Active optical fiber and communication equipment
By introducing erbium, aluminum and phosphorus in a specific ratio into the core of active optical fiber, the energy level structure of erbium ions is controlled, solving the problem that conventional erbium-doped optical fibers cannot simultaneously cover short-wavelength and long-wavelength signal light, and achieving efficient dual-band gain and low power consumption gain.
Patent Information
- Application Number
- CN202611182698.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-05
- Publication Date
- 2026-11-17
AI Technical Summary
Conventional erbium-doped fiber can only provide gain for long-wavelength signal light and cannot simultaneously cover the short-wavelength communication band of the pump light. Furthermore, it requires a high-power pump source, which increases system power consumption and cost.
By introducing a specific ratio of erbium, aluminum, and phosphorus elements into the core of an active optical fiber, an Er-Al-P multi-element doping system is formed, and the energy level structure of erbium ions is controlled to achieve simultaneous gain on both short-wavelength and long-wavelength signal light.
Simultaneous gain of short-wavelength S-band and long-wavelength L-band signal light under C-band pump light excitation was achieved, improving the gain-bandwidth product and pump light utilization efficiency, reducing the probability of non-radiative transitions, and increasing the luminescence quantum efficiency.
Smart Images

Figure CN123113077A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of communication technology, and in particular to an active optical fiber and a communication device. Background Technology
[0002] The practical application of erbium-doped fiber amplifiers (EDFAs) has greatly propelled the development of fiber optic communication systems towards higher capacity and longer distances. Erbium-doped fiber is produced by doping erbium ions (Er) into the core of a silica fiber. 3+ As a gain medium, when an external pump light is applied, erbium ions move from their ground state ( 4 I 15 / 2 The transition occurs to an excited state, followed by relaxation to a metastable state. 4 I 13 / 2 This process creates a population inversion. When the signal light passes through, the metastable particles undergo stimulated emission and transition back to the ground state, amplifying the signal light.
[0003] However, according to the energy level transition rules of erbium ions, the pump light will change the ground state ( 4 I 15 / 2 ) Particles are excited to a metastable state ( 4 I 13 / 2 After that, stimulated emission only occurs in the metastable state ( 4 I 13 / 2 ) to ground state ( 4 I 15 / 2 During the transition process, because the energy interval of this transition is always less than or equal to the energy interval corresponding to the pump absorption, the wavelength of the amplified signal light can only be greater than or equal to the pump light wavelength, and cannot amplify signal light with wavelengths shorter than the pump light. Therefore, conventional erbium-doped fiber can only provide gain for long-wavelength signal light at a certain pump wavelength, and cannot simultaneously cover the communication band on the short-wavelength side of the pump light. Summary of the Invention
[0004] This application provides an active optical fiber and a communication device, which achieves simultaneous gain of short-wavelength and long-wavelength signal light in the active optical fiber under C-band pump light excitation by co-doping Er, Al, P and Ge in a specific ratio in the active fiber core.
[0005] To achieve the above objectives, this application proposes an active optical fiber, wherein the core of the active optical fiber is doped with 0.1~0.5 wt.% Er, 8.0~10 wt.% Al and 10~15 wt.% P.
[0006] In addition, to achieve the above objectives, this application also proposes a communication device, which includes the active optical fiber described above.
[0007] One or more technical solutions proposed in this application have at least the following technical effects: An active optical fiber is provided, the core of which is doped with 0.1~0.5 wt.% Er, 8.0~10 wt.% Al, and 10~15 wt.% P. By simultaneously introducing erbium (Er), aluminum (Al), and phosphorus (P) elements into the core of the active optical fiber and precisely controlling the doping ratio of each element, an Er-Al-P multi-doped synergistic optical fiber system is formed. In this system, aluminum ions and phosphorus ions act together on the coordination field around erbium ions, altering the local crystal field environment of erbium ions, causing Stark splitting and broadening of the erbium ion energy levels, thereby effectively controlling the metastable state of erbium ions. 4 I 13 / 2 ) and ground state ( 4 I 15 / 2 The particle population distribution on each Stark sublevel within the energy level. Based on the modulation of the energy level structure, when the above active fiber is excited by pump light with a wavelength in the C-band (1525~1545nm), it is in the ground state ( 4 I 15 / 2 The electrons at the top are pumped to a metastable state. 4 I 13 / 2 The top and bottom of the metastable state allow electrons pumped to the bottom to relax further to lower Stark levels in the metastable state via phonon-assisted relaxation, thereby amplifying the long-wavelength L-band (1575~1580 nm) signal light. Simultaneously, the co-doping of aluminum and phosphorus broadens the metastable energy levels, allowing electrons at the bottom of the metastable state to absorb a second C-band pump photon and undergo excited-state absorption transitions to higher excited states. 4 I 11 / 2 The erbium-doped fiber enters a state at the top Stark sublevel, which then relaxes nonradiatively back to the metastable state. This significantly increases the population at the top metastable sublevel, enabling the active fiber to achieve population inversion and signal amplification in the short-wavelength S-band (1480-1500 nm). Furthermore, the introduction of phosphorus reduces the phonon energy of the fiber matrix material, decreases the probability of nonradiative transitions, and improves the luminescence quantum efficiency of erbium. Through the synergistic doping of erbium (Er), aluminum (Al), and phosphorus (P) within a specific ratio range, this embodiment overcomes the limitation of traditional erbium-doped fibers that can only amplify signal light with wavelengths longer than the pump light wavelength. It achieves simultaneous gain capability for both short-wavelength S-band and long-wavelength L-band signal light under C-band pump light excitation, effectively improving the gain-bandwidth product and pump light utilization efficiency of the active fiber. Attached Figure Description
[0008] Figure 1 This is a schematic diagram of the energy level structure of an active optical fiber under C-band pumping conditions according to an embodiment of this application; Figure 2This is a schematic diagram of the structure of an active optical fiber according to an embodiment of this application; Figure 3 This is a flowchart of the active optical fiber fabrication method according to an embodiment of this application; Figure 4 The images show the fiber absorption spectrum and small-signal gain spectrum of the active optical fiber in the embodiments of this application. Figure 5 This is a schematic diagram illustrating the testing principle of the effect of pump light on the amplification and gain characteristics of signal light in an embodiment of this application.
