A high-strength adhesive for bonding automotive metal structures and its preparation method
By improving the formulation and preparation process of the adhesive for bonding automotive metal structures, using ternary toughening agents, composite curing agents, and gradient-graded fillers, combined with gradient temperature-controlled vacuum stirring process, the problems of insufficient toughness and imbalance in storage and curing performance in existing technologies have been solved. This has resulted in high strength, environmental resistance, and construction stability, making it suitable for bonding modern automotive metal structures.
Patent Information
- Application Number
- CN202610947353.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-06-29
- Publication Date
- 2026-11-17
AI Technical Summary
Existing single-component epoxy adhesives for automotive metal structures suffer from problems such as insufficient toughness, imbalance between storage and curing performance, poor interfacial environmental resistance, poor application performance, and weak stability of the manufacturing process, which cannot meet the needs of modern automobiles for lightweighting, energy-saving production, and long service life.
A high-strength adhesive was prepared by using bisphenol F epoxy resin and flexible epoxy resin as the base resin matrix, combined with ternary composite toughening agent, composite latent curing agent, silane-titanium ester composite interface modifier, gradient-grade inorganic filler, composite rheology modifier and composite functional agent, through a three-step gradient temperature-controlled vacuum stirring process.
It significantly improves the peel strength, impact resistance, and fatigue resistance of the adhesive layer, extends the room temperature storage period, improves the brittleness problem under low temperature conditions, and enhances the salt spray resistance, damp heat resistance, and construction stability of the adhesive layer, making it suitable for the long-term service environment of automotive metal structures.
Abstract
Description
Technical Field
[0001] This invention belongs to the field of epoxy structural adhesive technology, and more specifically, it relates to a high-strength adhesive for bonding automotive metal structures and its preparation method. Background Technology
[0002] With the continuous development of automotive lightweighting technology, traditional welding and riveting processes are gradually being replaced by structural bonding processes. Metal structural components such as automotive body pillars, chassis floor plates, body side panels, and wheel arches are commonly bonded and assembled using epoxy structural adhesives. This type of application places several stringent requirements on adhesives: high bond strength, good toughness, resistance to high and low temperature cycling, salt spray resistance, and resistance to damp heat. They must also be compatible with the electrophoretic curing process in automotive production lines and possess the characteristics of convenient application and room temperature storage stability.
[0003] Currently, the most widely used adhesives on the market are solvent-free single-component epoxy structural adhesives. The conventional formulation of this type of adhesive uses bisphenol F epoxy resin or flexible epoxy resin as the base resin, selects ultrafine dicyandiamide combined with substituted urea as the latent curing system, uses a single core-shell rubber or polyurethane as the toughening component, and combines a single silane coupling agent, ordinary silica powder filler and conventional rheology modifiers. The preparation generally adopts a two-step mixing process: first mix the resin and conventional additives, then add the curing system, stir, degas, and dispense.
[0004] Traditional adhesives often use a single toughening component, making it difficult to balance the rigidity and toughness of the resin matrix, resulting in a brittle adhesive layer. Under long-term vehicle vibration and low-temperature environments, they are prone to microcracks and fatigue failure, and their peel strength is insufficient, failing to meet the long-term service requirements of automotive structural components.
[0005] In summary, existing single-component epoxy adhesives for automotive metal structures suffer from numerous problems, including insufficient toughness, imbalanced storage and curing properties, poor interfacial environmental resistance, unsatisfactory application performance, and weak stability of the manufacturing process. These shortcomings make them unsuitable for the modern automotive industry's demands for lightweight construction, energy-efficient production, and long service life. This invention addresses these deficiencies by comprehensively optimizing and improving the adhesive formulation system and manufacturing process, providing a high-strength adhesive with superior overall performance suitable for automotive mass production lines, along with its preparation method. Summary of the Invention
[0006] To address the aforementioned technical problems, this invention provides a high-strength adhesive for bonding automotive metal structures and its preparation method, thereby resolving the problems.
[0007] A high-strength adhesive for bonding automotive metal structures, using bisphenol F epoxy resin and flexible epoxy resin as base resin matrices, includes a ternary composite toughening agent, a composite latent curing agent, a silane-titanium ester composite interface modifier, a gradient-graded inorganic filler, a composite rheology modifier, and a composite functional agent.
