independently of the gas passage.
[0007] According to the above technical solution, in step S2, the high-transparency fiber reinforcement is evenly laid in the lower mold of the molding mold according to the designed number of layers and layup angle, wherein the fiber reinforcement includes E-glass fiber mat, high-transparency polyester fiber mesh, and aramid fiber fabric. Meanwhile, after the fiber reinforcement is laid, a gas-liquid separation medium is embedded in a specific position of the preform, so that the gas passage and the resin passage are spatially separated and functionally coordinated. The gas-liquid separation medium includes a microporous PTFE membrane, a three-dimensional spacer fabric, and a drainage mesh.
[0008] According to the above technical solution, in step S3, after the mold is closed, the mold needs to be tested for air tightness. In the specific test process, the vacuum is drawn through the gas passage to a set vacuum level, specifically -0.085MPa to -0.095MPa, and held for 5-15 minutes after vacuuming. During the holding time, the rate of decrease in vacuum is observed to determine whether the sealing performance of the mold and air circuit system meets the process requirements. After meeting the process requirements, the subsequent process flow can proceed. Otherwise, it is necessary to conduct further airtightness checks on the molding die and redesign the molding die.
[0009] According to the above technical solution, in step S4, after the airtightness of the molding die is qualified, the gas passage is continuously evacuated to reduce the air pressure in the mold cavity to a set value. At the same time, a small amount of inert gas or dry air is introduced into the far end of the mold cavity through the gas passage to establish a stable pressure gradient from the injection port to the vent.
[0010] According to the above technical solution, in step S5, the high-transparency resin matrix, curing agent, and accelerator are uniformly mixed according to the design ratio of the product to be processed, and then degassed. The high-transparency resin matrix includes transparent epoxy resin, transparent unsaturated polyester resin, and transparent polyurethane resin. After mixing and degassing, a small amount of resin is injected into the area near the injection port of the preform through the liquid channel to pre-wet the preform in that area.
[0011] According to the above technical solution, S6 specifically adopts a staged injection strategy of gas leading edge propulsion + resin trailing edge follow-up. The injection pressure gradient of the staged injection is adjusted in real time by the PLC control system. The injection process includes the following stages: Phase 1: Through continuous vacuuming and low-pressure propulsion via the gas passage, the gas forms a uniform and stable gas front in the preform and is propelled from the injection port to the exhaust port. Second stage: Resin is injected into the air front through the liquid channel at a set flow rate and pressure gradient, so that after the resin is injected, the fibers are quickly impregnated in the vacuumed preform, forming a propulsion front with clear liquid-gas separation. The third stage: When the air front reaches the vicinity of the exhaust port, switch to low-pressure injection or pressure holding impregnation mode to compress the residual gas and discharge it from the mold cavity through the exhaust port. Fourth stage: After the mold cavity is completely filled, the pressure holding stage begins. A constant pressure of 0.1-0.3 MPa is applied through the liquid passage, and the vacuum continues through the gas passage until all residual gas and volatiles are completely discharged.
[0012] According to the above technical solution, in step S7, the product to be processed is cured by step heating through a mold heating system or an ambient heating system according to the curing characteristics of the resin matrix. Specifically, it includes a low temperature pre-curing stage, a medium temperature curing stage and a high temperature post-curing stage. Through the three-stage step heating curing, the product to be processed is completely cured and formed. During the low-temperature pre-curing stage, the curing temperature is controlled at 40-60℃, and the curing time is maintained at 1-3 hours. During the medium-temperature curing stage, control the curing temperature at 70-90℃ and maintain the curing time for 2-4 hours; During the high-temperature post-curing stage, control the curing temperature at 100-120℃ and maintain the curing time at 1-2 hours.
[0013] According to the above technical solution, in step S8, after the product has completely cooled to the demolding temperature, the mold is opened and the product is taken out. Then, according to the actual processing needs, the product is subjected to post-processing steps, which specifically include edge trimming, polishing, cleaning, and coating, and finally a high-transmittance composite material product is obtained.