[0009] Explanation of reference numerals in the attached figures 10. Active optical fiber; 11. Fiber core; 12. Inner cladding; 13. Cladding; 14. Coating. Detailed Implementation
[0010] The following detailed description, with appropriate reference to the accompanying drawings, specifically discloses embodiments of the active optical fiber and communication device of this application. However, unnecessary detailed descriptions may be omitted. For example, detailed descriptions of well-known matters and repetitive descriptions of practically identical structures may be omitted. This is to avoid unnecessarily lengthy descriptions and to facilitate understanding by those skilled in the art. Furthermore, the accompanying drawings and the following description are provided for the purpose of enabling those skilled in the art to fully understand this application and are not intended to limit the subject matter of the claims.
[0011] The "range" disclosed in this application is defined by a lower limit and an upper limit. A given range is defined by selecting a lower limit and an upper limit, which define the boundaries of a particular range. Ranges defined in this way can include or exclude endpoints and can be arbitrarily combined; that is, any lower limit can be combined with any upper limit to form a range. For example, if ranges of 60~120 and 80~110 are listed for a specific parameter, it is also expected that ranges of 60~110 and 80~120 are also included. Furthermore, if minimum range values of 1 and 2 are listed, and if maximum range values of 3, 4, and 5 are listed, then the following ranges are all expected: 1~3, 1~4, 1~5, 2~3, 2~4, and 2~5. In this application, unless otherwise stated, the numerical range "a~b" represents a shortened representation of any combination of real numbers between a and b, where a and b are real numbers. For example, the numerical range "0~5" indicates that all real numbers between "0~5" have been listed in this article; "0~5" is simply a shortened representation of these numerical combinations. Furthermore, when a parameter is stated as an integer ≥2, it is equivalent to disclosing that the parameter is, for example, an integer such as 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, etc.
[0012] Unless otherwise specified, all embodiments and optional embodiments of this application can be combined to form new technical solutions.
[0013] Unless otherwise specified, all steps of this application may be performed sequentially or randomly, preferably sequentially. For example, if the method includes steps (a) and (b), it means that the method may include steps (a) and (b) performed sequentially, or it may include steps (b) and (a) performed sequentially. For example, if the method may also include step (c), it means that step (c) may be added to the method in any order. For example, the method may include steps (a), (b), and (c), or it may include steps (a), (c), and (b), or it may include steps (c), (a), and (b), etc.
[0014] The practical application of erbium-doped fiber amplifiers (EDFAs) has greatly propelled the development of fiber optic communication systems towards higher capacity and longer distances. Erbium-doped fiber is produced by doping erbium ions (Er) into the core of a silica fiber. 3+ As a gain medium, when an external pump light is applied, erbium ions move from their ground state ( 4 I 15 / 2 The transition occurs to an excited state, followed by relaxation to a metastable state. 4 I 13 / 2 This process creates a population inversion. When the signal light passes through, the metastable particles undergo stimulated emission and transition back to the ground state, amplifying the signal light.
[0015] However, according to the energy level transition rules of erbium ions, the pump light will change the ground state ( 4 I 15 / 2 ) Particles are excited to a metastable state ( 4 I 13 / 2 After that, stimulated emission only occurs in the metastable state ( 4 I 13 / 2 ) to ground state ( 4 I 15 / 2 During the transition process of erbium-doped fibers (EDBs), because the energy interval of this transition is always less than or equal to the energy interval corresponding to the pump absorption, the wavelength of the amplified signal light can only be greater than or equal to the pump light wavelength, and cannot amplify signal light with wavelengths shorter than the pump light. Therefore, conventional erbium-doped fibers can only provide gain for the longer wavelength signal light at a certain pump wavelength, and cannot simultaneously cover the communication band on the shorter wavelength side of the pump light. In addition, conventional erbium-doped fibers require high pump power to allow enough ions to transition to high energy levels, thereby achieving signal amplification. Therefore, to achieve sufficient gain, a high-power pump source is usually required, which increases system power consumption and cost.
