A component screening and development design method for functional polymer coatings
By using module division and puzzle matching logic to screen polymer coating components, the problems of numerous experiments, long cycles, and omissions in combinations in traditional methods are solved, achieving efficient and accurate component screening, reducing costs and improving adaptability.
Patent Information
- Application Number
- CN202611370853.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-04
- Publication Date
- 2026-11-17
AI Technical Summary
Traditional methods for screening components of functional polymer coatings involve numerous experiments, long cycles, high costs, and are prone to missing optimal combinations. They also lack prior assessment of the compatibility between components, leading to a large number of blind tests.
By employing a modular division and jigsaw puzzle matching logic, the coating components are divided into basic, functional, and auxiliary groups. Through pairwise matching of modules and visual compatibility scoring, the component combination with the best compatibility is quickly selected. A three-dimensional compatibility matrix and heat map are used for visualization to ensure the overall compatibility of candidate formulations.
It significantly reduces the number of experiments, shortens the development cycle, lowers R&D costs, improves the accuracy and efficiency of screening results, and ensures the overall compatibility between components.
Smart Images

Figure CN123120149A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of functional polymer materials technology, specifically relating to a method for screening and developing functional polymer coating components. Background Technology
[0002] Functional polymer coatings are a class of coating materials with special physicochemical properties, widely used in various industrial fields such as corrosion resistance, wear resistance, high temperature resistance, insulation, and antibacterial properties. The performance of the coating is mainly determined by its components and the interactions between them; therefore, component selection is a core step in the development of functional polymer coatings.
[0003] Traditional coating component screening methods generally adopt a "single variable first, then combination verification" approach. This approach first fixes all other components and changes only the type or amount of one component to screen for the optimal option. After all individual components have been screened, the optimal single component is then combined for verification. This method has the following significant drawbacks: First, the number of experiments is high, the development cycle is long, and the R&D cost is high. When the coating contains multiple components and each component has multiple alternatives, the number of experiments increases exponentially. For example, when the coating contains 4 resins, 4 curing agents, and 4 additives, screening for a single variable alone requires 12 experiments, and subsequent full combination validation experiments require 64 experiments, for a total of more than 70 experiments.
[0004] Second, it's easy to miss the truly optimal combination. Traditional methods assume no interaction between components, but in reality, there are complex synergistic or antagonistic effects between resins, curing agents, and additives. The optimal single component selected by a single variable may not necessarily form the best-performing coating system when combined.
[0005] Third, the lack of prior assessment of the compatibility between components leads to a large number of blind tests. Traditional methods cannot predict which components are compatible and which conflict with each other before conducting combination validation, so many experiments are invalid and a lot of human and material resources are wasted. Summary of the Invention
[0006] The purpose of this invention is to address the aforementioned shortcomings of existing technologies by providing a method for screening and developing functional polymer coating components. This method simulates a "puzzle matching" logic, dividing the coating components into three independent and functionally complementary modules. Through pairwise matching of modules and visual comparison, it quickly screens out the optimal component combination, effectively solving the problems of traditional screening methods involving numerous experiments, long cycles, and the tendency to miss the optimal combination.
[0007] To address the aforementioned technical problems, this invention provides the following technical solution: a method for screening and developing functional polymer coating components, comprising the following steps: S1 Module Division and Candidate Library Construction: All components of the functional polymer coating are divided into three independent and functionally complementary modules according to a "puzzle matching" logic: the basic group, the functional group, and the auxiliary group. Within each module, 3-4 commonly used industrial candidates with broad performance coverage are selected to establish a standardized candidate component library.
[0008] Preliminary experiment of pairwise matching of S2 modules: The matching experiment between the two modules was carried out in the order of "basic group-functional group", "basic group-auxiliary group" and "functional group-auxiliary group" to determine the key adaptability index of each matching combination.
[0009] S3 Adaptability Scoring and Visualization: Standardize the key adaptability indicators for each pair of matching combinations, construct a three-dimensional adaptability matrix, and visualize it in the form of a heatmap to intuitively show the degree of adaptability between different module components.
[0010] S4 Optimal Combination Initial Screening: Based on the three-dimensional compatibility heatmap, the top 3 component pairs with the highest compatibility scores between each pair of modules are selected, and candidate coating formulations are obtained through cross-combination.
[0011] S5 Comprehensive Performance Verification and Optimization: Conduct comprehensive performance tests on all formulations in the candidate coating formulation set, and determine the final optimal combination of functional polymer coating components based on the test results.
