An activated peat and its activation method

By using monoethanolamine dilution, desulfurized gypsum, and urea in combination with aerobic fermentation to treat wet peat, a synergistic effect of chemical and biological activation is achieved, solving the problems of high energy consumption and low efficiency in peat activation in existing technologies, and producing highly efficient activated peat for saline-alkali land improvement.

CN123106338APending Publication Date: 2026-11-17QINGDAO DIBAOLONG MICRO CARBON AGRI TECH CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202611418464.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-14
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing peat activation technologies suffer from high energy consumption, complex processes, high costs, and difficulty in directly activating high-moisture peat. Chemical and biological activation are usually carried out independently, failing to effectively increase the content of water-soluble humic acid and cation exchange capacity, thus failing to meet the needs of saline-alkali land improvement.

Method used

A diluted monoethanolamine solution was used in combination with desulfurized gypsum and urea to treat wet peat through atomized spraying and aerobic fermentation, achieving a synergistic effect of chemical amination and biodegradation to generate water-soluble humic acid ethanolamine salt. The temperature was controlled below 60℃, and chemical and biological activation were carried out simultaneously, avoiding pre-drying and the addition of bacterial agents.

Benefits of technology

With low energy consumption and a short cycle, the content of water-soluble humic acid and cation exchange capacity are significantly increased, and highly efficient activated peat suitable for saline-alkali land is prepared to promote crop growth and reduce production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

This invention provides an activated peat and its activation method, relating to the field of soil improvement technology. The activation method of this invention first pre-treats wet peat to obtain wet peat fragments. Then, a diluted monoethanolamine solution is applied to the wet peat fragments via atomized spraying. Simultaneously, the wet peat fragments are turned over and mixed with desulfurized gypsum and urea. After spraying, the peat is piled up to obtain strip piles. Finally, the strip piles undergo aerobic fermentation activation treatment, with periodic turning and the temperature of the strip piles controlled to not exceed 60°C. Activated peat is obtained when the wet peat has completed the expected activation. This activation method can simultaneously achieve chemical and biological activation, directly treating high-moisture peat with a low-energy, short-cycle, and dry-free solid-state process to obtain activated peat with high water-soluble humic acid content and improved cation exchange capacity. Furthermore, this activated peat is suitable for saline-alkali soils.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of soil improvement technology, and in particular to an activated peat and its activation method. Background Technology

[0002] Peat is an organic-mineral complex formed from the incomplete decomposition of swamp plant remains under long-term anaerobic conditions by microorganisms. Rich in humic acid, organic matter, and various plant nutrients, it is a high-quality raw material for preparing soil conditioners and organic fertilizers. However, the humic acid in native peat exists mainly in a water-insoluble free state or in a poorly soluble state bound to metal ions such as calcium, magnesium, and iron. Direct application results in low bioavailability, hindering its ability to fully improve soil structure and enhance cation exchange capacity, and it is also unsuitable for saline-alkali land. Therefore, peat activation is a crucial step in its high-value utilization.

[0003] Currently, peat activation technology is mainly divided into two categories: chemical activation and biological activation. In terms of chemical activation, existing technologies include using ammonium bicarbonate (Ammonium carbonate) as an ammonifying agent for dry ammoniation of peat (patent publication number CN103992168A), increasing the content of water-soluble humic acid, or using triethanolamine to chemically modify humic acid (patent publication number CN116622089A). In terms of biological activation, existing technologies include inoculating peat with microbial agents such as Aspergillus niger for open-air fermentation (patent publication number CN 106495792 A), or using compound microbial inoculants for aerobic fermentation of woody peat to activate the humic acid (patent publication number CN 110229039 A).

[0004] However, the aforementioned existing technologies all have significant limitations: chemical activation requires pre-drying or air-drying of the peat, resulting in high energy consumption, large equipment investment, complex operation, and safety hazards due to the high temperature and pressure conditions. While traditional ammoniation reagents, such as ammonium bicarbonate or ammonia, are lower in cost, their activation efficiency is limited, and the increase in water-soluble humic acid in the product is poor. Technologies using ethanolamines to modify humic acid involve modifying the extracted purified humic acid in a purely chemical system, rather than directly activating the native peat in situ. This results in complex processes, high costs, and difficulty in large-scale application. Although biological activation is environmentally friendly, relying solely on microbial degradation has a long cycle and insufficient activation depth, and usually requires the addition of specific bacterial strains or enzymes, increasing process complexity and production costs. Furthermore, in existing technologies, chemical and biological activation are typically performed sequentially as independent steps, failing to solve the industrialization challenge of directly activating medium-to-high moisture native peat without drying.

