Preparation method of collagen solution suitable for coating
By preparing collagen solution and using crosslinking equipment to achieve stepwise crosslinking of collagen fibers and glutaraldehyde, the problems of non-degradability and harmfulness of existing coating materials are solved, the moisture-proof and oil-proof properties of paper are improved, and high-end green and environmentally friendly applications are realized.
Patent Information
- Application Number
- CN202611278205.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-21
- Publication Date
- 2026-11-17
AI Technical Summary
Existing coating materials for food packaging paper have problems such as being non-degradable, not heat-resistant, and harmful to the environment and human body, and cannot meet the needs of high-end application scenarios.
Using natural cowhide collagen fibers as raw materials, collagen solution is prepared through acidification pretreatment, gradient stirring and multiple homogenization, combined with a stepwise cross-linking process. The cross-linking equipment is used to achieve cross-linking of collagen fibers with glutaraldehyde, forming a dense network structure, replacing the traditional combination of conveyor belt and drying box.
The prepared collagen solution is biodegradable, improves the moisture and oil resistance of paper, has a compact structure, occupies little space, is easy to install, and has high bonding strength between the coating and the paper, with stable performance.
Smart Images

Figure CN123108985A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of biopolymer adhesive preparation technology, specifically to a method for preparing a collagen adhesive that can be used for coating. Background Technology
[0002] Paper, as a traditional packaging and printing substrate, has natural defects in hydrophilicity and oil permeability. Unmodified ordinary paper has poor moisture and oil resistance properties, which cannot meet the needs of high-end application scenarios such as food packaging, protection of precision devices, and waterproof and oil-proof printing. Therefore, chemical synthetic coatings and plastic films are usually used to improve paper properties.
[0003] For example, the internal coating of food packaging paper currently mainly uses food-grade polyethylene (PE), paraffin / beeswax coating or PFAS fluorine coating to improve the paper's wrapping properties, giving it water-resistant, moisture-resistant and oil-resistant properties.
[0004] However, existing coatings used for food packaging paper include: food-grade polyethylene, which is non-degradable and makes paper and plastic difficult to separate; paraffin / beeswax coatings, although they have good waterproof properties, are not heat-resistant and are prone to melting at high temperatures; and PFAS fluorine coatings, although they have good oil-resistant properties, pose potential hazards to humans, animals and the environment due to their chemical properties and are being phased out. Summary of the Invention
[0005] To address the shortcomings of existing technologies, this invention provides a method for preparing a collagen solution that can be used for coating, thus solving the problems raised in the background art.
[0006] To achieve the above objectives, the present invention provides a method for preparing a collagen solution suitable for coating, comprising the following steps: S1. Preparation of collagen fiber pulp: The cowhide is pickled with lime and acidified to obtain transparent acidified hide. The acidified hide is then processed by pelleting, rolling, crushing and homogenizing to obtain collagen fiber pulp with a water content of 95wt%. S2, Collagen Fiber Solution Preparation: Take the collagen fiber pulp from S1 to prepare a collagen fiber solution, wherein the collagen fiber solid content is controlled at 8wt%-15wt%, and the viscosity of the solution is controlled at 500-1000cP through the coordinated regulation of pH value, stirring and homogenization process. S3. Paper coating treatment: The adhesive solution prepared in S2 is applied to the paper using a coating device; S4. Crosslinking: Dry the coated paper, spray it with glutaraldehyde crosslinking solution, and dry it after spraying. Repeat the spraying and drying process after drying, and complete three glutaraldehyde crosslinking solution spraying and curing operations in total.
[0007] Furthermore, the preparation process of the adhesive solution in S2 is as follows: the adhesive solution is continuously stirred at high speed for 30 minutes, and the pH value of the adhesive solution is adjusted to 2.3-2.5 during the stirring process. After the stirring is completed, the adhesive solution is circulated and homogenized 10 times. The temperature is controlled at low temperature throughout the process, and the temperature of the adhesive solution system is controlled not to exceed 30°C to avoid the collagen fiber denaturation and gelation caused by excessive temperature.
[0008] Furthermore, in S4, sodium hydroxide solution is used as a pH adjuster to adjust the pH value of the glutaraldehyde solution to 9.0-10.0, and control the effective concentration of glutaraldehyde to 200-500 ppm.