[0014] Compared with the prior art, the beneficial effects of the present invention are as follows: This invention improves the traditional RTM process by setting independent gas and liquid channels inside the molding die, which involves the injection of gas and resin liquid sharing the same channel. Instead, it sets independent gas and liquid channels inside the mold, and separately evacuates the gas channels and injects resin into the liquid channels in stages before injection. This achieves spatial and functional separation and control of gas and liquid, thereby obtaining composite material products with high light transmittance and high optical uniformity. Simultaneously, a graded injection strategy of gas leading edge propulsion + resin trailing edge follow-up is adopted, which eliminates the problems of flow front convergence and bubble entrainment in the traditional RTM process, and ensures that the prepared high-transmittance composite material products have the advantages of high transmittance, good optical uniformity and low defect rate. Attached Figure Description
[0015] The accompanying drawings are provided to further illustrate the invention and form part of the specification. They are used together with the embodiments of the invention to explain the invention and do not constitute a limitation thereof.
[0016] In the attached diagram: Figure 1 This is a flowchart of the RTM molding process of the present invention. Detailed Implementation
[0017] The preferred embodiments of the present invention will be described below with reference to the accompanying drawings. It should be understood that the preferred embodiments described herein are for illustration and explanation only and are not intended to limit the present invention.
[0018] Example: Figure 1 As shown, this invention provides a technical solution: a gas-liquid separation RTM molding process for high-transmittance composite materials. This molding process is suitable for molding high-transmittance products with planar, curved, hyperboloidal, and complex irregular shapes, and includes the following process flow: Step S1, mold preparation and gas-liquid channel design; Step S2: Fiber preform laying and gas-liquid medium integration; Step S3: Mold closing and mold airtightness test; Step S4: Vacuum pre-evacuation and gas passage pre-pressurization; Step S5, resin preparation and liquid channel pretreatment; Step S6, gas-liquid separation graded dispensing; Step S7, stepped heating and curing; Step S8: Demolding and post-processing of the product.
[0019] Based on the above technical solution, S1, according to the shape, size and light transmittance requirements of the product to be processed, design and process a molding die with independent gas passages and liquid passages. The gas passage is laid out along the pre-set guiding medium inside the preform to remove air from the mold cavity before injection and to provide a stable gas pressure gradient during the injection process. The liquid passage is evenly distributed along the thickness of the product and is used to transport resin to the fiber preform.
[0020] Based on the above technical solution, the gas passage adopts a microporous structure and is arranged on at least one side of the preform; The liquid passage adopts a porous media structure and is laid out independently of the gas passage.
[0021] Based on the above technical solution, S2, the high-transmittance fiber reinforcement is evenly laid in the lower mold of the molding mold according to the designed number of layers and layup angle, wherein the fiber reinforcement includes E-glass fiber mat, high-transmittance polyester fiber mesh, and aramid fiber fabric. Meanwhile, after the fiber reinforcement is laid, a gas-liquid separation medium is embedded in a specific position of the preform, so that the gas passage and the resin passage are spatially separated and functionally coordinated. The gas-liquid separation medium includes a microporous PTFE membrane, a three-dimensional spacer fabric, and a drainage mesh.
[0022] Based on the above technical solution, S3, after the mold is closed, it is necessary to test the airtightness of the mold. In the specific test process, the vacuum is drawn to a set vacuum level through the gas passage, specifically -0.090MPa, and held for 10 minutes after vacuuming. During the holding time, the rate of decrease in vacuum is observed to determine whether the sealing performance of the mold and air circuit system meets the process requirements. After meeting the process requirements, the subsequent process flow can proceed. Otherwise, it is necessary to conduct further airtightness checks on the molding die and redesign the molding die to ensure that the mold airtightness meets the process requirements.
[0023] Based on the above technical solution, S4, after the airtightness of the molding die is qualified, the gas passage is continuously evacuated to reduce the air pressure in the mold cavity to a set value. At the same time, a small amount of inert gas is introduced into the far end of the mold cavity through the gas passage to establish a stable pressure gradient from the injection port to the vent. Nitrogen is selected as the inert gas.
