Concrete battery cell and its preparation method
By designing porous conductive concrete battery cells, the cost and safety issues of traditional batteries in building applications are solved, enabling independent charging and discharging and low-voltage DC energy storage, making it suitable for low-cost building energy storage systems.
Patent Information
- Application Number
- CN202611613116.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-19
- Publication Date
- 2026-11-17
AI Technical Summary
Existing lithium-ion and lead-acid batteries have problems such as high cost, insufficient safety and environmental performance in building energy storage applications. In addition, traditional concrete energy storage solutions lack independent charging and discharging concrete battery modules, resulting in high construction complexity.
Design a concrete battery cell comprising a sealed insulating layer, a corrugated composite electrode concrete sandwich plate, a corrugated dense concrete diaphragm, positive and negative terminals, forming a porous conductive network by pouring in an electrolyte solution to achieve independent charging and discharging, and enhancing structural integration through interlayer interlocking connections.
It increases the total energy storage capacity and structural integrity of concrete batteries, reduces construction complexity, is suitable for low-voltage DC energy storage applications, and the cement-based material is low-cost and can be designed in shape, making it suitable for low-voltage LED lighting and photovoltaic charging scenarios.
Smart Images

Figure CN123120914A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the intersection of concrete materials and electrochemical energy storage, and in particular to a concrete battery cell with multiple interlocked concrete electrode plates and its preparation method. Background Technology
[0002] With the development of renewable energy power generation, low-voltage DC lighting, and distributed energy storage, energy storage devices need to simultaneously meet requirements such as low cost, safety, long lifespan, modular installation, and ease of maintenance. Traditional lithium-ion batteries have high energy density, but they also have high requirements for cost, thermal runaway risk, recycling, and safety management in building scenarios; lead-acid batteries have lower cost, but their lifespan and environmental performance are limited.
[0003] Concrete, with cement as its binder, boasts advantages such as wide availability of raw materials, low cost, high plasticity, and adjustable pore structure. By constructing electrolyte conduction channels within cement-based materials and incorporating electrode components with varying electrochemical potentials or energy storage characteristics, concrete batteries can be formed that combine structural bulk form with energy storage functionality.
[0004] Existing solutions related to concrete energy storage mostly emphasize integrated use with building structures. For demonstration applications and low-voltage DC applications, there is a greater need for a pre-packaged, sealed individual concrete battery module that can be manufactured, packaged, and tested in a factory or laboratory. On-site work only requires placement, fixing, series and parallel connection, and external electrical connections, thereby reducing construction complexity and improving safety.
[0005] Therefore, there is a need to provide a concrete battery cell that is independent of building structure, can be used as a load-bearing component of a building, and can be charged and discharged independently, along with its structure and manufacturing method. Summary of the Invention
[0006] The technical problem to be solved by the present invention is to provide a concrete battery unit that can be used as a load-bearing component of a building and can be charged and discharged independently.
[0007] To solve the above-mentioned technical problems, the technical solution adopted by the present invention is as follows: This invention first provides a concrete battery cell, comprising: Sealing insulation layer; An electrode body is disposed within the sealed insulating layer. The electrode body includes a corrugated composite electrode concrete clamping plate, a corrugated dense concrete diaphragm, a positive terminal, and a negative terminal. The corrugated composite electrode concrete clamping plates are arranged parallel to each other at intervals within the sealed insulating layer, and are divided into a positive electrode plate and a negative electrode plate, with the positive and negative electrode plates arranged alternately. The corrugated dense concrete diaphragm is disposed between two adjacent corrugated composite electrode concrete clamping plates. The positive terminal is connected to the positive electrode plate, and the negative terminal is connected to the negative electrode plate. An electrolyte solution is added to the insulating layer and comes into contact with the electrode body.
[0008] This invention also provides a method for preparing a concrete battery cell, comprising: Preparation of positive and negative electrode plates; The prepared positive and negative electrode sheets are alternately arranged in the sealed insulating layer; Pouring a corrugated, dense concrete diaphragm; Connect the positive and negative extremes; Add an electrolyte solution inside the sealed insulation layer.
[0009] The beneficial effects of this invention are as follows: First, the concrete electrode is made of porous conductive concrete. Its function is to generate a conductive network to expand the energy storage capacity of the internal electrode plates, thereby increasing the total energy storage of the concrete battery. Simultaneously, it connects to a corrugated, dense concrete membrane, integrating the internal structure of the concrete battery. Since the internal electrode plates require an electrolyte solution to maintain high electrochemical properties, the concrete electrode has a porosity of 25%-45%, simultaneously forming interconnected electrolyte solution channels. The porous morphology allows the electrolyte solution to fully penetrate the conductive concrete. The concrete battery unit is fabricated with porous composite positive and negative electrode concrete sandwich plates. This plate is a composite concrete electrode that combines electrochemical performance with load-bearing capacity.
[0010] Secondly, the concrete battery unit uses an interlocking interlayer to connect the composite positive and negative electrode concrete sandwich plates, which increases the cohesion between the concrete layers. At the same time, the pouring process is simple and can form an integrated concrete structure inside the concrete battery unit.
[0011] Third, the corrugated dense concrete membrane needs to maintain low porosity to improve structural integrity, reduce permeability, and enhance compressive strength and other properties. With the improvement of concrete grade, the porosity can be maintained at a low level compared to concrete of the same grade by reducing the water-cement ratio, adding defoamers, filling with mineral admixtures, and ensuring thorough compaction.