[0009] Furthermore, the crosslinking process of the adhesive in S4 is completed using a crosslinking device, which includes: an outer cylinder; an inner cylinder located in the middle of the inner side of the outer cylinder, wherein a spiral traction track for pulling the paper is provided between the inner cylinder and the outer cylinder; a spraying structure, which has three sets and is located on the track path of the spiral traction track, for spraying the glutaraldehyde crosslinking solution onto the paper in three stages; the outer cylinder has an air inlet tangentially to the track direction of the spiral traction track, for guiding the drying airflow tangentially into the spiral traction track and flowing along the track path of the spiral traction track, so that the drying airflow flows parallel to the paper surface for drying.
[0010] Furthermore, the crosslinking device also includes: a turntable located on one side of the track path of the spiral traction track; a guide track disposed on the turntable, wherein a slide table is slidably disposed on the guide track, wherein the upper half of the slide table is provided with a clamping structure for clamping and pulling the paper, and the lower half of the slide table is provided with a second slide column; a spiral guide rail is provided on one side of the track path of the spiral traction track, wherein the second slide column is located inside the spiral guide rail, so that after the clamping structure clamps the paper, it drives the second slide column to slide along the spiral guide rail, thereby pulling the paper to be laid out along the track path of the spiral traction track.
[0011] Furthermore, the clamping structure includes: a first clamping plate fixedly connected to a slide table; a second clamping plate slidably disposed on the slide table directly above the first clamping plate, and a second spring guide rod provided within the slide table to drive the second clamping plate to move elastically, wherein at least one end of the second clamping plate is provided with a first sliding column; the spiral traction track is provided with at least one set of first inclined guide rails near its loading port, the first inclined guide rails being located on the moving path of the first sliding column, so that when the first sliding column passes the first inclined guide rail, it makes way and moves, driving the second clamping plate to open and close relative to the first clamping plate, forming a paper clamping channel; the spiral traction track is provided with at least one set of second inclined guide rails near its discharge port, the second inclined guide rails being located on the moving path of the first sliding column, so that when the first sliding column passes the second inclined guide rail, it makes way and moves, driving the second clamping plate to open and close relative to the first clamping plate, forming a paper discharge channel.
[0012] Furthermore, the spray structure includes: a wind hood, located on the track path of the spiral traction track, wherein the wind hood is provided with a diversion pipe and spray heads are arranged separately along its pipe direction; a first spring guide rod, located at at least one end of the wind hood, wherein a wedge-shaped guide rail is provided on one side of the first spring guide rod.
[0013] Furthermore, the wedge guide rail is located on the moving path of the first sliding column; when the clamping structure clamps the paper and passes through the spraying structure, the first sliding column drives the wedge guide rail to move aside, causing the spraying structure to make way for the clamping structure, so that the paper passes under the spray head for spraying.
[0014] Furthermore, the crosslinking device also includes: a reciprocating screw guide rail located on the axial path of the inner cylinder; a support frame disposed on the slide of the reciprocating screw guide rail, and a second motor disposed on the support frame, wherein the output shaft of the second motor is provided with a winding drum for winding paper, so that the reciprocating screw guide rail drives the winding drum to extend into the inner cylinder to perform the winding operation of the paper.
[0015] Furthermore, the support frame is provided with a plug, which is used to seal one end of the inner cylinder channel; the inner cylinder is provided with a discharge platform near the discharge port of the spiral traction track, which is used for paper discharge and drying airflow, and the other end of the inner cylinder channel is provided with an air outlet to guide the outflowing drying airflow.
[0016] The present invention has the following beneficial effects: (1) The preparation method of the collagen solution that can be used for coating uses natural bovine collagen as the core raw material, and undergoes acidification pretreatment, gradient stirring + multiple homogenization by colloid milling, and stepwise cross-linking process. The whole process is green and environmentally friendly, with no toxic or harmful substances remaining. The modified paper has biodegradable characteristics. Compared with traditional chemical coating and film-modified paper, it is more green and low-carbon, and suitable for high-end scenarios such as food packaging and environmental protection packaging.
[0017] (2) The preparation method of the collagen liquid that can be used for coating can form a dense three-dimensional network cross-linked structure of collagen molecules through a stepwise cross-linking process, which greatly improves the density of the collagen coating, strengthens the bonding strength between the coating and paper fibers, avoids coating peeling and blistering, significantly improves the core performance of paper in terms of moisture resistance and oil resistance, and has better performance stability and durability.
