A Smart Electroplating Control Method Based on Online Film Thickness Monitoring

The intelligent electroplating control method, which uses online film thickness monitoring and multi-level parameter correction, solves the problem of coating thickness deviating from the target value during the electroplating process. It realizes real-time monitoring and automatic adjustment of coating thickness, thereby improving the stability and efficiency of the electroplating process.

CN123108710APending Publication Date: 2026-11-17CHINA UNITED ENG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611435231.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-16
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing electroplating technology cannot monitor the coating thickness in real time, which means that process parameters cannot automatically adapt to fluctuations in electrolyte concentration and changes in the surface condition of the workpiece, resulting in the coating thickness deviating from the target value and producing defective products.

Method used

An online film thickness monitoring method is adopted to collect electroplating process parameters in real time. Through multi-level parameter correction and control, current density, temperature, pH value, stirring and suspension posture are controlled to ensure the uniformity of coating thickness and consistency with the target value.

Benefits of technology

It enables real-time monitoring and automatic adjustment of coating thickness, reducing the generation of defective products and improving the stability and efficiency of the electroplating process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123108710A_ABST
    Figure CN123108710A_ABST
Patent Text Reader

Abstract

This invention discloses an intelligent electroplating control method based on online film thickness monitoring, relating to the field of electroplating processing technology. The method includes the following steps: S01, collecting real-time process parameters and online film thickness monitoring data during the electroplating process, and performing initial state analysis in conjunction with a preset target coating thickness value to obtain current coating growth state parameters and process deviation information; S02, based on the current coating growth state parameters and process deviation information, performing first-level parameter correction processing on the electroplating current density and electroplating temperature to obtain first-level correction parameters; S03, controlling the electroplating process according to the first-level correction parameters and simultaneously monitoring the film thickness change rate. This invention continuously monitors the film thickness change rate and regional distribution uniformity during the electroplating process, enabling timely parameter correction before the coating thickness deviates from the target value, avoiding material and energy waste caused by discovering defective products afterward.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of electroplating technology, and in particular to an intelligent electroplating control method based on online film thickness monitoring. Background Technology

[0002] In actual production, electroplating quality is affected by multiple process parameters, including current density, temperature, electroplating time, pH value, agitation, and additives. Among these, coating thickness is the core indicator for measuring electroplating quality, directly determining the product's key characteristics such as corrosion resistance, wear resistance, and conductivity.

[0003] Currently, the electroplating industry mainly relies on the following methods to control the coating thickness: One approach is to implement open-loop control through pre-set process parameters (such as current density and electroplating time), that is, to estimate the coating thickness based on empirical formulas. Secondly, after electroplating is completed, offline testing methods (such as X-ray fluorescence thickness measurement, eddy current thickness measurement, etc.) are used to conduct random checks on the coating thickness. Third, during the electroplating process, process parameters are manually adjusted after periodic sampling and testing.

[0004] In actual operation, the above-mentioned technical methods all have the same problem: they cannot know the actual growth of the coating thickness in real time. When the electrolyte concentration fluctuates, the temperature changes, or the surface condition of the workpiece changes, the preset process parameters cannot adapt automatically, causing the coating thickness to deviate from the target value and producing a large number of defective products. Summary of the Invention

[0005] To overcome the above problems, this invention proposes an intelligent electroplating control method based on online film thickness monitoring. During the electroplating process, the film thickness change rate and regional distribution uniformity are continuously monitored, and parameters can be corrected in time before the coating thickness deviates from the target value, avoiding material and energy waste caused by the discovery of defective products after the fact.

[0006] The technical solution adopted in this invention is: an intelligent electroplating control method based on online film thickness monitoring, comprising the following steps: S01. Collect real-time process parameters during the electroplating process, combine them with the preset target value of coating thickness to perform initial state analysis, and obtain the current coating growth state parameters and process deviation information. S02. Based on the current coating growth state parameters and process deviation information, perform first-level parameter correction processing on the electroplating current density and electroplating temperature to obtain first-level correction parameters; S03. Control the electroplating process according to the first-level correction parameters and monitor the film thickness change rate simultaneously. When the film thickness change rate deviates from the preset rate threshold, trigger the second-level parameter correction to obtain the second-level correction parameters. S04. Based on the second-level correction parameters, continue to execute the electroplating process and continuously collect film thickness distribution data in different areas of the workpiece surface. Perform uniformity analysis on the film thickness distribution data and generate regional uniformity labels. S05. Based on the regional uniformity label, perform third-level parameter correction processing on the electrolyte stirring parameters and the workpiece suspension posture to obtain the third-level correction parameters. S06. Based on the relationship between the cumulative charge and the film thickness change rate during the electroplating process, calculate the instantaneous dissolution efficiency of the anode and generate the anode supplement control signal and the anode-cathode spacing compensation amount. S07. Perform comprehensive electroplating control based on the first-level correction parameters, the second-level correction parameters, the third-level correction parameters, the anode supplement control signal, and the anode-cathode spacing compensation amount, and generate a complete process control record after electroplating is completed.

[0007] Step S01 of the present invention specifically includes the following steps: S11. Collect real-time process parameters during the electroplating process, perform parameter validity identification and outlier removal processing on the real-time process parameters, extract online film thickness monitoring data and generate film thickness-time series mapping information; S12. Based on the film thickness-time series mapping information, calculate the current actual growth rate of the coating and compare it with the preset theoretical growth rate to generate rate deviation information. S13. Perform a difference analysis between the rate deviation information and the preset coating thickness target value to generate thickness difference information; S14. The rate deviation information and thickness difference information are associated and registered to form the current coating growth state parameters and process deviation information.

[0008] In step S12 of the present invention: The actual growth rate of the current coating is calculated as follows: The controller extracts the most recent valid data from the film thickness-time series mapping information and uses linear regression or least squares method to fit the relationship between film thickness and time; since the film thickness and time are linearly related under ideal conditions during the electroplating process, the slope of the fitted line is the actual growth rate of the current coating. The preset formula for calculating the theoretical growth rate is: V theory =(η×M×i) / (n×F×ρ), where η is the current efficiency, M is the molar mass of the metal, i is the cathode current density, n is the valence state of the metal ion, F is the Faraday constant, and ρ is the coating metal density; After obtaining the actual growth rate and the theoretical growth rate, calculate the rate deviation: ΔV = V actual -V theory and the relative deviation rate δV=(Vactual -V theory ) / V theory ×100%.

