A nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire

By embedding a nano-inorganic coating device at the end of the hot-dip galvanized aluminum-magnesium alloy steel wire production line, and utilizing waste heat for coating, the problems of insufficient flexibility in color adjustment and high production costs have been solved, achieving color diversification and quality improvement.

CN123108460APending Publication Date: 2026-11-17HBZX HIGH TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611235500.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-14
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Traditional hot-dip galvanized aluminum-magnesium alloy steel wire coating processing methods suffer from insufficient flexibility in color adjustment, inability to integrate with the production process, resulting in high production costs and poor quality stability.

Method used

A nano-inorganic coating device is designed to utilize the residual heat of hot-dip galvanized aluminum-magnesium alloy steel wire for coating. Combined with an immersion tank, liquid supply pipe, colorant supply device, and steel wire cleaning device, it can achieve coating with diverse colors, simplify the production process, and reduce energy consumption.

Benefits of technology

This technology enables a diversification of colors for hot-dip galvanized aluminum-magnesium alloy steel wire, simplifies the production process, reduces production costs, and improves the corrosion resistance and quality stability of the steel wire.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123108460A_ABST
    Figure CN123108460A_ABST
Patent Text Reader

Abstract

This invention discloses a nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire, comprising an immersion tank, a liquid supply pipe, a colorant supply device, and a wire cleaning device. The immersion tank has a colorant inlet on its front wall and a colorant outlet at its bottom. The front end of the liquid supply pipe is sealed to the front wall of the immersion tank and communicates with the colorant supply device through the colorant inlet; the rear end is sealed to the rear wall of the immersion tank. An immersion pool is located at the top of the liquid supply pipe. The bottom of the immersion pool is connected to the liquid supply pipe through a liquid supply hole, and overflow grooves are provided on both the left and right side walls. The wire cleaning device is installed on one side of the immersion pool. The finished steel wire output from the hot-dip galvanized aluminum-magnesium alloy steel wire production line passes sequentially through the overflow grooves on both side walls of the immersion pool and the wire cleaning device. This invention utilizes the residual heat of the hot-dip galvanized aluminum-magnesium alloy steel wire for nano-inorganic coating, which not only allows for convenient adjustment of the wire color but also improves the wire quality and reduces production costs.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to a nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire, which can improve the corrosion resistance of the steel wire while conveniently adjusting the color of the steel wire, belonging to the field of alloy processing technology. Background Technology

[0002] Hot-dip galvanized aluminum-magnesium alloy steel wire has gained widespread recognition from users due to its excellent corrosion resistance, playing a vital role in the construction of high-standard farmland in Northeast China. With the continuous expansion of application scenarios, customers' demands for steel wire are no longer limited to good corrosion resistance; they also place higher requirements on its color diversity. By coating with different colors, the corrosion resistance of the steel wire can be further improved, and the product's color can be diversified, allowing users to flexibly choose according to different application scenarios, thereby expanding the downstream application areas of hot-dip galvanized aluminum-magnesium alloy steel wire.

[0003] While traditional plastic coating processes can form a protective layer on the surface of hot-dip galvanized aluminum-magnesium alloy steel wire, they have significant drawbacks: color adjustment flexibility is insufficient; currently, mainstream products only offer two colors, grass green and dark green, failing to meet users' diverse color demands. Furthermore, plastic coating equipment cannot be integrated into the production process of hot-dip galvanized aluminum-magnesium alloy steel wire, requiring a separate coating station or workshop. The steel wire is then transferred to the coating stage for secondary processing after production. This production model is not only complex, but also prone to contamination or damage during transportation, resulting in poor quality stability. Additionally, it fails to effectively utilize the residual heat from the steel wire production process, leading to higher production costs. Therefore, exploring new coating processing methods for hot-dip galvanized aluminum-magnesium alloy steel wire is of great practical significance and necessity. Summary of the Invention

[0004] The purpose of this invention is to address the shortcomings of existing technologies by providing a nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire, which allows for convenient adjustment of the wire color, improvement of wire quality, and reduction of production costs.

[0005] To achieve the above objectives, the present invention adopts the following technical solution: A nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire includes an immersion tank, a liquid supply pipe, a colorant supply device, and a wire cleaning device. The front wall of the immersion tank has a colorant inlet, and the bottom has a colorant outlet. The front end of the liquid supply pipe is sealed to the front wall of the immersion tank and communicates with the colorant supply device through the colorant inlet. The rear end is sealed to the rear wall of the immersion tank. The top of the liquid supply pipe is equipped with an immersion pool. The bottom of the immersion pool is connected to the liquid supply pipe through a liquid supply hole. Both the left and right side walls are equipped with wire overflow grooves. The wire cleaning device is installed on one side of the immersion pool. The finished steel wire output from the hot-dip galvanized aluminum-magnesium alloy steel wire production line passes sequentially through the wire overflow grooves on both side walls of the immersion pool and the wire cleaning device.

