A modular repair system and method for precast concrete box culverts in frigid regions
By using a modular repair system and low-temperature curing technology, the seasonal limitations and long construction periods of precast concrete box culvert repair in frigid regions have been resolved, enabling rapid and reliable box culvert repair, improving connection strength and monitoring capabilities, and reducing construction costs and social impact.
Patent Information
- Application Number
- CN202611287776.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-24
- Publication Date
- 2026-11-17
AI Technical Summary
Existing technologies for the maintenance of precast concrete box culverts in frigid regions suffer from seasonal limitations, long construction periods, unstable quality, and an inability to meet the demands for rapid repair. In particular, effective connection and monitoring are difficult to achieve during construction in low-temperature environments.
The modular repair system includes standardized repair units, dedicated positioning frames, low-temperature curing connection components, and temporary support and protection components. Through factory-prefabricated standardized components, low-temperature curing materials, and real-time monitoring technology, combined with precise alignment and thermal insulation, a fast and reliable repair process is achieved.
Achieving rapid and reliable box culvert repair in frigid environments shortens the construction period, reduces traffic disruption, improves connection strength and monitoring capabilities, extends structural lifespan, and reduces costs.
Smart Images

Figure CN123109078A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of municipal and transportation infrastructure operation and maintenance technology, specifically relating to a modular repair system and method for precast concrete box culverts in extremely cold regions. Background Technology
[0002] Precast concrete box culverts in frigid regions serve as core infrastructure for municipal drainage and transportation, operating under harsh conditions of low temperatures and frequent freeze-thaw cycles. This makes them prone to localized defects such as corner cracking, sidewall damage, and joint leakage. These defects often worsen in the low temperatures of winter. However, due to the extremely low winter temperatures in frigid regions, traditional cast-in-place concrete repair techniques are unavailable due to environmental temperature limitations, leading to minor defects becoming major problems that are difficult to repair, severely impacting the structural safety and service life of the box culverts.
[0003] The microscopic mechanism of freeze-thaw damage lies in the fact that external moisture seeps into the concrete through tiny pores or microcracks on the surface. When the ambient temperature drops below freezing, the moisture in the pores freezes and expands in volume by about 9%. This expansion generates enormous internal stress within the concrete, causing the microcracks to further expand and interconnect. With repeated freeze-thaw cycles, the concrete surface gradually peels away, the internal structure becomes porous, and the load-bearing capacity decreases significantly. In extremely cold regions, this process can often cause severe structural deterioration within a single winter.
[0004] Existing partial maintenance techniques for box culverts in cold regions have many shortcomings: Firstly, the repair work requires extensive excavation around the culvert, damaging the original roadbed or pavement structure, and the repair period can last for several months. In the harsh winter conditions, the earth freezes and is difficult to excavate; even with thawing measures, the cost is extremely high. Furthermore, the excavation and repair require prolonged traffic disruption, leading not only to high construction costs but also severe disruption to surrounding traffic and residents' lives, resulting in a negative social impact.
[0005] Secondly, the quality of on-site wet construction is greatly affected by ambient temperature. In winter, the hydration reaction of concrete is hindered at low temperatures, resulting in slow strength growth and even frost heave damage before reaching the critical freezing strength. In addition, the bonding strength at the interface between new and old concrete is insufficient at low temperatures, which can easily create new weak points in the structure, making it highly likely that defects will reappear in a short period of time after repair.
[0006] Third, existing maintenance technologies lack standardized designs tailored to the structural characteristics of prefabricated box culverts. The dimensions of maintenance components are inconsistent, and the construction processes are chaotic, making it impossible to achieve modular and rapid maintenance and failing to meet the needs of emergency maintenance of box culverts in cold regions during winter. Summary of the Invention
[0007] To address the aforementioned shortcomings of existing technologies, this invention provides a modular repair system and method for precast concrete box culverts in frigid regions, thereby solving the problems of seasonal limitations and long construction periods in existing localized repair technologies for box culverts in cold regions.
[0008] To achieve the above objectives, the technical solution adopted by the present invention is as follows: On one hand, this invention provides a modular repair system for precast concrete box culverts in frigid regions, including standardized repair units, dedicated positioning frames, low-temperature curing connection components, and temporary support and protection components; the original box culvert body retains the original box culvert mother channel. Specifically, the standardized repair unit is a factory-prefabricated concrete component, with pouring, curing, and surface treatment completed in the factory, avoiding the disadvantages of temperature-affected wet work on site. Its length adopts a modular design, covering 0.5m, 1.0m, and 1.5m series specifications, which can adapt to damaged areas of different sizes, achieving immediate use after replacement. The standardized repair unit has locking key structures at both ends that are compatible with the original box culvert mother channel, providing initial positioning and force transmission through physical interlocking. Grouting channels and injection holes are reserved on the inner side of the locking key structure, forming a dual-channel sealing and connection system. The standardized repair unit features pre-embedded heating cables and conduits for active heating of the components under extremely cold conditions, preventing internal moisture from freezing and expanding. Pre-embedded strain sensors, temperature sensors, and leakage sensors acquire real-time data on structural stress, environmental conditions, and sealing status, creating a full-lifecycle health monitoring network. A low-temperature antifreeze and anti-icing coating on the inner surface effectively reduces ice and water adhesion, lowering the risk of freeze-thaw damage. A dedicated positioning frame is installed on both sides of the repair area, including a load-bearing frame, a fine-tuning positioning mechanism, and temporary fixing clamps. Adjustable support feet at the bottom ensure the frame's horizontal stability under complex working conditions. The fine-tuning positioning mechanism achieves millimeter-level alignment, and the temporary fixing clamps provide a stable clamping force. The low-temperature curing connection components utilize the rapid bonding characteristics of low-temperature curing epoxy adhesive and the micro-expansion and compaction characteristics of low-temperature high-strength micro-expansion grouting material to achieve high-strength permanent connections under extremely cold conditions. Temporary support and protection components are installed inside and outside the standardized maintenance unit. The curved support templates abut against the inner wall of the standardized maintenance unit to resist lateral soil and water pressure. The thermal insulation and curing cover covers the external repair area, and its built-in electric heating elements provide the necessary temperature and humidity environment for curing.