[0018] (3) The preparation method of the collagen solution that can be used for coating utilizes a cross-linking device as a cross-linking preparation carrier for collagen fiber solution and glutaraldehyde cross-linking solution. It replaces the traditional combination of conveyor belt + drying box which occupies a large area. Its overall structure is more compact and small, occupies less space, and is more convenient to install and use. At the same time, it is simpler and more efficient for paper traction and layout.
[0019] (4) The preparation method of the collagen solution that can be used for coating, by arranging a spiral traction track in the crosslinking equipment, can provide the track required for paper traction, so that the glutaraldehyde crosslinking solution can crosslink with the collagen fiber solution on the paper step by step. On the other hand, the spiral traction track can guide the drying airflow to flow horizontally, so that the drying airflow always tends to dry the adhesive solution parallel to the paper surface, so as to avoid the direct blowing of the coating causing erosion, film cracking and other situations.
[0020] Of course, any product implementing this invention does not necessarily need to achieve all of the advantages described above at the same time. Attached Figure Description
[0021] Figure 1 This is a schematic diagram of the process of the present invention; Figure 2 This is a first structural schematic diagram of the crosslinking device in this invention; Figure 3 This is a schematic diagram of the second structure of the crosslinking device in this invention; Figure 4 For the present invention Figure 3 Enlarged view of point A in the middle; Figure 5 This is a schematic diagram of the assembly of the spiral guide rail and the spray structure in the crosslinking equipment of the present invention; Figure 6 This is a diagram showing the crosslinking path of the collagen solution and the state changes of the drying path of the drying airflow in this invention. Figure 7 This is a first assembly diagram of the outer cylinder, inner cylinder, and spiral traction track in the crosslinking equipment of the present invention. Figure 8 This is a second assembly diagram of the outer cylinder, inner cylinder, and spiral traction track in the crosslinking equipment of the present invention; Figure 9 This is a schematic diagram of the winding structure of the cross-linked paper in this invention; Figure 10 This is a schematic diagram of the layout of the spray structure in the crosslinking equipment of the present invention; Figure 11 This is a first structural schematic diagram of the spray structure in the crosslinking device of the present invention; Figure 12 This is a second structural schematic diagram of the spray structure in the crosslinking device of the present invention; Figure 13 This is a schematic diagram of the assembly of the spiral traction track and two sets of inclined guide rails in the crosslinking device of the present invention; Figure 14 For the present invention Figure 13 Enlarged view of point B in the middle; Figure 15 For the present invention Figure 13 Enlarged view of point C in the middle; Figure 16This is an assembly diagram of the clamping structure in the crosslinking device of the present invention; Figure 17 This is a first assembly enlarged view of the clamping structure in the crosslinking device of the present invention; Figure 18 This is a second enlarged assembly view of the clamping structure in the crosslinking device of the present invention; Figure 19 This is a third enlarged assembly view of the clamping structure in the crosslinking device of the present invention; Figure 20 (a) and (b) in the figure are, respectively, diagrams showing the opening and closing states of the clamping structure in the crosslinking device of the present invention.
[0022] In the diagram, 1 is the outer cylinder; 110 is the feeding platform; 120 is the air inlet; 2 is the inner cylinder; 210 is the discharging platform; 220 is the air outlet; 3 is the turntable; 4 is the transmission belt; 5 is the first motor; 6 is the reciprocating screw guide rail; 7 is the support frame; 8 is the second motor; 810 is the winding drum; 9 is the guide rail; 10 is the slide table; 1010 is the second sliding column; 11 is the first clamping plate; 12 is the second clamping plate; 13 is the first sliding column; 14 is the first inclined guide rail; 15 is the spiral traction rail; 1510 is the spiral guide rail; 16 is the spray structure; 1610 is the fan hood; 1620 is the first spring guide rod; 1630 is the wedge guide rail; 1640 is the liquid supply pipeline; 1650 is the liquid supply hose; 1660 is the diverter pipe; 1670 is the spray head; 17 is the second inclined guide rail; 18 is the second spring guide rod. Detailed Implementation
[0023] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0024] In the description of this invention, it should be understood that the terms "opening", "upper", "lower", "thickness", "top", "middle", "length", "inner", "around", etc., which indicate orientation or positional relationship, are only for the convenience of describing this invention and simplifying the description, and do not indicate or imply that the components or elements referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as limiting this invention.
[0025] The following is based on Figures 1-20 This invention describes a method for preparing a coating-compatible collagen solution according to embodiments of the present invention.
