Evaporation apparatus and metal mask adsorption method
By setting through holes and vacuum adsorption structures in the evaporation equipment, the gap between the substrate and the edge of the metal mask is eliminated, solving the problem of uneven evaporation in the edge area during OLED display panel manufacturing and achieving high-quality display effects.
Patent Information
- Application Number
- CN202510638182.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-16
- Publication Date
- 2026-11-17
Smart Images

Figure CN123108476A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of OLED display panel manufacturing technology, and in particular to a vapor deposition apparatus and a method for adsorbing metal mask plates. Background Technology
[0002] In the manufacturing process of organic light-emitting diode (OLED) display panels, evaporation deposition technology plays a crucial role. This process mainly involves heating organic light-emitting materials to an evaporation state, causing them to be uniformly deposited on a substrate to form a thin film layer with specific functions. Specifically, in the evaporation process, high-precision metal masks (FMMs) are widely used to achieve precise deposition of different color sub-pixels (such as red (R), green (G), and blue (B)).
[0003] The design and configuration of the vapor deposition apparatus are key factors in achieving high-quality vapor deposition results. A typical vapor deposition apparatus mainly consists of core components such as a deposition chamber, a metal mask, and a magnetic plate. During operation, the substrate to be processed is first precisely placed onto the metal mask, and then the magnetic plate is placed stably on top of the substrate. The strong magnetic force generated by the magnetic plate then attracts the metal mask upwards, ensuring close contact with the substrate and forming a closed deposition space. This ensures that the organic material can be uniformly and accurately deposited on the designated area of the substrate.
[0004] However, in the actual vapor deposition bonding process, such as Figure 1 Combination Figure 2 As shown, since both substrate 002 and metal mask 001 have a certain thickness and weight, under the continuous action of gravity, their middle area often exhibits a certain degree of sagging, and their edges exhibit a certain degree of upturning. More complexly, due to differences in structural design and material selection between substrate 002 and metal mask 001, their degrees of sagging and upturning are not consistent. This inconsistency further exacerbates the adhesion problem at the edges, preventing the edges from achieving an ideal tight fit.
[0005] like Figure 3 Combination Figure 4As shown, the conventional method involves inverting a metal mask 001 onto a metal frame and inverting a substrate 002 onto the metal mask 001. While the metal mask 001 and substrate 002 can initially adhere under the influence of a magnetic field, due to physical limitations, the two still exhibit loose edge adhesion during the bonding process, resulting in a gap 003. This gap can lead to a series of adverse consequences during the vapor deposition process. Most notably, it causes larger vapor deposition shadows in the edge areas, affecting the thickness and uniformity of the organic material deposition in these areas. Consequently, the OLED display panel exhibits uneven brightness and color distortion in the edge areas during display, severely impacting the overall display effect.
[0006] This section provides background information related to this application, which is not necessarily prior art. Summary of the Invention
[0007] The purpose of this invention is to provide a vapor deposition apparatus and a metal mask adsorption method that can eliminate the gap between the substrate and the edge of the metal mask, so that the two edge areas are tightly attached, ensuring the deposition thickness and uniformity of organic materials in the edge areas, and making the OLED display panel have uniform brightness and color without distortion in the edge areas during display.
[0008] To achieve the above objectives, the following technical solution is provided:
[0009] Evaporation apparatus, characterized in that it comprises:
[0010] The vapor deposition chamber has a receiving cavity;
[0011] A metal mask is disposed in the receiving cavity. The metal mask is used to place the substrate to be vapor-deposited. The substrate has a plurality of through holes spaced apart circumferentially at least at its edge.
[0012] A magnet plate is disposed within the receiving cavity. The magnet plate is located on the side of the substrate away from the metal mask plate. The magnet plate is used to magnetically attract the entire metal mask plate to the substrate.
[0013] A back plate is disposed within the receiving cavity. The back plate has a plurality of vacuum adsorption structures circumferentially spaced at least at its edges. The back plate is located between the metal mask and the substrate. The vacuum adsorption structures are connected to the through holes. The back plate is used at least to adsorb the edges of the metal mask and the edges of the substrate to make them fit tightly together. The suction force of the vacuum adsorption structure is not greater than the yield strength of the metal mask.
[0014] As an optional solution for the vapor deposition apparatus, the metal mask plate is provided with a plurality of blind holes at least circumferential intervals at its edges, and a plurality of through holes are provided in a one-to-one correspondence with a plurality of blind holes. The back plate is placed on the substrate, and the vacuum adsorption structure, the through holes and the blind holes are connected in sequence.
[0015] As an alternative to the vapor deposition apparatus, the vacuum adsorption structure includes a vacuum nozzle that extends in a direction close to the substrate, and all the vacuum nozzles have the same extension length.
[0016] As an optional solution for the vapor deposition apparatus, the inner diameter of the vacuum nozzle is larger than the inner diameter of the through hole.
[0017] As an optional solution for the vapor deposition apparatus, a plurality of first protrusion structures are circumferentially spaced at the edge of the back plate. The first protrusion structures extend in a direction close to the substrate, and the extension length of the first protrusion structure is equal to the extension length of the vacuum nozzle.
[0018] As an optional solution for the vapor deposition apparatus, the back plate is uniformly provided with a plurality of second protrusion structures at the non-edges. The second protrusion structures extend in a direction close to the substrate, and the extension length of the second protrusion structure is greater than the extension length of the first protrusion structure.
[0019] As an optional solution for the vapor deposition apparatus, a vacuum channel is provided in the back plate, and the vacuum adsorption structure includes a vacuum suction hole, which is opened on the side of the back plate close to the substrate and is connected to the vacuum channel.