[0009] Step S02 of the present invention specifically includes the following steps: S21. Based on the rate deviation information in the current coating growth state parameters and process deviation information, perform first-level correction calculation on the current density to generate a current density correction value. S22. Based on the thickness difference information in the current coating growth state parameters and process deviation information, perform first-level correction calculation on the electroplating temperature to generate an electroplating temperature correction value. S23. Perform a coupling effect verification on the current density correction value and the electroplating temperature correction value, and determine whether the corrected current density and electroplating temperature meet the preset cooperative constraint conditions: When the co-constraint conditions are met, the current density correction value and the electroplating temperature correction value are registered as first-level correction parameters; When the cooperative constraint conditions are not met, the current density correction value and the electroplating temperature correction value are adjusted by compromise until the cooperative constraint conditions are met and then registered as the first-level correction parameter.

[0010] Step S03 of the present invention specifically includes the following steps: S31. Control output is executed on the electroplating power supply and heating device according to the first-level correction parameters, so that the electroplating process operates at the corrected current density and electroplating temperature. S32. During the operation of the first-level correction parameters, continuously monitor the film thickness change rate and record the rate-time change curve; S33. When the film thickness change rate in the rate-time change curve exceeds the preset rate threshold range, the second-level parameter correction is triggered. S34. In the second-level parameter correction, the electroplating pH value and additive supply rate are corrected according to the direction and magnitude of the deviation between the film thickness change rate and the preset rate threshold, and the second-level correction parameters are generated.

[0011] Step S04 of the present invention specifically includes the following steps: S41. Continue the electroplating process according to the second-level correction parameters, and collect film thickness distribution data of different areas on the workpiece surface through multi-point film thickness sensors during the electroplating process. S42. Perform region location registration processing on the film thickness distribution data, associate and map each film thickness measurement value with the corresponding workpiece surface region location, and generate a region-film thickness mapping table. S43. Based on the region-film thickness mapping table, calculate the deviation between the film thickness value of each region and the overall average film thickness value, and classify and mark each region according to the degree of deviation to generate a region uniformity label.

[0012] The regional uniformity label of the present invention includes a uniform qualified region, a thinner region, and a thicker region.

[0013] Step S05 of the present invention specifically includes the following steps: S51. Based on the distribution positions of the thinner and thicker regions in the regional uniformity label, identify the direction of uneven electrolyte stirring and the direction of workpiece suspension posture deviation. S52. Based on the direction of uneven stirring of the electrolyte, perform correction processing on the stirring intensity and stirring direction of the stirring device to generate stirring parameter correction values; S53. Based on the direction of the workpiece suspension posture deviation, perform correction processing on the workpiece suspension angle and suspension depth to generate suspension posture correction values. S54. Register the stirring parameter correction value and the suspension attitude correction value as third-level correction parameters.

[0014] Step S06 of the present invention specifically includes the following steps: S61. Accumulate the amount of electricity applied during the electroplating process in real time, and calculate the theoretical dissolution mass of the anode based on the accumulated amount of electricity applied; S62. Calculate the actual deposited metal mass based on the film thickness change rate and the workpiece plating area, and divide the actual deposited metal mass by the theoretical dissolution mass to obtain the anode instantaneous dissolution efficiency. S63. When the instantaneous dissolution efficiency of the anode is lower than a preset efficiency threshold, an anode replenishment control signal is generated according to the efficiency difference. The anode replenishment control signal is used to trigger the anode replenishment actuator to replenish anode metal into the plating tank. S64. Based on the cumulative trigger frequency of the anode replenishment control signal and the anode dissolution history record, calculate the remaining effective volume of the anode and predict the remaining service life of the anode. When the remaining service life of the anode is lower than the preset service life threshold, generate an anode-cathode spacing compensation amount. The anode-cathode spacing compensation amount is used to drive the electromechanical actuator to adjust the anode suspension height to maintain the preset anode-cathode spacing.

[0015] Step S07 of the present invention specifically includes the following steps: S71. The first-level correction parameter, the second-level correction parameter, and the third-level correction parameter are arranged according to the time order of correction triggering to form a correction parameter sequence, and the anode-cathode spacing compensation amount is embedded as a spatial reference adjustment amount at the end of the correction parameter sequence. S72. Based on the modified parameter sequence, perform integrated linkage control on electroplating current density, electroplating temperature, electroplating pH value, additive supply rate, stirring parameters, workpiece suspension posture and anode suspension height. S73. During the integrated linkage control process, continuously monitor the film thickness change trend and the regional uniformity change trend; S74. When the film thickness variation trend and the regional uniformity variation trend meet the preset convergence conditions, lock the current control parameters and maintain operation until the electroplating is completed. S75. The real-time process parameter sequence, online film thickness monitoring data sequence, various correction parameter sequences, anode supplement control signal sequence, anode-cathode spacing compensation amount sequence, and regional uniformity label sequence of this electroplating process are correlated and organized to form a process control record. S76. Perform data compression and index encoding processing on the process control records to generate traceable process control record files; S77. Store the process control record file in the historical process database and associate it with the corresponding workpiece batch information and coating type information; S78. After electroplating is completed, the coating thickness compliance of this electroplating is comprehensively evaluated according to the process control record, and a coating quality evaluation report is generated. When the coating quality evaluation report shows that there are areas where the thickness does not meet the standard, the location information and degree of non-compliance information of the areas where the thickness does not meet the standard are marked as re-plating requirement information and output to the re-plating process control terminal.

[0016] The present invention has at least the following beneficial effects: The effective value of the current density directly depends on the actual dissolution output capacity of the anode. When the anode dissolution efficiency decreases, the actual concentration of metal ions deposited at the same set current density decreases, causing a reference shift in the current density correction value obtained from the first-level correction. This invention calculates the instantaneous anode dissolution efficiency in real time and feeds this efficiency value back to the first-level correction module for secondary calibration of the current density correction value, ensuring that the actual effect of the first-level correction is consistent with the preset target.

[0017] This invention optimizes the ion transport path by dynamically adjusting the anode-cathode spacing compensation amount, while replenishing the anode. This effectively alleviates local ion concentration fluctuations caused by anode consumption, thereby reducing the trigger frequency and adjustment range of the second-level correction, and allowing the pH value and additive supply rate to operate within a more stable range.

[0018] The anode-cathode spacing compensation amount generated by this invention can directly drive the electromechanical actuator to maintain the preset spacing in real time, so that the optimization effect of the third-level correction on the stirring direction and suspension angle can be fully utilized, ensuring the synchronous matching of ion migration path and electric field distribution, and fundamentally improving the accuracy of regional uniformity correction. Attached Figure Description

[0019] Figure 1 This is a structural diagram of the electroplating processing apparatus used in an embodiment of the present invention; Figure 2 This is a flowchart of an embodiment of the present invention; Figure 3 This is a flowchart illustrating the process execution decision in an embodiment of the present invention. Detailed Implementation

[0020] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0021] like Figure 2 As shown, this embodiment provides an intelligent electroplating control method based on online film thickness monitoring. This method is applied to processes such as... Figure 1 The electroplating and post-plating treatment steps in the electroplating apparatus shown include: The electroplating process includes: placing on the pickling cap - SUS degreasing - electrolytic degreasing (twice, in different pools) - water rinsing (twice, in different pools) - high-level water rinsing - pickling (at least four times, in different pools) - water rinsing (twice, in different pools) - spray water rinsing - neutralization - zinc plating (performed nine times in different pools).