[0026] like Figure 1 As shown, a method for preparing a collagen solution suitable for coating includes the following steps: S1. Preparation of collagen fiber pulp: The cowhide is pickled with lime and acidified to obtain transparent acidified hide. The acidified hide is then processed by pelleting, rolling, crushing and homogenizing to obtain collagen fiber pulp with a water content of 95wt%, ensuring the initial dispersion of the fibers and providing basic raw materials for the subsequent preparation of the glue solution. S2, Collagen Fiber Solution Preparation: Take the collagen fiber slurry from S1 to prepare a collagen fiber solution. Deionized water can be used to prepare the collagen fiber coating solution. The solid content of collagen fibers is controlled at 8wt%-15wt%. The viscosity of the solution is controlled at 500-1000cP through the coordinated regulation of pH value, stirring and homogenization processes to ensure that the collagen fibers are uniformly dispersed in the solution without agglomeration or precipitation. S3. Paper coating treatment: The adhesive solution prepared in S2 is applied to the paper using a coating device to form a uniform, continuous and complete collagen pre-coating layer, wherein 1-2 grams of collagen substance are applied to each square meter of paper. S4. Crosslinking: After the coated paper is dried, it is sprayed with glutaraldehyde crosslinking solution. After spraying, it is dried. After drying, the spraying and drying process is repeated. A total of three glutaraldehyde crosslinking solution spraying and curing operations are completed. Through multiple step-by-step crosslinking, the collagen molecules can fully undergo crosslinking reaction to build a dense and stable collagen coating structure, strengthen the bonding force between the coating and the paper substrate, and ensure the long-term moisture-proof and oil-proof performance of the modified paper.
[0027] As a further embodiment of this method, the preparation process of the adhesive solution in S2 is as follows: the adhesive solution is continuously stirred at high speed for 30 minutes, and the pH value of the adhesive solution is adjusted to 2.3-2.5 during the stirring process. After stirring, the adhesive solution is subjected to 10 cycles of homogenization treatment, and the temperature of the adhesive solution system is controlled at low temperature throughout the process, ensuring that the temperature of the adhesive solution system does not exceed 30°C. The specific process is as follows: the collagen fiber slurry is put into the stirring reaction equipment, and the high-speed stirring mode is turned on. During the stirring process, the pH value of the adhesive solution can be adjusted to 2.3-2.5 by means of a food-grade acid regulator. The acidic environment is used to destroy the aggregation force between collagen fiber molecules and promote the full dispersion of fibers. After continuous high-speed stirring for 30 minutes, the mixed adhesive solution is transferred to a colloid mill for cyclic homogenization treatment. The homogenization cycle is 10 times, and the temperature of the adhesive solution system is controlled at low temperature throughout the process, ensuring that the temperature of the adhesive solution system does not exceed 30°C. This avoids the denaturation of collagen, loss of adhesive solution viscosity, and damage to fiber structure caused by high temperature, and finally obtains a collagen adhesive solution with uniform dispersion, stable viscosity, and suitable for coating process.
[0028] Furthermore, in S4, sodium hydroxide solution is used as a pH adjuster to adjust the pH of the glutaraldehyde solution to 9.0-10.0. On the one hand, this activates the amino group activity (collagen amino groups are easily protonated in acidic environments and lose their reactivity; in a weakly alkaline environment of pH 9-10, the amino group is in a free -NH2 state, maximizing its reactivity with the aldehyde group, and the crosslinking efficiency is much higher than under acidic conditions). On the other hand, it promotes the crosslinking polymerization of glutaraldehyde (alkaline environments accelerate the self-polymerization of glutaraldehyde, forming longer polyaldehyde chains, longer crosslinking bridges, higher crosslinking density of the collagen network, and denser film formation). At the same time, the effective concentration of glutaraldehyde is controlled at 200-500 ppm to ensure crosslinking uniformity and compatibility.