[0012] Further, in step S1, the base group is the film-forming substance of the coating, selected from 3-4 types of epoxy resin, acrylic resin, polyurethane resin, and silicone resin. The functional group is the curing agent that determines the core performance of the coating, selected according to the type of resin in the base group, and selected from 3-4 types of amine curing agents, acid anhydride curing agents, isocyanate curing agents, and phenolic resin curing agents; among them, epoxy resin systems can be adapted to amine, acid anhydride, and phenolic resin curing agents; polyurethane resin systems are adapted to isocyanate curing agents; silicone resin systems are adapted to addition reaction curing agents; and acrylic resin systems can be adapted to amine and isocyanate curing agents. The auxiliary group is the additive that improves the processing and performance of the coating, selected from 3-4 types of leveling agents, defoamers, adhesion promoters, and weathering agents; the above four types of additives can be used in various base resin systems such as epoxy resin, acrylic resin, polyurethane resin, and silicone resin, only requiring adjustment of the specific grade according to the polarity of the system.
[0013] Further, in step S2, the key compatibility indicators determined in the "basic group-functional group" matching experiment include curing time, gel conversion rate, crosslinking density, and glass transition temperature. The key compatibility indicators determined in the "basic group-auxiliary group" matching experiment include compatibility, dispersion stability, and surface tension. The key compatibility indicators determined in the "functional group-auxiliary group" matching experiment include the effect of curing reactivity, storage stability, and side reaction rate.
[0014] For different types of functional coatings, the key compatibility indicators can be expanded accordingly: for insulating coatings, dielectric strength, volume resistivity, and breakdown voltage are added to the basic group-functional group matching indicators; for antibacterial coatings, antibacterial rate, antibacterial durability, and mildew resistance are added to the basic group-functional group matching indicators.
[0015] Furthermore, in step S2, each pairwise matching experiment was conducted using fixed ratios. Specifically, the mass ratio of the "basic group - functional group" was fixed at 100:(20~50), the mass ratio of the "basic group - auxiliary group" was fixed at 100:(0.5~5), and the mass ratio of the "functional group - auxiliary group" was fixed at 100:(1~10). Using fixed ratios eliminates the interference of ratio factors on the experimental results, allowing focus on evaluating the compatibility of the components themselves.
[0016] Furthermore, in step S3, the standardized score adopts a 0-10 point scale, where 10 points represents the best fit and 0 points represents no fit. For each key fit index, different weight coefficients are assigned according to their importance to the coating performance, and the comprehensive fit score of the pairwise matching combination is obtained by weighted calculation.
[0017] Furthermore, in step S3, the three coordinate axes of the three-dimensional adaptability matrix correspond to the candidate components of the basic group, functional group, and auxiliary group, respectively. The color intensity of each cell represents the overall adaptability score between the corresponding two components, with darker colors indicating better adaptability. The visualization of the heatmap allows R&D personnel to intuitively and quickly identify highly adaptable component pairs.
[0018] Further, in step S4, the cross-combination specifically involves: combining the top 3 component pairs in terms of compatibility between the "basic group and functional group," the top 3 component pairs in terms of compatibility between the "basic group and auxiliary group," and the top 3 component pairs in terms of compatibility between the "functional group and auxiliary group," retaining ternary component combinations that simultaneously meet the pairing requirements of all three groups: that is, in this combination, the basic component and functional component pairing is among the top 3 in the basic group-functional group, the basic component and auxiliary component pairing is among the top 3 in the basic group-auxiliary group, and the functional component and auxiliary component pairing is among the top 3 in the functional group-auxiliary group, forming a candidate coating formulation set. This screening logic ensures that the compatibility between any two components in the candidate formulation is at a high level, avoiding situations where two components are severely incompatible.
[0019] Furthermore, in step S5, the comprehensive performance test includes mechanical property testing, chemical corrosion resistance testing, weather resistance testing, and processing performance testing. Based on the requirements of different application scenarios, different weighting coefficients are assigned to the results of each performance test, and a weighted calculation is performed to obtain the comprehensive performance score for each candidate formulation. The formulation with the highest comprehensive performance score is the final optimal component combination.
[0020] Furthermore, step S5 is followed by step S6: optimizing the proportion of the determined optimal component combination, and using response surface methodology to fine-tune the mass ratio of each component based on the optimal component combination, thereby further improving the overall performance of the coating.