[0022] The post-plating treatment process includes: water washing - SUS ultrasonic washing - spray water washing - three-stage blue-white treatment - water washing - spray water washing - hot water washing - three-stage five-color treatment - water washing - spray water washing - air drying - packaging.

[0023] A smart electroplating control method based on online film thickness monitoring includes the following steps: S01. Collect real-time process parameters during the electroplating process, and perform initial state analysis in conjunction with the preset target coating thickness value to obtain the current coating growth state parameters and process deviation information. Specifically, this includes the following steps: S11. Collect real-time process parameters during the electroplating process, perform parameter validity identification and outlier removal processing on the real-time process parameters, extract online film thickness monitoring data and generate film thickness-time series mapping information; S12. Based on the film thickness-time series mapping information, calculate the actual growth rate of the current coating and compare it with the preset theoretical growth rate to generate rate deviation information. S13. Perform a gap analysis between the rate deviation information and the preset coating thickness target value to generate thickness difference information. S14. Complete the association and registration of rate deviation information and thickness difference information to form the current coating growth state parameters and process deviation information.

[0024] Specifically, a multi-type sensor acquisition system is deployed on the electroplating equipment. Current density is directly read through the digital output interface of the rectified power supply; electroplating temperature is acquired in real time by an immersion thermocouple or platinum resistance temperature sensor (PT100); pH value is continuously monitored by an online pH meter; additive supply rate is obtained through the pulse frequency of the metering pump or feedback from a flow meter; stirring parameters are obtained from the speed feedback signal of the stirring motor (galvanizing) driver; and electroplating time is recorded by the internal timer of the PLC controller. These sensor signals are fed into the central controller (PLC or industrial computer) via analog input modules (4-20mA or 0-10V) or fieldbus protocols (such as Modbus, Profibus, EtherCAT).

[0025] Secondly, online film thickness monitoring data is acquired using either an X-ray fluorescence thickness gauge or an eddy current thickness gauge. The X-ray fluorescence thickness gauge is installed at the end of the electroplating tank or at the detection station after the workpiece has been removed from the plating solution, periodically scanning the coating thickness on the workpiece surface in a non-contact manner. The eddy current thickness gauge, on the other hand, uses an eddy current probe close to the workpiece surface and infers the coating thickness by utilizing the impedance change due to the eddy current effect. Both thickness gauges output thickness values ​​at a fixed sampling frequency (e.g., 1Hz to 10Hz), synchronized with the controller's timestamp.

[0026] Furthermore, regarding data validity identification, the controller's built-in data preprocessing module performs three-fold validity checks on each received process parameter and film thickness data: First, determine whether the parameter value is within the preset physically feasible range (e.g., if the temperature is not within the 0-100℃ range, it is considered invalid). Secondly, determine whether the rate of change between adjacent sampling points exceeds the preset maximum rate of change threshold. If it does, it indicates that the sensor may have a jump fault. Third, for multiple sensors of the same physical quantity (such as multi-point temperature sensors), determine whether the deviation between each measurement value is within the allowable range. If the deviation is too large, remove outliers.

[0027] Finally, outlier removal can employ a strategy combining sliding window filtering and statistical thresholding. The controller maintains a fixed-length time window (e.g., the most recent 60 sampling points), calculates the moving average and standard deviation of the membrane thickness data within the window, and identifies outliers when the current membrane thickness data deviates from the average by more than three times the standard deviation, replacing it with a predicted value (e.g., linear interpolation or Kalman filter estimate). After this preprocessing, the valid membrane thickness data and corresponding timestamps are combined to form membrane thickness-time series mapping information, stored in the controller's memory as an array or linked list for subsequent steps.

[0028] In practical engineering implementation, the actual growth rate of the current coating is calculated as follows: The controller extracts the most recent valid data (such as film thickness data collected within the last 5 minutes) from the film thickness-time series mapping information, and uses linear regression or least squares method to fit the relationship between film thickness and time. Since film thickness and time have a linear relationship under ideal conditions during electroplating (according to Faraday's law of electrolysis), the slope of the fitted line is the actual growth rate of the current coating, expressed in μm / min. To improve computational stability and anti-interference capability, a recursive least squares method with a forgetting factor is used for online parameter estimation. The forgetting factor (e.g., 0.95 to 0.99) controls the weight of historical data, ensuring that the rate estimate can be both smoothed and timely in response to process changes.

[0029] Meanwhile, the preset theoretical growth rate is calculated in advance according to Faraday's law and stored in the controller parameter table. The formula for calculating the theoretical growth rate is: V theory =(η×M×i) / (n×F×ρ), where η is the current efficiency (empirical value, such as 0.90-0.98 for nickel plating), M is the molar mass of the metal, i is the cathode current density, n is the valence state of the metal ions, F is the Faraday constant (96485 C / mol), and ρ is the coating metal density. In actual operation, the theoretical growth rate will be updated in real time based on the current current density and temperature settings to reflect the dynamic changes in process parameters.

[0030] After obtaining the actual growth rate and the theoretical growth rate, the controller calculates the rate deviation: ΔV = V actual -V theory and the relative deviation rate δV=(V actual -V theory ) / V theory ×100%. The above rate deviation information includes the direction of the deviation (positive deviation indicates faster growth, negative deviation indicates slower growth) and the magnitude of the deviation, and is stored in the controller in a structured data format (containing fields such as deviation value, deviation rate, and timestamp).

[0031] In practical engineering implementation, the controller, based on the obtained information of the actual growth rate and rate deviation, combines the current electroplating time t... elapsed Total electroplating time T total Calculate the following three thickness-related quantities respectively: Firstly, the current theoretical cumulative thickness: D theory_total =V theory ×T total This refers to the target thickness that should be achieved by the end of electroplating under ideal growth rate (this value should be basically consistent with the preset target coating thickness value).

[0032] Secondly, the current actual cumulative projected thickness: D actual_projected =V actual ×t elapsed +V actual ×(T total -t elapsed )=V actual ×T total This refers to the final thickness at the end of the electroplating process, assuming the actual growth rate remains constant.

[0033] Third, the thickness difference ΔD=D actual_projected -D target =(V actual -V theory )×T total This refers to the difference between the final thickness and the target thickness.