[0024] Based on the above technical solution, S5, the high-transparency resin matrix, curing agent, and accelerator are uniformly mixed according to the design ratio of the product to be processed, and degassing treatment is performed. The high-transparency resin matrix includes transparent epoxy resin, transparent unsaturated polyester resin, and transparent polyurethane resin. After mixing and degassing, a small amount of resin is injected into the area near the injection port of the preform through the liquid channel to pre-wet the preform in this area and avoid the formation of dry spots during the actual injection.
[0025] Based on the above technical solution, S6 specifically adopts a staged injection strategy of gas leading edge propulsion + resin trailing edge follow-up. The injection pressure gradient of the staged injection is adjusted in real time by the PLC control system. The specific injection process includes the following stages: Phase 1: Through continuous vacuuming and low-pressure propulsion via the gas passage, the gas forms a uniform and stable gas front in the preform and is propelled from the injection port to the exhaust port. Second stage: Resin is injected into the air front through the liquid channel at a set flow rate and pressure gradient, so that after the resin is injected, the fibers are quickly impregnated in the vacuumed preform, forming a propulsion front with clear liquid-gas separation. The third stage: When the air front reaches the vicinity of the exhaust port, switch to low-pressure injection or pressure holding impregnation mode to compress the residual gas and discharge it from the mold cavity through the exhaust port. Fourth stage: After the mold cavity is completely filled, the pressure holding stage begins. A constant pressure of 0.2 MPa is applied through the liquid passage, and the vacuum continues through the gas passage until all residual gas and volatiles are completely discharged.
[0026] Based on the above technical solution, S7, according to the curing characteristics of the resin matrix, the product to be processed is cured by step heating through a mold heating system or an ambient heating system. Specifically, it includes a low temperature pre-curing stage, a medium temperature curing stage, and a high temperature post-curing stage. Through the three stages of step heating and curing, the product to be processed is completely cured and formed. During the low-temperature pre-curing stage, the curing temperature is controlled at 50℃ and the curing time is maintained at 2 hours. During the medium-temperature curing stage, the curing temperature is controlled at 80℃ and the curing time is maintained at 3 hours. During the high-temperature post-curing stage, the curing temperature is controlled at 110℃ and the curing time is maintained at 1.5h.
[0027] Based on the above technical solution, in step S8, after the product has completely cooled to the demolding temperature, the mold is opened and the product is taken out. Then, according to the actual processing needs, the product is subjected to post-processing steps, including edge trimming, polishing, cleaning, and coating, to finally obtain a high-transmittance composite material product.
[0028] Example 1: Molding and processing of high-transmittance shells for wind turbine blades, including the following steps: Based on the curvature and size requirements of the blade shell, the male and female molds are designed and manufactured. The mold interior is equipped with independent gas and liquid passages along the curved surface. The gas passage is arranged on one side along the thickness of the shell, and the liquid passage is arranged on the other side of the shell. Gas injection port, gas discharge port, resin injection port, and resin overflow port are reserved on the mold. E-glass fiber continuous mat was selected as the fiber reinforcement and laid in the lower mold in a layup sequence of 0°, 45°, -45°, and 90°. The total fiber areal density was 1200 g / m². 2 ; A three-dimensional spacer fabric is attached to the upper surface of the preform as a gas passage drainage medium, and a microporous drainage mesh is attached to the lower surface as a liquid passage drainage medium. After the mold is closed, a vacuum is drawn to -0.095 MPa through the gas passage and maintained for 10 minutes. The airtightness is qualified when the vacuum degree drops by less than 0.005 MPa. Pre-degassed transparent epoxy resin with a viscosity of 250 mPa·s, 25°C, injection pressure of 0.15 MPa, and injection time of 35 min is injected through a liquid channel. Simultaneously, a vacuum is continuously drawn through a gas channel to ensure that the gas is stably discharged from the gas outlet. After the glue injection is completed, the pressure holding stage begins. The liquid passage is