[0020] As an optional solution for the vapor deposition apparatus, the inner diameter of the vacuum suction hole is larger than the inner diameter of the through hole.
[0021] As an optional solution for the vapor deposition apparatus, the vapor deposition apparatus further includes a vacuum source, and several vacuum adsorption structures are all connected to the vacuum source, or
[0022] The vapor deposition apparatus includes several vacuum sources, and several vacuum adsorption structures are respectively connected to the corresponding several vacuum sources.
[0023] A metal mask adsorption method is applied to the vapor deposition apparatus mentioned above. The metal mask adsorption method includes: using a magnetic plate to magnetically attract the entire metal mask close to the substrate, starting vacuum adsorption from the edge of the metal mask, and then gradually expanding the adsorption range from the initial adsorption area until the edge of the metal mask is in contact with the edge of the substrate.
[0024] Compared with the prior art, the beneficial effects of the present invention are as follows:
[0025] The vapor deposition apparatus provided by this invention installs a metal mask, a substrate to be vapor-deposited, a back plate, and a magnet plate into the receiving cavity of the vapor deposition chamber, stacking them sequentially from bottom to top. The magnet plate magnetically attracts the entire metal mask close to the substrate, with a gap existing between the edge of the metal mask and the edge of the substrate. Multiple through-holes are circumferentially spaced along the edge of the metal mask, and multiple vacuum adsorption structures are circumferentially spaced along the edge of the back plate. These vacuum adsorption structures are correspondingly arranged with and interconnected with the through-holes. After the multiple vacuum adsorption structures are connected to a vacuum source, a negative pressure is created between the substrate to be vapor-deposited and the metal mask, adsorbing the edge of the metal mask onto the edge of the substrate, ensuring a tight fit between the edges of the metal mask and the substrate. The vapor deposition apparatus provided by this invention can eliminate the gap between the edges of the substrate and the metal mask, ensuring a tight fit between the two edge areas, guaranteeing the deposition thickness and uniformity of the organic material in the edge areas, and ensuring uniform brightness and color accuracy in the edge areas of the OLED display panel during display.
[0026] The metal mask adsorption method provided by this invention first uses a magnetic plate to magnetically attract the entire metal mask close to the substrate. Then, vacuum adsorption begins from the edge of the metal mask, gradually expanding the adsorption range from the initial adsorption area until the edge of the metal mask is in contact with the edge of the substrate. Through overall magnetic adsorption and edge vacuum adsorption, the gap between the substrate and the metal mask can be eliminated, making the substrate and the metal mask fit tightly together. This ensures the deposition thickness and uniformity of organic materials in the edge area, so that the OLED display panel has uniform brightness and no color distortion in the edge area during display. Attached Figure Description
[0027] To more clearly illustrate the technical solutions in the embodiments of the present invention, the accompanying drawings used in the description of the embodiments of the present invention will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on the content of the embodiments of the present invention and these drawings without creative effort.
[0028] Figure 1 A schematic diagram of a warped metal mask.
[0029] Figure 2 This is a schematic diagram of the substrate warping structure;
[0030] Figure 3 This is a schematic diagram of the structure of a metal mask plate before it is bonded to a substrate in the prior art.
[0031] Figure 4 This is a schematic diagram of the structure in the bonding of a metal mask plate and a substrate in the prior art;
[0032] Figure 5This is a cross-sectional view of the edge of the vapor deposition apparatus after assembly in Embodiment 1 of the present invention (vapor deposition chamber and protruding structure are not shown);
[0033] Figure 6 This is a cross-sectional view of the rear edge of the metal mask plate in Embodiment 1 of the present invention;
[0034] Figure 7 This is a cross-sectional view of the rear edge of the substrate in Embodiment 1 of the present invention;
[0035] Figure 8 This is a cross-sectional view of the edge of the vapor deposition apparatus after assembly in Embodiment 1 of the present invention (vapor deposition chamber is not shown);
[0036] Figure 9 This is a cross-sectional view of the edge of the back plate in Embodiment 1 of the present invention;
[0037] Figure 10 This is a cross-sectional schematic diagram of the entire back plate in Embodiment 1 of the present invention (vacuum adsorption structure not shown);
[0038] Figure 11 This is a cross-sectional view of the vapor deposition apparatus after assembly in Embodiment 2 of the present invention (vapor deposition chamber not shown);
[0039] Figure 12 This is a cross-sectional view of the edge of the back plate in Embodiment 2 of the present invention.
[0040] Figure label:
[0041] 001. Metal mask; 002. Substrate; 003. Gap;
[0042] 100, Metal mask; 101, Blind via; 200, Substrate; 201, Through-hole; 300, Backplate; 400, Magnet plate;
[0043] 301, Vacuum adsorption structure; 3011, Vacuum nozzle; 3012, Vacuum channel; 3013, Vacuum suction hole; 302, First protrusion structure; 303, Second protrusion structure. Detailed Implementation
[0044] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. The components of the embodiments of the present invention described and shown in the accompanying drawings can generally be arranged and designed in various different configurations.
[0045] In the description of this invention, it should be noted that the terms "upper," "lower," "left," "right," "vertical," "horizontal," "inner," and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, or the orientation or positional relationship commonly used when the product of this invention is in use. They are used only for the convenience of describing the invention and for simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on the invention. Furthermore, the terms "first," "second," and "third," etc., are used only to distinguish descriptions and should not be construed as indicating or implying relative importance. In the description of this invention, unless otherwise stated, "a plurality of" means two or more.
