A partially translucent marble slab and its preparation process
By combining the panel, base plate, and substrate structure with specific processes, the problem of controlling the light transmission of marble slabs has been solved, enabling flexible assembly and high-quality production of partially translucent marble slabs to meet diverse customer needs.
Patent Information
- Application Number
- CN202410778772.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-17
- Publication Date
- 2026-11-17
AI Technical Summary
The processing of translucent parts of existing marble is difficult to control, making it impossible to meet customers' customization needs.
It adopts a combination structure of panel, base plate and substrate, and achieves rapid docking through the design of positioning groove and positioning block, and uses structural adhesive for bonding. Combined with specific ingredients and process steps such as stirring, injection molding, molding, cutting and polishing, it forms a local light transmission effect.
It enables flexible assembly of partially translucent marble slabs, meeting diverse customer needs, improving aesthetics and assembly strength, and providing a realistic material texture with higher corrosion resistance and fire resistance.
Smart Images

Figure CN123104169A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of marble slab technology, specifically to a partially translucent marble slab and its preparation process. Background Technology
[0002] Marble slabs are a type of stone, primarily produced in Dali, Yunnan Province. Their appearance is characterized by patterns and natural capillary textures. With its soft, dignified texture, basic compressive strength, and good physical and chemical properties, marble is categorized as an aesthetically pleasing natural building and decorative stone. With large-scale mining, advancements in industrial technology, and the development of the social economy over the past decade, the application scope and usage of natural marble have become increasingly widespread.
[0003] Currently, most existing marble slabs are produced using a one-piece molding process, which makes it difficult to control the translucent parts of the marble. Therefore, marble slabs often cannot meet the customized needs of customers. As a result, we propose to design a partially translucent marble slab and its preparation process. Summary of the Invention
[0004] The purpose of this section is to outline some aspects of the embodiments of the present invention and to briefly describe some preferred embodiments. Simplifications or omissions may be made in this section, as well as in the abstract and title of this application, to avoid obscuring the purpose of these documents; however, such simplifications or omissions should not be construed as limiting the scope of the invention.
[0005] To address the aforementioned technical problems, according to one aspect of the present invention, the present invention provides the following technical solution:
[0006] A partially translucent marble slab includes a panel and a base plate, characterized in that a base plate is disposed between the panel and the base plate, a positioning groove is provided at the top edge of both the base plate and the base plate, and a positioning block is fixedly connected to the bottom of both the panel and the base plate.
[0007] The present invention further explains that the positioning block is arranged in the form of a rectangular frame, and the positioning block corresponds and fits with the positioning groove. After the groove is made, it is convenient to quickly connect the panel, the substrate and the bottom plate. Structural adhesive is used for bonding during assembly, resulting in high assembly strength.
[0008] The present invention further explains that the panel, base plate and substrate have the same external shape and size, and are cut uniformly during cutting, which facilitates later assembly. Moreover, after assembly, it is easy to remove burrs from the edges and polish the joints at the edges to form a whole, thereby improving the aesthetics of the marble.
[0009] A manufacturing process for partially translucent marble slabs includes the following specific steps:
[0010] S1: Ingredients: 600-800 components of 5-100 mesh rosin jade powder, 40-200 components of ultrafine calcium carbonate powder, 70-160 components of transparent unsaturated polyester resin, 1-2 components of initiator, 0.08-0.1 components of accelerator, 0.02-1.5 components of pigment, and 40-60 components of transparent nano-SiO2 material;
[0011] S2: Material preparation: Stir 5 to 100 mesh rosin powder and ultrafine calcium carbonate powder to obtain mixture A. Add pigment to mixture A and stir for 10 to 20 minutes to obtain mixture B. Add transparent unsaturated polyester resin, initiator and accelerator to mixture B, mix and stir, then apply vacuum at a vacuum degree of 60 to 70 cmHg, and continue stirring until the material becomes lumpy to obtain mixture C.