[0009] Furthermore, the locking key structure adopts a wedge-shaped tenon design, with the wedge-shaped tenons located at both ends of the standardized maintenance unit. The fit gap between the wedge-shaped tenons and the original box culvert mother channel is ≤3mm. The surface of the wedge-shaped tenons is provided with anti-slip texture, and HRB400 reinforcing steel mesh is pre-embedded inside the wedge-shaped tenons. The mesh spacing of the HRB400 reinforcing steel mesh is 100mm×100mm. The glue injection holes are symmetrically arranged on the upper part of the wedge-shaped tenons, and the grouting channel is horizontally connected to the bottom of the wedge-shaped tenons. The glue injection holes are connected to the grouting channel.
[0010] The wedge-shaped tenon design enhances the mechanical interlocking ability between the maintenance unit and the main body of the box culvert. Its inclined structure can convert some of the horizontal shear force into compressive force, further improving the reliability of the connection. A fit clearance of ≤3mm is a critical value set considering the material's cold contraction characteristics in frigid regions. Excessive clearance will lead to cracking and leakage of the sealing layer after low-temperature freeze-thaw cycles; insufficient clearance will cause assembly difficulties due to component deformation during winter freezing, and forced assembly can easily cause damage to the concrete edges and corners. HRB400 grade steel bars and a 100mm×100mm grid spacing provide sufficient shear and tensile strength, preventing local crushing or cracking of the locking key under stress. The injection holes and grouting channels form a three-dimensional network, with upper injection for venting and lower horizontal grouting for compaction. This utilizes fluid dynamics principles to eliminate the air pockets and voids that are prone to occur in traditional single-channel grouting.
[0011] Furthermore, the strain sensor has a measurement range of -2000με to 2000με and an accuracy of ±1με; the temperature sensor has a measurement range of -40℃ to 60℃ and an accuracy of ±0.5℃; the leakage sensor is a contact conductive sensor with a response time ≤1s; the strain sensor, the temperature sensor, and the leakage sensor are all embedded inside the concrete of the standardized maintenance unit.
[0012] The above parameters are strictly matched to the stress and environmental characteristics of box culverts in cold regions. The lower limit temperature measurement range of -40℃ covers the extreme air temperatures of extremely cold regions, and the accuracy of ±0.5℃ is sufficient to capture the tiny temperature fluctuations at the freeze-thaw critical point; the strain measurement range covers the extreme strain values under vehicle load and frost heave force; the contact conductive leakage sensor responds quickly, and once the seal fails and leakage occurs, the system can detect and alarm within 1 second to prevent water intrusion and further frost damage.
[0013] Furthermore, the load-bearing frame is welded from Q235 steel, and the rated load-bearing capacity of the frame is ≥50t; the fine-tuning positioning mechanism includes a horizontal adjusting screw and a vertical adjusting cylinder. The horizontal adjusting screw is located in the horizontal direction of the load-bearing frame, and the vertical adjusting cylinder is located in the vertical direction of the load-bearing frame. The adjustment stroke of both the horizontal adjusting screw and the vertical adjusting cylinder is 0~200mm, and the adjustment accuracy is ≤2mm; the vertical adjusting cylinder is connected to the horizontal adjusting screw through a slider, and the output end of the vertical adjusting cylinder is fixedly connected to the temporary fixing clamp. The temporary fixing clamp adopts a hydraulically driven arc-shaped gripper structure that abuts against the outer wall of the standardized maintenance unit.
[0014] Q235 steel possesses excellent mechanical properties and low-temperature toughness, and its load-bearing capacity of ≥50t is sufficient to handle the lifting weight of large precast concrete components. The vertical adjustment cylinder is mounted on the horizontal adjustment screw via a slider. Rotating the horizontal adjustment screw drives the slider and cylinder to move horizontally, achieving horizontal position adjustment. The vertical adjustment cylinder itself can achieve vertical lifting, thereby enabling decoupled adjustment of the clamp in both horizontal and vertical directions. This combination of mechanical transmission and hydraulic drive ensures both rigid and stable positioning and flexible, high-precision adjustment. The 0~200mm stroke meets the requirements for correcting conventional assembly errors. An adjustment accuracy of ≤2mm is necessary to ensure smooth tongue-and-groove engagement and uniform pressure on the sealing material. Excessive deviation can lead to stress concentration at low temperatures, causing seal failure or even component damage. The vertical adjustment cylinder directly drives the temporary fixing clamp. The hydraulic arc-shaped grippers can conform to the outer wall of the component, providing uniform surface contact clamping force and avoiding localized concrete crushing caused by point contact.
