A secondary aluminum ash denitrification process

By performing crushing, screening, and humidification treatments within a closed reaction mill, combined with a circulating gas path and a solid-phase ammonia capture module, the problems of material slurry formation and tail gas instability in secondary aluminum ash denitrification treatment were solved, achieving stable hydrolysis of aluminum nitride and controllable recovery of ammonia.

CN123108285APending Publication Date: 2026-11-17LUOYANG JUNJIANG BUILDING MATERIAL TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611181384.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-05
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing secondary aluminum ash denitrification treatments suffer from several problems, including the material easily forming a slurry system, increased load on subsequent solid-liquid separation and drying, easy scaling and clogging of exhaust gas, and a lack of closed-loop coordinated control between the reaction and exhaust gas treatment.

Method used

After crushing and screening in a closed reaction mill, a controlled water content is established by humidifying media, and shearing impact is applied by grinding media to cause aluminum nitride to react with water to generate ammonia. Combined with a circulating gas path and a solid-phase ammonia capture module, a closed-loop circulation is achieved to realize the stable hydrolysis of aluminum nitride and the controllable capture of ammonia.

Benefits of technology

Stable hydrolysis of aluminum nitride in secondary aluminum ash was achieved under solid-phase-dominated conditions, avoiding material slurry problems, ensuring the stability and closed-loop synergy of tail gas treatment, and improving process continuity and controllable recovery of ammonia.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123108285A_ABST
    Figure CN123108285A_ABST
Patent Text Reader

Abstract

This invention relates to the field of aluminum ash denitrification and discloses a secondary aluminum ash denitrification process; comprising: secondary aluminum ash crushing and screening to obtain aluminum ash material to be treated; the material being fed into a closed reaction mill and sealed to form a closed cavity, with liquid water or water vapor added to make the moisture content 3% to 12%; grinding media being placed in the closed cavity and the reaction mill being rotated to apply shearing and impact to the material, causing aluminum nitride to hydrolyze and generate ammonia gas; the ammonia-containing tail gas entering a dust removal unit, a gas-liquid separation unit and a solid phase ammonia capture module through a circulating gas path for collection, and then returning to the closed reaction mill through a return gas pipeline; the solid phase ammonia capture module being thermally regenerated or solution regenerated to obtain ammonia-containing recovery product and reuse the ammonia capture medium; the hydrolyzed solid material being discharged, and after solid-liquid separation, washing and drying, a denitrified aluminum ash solid product is obtained, and the filtrate is concentrated and crystallized to obtain a salt crystal product.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of low-altitude surveillance and target identification, specifically to a secondary aluminum ash denitrification process. Background Technology

[0002] Secondary aluminum ash is a solid byproduct generated during aluminum smelting and recycled aluminum smelting, typically containing metallic aluminum, alumina, salts, and aluminum nitride. Due to its complex composition, uneven particle size distribution, and potential for gas generation upon contact with water, the disposal and resource utilization of secondary aluminum ash are influenced by factors such as process safety and environmental compliance. Reducing the aluminum nitride content in secondary aluminum ash is a common process requirement in pretreatment stages aimed at the recycling or co-utilization of aluminum metallurgical raw materials.

[0003] Current methods for denitrifying secondary aluminum ash mostly employ a hydrolysis route. This involves adding water or introducing steam to the aluminum ash, causing aluminum nitride to react with water to generate ammonia, which is then collected or absorbed. These processes typically take place in hydrolysis tanks, reaction vessels, or stirring equipment, relying on agitation to achieve solid-liquid contact and mass transfer. The generated ammonia-containing tail gas is generally piped out and enters liquid-phase absorption devices such as scrubbing towers or absorption towers, or is treated and discharged under ventilation and purification conditions. Some methods, to increase the reaction rate, employ heating, extending the reaction time, or increasing the liquid-to-solid ratio to accelerate the hydrolysis process.

[0004] Nitrogen removal methods still have certain limitations in engineering applications. Firstly, when using a high liquid-to-solid ratio or prolonged wet hydrolysis, the material easily forms a slurry system, increasing the load on subsequent solid-liquid separation and drying, and affecting process continuity. Secondly, ammonia-containing tail gas treatment often relies on liquid-phase absorption units. When the tail gas contains dust, condensate, or droplets, it easily leads to scaling, blockage, or operational fluctuations in the absorption system. Furthermore, the stability of the tail gas organization and recovery path is significantly affected by equipment and operating conditions. Thirdly, some processes lack closed-loop coordinated control between the reaction and tail gas treatment, making it difficult to stably capture and controllably recover ammonia-containing gas while ensuring reaction progress. Summary of the Invention

[0005] To address the shortcomings of existing technologies, this invention provides a secondary aluminum ash denitrification process to solve the technical problems existing in the prior art.

