An environmentally friendly modified biochar organic fertilizer and its preparation method
By forming a core-shell structure of amino-functionalized biochar and triazine-trithiophene-based covalent organic framework material on the surface of biochar, the stability and catalytic efficiency of modified biochar organic fertilizer were solved, achieving a synergistic effect of nutrient slow release and soil pollution purification.
Patent Information
- Application Number
- CN202611369128.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-04
- Publication Date
- 2026-11-17
AI Technical Summary
Existing modified biochar organic fertilizers suffer from problems such as easy loss of functional materials, poor stability, weak near-infrared light response, and low catalytic efficiency, making it difficult to achieve the synergistic effect of nutrient slow release and soil pollution purification.
An environmentally friendly modified biochar organic fertilizer was prepared by forming a core-shell structure with amino-functionalized biochar and triazine-trithiophene covalent organic framework material, combined with the photocatalytic function of visible-near-infrared light response, and chemically bonded together.
It achieves a synergistic effect of slow nutrient release and soil pollution purification, improves the stability and catalytic efficiency of the functional layer, and enhances nutrient utilization and soil remediation effect.
Abstract
Description
Technical Field
[0001] This invention belongs to the field of agricultural environmentally friendly fertilizer technology, specifically relating to an environmentally friendly modified biochar organic fertilizer and its preparation method. Background Technology
[0002] With the increasing demand for green agricultural development, traditional organic fertilizers suffer from problems such as rapid nutrient release, low utilization rate, and difficulty in simultaneously addressing issues like pesticide residues and heavy metal pollution in the soil, thus hindering their application and promotion. Biochar, due to its porous structure and excellent adsorption properties, is often used as a carrier for organic fertilizers; however, unmodified biochar has weak nutrient binding capacity and lacks photocatalytic purification capabilities, making it unable to remediate contaminated soil.
[0003] Existing modified biochar organic fertilizers are mostly prepared by simply loading functional components, which has drawbacks such as easy detachment of functional materials and poor stability. Some photocatalytic organic fertilizers use traditional semiconductor materials, which have weak near-infrared light response and low catalytic efficiency. At the same time, although amination modification can enhance the binding ability of biochar and functional components, current technologies have not combined it with covalent organic framework (COF) materials with specific structures, making it difficult to balance the long-term slow release of nutrients with the targeted purification of pollution.
[0004] Therefore, there is an urgent need to develop an organic fertilizer that uses precise structural design to construct a core-shell structure by combining amino-functionalized biochar with near-infrared responsive triazine-trithiophene-based COF, thereby achieving controlled nutrient release and synergistic purification of soil pollution, and meeting the urgent needs of modern agriculture for efficient and environmentally friendly fertilizers. Summary of the Invention
[0005] To address the aforementioned problems, this invention proposes an environmentally friendly modified biochar organic fertilizer and its preparation method. This organic fertilizer uses amino-functionalized biochar as the core and a triazine-trithiophene covalent organic framework as the shell to form a core-shell structure. It has visible-near-infrared light response, nutrient slow release, and soil pollution purification functions. At the same time, it has high nutrient utilization and good stability, which can meet the application needs of green agricultural production and soil synergistic remediation.
[0006] To achieve the above objectives, the present invention adopts the following technical solution:
[0007] An environmentally friendly modified biochar organic fertilizer, wherein the organic fertilizer is composed of the following raw materials in the following mass percentages:
[0008] Amino-functionalized biochar 45%-60%, photocatalytic functional materials 5%-15%, humic acid 20%-30%, trace elements 3%-8%, binder 1%-3%;
[0009] The amino-functionalized biochar has amino functional groups grafted onto its surface. The organic fertilizer uses amino-functionalized biochar as its core, and a visible-near-infrared responsive photocatalytic functional material layer is grown in situ on its surface to form a core-shell structure with a light absorption range of 400-850 nm. The photocatalytic functional material layer is chemically bonded to the amino-functionalized biochar.
[0010] Optionally, the photocatalytic functional material is a triazine-trithiophene covalent organic framework material with a specific surface area of 400-800 m². 2 / g.
[0011] Optionally, the binder is one or more of starch, carboxymethyl cellulose, and polyvinyl alcohol.
[0012] Optionally, the trace elements include one or more of calcium, magnesium, iron, zinc, and boron.