[0015] Furthermore, the arc-shaped support template is made of high-strength aluminum alloy material, the curvature of the arc-shaped support template is adapted to the inner wall of the original box culvert body, and the template thickness is ≥8mm; the thermal insulation cover adopts a composite structure of flame-retardant thermal insulation cotton and waterproof cloth, and the power of the electric heating element is 5~8kW; the low-temperature curing epoxy adhesive has a curing time of ≤4h in an environment of -15℃~5℃, and the low-temperature high-strength micro-expansion grout has a compressive strength of ≥30MPa in an environment of -10℃ for 24h, with a micro-expansion rate of 0.02%~0.05%.
[0016] The arc-shaped support formwork possesses high specific strength, effectively resisting lateral pressure from the soil or water inside the culvert while maintaining a lightweight design, preventing deformation of the repaired area during grouting and curing. Flame-retardant insulation cotton combined with waterproof fabric not only provides excellent insulation but also prevents moisture intrusion during construction. The 5-8kW electric heating element power is calculated based on thermal balance, maintaining a positive temperature environment above 5℃ inside the enclosure even in frigid external environments. Epoxy adhesive that cures for 4 hours at -15℃ to 5℃ provides early stability for subsequent grouting; the grouting material with a micro-expansion rate of 0.02%-0.05% compensates for low-temperature shrinkage, ensuring seamless bonding between the new and old interfaces and preventing shrinkage cracks.
[0017] On the other hand, the present invention also provides a repair method for a modular repair system of precast concrete box culverts in frigid regions, comprising the following steps: S1. Survey and Positioning and Interface Pretreatment: Ultrasonic testing technology is used to conduct a comprehensive inspection of the original box culvert body to determine the location, extent, and degree of damage in localized areas. Based on the damage extent, the corresponding standardized repair unit is selected to determine the cutting boundary of the original box culvert body. A temporary protective shed is erected around the damaged area, and the damaged area is cut using a localized protective heating dry cutting method. During the cutting process, the ambient temperature of the cutting area is maintained above 10°C using heating equipment inside the protective shed. After cutting, an electric heating surface treatment device is used to grind, de-ice, and preheat the interface of the original box culvert mother channel to raise the interface temperature to 5°C~10°C and the surface roughness to Ra1.6~Ra3.2μm. In step S1, ultrasonic testing accurately identifies internal cracks, avoiding blind cutting. The localized protective heating dry cutting method raises the cutting environment to above 10°C by constructing a closed, insulated shed and heating it, effectively preventing brittle chipping and cracking of concrete during low-temperature cutting. Electrically heated grinding not only removes frost and loose layers but also preheats the interface to 5°C~10°C, reducing the temperature difference between new and old materials and minimizing temperature stress. A roughness of Ra1.6~Ra3.2μm is a parameter specifically optimized for low-temperature curing bonding systems. Excessive roughness can trap air, and the expansion of condensed water vapor can crack the bonding layer; insufficient roughness results in insufficient mechanical interlocking force, easily leading to overall debonding.
[0018] S2. Unit Lifting and Temporary Consolidation: The dedicated positioning frame is installed and fixed on both sides of the original culvert main body repair area. The positioning benchmark is adjusted by the fine-tuning positioning mechanism, and the standardized repair unit is lifted to the repair position. The dedicated positioning frame is used to achieve precise alignment, with an alignment deviation of ≤5mm. The standardized repair unit is temporarily fixed to the original culvert main body by the temporary fixing clamp. Then, the low-temperature curing epoxy adhesive is injected into the key gap to achieve temporary consolidation. In step S2, the step-by-step fine-tuning process, first horizontal and then vertical, ensures smooth engagement between the key and the mother groove. The alignment deviation of ≤5mm is within the allowable stress range. The hydraulic clamping of the temporary fixing clamp restricts component displacement, providing a undisturbed environment for the 4-hour curing period of the epoxy adhesive. The amount of adhesive injected is 1.2 times the gap volume, ensuring that the adhesive fully overflows and vents, ensuring full filling without voids.
[0019] S3. Permanent Connection and Thermal Insulation Curing: The low-temperature high-strength micro-expansion grout is injected through the grouting channel reserved in the standardized maintenance unit. The grouting pressure is controlled at 0.3~0.5MPa, and a layered grouting method is used to ensure full filling. After grouting, the maintenance area is covered with the thermal insulation curing cover, and the electric heating element is activated to maintain the curing temperature at 0℃~10℃ for ≥24h. In step S3, the grouting pressure of 0.3~0.5MPa ensures that the grout penetrates into the tiny gaps without causing structural cracking due to excessive pressure. Layered grouting (each layer ≤500mm, interval ≥30min) allows time for initial settling and air venting of the lower layer of grout, effectively preventing the accumulation of air bubbles and water separation that are prone to occur with overall grouting. Constant temperature curing at 0℃~10℃ avoids frost heave damage, and at the same time utilizes the antifreeze components of the low-temperature grout itself, achieving a strength of over 30MPa in 24h, meeting the requirements for rapid restoration of traffic.