[0046] In the description of this invention, it should also be noted that, unless otherwise explicitly specified and limited, the terms "set" and "connection" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances.
[0047] Embodiments of the present invention are described in detail below. Examples of these embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals denote the same or similar elements or elements having the same or similar functions throughout. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and should not be construed as limiting the present invention.
[0048] To eliminate the gap between the substrate and the metal mask edge, ensuring a tight fit between the two edge areas and guaranteeing the deposition thickness and uniformity of the organic material in the edge areas, thereby ensuring uniform brightness and color accuracy in the edge areas of the OLED display panel during display, this embodiment provides a vapor deposition apparatus and a metal mask adsorption method. The following describes the process in conjunction with... Figures 5 to 12 The specific details of this embodiment will be described in detail. It should be noted that the structural features designed in this embodiment will not interfere with the display area of the substrate (i.e., the thin film layer with a specific function, which can also be called the color area) and the AA area of the metal mask.
[0049] Example 1
[0050] like Figures 5 to 10As shown, the vapor deposition apparatus in this embodiment includes a vapor deposition chamber, a metal mask 100, a magnet plate 400, and a back plate 300. The vapor deposition chamber has a receiving cavity. The metal mask 100 is disposed in the receiving cavity, and a substrate 200 to be vapor-deposited is placed on the metal mask 100. The substrate 200 has a plurality of through holes 201 spaced circumferentially at least at its edges. The magnet plate 400 is disposed in the receiving cavity, and the magnet plate 400 is located on the side of the substrate 200 away from the metal mask 100. The magnet plate 400 is used to magnetically attract the entire metal mask 100 to the substrate 200. A back plate 300 is disposed within a receiving cavity. At least at its edges, the back plate 300 has a plurality of vacuum adsorption structures 301 spaced circumferentially. The back plate 300 is located between the metal mask 100 and the substrate 200. The vacuum adsorption structures 301 communicate with through holes 201. The back plate 300 is used to adsorb the edges of the metal mask 100 into close contact with the edges of the substrate 200. The suction force of the vacuum adsorption structures 301 is not greater than the yield strength of the metal mask 100. When it is necessary to adsorb the entire metal mask 100 onto the lower surface of the substrate 200, a plurality of vacuum adsorption structures 301 can be uniformly disposed on the entire back plate 300, and a plurality of through holes 201 can be uniformly opened on the entire substrate 200. The adsorption area and adsorption force of the metal mask 100 can be controlled by controlling the operating parameters of the vacuum generator connected to the vacuum adsorption structures 301.
[0051] In summary, the vapor deposition apparatus provided in this embodiment installs a metal mask 100, a substrate 200 to be vapor-deposited, a back plate 300, and a magnet plate 400 into the accommodating cavity of the vapor deposition chamber, stacking them sequentially from bottom to top. The magnet plate 400 magnetically attracts the entire metal mask 100 close to the substrate 200, and there is a gap between the edge of the metal mask 100 and the edge of the substrate 200. By circumferentially spaced multiple through holes 201 at the edge of the metal mask 100 and circumferentially spaced multiple vacuum adsorption structures 301 at the edge of the back plate 300, the multiple vacuum adsorption structures 301 are arranged one-to-one with the multiple through holes 201 and are interconnected. After the multiple vacuum adsorption structures 301 are connected to a vacuum source, a negative pressure is formed between the substrate 200 to be vapor-deposited and the metal mask 100, which attracts the edge of the metal mask 100 to the edge of the substrate 200, ensuring that the edge of the metal mask 100 is in close contact with the edge of the substrate 200. The vapor deposition apparatus provided by the present invention can eliminate the gap between the substrate 200 and the metal mask 100 edge, so that the two edge areas are tightly attached, ensuring the deposition thickness and uniformity of organic materials in the edge area, and making the OLED display panel have uniform brightness and color without distortion in the edge area when displayed.
[0052] Understandably, the vapor deposition apparatus provided in this embodiment, through its innovative structural design, cleverly solves the long-standing industry problem of gaps between the substrate 200 and the metal mask 100 in traditional vapor deposition processes, and has a significant effect on improving the display quality of OLED display panels.
[0053] In traditional vapor deposition apparatuses, it is difficult to achieve a perfectly flat and seamless fit between the metal mask 100 and the substrate 200 during installation, especially at the edges, where gaps often exist. These gaps prevent the organic material from being uniformly deposited on the substrate 200 during vapor deposition, thus affecting the display performance of the OLED panel. In this embodiment, the vapor deposition apparatus integrates the metal mask 100, the substrate 200 to be vapor-deposited, the backplate 300, and the magnet plate 400 within the vapor deposition chamber, stacking them sequentially from bottom to top to form a stable overall structure. The magnet plate 400 magnetically attracts the entire metal mask 100 close to the substrate 200, providing initial positioning and fixation, allowing the metal mask 100 to roughly adhere to the substrate 200. However, small gaps may still exist between the edges of the metal mask 100 and the edges of the substrate 200 at this stage. To further eliminate this gap, this device cleverly incorporates multiple through-holes 201 spaced circumferentially along the edge of the metal mask 100, and multiple vacuum adsorption structures 301 spaced circumferentially along the edge of the back plate 300. These vacuum adsorption structures 301 are arranged in a one-to-one correspondence with the through-holes 201 and are interconnected. When the multiple vacuum adsorption structures 301 are connected to a vacuum source, a negative pressure environment is created between the substrate 200 to be vapor-deposited and the metal mask 100. Under this negative pressure, the edge of the metal mask 100 is rapidly and uniformly adsorbed onto the edge of the substrate 200, achieving a tight fit between the edges of the metal mask 100 and the substrate 200. This process not only eliminates the edge gap but also ensures the uniformity and stability of the bonding, laying a solid foundation for subsequent vapor deposition processes.