[0005] Therefore, there is an urgent need to develop a peat treatment method that can achieve chemical-biological synergistic activation within the same system, without the need for pre-drying and the addition of bacterial agents. This method would directly treat high-moisture peat using a low-cost solid-state process, efficiently converting insoluble humic acid into a water-soluble active form, and obtaining activated peat products with high water-soluble humic acid content and high cation exchange capacity. This would meet the urgent need for high-quality peat-based materials in saline-alkali land improvement. Summary of the Invention

[0006] The purpose of this invention is to provide an activated peat and its activation method. This activation method can simultaneously achieve chemical activation and biological activation, and directly process high-moisture peat with a low-energy consumption, short cycle, and no-drying solid process to obtain activated peat with high water-soluble humic acid content and significantly improved cation exchange capacity.

[0007] To achieve the above objectives, the technical solution adopted by the present invention is as follows: The first aspect of this invention provides a method for activating peat, comprising the following steps: S1. Pre-treat wet peat to obtain wet peat fragments; S2. Apply the diluted monoethanolamine solution to the wet peat fragments obtained in step S1 by atomized spraying, and simultaneously turn the wet peat fragments and mix in desulfurized gypsum and urea. After spraying, build up the pile to obtain strip piles. S3. The strip pile obtained in step S2 is subjected to aerobic fermentation activation treatment. The pile is turned over regularly and the temperature of the strip pile is controlled not to exceed 60°C. When the wet peat is determined to have completed the expected activation, the activated peat is obtained.

[0008] In step S1, the wet peat is preferably lowland black peat. The pretreatment involves crushing the wet peat until the particle size is ≤5cm, thus obtaining wet peat fragments. The pretreatment does not require pre-drying or air-drying, resulting in low energy consumption. This crushing process has the dual functions of particle size control and mechanical dissociation of fiber bundles. Under shearing and kneading action, the interwoven plant fibers split and disperse longitudinally, increasing the specific surface area. This provides a sufficient interface for capillary wetting of the monoethanolamine dilution and attachment and proliferation of aerobic microorganisms, thereby improving the synergistic activation efficiency of chemical amination and biodegradation.

[0009] In step S2, the primary amino groups of monoethanolamine undergo an amination reaction with the carboxyl and phenolic hydroxyl groups of total humic acid, which exists in insoluble free and metal-bound states in wet peat fragments, to generate water-soluble humic acid ethanolamine salt. This transforms the coiled humic acid macromolecules into an extended conformation with hydrophilic groups, exposing more active functional groups, thus achieving chemical activation and increasing the content of water-soluble humic acid. Simultaneously, the desulfurization gypsum reduces sodium through calcium-sodium ion exchange, and the calcium ions react with CO3 in the system. 2- HCO3 -Plasma precipitation directly consumes alkaline substances that cause pH increases, buffering excessively high pH levels and preventing caking. Under these buffering conditions, urea will not decompose rapidly due to strong alkali; its slowly released free ammonia can further participate in humic acid amination, forming a synergistic activation with monoethanolamine. Simultaneously, monoethanolamine and urea can also synergistically serve as a nitrogen source to promote the proliferation of aerobic microorganisms. Atomized spraying combined with simultaneous turning ensures uniform distribution of all components and avoids the formation of localized strong alkaline zones. In step S3, the strip pile undergoes fermentation activation under aerobic conditions: during the heating period, the metabolic heat generated by aerobic microorganisms accelerates the amination reaction. Simultaneously, during metabolism, aerobic microorganisms degrade the inherent lignin and macromolecular humic substances in the peat, releasing previously encapsulated humic acid molecules (existing in insoluble free and metal-bound states), exposing more carboxyl and phenolic hydroxyl groups and promoting a full amination reaction. Turning the pile breaks up local anaerobic zones and homogenizes the pile. Subsequent turning maintains oxygen supply and the temperature is controlled at no more than 60°C throughout the process to avoid thermal reversal of humic acid condensation. Activated peat is obtained when the expected activation index is reached.

[0010] In some embodiments, the wet peat has a moisture content of 50-60%.

[0011] In some embodiments, the monoethanolamine diluent is prepared by diluting monoethanolamine with deionized water at a mass ratio of 1:(3-5).

[0012] In some embodiments, the amount of monoethanolamine added is 1.2-1.8 parts by weight, based on 100 parts by weight of the total wet peat pellets.