[0008] By weight, the adhesive components are distributed as follows: 20-30 parts bisphenol F epoxy resin, 10-20 parts flexible epoxy resin, 20-25 parts ternary composite toughening agent, 3-6 parts surface-modified ultrafine dicyandiamide, 2-5 parts substituted urea accelerator, 1-2 parts composite coupling agent, 3-8 parts composite functional agent, 10-25 parts gradient-graded silica powder, 0.2-0.3 parts fumed silica, 0.8-1.5 parts leveling agent, and 0.2-0.3 parts silicone defoamer.
[0009] Preferably, the ternary composite toughening agent is composed of a core-shell polymer toughening agent, a modified polyurethane toughening agent, and a carboxyl-terminated nitrile butadiene rubber; by weight, the core-shell polymer toughening agent comprises 12-16 parts, the modified polyurethane toughening agent comprises 5-7 parts, and the carboxyl-terminated nitrile butadiene rubber comprises 3-5 parts; the ternary composite toughening agent is dispersed in the resin matrix in a blending manner to form a multiphase toughening structure.
[0010] Preferably, the composite latent curing agent is a combination of surface-modified ultrafine dicyandiamide and substituted urea accelerator; the particle size D50 of the ultrafine dicyandiamide is controlled to be 3-4.5 μm, and the surface of the dicyandiamide is modified by coating with a silane coupling agent; the curing system remains inert at room temperature, and the curing reaction is initiated when the temperature rises above 140°C.
[0011] Preferably, the silane-titanium ester composite interface modifier is composed of KH-560 silane coupling agent and titanate coupling agent; the mass ratio of KH-560 to titanate coupling agent is 3:1; the composite functional agent is composed of cocoyl monoethanolamide, titanate, and acetylacetone mixed in a mass ratio of 3:2.5:1.8.
[0012] Preferably, the gradient-graded inorganic filler is composed of a compound of large-particle-size silica powder and nano-silica; the particle size D50 of the large-particle-size silica powder is 0.5-1 μm, and the particle size of the nano-silica is 20-50 nm; the mass ratio of large-particle-size silica powder to nano-silica is 15:3; the filler is surface activated by a coupling agent before use to form a dense packing structure inside the adhesive.
[0013] Preferably, the composite rheology modifier is composed of fumed silica and polyamide wax; by weight, fumed silica is 0.2-0.3 parts and polyamide wax is 0.1-0.2 parts; when the composite rheology modifier is in operation, it enables the adhesive to have thixotropic properties of static anti-sagging and dynamic easy flow.
[0014] Preferably, a method for preparing a high-strength adhesive for bonding automotive metal structures employs a three-step gradient temperature-controlled vacuum stirring process.
[0015] Overall operation process of preparation method: The first step is to mix the matrix resin, toughening system, filler and conventional additives;
[0016] After cooling in the second step, add the curing system and mix at low speed.
[0017] The third step is low-temperature vacuum homogenization, followed by cooling and packaging.
[0018] Preferably, the mixing equipment in the first step of the preparation method is a planetary mixer; the revolution speed is 20-30 rpm, the rotation speed is 500-600 rpm, the system temperature is 50-60℃; the vacuum degree is maintained at -0.095MPa, and the mixture is continuously stirred and dispersed for 25-35 minutes to complete the preparation of the matrix mixture.
[0019] Preferably, in the second step of the preparation method, a gradient cooling operation is performed, and the system temperature is reduced to 35-40℃; the revolution speed is 15-20 rpm, the rotation speed is 60-80 rpm, the vacuum degree is maintained at -0.095 MPa; the stirring time is 15-20 min, and the entire process is run at low speed to avoid premature triggering of the reaction in the curing system.
[0020] Preferably, the third step of the preparation method uses a vacuum homogenizer to complete the homogenization process; the system temperature is controlled below 40°C, the vacuum degree is -0.095MPa, and the homogenization time is 5 to 10 minutes; after homogenization, the system is rapidly cooled to below 25°C and then sealed and packaged at 20 to 25°C.
[0021] Compared with the prior art, the present invention has the following beneficial effects:
[0022] This invention employs a ternary toughening system composed of a core-shell polymer toughening agent, a modified polyurethane toughening agent, and a carboxyl-terminated nitrile butadiene rubber, forming a multiphase toughening structure within the resin matrix. Compared to a single toughening component, it significantly improves the peel strength, impact resistance, and fatigue resistance of the adhesive layer while ensuring the overall strength and modulus of the adhesive layer. It effectively addresses the problem of brittle fracture of the adhesive layer under low-temperature conditions, making it suitable for the long-term vibration and high / low temperature cycling service environment of automotive metal structures.