[0054] In the manufacturing process of OLED display panels, the deposition thickness and uniformity of organic materials are key factors affecting display quality. Uneven deposition thickness of the organic material on the substrate 200 can lead to brightness differences in different areas of the display panel, resulting in uneven brightness at the edges. Conversely, excessively thick or thin deposition thickness of the organic material can affect the color performance of the display panel, causing color distortion. The vapor deposition apparatus of this embodiment eliminates the gap between the substrate 200 and the metal mask 100, allowing the organic material to be deposited more uniformly on the substrate 200 during the vapor deposition process. Because the metal mask 100 is tightly attached to the edge of the substrate 200, the organic material, after passing through the vapor deposition holes of the metal mask 100, can be accurately deposited at the corresponding position on the substrate 200, avoiding deposition deviations caused by edge gaps. Simultaneously, the negative pressure adsorption effect keeps the metal mask 100 stable throughout the vapor deposition process, further ensuring the uniformity of organic material deposition. Therefore, the OLED display panel manufactured using the vapor deposition apparatus of this embodiment can present a high-quality display effect with uniform brightness in the edge area and no color distortion when displayed.
[0055] In addition to improving display quality, the vapor deposition apparatus of this embodiment also has the advantages of structural stability and high reliability. The rational layout and fixing method of components such as the magnet plate 400 and the back plate 300 in the apparatus design ensures that the entire apparatus maintains a stable working state during operation. The magnetic attraction of the magnet plate 400 not only provides sufficient adsorption force to ensure that the metal mask 100 is tightly attached to the substrate 200, but also allows adjustment of the adsorption force according to actual needs to accommodate metal masks 100 and substrates 200 of different specifications and materials. The vacuum adsorption structure 301 on the back plate 300 has good sealing and durability. During the vacuuming process, it can effectively maintain a negative pressure environment, ensuring a tight fit between the metal mask 100 and the edges of the substrate 200. Simultaneously, the suction force of the vacuum adsorption structure 301 is precisely controlled within the range not exceeding the yield strength of the metal mask 100, avoiding deformation or damage to the metal mask 100 due to excessive suction force. This design not only extends the service life of the metal mask 100, but also improves the stability and reliability of the entire vapor deposition apparatus, and reduces the maintenance cost and failure rate of the equipment.
[0056] The superior performance and significant effects of the vapor deposition apparatus in this embodiment enable its application in a wider range of fields. With the continuous development of OLED display technology, the quality requirements for display panels are becoming increasingly stringent. The solution provided by this apparatus for eliminating edge gaps and ensuring uniform organic material deposition is not only applicable to traditional OLED display panel manufacturing but also to emerging fields such as flexible OLED display panels and micro-OLED display panels. In the manufacturing of flexible OLED display panels, the requirements for the vapor deposition process are more stringent due to the bendable nature of the substrate 200. The stable structure and precise control capabilities of this apparatus can meet the high-precision requirements for organic material deposition in the manufacturing process of flexible OLED display panels, providing strong support for the development of flexible OLED display technology. In the manufacturing of micro-OLED display panels, the requirements for uniform organic material deposition and thickness control are even higher due to the smaller size of the display panels. The edge-tight bonding and uniform adsorption technology of this apparatus can effectively solve the edge effect problem in the manufacturing of micro-OLED display panels, improving product yield and display quality.
[0057] Furthermore, such as Figure 5 Combination Figure 6The metal mask 100 shown has a plurality of blind holes 101 spaced circumferentially at least its edges, and a plurality of through holes 201 corresponding one-to-one with the plurality of blind holes 101. A back plate 300 is placed on the substrate 200, and the vacuum adsorption structure 301, through holes 201, and blind holes 101 are sequentially connected. In some special cases, such as when there is significant airflow disturbance during the vapor deposition process or when the metal mask 100 itself is thin, unstable adsorption may occur, resulting in tiny gaps between the metal mask 100 and the edges of the substrate 200, affecting the deposition effect of organic materials. In this embodiment, after the blind holes 101 are provided at the edges of the metal mask 100, when the vacuum adsorption structure 301 starts working, air sequentially enters the vacuum adsorption structure 301 through the blind holes 101 and through holes 201. The presence of blind vias 101 is equivalent to forming tiny "adsorption chambers" at the edge of the metal mask 100. These "adsorption chambers" further enhance the adsorption force, making the edge of the metal mask 100 more firmly adsorbed onto the edge of the substrate 200. The blind vias 101 increase the contact area and depth of adsorption, greatly improving the stability of adsorption. Even when encountering external interference during the vapor deposition process, the metal mask 100 can maintain a tight fit with the edge of the substrate 200 without loosening or shifting, thus ensuring the stability and consistency of the vapor deposition process. The metal mask 100 needs to withstand a certain amount of adsorption force and mechanical stress during the vapor deposition process. In this embodiment, the blind vias 101 make the distribution of adsorption force at the edge of the metal mask 100 more uniform. The presence of blind vias 101 is equivalent to forming dispersed adsorption points at the edge of the metal mask 100. The adsorption force acts evenly on the edge of the metal mask 100 through these adsorption points, avoiding stress concentration at a few points. This uniform stress distribution effectively reduces stress concentration at the edges of the metal mask 100, protecting it from damage and extending its lifespan. Simultaneously, reduced deformation of the metal mask 100 ensures the deposition accuracy and quality of organic materials during the evaporation process. The evaporation apparatus of this embodiment significantly improves compatibility by incorporating blind vias 101. By adjusting parameters such as the diameter, depth, and number of blind vias 101, the magnitude and distribution of the adsorption force can be flexibly adjusted to adapt to different process requirements. For example, in the manufacture of high-resolution OLED display panels, the number of blind vias 101 can be appropriately increased and their diameter reduced to improve adsorption accuracy and uniformity; for the manufacture of large-size OLED display panels, the diameter and depth of the blind vias 101 can be appropriately increased to increase the adsorption force. This high degree of compatibility allows the evaporation apparatus of this embodiment to be widely applied in various types of OLED display panel manufacturing processes.