[0016] Based on this, this application provides an active optical fiber whose core is doped with 0.1~0.5 wt.% Er, 8.0~10 wt.% Al, and 10~15 wt.% P. By simultaneously introducing erbium (Er), aluminum (Al), and phosphorus (P) elements into the core of the active optical fiber and precisely controlling the doping ratio of each element, an Er-Al-P multi-doped synergistic optical fiber system is formed. In this system, aluminum and phosphorus ions act together on the coordination field around erbium ions, altering the local crystal field environment of erbium ions. This causes Stark splitting and broadening of the erbium ion energy levels, thereby effectively controlling the metastable state of erbium ions. 4 I 13 / 2 ) and ground state ( 4 I 15 / 2 The particle population distribution on each Stark sublevel within the energy level. Based on the modulation of the energy level structure, when the above active fiber is excited by pump light with a wavelength in the C-band (1525~1545nm), it is in the ground state ( 4 I 15 / 2 The electrons at the top are pumped to a metastable state. 4 I 13 / 2 The top and bottom of the metastable state allow electrons pumped to the bottom to relax further to lower Stark levels in the metastable state via phonon-assisted relaxation, thereby amplifying the long-wavelength L-band (1575~1580 nm) signal light. Simultaneously, the co-doping of aluminum and phosphorus broadens the metastable energy levels, allowing electrons at the bottom of the metastable state to absorb a second C-band pump photon and undergo excited-state absorption transitions to higher excited states. 4 I 11 / 2 The erbium-doped fiber enters a state at the top Stark sublevel, which then relaxes nonradiatively back to the metastable state. This significantly increases the population at the top metastable sublevel, enabling the active fiber to achieve population inversion and signal amplification in the short-wavelength S-band (1480-1500 nm). Furthermore, the introduction of phosphorus reduces the phonon energy of the fiber matrix material, decreases the probability of nonradiative transitions, and improves the luminescence quantum efficiency of erbium. Through the synergistic doping of erbium (Er), aluminum (Al), and phosphorus (P) within a specific ratio range, this embodiment overcomes the limitation of traditional erbium-doped fibers that can only amplify signal light with wavelengths longer than the pump light wavelength. It achieves simultaneous gain capability for both short-wavelength S-band and long-wavelength L-band signal light under C-band pump light excitation, effectively improving the gain-bandwidth product and pump light utilization efficiency of the active fiber.
[0017] The first aspect of this application provides an active optical fiber, wherein the core of the active optical fiber is doped with 0.1~0.5 wt.% Er, 8.0~10 wt.% Al and 10~15 wt.% P.
[0018] In one feasible embodiment, the fiber core is also doped with 3 to 5 wt.% Ge.
[0019] Optionally, the amount of Er doping in the fiber core can be: 0.1 wt.%, 0.15 wt.%, 0.2 wt.%, 0.25 wt.%, 0.3 wt.%, 0.35 wt.%, 0.4 wt.%, 0.45 wt.%, 0.5 wt.%, etc.
[0020] Optionally, the Al doping amount in the fiber core can be: 8 wt.%, 8.5 wt.%, 9 wt.%, 9.5 wt.%, 10 wt.%, etc.
[0021] Optionally, the doping amount of P in the fiber core can be: 10 wt.%, 10.5 wt.%, 11 wt.%, 11.5 wt.%, 12 wt.%, 12.5 wt.%, 13 wt.%, 13.5 wt.%, 14 wt.%, 14.5 wt.%, 15 wt.%, etc.
[0022] Optionally, the amount of Ge doped in the fiber core can be: 3 wt.%, 3.5 wt.%, 4 wt.%, 4.5 wt.%, 5 wt.%, etc.
[0023] Optionally, the fiber core, located in the innermost layer of the active optical fiber, is composed of a glass material (e.g., quartz glass) doped with, for example, Er, Al, P and Ge.
[0024] In one feasible embodiment, reference is made to Figure 1 Based on the modulation of energy level structure, when the above-mentioned active optical fiber is excited by pump light with a wavelength in the C-band (1525~1545nm), it is in the ground state ( 4 I 15 / 2 The electrons at the top are pumped to a metastable state. 4 I 13 / 2 The top and bottom of the metastable state allow electrons pumped to the bottom to relax further to lower Stark levels in the metastable state via phonon-assisted relaxation, thereby amplifying the long-wavelength L-band (1575~1580 nm) signal light. Simultaneously, the co-doping of aluminum and phosphorus broadens the metastable energy levels, allowing electrons at the bottom of the metastable state to absorb a second C-band pump photon and undergo excited-state absorption transitions to higher excited states. 4 I 11 / 2The erbium-doped fiber enters a metastable state by nonradiative relaxation and returns to the top Stark sublevel, significantly increasing the population at the top metastable sublevel. This enables the active fiber to achieve population inversion and signal amplification in the short-wavelength S-band (1480–1500 nm). Furthermore, germanium doping effectively increases the refractive index of the fiber core, ensuring effective confinement and low-loss transmission of the optical signal within the core under the aforementioned multi-doped system. The introduction of phosphorus also reduces the phonon energy of the fiber matrix material, decreasing the probability of nonradiative transitions and improving the luminescence quantum efficiency of erbium.
[0025] It should be noted that under C-band pump excitation, some electrons at the bottom of the metastable state will spontaneously transition back to the ground state and generate background loss. At the same time, electrons that have returned to the ground state may also reabsorb pump photons and undergo reabsorption. Although these effects will reduce pump efficiency, the embodiments of this application effectively suppress the adverse effects of the above-mentioned loss mechanism by adjusting the doping ratio of each element.
[0026] Optionally, active optical fiber can be applied to various passive optical network (PON) systems, suitable for deployment scenarios such as urban residential broadband access, commercial building leased lines, industrial park networking, and rural broadband coverage.