[0029] In addition to the above, such as Figures 2-19 , Figure 20 As shown in the state change diagrams (a) and (b) in section S4, the cross-linking process of the adhesive solution is completed using a cross-linking device. This device achieves the cross-linking polymerization of the adhesive solution and glutaraldehyde on the paper. On the one hand, it features a compact and small structure, requiring less space and being more convenient to install and use. On the other hand, it also has a highly efficient cross-linking effect, enabling multiple spraying and drying processes of the adhesive solution and glutaraldehyde in a continuous manner. Specifically: like Figure 2 , Figures 5-8 As shown, the crosslinking equipment includes an outer cylinder 1, an inner cylinder 2 located in the middle of the inner side of the outer cylinder 1, and a spiral traction track 15 for pulling paper between the inner cylinder 2 and the outer cylinder 1. A feeding platform 110 is located on the outer cylinder 1 near the inlet of the spiral traction track 15, and a discharge platform 210 is located on the inner cylinder 2 near the outlet of the spiral traction track 15. Simultaneously, three sets of spray structures 16 for spraying glutaraldehyde solution are also provided along the track path of the spiral traction track 15. After the collagen solution on the paper is dried, the paper is introduced into the spiral traction track 15 through the feeding platform 110. Utilizing the spiral guiding characteristics of the spiral traction track 15, the paper is pulled and conveyed in a "revolving" winding state, passing through the three sets of spray structures 16 to be sprayed with glutaraldehyde solution, allowing the glutaraldehyde solution and collagen solution to crosslink in steps. After the crosslinking reaction is completed and the paper slides out of the spiral traction track 15, the discharge platform 210 winds up the crosslinked paper. The structure is compact, occupies a small area, and the crosslinking reaction is more continuous.
[0030] In this embodiment, the outer cylinder 1 has an air inlet 120 on the track direction of the tangential spiral traction track 15, which guides the drying airflow tangentially into the spiral traction track 15 and along the track path of the spiral traction track 15, so that the drying airflow flows parallel to the paper surface for drying. At the same time, the inner cylinder 2 has an air outlet 220 at one end of the channel, which guides the outflowing drying airflow. During the stepwise crosslinking reaction of glutaraldehyde solution and collagen solution, a constant temperature drying oven can be used to dry the paper at a constant temperature (preferably 45-50°C). The air is blown into the outer cylinder 1 through the air inlet 120, and guided by the spiral traction track 15, the drying airflow tends to flow parallel to the paper surface, achieving a "parallel flow" drying state. This process dries the glutaraldehyde solution sprayed in three stages sequentially, resulting in a more continuous drying state with less interference from external environmental factors. Furthermore, the drying flow direction is stable and orderly, effectively reducing erosion and film cracking caused by direct blowing of the coating. The dried airflow is discharged into the inner cylinder 2 through the discharge platform 210 and then orderly guided out through the air outlet 220.
[0031] It should be noted that the spiral traction track 15 can be set to a spiral state corresponding to the track length by controlling the number of spiral turns, so as to adapt to the stepwise cross-linking reaction of collagen solution and glutaraldehyde solution on paper (paper is generally in roll form, its length is usually several kilometers or more, and it can be produced continuously by connecting the ends).
[0032] And, as Figure 3 , Figure 9 As shown, the crosslinking equipment also includes a reciprocating screw guide 6 located on the axial path of the inner cylinder 2, and a support frame 7 is installed on the slide of the reciprocating screw guide 6. The support frame 7 is equipped with a second motor 8, and the output shaft of the second motor 8 is equipped with a winding drum 810 for winding paper. The support frame 7 is also equipped with a plug 710 sleeved on the outside of the winding drum 810. When winding the crosslinked paper, the reciprocating screw guide 6 pushes the winding drum 810 into the inner cylinder 2, so that the winding drum 810 is facing the discharge platform 210 to perform the winding work on the paper. At the same time, the plug 710 seals the end away from the air outlet 220 to guide the dried airflow to be discharged in an orderly manner along the air outlet 220.