[0058] Furthermore, such as Figure 5 , Figure 8 Combination Figure 9 As shown, the vacuum adsorption structure 301 includes vacuum nozzles 3011, which extend along the side near the substrate 200, and all vacuum nozzles 3011 have the same extension length. In this embodiment, the uniform extension length of all vacuum nozzles 3011 ensures that the resistance encountered by the vacuum during transmission is basically consistent. When the vacuum source is activated, each vacuum nozzle 3011 can simultaneously and uniformly generate adsorption force, maintaining a stable vacuum pressure, acting on the edge region between the metal mask 100 and the substrate 200. This uniform adsorption force distribution ensures that the metal mask 100 and the substrate 200 are tightly bonded throughout the entire edge region, without local gaps or warping, thus providing a reliable guarantee for the precise deposition of organic materials and greatly improving the accuracy and quality of vapor deposition. Because all vacuum nozzles 3011 in this embodiment have the same extension length and uniform adsorption force distribution, during the equipment debugging phase, only the parameters of the vacuum source need to be uniformly set to achieve normal operation of the entire adsorption structure, greatly simplifying the debugging process. Regarding equipment maintenance, since the working conditions of each suction nozzle are basically the same, their wear and service life are also similar. Maintenance personnel can operate according to unified maintenance standards, reducing the complexity and difficulty of maintenance work. This not only reduces the time and labor costs of equipment debugging and maintenance, but also improves the reliability and stability of the equipment, reduces production losses caused by equipment failure, and thus effectively reduces overall production costs. In this embodiment, because all vacuum suction nozzles 3011 have the same extension length, their arrangement and layout can be more regular and compact. Under the premise of meeting the adsorption requirements, this makes the overall structure of the equipment simpler and more aesthetically pleasing.
[0059] Furthermore, the inner diameter of the vacuum nozzle 3011 is larger than the inner diameter of the through hole 201. When the inner diameter of the vacuum nozzle 3011 is equal to the inner diameter of the through hole 201, the direct adsorption effect of the vacuum nozzle 3011 on the substrate 200 is very small, and the vacuum nozzle 3011 only adsorbs the metal mask 100 through the through hole 201 of the substrate 200. However, this application designs the inner diameter of the vacuum nozzle 3011 to be larger than the inner diameter of the through hole 201, so that the vacuum adsorption structure 301 on the back plate 300 can act on both the metal mask 100 and the substrate 200 at the same time, providing dual protection. Moreover, the core principle of vacuum adsorption is to use atmospheric pressure to create a negative pressure between the metal mask 100 and the substrate 200, thus tightly adsorbing the two together. The inner diameter of the vacuum nozzle 3011, as the connecting channel between the vacuum source and the edge of the metal mask 100, directly determines the magnitude of the adsorption force. When the inner diameter of the vacuum nozzle 3011 is larger than the inner diameter of the through-hole 201 on the substrate 200, under the same vacuum conditions, the larger nozzle inner diameter can accommodate more air. Just as a wide river channel can transport water more smoothly than a narrow one, more airflow means a greater negative pressure is formed at the edge between the metal mask 100 and the substrate 200, resulting in stronger adsorption. For the metal mask 100, this enhanced adsorption ensures that it adheres tightly to the substrate 200 throughout the entire edge area, without localized lifting or gaps. As a key template in the vapor deposition process, the flatness and fit of the metal mask 100 directly affect the deposition accuracy of the organic material. If there are gaps between the metal mask 100 and the substrate 200, the organic material may leak or deposit unevenly at the gaps, leading to defects in the vapor deposition pattern, such as discontinuous lines or uneven color. The enhanced adsorption effectively avoids this situation, providing a solid foundation for the precise deposition of organic materials. For the substrate 200, the strong adsorption force also enables it to bond tightly with the metal mask 100. As the carrier of the organic material, the flatness and stability of the substrate 200's surface are crucial to the evaporation quality. If the substrate 200 experiences even slight movement or deformation during the evaporation process, it can cause deviations in the deposition position of the organic material, affecting the display panel's display effect. The design of the vacuum nozzle 3011 having an inner diameter larger than that of the through-hole 201 enhances the adsorption force, ensuring the stability of the substrate 200 during the evaporation process and guaranteeing a high-quality evaporation process.