[0006] The above-mentioned technical objective of the present invention is achieved through the following technical solution:

[0007] A secondary aluminum ash denitrification process includes the following steps:

[0008] S1: The secondary aluminum ash is crushed and screened to obtain the aluminum ash material to be processed;

[0009] S2: The aluminum ash material to be treated is fed into a closed reaction mill. After the feed inlet is closed, the closed reaction mill is sealed to form a closed cavity. Under closed conditions, a humidifying medium is added to the aluminum ash material to be treated, so that the aluminum ash material is in a controlled moisture content state, and the moisture content corresponding to the controlled moisture content state is 3% to 12%.

[0010] S3: Drive the closed reaction mill to apply shearing and impact to the aluminum ash material to be treated, so that the aluminum nitride in the aluminum ash material to be treated undergoes a hydrolysis reaction with water to generate ammonia gas. Grinding media are set in the closed cavity, and the closed reaction mill is driven to rotate, so that the grinding media and the aluminum ash material to be treated undergo relative motion to apply shearing and impact to the aluminum ash material to be treated.

[0011] S4: The ammonia-containing tail gas discharged from the closed reaction mill is introduced into the solid phase ammonia capture module through the circulation gas path, so that the ammonia-containing tail gas comes into contact with the ammonia capture medium to capture ammonia. The circulation gas path is connected in sequence to the tail gas outlet, dust removal unit, gas-liquid separation unit, solid phase ammonia capture module and return gas pipeline. The tail gas outlet is connected to the closed cavity, and the return gas pipeline is connected to the closed reaction mill, so that the ammonia-containing tail gas circulates between the closed cavity and the solid phase ammonia capture module.

[0012] S5: After the capture is completed, the solid phase ammonia capture module is regenerated to obtain ammonia-containing recovery products, and the regenerated ammonia capture medium is returned to the solid phase ammonia capture module for the next cycle of ammonia capture. The solid phase ammonia capture module is equipped with a regeneration inlet and a regeneration outlet, and the regeneration outlet is connected to the ammonia-containing recovery product collection pipeline.

[0013] S6: The solid material after hydrolysis reaction is discharged from the closed reaction mill to obtain denitrified aluminum ash solid product, which is used as a pretreatment product for aluminum metallurgical raw materials.

[0014] Preferably, the secondary aluminum ash is crushed and then screened to obtain undersize material with a particle size of no more than 5 mm as the aluminum ash material to be processed.

[0015] The material remaining on the sieve after screening is returned to the crushing process until all the material remaining on the sieve has passed through the screening process.

[0016] The crushing process is a two-stage crushing process, including primary coarse crushing and secondary fine crushing. The material after secondary fine crushing enters the screening process.

[0017] Preferably, the humidifying medium is liquid water or water vapor, and the liquid water is added to the closed cavity through the spray assembly. The spray assembly is disposed in the closed cavity and arranged toward the movement area of ​​the aluminum ash material to be treated.

[0018] The steam is introduced into the closed cavity through the steam inlet, and the steam inlet is connected to the closed cavity.

[0019] Preferably, the closed reaction mill is driven to rotate while the humidifying medium is added, so that the aluminum ash material to be treated is turned over and mixed with the humidifying medium in the closed cavity;

[0020] The sealed reaction mill is equipped with a pressure sensor and a temperature sensor, which are respectively connected to the sealed cavity to obtain pressure data and temperature data within the sealed cavity.

[0021] Preferably, the grinding medium is a grinding ball, and the grinding ball is made of alumina ceramic or zirconium oxide ceramic;

[0022] The filling volume of the grinding media accounts for 20% to 60% of the effective volume of the enclosed cavity;

[0023] The mass ratio of the aluminum ash material to be treated to the grinding media is 1:0.5 to 1:5;

[0024] The rotational speed of the closed reaction mill is from 30 rpm to 180 rpm.

[0025] Preferably, the reaction temperature of S3 is 40°C to 95°C, and is controlled by introducing water vapor into the closed cavity or by setting a heating jacket on the closed reaction mill.

[0026] The duration of S3 is from 20 min to 240 min;

[0027] The rotational speed of the closed reaction mill is controlled based on pressure and temperature data to maintain the pressure inside the closed chamber between 0.02 MPa and 0.20 MPa.

[0028] Preferably, a circulating fan is installed in the circulating gas path, and the circulating fan is located between the exhaust gas outlet and the dust removal unit or between the gas-liquid separation unit and the solid phase ammonia capture module;

[0029] The dust removal unit is a cyclone separator or a cartridge filter, and the gas-liquid separation unit is a demister or a condenser separator.

[0030] Preferably, the solid-phase ammonia capture module includes a shell and a packed bed disposed within the shell. The packed bed is formed by filling with an ammonia capture medium. The shell is provided with an inlet end and an outlet end. The inlet end is connected to a gas-liquid separation unit, and the outlet end is connected to a return gas pipeline.