[0027] Optionally, active optical fibers can be adapted to complex topology environments with multi-level splitting (such as a combination of primary and secondary splitting), for example, in a link scenario where an optical line terminal (OLT) is connected to an optical network terminal (ONT) via a primary splitter and a secondary splitter.
[0028] Optionally, active optical fibers can be used in optical fiber communication systems, which can adopt a point-to-multipoint (P2MP) topology architecture, covering PON technologies such as Gigabit-Capable PON (GPON), Ethernet PON (EPON), and 10-Gigabit-Capable PON (XG-PON) and its symmetrical variant (XGS-PON).
[0029] Optionally, the 480–1490 nm band is the downlink signal wavelength specified in the GPON standard, used to transmit data from the central office OLT to the user-end ONU (Optical Network Unit) / ONT. In a GPON system, the OLT transmits a 1480–1500 nm downlink optical signal, which is distributed to each user end via the ODN (Optical Distribution Network). As the number of splitting stages and the splitting ratio increase in the ODN, the power of the 1480–1500 nm signal is significantly weakened. In this embodiment, the active optical fiber provides amplification gain for the signal light in this band to compensate for the insertion loss introduced by the ODN and improve the coverage capability of the GPON system.
[0030] Optionally, the 1575-1580 nm band is the downlink signal wavelength specified in the XGS-PON standard, used to transmit data from the central office OLT to the user-end ONU / ONT. XGS-PON systems using 1577 nm downlink optical signals also face ODN power distribution loss issues. In this embodiment, the active optical fiber simultaneously provides amplification gain for this band of signal light to compensate for transmission losses in the ODN of the XGS-PON system.
[0031] In this embodiment, by simultaneously introducing erbium (Er), aluminum (Al), phosphorus (P), and germanium (Ge) elements into the core of an active optical fiber and precisely controlling the doping ratio of each element, an Er-Al-P-Ge multi-doped synergistic optical fiber system is formed. In this system, aluminum and phosphorus ions act together on the coordination field around erbium ions, altering the local crystal field environment of the erbium ions. This causes Stark splitting and broadening of the erbium ion energy levels, effectively regulating the metastable state of the erbium ions. 4 I 13 / 2 ) and ground state ( 4 I 15 / 2 The particle population distribution on each Stark sublevel within the energy level. This application's embodiments overcome the limitation of traditional erbium-doped fibers that can only amplify signal light with wavelengths longer than the pump light wavelength. It achieves simultaneous gain capability for both short-wavelength S-band and long-wavelength L-band signal light under C-band pump light excitation, while maintaining a high gain coefficient and low insertion loss, effectively improving the gain-bandwidth product and pump light utilization efficiency of the active fiber.
[0032] In one feasible implementation, refer to Figure 2 The active optical fiber 10 includes, from the inside out, the following components: fiber core 11, inner cladding 12, cladding 13 and coating layer 14.
[0033] Optionally, the inner cladding 12 covers the outer side of the fiber core 11 and is made of a glass material (e.g., fluorine-doped silica glass) with a refractive index lower than that of the fiber core 11. The inner cladding 12 is used to form an optical interface with a refractive index lower than that of the fiber core 11 on the periphery of the fiber core 11, thereby forming a refractive index-guided waveguide structure to confine the signal light and pump light to propagate within the fiber core 11. At the same time, the inner cladding 12 can also form a good interfacial bond with the fiber core 11 during high-temperature sintering, which is beneficial to reducing the background loss of the active fiber 10.
[0034] In one feasible embodiment, the refractive index difference between the core 11 and the cladding 13 is 0.0045~0.007.
[0035] Optionally, the refractive index difference between the core 11 and the cladding 13 is 0.0045, 0.005, 0.0055, 0.006, 0.0065, 0.007, etc.
[0036] Optionally, the cladding 13 covers the outside of the inner cladding 12 and is made of a glass material (e.g., pure quartz glass or fluorine-doped quartz glass). The cladding 13 provides the necessary mechanical strength and structural support for the active optical fiber 10, protecting the fiber core 11 and the inner cladding 12 from damage by external stress; at the same time, the cladding 13 and the inner cladding 12 together constitute the waveguide structure of the active optical fiber 10, further confining the propagation of the optical field in the fiber core 11.
[0037] Optionally, the coating layer 14 covers the outside of the cladding layer 13 and is composed of a polymer material (e.g., polyimide, acrylic resin, or silicone rubber). The coating layer 14 provides physical protection for the active optical fiber 10, isolating it from moisture, mechanical friction, and chemical corrosion in the external environment, enhancing the mechanical strength and bending resistance of the active optical fiber 10, and ensuring the reliability and stability of the active optical fiber 10 during cabling, wiring, and long-term use.
[0038] In one feasible embodiment, the diameter of the fiber core 11 is 4~8 μm.
[0039] Optionally, the diameter of the fiber core 11 can be 4 μm, 4.5 μm, 5 μm, 5.5 μm, 6 μm, 6.5 μm, 7 μm, 7.5 μm, 8 μm, etc.