[0060] In the vacuum adsorption process, airflow resistance is a significant influencing factor. A smaller inner diameter of the through-hole 201 increases airflow resistance, causing a greater attenuation of the vacuum pressure generated by the vacuum source during transmission, thus reducing the adsorption response speed. When the metal mask 100 needs to be quickly adsorbed onto the substrate 200, this low response speed may lead to delayed adsorption, affecting production efficiency. The vacuum nozzle 3011 in this design has an inner diameter larger than that of the through-hole 201, effectively reducing airflow resistance. When air enters the vacuum nozzle 3011 from the through-hole 201, the larger nozzle inner diameter allows for smoother airflow, reducing friction and collisions caused by narrow channels, thereby lowering airflow resistance. This allows the vacuum pressure generated by the vacuum source to be transmitted to the edges of the metal mask 100 and the substrate 200 more quickly, improving the adsorption response speed. In actual production, this means faster adsorption and positioning of the metal mask 100, shortening the production cycle, improving production efficiency, and achieving a dual rapid response for the adsorption of both the metal mask 100 and the substrate 200.
[0061] Furthermore, such as Figure 8 Combination Figure 9 As shown, a plurality of first protrusions 302 are circumferentially spaced along the edge of the back plate 300. The first protrusions 302 extend along the direction close to the substrate 200, and their extension length is equal to the extension length of the vacuum nozzle 3011. Since the extension length of the first protrusions 302 is equal to the extension length of the vacuum nozzle 3011, it can provide stable support throughout the entire effective adsorption range of the nozzle. This combination of mechanical fixation and vacuum adsorption achieves dual stable fixation of the substrate 200. Even with external interference, the substrate 200 can maintain a stable horizontal state under the combined action of mechanical and vacuum forces.
[0062] Furthermore, such as Figure 10 As shown, a plurality of second protrusions 303 are uniformly provided at the non-edge portion of the back plate 300. The second protrusions 303 extend in a direction close to the substrate 200, and the extension length of the second protrusions 303 is greater than the extension length of the first protrusions 302. Because the second protrusions 303 at the non-edge portion of the back plate 300 have a longer extension length, they can pre-form contact with the substrate 200. The second protrusions 303 can press down on the substrate 200 in advance by utilizing their length advantage, which helps to further reduce the gap between the substrate 200 and the metal mask 100.
[0063] For example, the backplate 300 in this embodiment can be made of aluminum or engineering plastic. When the backplate 300 is made of aluminum, aluminum has the characteristics of low density and high strength, which allows the backplate 300 to achieve significant weight reduction while ensuring structural rigidity. In high-speed automated equipment, the lightweight backplate 300 can reduce inertial load, reduce the energy consumption of the drive system, and improve the acceleration and positioning accuracy of the equipment. Aluminum has excellent processing performance and can be precisely formed into the first protrusion structure 302 and the second protrusion structure 303 to ensure its use in conjunction with the vacuum nozzle 3011. This synergistic design of structure and material allows the equipment to maintain stable adsorption performance during high-speed movement, avoiding adsorption failure or processing errors caused by deformation of the backplate 300. The thermal conductivity of aluminum is as high as 237 W / (m·K), which is much higher than that of traditional engineering plastics. The aluminum backplate 300 can quickly conduct heat to the heat dissipation system, avoiding deformation of the backplate 300 or vacuum adsorption failure caused by local overheating. Furthermore, the uniform temperature characteristics of the aluminum backplate 300 reduce thermal stress caused by temperature gradients, minimize minor deformations of the protruding structure and the nozzle mating surface, and further enhance the long-term stability of the adsorption system. A dense alumina protective film can form on the aluminum surface, giving it excellent corrosion resistance.
[0064] Furthermore, in some application scenarios, the vapor deposition apparatus also includes a vacuum source, with several vacuum adsorption structures 301 connected to it. The vacuum source employs modular integration technology, integrating components such as vacuum pumps, filters, pressure sensors, and solenoid valves into a closed cavity. A multi-stage gas distribution system enables independent or coordinated control of multiple vacuum adsorption structures 301. Each adsorption unit is equipped with an independent pressure regulating valve to ensure that pressure fluctuations at each adsorption site are less than ±0.5%, meeting the flatness control requirements of large-size substrates 200. Optionally, the interface between the vacuum source and the vacuum adsorption structure 301 adopts a quick-release design, allowing for rapid connection to a new vacuum source in case of a vacuum source failure, shortening maintenance time and improving work efficiency.
[0065] In other application scenarios, the vapor deposition apparatus includes several vacuum sources, with several vacuum adsorption structures 301 connected to corresponding vacuum sources. Each vacuum adsorption structure 301 is equipped with an independent vacuum source, enabling millimeter-level zoned control of the pressure within the adsorption surface. During vapor deposition on the substrate 200, the vacuum level in each area is dynamically adjusted using a PID algorithm, reducing the flatness deviation of the substrate 200 from the traditional ±50μm to within ±10μm, significantly improving the uniformity of the vapor-deposited film thickness. Independently setting up the vacuum sources not only shortens the start-up and shutdown response time, but also allows the system to automatically isolate the faulty unit if a vacuum adsorption structure 301 leaks, preventing a drop in the overall vacuum level and ensuring continuous operation of the equipment. Furthermore, a vacuum sensor is integrated into the pipeline of each vacuum source, combined with machine learning algorithms to predict the performance degradation of the adsorption structure in real time. When the adsorption force drops to a threshold, the system automatically triggers the vacuum source to evacuate.
[0066] This embodiment also provides a metal mask adsorption method, which is applied to the vapor deposition apparatus mentioned above. The metal mask adsorption method includes: using a magnetic plate 400 to magnetically attract the entire metal mask 100 close to the substrate 200, starting vacuum adsorption from the edge of the metal mask 100, and then gradually expanding the adsorption range from the initial adsorption area until the edge of the metal mask 100 is in contact with the edge of the substrate 200.