[0013] Optionally, the preparation method of the aforementioned environmentally friendly modified biochar organic fertilizer is as follows:
[0014] S1. Mix biochar and amination reagent at a mass ratio of 10:1-10:3, react at 80-120℃ for 2-4 hours, and then wash and dry to obtain amino-functionalized biochar.
[0015] S2. Disperse the amino-functionalized biochar obtained in step S1 in an ethanol-water mixed solvent, add triazine monomers and trithiophene monomers, and stir the reaction at 50-70℃ for 4-8 hours to form a core-shell structured complex.
[0016] S3. Add humic acid, trace elements and binder to the composite obtained in step S2, and stir and mix at 30-50℃ for 30-60 minutes to obtain a mixture.
[0017] S4. Dry and solidify the mixture obtained in step S3 at 60-80℃, and crush it to a particle size of 0.5-5mm to obtain environmentally friendly modified biochar organic fertilizer.
[0018] Optionally, the amination reagent is selected from one or more of ethylenediamine, diethylenetriamine, triethylenetetramine, ethanolamine, and urea.
[0019] Optionally, in step S2, the molar ratio of triazine monomers to trithiophene monomers is 1:1 to 1:2, and the total amount of monomers used is 5% to 15% of the mass of aminofunctionalized biochar.
[0020] The beneficial effects of this invention are as follows: The organic fertilizer prepared by this invention has excellent visible-near-infrared light responsive catalytic performance, which can efficiently degrade pollutants such as pesticides and antibiotics in the soil; the amino-functionalized biochar and the triazine-trithiophene covalent organic framework form a stable core-shell structure through chemical bonding, and the functional layer is not easy to fall off, which significantly improves the stability; the product has both nutrient slow release and nitrogen fixation and fertilizer retention functions, which can greatly improve nutrient utilization and reduce the application of chemical fertilizers; the high specific surface area and the core-shell structure work together to achieve controllable nutrient release, and with the addition of humic acid and trace elements, it can improve the soil environment and promote crop growth. Overall, it has the comprehensive and excellent effects of long-lasting fertilizer effect, pollution remediation, and green environmental protection. Detailed Implementation
[0021] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the embodiments of the present invention. All other embodiments obtained by those skilled in the art based on the embodiments of the present invention without creative effort are within the scope of protection of the present invention.
[0022] Example 1: This Example 1 describes an environmentally friendly modified biochar organic fertilizer, which is composed of the following raw materials in the following mass percentages:
[0023] 55% amino-functionalized biochar, 10% photocatalytic functional material, 25% humic acid, 7% trace elements (calcium, magnesium, iron, zinc, boron composite salt mass ratio 1:1:1:1:1), 3% binder (carboxymethyl cellulose).
[0024] The preparation method of the photocatalytic functional material (triazine-trithiophene-based covalent organic framework material) is as follows:
[0025] S1. Weigh 2,4,6-tris(4-aminophenyl)-1,3,5-triazine (TAPT) and benzo[1,2-B:3,4-B':5,6-B']trithiophene-2,5,8-trialdehyde (BTT), and add them to a mixed solvent of N,N-dimethylformamide / ethanol (volume ratio 4:1) at a molar ratio of 1:1, and ultrasonically disperse for 15 min until the system is homogeneous.
[0026] S2. The reaction system was evacuated and replaced with nitrogen three times. Under nitrogen protection, the reaction was carried out at 60°C and stirred at 400 rpm for 6 hours.
[0027] S3. After the reaction is complete, cool to room temperature, centrifuge at 9000 rpm for 10 min, and discard the supernatant.
[0028] S4. Wash the precipitate three times each with acetone, ethanol and deionized water.
[0029] S5. The washed product was vacuum dried at 60℃ for 12 h to obtain a triazine-trithiophene-based covalent organic framework material with a specific surface area of 685 m². 2 / g.
[0030] The specific preparation steps of this embodiment of an environmentally friendly modified biochar organic fertilizer are as follows:
[0031] S1. Mix biochar and ethylenediamine at a mass ratio of 10:2, place them in a hydrothermal reactor, and react at 100℃ for 3 hours. After the reaction is completed, cool to room temperature, filter, wash with deionized water until the filtrate is neutral, and dry at 60℃ for 4 hours to obtain amino-functionalized biochar.