[0013] By adjusting the amount of monoethanolamine added, the dual requirements of chemical activation efficiency and maintenance of microbial activity can be met. Sufficient monoethanolamine ensures full amination with the carboxyl and phenolic hydroxyl groups of total humic acid, generating a sufficient amount of water-soluble humic acid ethanolamine salt, thereby increasing the water-soluble humic acid content and cation exchange capacity. Simultaneously, this addition amount maintains the pile pH within the range tolerable by aerobic microorganisms (pH ≤ 9.0), avoiding excessive alkalinity that inhibits microbial metabolism. This ensures that monoethanolamine and urea work synergistically as nitrogen sources to continuously activate the aerobic fermentation process of aerobic microorganisms, achieving a synergistic effect of chemical and biological activation.

[0014] In some embodiments, based on 100 parts of the total mass of the wet peat fragments, the amount of desulfurized gypsum added is 0.8-1.2 parts by mass, and the amount of urea added is 0.4-0.6 parts by mass.

[0015] Within this ratio range, desulfurized gypsum and urea work synergistically to ensure the full progress of the chemical amination reaction while maintaining the system's pH stability and microbial metabolic activity. This results in the activated product having low sodium content, loose granular structure, and suitable physicochemical properties, meeting the multiple requirements of saline-alkali land for activated peat with low sodium content, high cation exchange capacity, and stable structure.

[0016] In some embodiments, the strip pile is a loose, uncompacted, aerated pile with a width-to-height ratio of (1.3-2.1):1.

[0017] The length of the strip pile is unlimited, and the range of its width-to-height ratio is determined based on the balance between the oxygen diffusion depth and the self-insulating effect of the pile during aerobic fermentation. It can maintain the aerobic state of the entire pile by regularly turning it over without the need for forced ventilation equipment, thus combining low equipment investment with stable activation effect.

[0018] In some embodiments, the activation process in step S3 specifically includes the following steps: A1. On days 1-3, the temperature of the strip pile naturally rises to 45-55℃, resulting in preliminarily activated peat. A2. On days 4-7, the preliminarily activated peat is turned over to obtain a homogenized pile. A3. During days 8-14, maintain the temperature of the homogenized pile at 40-50°C and turn the pile over every 4-6 days to obtain deeply activated peat. A4. During days 15-18, the deeply activated peat undergoes continuous fermentation, and the activated peat is obtained when the expected activation is determined to be completed.

[0019] In some embodiments, when the content of water-soluble humic acid in the deeply activated peat is greater than or equal to 32%, the pH is 8.0-8.6, and the percentage increase in cation exchange capacity compared to before activation is greater than or equal to 25%, the wet peat is determined to have completed the expected activation, and thus the activated peat is obtained.

[0020] The activation endpoint is reached when the water-soluble humic acid content of deeply activated peat is greater than or equal to 32%, the pH is 8.0-8.6, the cation exchange capacity increases by greater than or equal to 25% compared to before activation, and the peat strips are free of foul odor and have a loose granular structure. The water-soluble humic acid content directly reflects the degree of conversion of insoluble humic acid by the chemical amination reaction. The increase in cation exchange capacity reflects the synergistic contribution of chemical activation (introducing hydrophilic groups to expose active sites) and biological activation (microbial degradation of macromolecules releasing encapsulated functional groups). A pH controlled between 8.0 and 8.6 indicates that the amount of monoethanolamine added is appropriate and there is no excessive alkali residue, and also indicates that the aerobic microorganisms in the deeply activated peat are metabolically active and have not been inactivated due to excessively high pH. The absence of foul odor and the loose granular structure sensorily confirm that the peat strips have not undergone anaerobic putrefaction and have a good structure, which can serve as a rapid auxiliary basis for on-site judgment. This multi-indicator joint judgment method takes into account both the needs of precise laboratory testing and on-site sensory verification, ensuring that the output product has stable and reproducible activated quality.

[0021] In some embodiments, the total humic acid content in the wet peat is greater than or equal to 30 wt%, and the organic matter content is ≥50 wt%.

[0022] A second aspect of the present invention provides activated peat, which is prepared by the activation method described above.

[0023] When used directly as a soil conditioner, this activated peat can be applied directly to the field after being naturally dried to reduce its moisture content to 35%-45%. At this point, the activated peat remains loose and granular, making it easy to spread without further processing. When used as a raw material for water-soluble fertilizers, this activated peat can be further dehydrated and dried, or directly mixed with water to form a pulp, filtered, and the water-soluble humic acid active components extracted for use in the formulation of liquid or water-soluble fertilizers.

[0024] Compared with the prior art, the technical solution of the present invention has the following technical effects: 1. The activation method of the present invention can simultaneously achieve chemical activation and biological activation, and directly process high-moisture peat with a low-energy consumption, short cycle and no drying process to obtain activated peat with high water-soluble humic acid content and significantly improved cation exchange capacity.