[0021] Furthermore, the method is applicable to the component screening and development design of any one of the functional polymer coatings, including anti-corrosion coatings, wear-resistant coatings, high-temperature resistant coatings, insulating coatings, and antibacterial coatings.
[0022] One or more technical solutions provided in the embodiments of this application have at least the following technical effects or advantages compared with the prior art: 1. It changes the cumbersome screening mode of "first single variable, then combination verification" and simulates the logic of "puzzle matching" to transform the complex multi-component screening problem into a pairwise matching problem between three modules, which greatly reduces the complexity of the problem.
[0023] 2. By pre-assessing the compatibility between components, blind testing is effectively avoided, significantly reducing the number of experiments. Compared with traditional methods, the total number of experiments in this invention is reduced by approximately 20% with 4 components and by more than 30% with 5 or more components, greatly shortening the development cycle and reducing R&D costs.
[0024] 3. The use of a three-dimensional compatibility matrix and heat map for visualization makes the compatibility relationship between components clear at a glance, facilitating quick judgment by R&D personnel and improving the intuitiveness and efficiency of the screening process.
[0025] 4. By employing three sets of pairings that simultaneously satisfy the first three cross-combination screening logic, the overall compatibility among the components in the candidate formulation is ensured, effectively avoiding the problem of missing the optimal combination that is common in traditional methods, and improving the accuracy of the screening results.
[0026] Other advantages, objectives and features of the invention will be set forth in part in the description which follows, and in part will be apparent to those skilled in the art from the following examination or study, or may be learned from the practice of the invention. Attached Figure Description
[0027] Figure 1 This is the overall timeline diagram of the functional polymer coating component screening and development design method of the present invention.
[0028] Figure 2 This is a schematic diagram of the visualization of the three-dimensional adaptability matrix and heat map of the present invention.
[0029] Figure 3 This is the optimal combination initial screening cross-combination logic diagram of the present invention.
[0030] Figure 4 This is a detailed flowchart of the comprehensive performance verification and proportion optimization of the present invention.
[0031] Figure 5 This is a comparison chart of the efficiency of the method of the present invention and traditional screening methods. Detailed Implementation
[0032] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0033] It should be noted that the terms "vertical," "horizontal," "up," "down," "left," "right," and similar expressions used in this article are for illustrative purposes only and do not represent the only possible implementation.
[0034] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains; the terminology used herein in the description of the invention is for the purpose of describing particular embodiments only and is not intended to limit the invention; the term "and / or" as used herein includes any and all combinations of one or more of the associated listed items.
[0035] The present invention will now be described in further detail with reference to the accompanying drawings and specific embodiments. Those skilled in the art should understand that the described embodiments are for illustrative purposes only and do not limit the scope of the invention in any way.
[0036] This embodiment uses the development of an epoxy resin-based heavy-duty anti-corrosion coating suitable for marine engineering steel structures as an example to illustrate the specific implementation process of the method of the present invention. Figure 1 As shown, the overall process of this invention includes six steps in sequence: module division and candidate library construction, module pairwise matching pre-experiment, adaptability scoring and visualization, initial screening of optimal combination, comprehensive performance verification and ratio optimization.
[0037] Step S1: Module Division and Candidate Library Construction All components of the heavy-duty anti-corrosion coating are divided into three independent and functionally complementary modules according to a "puzzle matching" logic: the base group, the functional group, and the auxiliary group. The base group, as the film-forming substance of the coating, determines the basic mechanical properties and chemical resistance of the coating; the functional group, as the curing agent, determines the crosslinking structure and core anti-corrosion properties of the coating; and the auxiliary group, as additives, improves the processing and performance of the coating.
[0038] Within each module, four commonly used industrial components with broad performance coverage were selected to establish a standardized component library. The basic group consisted of epoxy resin E-51, epoxy resin E-44, phenolic epoxy resin F-51, and silicone-modified epoxy resin; the functional group consisted of polyamide curing agent 650, isophorone diamine, methylhexahydrophthalic anhydride, and phenolic amine curing agent; and the auxiliary group consisted of BYK-333 leveling agent, BYK-066N defoamer, KH-550 adhesion promoter, and UV-327 weathering agent.