[0031] The ammonia-catching medium is a porous carrier loaded with acidic components. The porous carrier is any one of activated alumina, zeolite, or activated carbon, and the acidic component is any one of phosphoric acid, sulfuric acid, or hydrochloric acid.

[0032] Preferably, the regeneration process in S5 is thermal regeneration or solution regeneration;

[0033] The thermal regeneration includes heating the solid-phase ammonia capture module after stopping the supply of ammonia-containing tail gas to the module, so that the ammonia capture medium desorbs ammonia gas and obtains the desorbed gas as the ammonia-containing recovery product. The heating temperature of the thermal regeneration is 60°C to 150°C, and the duration of the thermal regeneration is 10 min to 120 min.

[0034] Solution regeneration involves introducing a regenerated liquid into the solid-phase ammonia capture module, allowing the ammonium salt in the ammonia capture medium to enter the regenerated liquid and obtain an ammonium salt-containing regenerated liquid as an ammonia-containing recovery product. The regenerated liquid is water or sodium chloride solution.

[0035] After the solution regeneration is completed, the solid phase ammonia capture module is dried, and after the drying process is completed, the regenerated ammonia capture medium is returned to the solid phase ammonia capture module for the next cycle of ammonia capture.

[0036] The condition for completing the capture is that the ammonia concentration at the outlet of the solid-phase ammonia capture module reaches a set threshold, and the ammonia concentration is obtained by an ammonia concentration sensor installed at the outlet.

[0037] Preferably, after stopping the rotation of the closed reaction mill, the discharge port is opened to discharge the solid material after hydrolysis reaction into a closed collection container;

[0038] Before being discharged, the solid material after the hydrolysis reaction is cooled by introducing an inert gas into the closed cavity. The inert gas is either nitrogen or carbon dioxide.

[0039] The solid material after the hydrolysis reaction is subjected to solid-liquid separation to obtain denitrified aluminum ash solid product. The solid-liquid separation is performed by either pressure filtration or centrifugation.

[0040] Before solid-liquid separation, wash water is added to the solid material after hydrolysis reaction and mixed. The amount of wash water added makes the solid-liquid ratio 1:0.5 to 1:5.

[0041] The denitrified aluminum ash solid product is dried at a temperature of 60°C to 150°C, and the moisture content of the dried denitrified aluminum ash solid product is no more than 5%.

[0042] The filtrate obtained from the solid-liquid separation is evaporated, concentrated, and crystallized to obtain a salt crystal product.

[0043] The denitrified aluminum ash solid product is dried and then sealed in a moisture-proof bag or sealed container.

[0044] In summary, the present invention has the following main beneficial effects:

[0045] This invention establishes a controlled moisture content of 3% to 12% within a closed reaction mill. By applying shearing and impact forces to the aluminum ash material under treatment through the grinding media, the reaction interface is continuously renewed and the contact between aluminum nitride and water is enhanced under solid-phase-dominated conditions. This achieves stable hydrolysis and denitrification of aluminum nitride in secondary aluminum ash under controllable conditions of 40°C to 95°C and 0.02MPa to 0.20MPa, avoiding problems such as material slurry formation and increased burden on subsequent dehydration caused by wet hydrolysis with high liquid-to-solid ratio. This results in better process integration between the denitrification reaction, solid phase discharge, and post-treatment processes.

[0046] By sequentially introducing the ammonia-containing tail gas discharged from the closed reaction mill into the dust removal unit, gas-liquid separation unit, and solid-phase ammonia capture module through the circulating gas path, the dust, condensate, and droplets in the ammonia-containing tail gas are removed in stages, and the gas phase conditions are made controllable. This ensures that the ammonia-containing tail gas is in full contact with the ammonia capture medium in the packed bed and ammonia is captured stably. At the same time, the captured gas is returned to the closed reaction mill through the return gas pipeline to form a closed gas circulation loop between the closed cavity and the solid-phase ammonia capture module. This reduces the risk of ammonia gas escape and fugitive emissions, and makes the tail gas treatment and reaction system form a closed loop synergy.

[0047] By setting a regeneration inlet and outlet on the solid-phase ammonia capture module and employing thermal or solution regeneration methods, the ammonia capture medium is periodically regenerated and reused. This yields ammonia-containing recovery products in the form of desorbed gas or ammonium salt-containing regenerated liquid, enabling the reuse of the ammonia capture medium. Simultaneously, an ammonia concentration sensor acquires the ammonia concentration at the outlet, and a set threshold is used to determine the completion of capture, allowing for timely switching of the regeneration mode before the ammonia capture medium approaches saturation. This provides quantifiable operating boundaries and a stable basis for control of the capture, regeneration, and recycling processes. Attached Figure Description

[0048] Figure 1 This is a schematic diagram of the system connection of the present invention;

[0049] Figure 2 This is a process flow diagram of the present invention. Detailed Implementation

[0050] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0051] Example 1

[0052] refer to Figure 1-2A secondary aluminum ash denitrification process includes the following steps:

[0053] S1: The secondary aluminum ash is crushed and screened to obtain the aluminum ash material to be processed;

[0054] S2: The aluminum ash material to be treated is fed into a closed reaction mill. After the feed inlet is closed, the closed reaction mill is sealed to form a closed cavity. Under closed conditions, a humidifying medium is added to the aluminum ash material to be treated, so that the aluminum ash material is in a controlled moisture content state, and the moisture content corresponding to the controlled moisture content state is 3% to 12%.

