A lightweight structure for an environmentally friendly paper packaging container
By employing a composite structure of nanocellulose-coated columnar protrusion array, nonlinear design of corrugated core layer, and discontinuous laser seam of crease line in paper packaging containers, the problems of moisture and oil resistance, structural strength, and crease fatigue in paper packaging containers under the conditions of lightweighting and biodegradability are solved, achieving high-efficiency barrier performance and creep resistance.
Patent Information
- Application Number
- CN202611199175.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-09
- Publication Date
- 2026-11-17
AI Technical Summary
While existing paper packaging containers are lightweight and fully biodegradable, they cannot simultaneously solve the problems of insufficient moisture and oil barrier performance, creep decay of structural strength, and stress concentration at creases leading to barrier layer damage and fatigue failure.
A columnar protrusion array structure was constructed on the surface of the nanocellulose coating, the flute height and flute density of the corrugated core layer were designed to be nonlinearly gradient along the container area, and a composite structure of discontinuous wavy laser micro-slits at the crease line and flexible thermoplastic starch-based elastomer was constructed. The pulp fiber content and stress dispersion were optimized by combining finite element simulation and gradient parameter generation methods.
Achieving moisture and oil resistance without fluorine or thick plastic film improves the container's creep stability and fatigue life at creases in high humidity environments, while preventing continuous fiber breakage and localized damage to the barrier layer.
Smart Images

Figure CN123104152A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of paper packaging container technology, specifically to a lightweight structure for an environmentally friendly paper packaging container. Background Technology
[0002] Paper packaging containers are typically made of a composite of face paper, corrugated core layer and liner paper. The corrugated structure provides compression support, and the folding parts of the container are creased to form hinge lines. The inner wall is also reinforced with a moisture-proof and oil-proof functional layer to meet the needs of holding oily and watery materials.
[0003] In the prior art, one solution achieves moisture and oil resistance by attaching a perfluorinated / polyfluoroalkyl substance coating or a composite plastic film with a thickness greater than 15 micrometers to the inner wall of the paper base. However, such coatings or films face restrictions on being banned due to their environmental durability, and they are tightly bonded to the paper base and difficult to separate, causing the container to lose its recyclability and degradability.
[0004] Another option uses a uniform flute shape, flute height and flute density design for the corrugated core layer along the entire container. It does not distinguish the actual stress distribution differences in different parts. After the container is made lightweight and thinned, it is placed in a high humidity environment. The high stress concentration areas lack targeted reinforcement. Long-term stacking is prone to plastic creep collapse in weak parts such as bottom corners and columns.
[0005] Another approach is to use an indentation die to create a continuous and uninterrupted extrusion groove at the fold. This continuous indentation causes the fibers at the fold to be directly crushed, and the barrier continuity of the moisture-proof and oil-proof functional layer is simultaneously destroyed. Furthermore, when the container is frequently opened and closed or subjected to material vibration, the stress is continuously concentrated on the same fracture path, which can easily lead to fatigue crack propagation and even fold cracking.
[0006] Therefore, how to simultaneously address the issues of moisture and oil resistance, structural strength creep, and crease fatigue failure while ensuring that paper packaging containers are lightweight and fully biodegradable has become an urgent technical problem to be solved in this field. Summary of the Invention
[0007] The technical problem to be solved by this invention is that, under the premise of achieving lightweight and complete biodegradability, existing paper packaging containers are difficult to solve the problems of insufficient moisture and oil barrier performance, creep attenuation of structural strength under humid and hot environments, and damage and fatigue failure of the barrier layer due to stress concentration at creases, without using per- or polyfluoroalkyl substances and non-degradable thick plastic film composite layers.
[0008] To solve the above technical problems, the present invention provides a lightweight structure for an environmentally friendly paper packaging container, including a face paper layer, an inner paper layer, and a corrugated core layer disposed between the face paper layer and the inner paper layer. The inner paper layer is provided with a barrier coating on the side facing the inside of the container, and the container is provided with crease lines for folding.