[0034] Simultaneously, the controller also calculates the deviation rate of the aforementioned thickness difference relative to the target thickness: δD=ΔD / D target ×100%.

[0035] In actual electroplating control, this step is not calculated only once, but is continuously updated in each control cycle (e.g., every 10 seconds or every 30 seconds). In each cycle, the controller calculates the projected thickness difference from the current moment to the end of electroplating based on the most recent actual growth rate, continuously approaching the final state, and providing a basis for subsequent parameter adjustments. The generated thickness difference information is stored numerically in the controller's shared data area, and step S14 integrates it with the rate deviation information.

[0036] In practical engineering implementation, this step is essentially a data fusion and structured storage process. The controller timestamps the rate deviation information (including actual rate value, theoretical rate value, absolute deviation, relative deviation rate, and timestamp) and the thickness difference information (including final projected thickness, thickness difference amount, thickness deviation rate, and timestamp).

[0037] S02. Based on the current coating growth state parameters and process deviation information, perform first-level parameter correction processing on the electroplating current density and electroplating temperature to obtain the first-level correction parameters. Specifically, this includes the following steps: S21. Based on the current coating growth state parameters and the rate deviation information in the process deviation information, perform the first-level correction calculation on the current density to generate the current density correction value. S22. Based on the thickness difference information in the current coating growth state parameters and process deviation information, perform the first-level correction calculation on the electroplating temperature to generate the electroplating temperature correction value. S23. Verify the coupling effect of the current density correction value and the electroplating temperature correction value, and determine whether the corrected current density and electroplating temperature meet the preset cooperative constraint conditions: When the co-constraint conditions are met, the current density correction value and the electroplating temperature correction value are registered as first-level correction parameters; When the cooperative constraint conditions are not met, the current density correction value and the electroplating temperature correction value are adjusted by compromise until the cooperative constraint conditions are met and then registered as the first-level correction parameter.

[0038] Specifically, for specific plating types (such as nickel plating, copper plating, chromium plating, etc.), orthogonal experiments or response surface methodology are used to obtain plating quality evaluation data (including plating crystal morphology, deposition rate, internal stress, and additive consumption rate, etc.) under different combinations of current density and temperature. The combination of (current density, temperature) points that meet the plating quality requirements is then fitted as the boundary of a continuous feasible region. This feasible region boundary can be expressed using a piecewise linear function or a quadratic curve equation. For example, for nickel plating, the current density (J, unit A / dm³) is... 2 The co-constraint between temperature (T, in °C) and the control system parameter J can be expressed as follows: when T∈[45,55], J≤6.5×ln(T-42); when T∈(55,65], J≤0.3×T+0.5, etc. This constraint is pre-stored in the parameter database of the control system for real-time verification.

[0039] Furthermore, when generating the current density correction value (J) corr ), and generate electroplating temperature correction value (T) corr After that, the system will (J) corr T corr The coordinate point is substituted into the collaborative constraint condition for judgment. If the coordinate point is located inside the feasible region or on its boundary, the collaborative constraint condition is satisfied, and both are directly registered as first-level correction parameters and output for execution. If the coordinate point falls outside the feasible region (i.e., beyond the collaborative constraint boundary), the compromise adjustment process is triggered.

[0040] Furthermore, (J) corr Tcorr The parameters are adjusted along a specific path to the boundary of the cooperative feasible region or within the boundary. The steps are as follows: First, calculate the deviation priority of the current density correction value and the temperature correction value relative to their initial correction requirements. That is, assess the impact of not correcting the current density or not correcting the temperature on the coating quality; parameters with a greater impact receive higher adjustment weights. Then, (J...) corr T corr The projection is directed onto the feasible region boundary, with the projection direction determined inversely proportional to the adjustment weights. This means parameters with larger weights change less during the compromise process, while parameters with smaller weights bear a greater share of the compromise. For example, if the thickness difference information indicates a severely insufficient coating thickness, then current density correction is more necessary, and J should be prioritized during the compromise. corr It is close to its original calculated value, while for T corr A significant pullback will occur until (J) corr' T corr' (J) falls into the feasible region. The compromised (J) corr' T corr' After the system verifies and confirms that the collaborative constraint conditions are met, it is registered as the final first-level correction parameter.

[0041] S03. Control the electroplating process according to the first-level correction parameters and simultaneously monitor the film thickness change rate. When the film thickness change rate deviates from the preset rate threshold, trigger the second-level parameter correction to obtain the second-level correction parameters. Specifically, this includes the following steps: S31. Control output is executed on the electroplating power supply and heating device according to the first-level correction parameters, so that the electroplating process operates at the corrected current density and electroplating temperature. S32. During the operation of the first-level correction parameters, continuously monitor the film thickness change rate and record the rate-time change curve; S33. When the film thickness change rate in the rate-time change curve exceeds the preset rate threshold range, the second-level parameter correction is triggered. S34. In the second-level parameter correction, the electroplating pH value and additive supply rate are corrected according to the direction and magnitude of the deviation between the film thickness change rate and the preset rate threshold, and the second-level correction parameters are generated.

[0042] Specifically, step S31 relies on the communication interface between the electroplating control system and the power supply and heating modules. Correction parameters are sent to the rectifier (for current density adjustment) and the temperature controller (for temperature adjustment) in the form of analog or digital commands to ensure that the actual operating parameters of the electroplating tank are consistent with the correction target. Step S32 relies on the high-frequency sampling capability of the thickness sensor. The sampling interval is typically set to milliseconds or seconds. After filtering, the sampled data updates the rate-time curve in real time. This curve serves as the basis for determining whether secondary correction is triggered and is also used for subsequent analysis of the trend characteristics of rate changes. The preset rate threshold range in step S33 is not fixed but is set differently based on the current plating type (e.g., protective zinc plating, decorative copper-nickel-chromium plating, or functional hard chromium plating) and the plating solution system. When the rate values ​​of multiple consecutive sampling points on the curve exceed this threshold range, to avoid false triggering, a certain cumulative over-limit time (e.g., exceeding 5 seconds) is usually set before confirming the trigger. In step S34, the direction of deviation determines the polarity of the correction. If the rate is too low, the pH value needs to be increased to the optimal range and a brightener or leveling agent needs to be added appropriately to activate the deposition process. If the rate is too high, the pH value needs to be lowered and the additive supply needs to be reduced to prevent the coating from burning or coarsening. The deviation magnitude is converted into a specific pH adjustment amount and the speed increment of the additive metering pump through preset fuzzy control rules or PID control algorithms to achieve quantitative output.