[0040] In one feasible embodiment, when the diameter of the fiber core 11 is within a narrow range, the transmission mode field cross-section of the pump light (e.g., C-band 1525~1545nm pump light) is significantly compressed. Even with a low pump power, the pump light can still generate a high power density per unit area within the fiber core 11. This high power density means a significant increase in the number of pump photons available for erbium ion absorption per unit volume, thereby achieving a sufficiently high population inversion within a shorter length of the fiber core 11. This effectively excites ground-state particles to a metastable state, providing ample gain medium for subsequent signal amplification. Meanwhile, the high pump power density also enhances the triggering efficiency of the excited-state absorption process, enabling electrons in the metastable state to absorb the second C-band pump photon and transition to a higher excited state. Subsequently, they return to the top Stark sublevel of the metastable state through nonradiative relaxation, thereby significantly increasing the particle population at the top sublevel of the metastable state. This allows the active fiber 10 to also achieve population inversion and signal amplification in the short-wavelength S-band (1480~1500nm).
[0041] Optionally, the length of the active optical fiber can be 150 to 200 mm. For example, the length of the active optical fiber can be 150 mm, 160 mm, 170 mm, 180 mm, 190 mm, 200 mm, etc.
[0042] In this embodiment, a finer core diameter (4~8 μm) can effectively increase the interaction density between the pump light and the gain medium (i.e., the erbium ions doped in the core) under low pump power conditions, thereby avoiding insufficient amplification gain caused by the dispersion of pump light power in a thicker core.
[0043] In one feasible embodiment, the small-signal gain coefficient of the active optical fiber for signal light in the 1480~1500 nm band is 3.3~6.6 dB / m; the absorption coefficient of the active optical fiber at the 1480~1500 nm wavelength is <10 dB / m.
[0044] Optionally, the small-signal gain coefficient of the active optical fiber for signal light in the 1480~1500 nm band is 3.3 dB / m, 3.5 dB / m, 3.6 dB / m, 3.8 dB / m, 4 dB / m, 4.2 dB / m, 4.4 dB / m, 4.6 dB / m, 4.8 dB / m, 5 dB / m, 5.2 dB / m, 5.4 dB / m, 5.6 dB / m, 5.8 dB / m, 6 dB / m, 6.2 dB / m, 6.4 dB / m, 6.5 dB / m, 6.6 dB / m, etc.
[0045] Optionally, the gain coefficient reflects the amplification capability of the active optical fiber per unit length of signal light in a specific wavelength band, and its value is determined by the erbium ion doping concentration in the fiber core, the aluminum / phosphorus / germanium co-doping ratio, the fiber core diameter, etc.
[0046] In one feasible embodiment, when weak signal light with wavelength in the range of 1480 to 1500 nm passes through an active optical fiber of a unit length (1 m), the power of the signal light can be increased by 3.3 to 6.6 dB.
[0047] In this embodiment, the Stark splitting and broadening of the erbium ion energy level is modulated through an Er-Al-P multi-doped synergistic system, making the 1480–1500 nm wavelength band a positive gain region, achieving a gain coefficient of 3.3–6.6 dB / m. Simultaneously, the absorption coefficient at the corresponding 1490 nm wavelength in this band is controlled below 10 dB / m, ensuring that the loss due to ground-state absorption when the signal light passes through the optical fiber is much less than the gain, thus obtaining a positive net gain; that is, the signal light is ultimately effectively amplified rather than attenuated.
[0048] In one feasible embodiment, the small-signal gain coefficient of the active optical fiber for signal light in the 1575~1580 nm band is 2.0~6.6 dB / m; the absorption coefficient of the active optical fiber at the 1575~1580 nm wavelength is <3.5 dB / m.
[0049] Optionally, the small-signal gain coefficient of the active optical fiber for signal light in the 1575~1580 nm band is 2.0 dB / m, 2.1 dB / m, 2.2 dB / m, 2.4 dB / m, 2.6 dB / m, 2.8 dB / m, 3.0 dB / m, 3.1 dB / m, 3.3 dB / m, 3.5 dB / m, 3.6 dB / m, 3.8 dB / m, 4 dB / m, 4.2 dB / m, 4.4 dB / m, 4.6 dB / m, 4.8 dB / m, 5 dB / m, 5.2 dB / m, 5.4 dB / m, 5.6 dB / m, 5.8 dB / m, 6 dB / m, 6.2 dB / m, 6.4 dB / m, 6.5 dB / m, 6.6 dB / m, etc.
[0050] In one feasible embodiment, when weak signal light with wavelength in the range of 1575 to 1580 nm passes through an active optical fiber of a unit length (1 m), the power of the signal light can be increased by 2.0 to 6.6 dB.
[0051] In this embodiment, the Stark splitting and broadening of erbium ion energy levels are controlled through an Er-Al-P multi-doped synergistic system. When the C-band pump light excites electrons from the top of the ground state to the bottom of the metastable state, these electrons relax to a lower Stark sublevel in the metastable state via phonon-assisted relaxation, thereby establishing population inversion and generating stimulated emission in the 1575–1580 nm band. This band becomes a positive gain region, achieving a gain coefficient of 2.0–6.6 dB / m. Simultaneously, the absorption coefficient in this band is controlled below 3.5 dB / m, lower than the gain coefficient, ensuring that the loss due to ground state absorption when the signal light passes through the optical fiber is much less than the gain, thus obtaining a positive net gain. In other words, the signal light is ultimately effectively amplified rather than attenuated.
[0052] In one feasible embodiment, the active optical fiber has an absorption coefficient of 20~30 dB / m at a wavelength of 1535 nm.
[0053] Optionally, the active optical fiber has an absorption coefficient of 20 dB / m, 21 dB / m, 22 dB / m, 23 dB / m, 24 dB / m, 25 dB / m, 26 dB / m, 27 dB / m, 28 dB / m, 29 dB / m, 30 dB / m, etc. at a wavelength of 1535 nm.