[0033] like Figures 3-4 , Figures 13-19 , Figure 20As shown in the state change diagrams (a) and (b), to guide the paper along the spiral traction track 15, the crosslinking device also includes a turntable 3 located on one side of the track path of the spiral traction track 15. The turntable 3 is rotatably mounted on the inner cylinder 2, and a guide track 9 is provided on the turntable 3. A slide table 10 is slidably provided on the guide track 9. The upper half of the slide table 10 is provided with a clamping structure for clamping and pulling the paper, and the lower half of the slide table 10 is provided with a second slide column 1010. At the same time, a spiral guide rail 1510 is provided on one side of the track path of the spiral traction track 15, and the second slide column 1010 is located inside the spiral guide rail 1510. Furthermore, the bottom of the outer cylinder 1 is equipped with a first motor 5, and a transmission belt 4 connects the first motor 5 and the turntable 3. After the paper on the feeding platform 110 is clamped by the clamping structure, the combination of the first motor 5 and the transmission belt 4 drives the turntable 3 to rotate, guiding the second sliding column 1010 to slide along the spiral guide rail 1510. Then, under the sliding support of the guide rail 9 and the slide table 10, the clamping structure moves "round by round" along the track path of the spiral traction rail 15, winding the paper sequentially onto the spiral traction rail 15, and finally pulling it to the discharge platform 210 for winding. Specifically: The clamping structure includes a first clamping plate 11 fixed to a slide table 10. A second clamping plate 12 is slidably disposed on the slide table 10 above the first clamping plate 11. A second spring guide rod 18 is disposed within the slide table 10 to drive the second clamping plate 12 to slide elastically. At least one end of the second clamping plate 12 is provided with a first sliding post 13. In the initial state, the clamping structure moves along the spiral traction track 15 towards the feeding platform 110. Driven by the force of the first sliding post 13, the clamping structure opens, allowing the paper to pass through the clamping structure. After the paper feeding is completed, during the initial movement of the clamping structure towards the spiral traction track 15, the clamping structure is controlled to clamp the paper and maintain this state, pulling the paper along the spiral traction track 15 to the discharge platform 210. When approaching the discharge platform 210, driven again by the force of the first sliding post 13, the clamping structure opens again and remains open, serving as a guide to guide the paper to be wound onto the take-up drum 810. ① At least one set of first inclined guide rails 14 are provided near the feeding platform 110 on the spiral traction track 15. The first inclined guide rails 14 are located on the moving path of the first sliding column 13. During the process of the clamping structure moving along the spiral traction track 15 and approaching the feeding platform 110, the first sliding column 13 is driven to pass through the first inclined guide rails 14. The first sliding column 13 makes relative clearance movement, which drives the second clamping plate 12 to open and close relative to the first clamping plate 11, forming a paper clamping channel. At this time, the paper is conveyed into the spiral traction track 15 along the clamping channel. Sufficient length (the conveying length is greater than the track length of the first inclined guide rail 14 so that the paper is self-clamped when the clamping structure moves in the reverse direction to close), and then the clamping structure is controlled to move in the reverse direction, so that the first sliding column 13 slides down from the first inclined guide rail 14, and under the elastic drive of the second spring guide rod 18, the second clamping plate 12 is driven to move towards the first clamping plate 11 to clamp and fix the paper, so that the clamping structure drives the paper to be synchronously pulled and laid along the spiral traction track 15 during the movement of the clamping structure along the track path of the spiral traction track 15.
[0034] ② The spiral traction track 15 is provided with at least one set of second inclined guide rails 17 near the discharge platform 210. The second inclined guide rails 17 are located on the moving path of the first sliding column 13. During the process of the clamping structure driving the paper to move along the spiral traction track 15 and approach the discharge platform 210, the first sliding column 13 is driven to pass through the second inclined guide rails 17 again, and the second clamping plate 12 is driven to open and close again relative to the first clamping plate 11 to form a paper discharge channel, guiding the paper to the winding drum 810 for winding.
[0035] like Figure 3 , Figures 10-12 As shown, Figure 20As shown in diagram (b) of the diagram, to guide the paper from below the spray structure 16, glutaraldehyde solution is sprayed onto the collagen solution of the paper. The spray structure 16 includes a hood 1610 located on the track path of the spiral traction track 15. The hood 1610 is used to block the influence of the drying airflow on the spraying state of the glutaraldehyde solution, and there is a channel between the hood 1610 and the track of the spiral traction track 15 to provide paper traction and transportation. The hood 1610 is provided with a diversion pipe 1660, and spray heads 1670 are arranged separately along its pipe direction. At the same time, the hood 1610 is also provided with a first spring guide rod 1620 installed on the spiral traction track 15 at both ends. A wedge-shaped guide rail 1630 is provided on one side of a spring guide rod 1620, and the wedge-shaped guide rail 1630 is located on the moving path of the first sliding column 13. During the process of the clamping structure driving the paper to move along the spiral traction track 15, when the clamping structure passes close to the spray structure 16, the first sliding column 13 pushes the wedge-shaped guide rail 1630 to move aside. Then, under the elastic support of the first spring guide rod 1620, the wind cover 1610 is pushed to move synchronously. On the one hand, it makes way for the clamping structure to avoid interference. On the other hand, it allows the paper to be pulled and laid out from under the spray head 1670 to prepare for spraying. Then, in this manner, the clamping structure drives the paper to be pulled out from under the three sets of spray structures 16 in sequence.