[0043] S04. Based on the second-level correction parameters, continue the electroplating process and continuously collect film thickness distribution data in different areas of the workpiece surface. Perform uniformity analysis on the film thickness distribution data and generate area uniformity labels. Specifically, this includes the following steps: S41. Continue the electroplating process according to the second-level correction parameters, and collect film thickness distribution data of different areas on the workpiece surface through multi-point film thickness sensors during the electroplating process. S42. Perform region location registration processing on the film thickness distribution data, associate and map each film thickness measurement value with the corresponding workpiece surface region location, and generate a region-film thickness mapping table. S43. Based on the region-film thickness mapping table, calculate the deviation between the film thickness value of each region and the overall average film thickness value, and classify and mark each region according to the degree of deviation to generate region uniformity labels. The regional uniformity label includes uniform and qualified areas, thinner areas, and thicker areas.

[0044] Specifically, in actual electroplating tanks, the coating growth rate often varies significantly across different areas of the workpiece surface (such as the upper edge, lower edge, center area, and corner areas) due to factors such as edge effects of electric field distribution, differences in distance between the anode and cathode, and spatial unevenness of electrolyte convection intensity. To capture this spatial distribution information, this invention arranges multiple online film thickness sensors (such as X-ray fluorescence thickness probes or eddy current thickness probes) within the electroplating tank. These sensors are arranged in an array along the transverse and longitudinal directions of the workpiece surface, or, during the electroplating process, a sensor scanning mechanism performs multi-point cyclic detection of the workpiece surface along a preset trajectory. Each sensor is equipped with an independent position code, ensuring that each film thickness measurement value can be traced back to a unique physical area on the workpiece surface. During the electroplating process, each sensor synchronously triggers measurement at a preset sampling frequency, forming a multi-channel parallel acquisition of raw film thickness data stream. This data stream, indexed by timestamps and position codes, is transmitted in real-time to the data preprocessing module of the control system.

[0045] Furthermore, due to the geometric mapping relationship between the sensor installation location and the actual area of ​​the workpiece surface, the control system pre-stores a registration matrix between the sensor position code and the workpiece surface coordinates. When the film thickness measurement value arrives, the registration processing module, based on the sensor position code corresponding to the measurement value, looks up the corresponding workpiece surface coordinates from the registration matrix, thereby transforming the raw information such as the thickness measured by sensor A as X micrometers into spatial semantic information of a thickness of X micrometers at workpiece surface coordinates (X1, Y1). After completing the coordinate mapping of all measurement points, the system merges and organizes these discrete coordinate-film thickness data pairs to generate a region-film thickness mapping table. This mapping table is essentially a two-dimensional data matrix, with rows and columns corresponding to the horizontal and vertical partitions of the workpiece surface, respectively, and the matrix elements being the film thickness measurement values ​​corresponding to the partition locations. For areas not directly covered by the sensor, data completion can be achieved through interpolation algorithms (such as bilinear interpolation or Kriging interpolation) to obtain a complete film thickness distribution map of the entire workpiece surface.

[0046] Furthermore, deviation calculation and grading are the final steps in generating region uniformity labels. The system first calculates the average of all film thickness data in the region-film thickness mapping table to obtain the overall average film thickness value, which represents the overall level of the coating thickness on the workpiece surface at the current moment. Then, it iterates through each region in the mapping table, calculates the difference between the region's film thickness value and the overall average film thickness value, and divides this difference by the overall average film thickness value to obtain the relative deviation percentage. Based on the degree of deviation, the system marks each region according to preset grading thresholds: regions with relative deviations within the preset acceptable threshold range are marked as uniform and acceptable regions; regions with relative deviations below the lower threshold are marked as thin regions, indicating insufficient coating growth in that region; and regions with relative deviations above the upper threshold are marked as thick regions, indicating excessive coating growth in that region. These labels are presented on the control interface in the form of a visual heat map, and stored in the system memory in the form of structured data. They are directly used as input conditions for the third-level parameter correction in step S06. The concentrated location of the thinner areas indicates the areas where the stirring intensity and stirring direction need to be compensated, while the distribution characteristics of the thicker areas indicate the direction and magnitude of the workpiece suspension angle and suspension depth that need to be adjusted.

[0047] S05. Based on the regional uniformity label, perform third-level parameter correction processing on the electrolyte stirring parameters and workpiece suspension posture to obtain the third-level correction parameters. Specifically, this includes the following steps: S51. Based on the distribution locations of thinner and thicker regions in the regional uniformity label, identify the direction of uneven electrolyte stirring and the direction of workpiece suspension posture deviation. S52. Based on the direction of uneven electrolyte stirring, perform correction processing on the stirring intensity and stirring direction of the stirring device to generate stirring parameter correction values; S53. Based on the direction of the workpiece suspension posture deviation, perform correction processing on the workpiece suspension angle and suspension depth to generate suspension posture correction values. S54. Register the stirring parameter correction value and the suspension attitude correction value as the third-level correction parameters.

[0048] Specifically, the regional uniformity label includes information on the film thickness deviation classification of various regions on the workpiece surface (uniform and qualified regions, thinner regions, and thicker regions). Based on the spatial distribution of thinner and thicker regions on the workpiece surface, the system infers the physical causes of film thickness non-uniformity. Specifically, when thinner and thicker regions are linearly symmetrically distributed, it indicates insufficient or excessive electrolyte flow in a certain direction, resulting in a gradient difference in ion concentration along that direction, thus identifying the direction of uneven electrolyte agitation. When thinner regions are concentrated on the lower side of the workpiece or on the concealed surface facing away from the cathode, it indicates a poor workpiece suspension angle or inappropriate suspension depth, leading to uneven electric field distribution or ion shielding effects, thus identifying the direction of workpiece suspension posture deviation.

[0049] The system determines the degree to which the current stirring direction and intensity of the stirring device deviate from the ideal state. If the thinner region is located downstream of the stirring flow direction, it indicates that insufficient stirring intensity has led to a lag in ion replenishment. In this case, the system will increase the stirring intensity and adjust the stirring direction deflection as a correction. If the thicker region is concentrated on the stirring impact surface, it indicates that excessive stirring has led to increased local ion turbulence and an abnormally high deposition rate. In this case, the system will decrease the stirring intensity or adjust the stirring direction to disperse the impact as a correction. Finally, the system will output the corrected stirring parameters.

[0050] Furthermore, the system determines the degree to which the current suspension angle and suspension depth of the workpiece deviate from the ideal electric field distribution in the electroplating tank. If the thinner area is located at the bottom or back of the workpiece, the suspension tilt angle is increased or the suspension depth is adjusted accordingly to make the distance between each surface of the workpiece and the anode more balanced, improve the uniformity of the current density distribution, and finally output the suspension attitude correction value.

[0051] Furthermore, the above-mentioned stirring parameter correction values ​​and suspension attitude correction values ​​are merged to form a third-level correction parameter, which is used to drive the stirring actuator and the workpiece suspension actuator to implement linkage adjustment.