[0020] S4. Traffic Restoration and Long-Term Monitoring: After maintenance, the temporary support and protection components and the dedicated positioning frame are removed, temporary traffic guidance facilities are installed, and traffic is restored using a half-width traffic mode. The repaired area is monitored long-term using the strain sensors, temperature sensors, and leakage sensors pre-embedded in the standardized maintenance unit. The half-width traffic mode minimizes the disruption to urban traffic caused by maintenance work. Long-term monitoring by the pre-embedded sensors constructs a digital twin operation and maintenance system. Through real-time data comparison and historical trend analysis, it is possible to predict structural deterioration trends in advance, realizing a shift from "post-event maintenance" to "preventive maintenance," and greatly extending the overall service life of the box culvert.
[0021] Furthermore, the localized protective heating dry cutting method described in step S1 employs a diamond wire saw with an insulation cover, controlling the cutting speed at 5-10 cm / min. The heating equipment uses a fuel-fired heater, and temperature monitoring points are set up inside the protective shed, recording temperature data every 30 minutes. The diamond wire saw offers high cutting precision and low vibration, maximizing the protection of undamaged areas of the culvert. The low cutting speed of 5-10 cm / min avoids stress concentration and heat loss caused by high-speed friction. The fuel-fired heater provides high heat output, and combined with the 30-minute temperature recording, forms a closed-loop temperature control system, ensuring a positive temperature environment throughout the cutting operation.
[0022] Furthermore, the electrically heated surface treatment equipment described in step S1 includes an electrically heated grinding wheel and a hot air preheating device. The heating power of the electrically heated grinding wheel is 2-3kW, and the hot air temperature of the preheating device is 80-100℃. After the interface treatment is completed, the subsequent temporary consolidation construction must be completed within 2 hours. The 2-3kW electrically heated grinding wheel conducts heat into the concrete while cutting, and the 80-100℃ hot air can penetrate the surface micro-cracks and remove deep ice crystals. The 2-hour construction window is calculated based on the interface temperature loss rate under extremely cold conditions. Failure to consolidate within this time will lead to secondary icing or contamination of the interface, severely affecting the bonding strength.
[0023] Furthermore, the specific parameters for the layered grouting method described in step S3 are as follows: the height of each grouting layer is ≤500mm, and the interval between two adjacent grouting layers is ≥30min; after grouting, ultrasonic testing technology is used to check the grout fullness, and the pass rate must reach 100%. Ultrasonic transmission is used to check the grout fullness; sound waves will reflect and attenuate at voids, and the difference in amplitude can accurately locate the non-dense areas. The 100% pass rate requirement ensures that there are no mechanically weak points at the connection interface, guaranteeing the overall sealing and load-bearing capacity of the structure.
[0024] Furthermore, the specific parameters for long-term monitoring in step S4 are as follows: temperature and strain data are collected every hour, leakage data is collected in real time, and the monitoring data is uploaded to the operation and maintenance management platform via a wireless transmission module; the preset thresholds for monitoring data are: strain ±1500με, temperature -35℃ to 50℃, and contact conductivity response of the leakage sensor. When the threshold is exceeded, the platform automatically issues an early warning signal. The 1-hour data acquisition frequency balances data continuity and equipment power consumption. The strain early warning threshold of ±1500με is lower than the critical strain for concrete cracking, leaving a safety margin; the temperature threshold of -35℃ to 50℃ covers the extreme temperature difference in cold regions. An abnormally high temperature may indicate internal frictional heating or abnormal groundwater temperature, and the contact conductivity response is the most direct criterion for determining leakage. The automatic SMS early warning mechanism ensures that management personnel can intervene and handle the situation immediately.
[0025] Compared with existing partial maintenance techniques for box culverts in cold regions, this invention has the following advantages: I. This invention solves the problem that traditional maintenance techniques cannot be carried out in low-temperature winter environments by using low-temperature curing connection components and thermal insulation maintenance technology. It can carry out local damage repair of box culverts in environments above -15℃, effectively avoiding the "minor problems becoming major" and ensuring the safe operation of box culverts in cold regions during winter.
[0026] Second, this invention adopts a standardized and modular maintenance unit design, and with the help of a special positioning frame, it can achieve precise and rapid positioning. Through the four-step construction method of "pretreatment-hoisting-consolidation-grouting-curing-restoration-monitoring", the construction period of traditional maintenance, which takes several months, can be shortened to a few days or even overnight. At the same time, the traffic organization scheme of half-width construction and temporary support is adopted to achieve uninterrupted operation or minimal disruption to traffic.
[0027] Third, the standardized maintenance unit of this invention adopts a factory prefabrication method, which makes the production process controllable and the quality stable; through the three-in-one connection method of "mother tank key grouting" combined with low temperature curing materials, it ensures that the connection between the new and old structures is firm and the bonding strength is high, avoiding the formation of new weak links; the monitoring system integrated in the maintenance unit can realize long-term real-time monitoring.
