A potted integrated inductor
By filling the space between the housing and the magnetic core with magnetic glue, the problem of existing potting compounds not participating in the magnetic circuit is solved, achieving high magnetic permeability, low noise and excellent heat dissipation performance, and improving the electrical performance and structural stability of the inductor.
Patent Information
- Application Number
- CN202611447951.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-17
- Publication Date
- 2026-11-17
AI Technical Summary
Existing potting compounds do not participate in the magnetic circuit, resulting in significant magnetic leakage and limited inductance improvement; they also suffer from serious heat dissipation and noise problems, poor vibration resistance, and difficulty in meeting the needs of high power density equipment.
Magnetic adhesive is used in the magnetic circuit. The magnetic adhesive is a composite of resin matrix and high proportion of magnetic powder. It is filled between the shell and the magnetic core and covers the outer surface of the coil to form an overall structure with high magnetic permeability, high thermal conductivity and low noise.
It significantly increases inductance, reduces high-frequency eddy current losses, reduces noise, enhances vibration resistance and heat dissipation performance, and extends service life.
Smart Images

Figure CN123120464A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of electronic components technology, specifically a potted integrated inductor. Background Technology
[0002] With the continuous increase in power density of switching power supplies, on-board chargers (OBCs) and 5G base station equipment, integrated inductors, as the core components for energy storage and filtering, are subject to higher requirements for miniaturization, low loss and electromagnetic interference (EMI) performance.
[0003] In existing technologies, common I-shaped inductors typically use a plastic casing to encapsulate the magnetic core and coil. To secure the coil and prevent the magnetic core from breaking, the industry commonly employs a potting process, which involves filling the gap between the casing and the magnetic core with epoxy resin.
[0004] However, the aforementioned existing technologies have the following technical problems in practical use: Encapsulating materials do not participate in the magnetic circuit: Most existing encapsulating materials are pure resins or have a small amount of inorganic fillers (such as quartz powder and alumina) added, and their magnetic permeability is close to that of air (μi≈1). These types of adhesives only play a physical fixing and insulating role and cannot guide magnetic lines of force, resulting in large leakage magnetic field and limited inductance improvement. Heat dissipation and noise issues: Pure resin adhesive has a low thermal conductivity and high hardness. Under high current conditions, the heat generated by the coil is difficult to be effectively conducted to the outer casing, and the magnetostriction effect of the magnetic core under alternating magnetic fields cannot be effectively damped by the potting layer, which can easily cause high-frequency acoustic noise. Poor vibration resistance: Traditional epoxy potting compound has a large difference in linear expansion coefficient with magnetic core and coil, which can easily generate micro-cracks under thermal shock environment, leading to wear of coil insulation layer or loosening of magnetic core. Summary of the Invention
[0005] The purpose of this invention is to provide a potted integrated inductor that has the effect of significantly improving electrical performance by having magnetic adhesive participate in the magnetic circuit.
[0006] The above-mentioned technical objective of the present invention is achieved through the following technical solution: a potted integrated inductor, comprising: case; The magnetic core is disposed inside the housing along the axial direction of the housing, and a gap is left between it and the inner wall of the housing; A coil is wound around the outer periphery of the magnetic core; Magnetic adhesive is used to fill the gap between the housing and the magnetic core and to cover the outer surface of the coil.
[0007] A further provision of the present invention is that the magnetic adhesive is composed of a resin matrix and magnetic powder dispersed in the resin matrix, wherein the magnetic powder is selected from at least one of iron-silicon-chromium alloy powder, carbonyl iron powder, and iron-silicon-aluminum powder, and the magnetic powder accounts for 40% to 75% of the total volume of the magnetic adhesive.
[0008] A further feature of the present invention is that the resin matrix is epoxy resin, polyurethane resin or silicone rubber, and the initial magnetic permeability μi of the magnetic adhesive is 2~15.
[0009] A further feature of the present invention is that the housing is a cylindrical structure with an open top, and end caps or buckles are provided at both ends of the housing along the axial direction to axially confine the magnetic core within the housing.
[0010] A further configuration of the present invention is that the axial ends of the magnetic core extend out of the housing and form pin support portions, and the leads of the coil are fixed to the pin support portions.