[0055] S3: Drive the closed reaction mill to apply shearing and impact to the aluminum ash material to be treated, so that the aluminum nitride in the aluminum ash material to be treated undergoes a hydrolysis reaction with water to generate ammonia gas. Grinding media are set in the closed cavity, and the closed reaction mill is driven to rotate, so that the grinding media and the aluminum ash material to be treated undergo relative motion to apply shearing and impact to the aluminum ash material to be treated.

[0056] S4: The ammonia-containing tail gas discharged from the closed reaction mill is introduced into the solid phase ammonia capture module through the circulation gas path, so that the ammonia-containing tail gas comes into contact with the ammonia capture medium to capture ammonia. The circulation gas path is connected in sequence to the tail gas outlet, dust removal unit, gas-liquid separation unit, solid phase ammonia capture module and return gas pipeline. The tail gas outlet is connected to the closed cavity, and the return gas pipeline is connected to the closed reaction mill, so that the ammonia-containing tail gas circulates between the closed cavity and the solid phase ammonia capture module.

[0057] S5: After the capture is completed, the solid phase ammonia capture module is regenerated to obtain ammonia-containing recovery products, and the regenerated ammonia capture medium is returned to the solid phase ammonia capture module for the next cycle of ammonia capture. The solid phase ammonia capture module is equipped with a regeneration inlet and a regeneration outlet, and the regeneration outlet is connected to the ammonia-containing recovery product collection pipeline.

[0058] S6: The solid material after hydrolysis reaction is discharged from the closed reaction mill to obtain denitrified aluminum ash solid product, which is used as a pretreatment product for aluminum metallurgical raw materials.

[0059] The secondary aluminum ash is subjected to two-stage crushing: a primary coarse crusher and a secondary fine crusher. The material after the secondary fine crushing then enters the screening unit for further screening. The screening unit uses a 5mm mesh screen. The undersize material obtained from screening is used as the aluminum ash material to be processed and enters the next process. The oversize material obtained from screening is returned to the secondary fine crusher for further crushing and screening, until all the oversize material passes through the screening process.

[0060] To avoid unclear particle size description, in this embodiment, a particle size of no more than 5 mm means that the material can pass through a sieve with a sieve hole size of 5 mm. The material that passes through the sieve is the aluminum ash material to be processed with a particle size of no more than 5 mm.

[0061] The aluminum ash material to be processed is added through the feed inlet of the closed reaction mill. After the feed inlet is closed, the closed reaction mill is sealed to form a closed cavity. The closed reaction mill includes a cylinder, end caps, sealing rings, a feed inlet, a discharge outlet, a tail gas outlet, and a return gas inlet. The end caps and cylinder are sealed together by the sealing rings. Temperature and pressure sensors are installed inside the closed cavity to acquire temperature and pressure data, respectively.

[0062] The humidifying medium is liquid water or water vapor.

[0063] 1) When the humidifying medium is liquid water, the liquid water is added to the closed cavity through the spray assembly. The spray assembly is set in the closed cavity and arranged towards the movement area of ​​the aluminum ash material to be treated. The spray assembly is connected to the metering pump to control the spray volume.

[0064] 2) When the humidifying medium is water vapor, the water vapor is introduced into the closed cavity through the steam inlet. The steam inlet is connected to the closed cavity, and a regulating valve is installed on the steam pipeline to control the amount of water introduced.

[0065] To ensure the aluminum ash material to be treated is in a controlled moisture content state, this embodiment defines a controlled moisture content state as a moisture content of 3% to 12% in the aluminum ash material to be treated. The moisture content is calculated using the following formula:

[0066] ;

[0067] in, Moisture content, For dry-based solid phase quality, Let be the mass of water in the material. The initial moisture content of the aluminum ash material to be treated is denoted as . The target moisture content is denoted as ,and Take 3% to 12%.

[0068] When the initial mass of the aluminum ash material to be processed is The initial moisture content was At that time, in order to achieve the target moisture content The required increase in water quality Determine by the following formula:

[0069] ;

[0070] in, and Expressed as a decimal.