[0052] S06. Based on the relationship between the cumulative charge and the film thickness change rate during the electroplating process, calculate the instantaneous anode dissolution efficiency and generate the anode replenishment control signal and the anode-cathode distance compensation amount. Specifically, this includes the following steps: S61. Accumulate the amount of electricity applied during the electroplating process in real time, and calculate the theoretical dissolution mass of the anode based on the accumulated amount of electricity applied; S62. Calculate the actual deposited metal mass based on the film thickness change rate and the workpiece plating area, and divide the actual deposited metal mass by the theoretical dissolution mass to obtain the anode instantaneous dissolution efficiency. S63. When the instantaneous dissolution efficiency of the anode is lower than the preset efficiency threshold, an anode replenishment control signal is generated according to the efficiency difference. The anode replenishment control signal is used to trigger the anode replenishment actuator to replenish anode metal into the plating tank. S64. Based on the cumulative trigger frequency of the anode replenishment control signal and the anode dissolution history record, calculate the remaining effective volume of the anode and predict the remaining service life of the anode. When the remaining service life of the anode is lower than the preset service life threshold, generate the anode-cathode spacing compensation amount. The anode-cathode spacing compensation amount is used to drive the electromechanical actuator to adjust the anode suspension height to maintain the preset anode-cathode spacing.

[0053] Specifically, the system collects the instantaneous current value of the electroplating circuit in real time through the current sampling module of the DC power supply, and performs integration calculations over time to accumulate the total amount of electricity (unit: ampere-hours) from the start of electroplating to the current moment. Based on Faraday's first law, the theoretical dissolution mass of the anode is directly proportional to the cumulative amount of electricity.

[0054] Furthermore, the system continuously acquires the film thickness change rate (unit: μm / min) using an online film thickness monitoring device (such as an X-ray fluorescence thickness gauge), multiplies it by the workpiece plating area and the coating metal density, and then divides it by the electroplating time to calculate the actual mass of metal deposited on the cathode. Since some of the metal ions generated during anodic dissolution during electroplating are deposited on the cathode, while others may be lost due to side reactions (such as hydrogen evolution and oxidation), the actual deposited mass is usually less than the theoretical anodic dissolution mass. Dividing the actual deposited mass by the theoretical dissolution mass yields the instantaneous anodic dissolution efficiency (a ratio between 0 and 1). This ratio reflects the actual dissolution output capacity of the anode under the current conditions.

[0055] Secondly, the system compares the calculated instantaneous anode dissolution efficiency with a preset efficiency threshold (e.g., 0.85). When the efficiency is lower than the threshold, it indicates that the anode surface has experienced passivation, uneven dissolution, or a significant reduction in effective area. The system then generates an anode supplementation control signal according to the ratio of the efficiency difference. This control signal is a digital or analog command, transmitted to the anode supplementation actuator via an industrial bus (such as Modbus or Profibus).

[0056] Furthermore, the system continuously records the cumulative trigger frequency of the anode replenishment control signal and, combined with the initial mass of the anode, the mass of the anode replenished each time, and the anode dissolution history (including cumulative charge, dissolution efficiency change curves, etc.), establishes a mathematical model for the remaining effective volume of the anode. The specific calculation formula is: Remaining effective volume of the anode = Initial anode volume − Dissolved volume + Replenished volume − Insoluble residue volume. Based on this remaining volume and the current average dissolution rate, the remaining anode lifespan (in hours) can be predicted. When the predicted lifespan is lower than a preset lifespan threshold (e.g., remaining lifespan less than 2 hours), the system further generates an anode-cathode spacing compensation amount. This compensation amount is calculated based on the fact that a decrease in the remaining anode volume leads to a reduction in the anode plate size, resulting in an increase in the actual spacing between the anode and cathode. The system calculates the required downward adjustment displacement based on the geometric relationship (initial spacing − equivalent thickness change of remaining volume). This compensation amount is used to adjust the anode's suspension height in real time via an electromechanical actuator (such as a servo motor-driven lifting device), moving the anode downward to compensate for the increased spacing caused by consumption, ensuring that the anode-cathode spacing is always maintained within a preset optimal range (e.g., 10~20cm).

[0057] S07. Based on the first-level correction parameters, second-level correction parameters, third-level correction parameters, anode supplementary control signals, and anode-cathode spacing compensation, comprehensive electroplating control is performed, and a complete process control record is generated after electroplating is completed. Specifically, this includes the following steps: S71. Arrange the first-level correction parameters, second-level correction parameters, and third-level correction parameters according to the time sequence of correction triggering to form a correction parameter sequence, and embed the anode-cathode spacing compensation amount as a spatial reference adjustment amount at the end of the correction parameter sequence. S72. Based on the modified parameter sequence, perform integrated linkage control on electroplating current density, electroplating temperature, electroplating pH value, additive supply rate, stirring parameters, workpiece suspension posture and anode suspension height. S73. During the integrated linkage control process, continuously monitor the film thickness change trend and the regional uniformity change trend; S74. When the film thickness variation trend and the regional uniformity variation trend meet the preset convergence conditions, lock the current control parameters and maintain operation until the electroplating is completed. S75. The real-time process parameter sequence, online film thickness monitoring data sequence, various correction parameter sequences, anode supplement control signal sequence, anode-cathode spacing compensation amount sequence, and regional uniformity label sequence of this electroplating process are correlated and organized to form a process control record. S76. Perform data compression and index coding on the process control records to generate traceable process control record files; S77. Store the process control record file in the historical process database and associate it with the corresponding workpiece batch information and coating type information; S78. After electroplating is completed, a comprehensive evaluation of the plating thickness compliance status is conducted based on the process control records, and a plating quality evaluation report is generated. When the plating quality evaluation report shows that there are areas with substandard thickness, the location information and degree of substandard thickness of the areas are marked as re-plating requirement information and output to the re-plating process control terminal.

[0058] Specifically, the system arranges the previously generated first-level correction parameters (current density correction value, electroplating temperature correction value), second-level correction parameters (pH value correction value, additive supply rate correction value), and third-level correction parameters (stirring parameter correction value, suspension posture correction value) according to their respective triggering times, forming a sequence of correction parameters with temporal logic. This sequence reflects the correction logic of the electroplating process from overall to local, and from macroscopic to microscopic. Typically, the first-level correction is triggered first (based on initial deviation), the second-level correction is triggered during the first-level correction (based on rate deviation), and the third-level correction is triggered after the second-level correction stabilizes (based on regional non-uniformity). At the same time, the system embeds the anode-cathode spacing compensation amount as a spatial reference adjustment amount at the end of this sequence. This is because adjusting the anode-cathode spacing changes the electric field distribution and ion migration path of the entire electroplating tank. Once this adjustment is executed, it will serve as the physical spatial reference for all subsequent process parameters. Therefore, placing it at the end of the sequence ensures that it will not be interfered with by other parameter corrections after it takes effect.