[0009] The barrier coating is a nanocellulose coating. The nanocellulose coating is pressed into the surface facing the inside of the container to form a plurality of columnar protrusions arranged in an array. A recessed area is formed between adjacent columnar protrusions. The recessed area is used to trap air to reduce the actual contact area between the droplets and the nanocellulose coating.
[0010] The corrugated core layer has a lower corrugated height and density in the container sidewall region than in the container bottom corner and column regions, and the corrugated core layer has a continuously nonlinearly increasing corrugated height and density along the direction from the container sidewall region to the container bottom corner and column region.
[0011] The crease line is provided with multiple discontinuous laser micro-slits arranged in a wavy pattern along the crease line, and fiber connecting bridges are retained between adjacent discontinuous laser micro-slits. The discontinuous laser micro-slits are filled with flexible thermoplastic starch-based elastomer.
[0012] This invention also provides a method for generating gradient parameters of the lightweight structure of the above-mentioned environmentally friendly paper packaging container, used to determine the flute height and flute density of the corrugated core layer. The method obtains the local stress distribution by establishing a three-dimensional geometric model of the container and performing finite element simulation, divides the container wall into sections and calculates the normalized stress coefficient of each section, calculates the flute height and flute density parameters corresponding to each section according to a preset nonlinear gradient function and generates a section processing parameter table, drives the section pressing roller unit to perform section pressing and forming, and then iteratively adjusts the shape parameters of the gradient function through wet heat creep simulation until the deformation of each section meets the design requirements.
[0013] Compared with the prior art, the beneficial effects of the present invention by adopting the above technical solution are as follows:
[0014] 1. This invention reduces the contact area and capillary adsorption path at the solid-liquid interface by constructing a columnar protrusion array structure on the surface of the nanocellulose coating, achieving moisture and oil resistance under fluorine-free and thick plastic film-free conditions, and avoiding the non-recyclable degradation problem caused by the composite structure of fluorine-containing coating and thick plastic film.
[0015] 2. This invention achieves lightweighting by using a continuous nonlinear gradient design of the flute height and flute density of the corrugated core layer from the high-stress region to the low-stress region of the container, which reduces the amount of pulp fiber used in the side wall region of the container by 15% to 20% compared to a homogeneous corrugated core layer, thereby improving the anti-creep stacking stability of the container in a high-humidity environment.
[0016] 3. This invention utilizes a composite structure of discontinuous wavy laser micro-slits at the crease line and flexible thermoplastic starch-based elastomer to disperse and release folding stress along multiple fiber connecting bridges, thereby avoiding continuous fiber breakage and local damage to the barrier layer, and improving the fatigue life and dynamic barrier performance of the crease area. Attached Figure Description
[0017] Figure 1 This is a flowchart illustrating the overall production process of the environmentally friendly paper container in this embodiment of the invention.
[0018] Figure 2 This is a flowchart illustrating the calculation process for generating gradient parameters of the corrugated core layer in an embodiment of the present invention. Detailed Implementation
[0019] The following is in conjunction with the appendix Figure 1-2 The specific embodiments of the present invention will be further described below. It should be noted that the description of these embodiments is for the purpose of helping to understand the present invention, but does not constitute a limitation of the present invention.
[0020] This embodiment provides a lightweight structure for an environmentally friendly paper packaging container. The container is a rectangular folding cardboard box, including a top cover, side walls, and bottom corners and pillars formed by the turning of the side walls. The container wall consists of a face paper layer, a corrugated core layer, and an inner paper layer from the outside to the inside. A nano-cellulose coating is provided on the side of the inner paper layer facing the inside of the container. Crease lines are provided on the edges of the container and the folded edges of the lid.
[0021] The nanocellulose coating facing the inside of the container is pressed into an array of columnar protrusions using a hot press mold. Recessed areas are formed between adjacent columnar protrusions. In this embodiment, the column height is 20 micrometers, the column spacing is 40 micrometers, and the column top diameter is 15 micrometers. When a droplet falls onto the surface of this texture, it only contacts the top surface of the columnar protrusions. The air layer trapped in the recessed areas forms a solid-air composite contact, blocking continuous capillary channels. The wetting properties of this hydrophobic texture can be designed using the following formula for structural parameters:
[0022] ;
[0023] In the formula, The apparent contact angle of the columnar array composite surface to the droplet;
[0024] The intrinsic contact angle of the droplet on the flat surface of the nanocellulose coating without pressing is determined by the surface energy of the coating material itself.