[0067] In precision processes such as advanced semiconductor manufacturing or high-precision display panel production, an innovative magnetic-vacuum composite positioning technology can be used to achieve high-precision bonding between a metal mask 100 (typically a single piece of high-strength, high-flatness metal structure) and a substrate 200 (such as a glass substrate 200, silicon wafer, etc.). The specific implementation process is as follows: First, the metal mask 100 is selected as the fixing carrier, and the substrate 200 is placed on the upper surface of the metal mask 100. The back plate 300 and the magnet plate 400 are then pressed down in sequence. The surface of the strongly magnetic magnet plate 400 undergoes precision machining to ensure that its flatness and roughness meet the requirements for high-precision positioning. Initial physical positioning is achieved using magnetic attraction, at which point a stable magnetic attraction force is formed between the metal mask 100 and the magnet plate 400. Subsequently, the vacuum adsorption system is activated. This system generates a localized negative pressure environment by using a vacuum adsorption structure 301 (micropore array or vacuum cavity structure) pre-set at the edge of the backplate 300 and through holes 201 spaced circumferentially at the edge of the substrate 200. Starting from a fixed point or segmented area at the edge of the metal mask 100, a vacuum adsorption force is gradually applied, ensuring a tight, airtight contact between the metal mask 100 and the substrate 200 above it in that area. During this process, the application of the vacuum adsorption force must be precisely controlled to avoid deformation of the metal mask 100 or damage to the substrate 200 due to excessive pressure. As vacuum adsorption continues, the adsorption area gradually expands outward from the initial point or segment, forming a continuous adsorption band. During this process, a high-precision displacement sensor or vision inspection system is required to monitor the relative position and adhesion status between the metal mask 100 and the substrate 200 in real time, ensuring that the expansion path of the adsorption area is consistent with the preset trajectory, while avoiding minor displacements or tilting during the adsorption process. Finally, when the vacuum adsorption range expands to the entire edge area of the metal mask 100, the edge of the metal mask 100 achieves precise adhesion to the edge of the substrate 200 under the combined action of magnetic attraction and vacuum adsorption. At this point, minor deformations caused by environmental factors (such as temperature changes, air pressure fluctuations, etc.) can be eliminated through pressure balance adjustment or temperature compensation, ensuring optimal adhesion between the metal mask 100 and the substrate 200, and providing reliable assurance for subsequent high-precision pattern transfer or material deposition processes.
[0068] Example 2
[0069] This embodiment provides a vapor deposition apparatus. Compared with Embodiment 1, the basic structure of the vapor deposition apparatus provided in this embodiment is the same as that in Embodiment 1, except that the setting of the vacuum adsorption structure 301 is different. This embodiment will not describe the structure that is the same as that in Embodiment 1 again.
[0070] Furthermore, such as Figure 11 Combination Figure 12As shown, a vacuum channel 3012 is provided within the backplate 300, and the vacuum adsorption structure 301 includes vacuum suction holes 3013. The vacuum suction holes 3013 are located on the side of the backplate 300 near the substrate 200 and are connected to the vacuum channel 3012. In the design of precision equipment, the backplate 300, as one of the core support components, is crucial for achieving efficient process operations due to its rational internal structure layout. Specifically, the vacuum channel 3012 is carefully designed within the backplate 300. This design aims to achieve stable and precise bonding between the metal mask 100 and the substrate 200 through vacuum adsorption technology. One of the core components of the vacuum adsorption structure 301 is the vacuum suction holes 3013. These tiny but crucial holes are precisely formed on the surface of the backplate 300 near the substrate 200. Each vacuum suction hole 3013 is directly connected to the vacuum channel 3012 inside the backplate 300, forming a complete vacuum adsorption network. When the vacuum pump starts and evacuates the vacuum channel 3012, a negative pressure environment is rapidly formed between the edge of the metal mask 100 and the edge of the substrate 200. This negative pressure environment acts directly on the surface of the metal mask 100 through the vacuum suction hole 3013 and the through hole 201 of the substrate 200, generating a strong adsorption force. As the vacuum level gradually increases, the edge of the metal mask 100 is firmly adsorbed onto the lower surface of the edge of the substrate 200, forming a tight fit between the two. This bonding method not only ensures the stability of the metal mask 100 and the substrate 200 in subsequent process operations, effectively preventing accuracy loss due to vibration or displacement, but also greatly improves the repeatability and consistency of the process.