[0023] This invention modifies the surface of ultrafine dicyandiamide with a particle size D50 of 3-4.5 μm by coating it with a silane coupling agent. The curing component is in an inert and isolated state at room temperature, which greatly extends the storage period of the product at room temperature. With the synergistic effect of the substituted urea accelerator, the cross-linking curing reaction can be rapidly triggered in the temperature range of 140-150℃. This not only retains the high-temperature curing efficiency, but also solves the core problem of "mutual restriction between storage stability and curing activity" in the existing technology. At the same time, it is fully compatible with the mainstream electrophoresis production process in the automotive industry.
[0024] This invention employs a silane-titanium ester composite coupling agent combined with a specialized composite functional agent for synergistic modification, simultaneously enhancing the wetting ability and interfacial bonding strength of the adhesive to galvanized steel sheets, aluminum alloys, and hot-formed high-strength steel. The composite system forms a dense protective layer at the adhesive-metal interface, effectively blocking the penetration of moisture and salt spray, reducing the risk of debonding at dissimilar metal interfaces, and significantly improving the long-term salt spray and damp heat resistance of the adhesive system.
[0025] This invention employs a gradient-graded filler composed of large-particle-size silica micropowder and nano-silica, and the filler is pre-activated by a coupling agent. The filler is uniformly dispersed in the resin system without agglomeration, resulting in a denser internal packing of the adhesive layer. Simultaneously, it effectively reduces the coefficient of thermal expansion of the adhesive layer, minimizes the difference in physical properties between the adhesive layer and the metal substrate, alleviates internal stress caused by thermal cycling, and improves the long-term reliability of the bonded structure.
[0026] This invention combines polyamide wax with traditional fumed silica to form a composite rheology modifier, giving the adhesive stable thixotropic properties over a wide temperature range. When statically placed, it effectively prevents adhesive sagging, making it suitable for vertical workstations on vehicle bodies; during dynamic coating, it exhibits good flowability, avoiding defects such as pinholes, stringing, and adhesive buildup during automated dispensing and scraping processes, significantly improving the stability of the production line.
[0027] This invention employs a three-step gradient temperature-controlled vacuum stirring process, distinct from traditional methods. The curing system is added under low-temperature, low-speed stirring conditions, completely avoiding premature activation and deactivation of the curing agent due to heat generated by stirring friction. Multi-stage vacuum stirring and low-temperature homogenization effectively remove air bubbles from the adhesive solution, resulting in a dense, defect-free finished adhesive layer. The entire process effectively reduces performance deviations between different production batches, significantly improving overall product qualification rate and production stability.
[0028] The adhesive of this invention is a solvent-free formulation with low VOC content, meeting the environmental regulations of the automotive industry. All formulation components are commercially available raw materials, making raw material procurement convenient. The preparation process requires no modification to existing mass production equipment such as planetary mixers and vacuum homogenizers, and can be directly integrated into existing automotive adhesive production lines. The production process is simple, highly controllable, and suitable for large-scale industrial production.
[0029] The adhesive of this invention has excellent bonding effect on a variety of mainstream automotive metal substrates and can be widely used for bonding various metal structural parts such as automotive body pillars, chassis floor plates, and body side panels. It has strong versatility and can reduce the inventory and management costs of multiple types of adhesives for car manufacturers. Detailed Implementation
[0030] The embodiments of the present invention will be described in further detail below with reference to examples. These examples are for illustrative purposes only and should not be construed as limiting the scope of the invention.
[0031] A high-strength adhesive for bonding automotive metal structures and its preparation method are disclosed. The adhesive is a solvent-free, single-component epoxy structural adhesive commonly used in the automotive industry.
[0032] The adhesive uses conventional bisphenol F epoxy resin and flexible epoxy resin as the base resin matrix.
[0033] The adhesive is equipped with an improved functional system, including a ternary composite toughening system, a composite latent curing system, a silane-titanium ester composite interface modification system, a gradient-graded inorganic filler, a composite rheology modifier, and a composite functional agent.