[0025] This is the ratio of the actual contact area between the droplet and the solid surface at the top of the column to the theoretical total contact area, i.e., the solid fraction.
[0026] This represents the proportion of the area occupied by the concave region, i.e., the gas phase fraction. and The sum is 1. By reducing the diameter of the column tops of the columnar protrusions and increasing the column spacing, the intrinsic contact angle of the coating can be increased without increasing the value of the column. Under the premise of making the apparent contact angle The size increases, thus achieving moisture and oil resistance under fluorine-free conditions.
[0027] The corrugated core layer is configured with a low flute height and low flute density in the container side wall area, and a high flute height and high flute density in the container bottom corner and column areas. The transition between the two is continuous along the extension direction of the container wall, without any abrupt changes. In this embodiment, the flute height of the corrugated structure in the side wall area is 3 mm, and the flute height of the corrugated structure in the bottom corner and column areas is 5 mm. The amount of pulp fiber used in the container side wall area is reduced by 18% compared to a homogeneous corrugated core layer with the same flute height and flute density.
[0028] The flute height and flute density parameters of the corrugated core layer are determined by the following gradient parameter generation method: First, a three-dimensional geometric model of the container is established. Boundary conditions and load conditions are set according to the container stacking load, drop impact and transportation vibration. Local stress distribution data at various points on the container wall are obtained through finite element simulation.
[0029] The container wall was then divided into multiple rectangular partition units. The stress peak values in each partition unit were extracted and normalized to obtain the normalized stress coefficients of each partition unit.
[0030] Next, according to the preset gradient ridge height function and gradient ridge density function, the ridge height and ridge density parameters corresponding to each partition unit are calculated. The gradient ridge height function and gradient ridge density function are specifically expressed as follows:
[0031] ;
[0032] ;
[0033] In the formula, For any point on the container wall The corresponding corrugated height;
[0034] This represents the corrugation density at that location point, i.e., the number of corrugation peaks per unit length.
[0035] , These are the pre-set lower and upper limits of the corrugated height, corresponding to the structural limits of the container sidewall area, bottom corner, and column area;
[0036] , These are the lower and upper limits of the corrugated density, respectively.
[0037] Location point The local stress amplitude obtained through finite element simulation;
[0038] , These are the lower and upper limits of the stress values for all zones of the container, respectively, used to normalize local stress.
[0039] A shape parameter greater than 0 is used to control the degree of gradual nonlinearity of the rib height and rib density along the stress variation direction. In this embodiment... The value is 1.5.
[0040] The parameters of flute height and flute density corresponding to each partition unit are summarized to generate a partition processing parameter table. The partition pressure roller unit is driven to perform partition pressing and forming. The partition pressure roller unit is divided into multiple pressure roller units that can independently adjust the pressure and tooth depth along the container unfolding direction. The corresponding corrugated structure is pressed out partition by partition. The corrugated core layer after forming is subjected to wet heat creep simulation verification to simulate long-term stacking conditions under high humidity environment and determine whether the deformation of each partition exceeds the preset threshold.
[0041] If the deformation of any partition exceeds the preset threshold, adjust the shape parameters of the gradient ridge height function and the gradient ridge density function. And recalculate until the deformation of all zones meets the design requirements.