[0012] S3: Injection molding: Add transparent nano-SiO2 material to mixture C, stir, vacuum, and then inject the material into the mold;
[0013] S4: Molding: Place the mold containing the injected material in a vacuum chamber, apply pressure and vibration to form the material, demold after curing, and then cure it.
[0014] S5: Cut, grooving, assembling and polishing the cured material.
[0015] The present invention further explains that in S1, the initiator is methyl ethyl ketone peroxide, the transparent unsaturated polyester resin is crystal resin, the ultrafine calcium carbonate powder is calcium carbonate powder with a mesh size of 1300 or higher, the stone powder raw material is fine, which is convenient to improve the fineness of the pattern when the stone is processed, and to restore the appearance of marble to the greatest extent. The accelerator is cobalt isooctanoate, and the pigments are titanium dioxide, iron yellow and molybdenum red, which are convenient for dyeing stone raw materials.
[0016] The present invention further explains that in step S2, the mixtures A, B, and C are all stirred using a mixer. When dyeing different pigments, they can be placed in different mixers for stirring. After the pigments are evenly mixed, the several evenly dyed raw materials of different colors are then mixed together, which makes it easier to achieve a better mixing effect between the pigments and raw materials.
[0017] The present invention further explains that in step S4, the curing time of the material is not less than 24 hours, and the curing time of the material after demolding is not less than 7 days, which helps to prevent the stone from cracking and improve the quality of the stone.
[0018] The present invention further explains that, in S5, the cutting method is to cut the material into thin plates with a thickness of one centimeter using a water jet. During assembly, thin plates with different light-transmitting parts can be selected for assembly. Compared with the traditional one-piece marble material, the assembled marble has more local light-transmitting patterns and is more diverse, making it easier to meet customer needs and market sales needs. The polishing method is to pass the periphery of the assembled material through a polishing wheel at a uniform speed to remove burrs, making it easier to polish the joints and make its exterior resemble a complete stone.
[0019] Compared with the prior art, the beneficial effects of the present invention are:
[0020] This invention allows for the interaction between the panel, base plate, and substrate. Depending on the location and purpose of use, users can flexibly assemble various locally translucent substrates between the panel and base plate to create a locally translucent effect on marble slabs. The installation method is based on the pattern formed after the slab blank is demolded, and the assembly sequence and thickness can be flexibly controlled to better meet user needs. Attached Figure Description
[0021] To more clearly illustrate the technical solutions of the embodiments of the present invention, the present invention will be described in detail below with reference to the accompanying drawings and detailed embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort. Wherein:
[0022] Figure 1 This is a schematic diagram of the appearance of a partially translucent marble slab and its preparation process according to the present invention;
[0023] Figure 2 This is a schematic diagram of the assembly structure of a partially translucent marble slab and its preparation process according to the present invention.
[0024] Illustration: 1. Front panel; 2. Base plate; 3. Substrate; 4. Positioning groove; 5. Positioning block. Detailed Implementation
[0025] To make the above-mentioned objects, features and advantages of the present invention more apparent and understandable, the specific embodiments of the present invention will be described in detail below with reference to the accompanying drawings.
[0026] Secondly, the present invention is described in detail with reference to the schematic diagrams. When detailing the embodiments of the present invention, for ease of explanation, the cross-sectional views illustrating the device structure may be partially enlarged, not according to the usual scale. Furthermore, the schematic diagrams are merely examples and should not limit the scope of protection of the present invention. In addition, actual fabrication should include three-dimensional spatial dimensions of length, width, and depth.
[0027] To make the objectives, technical solutions, and advantages of the present invention clearer, the embodiments of the present invention will be described in further detail below with reference to the accompanying drawings.
[0028] Example 1:
[0029] Please see Figure 1-2 The present invention provides a partially translucent marble slab, comprising a panel 1 and a base plate 2, characterized in that a base plate 3 is provided between the panel 1 and the base plate 2, a positioning groove 4 is provided at the top edge of both the base plate 2 and the base plate 3, and a positioning block 5 is fixedly connected to the bottom of both the panel 1 and the base plate 3.