[0071] When the humidifying medium is liquid water, the mass of liquid water sprayed in is taken as... When the humidifying medium is water vapor, the mass of the condensate formed by the condensation of the introduced water vapor in the closed cavity is taken as the humidifying medium. As the equivalent water addition, the control target is .

[0072] While adding the humidifying medium, the closed reaction mill is driven to rotate, causing the aluminum ash material to be treated to tumble and mix with the humidifying medium in the closed chamber, so that the humidifying medium is evenly distributed in the material.

[0073] To avoid describing humidification adjustment solely in a functional manner, this embodiment uses temperature and pressure as control variables to regulate the flow rate of the humidification medium. Temperature sensor output. Pressure sensor output Set an upper temperature limit. With pressure upper limit Construct the overall deviation:

[0074] ;

[0075] The injection flow rate is obtained using proportional-integral-derivative control with saturation constraints. :

[0076] ;

[0077] in, and These are the weighting coefficients. As the baseline flow rate, , , These are the proportional, integral, and differential coefficients, respectively. It is a saturation function used to saturate... Limited to Inside, avoid excessive humidification. By using the above methods, the target moisture content can be established while maintaining stable operation of the closed cavity.

[0078] Abrasive media, consisting of abrasive balls made of alumina ceramic or zirconia ceramic, is placed within a closed cavity. The volume of the abrasive media occupies 20% to 60% of the effective volume of the closed cavity. The mass ratio of the aluminum ash material to be treated to the abrasive media is 1:0.5 to 1:5.

[0079] The closed reaction mill is driven to rotate at a speed controlled between 30 rpm and 180 rpm, causing relative motion between the grinding media and the aluminum ash material to be treated, applying shearing and impact forces to the material. Under controlled moisture conditions, the aluminum nitride in the aluminum ash material undergoes a hydrolysis reaction with water to generate ammonia gas, the reaction expression of which is:

[0080] ;

[0081] in, It is aluminum nitride. For water, It is aluminum hydroxide. It is ammonia.

[0082] The reaction temperature of S3 is between 40°C and 95°C, and the reaction temperature is controlled by introducing water vapor into the closed cavity or by setting a heating jacket on the sealed reaction mill. The duration of S3 is between 20 min and 240 min.

[0083] To maintain the pressure in the closed cavity between 0.02 MPa and 0.20 MPa, this embodiment uses closed-loop regulation of the rotational speed based on pressure and temperature data. Let the rotational speed be... The reference speed is Pressure set value Temperature set value The rotational speed is then controlled by the following formula:

[0084] ;

[0085] in, and For control coefficients, Used to The speed is limited to the range of 30 rpm to 180 rpm. This control maintains the pressure in the closed chamber within the range of 0.02 MPa to 0.20 MPa.

[0086] The closed reaction mill introduces ammonia-containing tail gas into the circulating gas path through the tail gas outlet. The circulating gas path sequentially connects the tail gas outlet, dust removal unit, gas-liquid separation unit, solid-phase ammonia capture module, and return gas pipeline. The tail gas outlet is connected to the closed cavity, and the return gas pipeline is connected to the return gas inlet of the closed reaction mill, allowing the ammonia-containing tail gas to circulate between the closed cavity and the solid-phase ammonia capture module, thus forming a closed gas circulation loop.

[0087] A circulating fan is installed in the circulating air circuit to provide circulation power. The location of the circulating fan must meet any of the following conditions:

[0088] 1) The circulating fan is located between the exhaust gas outlet and the dust removal unit;

[0089] 2) The circulating fan is located between the gas-liquid separation unit and the solid phase ammonia capture module.

[0090] The dust removal unit, consisting of a cyclone separator or cartridge filter, removes solid dust carried in the exhaust gas. The gas-liquid separation unit, consisting of a demister or condenser separator, separates the condensate from entrained droplets. The condensate separated by the gas-liquid separation unit enters a condensate collection container, while the gas phase enters the solid-phase ammonia capture module.

[0091] The solid-phase ammonia capture module includes a housing and a packed bed disposed within the housing, the packed bed being formed by filling with an ammonia capture medium. The housing has an inlet end and an outlet end, the inlet end being connected to a gas-liquid separation unit, and the outlet end being connected to a return gas pipeline.

[0092] The ammonia-catching medium is a porous support loaded with an acidic component. The porous support can be any one of activated alumina, zeolite, or activated carbon, and the acidic component can be any one of phosphoric acid, sulfuric acid, or hydrochloric acid. Taking activated alumina-loaded phosphoric acid as an example, the ammonia-catching medium is prepared by impregnating activated alumina in an aqueous phosphoric acid solution, followed by drying at 80°C to 120°C to constant weight, thus loading the acidic component onto the porous support. Besides phosphoric acid loading, when sulfuric acid or hydrochloric acid is used as the acidic component, the same impregnation and drying method is employed to prepare the ammonia-catching medium.