[0036] Furthermore, one end of the diversion pipe 1660 is connected to a liquid supply hose 1650, and the other end of the liquid supply hose 1650 is connected to a liquid supply line 1640. The liquid supply line 1640 is connected to a glutaraldehyde solution storage device. The glutaraldehyde solution can be pumped through the combination of the liquid supply line 1640 and the liquid supply hose 1650 into the diversion pipe 1660, and then sprayed out through the spray head 1670. The glutaraldehyde solution is sprayed onto the collagen solution of the paper in three stages, so that the two undergo a cross-linking reaction in a stepwise manner.
[0037] During use (working), the paper coated with collagen solution and dried is pulled and transported along the feeding platform 110 to the spiral traction track 15 by the clamping and traction action of the clamping structure. During the transport process, the paper is guided to pass through three sets of spray structures 16 in sequence, and finally the paper is pulled out through the discharge platform 210 and guided to the winding drum 810 for winding. In this process, glutaraldehyde solution is sprayed onto the collagen solution of the paper in three separate spraying stages using three sets of spraying structures 16. Simultaneously, the "adaptive" drying characteristics of the drying airflow along the spiral traction track 15 are utilized to dry the glutaraldehyde solution sprayed in three stages in sequence. As the paper is transported along the spiral traction track 15, the glutaraldehyde solution and collagen solution are repeatedly sprayed and dried, allowing the paper to complete the step-by-step cross-linking process within the spiral traction track 15. On the one hand, this replaces the traditional large-area combination of conveyor belt and drying box, resulting in a more compact and smaller overall structure with less space required and greater ease of use. On the other hand, its step-by-step cross-linking process is more coherent and complete, significantly improving the density and bonding strength of the collagen coating, as well as the paper's core moisture-proof and oil-proof properties.
[0038] It should be noted that, in this document, relational terms such as "first" and "second" are used only to distinguish one entity or operation from another, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Furthermore, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such process, method, article, or apparatus.
[0039] The preferred embodiments of the present invention disclosed above are merely illustrative of the invention. These preferred embodiments do not exhaustively describe all details, nor do they limit the invention to the specific implementations described. Clearly, many modifications and variations can be made based on the content of this specification. This specification selects and specifically describes these embodiments to better explain the principles and practical applications of the invention, thereby enabling those skilled in the art to better understand and utilize the invention. The invention is limited only by the claims and their full scope and equivalents.
Claims
1. A method for preparing a collagen solution suitable for coating, characterized in that, Includes the following steps: S1. Preparation of collagen fiber pulp: The cowhide is pickled with lime and acidified to obtain transparent acidified hide. The acidified hide is then processed by pelleting, rolling, crushing and homogenizing to obtain collagen fiber pulp with a water content of 95wt%. S2, Collagen Fiber Solution Preparation: Take the collagen fiber pulp from S1 to prepare a collagen fiber solution, wherein the collagen fiber solid content is controlled at 8wt%-15wt%, and the viscosity of the solution is controlled at 500-1000cP through the coordinated regulation of pH value, stirring and homogenization process. S3. Paper coating treatment: The adhesive solution prepared in S2 is applied to the paper using a coating device; S4. Crosslinking: Dry the coated paper, spray it with glutaraldehyde crosslinking solution, and dry it after spraying. Repeat the spraying and drying process after drying, and complete three glutaraldehyde crosslinking solution spraying and curing operations in total.
2. The method for preparing the collagen solution suitable for coating according to claim 1, characterized in that, The preparation process of the adhesive solution in S2 is as follows: continuously stir the adhesive solution at high speed for 30 minutes, adjust the pH value of the adhesive solution to 2.3-2.5 during the stirring process, and after the stirring is completed, the adhesive solution is circulated and homogenized 10 times; and the temperature is controlled at low temperature throughout the process, controlling the temperature of the adhesive solution system to not exceed 30℃, so as to avoid the denaturation and gelation of collagen fibers due to excessive temperature.
3. The method for preparing the collagen solution suitable for coating according to claim 1, characterized in that, In S4, sodium hydroxide solution is used as a pH adjuster to adjust the pH value of the glutaraldehyde solution to 9.0-10.0, and control the effective concentration of glutaraldehyde to 200-500 ppm.