[0032] S2. Take the amino-functionalized biochar prepared in step S1 and disperse it in deionized water with a total mass of 10 times that of the amino-functionalized biochar and photocatalytic functional material. Add the prepared triazine-trithiophene covalent organic framework material and place it in a constant temperature stirred tank. Stir at 60°C and 400 rpm for 6 hours to form a COF layer on the surface of the amino-functionalized biochar, forming a core-shell complex suspension.
[0033] S3. Take the specified amount of the complex salt of trace elements, add 10 times the mass of the trace elements to deionized water, stir at 300 rpm until completely dissolved, and obtain an aqueous solution of trace elements.
[0034] S4. Humic acid, trace element aqueous solution and carboxymethyl cellulose are added sequentially to the core-shell complex suspension. The mixture is stirred at 40°C and 400 rpm for 45 min to obtain a uniform slurry.
[0035] S5. Dry and solidify at 70℃, then pulverize to a particle size ≤2mm to obtain environmentally friendly modified biochar organic fertilizer.
[0036] Example 2: This Example 2 describes an environmentally friendly modified biochar organic fertilizer, which is composed of the following raw materials in the following mass percentages:
[0037] Amino-functionalized biochar 58%, photocatalytic functional material 7%, humic acid 25%, trace elements 7% (calcium, magnesium, iron, zinc, boron composite salt mass ratio 1:1:1:1:1), binder 3% (carboxymethyl cellulose);
[0038] The preparation method of the photocatalytic functional material (triazine-trithiophene covalent organic framework material) is the same as that in Example 1;
[0039] The preparation method of the environmentally friendly modified biochar organic fertilizer in this embodiment is the same as that in Example 1, except that the amount of photocatalytic material added is reduced to 7%.
[0040] Example 3: This Example 3 describes an environmentally friendly modified biochar organic fertilizer, which is composed of the following raw materials in the following mass percentages:
[0041] Amino-functionalized biochar 52%, photocatalytic functional material 13%, humic acid 25%, trace elements 7% (calcium, magnesium, iron, zinc, boron composite salt mass ratio 1:1:1:1:1), binder 3% (carboxymethyl cellulose);
[0042] The preparation method of the photocatalytic functional material (triazine-trithiophene covalent organic framework material) is the same as that in Example 1;
[0043] The preparation method of the environmentally friendly modified biochar organic fertilizer in this embodiment is the same as that in Example 1, except that the amount of photocatalytic material added is increased to 13%.
[0044] Comparative Example 1: The organic fertilizer of Comparative Example 1 is composed of the following raw materials by mass percentage:
[0045] 55% unmodified biochar, 10% photocatalytic functional material, 25% humic acid, 7% trace elements (calcium, magnesium, iron, zinc, boron composite salt mass ratio 1:1:1:1:1), 3% binder (carboxymethyl cellulose).
[0046] The preparation method of the photocatalytic functional material (triazine-trithiophene covalent organic framework material) is the same as that in Example 1;
[0047] The preparation method of the organic fertilizer in this comparative example is the same as that in Example 1, except that the amino-functionalized biochar is replaced with unmodified biochar.
[0048] Comparative Example 2: The organic fertilizer of Comparative Example 2 is composed of the following raw materials by mass percentage:
[0049] The composition includes 65% amino-functionalized biochar, 25% humic acid, 7% trace elements (calcium, magnesium, iron, zinc, and boron compound salt in a mass ratio of 1:1:1:1:1), and 3% binder (carboxymethyl cellulose).
[0050] The preparation method of the organic fertilizer in this comparative example is the same as that in Example 1, except that no photocatalytic functional material is added.
[0051] Performance testing
[0052] 1. Photocatalytic degradation performance of organic matter
[0053] Using methylene blue as a simulated organic pollutant, a 10 mg / L methylene blue solution was prepared. 50 mg of each of the organic fertilizer samples from Examples 1-3 and Comparative Examples 1-2 were added to 50 mL of the above methylene blue solution. The mixture was stirred for 30 min under light-protected conditions to reach adsorption-desorption equilibrium. Subsequently, a 300 W xenon lamp was used to simulate visible light irradiation, and the reaction was continuously stirred for 5 h. Samples were taken every 1 h, filtered through a 0.22 μm filter membrane, and the absorbance was measured at 664 nm using a UV-Vis spectrophotometer. The degradation rate of methylene blue at different time points was calculated to evaluate the photocatalytic degradation performance of the samples.