held at 0.2 MPa for 1 hour, while the gas passage is continuously evacuated until no visible bubbles are released. The specific steps for entering the stepped curing process are as follows: Low-temperature pre-curing stage: temperature 60℃, time 2h; Medium-temperature curing stage: temperature 80℃, time 3 hours; High-temperature post-curing stage: temperature 110℃, time 2h; The mold is opened when the temperature is cooled to below 40°C to obtain a high-transmittance wind turbine blade shell; The prepared shell has a light transmittance of ≥88%, a haze of ≤1.5%, and no visible bubbles, cracks, or flow marks. Example 2: Molding and processing for building skylights, differing from Example 1 in that: The fiber reinforcement is made of high-transmittance polyester fiber fabric, with 6 layers laid up; The resin used is a transparent unsaturated polyester resin with a viscosity of 180 mPa·s and a temperature of 25℃. Gas passages are located on the upper and lower sides of the preform, while liquid passages are located in the middle of the preform. The injection pressure gradient is controlled by a three-stage PLC: the first stage is 0.08MPa, the second stage is 0.15MPa, and the third stage is 0.25MPa. The prepared light-transmitting dome has a light transmittance of ≥90%, a haze of ≤1.0%, and no appearance defects; Example 3: The molding and processing of high-transmittance protective lenses for face shields includes the following: The fiber reinforcement is made of aramid fiber fabric and a transparent polyurethane resin matrix; Gas passages and liquid passages are alternately arranged inside the preform, in a sandwich distribution; After the adhesive is applied, it is pre-cured at 60℃ for 1 hour and then cured at room temperature for 24 hours. The prepared protective lenses have a light transmittance of ≥92%, a haze of ≤0.8%, and excellent impact resistance.
[0029] Finally, it should be noted that the above descriptions are merely preferred embodiments of the present invention and are not intended to limit the present invention. Although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art can still modify the technical solutions described in the foregoing embodiments or make equivalent substitutions for some of the technical features. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the protection scope of the present invention.
Claims
1. A gas-liquid separation RTM molding process for high light transmission composites, characterized in that: The process flow includes the following: Step S1, mold preparation and gas-liquid channel design; Step S2: Fiber preform laying and gas-liquid medium integration; Step S3: Mold closing and mold airtightness test; Step S4: Vacuum pre-evacuation and gas passage pre-pressurization; Step S5, resin preparation and liquid channel pretreatment; Step S6, gas-liquid separation graded dispensing; Step S7: Step heating and curing. Step S8: Demolding and post-processing of the product.
2. The gas-liquid separation RTM molding process for high-transmittance composite materials according to claim 1, characterized in that: S1 involves designing and processing a molding die with independent gas and liquid passages based on the shape, size, and light transmittance requirements of the product to be processed. Among them, the gas passage is laid out along the mold closing surface or the pre-set guiding medium inside the preform to remove air from the mold cavity before injection and to provide a stable gas pressure gradient during the injection process. The liquid passage is uniformly laid out along the thickness or width of the product to transport resin to the fiber preform.
3. The gas-liquid separation RTM molding process for high-transmittance composite materials according to claim 2, characterized in that: The gas passage adopts a microporous structure or a drainage mesh structure and is arranged on at least one side of the preform; The liquid passage adopts a trough-type, flow channel-type, or porous medium-type structure, and is laid out independently of the gas passage.
4. The gas-liquid separation RTM molding process for high-transmittance composite materials according to claim 1, characterized in that: In step S2, the high-transmittance fiber reinforcement is evenly laid in the lower mold of the molding mold according to the designed number of layers and layup angle. The fiber reinforcement includes E-glass fiber mat, high-transmittance polyester fiber mesh, and aramid fiber fabric. Meanwhile, after the fiber reinforcement is laid, a gas-liquid separation medium is embedded in a specific position of the preform, so that the gas passage and the resin passage are spatially separated and functionally coordinated. The gas-liquid separation medium includes a microporous PTFE membrane, a three-dimensional spacer fabric, and a drainage mesh.