[0034] By weight, the adhesive components are distributed as follows: 20-30 parts bisphenol F epoxy resin, 10-20 parts flexible epoxy resin, 20-25 parts ternary composite toughening agent, 3-6 parts surface-modified ultrafine dicyandiamide, 2-5 parts substituted urea accelerator, 1-2 parts composite coupling agent, 3-8 parts composite functional agent, 10-25 parts gradient-graded silica powder, 0.2-0.3 parts fumed silica, 0.8-1.5 parts leveling agent, and 0.2-0.3 parts silicone defoamer.
[0035] The adhesive operates by being stored in a sealed container at room temperature and then undergoing cross-linking and curing via high-temperature thermal triggering.
[0036] When applying the adhesive, the thickness of the adhesive layer should be controlled between 0.1 and 0.5 mm; the curing conditions are 140℃ to 150℃, and the temperature should be maintained for 8 to 12 minutes.
[0037] The preparation method differs from the conventional two-step mixing process in existing technologies by employing a three-step gradient temperature-controlled vacuum stirring process.
[0038] Overall operation process of preparation method: Step 1: Mix the matrix resin, toughening system, filler and conventional additives; the mixing equipment is a planetary mixer; the revolution speed is 20-30 rpm, the rotation speed is 500-600 rpm, the system temperature is 50-60℃; the vacuum degree is maintained at -0.095MPa, and the mixture is continuously stirred and dispersed for 25-35 minutes to complete the preparation of the matrix mixture;
[0039] After cooling in the second step, add the curing system and mix at low speed; perform gradient cooling operation, and reduce the system temperature to 35-40℃; the revolution speed is 15-20 rpm, the rotation speed is 60-80 rpm, and the vacuum degree is maintained at -0.095MPa; the stirring time is 15-20 minutes, and the entire process is run at low speed to avoid premature triggering of the reaction in the curing system.
[0040] The third step is low-temperature vacuum homogenization, followed by cooling and packaging. A vacuum homogenizer is used to complete the homogenization process. The system temperature is controlled below 40℃, the vacuum degree is -0.095MPa, and the homogenization time is 5 to 10 minutes. After homogenization, the system is rapidly cooled to below 25℃ and then sealed and packaged at 20 to 25℃.
[0041] The ternary composite toughening agent is composed of a core-shell polymer toughening agent, a modified polyurethane toughening agent, and a carboxyl-terminated nitrile butadiene rubber compounded together. By weight, the core-shell polymer toughening agent comprises 12-16 parts, the modified polyurethane toughening agent comprises 5-7 parts, and the carboxyl-terminated nitrile butadiene rubber comprises 3-5 parts. The ternary composite toughening agent is dispersed in the resin matrix in a blending manner to form a multiphase toughening structure.
[0042] The composite latent curing agent is a combination of surface-modified ultrafine dicyandiamide and substituted urea accelerator; the particle size D50 of the ultrafine dicyandiamide is controlled to be 3-4.5 μm, and the surface of the dicyandiamide is modified by coating with a silane coupling agent; the curing system remains inert at room temperature, and the curing reaction is initiated when the temperature rises above 140℃;
[0043] The silane-titanium ester composite interface modifier is composed of KH-560 silane coupling agent and titanate coupling agent; by mass ratio, KH-560 to titanate coupling agent is 3:1; the composite functional agent is composed of cocoyl monoethanolamide, titanate, and acetylacetone mixed in a mass ratio of 3:2.5:1.8.
[0044] The gradient-graded inorganic filler is composed of a compound of large-particle-size silica powder and nano-silica; the particle size D50 of the large-particle-size silica powder is 0.5-1μm, and the particle size of the nano-silica is 20-50nm; the mass ratio of large-particle-size silica powder to nano-silica is 15:3; the filler is surface activated by a coupling agent before use to form a dense packing structure inside the adhesive;
[0045] The composite rheology modifier is composed of fumed silica and polyamide wax; by weight, fumed silica is 0.2-0.3 parts and polyamide wax is 0.1-0.2 parts; when the composite rheology modifier is in operation, it enables the adhesive to have thixotropic properties of static anti-sagging and dynamic easy flow.
Claims
1. A high-strength adhesive for bonding automotive metal structures, using bisphenol F epoxy resin and flexible epoxy resin as the base resin matrix, characterized in that: Including ternary composite toughening agents, composite latent curing agents, silane-titanium ester composite interface modifiers, gradient-graded inorganic fillers, composite rheology modifiers, and composite functional agents; By weight, the adhesive components are distributed as follows: 20-30 parts bisphenol F epoxy resin, 10-20 parts flexible epoxy resin, 20-25 parts ternary composite toughening agent, 3-6 parts surface-modified ultrafine dicyandiamide, 2-5 parts substituted urea accelerator, 1-2 parts composite coupling agent, 3-8 parts composite functional agent, 10-25 parts gradient-graded silica powder, 0.2-0.3 parts fumed silica, 0.8-1.5 parts leveling agent, and 0.2-0.3 parts silicone defoamer.