[0039] Step S2 Module Pairwise Matching Pre-Experiment Matching experiments between modules were conducted in the order of "basic group-functional group", "basic group-auxiliary group", and "functional group-auxiliary group". Each pairwise matching experiment used a fixed ratio to eliminate the interference of ratio factors on the experimental results and focus on evaluating the compatibility of the components themselves. Specifically, the mass ratio of the "basic group-functional group" was fixed at 100:20, 100:30, or 100:50; the mass ratio of the "basic group-auxiliary group" was fixed at 100:0.5, 100:1, or 100:5; and the mass ratio of the "functional group-auxiliary group" was fixed at 100:1, 100:5, or 100:10. All experiments were conducted under standard environmental conditions of 25℃ and 50% relative humidity.
[0040] For the "basic group-functional group" matching combination, four key compatibility indicators were measured: curing time, gel conversion rate, crosslinking density, and glass transition temperature. For the "basic group-auxiliary group" matching combination, three key compatibility indicators were measured: compatibility, dispersion stability, and surface tension. For the "functional group-auxiliary group" matching combination, three key compatibility indicators were measured: influence on curing reactivity, storage stability, and side reaction rate.
[0041] Step S3: Adaptability Scoring and Visualization A standardized scoring system of 0-10 was used to evaluate the key compatibility indicators for each pairwise matching combination, with 10 indicating the best compatibility and 0 indicating no compatibility. Different weighting coefficients were assigned to each indicator based on the performance requirements of heavy-duty anti-corrosion coatings for marine engineering. Weighting of indicators for the basic group and functional group: Curing time 0.2, gel conversion rate 0.3, crosslinking density 0.3, glass transition temperature 0.2. Weighting of indicators for the base group and auxiliary group: compatibility 0.4, dispersion stability 0.3, surface tension 0.3. Functional group - auxiliary group indicator weights: Influence on curing reaction activity 0.4, storage stability 0.3, incidence of side reactions 0.3. Based on the weighted calculation results, a comprehensive fit score is obtained for each pairwise matching combination. For example... Figure 2 As shown, a three-dimensional fit matrix is constructed with the basic group, functional group, and auxiliary group as the three coordinate axes. Each cell in the matrix corresponds to a matching combination of two specific components. The color intensity of the cell represents the overall fit score between the two components, with darker colors indicating better fit. The three-dimensional fit matrix is then converted into a heatmap for visualization, enabling R&D personnel to intuitively and quickly identify highly compatible component pairs.
[0042] Step S4: Initial screening of optimal combination Based on the 3D compatibility heatmap, the top 3 component pairs with the highest compatibility scores between any two modules were selected. In this embodiment, the top 3 component pairs are as follows: Basic Group - Top 3 Functional Groups: E-51 / 650, E-51 / Phenolic Amine, E-44 / 650 Top 3 in the Basic / Assistant Group: E-51 / BYK-333, E-51 / KH-550, E-44 / BYK-333 Functional Group - Auxiliary Group Top 3: 650 / BYK-333, 650 / KH-550, Phenolic Amine / BYK-333 like Figure 3As shown, the first three pairs of the above three groups are cross-combined, retaining the ternary component combinations that simultaneously meet the three pairing requirements: that is, the basic-functional pairing, the basic-auxiliary pairing, and the functional-auxiliary pairing are all in the top three. Combinations with any pairing not in the top three are eliminated, resulting in four candidate coating formulations: Formula 1: E-51 + 650 + BYK-333 (E-51 / 650 in the first 3, E-51 / BYK-333 in the first 3, 650 / BYK-333 in the first 3) Formula 2: E-51+650+KH-550 (E-51 / 650 in the first 3, E-51 / KH-550 in the first 3, 650 / KH-550 in the first 3) Formula 3: E-51 + Phenolic Amine + BYK-333 (E-51 / Phenolic Amine in the first 3, E-51 / BYK-333 in the first 3, Phenolic Amine / BYK-333 in the first 3) Formula 4: E-44 + 650 + BYK-333 (E-44 / 650 in the first 3, E-44 / BYK-333 in the first 3, 650 / BYK-333 in the first 3) This screening logic ensures that the compatibility between any two components in the candidate formulation is at a high level, avoiding the situation where two components are seriously incompatible, which may occur in traditional methods.
[0043] Step S5: Comprehensive Performance Verification and Proportion Optimization like Figure 4 As shown, comprehensive performance tests were conducted on all four formulations in the candidate coating formulation set. Test items included adhesion, impact strength, pencil hardness, salt spray resistance, acid and alkali resistance, and application performance. Based on the application requirements of heavy-duty anti-corrosion coatings for marine engineering, the following weighting coefficients were assigned to each test item: salt spray resistance 0.4, adhesion 0.2, impact strength 0.15, pencil hardness 0.1, acid and alkali resistance 0.1, and application performance 0.05.