[0006] The above-mentioned nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire includes a steel wire cleaning device comprising an air distribution pipe, an air supply pipe, a high-pressure air source, and a return air pipe. The front end of the air distribution pipe is sealed to the front wall of the immersion tank and connected to one end of the air supply pipe through an air inlet provided on the front wall of the immersion tank. The other end of the air supply pipe is connected to the high-pressure air source. The rear end of the air distribution pipe is sealed to the rear wall of the immersion tank. The return air pipe penetrates through both side walls of the air distribution pipe and is fixedly connected to the air distribution pipe. The middle part of the return air pipe is located inside the air distribution pipe and the pipe wall is provided with an air inlet. The finished steel wire output from the hot-dip galvanized aluminum-magnesium alloy steel wire production line passes through the return air pipe.

[0007] In the above-mentioned nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire, the high-pressure air source is compressed air.

[0008] The above-mentioned nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire includes a colorant supply device comprising a motor, a return pipe, a colorant delivery pipe, a booster pump, and a colorant tank. The colorant tank stores the desired colorant. The output shaft of the motor is connected to the input shaft of the booster pump. The inlet pipe of the booster pump is inserted into the colorant stored in the colorant tank, and the outlet is connected to the colorant inlet on the front wall of the immersion tank via the colorant delivery pipe. One end of the return pipe is connected to the colorant outlet at the bottom of the immersion tank, and the other end is inserted into the colorant tank.

[0009] The above-mentioned nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire has wire-passing windows on both side walls of the immersion tank, through which the finished steel wire output from the hot-dip galvanized aluminum-magnesium alloy steel wire production line passes.

[0010] The above-mentioned nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire includes multiple immersion tanks arranged along the length of the liquid supply pipe, and multiple return pipes corresponding to the multiple immersion tanks.

[0011] In the above-mentioned nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire, valves are installed on both the return pipe and the colorant delivery pipe.

[0012] The above-mentioned nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire has a heat tracing device installed in the colorant tank.

[0013] This invention utilizes the residual heat of hot-dip galvanized aluminum-magnesium alloy steel wire to coat a nano-inorganic coating. This not only allows for convenient adjustment of the steel wire color to meet customers' diverse color requirements, but also simplifies the steel wire production process, avoids energy waste, improves steel wire quality, and reduces production costs. Attached Figure Description

[0014] The present invention will now be described in further detail with reference to the accompanying drawings and specific embodiments.

[0015] Figure 1 This is a schematic diagram of the structure of the present invention; Figure 2 This is the front view of the immersion plating tank; Figure 3 This is a top view of the immersion plating tank; Figure 4 This is the left view of the immersion plating tank; Figure 5 yes Figure 2 AA section view; Figure 6 This is a rear view of the immersion plating tank; Figure 7 yes Figure 3 BB section view; Figure 8 Yes, this is a diagram showing the steel wire being dipped in a coloring agent.

[0016] The following are the labels in the diagram: 1. Wire overflow trough, 2. Liquid supply hole, 3. Colorant inlet, 4. Colorant outlet, 5. Immersion tank, 6. Liquid supply pipe, 7. Immersion box, 8. Air inlet, 9. Gas distribution pipe, 10. Motor, 11. Return pipe, 12. Colorant delivery pipe, 13. Booster pump, 14. Colorant tank, 15. Air supply pipe, 16. High-pressure air source, 17. Steel wire, 18. Backflush pipe, 19. Wire guide window, 20. Colorant. Detailed Implementation

[0017] This invention provides a nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire. This device can be integrated into the hot-dip galvanized aluminum-magnesium alloy steel wire process, making full use of the residual heat of the hot-dip galvanized aluminum-magnesium alloy steel wire to complete the coating of nano-inorganic coatings of different colors, realizing the diversification of product colors and opening up a new process path for the hot-dip galvanizing industry.