[0028] Fourth, this invention eliminates the need for large-scale excavation, reducing roadbed and pavement damage and restoration costs; it shortens the maintenance period, reducing labor and machinery rental costs; and it improves maintenance quality, reducing subsequent secondary maintenance costs, resulting in significant overall economic and social benefits. Attached Figure Description
[0029] Figure 1 This is a schematic diagram of a modular rapid repair method for precast concrete box culverts in extremely cold regions.
[0030] Figure 2 This is a sectional view of the interior of a standardized maintenance unit.
[0031] Figure 3 This is a detailed enlarged view of a wedge-shaped locking key structure.
[0032] Figure 4 This is the front view of the dedicated positioning frame.
[0033] Figure 5 This is a cross-sectional view of the temporary support and protection components.
[0034] Figure 6 Axonometric drawing of the temporary support and protection components for three-dimensional installation.
[0035] The components include: 1. Standardized maintenance unit; 2. Wedge-shaped tenon; 3. Glue injection hole; 4. Grouting channel; 5. HRB400 reinforced steel mesh; 6. Low-temperature antifreeze and anti-icing coating; 7. Pre-installed conduit for heating cables; 8. Strain sensor; 9. Temperature sensor; 10. Leakage sensor; 11. Dedicated positioning frame; 12. Load-bearing frame; 13. Horizontal adjusting screw; 14. Vertical adjusting cylinder; 15. Temporary fixing clamp; 16. Adjustable support feet; 17. Temporary support and protection components; 18. Arc-shaped support template; 19. Thermal insulation and curing cover; 20. Original box culvert main body; 21. Original box culvert mother channel. Detailed Implementation
[0036] The specific embodiments of the present invention are described below to enable those skilled in the art to understand the present invention. However, it should be understood that the present invention is not limited to the scope of the specific embodiments. For those skilled in the art, various changes are obvious as long as they are within the spirit and scope of the present invention as defined and determined by the appended claims. All inventions utilizing the concept of the present invention are protected.
[0037] like Figures 1 to 6 As shown, this embodiment provides a modular repair system and method for precast concrete box culverts in frigid regions, with a detailed description based on a winter emergency repair project of a box culvert in a northern city. In this project, the original box culvert body 20 was used in a frigid region with a winter minimum temperature of -35℃. Inspection revealed a localized damaged area with a length of 1.2m and a width of 0.8m on the left side wall of the box culvert, 20m from the starting point, accompanied by a crack with a depth of 50mm.
[0038] This embodiment provides a modular repair system for precast concrete box culverts in extremely cold regions, including a standardized repair unit 1, a dedicated positioning frame 11, a low-temperature curing connection assembly, and a temporary support and protection assembly 17. The original box culvert body 20 is equipped with the original box culvert mother channel 21.
[0039] Specifically, the standardized maintenance unit 1 is a factory-prefabricated C50 concrete component with a modular design for its length, covering specifications of 0.5m, 1.0m, and 1.5m. This embodiment selects a 1.5m standardized maintenance unit 1. Both ends of the standardized maintenance unit 1 are equipped with wedge-shaped tenons 2 that fit with the original box culvert mother channel 21. The fit clearance between the wedge-shaped tenons 2 and the original box culvert mother channel 21 is ≤3mm; in this embodiment, the fit clearance is controlled at 2mm. The surface of the wedge-shaped tenons 2 has an anti-slip texture, and HRB400 reinforcing steel mesh 5 is pre-embedded inside the wedge-shaped tenons 2, with a mesh spacing of 100mm × 100mm. The upper part of the wedge-shaped tenons 2 is symmetrically equipped with glue injection holes 3, and the bottom is horizontally connected with a grouting channel 4, with the glue injection holes 3 and the grouting channel 4 communicating. The standardized maintenance unit 1 is pre-embedded with a heating cable pre-installed pipe 7, a strain sensor 8, a temperature sensor 9, and a leakage sensor 10. The strain sensor 8 has a measurement range of -2000με to 2000με and an accuracy of ±1με; the temperature sensor 9 has a measurement range of -40℃ to 60℃ and an accuracy of ±0.5℃; the leakage sensor 10 is a contact-type conductive sensor with a response time ≤1s. The inner surface of the standardized maintenance unit 1 is coated with a low-temperature antifreeze and anti-icing coating 6, which in this embodiment uses a polyurea coating.
[0040] A dedicated positioning frame 11 is installed on both sides of the repair area of the standardized repair unit 1. The dedicated positioning frame 11 includes a load-bearing frame 12, a fine-tuning positioning mechanism, and a temporary fixing clamp 15. The load-bearing frame 12 is welded from Q235 steel and has a rated load-bearing capacity of 50t. The bottom of the load-bearing frame 12 is equipped with adjustable support feet 16. The fine-tuning positioning mechanism includes a horizontal adjusting screw 13 and a vertical adjusting cylinder 14, both with an adjustment stroke of 0~200mm and an adjustment accuracy of ≤2mm. The vertical adjusting cylinder 14 is connected to the horizontal adjusting screw 13 via a slider. The output end of the vertical adjusting cylinder 14 is fixedly connected to the temporary fixing clamp 15. The temporary fixing clamp 15 adopts a hydraulically driven arc-shaped gripper structure, and the grippers of the temporary fixing clamp 15 abut against the outer wall of the standardized repair unit 1.