5. The gas-liquid separation RTM molding process for high-transmittance composite materials according to claim 1, characterized in that: In step S3, after the mold is closed, the mold needs to be tested for air tightness. In the specific test process, the vacuum is drawn through the gas passage to a set vacuum level, specifically -0.085MPa to -0.095MPa, and held for 5-15 minutes after vacuuming. During the holding time, the rate of decrease in vacuum is observed to determine whether the sealing performance of the mold and air circuit system meets the process requirements. After meeting the process requirements, the subsequent process flow can proceed. Otherwise, it is necessary to conduct further airtightness checks on the molding die and redesign the molding die.
6. The gas-liquid separation RTM molding process for high-transmittance composite materials according to claim 5, characterized in that: In step S4, after the airtightness of the molding die is qualified, the gas passage is continuously evacuated to reduce the air pressure in the mold cavity to a set value. At the same time, a small amount of inert gas or dry air is introduced into the far end of the mold cavity through the gas passage to establish a stable pressure gradient from the injection port to the vent.
7. The gas-liquid separation RTM molding process for high-transmittance composite materials according to claim 1, characterized in that: In step S5, the high-transparency resin matrix, curing agent, and accelerator are uniformly mixed according to the design ratio of the product to be processed, and then degassed. The high-transparency resin matrix includes transparent epoxy resin, transparent unsaturated polyester resin, and transparent polyurethane resin. After mixing and degassing, a small amount of resin is injected into the area near the injection port of the preform through the liquid channel to pre-wet the preform in that area.
8. The gas-liquid separation RTM molding process for high-transmittance composite materials according to claim 1, characterized in that: Specifically, S6 employs a staged injection strategy of gas leading-edge propulsion + resin trailing-edge follow-up. The injection pressure gradient of the staged injection is adjusted in real time by a PLC control system. The injection process includes the following stages: Phase 1: Through continuous vacuuming and low-pressure propulsion via the gas passage, the gas forms a uniform and stable gas front in the preform and is propelled from the injection port to the exhaust port. Second stage: Resin is injected into the air front through the liquid channel at a set flow rate and pressure gradient, so that after the resin is injected, the fibers are quickly impregnated in the vacuumed preform, forming a propulsion front with clear liquid-gas separation. The third stage: When the air front reaches the vicinity of the exhaust port, switch to low-pressure injection or pressure holding impregnation mode to compress the residual gas and discharge it from the mold cavity through the exhaust port. Fourth stage: After the mold cavity is completely filled, the pressure holding stage begins. A constant pressure of 0.1-0.3 MPa is applied through the liquid passage, and the vacuum continues through the gas passage until all residual gas and volatiles are completely discharged.
9. The gas-liquid separation RTM molding process for high-transmittance composite materials according to claim 1, characterized in that: S7, according to the curing characteristics of the resin matrix, uses a mold heating system or an ambient heating system to perform step-by-step temperature curing on the product to be processed. Specifically, it includes a low-temperature pre-curing stage, a medium-temperature curing stage, and a high-temperature post-curing stage. Through the three-stage step-by-step temperature curing, the product to be processed is completely cured and formed. During the low-temperature pre-curing stage, the curing temperature is controlled at 40-60℃, and the curing time is maintained at 1-3 hours. During the medium-temperature curing stage, control the curing temperature at 70-90℃ and maintain the curing time for 2-4 hours; During the high-temperature post-curing stage, control the curing temperature at 100-120℃ and maintain the curing time at 1-2 hours.
10. The gas-liquid separation RTM molding process for high-transmittance composite materials according to claim 1, characterized in that: In step S8, after the product has completely cooled to the demolding temperature, the mold is opened and the product is taken out. Then, according to the actual processing needs, the product is subjected to post-processing steps, including edge trimming, polishing, cleaning, and coating, to finally obtain a high-transmittance composite material product.