[0018] See Figures 1 to 8The present invention mainly includes an immersion tank 7, a liquid supply pipe 6, an immersion pool 5, a colorant supply device, and a wire cleaning device, which are set at the end of the hot-dip galvanized aluminum-magnesium alloy steel wire production line. The immersion tank 7 has an opening at the top, a colorant inlet 3 on the front wall, and a colorant outlet 4 at the bottom. The liquid supply pipe 6 is a horizontally set rectangular tube. Its front end is sealed to the front wall of the immersion tank 7 and communicates with the colorant supply device through the colorant inlet 3. Its rear end is sealed to the rear wall of the immersion tank 7. The immersion pool 5 is set at the top of the liquid supply pipe 6. The bottom of the immersion pool 5 is communicated with the inner cavity of the liquid supply pipe 6 through the liquid supply hole 2. U-shaped wire overflow grooves 1 are provided on both the left and right side walls. The wire cleaning device is installed on one side of the immersion pool 5. The finished steel wire 17 output from the hot-dip galvanized aluminum-magnesium alloy steel wire production line passes through the wire overflow grooves 1 and the wire cleaning device on both side walls of the immersion pool 5 in sequence.

[0019] Both side walls of the immersion coating tank 7 have wire-passing windows 19, through which the finished steel wires 17 output from the hot-dip galvanized aluminum-magnesium alloy steel wire production line pass. Alternatively, the two side walls of the immersion coating tank 7 can be lower than the steel wires 17 to avoid interference between the two side walls of the immersion coating tank 7 and the steel wires 17.

[0020] The colorant supply device includes a motor 10, a return pipe 11, a colorant delivery pipe 12, a booster pump 13, and a colorant tank 14. The colorant tank 14 stores the required colorant. The output shaft of the motor 10 is connected to the input shaft of the booster pump 13. The inlet pipe of the booster pump 13 is inserted into the colorant stored in the colorant tank 14, and the outlet is connected to the colorant inlet 3 on the front wall of the immersion tank 7 through the colorant delivery pipe 12. One end of the return pipe 11 is connected to the colorant outlet 4 at the bottom of the immersion tank 7, and the other end is inserted into the colorant tank 14. When the motor 10 drives the booster pump 13, the colorant in the colorant tank 14 enters the supply pipe 6 through the booster pump 13 and the colorant delivery pipe 12, then enters the immersion tank 5 through the supply hole 2, overflows to the bottom of the immersion tank 7 through the overflow trough 1, and finally flows back to the colorant tank 14 through the return pipe 11 for reuse. By appropriately adjusting the overflow rate of the colorant, the liquid level of the colorant in the immersion plating tank 5 can be made higher than that of the steel wire 17 in the wire overflow tank 1, thereby achieving the coating of the steel wire 17.

[0021] The steel wire cleaning device includes an air distribution pipe 9, an air supply pipe 15, a high-pressure air source 16, and a return air pipe 18. The front end of the air distribution pipe 9 is sealed to the front wall of the immersion tank 7 and connected to one end of the air supply pipe 15 through an air inlet 8 located on the front wall of the immersion tank 7. The other end of the air supply pipe 15 is connected to the high-pressure air source 16. The rear end of the air distribution pipe 9 is sealed to the rear wall of the immersion tank 7. The return air pipe 18 passes through both side walls of the air distribution pipe 9 and is fixedly connected to the air distribution pipe 9. The middle part of the return air pipe 18 is located inside the air distribution pipe 9, and the pipe wall is provided with an air inlet. The finished steel wire 17 output from the hot-dip galvanized aluminum-magnesium alloy steel wire production line passes through the return air pipe 18. The high-pressure air source 16 is compressed air, which can be provided by an air compressor or a high-pressure gas cylinder. High-pressure gas from high-pressure gas source 16 enters gas distribution pipe 9 through gas supply pipe 15, then enters return pipe 18 through air inlet in the middle of return pipe 18, and finally blows out from both ends of return pipe 18 (the airflow blown out from the end closer to liquid supply pipe 6 can blow the residual colorant on the surface of steel wire 17 back to immersion plating tank 7, and the airflow blown out from the end farther from liquid supply pipe 6 can dry steel wire 17), thus removing the residual colorant on the surface of steel wire 17.

[0022] Multiple immersion plating tanks 5 are provided, arranged along the length of the liquid supply pipe 6. Multiple return blow pipes 18 are also provided, each corresponding to one of the immersion plating tanks 5; that is, one return blow pipe is located downstream of each immersion plating tank. Increasing the number of immersion plating tanks 5 and return blow pipes 18 can improve production efficiency.

[0023] Valves are installed on both the return pipe 11 and the colorant delivery pipe 12.

[0024] The colorant tank 14 is equipped with a heating device to adjust the temperature of the colorant.