[0041] The low-temperature curing connection components include low-temperature curing epoxy adhesive and low-temperature high-strength micro-expansion grout. The low-temperature curing epoxy adhesive uses modified epoxy resin as a base material, with added low-temperature curing agents and antifreeze agents, and its curing time is ≤4 hours at -15℃ to 5℃. The low-temperature high-strength micro-expansion grout uses Portland cement as a base material, incorporating ultrafine admixtures, high-efficiency water-reducing agents, and micro-expansion agents. Its flowability is ≥300mm, and its compressive strength is ≥30MPa after 24 hours and ≥50MPa after 28 days at -10℃, with a micro-expansion rate of 0.02%~0.05%.
[0042] Temporary support and protection components 17 are installed both inside and outside the standardized maintenance unit 1. These include an arc-shaped support template 18, an insulated curing cover 19, and temporary traffic guidance facilities. The arc-shaped support template 18 is made of high-strength aluminum alloy, with a template thickness ≥8mm, and its curvature matches the inner wall of the original box culvert body 20. The insulated curing cover 19 uses a composite structure of flame-retardant insulation cotton and waterproof cloth, covering the external repair area of the standardized maintenance unit 1, and has built-in electric heating elements with a power of 5~8kW.
[0043] Based on the above system, the repair method in this embodiment is as follows: Figure 1 As shown, the specific steps include: S1. Survey and Location and Interface Pretreatment: Ultrasonic testing technology was used to conduct a comprehensive inspection of the original box culvert body 20 to determine the location, extent, and degree of damage to localized areas. Based on the damage range of 1.2m × 0.8m, a standardized repair unit 1 with a length of 1.5m was selected, and the cutting boundary was determined to be 100mm beyond the damaged area.
[0044] A temporary protective shed measuring 3m × 2m × 2.5m was erected around the damaged area. The shed had a steel frame structure covered with waterproof and thermal insulation fabric, and two 5kW fuel-fired heaters were installed inside. A diamond wire saw with an insulated cover was used to cut the damaged area at a speed controlled at 8cm / min. During the cutting process, the temperature inside the shed was maintained at 8℃~5℃ using the heaters, and the temperature data was recorded every 30 minutes.
[0045] After cutting, an electrically heated surface treatment device was used to treat the interface of the original box culvert mother channel 21. The electrically heated grinding wheel had a power of 2.5kW and a grinding speed of 1500r / min. Simultaneously, a hot air preheating device was activated at a temperature of 90℃. The interface was ground to a surface roughness Ra of 2.5μm, and the temperature was raised to 8℃. Dust, frost, and loose concrete layers were then removed from the interface. Subsequent construction work commenced within 1.5 hours of the interface treatment to prevent refreezing or contamination.
[0046] S2. Unit Lifting and Temporary Fixing: The special positioning frame 11 is installed and fixed on both sides of the repair area of the original box culvert body 20. The level of the load-bearing frame 12 is adjusted by the adjustable support feet 16 at the bottom, with a horizontal deviation ≤1mm / m. A 25t truck crane is used to lift the standardized repair unit 1 to the repair position. First, the horizontal adjusting screw 13 drives the slider and the vertical adjusting cylinder 14 to move horizontally to complete the left and right alignment. After the position is correct, the nut is tightened. Then, the vertical adjusting cylinder 14 drives the repair unit to lift and lower to complete the height calibration. After the alignment is correct, the hydraulic self-locking function is used to lock it. In this embodiment, the horizontal adjustment stroke is 80mm, the vertical adjustment stroke is 50mm, and the final alignment deviation is 3mm.
[0047] After alignment, the hydraulic system is activated to push the two arc-shaped grippers on both sides of the temporary fixing clamp 15 inward simultaneously, achieving surface contact clamping from the left and right outer walls of the maintenance unit 1. Then, low-temperature curing epoxy resin is injected into the key gap through the injection hole 3, with the injection volume being 1.2 times the gap volume to ensure full filling. Temporary curing is completed by standing at 8℃ for 4 hours, at which point the epoxy resin shear strength reaches 4.2 MPa.
[0048] S3. Permanent Connection and Thermal Insulation Curing: A high-pressure grouting pump is used to inject low-temperature, high-strength, micro-expansion grouting material through grouting channel 4. The grouting pressure is controlled at 0.4 MPa. A layered grouting method is adopted, with each layer having a height of 400 mm and an interval of 30 minutes between adjacent layers, for a total grouting volume of 1.8 m³. Layered grouting effectively avoids air bubble accumulation and water bleeding.
[0049] After grouting, an insulating curing cover was placed over the repair area, and a 6kW electric heating element was activated to maintain the curing temperature at 5℃~8℃ for 24 hours. During curing, the grout temperature and strength were monitored every 2 hours. The compressive strength reached 32MPa after 24 hours, meeting the design requirements. After grouting, ultrasonic testing was used to check the grout fullness, and the pass rate reached 100%.
[0050] S4. Traffic Restoration and Long-Term Monitoring: After maintenance, the hydraulic system is depressurized to release the clamps, and the temporary protective shed, special positioning frame 11, and temporary support and protection components 17 are removed. Temporary traffic guidance facilities, including warning signs, reflective cones, and temporary guardrails, are set up on both sides of the culvert, and traffic is restored using a half-width traffic mode.