[0071] Furthermore, the inner diameter of the vacuum suction hole 3013 is larger than the inner diameter of the through hole 201. When the inner diameter of the vacuum suction hole 3013 is equal to the inner diameter of the through hole 201, the direct adsorption effect of the vacuum suction hole 3013 on the substrate 200 is very small, and the vacuum suction hole 3013 only adsorbs the metal mask plate 100 through the through hole 201 of the substrate 200. However, this application designs the inner diameter of the vacuum suction hole 3013 to be larger than the inner diameter of the through hole 201, so that the vacuum adsorption structure 301 on the back plate 300 can act on both the metal mask plate 100 and the substrate 200 at the same time, providing dual protection. Moreover, the core principle of vacuum adsorption is to use atmospheric pressure to create a negative pressure between the metal mask plate 100 and the substrate 200, thus tightly adsorbing the two together. The inner diameter of the vacuum suction hole 3013, as the connection channel between the vacuum source and the edge of the metal mask plate 100, directly determines the magnitude of the adsorption force. When the inner diameter of the vacuum suction orifice 3013 is larger than the inner diameter of the through-hole 201 on the substrate 200, under the same vacuum conditions, the larger inner diameter of the vacuum suction orifice 3013 can accommodate more airflow. More airflow means a greater negative pressure is formed at the edge between the metal mask 100 and the substrate 200, resulting in stronger adsorption force. For the metal mask 100, this enhanced adsorption force ensures that it adheres tightly to the substrate 200 throughout the entire edge area, preventing localized lifting or gaps. As a key template in the vapor deposition process, the flatness and adhesion of the metal mask 100 directly affect the deposition accuracy of the organic material. If there are gaps between the metal mask 100 and the substrate 200, the organic material may leak or deposit unevenly at the gaps, leading to defects in the vapor deposition pattern, such as discontinuous lines or uneven color. The enhanced adsorption force effectively avoids this, providing a solid foundation for the precise deposition of the organic material. Similarly, the strong adsorption force ensures that the substrate 200 adheres tightly to the metal mask 100. As the carrier of organic materials, the flatness and stability of the substrate 200 surface are crucial to the quality of vapor deposition. Even slight movement or deformation of the substrate 200 during the vapor deposition process can cause deviations in the deposition position of the organic materials, affecting the display panel's performance. The design of the vacuum suction hole 3013 having an inner diameter larger than that of the through hole 201 enhances the adsorption force, ensuring the stability of the substrate 200 during the vapor deposition process and guaranteeing a high-quality vapor deposition process.
[0072] Note that the above description is merely a preferred embodiment of the present invention and the technical principles employed. Those skilled in the art will understand that the present invention is not limited to the specific embodiments described herein, and various obvious changes, readjustments, and substitutions can be made without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in detail through the above embodiments, the present invention is not limited to the above embodiments, and may include many other equivalent embodiments without departing from the concept of the present invention, the scope of which is determined by the scope of the appended claims.
Claims
1. A vapor deposition apparatus, characterized in that, include: The vapor deposition chamber has a receiving cavity; A metal mask plate (100) is disposed in the receiving cavity. The metal mask plate (100) is used to place the substrate (200) to be vapor-deposited. The substrate (200) has a plurality of through holes (201) spaced circumferentially at least at its edge. A magnet plate (400) is disposed in the receiving cavity. The magnet plate (400) is located on the side of the substrate (200) away from the metal mask plate (100). The magnet plate (400) is used to magnetically attract the entire metal mask plate (100) close to the substrate (200). A back plate (300) is disposed within the receiving cavity. The back plate (300) has a plurality of vacuum adsorption structures (301) spaced circumferentially at least its edges. The back plate (300) is located between the metal mask plate (100) and the substrate (200). The vacuum adsorption structures (301) communicate with the through holes (201). The back plate (300) is at least used to adsorb the edges of the metal mask plate (100) and the edges of the substrate (200) to fit tightly together. The suction force of the vacuum adsorption structure (301) is not greater than the yield strength of the metal mask plate (100).
2. The vapor deposition apparatus according to claim 1, characterized in that, The metal mask plate (100) has a plurality of blind holes (101) spaced circumferentially at least at its edge. A plurality of through holes (201) are provided in a one-to-one correspondence with a plurality of blind holes (101). The back plate (300) is placed on the substrate (200). The vacuum adsorption structure (301), the through holes (201) and the blind holes (101) are connected in sequence.
3. The vapor deposition apparatus according to claim 1, characterized in that, The vacuum adsorption structure (301) includes a vacuum nozzle (3011) that extends in a direction close to the substrate (200), and all the vacuum nozzles (3011) have the same extension length.
4. The vapor deposition apparatus according to claim 3, characterized in that, The inner diameter of the vacuum nozzle (3011) is larger than the inner diameter of the through hole (201).
5. The vapor deposition apparatus according to claim 3, characterized in that, The back plate (300) has a plurality of first protrusions (302) spaced circumferentially at its edge. The first protrusions (302) extend in a direction close to the substrate (200), and the extension length of the first protrusions (302) is equal to the extension length of the vacuum nozzle (3011).
6. The vapor deposition apparatus according to claim 5, characterized in that, The back plate (300) is uniformly provided with a plurality of second protrusion structures (303) at the non-edges. The second protrusion structures (303) extend in a direction close to the substrate (200), and the extension length of the second protrusion structure (303) is greater than the extension length of the first protrusion structure (302).
7. The vapor deposition apparatus according to claim 1, characterized in that, A vacuum channel (3012) is provided in the back plate (300), and the vacuum adsorption structure (301) includes a vacuum suction hole (3013). The vacuum suction hole (3013) is opened on the side of the back plate (300) near the substrate (200), and the vacuum suction hole (3013) is connected to the vacuum channel (3012).
8. The vapor deposition apparatus according to claim 7, characterized in that, The inner diameter of the vacuum suction hole (3013) is larger than the inner diameter of the through hole (201).
9. The vapor deposition apparatus according to any one of claims 1-8, characterized in that, The vapor deposition apparatus also includes a vacuum source, and several vacuum adsorption structures (301) are connected to the vacuum source, or The vapor deposition apparatus includes several vacuum sources, and several vacuum adsorption structures (301) are respectively connected to the corresponding several vacuum sources.
10. A metal mask adsorption method, characterized in that, The metal mask adsorption method is applied to the vapor deposition apparatus as described in any one of claims 1 to 9. The metal mask adsorption method includes: using a magnetic plate (400) to magnetically attract the entire metal mask (100) close to the substrate (200), starting vacuum adsorption from the edge of the metal mask (100), and then gradually expanding the adsorption range from the initial adsorption area until the edge of the metal mask (100) is in contact with the edge of the substrate (200).