[0054] Optionally, the absorption coefficient is a parameter characterizing the ability of an optical fiber to absorb optical signals of a specific wavelength. It represents the number of decibels by which the optical power is attenuated by the absorption of erbium ions in the fiber core when an optical signal of a specific wavelength passes through a unit length of optical fiber.
[0055] In this embodiment, the active optical fiber has an absorption coefficient of 25~30 dB / m at a wavelength of 1535 nm, and the core diameter is 4~8 μm. This ensures that the weak pump light can be uniformly and moderately absorbed over an optical fiber length of 150~200 mm, thereby forming a relatively uniform population inversion distribution along the entire fiber length, providing the necessary gain medium conditions for subsequent dual-band signal amplification.
[0056] Optionally, the core of the active optical fiber is doped with 0.1~0.5 wt.% Er, 8.0~10 wt.% Al, 10~15 wt.% P and 3~5 wt.% Ge.
[0057] In one feasible embodiment, under pump light excitation in the 1525~1545 nm band with a pump power ≥-15 dBm, the small-signal gain coefficient of the active optical fiber for signal light in the 1480~1500 nm band is 3.3~6.6 dB / m, and the absorption coefficient is <10 dB / m; the small-signal gain coefficient of the active optical fiber for signal light in the 1575~1580 nm band is 2.0~6.6 dB / m, and the absorption coefficient is <3.5 dB / m.
[0058] Optionally, refer to Figure 4 The active optical fiber in this application embodiment can achieve a predetermined power perturbation value under pump light excitation in the 1525~1545 nm band, and generate power perturbation gain in both the 1480~1500 nm and 1575~1581 nm bands, while the insertion loss is controlled within an acceptable range.
[0059] In this embodiment, the 1525–1545 nm band corresponds to the C-band pump light wavelength range. This band matches the erbium ion absorption peak and can effectively excite ground-state particles to a metastable state, with a pump power ≥ -15 dBm, indicating that the active fiber of this embodiment can operate under weak pump conditions. Signal light with wavelengths in the 1480–1500 nm range, after passing through the active fiber, exhibits a small-signal gain coefficient of 3.3–6.6 dB / m per meter, while the absorption coefficient corresponding to this band is less than 10 dB / m, indicating that the active fiber has high intrinsic amplification capability in this band and low loss due to signal light absorption by the ground state. Furthermore, for signal light in the 1575–1580 nm band, the active fiber exhibits a small-signal gain coefficient of 2.0–6.6 dB / m per meter and an absorption coefficient less than 3.5 dB / m, indicating that the active fiber also possesses intrinsic amplification capability in the L-band, and its absorption loss is even lower due to its distance from the erbium ion absorption peak. The above data verifies that the active optical fiber in this application embodiment can effectively amplify both the short-wavelength S-band and the long-wavelength L-band signal light under weak pumping excitation in the C-band, while also maintaining low insertion loss.
[0060] In one feasible implementation, refer to Figure 2 The diameter of the inner cladding 12 is 8~10 μm. For example, the diameter of the inner cladding 12 is 8 μm, 8.5 μm, 9 μm, 9.5 μm, 10 μm, etc.
[0061] In one feasible implementation, refer to Figure 2 The diameter of the cladding 13 is 120~130 μm. For example, the diameter of the cladding 13 is 120 μm, 125 μm, 130 μm, etc.
[0062] In one feasible implementation, refer to Figure 2 The thickness of the coating layer 14 is 125~250 μm. For example, the thickness of the coating layer 14 is 125 μm, 130 μm, 150 μm, 200 μm, 250 μm, etc.
[0063] In this embodiment, the diameter of the inner cladding 12 needs to be sufficient to effectively confine the optical field to the fiber core 11 and prevent leakage to the cladding 13, but it should not be too thick to maintain the bending flexibility of the active optical fiber 10; while the cladding 13 needs to provide sufficient mechanical strength to protect the fiber core 11, while avoiding excessive increase in material cost and bending stiffness; the thickness of the coating layer 14 needs to be sufficient to isolate moisture and buffer external stress to prevent the generation of microcracks; the three work together to achieve a balance between optical field confinement, mechanical strength and bending resistance.
[0064] Optionally, refer to Figure 3 The fabrication method of active optical fiber includes the following steps: First, using a high-purity quartz tube as a substrate, a porous material (e.g., a SiO2 porous layer) is deposited on the inner wall of the quartz tube using MCVD (chemical vapor deposition) as a carrier for subsequent doping. During the deposition process, halide reaction gases such as SiCl4 and GeCl4 are introduced into the quartz tube and heated in stages by an external oxyhydrogen flame (temperatures reach 1400~2100℃), causing the reaction gases to undergo hydrolysis / oxidation reactions at high temperatures, generating oxide particles such as SiO2 and GeO2, which are deposited on the inner wall of the quartz tube to form a porous layer. Second, atomic layer deposition (ALD) or solution doping technology is used to introduce dopant materials (including elements such as erbium, aluminum, phosphorus, and germanium) into the above-mentioned porous layer. ALD (Alternating Layer Deposition) technology achieves atomically precise layer-by-layer deposition by alternately and pulsedly introducing two or more reactive precursors into a vacuum reaction chamber, utilizing self-limiting surface reactions. Each precursor undergoes a single-atom-layer self-limiting reaction with the substrate surface (i.e., the reaction stops once the surface is saturated). Unreacted gases and byproducts are removed by purging with inert gas between precursor pulses. Through a cyclical process of precursor A pulse-purging-precursor B pulse-purging, uniform and high-precision doping of rare earth ions (such as erbium ions) and co-doped ions (such as aluminum, phosphorus, and germanium ions) is achieved in the porous layer. Subsequently, the doped porous layer is subjected to high-temperature semi-vitrification using the MCVD (Metal-Containment Variability Deposition) process, partially densifying the porous layer to form a semi-vitrified doped layer. Based on this, a quartz core layer is deposited again using the MCVD process, followed by high-temperature vitrification and shrinkage treatment, gradually shrinking the quartz tube into a solid optical fiber preform. Finally, the prepared optical fiber preform is placed in a drawing tower and drawn into an active optical fiber with a core diameter of 4~8 μm at high temperature. During the drawing process, a polymer coating layer is simultaneously applied, and finally an active optical fiber is obtained with the core, inner cladding, outer cladding and coating layer arranged from the inside out.