[0044] Weighted calculation results showed that Formula 1 had the highest overall performance score and was determined as the initial optimal component combination. Response surface methodology was used to further optimize the component ratio of Formula 1. A three-factor, three-level response surface experimental design was conducted, using the mass ratio of E-51, 650, and BYK-333 as the independent variable and salt spray resistance time as the response value. Experimental results showed that the salt spray resistance time of the coating reached its maximum value when the mass ratio of E-51:650:BYK-333 was 100:32:0.8.
[0045] Performance test results A comprehensive performance test was conducted on the optimized final formula, and the results are as follows: Adhesion: Grade 1 (GB / T9286-1998) Impact strength: 50kg cm (GB / T1732-1993) Pencil hardness: 2H (GB / T6739-2006) Salt spray resistance time: 1200 hours (GB / T1771-2007) Resistance to 10% sulfuric acid solution: no change after 30 days (GB / T9274-1988) Resistance to 10% sodium hydroxide solution: no change after 30 days (GB / T9274-1988) Application performance: Good, excellent leveling properties, no obvious air bubbles or pinholes. Test results show that the heavy-duty anti-corrosion coating developed using the method of this invention has excellent comprehensive performance and fully meets the requirements for heavy-duty anti-corrosion application of marine engineering steel structures.
[0046] like Figure 5 As shown, the efficiency of the method of this invention is compared with that of the traditional screening method of "first single variable, then combined verification". The traditional method requires 12 single variable screening experiments and 64 combined verification experiments, for a total of 76 experiments; while the method of this invention only requires 48 pairwise matching pre-experiments and 4 comprehensive performance verification experiments, plus 9 response surface optimization experiments, for a total of 61 experiments. Compared with the traditional method, the total number of experiments of this invention is reduced by about 20%, and because a large number of ineffective blind tests are avoided, the actual development cycle is shortened by more than 40%, and the R&D cost is significantly reduced.
[0047] Extended explanation of different resin systems and coating types: For polyurethane resin systems, isocyanate-based curing agents should be prioritized for the functional group, while the auxiliary group can continue using the original additive system, only needing to be adjusted to polyurethane-compatible grades. For silicone resin systems, platinum chelate addition-type curing agents should be selected for the functional group, while silicone-specific leveling agents and defoamers should be used for the auxiliary group. For insulating coatings, dielectric strength, volume resistivity, and breakdown voltage should be added to the basic-functional group matching experiment, and the weighting coefficients should be adjusted accordingly. For antibacterial coatings, antibacterial rate, antibacterial durability, and mildew resistance should be added, and the weights can be set according to application requirements.
[0048] Although the present invention has been disclosed above with reference to preferred embodiments, it is not intended to limit the present invention. Anyone skilled in the art can make various modifications and alterations without departing from the spirit and scope of the present invention. Therefore, the scope of protection of the present invention should be determined by the claims.
Claims
1. A method for component screening and development design of functional polymer coatings, characterized in that, Includes the following steps: S1 Module Division and Candidate Library Construction: All components of the functional polymer coating are divided into three independent and functionally complementary modules according to the jigsaw puzzle matching logic, namely the basic group, the functional group and the auxiliary group; within each module, 3 to 4 commonly used industrial candidates with a wide performance coverage are selected to establish a standardized candidate component library. S2 module pairwise matching pre-experiment: The pairwise matching experiments between modules were carried out in the order of basic group-functional group, basic group-auxiliary group, and functional group-auxiliary group to determine the key compatibility indicators of each matching combination. S3 Adaptability Scoring and Visualization: Standardize the key adaptability indicators for each pairwise matching combination, construct a three-dimensional adaptability matrix, and visualize it in the form of a heatmap to intuitively show the degree of adaptability between different module components. S4 Optimal Combination Initial Screening: Based on the three-dimensional compatibility heatmap, the top 3 component pairs with the highest compatibility scores between each pair of modules are selected, and candidate coating formulation sets are obtained through cross-combination. S5 Comprehensive Performance Verification and Optimization: Conduct comprehensive performance tests on all formulations in the candidate coating formulation set, and determine the final optimal combination of functional polymer coating components based on the test results.