[0093] Ammonia-containing tail gas enters from the inlet of the solid-phase ammonia capture module, passes through the packed bed and comes into contact with the ammonia capture medium, and is discharged from the outlet and returned to the closed reaction mill via the return gas pipeline, completing the closed cycle.

[0094] An ammonia concentration sensor is installed at the outlet of the solid-phase ammonia capture module to output the instantaneous ammonia concentration. To determine stability, this embodiment uses the moving average ammonia concentration. :

[0095]

[0096] in, The sampling period is The number of points in the sliding window. Set a threshold. ,when Once the collection is complete, the process enters the regeneration stage. Threshold The setting ranges from 50 ppm to 2000 ppm, depending on the amount of ammonia-catching medium and the amount of circulating gas.

[0097] The solid-phase ammonia capture module is equipped with a regeneration inlet and a regeneration outlet, with the regeneration outlet connected to a collection pipeline containing ammonia recovery products. Capture and regeneration are achieved by switching valves, which isolates the solid-phase ammonia capture module from the circulating gas path during regeneration, preventing regeneration gas from returning to the circulating gas path.

[0098] The solid-phase ammonia capture module is equipped with a regeneration inlet and a regeneration outlet, with the regeneration outlet connected to a collection pipeline containing ammonia recovery products. Capture and regeneration are achieved by switching valves, which isolates the solid-phase ammonia capture module from the circulating gas path during regeneration, preventing regeneration gas from returning to the circulating gas path.

[0099] The regeneration process is either thermal regeneration or solution regeneration.

[0100] 1) Thermal regeneration: Stop supplying ammonia-containing tail gas to the solid-phase ammonia capture module, and heat the module to desorb ammonia gas from the ammonia capture medium, obtaining the desorbed gas as the ammonia-containing recovery product. The thermal regeneration heating temperature is 60℃ to 150℃, and the duration is 10 min to 120 min. The desorbed gas enters the ammonia-containing recovery product collection pipeline through the regeneration outlet.

[0101] 2) Solution regeneration: A regeneration solution is introduced into the solid-phase ammonia capture module, allowing the ammonium salts in the ammonia capture medium to enter the regeneration solution and obtain an ammonium salt-containing regeneration solution as the ammonia recovery product. The regeneration solution is water or sodium chloride solution. After solution regeneration, the solid-phase ammonia capture module is dried. After drying, the regenerated ammonia capture medium is returned to the solid-phase ammonia capture module for the next ammonia capture cycle.

[0102] After stopping the rotation of the closed reaction mill, open the discharge port to discharge the solid material after hydrolysis into the closed collection container. To reduce the temperature and gas disturbance in the closed cavity during the discharge stage, an inert gas is introduced into the closed cavity for cooling before discharge. The inert gas can be either nitrogen or carbon dioxide.

[0103] The solid phase material after hydrolysis reaction is subjected to solid-liquid separation to obtain denitrified aluminum ash solid product. The solid-liquid separation is carried out by either pressure filtration or centrifugation. Before solid-liquid separation, washing water is added to the solid phase material after hydrolysis reaction and mixed. The amount of washing water added is such that the solid-liquid ratio is 1:0.5 to 1:5.

[0104] The denitrified aluminum ash solid product is dried at a temperature of 60℃ to 150℃, and the moisture content of the dried denitrified aluminum ash solid product is no more than 5%. The moisture content is also determined according to the aforementioned moisture content calculation formula.

[0105] The filtrate obtained from solid-liquid separation enters the evaporation, concentration, and crystallization unit, where it is evaporated, concentrated, and crystallized to obtain salt crystals. The dried denitrified aluminum ash solid product is then sealed in moisture-proof bags or sealed containers.

[0106] This invention is based on the hydrolysis reaction of aluminum nitride in secondary aluminum ash for denitrification. First, the aluminum ash material to be treated is crushed and sieved to obtain particles no larger than 5 mm in diameter, ensuring consistent stress and mass transfer conditions within the closed reaction mill. Then, the aluminum ash material is fed into the closed reaction mill and sealed to form a closed chamber. Within the closed chamber, a controlled moisture content is established by spraying liquid water or introducing steam, stabilizing the material's moisture content at 3% to 12%, providing the reaction medium for the contact reaction between aluminum nitride and water. As the closed reaction mill rotates, the grinding media within the closed chamber and the aluminum ash material undergo relative motion, continuously applying shearing and impact forces to the material. This constantly renews the particle surface and maintains the spread and penetration of moisture on the particle surface, thereby promoting the hydrolysis reaction between aluminum nitride and water to generate ammonia gas. During the reaction, the amount of humidifying medium added and the rotation speed of the closed reaction mill were adjusted based on the temperature and pressure data of the closed chamber, so that the reaction could proceed stably within a temperature range of 40℃ to 95℃ and a pressure range of 0.02MPa to 0.20MPa.