[0042] Multiple discontinuous laser micro-slits are arranged in a wavy pattern along the crease line. These discontinuous laser micro-slits penetrate the paper base layer at the crease line along the thickness direction of the container wall. Fiber connecting bridges are maintained between adjacent discontinuous laser micro-slits. In this embodiment, the length of a single discontinuous laser micro-slit is 2 mm, the spacing between adjacent discontinuous laser micro-slits is 0.5 mm, and the width of the fiber connecting bridge is 0.3 mm. The discontinuous laser micro-slits are filled with a flexible thermoplastic starch-based elastomer. This elastomer undergoes localized micro-tensile deformation synchronously with the fiber connecting bridges when the container is folded. The effect of this structure on the dispersion and release of folding stress can be explained by the following formula:
[0043] ;
[0044] In the formula, This represents the local strain actually borne by a single fiber-connected bridge when folded at the crease.
[0045] This is the theoretical total bending strain corresponding to the overall folding angle of the crease;
[0046] This refers to the number of discontinuous laser micro-slits distributed within a unit length of the crease. The larger the value, the more fiber-connected bridges participate in sharing the strain;
[0047] The stress redistribution factor is determined by the wavy geometry of the discontinuous laser micro-slits and the elastic modulus of the flexible thermoplastic starch-based elastomer. The flexible buffering effect of the elastomer can reduce... The value is selected to reduce the actual strain borne by a single fiber connecting bridge. Compared with the failure mode of traditional continuous indentation and extrusion, this embodiment has been verified by indentation fatigue test. No continuous fiber breakage or local damage to the barrier layer occurred at the indentation site under repeated folding conditions.
[0048] The manufacturing process of the container in this embodiment includes: preparing raw paper, selecting face paper, inner paper and corrugated base paper;
[0049] The aforementioned gradient parameter generation method is used to drive the partitioned pressure roller unit to perform partitioned gradient corrugation forming, thereby obtaining a corrugated core layer.
[0050] The face paper layer, inner paper layer and corrugated core layer are laminated together;
[0051] A nano-cellulose coating is applied to the inner wall of the inner paper layer;
[0052] A columnar protrusion structure was pressed onto the surface of the nanocellulose coating using a hot press mold to form a micro-embossed biomimetic hydrophobic texture.
[0053] Laser discontinuous micro-slit processing is performed at the crease line to form a bridge connecting the discontinuous laser micro-slit and the fiber.
[0054] A flexible thermoplastic starch-based elastomer is filled and cured within discontinuous laser micro-grooves;
[0055] The container is die-cut into shape;
[0056] The molded containers are tested for moisture and oil resistance, stacking strength, and crease fatigue to obtain the finished packaging containers.
[0057] In other embodiments, the micro-embossed biomimetic hydrophobic texture can also be replaced by a sharkskin-inspired groove array texture, which reduces the actual contact area between the droplets and the solid surface through the directional arrangement of the micro-groove structure.
[0058] The corrugated core layer can also be replaced with a biodegradable paper-based honeycomb core layer structure. The aforementioned gradient parameter generation method is used to nonlinearly and gradually design the honeycomb pore size and pore wall thickness along the high-stress region to the low-stress region of the container. This can also achieve a spatially differentiated allocation of material usage. The face paper layer, inner paper layer, corrugated core layer, nanocellulose coating, and flexible thermoplastic starch-based elastomer used in the above container are all biodegradable materials. The container does not contain perfluorinated / polyfluoroalkyl substances coatings, nor does it contain plastic film composite layers with a thickness greater than 15 micrometers.
[0059] Although the present invention has been disclosed above with reference to preferred embodiments, it is not intended to limit the present invention. Any person skilled in the art can make possible changes and modifications without departing from the spirit and scope of the present invention. Therefore, any modifications, equivalent changes and alterations made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention shall fall within the protection scope defined by the claims of the present invention.