[0030] The positioning block 5 is set in a rectangular frame. The positioning block 5 corresponds to and fits into the positioning groove 4. After the groove is cut, it is easy to quickly connect the panel 1, the substrate 3 and the base plate 2. Structural adhesive is used for bonding during assembly, resulting in high assembly strength.
[0031] Panel 1, base plate 2, and base plate 3 have the same external shape and size. They are cut uniformly during the cutting process, which facilitates later assembly. After assembly, it is easy to remove burrs from the edges and polish the joints at the edges to form a whole, thereby improving the aesthetics of the marble.
[0032] A manufacturing process for partially translucent marble slabs includes the following specific steps:
[0033] S1: Ingredients: 600-800 components of 5-100 mesh rosin jade powder, 40-200 components of ultrafine calcium carbonate powder, 70-160 components of transparent unsaturated polyester resin, 1-2 components of initiator, 0.08-0.1 components of accelerator, 0.02-1.5 components of pigment, and 40-60 components of transparent nano-SiO2 material;
[0034] S2: Material preparation: Mix 600 components of 50-mesh rosin jade powder and 200 components of ultrafine calcium carbonate powder to obtain mixture A. Add 0.02 components of pigment to mixture A and stir for 20 minutes to obtain mixture B. Add 70 components of transparent unsaturated polyester resin, 1.5 components of initiator and 0.09 components of accelerator to mixture B, mix and stir, then apply vacuum at a vacuum degree of 60 cmHg, and continue stirring until the material becomes lumpy to obtain mixture C.
[0035] S3: Injection molding: Add 40 components of transparent nano-SiO2 material to mixture C, stir, vacuum, and then inject the material into the mold;
[0036] S4: Molding: Place the mold containing the injected material in a vacuum chamber, apply pressure and vibration to form the material, demold after curing, and then cure it.
[0037] S5: Cut, grooving, assembling and polishing the cured material.
[0038] In S1, the initiator is methyl ethyl ketone peroxide, the transparent unsaturated polyester resin is crystal resin, the ultrafine calcium carbonate powder is calcium carbonate powder with a mesh size of 1300 or higher, the stone powder raw material is fine, which makes it easy to improve the fineness of the pattern when the stone is processed, and to restore the appearance of marble to the greatest extent. The accelerator is cobalt isooctanoate, and the pigments are titanium dioxide, iron yellow and molybdenum red, which makes it easy to dye the stone raw material.
[0039] In S2, mixtures A, B, and C are all mixed using a mixer. When dyeing different pigments, they can be placed in different mixers for mixing. After the pigments are evenly mixed, the several evenly dyed raw materials of different colors are mixed together to make the mixing effect of pigments and raw materials better.
[0040] In S4, the curing time of the material is no less than 24 hours, and the curing time after demolding is no less than 7 days, which helps to prevent the stone from cracking and improve the quality of the stone.
[0041] In S5, the cutting method involves cutting the material into thin slabs with a thickness of one centimeter using a water jet. During assembly, thin slabs with different light-transmitting parts can be selected for assembly. Compared with traditional one-piece marble, the assembled marble has more local light-transmitting patterns and is more diverse, making it easier to meet customer needs and market sales requirements. The polishing method involves passing the assembled material around its perimeter at a uniform speed through a grinding wheel to remove burrs, making it easier to polish the joints and making its exterior resemble a complete stone.
[0042] In this embodiment, a smaller amount of rosin jade powder and a high content of ultrafine calcium carbonate powder are used, which makes the processed marble material harder, and its corrosion resistance and fire resistance are also improved, making it easier to apply in various pressure-bearing positions.
[0043] The material contains relatively little transparent unsaturated polyester resin and transparent nano-SiO2 material. While ensuring a certain degree of light transmittance, the main body of the board serves as a load-bearing and pressure-bearing component. Therefore, the requirements for the material texture are not high, and its practical value outweighs its artistic value.