2. The high-strength adhesive for bonding automotive metal structures according to claim 1, characterized in that, The ternary composite toughening agent is composed of a core-shell polymer toughening agent, a modified polyurethane toughening agent, and a carboxyl-terminated nitrile butadiene rubber compounded together. By weight, the core-shell polymer toughening agent comprises 12-16 parts, the modified polyurethane toughening agent comprises 5-7 parts, and the carboxyl-terminated nitrile butadiene rubber comprises 3-5 parts. The ternary composite toughening agent is dispersed in the resin matrix in a blending manner to form a multiphase toughening structure.
3. The high-strength adhesive for bonding automotive metal structures according to claim 1, characterized in that, The composite latent curing agent is a combination of surface-modified ultrafine dicyandiamide and substituted urea accelerator; the particle size D50 of the ultrafine dicyandiamide is controlled to be 3-4.5 μm, and the surface of the dicyandiamide is modified by coating with a silane coupling agent; the curing system remains inert at room temperature, and the curing reaction is initiated when the temperature rises above 140°C.
4. The high-strength adhesive for bonding automotive metal structures according to claim 1, characterized in that, The silane-titanium ester composite interface modifier is composed of KH-560 silane coupling agent and titanate coupling agent; by mass ratio, KH-560 to titanate coupling agent is 3:1; the composite functional agent is composed of cocoyl monoethanolamide, titanate, and acetylacetone mixed in a mass ratio of 3:2.5:1.
8.
5. The high-strength adhesive for bonding automotive metal structures according to claim 1, characterized in that, The gradient-graded inorganic filler is composed of a compound of large-particle-size silica powder and nano-silica; the particle size D50 of the large-particle-size silica powder is 0.5-1 μm, and the particle size of the nano-silica is 20-50 nm; the mass ratio of large-particle-size silica powder to nano-silica is 15:3; the filler is surface activated by a coupling agent before use to form a dense packing structure inside the adhesive.
6. The high-strength adhesive for bonding automotive metal structures according to claim 1, characterized in that, The composite rheology modifier is composed of fumed silica and polyamide wax; by weight, fumed silica is 0.2-0.3 parts and polyamide wax is 0.1-0.2 parts; when the composite rheology modifier is in operation, it enables the adhesive to have thixotropic properties of static anti-sagging and dynamic easy flow.
7. The method for preparing a high-strength adhesive for bonding automotive metal structures according to claim 1, characterized in that, A three-step gradient temperature-controlled vacuum stirring process is adopted; Overall operation process of preparation method: The first step is to mix the matrix resin, toughening system, filler and conventional additives; After cooling in the second step, add the curing system and mix at low speed. The third step is low-temperature vacuum homogenization, followed by cooling and packaging.
8. The high-strength adhesive for bonding automotive metal structures according to claim 7 and its preparation method, characterized in that, The first step of the preparation method uses a planetary mixer with a revolution speed of 20-30 rpm, a rotation speed of 500-600 rpm, a system temperature of 50-60℃, a vacuum degree maintained at -0.095 MPa, and continuous stirring and dispersion for 25-35 min to complete the preparation of the matrix mixture.
9. The high-strength adhesive for bonding automotive metal structures according to claim 7 and its preparation method, characterized in that, The second step of the preparation method involves a gradient cooling operation, reducing the system temperature to 35–40°C; the revolution speed is 15–20 rpm, the rotation speed is 60–80 rpm, and the vacuum degree is maintained at -0.095 MPa; the stirring time is 15–20 min, and the entire process is carried out at a low speed to avoid premature triggering of the reaction in the curing system.
10. The high-strength adhesive for bonding automotive metal structures according to claim 7 and its preparation method, characterized in that, The third step of the preparation method involves using a vacuum homogenizer to perform homogenization. The system temperature is controlled below 40°C, the vacuum degree is -0.095MPa, and the homogenization time is 5 to 10 minutes. After homogenization, the system is rapidly cooled to below 25°C and then sealed and packaged at 20 to 25°C.