[0025] The temperature of the steel wire 17 before entering the immersion plating bath 5 must be maintained at 150℃-200℃. This is the key to ensuring the firmness of the coating. In northern regions, when the ambient temperature is low in winter, the steel wire should be kept warm when entering the immersion plating bath 5.

[0026] The working principle of this invention: Hot-dip galvanized aluminum-magnesium steel wire exits the zinc pot and undergoes high-pressure nitrogen ring blowing, completing the zinc-aluminum-magnesium coating process. At this point, the temperature of the zinc-aluminum-magnesium steel wire is around 400℃. The wire continues to move forward via the guide spool. When it reaches the immersion bath 5, the temperature is still maintained at 150℃-200℃. Due to the different wire diameters, there is a certain temperature deviation. As the wire passes through the immersion bath 5, the colorant adheres to the surface of the wire. After exiting the immersion bath 5, the excess colorant is blown away using a wire cleaning device (compressed air knife). At this point, the wire temperature is around 80℃. When the wire reaches the take-up point, the nano-inorganic coating has firmly adhered to the outside of the zinc-aluminum-magnesium steel wire using the heat of the wire, forming a dense protective film. This further enhances the corrosion resistance and environmental adaptability of the zinc-aluminum-magnesium steel wire.

[0027] This device is embedded at the end of the hot-dip galvanized aluminum-magnesium alloy steel wire production line, before the take-up device. It can fully utilize the residual heat of the hot-dip galvanized aluminum-magnesium alloy steel wire to complete the coating of the nano-inorganic coating. Moreover, it does not require additional workstations or workshops, thus simplifying the production process and reducing production costs.

[0028] The specific operation process of this invention is as follows: First, the device is embedded into the hot-dip galvanized aluminum-magnesium alloy steel wire production line. The coloring agent is prepared, which consists of a colorant and a curing agent. Before operation, the ambient temperature should be fully considered, and it should be selected whether to turn on the heat tracing function of the coloring agent.

[0029] When the motor 10 is started, the colorant in the colorant tank 14 is delivered to the supply pipe 6 via the lift pump 13 and the colorant delivery pipe 12. It then enters the immersion plating tank 5 through the supply hole 2, overflows through the wire overflow trough 1 to the bottom of the immersion plating box 7, and flows back to the colorant tank 14 through the return pipe 11. This allows the colorant to circulate in the device for at least 10 minutes, ensuring uniform mixing of the colorant and curing agent, and maintaining a stable colorant level in the immersion plating tank 5 that is higher than the steel wire 17.

[0030] The high-temperature steel wire 17 produced by the hot-dip galvanized aluminum-magnesium alloy steel wire production line is sequentially fed into the take-up device through the wire overflow trough 1 and the return blow pipe 18, and connected to the high-pressure air source 16. After the steel wire 17 is dip-coated and colored in the immersion tank 5, it enters the return blow pipe 18, where compressed air is used to blow the residual colorant on the surface of the steel wire 17 back into the immersion tank 7, and then back to the colorant tank 14 through the return pipe 11.

[0031] When the hot-dip galvanized steel wire 17 enters the immersion bath 5, it must be ensured that the colorant completely submerges the steel wire 17. The immersion time is calculated based on a DV value of 120 mm·m / min for zinc-aluminum-magnesium wire. The width of the immersion bath 5 is 0.3 m, and the immersion time is 0.15 seconds. The temperature drop during the immersion process is controlled within 90-100℃. If the temperature drop is large, and the wire temperature is not within the 70-80℃ range after the steel wire is pulled out of the immersion bath 5, it must be adjusted in time to ensure the adhesion of the colorant. There are two adjustment routes: 1. Adjust the DV value of the steel wire. Increasing the DV value is equivalent to shortening the immersion time of the steel wire in the immersion bath, thereby reducing the temperature drop of the steel wire. During this process, it is necessary to closely monitor the change in the amount of zinc on the zinc-aluminum-magnesium alloy steel wire. As the DV value increases, the amount of zinc will increase. It is necessary to adjust flexibly according to the change in the amount of zinc to reduce the excessive consumption of precious metals.

[0032] 2. Heat the colorant bath to increase the temperature of the colorant, thereby reducing the temperature drop of the steel wire in the immersion bath and ensuring the normal process temperature. Note that the temperature of the colorant bath should not exceed 80℃, otherwise it will cause the colorant to become unstable and the curing agent will be consumed faster.

[0033] The above adjustment process requires process technicians to be familiar with the on-site process parameters, accurately judge the quality stability of the nano-inorganic coating, and make flexible adjustments based on comprehensive analysis.