[0065] Optionally, the doping thickness of the fiber core is 0.01~10.0 μm.
[0066] Alternatively, the preparation method for doping rare earth ions in the fiber core can be atomic layer deposition doping technology and / or solution doping technology.
[0067] Optionally, the above-described method for preparing active optical fibers is merely an example, and other methods can also be used to prepare the active optical fibers of the embodiments of this application.
[0068] The second aspect of this application provides a communication device. The communication device includes the active optical fiber provided in the first aspect of this application. The function of the communication device of the second aspect of this application can be referred to the function of the active optical fiber provided in the first aspect of this application. Other technical features of this communication device are the same as those disclosed in the methods of the above embodiments, and will not be repeated here.
[0069] Optionally, the communication equipment can be any one of OLT, ONU, ONT, optical splitter, optical amplifier or optical receiver assembly.
[0070] Optionally, when the communication equipment is an OLT, it is deployed in the operator's equipment room and has the ability to transmit and receive optical signals, detect optical power and process data. It also needs to support linkage control with remote pump light source, be able to identify changes in signal optical power and match the mapping relationship of splitter ports, and be compatible with the service wavelengths of existing PON systems.
[0071] Optionally, when the communication equipment is an ODN, it is a passive optical distribution network, including 1 to N levels of optical splitters (the splitting ratio supports 1:M configuration, where M is an integer, covering mainstream specifications such as 1:2, 1:4, 1:8, 1:9, 1:16, 1:32, and 1:64), single-mode optical fibers, optical couplers, optical fiber connectors, wavelength division multiplexers, and other passive devices; wherein, all output ports of each level of optical splitter need to be reserved for installation positions to deploy the power conversion components of this invention, and the ODN link transmission distance needs to meet the PON standard.
[0072] Optionally, when the communication equipment is an ONU or ONT, it is an existing or newly added PON terminal equipment that does not require any hardware modification or software upgrade. It only needs to have the ability to receive PON downlink signal light normally and to feed back the received optical power data to the OLT (or indirectly obtain power data through the OLT-side detection terminal).
[0073] The following describes embodiments of this application. The embodiments described below are exemplary and are only used to explain this application, and should not be construed as limiting this application. Where specific techniques or conditions are not specified in the embodiments, they are performed according to the techniques or conditions described in the literature in this field or according to the product instructions. Reagents or instruments used, unless otherwise specified, are all conventional products that can be obtained commercially.
[0074] Example The first step involves depositing a loose layer of fluorine-doped SiO2 on the inner wall of a quartz glass tube using chemical vapor deposition (MCVD). During the deposition process, the SiCl4 flow rate is controlled at 1.3 g / min, the CF4 flow rate at 80 sccm, the O2 flow rate at 2.6 L / min, and the heating temperature is controlled at 1450℃. The second step involves introducing Er₂O₃ and Al₂O₃ into the porous layer of the quartz glass tube using atomic layer deposition (ALD) doping technology. During the ALD doping process, the reaction chamber temperature is controlled at 360℃, the Er precursor pulse time is 0.8 s, the Al precursor pulse time is 0.6 s, the purge time is 18 s, and the number of cycles is 500–2000. The doping amounts of Er₂O₃ and Al₂O₃ are controlled by adjusting the number of cycles. Subsequently, MCVD technology is used to further introduce P₂O₅ and GeO₂ into the porous layer. The flow rates of POCl₃ are controlled at 0.1–0.3 g / min, GeCl₄ at 0.2–0.5 g / min, and O₂ at 1–2 g / min. The deposition rate was L / min, and the deposition temperature was 1550℃. Then, the doped loose layer was sintered at high temperature into a transparent quartz preform using the MCVD process, wherein the heating rate was controlled at 3℃ / min, the sintering temperature was 2000℃, and the sintering time was 1.3h.
[0075] The third step involves placing a quartz preform in a drawing tower and drawing it into an optical fiber at a high temperature of 2000℃. During the drawing process, the drawing speed is controlled at 50~60 m / min, and an inner coating layer and an outer coating layer are applied sequentially. The coating layer material is a polyacrylic resin. After drawing and coating, an active optical fiber (i.e., erbium-doped fiber) is finally obtained, which consists of, from the inside out: a core, a cladding, an inner cladding, and a coating layer. The core diameter is 7.0 μm, the cladding diameter is 9.0 μm, the inner cladding diameter is 125.0 μm, and the coating layer thickness is 245.0 μm.