[0051] Long-term monitoring of the repair area is achieved through sensors pre-embedded within standardized maintenance unit 1. Strain sensor 8 collects data every hour, with a measurement range of -2000με to 2000με and an accuracy of ±1με; temperature sensor 9 collects data every hour, with a measurement range of -40℃ to 60℃ and an accuracy of ±0.5℃; leakage sensor 10 collects data in real time, with a response time ≤1s. Monitoring data is uploaded to the operation and maintenance management platform via a GPRS wireless transmission module. The strain warning threshold is set at ±1500με, the temperature warning threshold at -35℃ to 50℃, and the leakage warning threshold at contact conductivity response. When the monitoring data exceeds the preset thresholds, the platform automatically sends an SMS warning.
[0052] In this embodiment, the entire repair process took 3 days, which is more than 90% shorter than the traditional repair period. The bonding strength at the interface between the new and old structures was 4.5 MPa. Through monitoring over one winter, the strain in the repaired area remained stable between -200 με and 150 με, the temperature change was synchronized with the ambient temperature, there was no leakage, the repair quality was reliable, and rapid and high-quality repair of box culverts in cold regions during winter was achieved.
Claims
1. A modular repair system for precast concrete box culverts in cold regions, characterized in that, Includes a standardized maintenance unit (1), a dedicated positioning frame (11), a low-temperature curing connection assembly and a temporary support and protection assembly (17); the original box culvert body (20) is equipped with the original box culvert mother channel (21); The standardized repair unit (1) is a precast concrete component in the factory. Its length is modularly designed. The standardized repair unit (1) is located in the damaged area of the original box culvert body (20). Both ends of the standardized repair unit (1) are equipped with key structures that are compatible with the original box culvert mother channel (21). The key structure has a grouting channel (4) and an injection hole (3) reserved on the inner side. The standardized repair unit (1) has a pre-embedded heating cable pipe (7), strain sensor (8), temperature sensor (9) and leakage sensor (10). The inner surface of the standardized repair unit (1) is coated with a low-temperature antifreeze and anti-icing coating (6). The dedicated positioning frame (11) is located on both sides of the repair area of the standardized repair unit (1). The dedicated positioning frame (11) includes a load-bearing frame (12), a fine-tuning positioning mechanism and a temporary fixing clamp (15). The load-bearing frame (12) has adjustable support feet (16) at the bottom. The fine-tuning positioning mechanism is connected to the temporary fixing clamp (15). The temporary fixing clamp (15) abuts against the outer wall of the standardized repair unit (1). The low-temperature curing connection component includes a low-temperature curing epoxy adhesive and a low-temperature high-strength micro-expansion grout. The low-temperature curing epoxy adhesive fills the gap in the key structure, and the low-temperature high-strength micro-expansion grout fills the grouting channel (4). The temporary support and protection assembly (17) is located inside and outside the standardized maintenance unit (1). The temporary support and protection assembly (17) includes an arc-shaped support template (18), a thermal insulation cover (19), and temporary traffic guidance facilities. The arc-shaped support template (18) abuts against the inner wall of the standardized maintenance unit (1). The thermal insulation cover (19) covers the external repair area of the standardized maintenance unit (1). The thermal insulation cover (19) has an electric heating element built in.
2. The modular repair system for precast concrete box culverts in cold regions according to claim 1, wherein, The locking key structure adopts a wedge-shaped tenon (2) design. The wedge-shaped tenon (2) is located at both ends of the standardized maintenance unit (1). The fit gap between the wedge-shaped tenon (2) and the original box culvert mother groove (21) is ≤3mm. The surface of the wedge-shaped tenon (2) is provided with anti-slip texture. The wedge-shaped tenon (2) is pre-embedded with HRB400 reinforcing steel mesh (5). The mesh spacing of the HRB400 reinforcing steel mesh (5) is 100mm×100mm. The glue injection hole (3) is symmetrically arranged on the upper part of the wedge-shaped tenon (2). The grouting channel (4) is horizontally connected to the bottom of the wedge-shaped tenon (2). The glue injection hole (3) is connected to the grouting channel (4).
3. The modular repair system for precast concrete box culverts in cold regions according to claim 1, wherein, The strain sensor (8) has a measurement range of -2000με to 2000με and an accuracy of ±1με; the temperature sensor (9) has a measurement range of -40℃ to 60℃ and an accuracy of ±0.5℃; the leakage sensor (10) is a contact conductive sensor with a response time ≤1s; the strain sensor (8), the temperature sensor (9) and the leakage sensor (10) are all embedded in the concrete of the standardized maintenance unit (1).
4. The modular repair system for precast concrete box culverts in cold regions according to claim 1, wherein, The load-bearing frame (12) is welded from Q235 steel, and the frame has a rated load-bearing capacity of ≥50t. The fine-tuning positioning mechanism includes a horizontal adjusting screw (13) and a vertical adjusting cylinder (14). The horizontal adjusting screw (13) is located in the horizontal direction of the load-bearing frame (12), and the vertical adjusting cylinder (14) is located in the vertical direction of the load-bearing frame (12). The adjustment stroke of the horizontal adjusting screw (13) and the vertical adjusting cylinder (14) are both 0~200mm, and the adjustment accuracy is ≤2mm. The vertical adjusting cylinder (14) is connected to the horizontal adjusting screw (13) through a slider. The output end of the vertical adjusting cylinder (14) is fixedly connected to the temporary fixing clamp (15). The temporary fixing clamp (15) adopts a hydraulically driven arc-shaped gripper structure and abuts against the outer wall of the standardized maintenance unit (1).