[0025] 2. This invention integrates the chemical amination of monoethanolamine with aerobic fermentation in the same system. Chemical amination involves the reaction of monoethanolamine with the carboxyl and phenolic hydroxyl groups of total humic acid (mainly in insoluble free and metal-bound states) to generate water-soluble humic acid ethanolamine salts, extending the humic acid macromolecular chains and exposing more active sites. Simultaneously, aerobic microorganisms metabolize and degrade lignin, macromolecular humic substances, and other plant tissues in the wet peat fragments, releasing previously encapsulated humic acid molecules, further exposing their carboxyl and phenolic hydroxyl groups to participate in the amination reaction. These two processes mutually promote and complement each other, achieving a synergistic effect of chemical and biological activation in the same solid-state system, significantly increasing both the water-soluble humic acid content and cation exchange capacity of the activated peat.

[0026] 3. The synergistic use of urea and desulfurized gypsum can effectively regulate the carbon-nitrogen ratio of wet peat fragments, maintain pH stability, promote the proliferation and metabolic activity of inherent aerobic microorganisms in wet peat, reduce the sodium content of activated peat and improve the agglomeration structure, thereby enhancing the adaptability of activated peat to saline-alkali land. Detailed Implementation

[0027] Various exemplary embodiments of the present invention will now be described in detail. This detailed description should not be considered as a limitation of the present invention, but rather as a more detailed description of certain aspects, features, and embodiments of the present invention.

[0028] It should be understood that the terminology used in this invention is merely for describing particular embodiments and is not intended to limit the invention. Furthermore, with respect to numerical ranges in this invention, it should be understood that each intermediate value between the upper and lower limits of the range is also specifically disclosed. Every smaller range between any stated value or intermediate value within a stated range, and any other stated value or intermediate value within said range, is also included in this invention. The upper and lower limits of these smaller ranges may be independently included or excluded from the range.

[0029] Unless otherwise stated, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art. While only preferred methods and materials have been described herein, any methods and materials similar or equivalent to those described herein may be used in the implementation or testing of the invention. Various modifications and variations to the specific embodiments described in this specification are apparent to those skilled in the art without departing from the scope or spirit of the invention. Other embodiments derived from this specification will be apparent to those skilled in the art. This application specification and embodiments are merely exemplary.

[0030] The following detailed description uses specific examples and comparative examples, all of which are commercially available. Specifically, the wet peat was purchased from Ekertry Peat Research and Production Co., Ltd. in Russia, monoethanolamine was purchased from Zibo Xinzhonghui Chemical Co., Ltd., and desulfurized gypsum was purchased from Guizhou Zhuoshengfengye Environmental Protection New Material Development Co., Ltd.

[0031] Total humic acid content was tested according to GB / T 34766-2017 "Determination of Total Humic Acid Content from Mineral Sources"; cation exchange capacity was determined according to the ammonium acetate exchange method (refer to LY / T 1243-1999); water-soluble humic acid content was determined according to NY / T 1971-2010 "Determination of Humic Acid Content in Water-Soluble Fertilizers" using the potassium dichromate redox titration method after acid precipitation; pH value of activated peat was determined according to DB22 / T 2242-2015 "Determination of pH Value of Peat and Its Products" using the potentiometric method; sodium adsorption ratio was determined according to LY / T 2445-2015 "Technical Specification for Topsoil Protection for Greening" (Appendix H) by measuring the Na+ content in the activated peat extract. + Ca 2+ Mg 2+ After adjusting the ion concentration, use the formula: Sodium adsorption ratio = Na + / √((Ca 2+ +Mg 2+ The result is calculated as ) / 2).

[0032] Example 1 The activation method for activated peat includes the following steps: S1. Take 100 kg of wet peat (moisture content 55%, total humic acid content 42 wt%, organic matter content 65 wt%, pH 5.8), crush it with a single-shaft crusher, and control the peat particle size ≤ 5 cm to obtain wet peat fragments. S2. Apply 7500 mL of monoethanolamine dilution (monoethanolamine (purity ≥99%) to deionized water in a mass ratio of 1:4) to 100 kg of wet peat fragments obtained in step S1 by atomized spraying. Simultaneously turn the wet peat fragments and mix in 1000 g of desulfurized gypsum and 500 g of urea. After spraying, build up the pile to obtain a strip pile (width 1.0 m, height 0.6 m, length 0.8 m). S3. Place the strip pile obtained in step S2 under open-air conditions for aerobic fermentation activation treatment. Cover the surface of the strip pile with a layer of breathable heat-insulating covering material, turn the pile regularly and control the temperature of the strip pile to not exceed 60°C. When it is determined that the wet peat has completed the expected activation, activated peat is obtained.