4. The method for preparing a coating-compatible collagen solution according to any one of claims 1-3, characterized in that... The crosslinking process of the adhesive in S4 is completed using crosslinking equipment, which includes: outer cylinder (1); The inner cylinder (2) is located in the middle of the inner side of the outer cylinder (1), wherein a spiral traction track (15) for pulling paper is provided between the inner cylinder (2) and the outer cylinder (1). The spray structure (16) has three sets and is located on the track path of the spiral traction track (15) for spraying the glutaraldehyde crosslinking solution onto the paper in three stages. The outer cylinder (1) has an air inlet (120) in the track direction of the tangential spiral traction track (15) to guide the drying airflow tangentially into the spiral traction track (15) and flow along the track path of the spiral traction track (15), so that the drying airflow flows parallel to the paper surface for drying.
5. The method for preparing the collagen solution suitable for coating according to claim 4, characterized in that, The crosslinking device further includes: Turntable (3) is located on one side of the track path of the helical traction rail (15); A guide rail (9) is provided on a turntable (3). A slide table (10) is slidably provided on the guide rail (9). The upper half of the slide table (10) is provided with a clamping structure for holding and pulling the paper, and the lower half of the slide table (10) is provided with a second slide column (1010). The spiral traction track (15) has a spiral guide rail (1510) on one side of the track path. The second slide column (1010) is located inside the spiral guide rail (1510). After the clamping structure clamps the paper, it drives the second slide column (1010) to slide along the spiral guide rail (1510) and pulls the paper to be laid along the track path of the spiral traction track (15).
6. The method for preparing the collagen solution suitable for coating according to claim 5, characterized in that, The clamping structure includes: The first clamping plate (11) is fixedly connected to the slide table (10); The second clamping plate (12) is slidably disposed on the slide table (10) directly above the first clamping plate (11), and a second spring guide rod (18) is provided in the slide table (10) to drive the second clamping plate (12) to move elastically. The second clamping plate (12) is provided with a first sliding column (13) at least one end. The spiral traction track (15) is provided with at least one set of first inclined guide rails (14) near its loading port. The first inclined guide rails (14) are located on the moving path of the first sliding column (13), so that the first sliding column (13) moves to make way when it passes the first inclined guide rails (14), thereby driving the second clamping plate (12) to open and close relative to the first clamping plate (11) to form a paper clamping channel. The spiral traction track (15) is provided with at least one set of second inclined guide rails (17) near its discharge port. The second inclined guide rails (17) are located on the moving path of the first sliding column (13), so that the first sliding column (13) moves to make way when it passes the second inclined guide rails (17), thereby driving the second clamping plate (12) to open and close relative to the first clamping plate (11) to form a paper discharge channel.
7. The method for preparing the collagen solution suitable for coating according to claim 6, characterized in that, The spray structure (16) includes: The wind hood (1610) is located on the track path of the spiral traction track (15). The wind hood (1610) is equipped with a diversion pipe (1660) and spray heads (1670) are arranged separately along its pipe direction. The first spring guide rod (1620) is located at at least one end of the wind cover (1610), wherein a wedge-shaped guide rail (1630) is provided on one side of the first spring guide rod (1620).
8. The method for preparing the collagen solution suitable for coating according to claim 7, characterized in that, The wedge guide rail (1630) is located on the moving path of the first sliding column (13); When the paper passes through the spray structure (16) after being clamped by the clamping structure, the first sliding column (13) drives the wedge guide rail (1630) to move aside, causing the spray structure (16) to make way for the clamping structure, so that the paper passes under the spray head (1670) for spraying.
9. The method for preparing a coating-compatible collagen solution according to claim 6, characterized in that, The crosslinking device further includes: The reciprocating lead screw guide (6) is located on the axial path of the inner cylinder (2); A support frame (7) is provided on the slide of the reciprocating screw guide (6), and a second motor (8) is provided on the support frame (7). The output shaft of the second motor (8) is provided with a winding drum (810) for winding paper, so that the reciprocating screw guide (6) drives the winding drum (810) to extend into the inner cylinder (2) to perform the winding operation of paper.
10. The method for preparing the collagen solution suitable for coating according to claim 9, characterized in that, The support frame (7) is provided with a plug (710), which is used to seal one end of the inner cylinder (2) channel; The inner cylinder (2) is provided with a discharge platform (210) near the discharge port of the spiral traction track (15). The discharge platform (210) is used for paper discharge and drying airflow. The other end of the inner cylinder (2) channel is provided with an air outlet (220) to guide the outflowing drying airflow.