[0054] Table 1. Test data on the photocatalytic degradation performance of organic matter of different samples (%)
[0055] sample 1h 2h 3h 4h 5h Example 1 22.6 41.3 62.8 81.5 92.3 Example 2 18.2 32.5 48.7 64.2 76.8 Example 3 24.1 43.6 65.2 79.8 88.5 Comparative Example 1 12.5 23.7 34.2 43.6 52.1 Comparative Example 2 9.8 17.3 24.6 31.5 37.2
[0056] Examples 1-3 showed significantly higher degradation rates of methylene blue than the comparative examples, with Example 1 achieving a degradation rate of 92.3% after 5 hours, demonstrating the best performance. The results indicate that the core-shell structure formed by amino-modified biochar and triazine-trithiophene COF exhibits excellent photocatalytic activity, while the unmodified or non-photocatalyst-based comparative examples relied solely on physical adsorption, resulting in significantly poorer degradation.
[0057] 2. Nutrient slow-release performance
[0058] Nutrient slow-release performance was determined using the water extraction method. 5.0 g of each organic fertilizer sample from Examples 1-3 and Comparative Examples 1-2 were placed in 500 mL stoppered conical flasks, 250 mL of deionized water was added, and the flasks were sealed and placed in a 25°C constant-temperature shaker at 150 rpm for extraction. 5 mL samples were taken at 1, 3, 7, 14, and 28 days after extraction. The samples were filtered through a 0.45 μm filter membrane, and nitrogen content was determined using the Kjeldahl method, phosphorus content using the molybdenum-antimony colorimetric method, and potassium content using the flame photometry method. An equal amount of deionized water was added after each sampling to maintain a constant liquid-solid ratio. The cumulative nitrogen release rate at different time points was calculated to evaluate the nutrient slow-release effect of the samples.
[0059] Table 2. Cumulative total nitrogen release rate data for different samples (%)
[0060] sample 1d 3d 7d 14d 28d Example 1 12.5 24.8 38.6 57.2 72.3 Example 2 15.2 29.6 45.3 63.8 78.5 Example 3 11.8 23.5 36.9 54.6 69.2 Comparative Example 1 22.6 39.5 56.8 74.2 85.6 Comparative Example 2 28.3 48.7 65.2 81.5 92.1
[0061] Examples 1-3 showed a gradual nutrient release with a moderate total nitrogen release rate over 28 days, with Example 1 exhibiting the best controlled-release effect. Comparative Examples 1 and 2 showed excessively rapid release and short-lived fertilizer effects. This demonstrates that the core-shell structure of this invention can effectively delay nutrient release and prolong fertilizer effect; unmodified or uncatalyzed examples show no significant controlled-release effect.
[0062] 3. Heavy metal adsorption capacity
[0063] With cadmium (Cd) 2+), lead (Pb) 2+ Using Cd(NO3)2 and Pb(NO3)2 solutions with a concentration of 100 mg / L as the target heavy metal ions, 0.5 g of each of the organic fertilizer samples from Examples 1-3 and Comparative Examples 1-2 were added to 50 mL of the above heavy metal ion solutions. The pH of the system was adjusted to 5.5 (simulating an acidic soil environment), and the system was placed in a 25°C constant temperature shaker at 150 rpm for 24 h to reach equilibrium. Subsequently, the solution was filtered through a 0.45 μm filter membrane, and the remaining Cd in the filtrate was determined using an atomic absorption spectrophotometer. 2+ Pb 2+ Concentration was determined and adsorption capacity was calculated. Simultaneously, leaching tests were performed using TCLP (Toxicity Characteristic Leaching Procedure). The adsorbed sample was mixed with the extract at a liquid-to-solid ratio of 20:1, shaken for 18 hours, and then filtered. The concentration of heavy metals in the leachate was measured to evaluate the stability of heavy metal fixation.
[0064] Table 3. Test data on the heavy metal adsorption capacity of different samples
[0065] sample <![CDATA[Cd 2+ Adsorption capacity (mg / g) <![CDATA[Pb 2+ Adsorption capacity (mg / g) <![CDATA[Cd 2+ Leachate concentration (mg / L) <![CDATA[Pb 2+ Leachate concentration (mg / L) Example 1 86.3 128.5 0.08 0.12 Example 2 81.7 121.3 0.11 0.15 Example 3 83.5 124.7 0.09 0.13 Comparative Example 1 58.2 89.6 0.35 0.42 Comparative Example 2 65.4 98.3 0.28 0.34
[0066] Examples 1-3 on Cd 2+ Pb 2+ Example 1 showed the best performance with high adsorption capacity and low leaching concentration. Amino modification provides chelation sites, which, combined with the porous structure of COF, achieves efficient adsorption and stable immobilization; the comparative example has insufficient active sites, making it easy for heavy metals to leach out and resulting in poor safety.