[0033] The activation process specifically includes the following steps: A1. During the first 1-3 days, the temperature of the peat pile naturally rises to 50°C, resulting in preliminarily activated peat. A2. On days 4-7, the pile is turned over on day 5. The material inside and outside the pile is completely replaced by manual turning. After turning, the pile is rebuilt into a pile of the same specifications to obtain a homogeneous pile. A3. During days 8-14, maintain the temperature of the homogenized pile at 45°C, turn the pile over every 5 days, and perform the same turning operation as step A2 each time to obtain deeply activated peat; if the pile temperature exceeds 50°C, uncover the covering to accelerate heat dissipation, and cover it again when the temperature drops below 45°C. A4. On days 15-18, continue to maintain an aerobic state, stop turning the pile, and allow the deeply activated peat to mature naturally. The deeply activated peat undergoes continuous fermentation. Throughout the process, the temperature of the pile is monitored in real time by a thermometer buried in the center of the pile to ensure that the temperature of the pile does not exceed 60°C. When the expected activation is completed, the activated peat is obtained.

[0034] Activation endpoint determination: On the 16th day, the water-soluble humic acid content in the pile was 34.6%, the pH value was 8.2, the cation exchange capacity was 61 cmol / kg, which was 27.1% higher than before activation (48 cmol / kg), the sodium adsorption ratio was 5.8, the pile had no foul odor, and was loose and granular, which met the expected activation indicators, and thus the activated peat product was obtained.

[0035] Example 2 The activation method for activated peat includes the following steps: S1. Take 100 kg of wet peat (moisture content 60%, total humic acid content 30 wt%, organic matter content 50 wt%, pH 5.5), crush it with a single-shaft crusher, and control the peat particle size ≤ 5 cm to obtain wet peat fragments. S2. Apply 9000 mL of monoethanolamine dilution (monoethanolamine (purity ≥99%) to deionized water in a mass ratio of 1:5) to 100 kg of wet peat fragments obtained in step S1 by atomized spraying. Simultaneously turn the wet peat fragments and mix in 1200 g of desulfurized gypsum and 600 g of urea. After spraying, build up the pile to obtain a strip pile (width 1.2 m, height 0.6 m, length 0.7 m). S3. Place the strip pile obtained in step S2 under open-air conditions for aerobic fermentation activation treatment. Cover the surface of the strip pile with a layer of breathable heat-insulating covering material, turn the pile regularly and control the temperature of the strip pile to not exceed 60°C. When it is determined that the wet peat has completed the expected activation, activated peat is obtained.

[0036] The activation process specifically includes the following steps: A1. During the first 1-3 days, the temperature of the peat pile naturally rises to 55℃, resulting in preliminarily activated peat. A2. On days 4-7, the pile is turned over on day 4. The material inside and outside the pile is completely replaced by manual turning. After turning, the pile is rebuilt into a pile of the same specifications to obtain a homogenized pile. A3. During days 8-14, maintain the temperature of the homogenized pile at 50°C. Turn the pile over every 4 days, and perform the same turning operation as step A2 each time to obtain deeply activated peat. If the pile temperature exceeds 50°C, the covering can be removed to accelerate heat dissipation. When the temperature drops below 50°C, cover it again. A4. On days 15-18, continue to maintain an aerobic state, stop turning the pile, and allow the deeply activated peat to mature naturally. The deeply activated peat undergoes continuous fermentation. Throughout the process, the temperature of the pile is monitored in real time by a thermometer buried in the center of the pile to ensure that the temperature of the pile does not exceed 60°C. When the expected activation is completed, the activated peat is obtained.

[0037] Activation endpoint determination: On the 18th day, the water-soluble humic acid content in the pile was 33.8%, the pH value was 8.6, the cation exchange capacity was 60 cmol / kg, which was 30.4% higher than before activation (46 cmol / kg), the sodium adsorption ratio was 5.5, the pile had no foul odor, and was loose and granular, which met the expected activation indicators, and thus the activated peat product was obtained.

[0038] Example 3 The activation method for activated peat includes the following steps: S1. Take 100 kg of wet peat (moisture content 50%, total humic acid content 38 wt%, organic matter content 55 wt%, pH 6.0), crush it with a single-shaft crusher, and control the peat particle size ≤ 5 cm to obtain wet peat fragments. S2. Apply 6000 mL of monoethanolamine dilution (monoethanolamine (purity ≥99%) to deionized water in a mass ratio of 1:3) to 100 kg of wet peat fragments obtained in step S1 by atomized spraying. Simultaneously turn the wet peat fragments and mix in 800 g of desulfurized gypsum and 400 g of urea. After spraying, build up the pile to obtain a strip pile (width 0.91 m, height 0.7 m, length 0.9 m). S3. Place the strip pile obtained in step S2 under open-air conditions for aerobic fermentation activation treatment. Cover the surface of the strip pile with a layer of breathable heat-insulating covering material, turn the pile regularly and control the temperature of the strip pile to not exceed 60°C. When it is determined that the wet peat has completed the expected activation, activated peat is obtained.