Claims
1. A lightweight structure for an environmentally friendly paper packaging container, comprising a face paper layer, an inner paper layer, and a corrugated core layer disposed between the face paper layer and the inner paper layer, wherein the inner paper layer has a barrier coating on the side facing the inside of the container, and the container has crease lines for folding, characterized in that: The barrier coating is a nanocellulose coating. The nanocellulose coating is pressed into the surface facing the inside of the container to form a plurality of columnar protrusions arranged in an array. A recessed area is formed between adjacent columnar protrusions. The recessed area is used to trap air to reduce the actual contact area between the droplets and the nanocellulose coating. The corrugated core layer has a lower corrugated height and density in the container sidewall region than in the container bottom corner and column regions, and the corrugated core layer has a continuously nonlinearly increasing corrugated height and density along the direction from the container sidewall region to the container bottom corner and column region. The crease line is set on the transition path between the corrugation height and the corrugation density of the corrugated core layer. The arrangement density of the discontinuous laser micro-slits at the crease line changes nonlinearly along the transition path in sync with the gradient of the corrugation height of the corrugated core layer. Fiber connecting bridges are retained between adjacent discontinuous laser micro-slits. The discontinuous laser micro-slits are filled with flexible thermoplastic starch-based elastomer.
2. The lightweight structure of the environmentally friendly paper packaging container according to claim 1, characterized in that, The columnar protrusion structure has a column height of 1 micrometer to 50 micrometers, a column spacing of 2 micrometers to 80 micrometers, and a column top diameter of 1 micrometer to 30 micrometers. The top surface of the columnar protrusion structure is in contact with the droplet, and a solid-gas composite contact is formed between the recessed area and the droplet.
3. The lightweight structure of the environmentally friendly paper packaging container according to claim 1, characterized in that, The amount of pulp fiber used in the corrugated core layer in the container sidewall area is reduced by 15% to 20% compared to a homogeneous corrugated core layer with the same flute height and flute density in all parts of the container.
4. The lightweight structure of the environmentally friendly paper packaging container according to claim 1, characterized in that, The discontinuous laser micro-slits penetrate the paper substrate along the thickness direction of the container wall at the crease line, and the width of the fiber connecting bridge between adjacent discontinuous laser micro-slits is 0.1 mm to 0.5 mm.
5. The lightweight structure of the environmentally friendly paper packaging container according to any one of claims 1 to 4, characterized in that, The container does not contain a coating of perfluorinated / polyfluoroalkyl substances, nor does it contain a plastic film composite layer with a thickness greater than 15 micrometers. The face paper layer, the inner paper layer, the corrugated core layer, the nanocellulose coating, and the flexible thermoplastic starch-based elastomer are all biodegradable materials.
6. A method for generating gradient parameters of a lightweight structure for an environmentally friendly paper packaging container, used to determine the flute height and flute density of the corrugated core layer as described in claim 1, characterized in that, include: A three-dimensional geometric model of the container is established. Boundary conditions and load conditions are set according to the container's stacking load, drop impact and transportation vibration. Local stress distribution data at various points on the container wall are obtained through finite element simulation. The container wall is divided into multiple partition units, the stress peak value in each partition unit is extracted, and the stress peak value of all partition units is normalized to obtain the normalized stress coefficient of each partition unit. Based on the normalized stress coefficient of each partition unit, the rib height parameter and rib density parameter corresponding to each partition unit are calculated according to the preset gradient rib height function and gradient rib density function. The gradient rib height function and the gradient rib density function are both nonlinear functions that monotonically increase with the normalized stress coefficient. The flute height and flute density parameters corresponding to each partition unit are summarized to generate a partition processing parameter table. Based on the partition processing parameter table, the partition pressure roller unit is driven to perform partition pressing and forming on each partition unit to obtain the corrugated core layer. The partition pressure roller unit is divided into multiple pressure roller units that can independently adjust the pressure and tooth depth along the container unfolding direction. The corrugated core layer after molding is subjected to wet heat creep simulation verification to determine whether the deformation of each partition unit exceeds a preset threshold. If the deformation of any partition unit exceeds the preset threshold, the shape parameters of the gradient corrugation height function and the gradient corrugation density function are adjusted, and the corrugation height parameter and corrugation density parameter corresponding to each partition unit are recalculated until the deformation of all partition units does not exceed the preset threshold.
7. The method according to claim 6, characterized in that, The partitioning unit is a rectangular partitioning unit.
8. The method according to claim 6, characterized in that, The degree of nonlinearity of the gradient rib height function and the gradient rib density function as a function of normalized stress coefficient is controlled by a shape parameter greater than 0.