[0011] A further provision of the present invention is that the shell is made of reinforced engineering plastic containing 10% to 40% glass fiber, preferably PBT, PA6 or PA66.
[0012] A further feature of the present invention is that the magnetic core is a ferrite magnetic core or a sintered soft magnetic powder core.
[0013] A method for manufacturing a potted integrated inductor, applicable to the aforementioned potted integrated inductor, includes the following steps: S1: Insert the magnetic core into the housing, leaving a gap between the magnetic core and the inner wall of the housing; S2: Wind a coil around the outer circumference of the magnetic core and pre-fix the coil leads; S3: Fill the gap with magnetic glue so that the magnetic glue covers the outer surface of the coil; S4: Heat curing to bond the magnetic adhesive to the shell, magnetic core, and coil as a whole.
[0014] A further feature of the present invention is that the magnetic adhesive in step S3 is filled by vacuum injection or pressure injection, and after injection, it is allowed to stand for 5-15 minutes to degas before being heated and cured in step S4.
[0015] In summary, the present invention has the following beneficial effects: 1. The magnetic adhesive filled between the shell and the magnetic core in this invention is composed of a resin matrix and a high proportion (40%~75% by volume) of magnetic powder, with an initial permeability μi of 2~15. Compared with the ordinary epoxy adhesive with a permeability close to 1 used in the prior art, the magnetic adhesive in this invention can directly participate in the magnetic circuit closure, reduce air gap leakage, and thus effectively increase the inductance in the same volume (measured increase of about 9.7%). At the same time, the introduction of magnetic adhesive optimizes the magnetic resistance distribution, helps to reduce high-frequency eddy current loss, and improves the quality factor Q value (measured increase of about 16%), solving the technical bottleneck of traditional potted inductors that are "only fixed and not magnetic". 2. This invention defines the outer surface of the coil by magnetically coated with adhesive, and utilizes the high damping characteristics of the adhesive to suppress the transmission of micron-level vibrations caused by magnetostriction of the magnetic core to the shell. At the same time, the magnetic powder in the adhesive can effectively absorb high-frequency stray magnetic flux, playing an electromagnetic shielding role. Under the same high current load conditions, the noise sound pressure level of the product of this invention is reduced by more than 9dB compared with ordinary epoxy potting inductors, solving the problem of high-frequency howling of power inductors under high current. 3. The magnetic adhesive formula used in this invention significantly improves the thermal conductivity (up to 1.3 W / (m·K) or higher) while ensuring insulation strength; the magnetic adhesive tightly wraps the coil, forming an efficient heat conduction path from the coil to the outer shell, greatly reducing the temperature rise (measured temperature drop of up to 26%); in addition, after the magnetic adhesive is cured, it is bonded to the shell, magnetic core and coil as a whole, eliminating internal gaps, enhancing the vibration resistance and thermal shock resistance of the overall structure, and extending the service life of the components. Attached Figure Description
[0016] Figure 1 This is a cross-sectional structural diagram of the present invention.
[0017] In the diagram: 1. Shell; 2. Magnetic core; 3. Coil; 4. Magnetic glue. Detailed Implementation
[0018] The present invention will be further described below with reference to the accompanying drawings in the embodiments of the present invention.
[0019] Please see Figure 1 In this embodiment of the invention, an encapsulated integrated inductor includes a housing 1, a magnetic core 2, a coil 3, and magnetic adhesive 4.
[0020] The housing 1 is a square cylindrical structure (or a circular cylindrical structure) with an open top. It has snap-on end caps at both axial ends to axially confine the magnetic core 2 within the housing 1. The magnetic core 2 is arranged axially along the housing 1, with a radial gap between it and the inner wall of the housing 1. This gap forms the filling channel for the magnetic adhesive 4. The coil 3 is a helical winding formed by enameled copper wire wound around the outer circumference of the magnetic core 2. The two leads of the coil 3 extend from the pin support portions at both axial ends of the magnetic core 2 and are fixed to these support portions (either by soldering or clamping). The magnetic adhesive 4 fills the gap between the housing 1 and the magnetic core 2 and covers the outer surface of the coil 3 winding, embedding the coil 3 within the magnetic adhesive 4. After the magnetic adhesive 4 cures, it bonds to the housing 1, the magnetic core 2, and the coil 3 as a single unit.