[0039] The activation process specifically includes the following steps: A1. During the first 1-3 days, the temperature of the peat pile naturally rises to 45°C, resulting in preliminarily activated peat. A2. On days 4-7, the pile is turned over on day 7. The material inside and outside the pile is completely replaced by manual turning. After turning, the pile is rebuilt into a pile of the same specifications to obtain a homogenized pile. A3. During days 8-14, maintain the temperature of the homogenized pile at 40°C. Turn the pile over every 6 days, and perform the same turning operation as step A2 each time to obtain deeply activated peat. If the pile temperature exceeds 50°C, the covering can be removed to accelerate heat dissipation. When the temperature drops below 50°C, cover it again. A4. On days 15-18, continue to maintain an aerobic state, stop turning the pile, and allow the deeply activated peat to mature naturally. The deeply activated peat undergoes continuous fermentation. Throughout the process, the temperature of the pile is monitored in real time by a thermometer buried in the center of the pile to ensure that the temperature of the pile does not exceed 60°C. When the expected activation is completed, the activated peat is obtained.

[0040] Activation endpoint determination: On the 14th day, the water-soluble humic acid content in the pile was 32.5%, the pH value was 8.0, the cation exchange capacity was 61 cmol / kg, which was 27.1% higher than before activation (48 cmol / kg), the sodium adsorption ratio was 5.6, the pile had no foul odor, and was loose and granular, which met the expected activation indicators, and thus the activated peat product was obtained.

[0041] Comparative Example 1 Comparative Example 1 provides an activated peat and its activation method, which differs from Example 1 in that monoethanolamine is replaced with an equal amount of ammonium bicarbonate.

[0042] Test results: On day 16, the water-soluble humic acid content was 12.3%, the pH value was 6.8, and the cation exchange capacity was 52 cmol / kg, which was 8.3% higher than before activation (48 cmol / kg).

[0043] Comparative Example 2 Comparative Example 2 provides an activated peat and its activation method, which differs from Example 1 in that monoethanolamine is replaced with an equal amount of triethanolamine.

[0044] Test results: On day 16, the water-soluble humic acid content was 11.8%, the pH value was 7.2, and the cation exchange capacity was 53 cmol / kg, which was 10.4% higher than before activation (48 cmol / kg).

[0045] Comparative Example 3 Comparative Example 3 provides an activated peat and its activation method. The difference from Example 1 is that the amount of monoethanolamine diluent used in step S2 is adjusted to 11000 mL.

[0046] Results: On the second day after pile construction, the local pH of the pile reached 9.7. The pile temperature only rose to 38℃ on the third day and then stopped rising. A pungent amine odor was noticeable when turning the pile. After 16 days of fermentation, the water-soluble humic acid content was 12.5%, the pH value was 9.2, and the cation exchange capacity was 51 cmol / kg, which was 6.3% higher than before activation (48 cmol / kg). The product had a distinctly foul odor.

[0047] Comparative Example 4 Comparative Example 4 provides an activated peat and its activation method, which differs from Example 1 in that no desulfurized gypsum is added.

[0048] Test results: The water-soluble humic acid content was 30.1%, the pH value was 8.5, the cation exchange capacity was 58 cmol / kg, which was 20.8% higher than before activation (48 cmol / kg), and the sodium adsorption ratio was 12.5.

[0049] Comparative Example 5 Comparative Example 5 provides an activated peat and its activation method, which differs from Example 1 in that the width of the strip pile is 0.5m, the height is 0.7m, and the length is 0.7m.

[0050] Results: Although the temperature at the center of the pile rose to 52℃ on day 3, it rapidly dropped to below 35℃ after day 8 due to the narrow and tall pile and large heat dissipation area, making it impossible to maintain a deep fermentation temperature of 40-50℃ thereafter. After 16 days of fermentation, the water-soluble humic acid content was 22.4%, the pH value was 7.8, and the cation exchange capacity was 56 cmol / kg, an increase of 16.7% compared to before activation (48 cmol / kg).