[0044] Example 2:
[0045] The present invention provides a partially translucent marble slab, comprising a panel 1 and a base plate 2, characterized in that a base plate 3 is provided between the panel 1 and the base plate 2, a positioning groove 4 is provided at the top edge of both the base plate 2 and the base plate 3, and a positioning block 5 is fixedly connected to the bottom of both the panel 1 and the base plate 3.
[0046] The positioning block 5 is set in a rectangular frame. The positioning block 5 corresponds to and fits into the positioning groove 4. After the groove is cut, it is easy to quickly connect the panel 1, the substrate 3 and the base plate 2. Structural adhesive is used for bonding during assembly, resulting in high assembly strength.
[0047] Panel 1, base plate 2, and base plate 3 have the same external shape and size. They are cut uniformly during the cutting process, which facilitates later assembly. After assembly, it is easy to remove burrs from the edges and polish the joints at the edges to form a whole, thereby improving the aesthetics of the marble.
[0048] A manufacturing process for partially translucent marble slabs includes the following specific steps:
[0049] S1: Ingredients: 600-800 components of 5-100 mesh rosin jade powder, 40-200 components of ultrafine calcium carbonate powder, 70-160 components of transparent unsaturated polyester resin, 1-2 components of initiator, 0.08-0.1 components of accelerator, 0.02-1.5 components of pigment, and 40-60 components of transparent nano-SiO2 material;
[0050] S2: Material preparation: Mix 800 components of 50-mesh rosin jade powder and 40 components of ultrafine calcium carbonate powder to obtain mixture A. Add 1.5 components of pigment to mixture A and stir for 20 minutes to obtain mixture B. Add 160 components of transparent unsaturated polyester resin, 1.5 components of initiator and 0.09 components of accelerator to mixture B, mix and stir, then apply vacuum at a vacuum degree of 70 cmHg, and continue stirring until the material becomes lumpy to obtain mixture C.
[0051] S3: Molding: Add 60 components of transparent nano-SiO2 material to mixture C, stir, vacuum, and then inject the material into the mold;
[0052] S4: Molding: Place the mold containing the injected material in a vacuum chamber, apply pressure and vibration to form the material, demold after curing, and then cure it.
[0053] S5: Cut, grooving, assembling and polishing the cured material.
[0054] In S1, the initiator is methyl ethyl ketone peroxide, the transparent unsaturated polyester resin is crystal resin, the ultrafine calcium carbonate powder is calcium carbonate powder with a mesh size of 1300 or higher, the stone powder raw material is fine, which makes it easy to improve the fineness of the pattern when the stone is processed, and to restore the appearance of marble to the greatest extent. The accelerator is cobalt isooctanoate, and the pigments are titanium dioxide, iron yellow and molybdenum red, which makes it easy to dye the stone raw material.
[0055] In S2, mixtures A, B, and C are all mixed using a mixer. When dyeing different pigments, they can be placed in different mixers for mixing. After the pigments are evenly mixed, the several evenly dyed raw materials of different colors are mixed together to make the mixing effect of pigments and raw materials better.
[0056] In S4, the curing time of the material is no less than 24 hours, and the curing time after demolding is no less than 7 days, which helps to prevent the stone from cracking and improve the quality of the stone.
[0057] In S5, the cutting method involves cutting the material into thin plates with a thickness of one centimeter using a water jet. During assembly, thin plates with different light-transmitting parts can be selected for assembly. Compared with traditional one-piece marble, the assembled marble has more local light-transmitting patterns and is more diverse, making it easier to meet customer needs and market sales requirements. The polishing method involves passing the assembled material around its perimeter at a uniform speed through a polishing wheel to remove burrs.
[0058] In this embodiment, a high-component rosin jade powder is used, while the amount of ultrafine calcium carbonate powder used is relatively low. While discarding some of the physical properties of marble such as hardness, pressure resistance and corrosion resistance, more attention is paid to the texture of marble, making the processed marble texture more realistic.