[0107] The ammonia-containing tail gas generated by the hydrolysis reaction enters the circulating gas path through the tail gas outlet. Under the action of the circulating fan, it passes sequentially through the dust removal unit and the gas-liquid separation unit to remove entrained dust, condensate, and droplets, making the composition and moisture content of the gas phase entering the solid-phase ammonia capture module controllable. The pretreated ammonia-containing gas phase enters the packed bed of the solid-phase ammonia capture module, where it comes into full contact with the porous carrier ammonia capture medium loaded with acidic components. After the ammonia is captured, the treated gas flows back to the closed reaction mill through the return gas pipeline, forming a closed gas circulation loop with the closed cavity. This allows the ammonia-containing tail gas to circulate between the closed cavity and the solid-phase ammonia capture module and be continuously captured. As the ammonia capture medium gradually approaches saturation, the ammonia concentration at the outlet of the solid-phase ammonia capture module increases. When the ammonia concentration reaches a set threshold, the capture is considered complete. The solid-phase ammonia capture module is then isolated from the circulating gas path and enters the regeneration stage by switching valves. The regeneration stage can employ either thermal regeneration or solution regeneration: In thermal regeneration, the packed bed is heated to desorb the captured ammonia, forming desorbed gas which is collected at the regeneration outlet as an ammonia-containing recovery product; in solution regeneration, a regeneration solution is introduced, allowing the captured ammonium salts to enter the regeneration solution, resulting in an ammonium salt-containing regeneration solution as an ammonia-containing recovery product. After solution regeneration, the packed bed is dried, and the ammonia-capturing medium is reused in the next ammonia capture cycle. After the denitrification reaction is completed, the closed reaction mill is stopped, and the solid material from the hydrolysis reaction is discharged into a closed collection container. Under inert gas cooling conditions, the solid material undergoes solid-liquid separation, washing, and drying to obtain denitrified aluminum ash solid product. The filtrate obtained from the solid-liquid separation is evaporated, concentrated, and crystallized to obtain salt crystal products, thus completing the secondary aluminum ash denitrification treatment and the resource recovery of by-product streams.

[0108] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.

Claims

1. A secondary aluminum ash denitrification process, characterized in that, Includes the following steps: S1: The secondary aluminum ash is crushed and screened to obtain the aluminum ash material to be processed; S2: The aluminum ash material to be treated is fed into a closed reaction mill. After the feed inlet is closed, the closed reaction mill is sealed to form a closed cavity. Under closed conditions, a humidifying medium is added to the aluminum ash material to be treated, so that the aluminum ash material is in a controlled moisture content state, and the moisture content corresponding to the controlled moisture content state is 3% to 12%. S3: Drive the closed reaction mill to apply shearing and impact to the aluminum ash material to be treated, so that the aluminum nitride in the aluminum ash material to be treated undergoes a hydrolysis reaction with water to generate ammonia gas. Grinding media are set in the closed cavity, and the closed reaction mill is driven to rotate, so that the grinding media and the aluminum ash material to be treated undergo relative motion to apply shearing and impact to the aluminum ash material to be treated. S4: The ammonia-containing tail gas discharged from the closed reaction mill is introduced into the solid phase ammonia capture module through the circulation gas path, so that the ammonia-containing tail gas comes into contact with the ammonia capture medium to capture ammonia. The circulation gas path is connected in sequence to the tail gas outlet, dust removal unit, gas-liquid separation unit, solid phase ammonia capture module and return gas pipeline. The tail gas outlet is connected to the closed cavity, and the return gas pipeline is connected to the closed reaction mill, so that the ammonia-containing tail gas circulates between the closed cavity and the solid phase ammonia capture module. S5: After the capture is completed, the solid phase ammonia capture module is regenerated to obtain ammonia-containing recovery products, and the regenerated ammonia capture medium is returned to the solid phase ammonia capture module for the next cycle of ammonia capture. The solid phase ammonia capture module is equipped with a regeneration inlet and a regeneration outlet, and the regeneration outlet is connected to the ammonia-containing recovery product collection pipeline. S6: The solid material after hydrolysis reaction is discharged from the closed reaction mill to obtain denitrified aluminum ash solid product, which is used as a pretreatment product for aluminum metallurgical raw materials.

2. The secondary aluminum ash denitrification process according to claim 1, characterized in that, S1 includes: crushing the secondary aluminum ash and then screening it to obtain undersize material with a particle size of no more than 5 mm as the aluminum ash material to be processed. The material remaining on the sieve after screening is returned to the crushing process until all the material remaining on the sieve has passed through the screening process. The crushing process is a two-stage crushing process, including primary coarse crushing and secondary fine crushing. The material after secondary fine crushing enters the screening process.