[0034] The concentration of the colorant decreases continuously during actual use, causing the color of the steel wire to change. This requires the process engineer to replenish the colorant and curing agent in a timely manner to ensure the uniformity of the steel wire color.

[0035] This coating device is a self-contained system that can be integrated into a hot-dip galvanized steel wire production line to complete the coating of the steel wire with a nano-inorganic coating, effectively reducing the investment cost of the hot-dip galvanized steel wire production line.

[0036] The beneficial effects of this invention are: 1. The residual heat of the hot-dip galvanized aluminum-magnesium steel wire itself is fully utilized to complete the coating of the nano-inorganic coating, without the need to increase secondary energy consumption. The whole process is stable and controlled, which can improve the corrosion resistance of the hot-dip galvanized aluminum-magnesium steel wire and meet the diversified color requirements of the hot-dip galvanized aluminum-magnesium steel wire.

[0037] 2. This device occupies only about 1 meter of space in the hot-dip galvanized steel wire production line, and the highest point of the device is 0.1 meters above the steel wire. It has strong process applicability and low production line upgrade and transformation costs.

Claims

1. A nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire, characterized in that, The system includes an immersion plating tank (7), a liquid supply pipe (6), a colorant supply device, and a wire cleaning device. The front wall of the immersion plating tank (7) is provided with a colorant inlet (3), and the bottom is provided with a colorant outlet (4). The front end of the liquid supply pipe (6) is sealed to the front wall of the immersion plating tank (7) and connected to the colorant supply device through the colorant inlet (3). The rear end is sealed to the rear wall of the immersion plating tank (7). The top of the liquid supply pipe (6) is provided with an immersion plating pool (5). The bottom of the immersion plating pool (5) is connected to the liquid supply pipe (6) through a liquid supply hole (2). Both the left and right side walls are provided with wire overflow grooves (1). The wire cleaning device is installed on one side of the immersion plating pool (5). The finished wire (17) output from the hot-dip galvanized aluminum-magnesium alloy steel wire production line passes through the wire overflow grooves (1) and the wire cleaning device on both sides of the immersion plating pool (5) in sequence.

2. The nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire according to claim 1, characterized in that, The steel wire cleaning device includes an air distribution pipe (9), an air supply pipe (15), a high-pressure air source (16), and a return pipe (18). The front end of the air distribution pipe (9) is sealed to the front wall of the immersion tank (7) and connected to one end of the air supply pipe (15) through an air inlet (8) provided on the front wall of the immersion tank (7). The other end of the air supply pipe (15) is connected to the high-pressure air source (16). The rear end of the air distribution pipe (9) is sealed to the rear wall of the immersion tank (7). The return pipe (18) passes through the two side walls of the air distribution pipe (9) and is fixedly connected to the air distribution pipe (9). The middle part of the return pipe (18) is located inside the air distribution pipe (9) and the pipe wall is provided with an air inlet. The finished steel wire (17) output from the hot-dip galvanized aluminum-magnesium alloy steel wire production line passes through the return pipe (18).

3. The nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire according to claim 2, characterized in that, The high-pressure air source (16) is compressed air.

4. A nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire according to any one of claims 1-3, characterized in that, The colorant supply device includes a motor (10), a return pipe (11), a colorant delivery pipe (12), a booster pump (13), and a colorant tank (14). The colorant tank (14) stores the colorant of the required color. The output shaft of the motor (10) is connected to the input shaft of the booster pump (13). The inlet pipe of the booster pump (13) is inserted into the colorant stored in the colorant tank (14). The outlet is connected to the colorant inlet (3) on the front wall of the immersion tank (7) through the colorant delivery pipe (12). One end of the return pipe (11) is connected to the colorant outlet (4) at the bottom of the immersion tank (7), and the other end is inserted into the colorant tank (14).

5. The nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire according to claim 4, characterized in that, The two side walls of the immersion tank (7) are provided with wire-passing windows (19), through which the finished steel wire (17) output from the hot-dip galvanized aluminum-magnesium alloy steel wire production line passes.

6. The nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire according to claim 2, characterized in that, Multiple immersion plating tanks (5) are provided, and the multiple immersion plating tanks (5) are arranged along the length direction of the liquid supply pipe (6). Multiple return blow pipes (18) are also provided, and they correspond one-to-one with the multiple immersion plating tanks (5).

7. The nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire according to claim 4, characterized in that, Valves are installed on both the return pipe (11) and the colorant delivery pipe (12).

8. The nano-inorganic coating device for hot-dip galvanized aluminum-magnesium alloy steel wire according to claim 4, characterized in that, The colorant tank (14) is equipped with a heat tracing device.