[0021] The housing 1 is made of reinforced engineering plastic containing 10%~40% glass fiber. In this embodiment, PA66+30%GF (glass fiber content 30wt%) is selected and injection molded. The inner wall of the housing 1 can be roughened (Ra=1.6~3.2μm) to improve the bonding strength with the magnetic adhesive 4. The axial ends of the housing 1 are snapped together to abut against the end faces of the magnetic core 2, restricting the axial movement of the magnetic core 2.
[0022] The magnetic core 2 is cylindrical (either I-shaped or straight cylindrical), and the material is selected from manganese-zinc ferrite (PC40 grade) or iron-silicon-chromium sintered powder core. In this embodiment, a cylindrical iron-silicon-chromium powder core with an outer diameter of 8mm, an inner diameter of 4mm, and a height of 10mm (Sendust, μi≈60) is used. The magnetic core 2 extends outward at both ends along the axis to form pin support parts for fixing the leads of the coil 3.
[0023] Coil 3 is made of Φ0.8mm polyurethane enameled copper wire, wound around the outer circumference of magnetic core 2, with 50 turns and a DC resistance DCR≈18mΩ. After winding, the two leads are soldered to the pin supports at both ends of magnetic core 2 to form inductor terminals.
[0024] Magnetic adhesive 4 is composed of a resin matrix and magnetic powder. The magnetic powder accounts for 40% to 75% of the total volume of the magnetic adhesive, and the resin matrix is epoxy resin, polyurethane resin or silicone rubber.
[0025] Example 1 (Magnetic powder volume percentage ≈ 45%, close to the lower limit) Resin matrix: Bisphenol A type epoxy resin (E-51) 60g Magnetic powder: Iron-silicon-chromium alloy powder (Fe-Si-Cr, particle size D50=15μm) 35g Excipients: 3g nano-SiO2 (reinforced), 0.8g KH560 coupling agent, 18g methyltetrahydrophthalic anhydride curing agent Preparation: Pre-disperse iron-silicon-chromium powder and coupling agent for 10 min, add epoxy resin and nano-SiO2 and stir for 2 h (vacuum degree -0.095MPa, 60℃), finally add curing agent and stir well, and vacuum degas for 8 min.
[0026] Performance: After curing, the density of the magnetic adhesive is about 3.2 g / cm³, the volume ratio of magnetic powder is about 45%, the initial magnetic permeability μi is about 4.2 (1 MHz, coaxial method), the hardness is Shore D 82, and the thermal conductivity is 0.9 W / (m·K).
[0027] Example 2 (Magnetic powder volume ratio ≈ 60%, intermediate value, preferred example) Resin matrix: Bisphenol A type epoxy resin (E-51) 50g Magnetic powder: Carbonyl iron powder (D50=8μm) 55g Excipients: Nano SiO2 4g, KH560 1.0g, Methyltetrahydrophthalic anhydride 15g The preparation method is the same as in Example 1.
[0028] Performance: Magnetic powder volume percentage ≈ 60%, μi ≈ 8.6 (1MHz), hardness Shore D 88, thermal conductivity 1.3 W / (m·K). Preferred embodiment of this invention.
[0029] Example 3 (Magnetic powder volume ratio ≈ 72%, close to the upper limit) Resin matrix: Vinyl silicone resin (A / B two-component) 40g Magnetic powder: Mn-Zn ferrite micro powder (D50=12μm) 65g Excipients: 5g fumed silica, 0.5g platinum catalyst Preparation: After pre-dispersing the magnetic powder and coupling agent, add the organosilicon component A, and knead under vacuum for 100 min (80℃, vacuum degree -0.09MPa). Then add the component B, stir well, and remove bubbles.
[0030] Performance: Magnetic powder volume ratio ≈72%, μi≈13.5 (100MHz, S-parameter method, comparable to Toda MG-001 system), hardness Asker C 95, low elastic modulus, and good damping and shock absorption effect.