[0059] This material contains a relatively high proportion of transparent unsaturated polyester resin and transparent nano-SiO2 material, resulting in stone slabs with better light transmittance and more light-transmitting areas. During later assembly and processing, corresponding locally light-transmitting panels can be selected from multiple slabs based on the local light-transmitting areas on the thin slabs to form various styles of high-transmittance marble slabs. At the same time, the pigment content is relatively high, making it more aesthetically pleasing when used as a decorative panel, with artistic value exceeding its practical value.
[0060] Although the present invention has been described above with reference to embodiments, various modifications can be made and components can be replaced with equivalents without departing from the scope of the invention. In particular, as long as there is no structural conflict, the features in the disclosed embodiments can be combined with each other in any manner. The lack of an exhaustive description of these combinations in this specification is merely for the sake of brevity and resource conservation. Therefore, the present invention is not limited to the specific embodiments disclosed herein, but includes all technical solutions falling within the scope of the claims.
Claims
1. A partially translucent marble slab, comprising a panel (1) and a base plate (2), characterized in that, A base plate (3) is provided between the panel (1) and the base plate (2). A positioning groove (4) is provided at the top edge of both the base plate (2) and the base plate (3). A positioning block (5) is fixedly connected to the bottom of both the panel (1) and the base plate (3).
2. The partially translucent marble slab and its preparation process according to claim 1, characterized in that, The positioning block (5) is set in the form of a rectangular frame, and the positioning block (5) corresponds to and fits into the positioning groove (4).
3. The partially translucent marble slab and its preparation process according to claim 1, characterized in that, The panel (1), the base plate (2), and the substrate (3) have the same external shape and size.
4. A manufacturing process for a partially translucent marble slab as described in any one of claims 1-3, characterized in that, The specific steps include the following: S1: Ingredients: 600-800 components of 5-100 mesh rosin jade powder, 40-200 components of ultrafine calcium carbonate powder, 70-160 components of transparent unsaturated polyester resin, 1-2 components of initiator, 0.08-0.1 components of accelerator, 0.02-1.5 components of pigment, and 40-60 components of transparent nano-SiO2 material; S2: Material preparation: Stir 5 to 100 mesh rosin powder and ultrafine calcium carbonate powder to obtain mixture A. Add pigment to mixture A and stir for 10 to 20 minutes to obtain mixture B. Add transparent unsaturated polyester resin, initiator and accelerator to mixture B, mix and stir, then apply vacuum at a vacuum degree of 60 to 70 cmHg, and continue stirring until the material becomes lumpy to obtain mixture C. S3: Injection molding: Add transparent nano-SiO2 material to mixture C, stir, vacuum, and then inject the material into the mold; S4: Molding: Place the mold containing the injected material in a vacuum chamber, apply pressure and vibrate to form the material, demold after curing, and then cure it. S5: Cut, grooving, assembling and polishing the cured material.
5. The preparation process of a partially translucent marble slab according to claim 4, characterized in that: In step S1, the initiator is methyl ethyl ketone peroxide, the transparent unsaturated polyester resin is crystal resin, the ultrafine calcium carbonate powder is calcium carbonate powder with a mesh size of 1300 or higher, the accelerator is cobalt isooctanoate, and the pigment is titanium dioxide, iron yellow, and molybdenum red.
6. The preparation process of a partially translucent marble slab according to claim 4, characterized in that: In step S2, mixtures A, B, and C are all mixed using a mixer.
7. The preparation process of a partially translucent marble slab according to claim 4, characterized in that: In step S4, the curing time of the material is not less than 24 hours, and the curing time of the material after demolding is not less than 7 days.
8. The preparation process of a partially translucent marble slab according to claim 4, characterized in that: In step S5, the cutting method involves cutting the material into a thin plate with a thickness of one centimeter using a water jet, and the grinding method involves passing the assembled material around its periphery at a uniform speed through a grinding wheel to remove burrs.