[0067] 4. Organic matter content and nutrient content test
[0068] Organic matter content was determined using the potassium dichromate volumetric-external heating method: 0.5g of each organic fertilizer sample from Examples 1-3 and Comparative Examples 1-2 was added to 10mL of 0.4mol / L potassium dichromate-sulfuric acid solution, digested in an oil bath at 170-180℃ for 15min, and after cooling, titrated with 0.2mol / L ferrous sulfate standard solution to calculate the organic matter mass fraction. Total nitrogen content was determined using the Kjeldahl method: 0.2g of sample was weighed, digested with concentrated sulfuric acid-catalyst, and brought to a final volume of 100mL. 10mL was then distilled and titrated according to the Kjeldahl method. Total phosphorus content was determined using the molybdenum-antimony colorimetric method: after color development with ammonium vanadate, the absorbance of the digested solution was measured at a wavelength of 700nm, and the content was calculated from the standard curve. Total potassium content was determined using the flame photometry method: after dilution of the digested solution, the potassium ion emission intensity was measured using a flame photometer and converted to the total potassium mass fraction. The four indicators were measured in parallel three times, and the average value was taken to comprehensively evaluate the basic nutrients and organic matter level of the product.
[0069] Table 4. Test data on organic matter and nutrient content of different samples
[0070] sample organic matter Total nitrogen (N) <![CDATA[Total phosphorus (P2O5)]]> <![CDATA[Total potassium (K₂O)]]> <![CDATA[Total Nutrient (N+P2O5+K2O)]]> Example 1 52.6 2.18 1.65 1.42 5.25 Example 2 51.8 2.12 1.61 1.39 5.12 Example 3 52.2 2.15 1.63 1.41 5.19 Comparative Example 1 48.3 1.86 1.43 1.21 4.50 Comparative Example 2 49.5 1.94 1.48 1.26 4.68
[0071] Examples 1-3 all showed higher organic matter and total nutrient content than the comparative example, with Example 1 reaching the level of a superior organic fertilizer. The process of this invention can effectively retain and enrich nutrients, while the comparative example had lower organic matter and nutrient carrying capacity due to structural defects.
[0072] 5. pH value, moisture content, and particle size testing
[0073] pH value determination: Take 10g of organic fertilizer samples from Examples 1-3 and Comparative Examples 1-2, add 100mL of deionized water, stir evenly and soak for 30min, stirring once every 10min during the period, and use a calibrated pH meter to measure the pH value of the supernatant.
[0074] Moisture content was determined by the drying weight loss method: 5g of sample was weighed and placed in a weighing bottle that had been pre-weighed, and dried at 105℃ until constant weight. The ratio of the mass difference before and after drying to the initial mass of the sample was calculated, which is the moisture content.
[0075] Particle size distribution was determined by sieving: 20g of dried sample was passed through 2mm, 1mm and 0.5mm standard sieves in sequence, shaken for 10min and then weighed to measure the mass of the residual sample in each sieve layer. The mass fraction of different particle size ranges was calculated to evaluate the physical properties of the product.
[0076] Table 5. Test data of pH value, moisture content, and particle size for different samples.
[0077] sample pH value Moisture (%) Particle size ≤ 0.5 mm (%) Example 1 7.2 4.1 92.6 Example 2 7.1 4.3 91.8 Example 3 7.3 4.0 92.3 Comparative Example 1 6.8 5.8 82.5 Comparative Example 2 6.9 5.2 85.7
[0078] Examples 1-3 exhibited neutral pH, moderate moisture content, fine and uniform particle size, and excellent physical properties; the comparative examples were slightly acidic, had higher moisture content, and uneven particle size. The core-shell structure of this invention optimizes the physical stability of the product, making it more suitable for field application.