[0076] Using the above preparation method, optical fiber samples with different Er / Al / P / Ge doping concentrations and ratios can be obtained. The only difference between the samples is the doping ratio of Er2O3 and Al2O3 and the amount of P2O5 and GeO2 introduced. All other preparation conditions are kept the same. The absorption loss data of each active optical fiber sample at a wavelength of 1530 nm are shown in Table 1 below.
[0077] Table 1
[0078] As shown in Table 1, the peak absorption coefficient of active optical fibers can be effectively controlled by adjusting the doping ratios of Er, Al, Ge, and P. This allows the fiber to achieve a predetermined power perturbation value under pump light excitation in the 1525–1545 nm band, and simultaneously generate power perturbation gain in both the 1480–1500 nm and 1575–1581 nm bands, while keeping the insertion loss within an acceptable range. Furthermore, controlling the doping ratio of Al and Ge effectively adjusts the center wavelength position corresponding to the peak absorption coefficient of the fiber. This active optical fiber can be used as an active gain medium in a beam splitter, and combined with various distributed sensing technologies, it can effectively distinguish and identify the characteristics of each branch fiber link in the beam splitter.
[0079] Furthermore, through Figure 5 The test optical path shown measures the signal light gain and insertion loss of the active fiber (i.e., erbium-doped fiber). The insertion loss is represented by the power difference (dBm) of the 1490nm / 1580nm dual-wavelength laser before and after being introduced into the active fiber. The power change of the optical signal power after being excited by pump light at 1530nm~1540nm after being introduced into the active erbium-doped fiber is represented by the power perturbation gain. The insertion loss and power perturbation gain at the corresponding signal light wavelengths for different doping element ratios are shown in Table 2 below. Table 2
[0080] As shown in Table 2 above, by rationally adjusting the doping ratios of Er, Al, Ge, and P, active optical fibers can simultaneously generate power perturbation gain for signal light in the 1480–1500 nm and 1575–1581 nm bands under C-band pump light excitation in the 1525–1545 nm band, while keeping the insertion loss at a low level. Specifically, at 1490 nm, all samples exhibit positive power amplification gain with insertion loss within an acceptable range; at 1578 nm, all samples also exhibit positive power amplification gain with even lower insertion loss. These results demonstrate that by introducing an Er-Al-P-Ge multi-element doping synergistic system into the fiber core and rationally controlling the doping ratios of each element, the absorption coefficient and center wavelength position of the optical fiber at the peak absorption wavelength can be effectively controlled. This allows the optical fiber to simultaneously achieve gain amplification for both the short-wavelength S-band and long-wavelength L-band signal light under weak C-band pump conditions, while maintaining low insertion loss.
[0081] It should be noted that this application is not limited to the above-described embodiments. The above embodiments are merely examples, and any embodiments with the same structure and effect as the technical concept within the scope of this application are included in the technical scope of this application. Furthermore, various modifications that can be conceived by those skilled in the art to the embodiments, and other ways of constructing by combining some of the constituent elements of the embodiments, without departing from the spirit of this application, are also included in the scope of this application.
Claims
1. An active optical fiber, characterized in that, The active optical fiber core is doped with 0.1~0.5 wt.% Er, 8.0~10 wt.% Al and 10~15 wt.% P.
2. The active optical fiber as described in claim 1, characterized in that, The diameter of the fiber core is 4~8 μm.
3. The active optical fiber as described in claim 1, characterized in that, The active optical fiber has a small-signal gain coefficient of 3.3~6.6dB / m for signal light in the 1480~1500 nm band; The active optical fiber has an absorption coefficient of <10 dB / m at wavelengths of 1480~1500 nm.
4. The active optical fiber as described in claim 1, characterized in that, The active optical fiber has a small-signal gain coefficient of 2.0~6.6 dB / m for signal light in the 1575~1580 nm band; The active optical fiber has an absorption coefficient of <3.5 dB / m at a wavelength of 1575~1580 nm.
5. The active optical fiber as described in claim 1, characterized in that, The active optical fiber has an absorption coefficient of 20-30 dB / m in the 1525-1545 nm band.
6. The active optical fiber as described in claim 1, characterized in that, The fiber core is also doped with 3-5 wt.% Ge.
7. The active optical fiber as described in claim 1, characterized in that, Under pump light excitation in the 1525~1545 nm band with a pump power ≥ -15 dBm, the active optical fiber has a small-signal gain coefficient of 3.3~6.6 dB / m and an absorption coefficient of <10 dB / m for signal light in the 1480~1500 nm band; the active optical fiber has a small-signal gain coefficient of 2.0~6.6 dB / m and an absorption coefficient of <3.5 dB / m for signal light in the 1575~1580 nm band.
8. The active optical fiber as described in any one of claims 1 to 7, characterized in that, The active optical fiber comprises, from the inside out, a core, an inner cladding, a cladding layer, and a coating layer.
9. The active optical fiber as described in claim 8, characterized in that, The refractive index difference between the fiber core and the cladding is 0.0045~0.
007.
10. The active optical fiber as described in claim 8, characterized in that, The diameter of the inner cladding is 8~10 μm; And / or, the diameter of the cladding is 120~130 μm; And / or, the thickness of the coating layer is 125~250 μm.
11. A communication device, characterized in that, The communication device includes an active optical fiber as described in any one of claims 1 to 10.