5. The modular repair system for precast concrete box culverts in cold regions according to claim 1, wherein, The arc-shaped support template (18) is made of high-strength aluminum alloy material. The arc of the arc-shaped support template (18) is adapted to the inner wall of the original box culvert body (20). The template thickness is ≥8mm. The thermal insulation cover (19) adopts a composite structure of flame-retardant thermal insulation cotton and waterproof cloth. The power of the electric heating element is 5~8kW. The low-temperature curing epoxy adhesive has a curing time of ≤4h in an environment of -15℃~5℃. The low-temperature high-strength micro-expansion grout has a compressive strength of ≥30MPa in an environment of -10℃ for 24h. The micro-expansion rate is 0.02%~0.05%.
6. A method of repairing a modular repair system for a precast concrete box culvert in cold regions according to any one of claims 1-5, characterized in that, Includes the following steps: S1. Survey and positioning and interface pretreatment: The original box culvert body (20) is fully inspected using ultrasonic testing technology to determine the location, range and degree of damage of the local damaged area. The corresponding standard maintenance unit (1) is selected according to the damage range to determine the cutting boundary of the original box culvert body (20). Temporary protective sheds are set up around the damaged area, and the damaged area is cut using the local protective heating dry cutting method. During the cutting process, the ambient temperature of the cutting area is maintained above 10℃ by the heating equipment in the protective shed. After the cutting is completed, the interface of the original box culvert mother channel (21) is polished, de-iced and preheated using an electric heating surface treatment device to raise the interface temperature to 5℃~10℃ and the surface roughness to Ra1.6~Ra3.2μm. S2. Unit hoisting and temporary consolidation: The special positioning frame (11) is installed and fixed on both sides of the repair area of the original box culvert body (20). The positioning reference is adjusted by the fine-tuning positioning mechanism, and the standardized repair unit (1) is hoisted to the repair position. The special positioning frame (11) is used to achieve precise alignment with an alignment deviation of ≤5mm. The standardized repair unit (1) is temporarily fixed to the original box culvert body (20) by the temporary fixing clamp (15). Then, the low-temperature curing epoxy glue is injected into the key gap to achieve temporary consolidation. S3. Permanent connection and thermal insulation maintenance: The low-temperature high-strength micro-expansion grout is injected through the grouting channel (4) reserved in the standardized maintenance unit (1). The grouting pressure is controlled at 0.3~0.5MPa. The layered grouting method is adopted to ensure full filling. After the grouting is completed, the thermal insulation maintenance cover (19) is covered in the maintenance area. The electric heating element is activated to maintain the maintenance temperature at 0℃~10℃. The maintenance time is ≥24h. S4. Traffic restoration and long-term monitoring: After maintenance is completed, the temporary support and protection components (17) and the special positioning frame (11) are removed, temporary traffic guidance facilities are set up, and traffic is restored by adopting a half-width traffic mode; the repair area is monitored for a long time by the strain sensor (8), the temperature sensor (9) and the leakage sensor (10) pre-embedded in the standardized maintenance unit (1).
7. The method of rehabilitating a modular rehabilitation system for a precast concrete box culvert in cold regions according to claim 6, wherein, The localized protective heating dry cutting method described in step S1 uses a diamond wire saw with an insulation cover. The cutting speed is controlled at 5~10cm / min. The heating equipment is a fuel-fired heater. Temperature monitoring points are set up inside the protective shed, and temperature data is recorded every 30 minutes.
8. The method of rehabilitating a modular rehabilitation system for a precast concrete box culvert in cold regions according to claim 6, wherein, The electrically heated surface treatment equipment mentioned in step S1 includes an electrically heated grinding wheel and a hot air preheating device. The heating power of the electrically heated grinding wheel is 2-3kW, and the hot air temperature of the preheating device is 80~100℃. After the interface treatment is completed, the subsequent temporary consolidation construction needs to be completed within 2 hours.
9. The method of rehabilitating a modular rehabilitation system for a precast concrete box culvert in cold regions according to claim 6, wherein, The specific parameters of the layered grouting method described in step S3 are as follows: the grouting height of each layer is ≤500mm, the interval between two adjacent grouting layers is ≥30min; after grouting is completed, ultrasonic testing technology is used to test the grouting fullness, and the pass rate of the test must reach 100%.
10. The method of rehabilitating a modular rehabilitation system for a precast concrete box culvert in cold regions according to claim 6, wherein, The specific parameters for long-term monitoring in step S4 are as follows: temperature and strain data are collected every 1 hour, leakage data is collected in real time, and the monitoring data is uploaded to the operation and maintenance management platform through a wireless transmission module; the preset thresholds for monitoring data are: strain ±1500με, temperature -35℃~50℃, and contact conductivity response of the leakage sensor. When the threshold is exceeded, the platform automatically issues an early warning signal.