[0031] Taking Example 2 as an example, the manufacturing steps are as follows: (1) Inserting the magnetic core into the housing: Insert the magnetic core 2 into the housing 1 through the top opening, so that there is a radial gap of about 0.8~1.2mm between the magnetic core 2 and the inner wall of the housing 1, and the two ends of the magnetic core 2 are axially limited by the two ends of the housing 1; (2) Winding and lead fixing: a coil 3 (50Ts, Φ0.8mm enameled wire) is wound around the outer circumference of the magnetic core 2, and the two lead ends are soldered to the pin support parts at both ends of the magnetic core 2; (3) Magnetic glue filling: Vacuum injection method is used to inject the prepared magnetic glue 4 into the gap between the housing 1 and the magnetic core 2; the vacuum degree of the cavity is maintained at -0.095~-0.098MPa during injection, so that the magnetic glue 4 penetrates into the coil 3 between the turns under negative pressure and covers the outer surface of the coil 3, ensuring that no air bubbles remain. After the injection is completed, stand at normal pressure for 10 minutes to remove bubbles; (4) Heating and curing: Place the potted product into an oven and bake at 140~160℃ for 40~60min (150℃×50min in this example). After natural cooling to room temperature, the magnetic glue 4 will be cured and form an integral structure with the shell 1, magnetic core 2 and coil 3, thus obtaining the potted integrated inductor.
[0032] The above description is only a preferred embodiment of the present invention. Therefore, all equivalent changes or modifications made to the structure, features and principles described in the claims of this patent application are included in the scope of this patent application.
Claims
1. A potted integrated inductor, characterized in that, include: Shell (1); The magnetic core (2) is disposed inside the housing (1) along the axial direction of the housing (1) and a gap is left between it and the inner wall of the housing (1); A coil (3) is wound around the outer periphery of the magnetic core (2); Magnetic adhesive (4) is filled in the gap between the housing (1) and the magnetic core (2) and covers the outer surface of the coil (3).
2. The potted integrated inductor according to claim 1, characterized in that, The magnetic adhesive (4) is composed of a resin matrix and magnetic powder dispersed in the resin matrix. The magnetic powder is selected from at least one of iron-silicon-chromium alloy powder, carbonyl iron powder, and iron-silicon-aluminum powder. The magnetic powder accounts for 40% to 75% of the total volume of the magnetic adhesive.
3. The potted integrated inductor according to claim 2, characterized in that, The resin matrix is epoxy resin, polyurethane resin or silicone rubber, and the initial magnetic permeability μi of the magnetic adhesive (4) is 2~15.
4. The potted integrated inductor according to claim 1, characterized in that, The housing (1) is a cylindrical structure with an open top. The two ends of the housing (1) are provided with end caps or buckles in the axial direction to confine the magnetic core (2) in the housing (1) in the axial direction.
5. The potted integrated inductor according to claim 4, characterized in that, The magnetic core (2) extends out of the housing (1) at both ends and forms a pin support portion, and the lead wire of the coil (3) is fixed on the pin support portion.
6. The potted integrated inductor according to claim 1, characterized in that, The shell (1) is made of reinforced engineering plastic containing 10% to 40% glass fiber, preferably PBT, PA6 or PA66.
7. The potted integrated inductor according to claim 1, characterized in that, The magnetic core (2) is a ferrite core or a sintered soft magnetic powder core.
8. A method for manufacturing a potted integrated inductor, applicable to the potted integrated inductor according to any one of claims 1 to 7, characterized in that, Includes the following steps: S1: Insert the magnetic core (2) into the housing (1) so that there is a gap between the magnetic core (2) and the inner wall of the housing (1); S2: Wind a coil (3) around the outer periphery of the magnetic core (2) and pre-fix the coil leads; S3: Fill the gap with magnetic glue (4) so that the magnetic glue (4) covers the outer surface of the coil (3); S4: Heat and cure to bond the magnetic adhesive (4) to the shell (1), magnetic core (2), and coil (3) as a whole.
9. The method for manufacturing an encapsulated integrated inductor according to claim 8, characterized in that, The magnetic adhesive (4) in step S3 is filled by vacuum injection or pressure injection. After injection, it is allowed to stand for 5-15 minutes to degas before being heated and cured in step S4.