3. The secondary aluminum ash denitrification process according to claim 2, characterized in that, The humidifying medium is liquid water or water vapor. The liquid water is added to the closed cavity through the spray assembly, which is located in the closed cavity and arranged towards the movement area of ​​the aluminum ash material to be treated. The steam is introduced into the closed cavity through the steam inlet, and the steam inlet is connected to the closed cavity.

4. The secondary aluminum ash denitrification process according to claim 3, characterized in that, While adding the humidifying medium, the closed reaction mill is driven to rotate, causing the aluminum ash material to be treated to tumble and mix with the humidifying medium in the closed cavity. The sealed reaction mill is equipped with a pressure sensor and a temperature sensor, which are respectively connected to the sealed cavity to obtain pressure data and temperature data within the sealed cavity.

5. The secondary aluminum ash denitrification process according to claim 4, characterized in that, The grinding medium is a grinding ball, and the grinding ball is made of alumina ceramic or zirconium oxide ceramic; The filling volume of the grinding media accounts for 20% to 60% of the effective volume of the enclosed cavity; The mass ratio of the aluminum ash material to be treated to the grinding media is 1:0.5 to 1:5; The rotational speed of the closed reaction mill is from 30 rpm to 180 rpm.

6. The secondary aluminum ash denitrification process according to claim 5, characterized in that, The reaction temperature of S3 is 40°C to 95°C and is controlled by introducing water vapor into the closed cavity or by setting a heating jacket on the closed reaction mill. The duration of S3 is from 20 min to 240 min; The rotational speed of the closed reaction mill is controlled based on pressure and temperature data to maintain the pressure inside the closed chamber between 0.02 MPa and 0.20 MPa.

7. The secondary aluminum ash denitrification process according to claim 6, characterized in that, A circulating fan is installed on the circulating gas path. The circulating fan is located between the exhaust gas outlet and the dust removal unit or between the gas-liquid separation unit and the solid phase ammonia capture module. The dust removal unit is a cyclone separator or a cartridge filter, and the gas-liquid separation unit is a demister or a condenser separator.

8. The secondary aluminum ash denitrification process according to claim 7, characterized in that, The solid-phase ammonia capture module includes a shell and a packed bed disposed within the shell. The packed bed is formed by filling with an ammonia capture medium. The shell is provided with an inlet end and an outlet end. The inlet end is connected to the gas-liquid separation unit, and the outlet end is connected to the return gas pipeline. The ammonia-catching medium is a porous carrier loaded with acidic components. The porous carrier is any one of activated alumina, zeolite, or activated carbon, and the acidic component is any one of phosphoric acid, sulfuric acid, or hydrochloric acid.

9. The secondary aluminum ash denitrification process according to claim 8, characterized in that, The regeneration process in S5 is either thermal regeneration or solution regeneration. The thermal regeneration includes heating the solid-phase ammonia capture module after stopping the supply of ammonia-containing tail gas to the module, so that the ammonia capture medium desorbs ammonia gas and obtains the desorbed gas as the ammonia-containing recovery product. The heating temperature of the thermal regeneration is 60°C to 150°C, and the duration of the thermal regeneration is 10 min to 120 min. Solution regeneration involves introducing a regenerated liquid into the solid-phase ammonia capture module, allowing the ammonium salt in the ammonia capture medium to enter the regenerated liquid and obtain an ammonium salt-containing regenerated liquid as an ammonia-containing recovery product. The regenerated liquid is water or sodium chloride solution. After the solution regeneration is completed, the solid phase ammonia capture module is dried, and after the drying process is completed, the regenerated ammonia capture medium is returned to the solid phase ammonia capture module for the next cycle of ammonia capture. The condition for completing the capture is that the ammonia concentration at the outlet of the solid-phase ammonia capture module reaches a set threshold, and the ammonia concentration is obtained by an ammonia concentration sensor installed at the outlet.

10. A secondary aluminum ash denitrification process according to claim 9, characterized in that, S6 includes: after stopping the rotation of the closed reaction mill, opening the discharge port to discharge the solid material after hydrolysis reaction into a closed collection container; Before being discharged, the solid material after the hydrolysis reaction is cooled by introducing an inert gas into the closed cavity. The inert gas is either nitrogen or carbon dioxide. The solid material after the hydrolysis reaction is subjected to solid-liquid separation to obtain denitrified aluminum ash solid product. The solid-liquid separation is performed by either pressure filtration or centrifugation. Before solid-liquid separation, wash water is added to the solid material after hydrolysis reaction and mixed. The amount of wash water added makes the solid-liquid ratio 1:0.5 to 1:

5. The denitrified aluminum ash solid product is dried at a temperature of 60°C to 150°C, and the moisture content of the dried denitrified aluminum ash solid product is no more than 5%. The filtrate obtained from the solid-liquid separation is evaporated, concentrated, and crystallized to obtain a salt crystal product. The denitrified aluminum ash solid product is dried and then sealed in a moisture-proof bag or sealed container.