[0079] 6. Pot experiment
[0080] Using Chinese cabbage as the test crop, homogeneous garden soil was selected, and 2.0 kg of soil was placed in each pot. Organic fertilizer samples prepared in Examples 1-3 and Comparative Examples 1-2 were added at a soil weight of 5%, respectively. After mixing, the samples were placed in pots, and a blank control group was set up. Each treatment was repeated 3 times. Ten seeds were sown in each pot. After emergence, the seedlings were thinned to 4 plants and placed in a greenhouse for routine management. The light, temperature and watering were kept consistent. After 30 days of growth, the plants were harvested, and the plant height, fresh weight, dry weight and leaf chlorophyll content (SPAD value) were measured. The biomass growth rate was calculated to evaluate the actual fertilizer efficiency and growth-promoting effect of the organic fertilizer.
[0081] Table 6. Data from potted plant experiments with different samples
[0082] sample Plant height (cm) Fresh weight (g / plant) Dry weight (g / plant) chlorophyll SPAD value Example 1 16.8 28.6 3.25 42.5 Example 2 15.3 25.1 2.86 39.2 Example 3 15.9 26.7 3.01 40.6 Comparative Example 1 12.6 18.3 2.14 33.7 Comparative Example 2 13.5 20.6 2.37 35.8 Blank control 10.2 14.2 1.62 29.3
[0083] In Examples 1-3, the plant height, biomass, and chlorophyll content of the pak choi were significantly higher than those in the control and blank samples, with Example 1 showing the best growth-promoting effect. This invention significantly enhances crop growth through the synergistic effects of nutrient slow release, photocatalytic activation, and heavy metal fixation, while the effects in the control samples were significantly weaker.
[0084] The above embodiments are only used to illustrate the technical solutions of the present invention, and are not intended to limit it. Although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.
Claims
1. An environmentally friendly modified biochar organic fertilizer, characterized in that, The organic fertilizer is composed of the following raw materials in the following mass percentages: Amino-functionalized biochar 45%-60%, photocatalytic functional materials 5%-15%, humic acid 20%-30%, trace elements 3%-8%, binder 1%-3%; The amino-functionalized biochar has amino functional groups grafted onto its surface. The organic fertilizer uses amino-functionalized biochar as its core, and a visible-near-infrared responsive photocatalytic functional material layer is grown in situ on its surface to form a core-shell structure with a light absorption range of 400-850 nm. The photocatalytic functional material layer is chemically bonded to the amino-functionalized biochar.
2. The environmentally friendly modified biochar organic fertilizer according to claim 1, characterized in that, The photocatalytic functional material is a triazine-trithiophene covalent organic framework material with a specific surface area of 400-800 m². 2 / g.
3. The environmentally friendly modified biochar organic fertilizer according to claim 1, characterized in that, The binder is one or more of starch, carboxymethyl cellulose, and polyvinyl alcohol.
4. The environmentally friendly modified biochar organic fertilizer according to claim 1, characterized in that, The trace elements include one or more of calcium, magnesium, iron, zinc, and boron.
5. A method for preparing an environmentally friendly modified biochar organic fertilizer, used to prepare the environmentally friendly modified biochar organic fertilizer according to any one of claims 1-4, characterized in that, The specific preparation method is as follows: S1. Mix biochar and amination reagent at a mass ratio of 10:1-10:3, react at 80-120℃ for 2-4 hours, and then wash and dry to obtain amino-functionalized biochar. S2. Disperse the amino-functionalized biochar obtained in step S1 in an ethanol-water mixed solvent, add triazine monomers and trithiophene monomers, and stir the reaction at 50-70℃ for 4-8 hours to form a core-shell structured complex. S3. Add humic acid, trace elements and binder to the composite obtained in step S2, and stir and mix at 30-50℃ for 30-60 minutes to obtain a mixture. S4. Dry and solidify the mixture obtained in step S3 at 60-80℃, and crush it to a particle size of 0.5-5mm to obtain environmentally friendly modified biochar organic fertilizer.
6. The method for preparing an environmentally friendly modified biochar organic fertilizer according to claim 5, characterized in that, The amination reagent is selected from one or more of ethylenediamine, diethylenetriamine, triethylenetetramine, ethanolamine, and urea.
7. The method for preparing an environmentally friendly modified biochar organic fertilizer according to claim 5, characterized in that, In step S2, the molar ratio of triazine monomers to trithiophene monomers is 1:1 to 1:2, and the total amount of monomers used is 5% to 15% of the mass of aminofunctionalized biochar.