2. The method for component screening and development design of functional polymer coatings according to claim 1, characterized in that, In step S1, the base group is the film-forming substance of the coating, selected from 3-4 types of epoxy resin, acrylic resin, polyurethane resin, and silicone resin; the functional group is the curing agent that determines the core performance of the coating, selected according to the type of resin in the base group, and selected from 3-4 types of amine curing agents, acid anhydride curing agents, isocyanate curing agents, and phenolic resin curing agents. Among them, epoxy resin systems are suitable for amine, acid anhydride, and phenolic resin curing agents, polyurethane resin systems are suitable for isocyanate curing agents, and silicone resin systems are suitable for addition reaction curing agents; the auxiliary group is the additive that improves the processing and performance of the coating, selected from 3-4 types of leveling agents, defoamers, adhesion promoters, and weathering agents. The above four types of additives are applicable to various base systems of epoxy resin, acrylic resin, polyurethane resin, and silicone resin, and the specific grade is adjusted according to the polarity of the system.
3. The method for component screening and development design of functional polymer coatings according to claim 1, characterized in that, In step S2, the key compatibility indicators determined by the basic group-functional group matching experiment include curing time, gel conversion rate, crosslinking density, and glass transition temperature; the key compatibility indicators determined by the basic group-auxiliary group matching experiment include compatibility, dispersion stability, and surface tension; and the key compatibility indicators determined by the functional group-auxiliary group matching experiment include the effect of curing reactivity, storage stability, and side reaction rate.
4. The method for component screening and development design of functional polymer coatings according to claim 1, characterized in that, In step S2, each pairwise matching experiment was conducted with a fixed ratio, wherein the mass ratio of the basic group to the functional group was fixed at 100:(20~50), the mass ratio of the basic group to the auxiliary group was fixed at 100:(0.5~5), and the mass ratio of the functional group to the auxiliary group was fixed at 100:(1~10).
5. The method for component screening and development design of functional polymer coatings according to claim 1, characterized in that, In step S3, the standardized score adopts a 0-10 point system, where 10 points indicates the best compatibility and 0 points indicates no compatibility. For each key compatibility index, different weight coefficients are assigned according to their importance to the coating performance, and the comprehensive compatibility score of the pairwise matching combination is obtained by weighted calculation.
6. The method for component screening and development design of functional polymer coatings according to claim 1, characterized in that, In step S3, the three axes of the three-dimensional adaptability heatmap correspond to the candidate components of the basic group, functional group and auxiliary group, respectively. The color depth of each cell represents the overall adaptability score between the two corresponding components. The darker the color, the better the adaptability.
7. The method for component screening and development design of functional polymer coatings according to claim 1, characterized in that, In step S4, the cross-combination specifically involves: combining the top 3 component pairs in terms of compatibility between the basic group and the functional group, the top 3 component pairs in terms of compatibility between the basic group and the auxiliary group, and the top 3 component pairs in terms of compatibility between the functional group and the auxiliary group, and retaining the ternary component combinations that simultaneously meet the pairing requirements of the three groups: that is, in this combination, the basic component and the functional component are paired in the top 3 of the basic group-functional group, the basic component and the auxiliary component are paired in the top 3 of the basic group-auxiliary group, and the functional component and the auxiliary component are paired in the top 3 of the functional group-auxiliary group, thus forming a candidate coating formulation set.
8. The method for component screening and development design of functional polymer coatings according to claim 1, characterized in that, In step S5, the comprehensive performance test includes mechanical performance test, chemical corrosion resistance test, weather resistance test and processing performance test; according to the needs of different application scenarios, different weight coefficients are assigned to the results of each performance test, and the comprehensive performance score of each candidate formulation is calculated by weighting, and the one with the highest comprehensive performance score is the final optimal component combination.
9. The method for component screening and development design of functional polymer coatings according to claim 1, characterized in that, It also includes step S6: optimizing the proportions of the determined optimal component combination by using response surface methodology to adjust the mass ratio of each component based on the optimal component combination.
10. The method for component screening and development design of functional polymer coatings according to claim 1, characterized in that, The method is applicable to the component screening and development design of any functional polymer coating among anti-corrosion coatings, wear-resistant coatings, high-temperature resistant coatings, insulating coatings, and antibacterial coatings. For different coating types, the key compatibility indicators in step S2 can be adjusted accordingly: for insulating coatings, dielectric strength, volume resistivity, and breakdown voltage are added to the basic matching indicators; for antibacterial coatings, antibacterial rate, antibacterial durability, and mildew resistance are added to the basic matching indicators.