[0051] Comparative Example 6 Comparative Example 6 provides an activated peat and its activation method, which differs from Example 1 in that the activation treatment is replaced by the following steps: A1. During the first 1-3 days, the temperature of the peat pile naturally rises to 45°C, resulting in preliminarily activated peat. A2. On days 4-7, the pile is turned over on day 7. The material inside and outside the pile is replaced by manual turning. After turning, the pile is rebuilt into a pile of the same specifications to obtain a homogenized pile. A3. On days 8-14, the temperature continues to rise to 68℃. Without any cooling treatment, the pile is turned over every 6 days, and each turning operation is the same as step A2, to obtain deeply activated peat. A4. During days 15-18, continue to maintain the natural state, stop turning the pile, and allow the deeply activated peat to mature naturally. The deeply activated peat will continue to ferment. Throughout the process, the temperature of the pile will be monitored in real time by a thermometer buried in the center of the pile, but no temperature intervention will be made.

[0052] Results: On day 16, the water-soluble humic acid content was 9.8%, the pH value was 8.0, and the cation exchange capacity was 49 cmol / kg, which was only 2.1% higher than before activation (48 cmol / kg). The product was in the form of black hard lumps.

[0053] Performance testing: 1. Test soil The soil samples were taken from the top 10cm layer of a typical saline-alkali land area. The soil type was inland saline-alkali soil (soil pH value of 9, total salt content of 4g / kg, and exchangeable sodium percentage of 20%). After collection, the soil was air-dried and sieved through a 2mm sieve for later use.

[0054] 2. Experimental Design The experiment used a pot experiment method and set up the following treatment groups: (1) Blank control group: No activated peat was added, and only indicator crops were planted.

[0055] (2) Examples 1-3: The activated peat prepared in Examples 1-3 were added respectively.

[0056] (3) Comparative Examples 1-6: The activated peat prepared in Comparative Examples 1-6 were added respectively.

[0057] Each treatment group was replicated in triplicate using a randomized block design. Each pot contained 5.0 kg of test soil, with 200 g of activated peat added per pot on an air-dried basis. The peat was thoroughly mixed with the soil before potting. All treatment groups were managed under identical environmental conditions, including uniform watering, natural light, and a temperature maintained at 25℃.

[0058] 3. Indicator crop planting The indicator crop used in the experiment was wheat, which is sensitive to salt and alkali stress. 20 seeds were sown per pot, and the seedlings were thinned to 10 plants per pot after emergence. The planting period was 45 days, during which the management conditions such as watering and light were kept consistent across all treatment groups.

[0059] 4. Crop growth index measurement After planting, the growth of the indicator crops in each treatment group was measured, and the specific indicators are as follows: (1) Emergence rate: On the 7th day after sowing, the number of seedlings in each treatment group was counted and the emergence rate (%) was calculated.

[0060] (2) Plant height: After planting, select 5 representative plants from each pot and measure the natural height from the base of the root to the highest leaf tip, and take the average value (cm).

[0061] (3) Aboveground biomass: The aboveground part of the indicator crop was cut from the root base, blanched at 105℃ for 30 min, dried at 75℃ to constant weight, and the aboveground dry matter mass (g / pot) was measured.

[0062] (4) Root dry weight: Remove all the soil from the pot, separate the roots, rinse them with deionized water, dry them at 75℃ to constant weight, and weigh the dry weight of the roots (g / pot).

[0063] (5) Growth observation: Observe and record the leaf color, plant growth, root development and salt damage symptoms (such as yellowing and wilting of leaves) of each treatment group. The score is based on a 10-point scale, where 8-10 points is excellent (dark green leaves, strong plants, well-developed roots, no salt damage symptoms), 5-7 points is good (greener leaves, taller plants, well-developed roots, mild salt damage symptoms), and 1-4 points is poor (yellowed or wilted leaves, short plants, sparse roots, severe salt damage symptoms). The higher the score, the better the crop growth.

[0064] Table 1 below shows the comprehensive performance comparison results of the activated peat prepared in the examples and the comparative examples.

[0065] Table 1 As shown in Table 1, the activated peat prepared in Examples 1-3 is superior to the blank control group and the comparative examples in all growth indicators, indicating that the activated peat prepared by the present invention can effectively alleviate the inhibitory effect of salt and alkali stress on crop seed germination and plant growth, and promote the growth of crops in saline-alkali land.