[0059] The system implements integrated, coordinated control of multiple actuators in the electroplating equipment based on a pre-arranged sequence of corrected parameters. Specifically: the power supply unit adjusts the output current according to the current density correction value; the heating / cooling unit adjusts the bath temperature according to the temperature correction value; the chemical dosing unit performs quantitative addition of acid / alkali solutions and quantitative supply of brightener / leveling agent according to the pH correction value and additive supply rate correction value; the stirring unit adjusts the stirring motor speed and guide vane angle according to the stirring parameter correction value; the workpiece suspension actuator adjusts the tilt angle and lifting height of the suspension frame according to the suspension posture correction value; and the anode lifting actuator drives the lifting motor of the anode bracket according to the anode-cathode distance compensation to maintain the preset anode-cathode distance. The adjustment values ​​of each actuator are synchronously issued through a PLC (Programmable Logic Controller) or an industrial control computer, ensuring that multiple parameters change collaboratively under the same time reference, avoiding mismatch problems caused by the adjustment of a single parameter first and the lagging response of other parameters.

[0060] During the execution of integrated control, the system continuously collects film thickness data through online film thickness monitoring devices (X-ray fluorescence thickness gauges or eddy current thickness gauges) to generate film thickness variation trend curves. Simultaneously, it continuously collects film thickness distribution data for different regions of the workpiece surface through an array of multi-point film thickness sensors, generating regional uniformity variation trends. These two sets of trend data are updated in real-time in time series format, serving as a dynamic basis for determining whether the current control effect has achieved the expected goals.

[0061] The system performs real-time judgment on the film thickness variation trend and regional uniformity variation trend based on preset convergence conditions. The convergence conditions include two dimensions: first, the deviation of the film thickness variation rate from the theoretical target rate remains consistently within a preset tolerance range (e.g., within ±5%) for a duration reaching a set threshold (e.g., continuously for 30 seconds), indicating that the overall deposition rate has returned to the target range; second, the deviation of the film thickness value in each region from the overall average value remains consistently within a preset tolerance range (e.g., within ±8%) for a duration reaching a set threshold, indicating that spatial uniformity has been effectively improved. When both conditions are met simultaneously, the system determines that the current control parameter combination has reached an ideal state, then locks the current control parameters of all actuators, no longer responds to new correction trigger signals, and maintains the stable operation of this parameter combination until the electroplating process ends.

[0062] The system correlates and organizes all data sequences recorded throughout the electroplating process, including real-time process parameters at each time point (current density, temperature, pH value, additive supply rate, stirring parameters, workpiece suspension posture, anode suspension height), online film thickness monitoring data, trigger records of various correction parameters, trigger records of anode supplementation control signals, output records of anode-cathode spacing compensation, and regional uniformity label update records, forming a complete process control record. The system compresses this process control record to save storage space and generates an index code according to preset indexing rules (e.g., date-batch number-plating type-serial number format), giving the record a unique traceability identifier. The system stores the compressed and coded process control record file in the historical process database, simultaneously associating it with corresponding workpiece batch information (e.g., batch number, workpiece model) and plating type information (e.g., zinc plating, nickel plating, chromium plating, etc.) for subsequent conditional retrieval and historical data analysis. The system comprehensively evaluates the final coating thickness compliance of the electroplating process based on complete process control records. It compares the final film thickness data with the preset target coating thickness value region by region, generating a quality evaluation report that includes indicators such as overall pass rate, thickness distribution in each region, and maximum / minimum thickness values. If the report shows areas with substandard thickness, the system marks the location coordinates of that area and the degree of thickness deviation as re-plating requirement information. This information is then output to the control terminal of the re-plating process via a network communication interface or data exchange protocol, guiding the re-plating process to perform localized re-plating treatment on specific areas and preventing the entire workpiece from being scrapped.

[0063] The above description is merely a preferred embodiment of the present invention and is not intended to limit the present invention in any way. Although the present invention has been disclosed above with reference to preferred embodiments, it is not intended to limit the present invention. Any person skilled in the art can make some modifications or alterations to the above-disclosed technical content to create equivalent embodiments without departing from the scope of the present invention. Any simple modifications, equivalent changes and alterations made to the above embodiments based on the technical essence of the present invention without departing from the scope of the present invention shall still fall within the scope of the present invention.

Claims

1. A smart electroplating control method based on online film thickness monitoring, characterized in that: Includes the following steps: S01. Collect real-time process parameters during the electroplating process, combine them with the preset target value of coating thickness to perform initial state analysis, and obtain the current coating growth state parameters and process deviation information. S02. Based on the current coating growth state parameters and process deviation information, perform first-level parameter correction processing on the electroplating current density and electroplating temperature to obtain first-level correction parameters; S03. Control the electroplating process according to the first-level correction parameters and monitor the film thickness change rate simultaneously. When the film thickness change rate deviates from the preset rate threshold, trigger the second-level parameter correction to obtain the second-level correction parameters. S04. Based on the second-level correction parameters, continue to execute the electroplating process and continuously collect film thickness distribution data in different areas of the workpiece surface. Perform uniformity analysis on the film thickness distribution data and generate regional uniformity labels. S05. Based on the regional uniformity label, perform third-level parameter correction processing on the electrolyte stirring parameters and the workpiece suspension posture to obtain the third-level correction parameters. S06. Based on the relationship between the cumulative charge and the film thickness change rate during the electroplating process, calculate the instantaneous dissolution efficiency of the anode and generate the anode supplement control signal and the anode-cathode spacing compensation amount. S07. Perform comprehensive electroplating control based on the first-level correction parameters, the second-level correction parameters, the third-level correction parameters, the anode supplement control signal, and the anode-cathode spacing compensation amount, and generate a complete process control record after electroplating is completed.

2. The intelligent electroplating control method based on online film thickness monitoring according to claim 1, characterized in that: Step S01 specifically includes the following steps: S11. Collect real-time process parameters during the electroplating process, perform parameter validity identification and outlier removal processing on the real-time process parameters, extract online film thickness monitoring data and generate film thickness-time series mapping information; S12. Based on the film thickness-time series mapping information, calculate the current actual growth rate of the coating and compare it with the preset theoretical growth rate to generate rate deviation information. S13. Perform a difference analysis between the rate deviation information and the preset coating thickness target value to generate thickness difference information; S14. The rate deviation information and thickness difference information are associated and registered to form the current coating growth state parameters and process deviation information.

3. The intelligent electroplating control method based on online film thickness monitoring according to claim 2, characterized in that: In step S12: The actual growth rate of the current coating is calculated as follows: The controller extracts the most recent valid data from the film thickness-time series mapping information and uses linear regression or least squares method to fit the relationship between film thickness and time; since the film thickness and time are linearly related under ideal conditions during the electroplating process, the slope of the fitted line is the actual growth rate of the current coating. The preset formula for calculating the theoretical growth rate is: V theory =(η×M×i) / (n×F×ρ), where η is the current efficiency, M is the molar mass of the metal, i is the cathode current density, n is the valence state of the metal ion, F is the Faraday constant, and ρ is the coating metal density; After obtaining the actual growth rate and the theoretical growth rate, calculate the rate deviation: ΔV = V actual -V theory and the relative deviation rate δV=(V actual -V theory ) / V theory ×100%.

4. The intelligent electroplating control method based on online film thickness monitoring according to claim 1, characterized in that: Step S02 specifically includes the following steps: S21. Based on the rate deviation information in the current coating growth state parameters and process deviation information, perform first-level correction calculation on the current density to generate a current density correction value. S22. Based on the thickness difference information in the current coating growth state parameters and process deviation information, perform first-level correction calculation on the electroplating temperature to generate an electroplating temperature correction value. S23. Perform a coupling effect verification on the current density correction value and the electroplating temperature correction value, and determine whether the corrected current density and electroplating temperature meet the preset cooperative constraint conditions: When the co-constraint conditions are met, the current density correction value and the electroplating temperature correction value are registered as first-level correction parameters; When the cooperative constraint conditions are not met, the current density correction value and the electroplating temperature correction value are adjusted by compromise until the cooperative constraint conditions are met and then registered as the first-level correction parameter.

5. The intelligent electroplating control method based on online film thickness monitoring according to claim 1, characterized in that: Step S03 specifically includes the following steps: S31. Control output is executed on the electroplating power supply and heating device according to the first-level correction parameters, so that the electroplating process operates at the corrected current density and electroplating temperature. S32. During the operation of the first-level correction parameters, continuously monitor the film thickness change rate and record the rate-time change curve; S33. When the film thickness change rate in the rate-time change curve exceeds the preset rate threshold range, the second-level parameter correction is triggered. S34. In the second-level parameter correction, the electroplating pH value and additive supply rate are corrected according to the direction and magnitude of the deviation between the film thickness change rate and the preset rate threshold, and the second-level correction parameters are generated.

6. The intelligent electroplating control method based on online film thickness monitoring according to claim 1, characterized in that: Step S04 specifically includes the following steps: S41. Continue the electroplating process according to the second-level correction parameters, and collect film thickness distribution data of different areas on the workpiece surface through multi-point film thickness sensors during the electroplating process. S42. Perform region location registration processing on the film thickness distribution data, associate and map each film thickness measurement value with the corresponding workpiece surface region location, and generate a region-film thickness mapping table. S43. Based on the region-film thickness mapping table, calculate the deviation between the film thickness value of each region and the overall average film thickness value, and classify and mark each region according to the degree of deviation to generate a region uniformity label.

7. The intelligent electroplating control method based on online film thickness monitoring according to claim 6, characterized in that: The regional uniformity label includes uniform qualified areas, thinner areas, and thicker areas.

8. The intelligent electroplating control method based on online film thickness monitoring according to claim 7, characterized in that: Step S05 specifically includes the following steps: S51. Based on the distribution positions of the thinner and thicker regions in the regional uniformity label, identify the direction of uneven electrolyte stirring and the direction of workpiece suspension posture deviation. S52. Based on the direction of uneven stirring of the electrolyte, perform correction processing on the stirring intensity and stirring direction of the stirring device to generate stirring parameter correction values; S53. Based on the direction of the workpiece suspension posture deviation, perform correction processing on the workpiece suspension angle and suspension depth to generate suspension posture correction values. S54. Register the stirring parameter correction value and the suspension attitude correction value as third-level correction parameters.

9. The intelligent electroplating control method based on online film thickness monitoring according to claim 1, characterized in that: Step S06 specifically includes the following steps: S61. Accumulate the amount of electricity applied during the electroplating process in real time, and calculate the theoretical dissolution mass of the anode based on the accumulated amount of electricity applied; S62. Calculate the actual deposited metal mass based on the film thickness change rate and the workpiece plating area, and divide the actual deposited metal mass by the theoretical dissolution mass to obtain the anode instantaneous dissolution efficiency. S63. When the instantaneous dissolution efficiency of the anode is lower than a preset efficiency threshold, an anode replenishment control signal is generated according to the efficiency difference. The anode replenishment control signal is used to trigger the anode replenishment actuator to replenish anode metal into the plating tank. S64. Based on the cumulative trigger frequency of the anode replenishment control signal and the anode dissolution history record, calculate the remaining effective volume of the anode and predict the remaining service life of the anode. When the remaining service life of the anode is lower than the preset service life threshold, generate an anode-cathode spacing compensation amount. The anode-cathode spacing compensation amount is used to drive the electromechanical actuator to adjust the anode suspension height to maintain the preset anode-cathode spacing.

10. The intelligent electroplating control method based on online film thickness monitoring according to claim 1, characterized in that: Step S07 specifically includes the following steps: S71. The first-level correction parameter, the second-level correction parameter, and the third-level correction parameter are arranged according to the time order of correction triggering to form a correction parameter sequence, and the anode-cathode spacing compensation amount is embedded as a spatial reference adjustment amount at the end of the correction parameter sequence. S72. Based on the modified parameter sequence, perform integrated linkage control on electroplating current density, electroplating temperature, electroplating pH value, additive supply rate, stirring parameters, workpiece suspension posture and anode suspension height. S73. During the integrated linkage control process, continuously monitor the film thickness change trend and the regional uniformity change trend; S74. When the film thickness variation trend and the regional uniformity variation trend meet the preset convergence conditions, lock the current control parameters and maintain operation until the electroplating is completed. S75. The real-time process parameter sequence, online film thickness monitoring data sequence, various correction parameter sequences, anode supplement control signal sequence, anode-cathode spacing compensation amount sequence, and regional uniformity label sequence of this electroplating process are correlated and organized to form a process control record. S76. Perform data compression and index encoding processing on the process control records to generate traceable process control record files; S77. Store the process control record file in the historical process database and associate it with the corresponding workpiece batch information and coating type information; S78. After electroplating is completed, the coating thickness compliance of this electroplating is comprehensively evaluated according to the process control record, and a coating quality evaluation report is generated. When the coating quality evaluation report shows that there are areas where the thickness does not meet the standard, the location information and degree of non-compliance information of the areas where the thickness does not meet the standard are marked as re-plating requirement information and output to the re-plating process control terminal.