[0066] Comparative Example 1 used ammonium bicarbonate instead of monoethanolamine as the activator. Due to the limited ammoniation efficiency of ammonium bicarbonate, it could not undergo an effective amination reaction with total humic acid (mainly insoluble free and metal-bound states), resulting in a significantly lower growth-promoting effect of activated peat on crops in saline-alkali soil compared to the examples. Comparative Example 2 used triethanolamine instead of monoethanolamine. Because the tertiary amine group of triethanolamine lacks active hydrogen, it could not undergo a dehydration condensation reaction with the carboxyl groups of total humic acid in the wet peat fragments, only forming a very weak physical adsorption. Its effect on improving saline-alkali soil was weaker than in the examples. In Comparative Example 3, the amount of monoethanolamine added exceeded the limits specified in this invention, leading to excessively high alkalinity in the peat pile, inhibiting the activity of aerobic microorganisms, and resulting in poor crop growth promotion effect of the activated peat. Comparative Example 4 did not add desulfurized gypsum. The activated peat had a high exchangeable sodium content and large local pH fluctuations, resulting in a lower improvement effect on saline-alkali soil compared to the examples. This indicates that the sodium-reducing and pH-buffering functions of desulfurized gypsum contribute to the applicability of activated peat in saline-alkali soils. In Comparative Example 5, the width-to-height ratio of the peat pile exceeded the limits defined in this invention. The excessively narrow and tall pile resulted in rapid heat dissipation, making it impossible to maintain the deep fermentation temperature and leading to insufficient activation. Consequently, the growth-promoting effect of the activated peat on crops in saline-alkali soil was significantly reduced. In Comparative Example 6, no temperature control measures were taken during fermentation, and the pile temperature exceeded 60°C. The amination of water-soluble humic acid ethanolamine salts underwent thermally induced decarboxylation and cross-linking condensation reactions, reverting to an insoluble state. This resulted in poor crop growth promotion efficacy of the activated peat.

[0067] Therefore, those skilled in the art should recognize that although numerous exemplary embodiments of the present invention have been shown and described in detail herein, many other variations or modifications conforming to the principles of the present invention can be directly determined or derived from the disclosure of the present invention without departing from the spirit and scope of the invention. Thus, the scope of the present invention should be understood and construed as covering all such other variations or modifications.

Claims

1. A method for activating peat, characterized in that, Includes the following steps: S1. Pre-treat wet peat to obtain wet peat fragments; S2. Apply the diluted monoethanolamine solution to the wet peat fragments obtained in step S1 by atomized spraying, and simultaneously turn the wet peat fragments and mix in desulfurized gypsum and urea. After spraying, build up the pile to obtain strip piles. S3. The strip pile obtained in step S2 is subjected to aerobic fermentation activation treatment. The pile is turned over regularly and the temperature of the strip pile is controlled not to exceed 60°C. When the wet peat is determined to have completed the expected activation, the activated peat is obtained.

2. The activation method according to claim 1, characterized in that, The wet peat contains 50-60% moisture.

3. The activation method according to claim 1, characterized in that, The monoethanolamine diluent was prepared by diluting monoethanolamine with deionized water at a mass ratio of 1:(3-5).

4. The activation method according to claim 3, characterized in that, Based on 100 parts of the total mass of the wet peat fragments, the amount of monoethanolamine added is 1.2-1.8 parts by mass.

5. The activation method according to claim 1, characterized in that, Based on 100 parts of the total mass of the wet peat fragments, the amount of desulfurized gypsum added is 0.8-1.2 parts by mass, and the amount of urea added is 0.4-0.6 parts by mass.

6. The activation method according to claim 1, characterized in that, The strip pile is a loose, uncompacted, aerated pile with a width-to-height ratio of (1.3-2.1):

1.

7. The activation method according to claim 1, characterized in that, The activation process in step S3 specifically includes the following steps: A1. On days 1-3, the temperature of the strip pile naturally rises to 45-55℃, resulting in preliminarily activated peat. A2. On days 4-7, the preliminarily activated peat is turned over to obtain a homogenized pile. A3. During days 8-14, maintain the temperature of the homogenized pile at 40-50°C and turn the pile over every 4-6 days to obtain deeply activated peat. A4. During days 15-18, the deeply activated peat undergoes continuous fermentation, and the activated peat is obtained when the expected activation is determined to be completed.

8. The activation method according to claim 7, characterized in that, When the content of water-soluble humic acid in the deeply activated peat is greater than or equal to 32%, the pH is 8.0-8.6, and the percentage increase in cation exchange capacity compared to before activation is greater than or equal to 25%, the wet peat is determined to have completed the expected activation, and thus the activated peat is obtained.

9. The activation method according to claim 1, characterized in that, The wet peat contains a total humic acid content greater than or equal to 30 wt% and an organic matter content greater than or equal to 50 wt%.

10. An activated peat, characterized in that, The activated peat is prepared by the activation method according to any one of claims 1-9.

Citation Information

Patent Citations

  • Preparation method of ammonuim humate fertilizer

    CN103992168A

  • Production technology of peat organic granular fertilizer

    CN106495792A

  • Method for biologically activating humic acid in wood peat and prepared bio-organic fertilizer

    CN110229039A

  • Multi-sulfonic-group anti-flocculation humic acid as well as preparation method and application thereof

    CN116622089A