[0012] Fourth, multiple concrete battery units can be connected in series and parallel to form a low-voltage DC energy storage battery pack with target voltage and capacity. Multiple concrete battery units can be connected in series and parallel to form a low-voltage DC energy storage building structure of about 10~12V.
[0013] Fifth, cement-based materials are widely available, low in cost, and can be designed in various shapes, making them suitable for integration with low-voltage LED lighting, photovoltaic charging, and building energy storage demonstrations. Attached Figure Description
[0014] Figure 1 This is a schematic diagram illustrating the manufacturing process of the concrete battery unit of the present invention.
[0015] Figure 2 This is a schematic diagram of the overall structure of the concrete battery unit of the present invention.
[0016] Figure 3 This is a schematic diagram of the internal structure of the concrete battery cell of the present invention.
[0017] Figure 4 This is a schematic diagram of the structure of the corrugated composite electrode concrete clamping plate of the present invention.
[0018] Figure 5 This is a schematic diagram of the base structure for fixing the clamping plate of the present invention.
[0019] Figure 6 This is the finite element simulation load-bearing model of the concrete battery unit of the present invention.
[0020] Figure 7 The finite element unit of the concrete battery cell in this invention achieves plastic damage.
[0021] Figure 8 This is a stress-displacement comparison curve of the concrete battery cell of the present invention.
[0022] Figure 9 This is the constant current charge-discharge curve of the concrete battery cell of the present invention.
[0023] The diagram includes: 1. Electrode body; 2. Corrugated composite electrode concrete clamp plate; 3. Corrugated dense concrete diaphragm; 4. Positive terminal; 5. Negative terminal; 6. Sealing insulation layer; 7. Insulating protective cover; 8. Connector plate. Detailed Implementation
[0024] The present invention will be further described below with reference to embodiments. These embodiments are for illustrative purposes only and are not intended to limit the scope of protection of the present invention. Where there is no conflict, the technical features of the various embodiments can be combined with each other.
[0025] Example 1 This embodiment provides a concrete battery unit; see [link to relevant documentation]. Figure 2 and Figure 3 It includes an electrode body 1, a sealing and insulating layer 6, and an electrolyte solution. The electrode body 1 is disposed inside the sealing and insulating layer 6, and the electrolyte solution is added inside the sealing and insulating layer 6 and comes into contact with the electrode body 1.
[0026] The electrode body 1 includes a corrugated composite electrode concrete clamping plate 2, a corrugated dense concrete diaphragm 3, a positive terminal 4, and a negative terminal 5. The corrugated composite electrode concrete clamping plates 2 are arranged parallel to each other at intervals within the sealed insulating layer 6, and are divided into positive and negative plates, which are arranged alternately. The angle between the line segment forming the highest point of the wave crest and the lowest point of the wave and the horizontal line is set to α degrees. Considering that too small an angle α would reduce the interlocking effect, and too large an angle α would easily cause the concrete battery to be damaged by bias voltage under load, the angle α is now set to 30 degrees. The corrugated dense concrete diaphragm 3 is cast between two adjacent corrugated composite electrode concrete clamping plates 2. The positive terminal 4 and the negative terminal 5 are respectively connected to the corresponding terminals 8 of the corrugated composite electrode concrete clamping plates 2.
[0027] The sealing insulation layer 6 covers the outer surface of the concrete battery cell and seals the terminal lead-out areas with an insulating protective cover 7. The sealing insulation layer includes one or more of the following: a cement-based waterproof layer, a polymer waterproof layer, an epoxy resin layer, a polyurethane layer, a silicone sealing layer, or an insulating composite coating. The sealing insulation layer is required to undergo elastic-plastic deformation to transfer the upper pressure to the corrugated dense concrete diaphragm and corrugated composite electrode concrete sandwich plate inside the concrete battery for bearing, thus preventing the insulating container from breaking and causing electrolyte leakage during the bearing process.
[0028] In one embodiment, a base is provided inside the sealing insulation layer 6, and the corrugated composite electrode concrete clamp plate 2 is embedded in the base. The composite electrode concrete clamp plate can be fixed inside the multi-concrete electrode plate concrete battery unit, which facilitates the subsequent casting of the corrugated dense concrete diaphragm.
[0029] The corrugated composite electrode concrete sandwich plate 2 is a dual-electrode system formed by assembling an electrode plate and a concrete electrode. The concrete electrode in the corrugated composite electrode concrete sandwich plate 2 is composed of porous organic conductive carbon black concrete mortar.
[0030] Porous organic conductive carbon black concrete mortar includes cement, water, foaming agent, and organic conductive carbon black. The cement is 200 parts, the water is 110 parts, the water-cement ratio is controlled at 0.6, the foaming agent is 2-9 parts, and the organic conductive carbon black is 10 parts.
[0031] The cement used is P·O 42.5 cement; the foaming agent is 30 wt% H2O2 solution, the reaction principle is that H2O2 decomposes into water and oxygen during the hydrolysis and heat release of cement, thereby generating bubbles; the organic conductive carbon black used is Superp Li conductive carbon black.
[0032] The template for the corrugated composite electrode concrete sandwich panel 2 is custom-cast to form a concrete panel with dimensions of 160mm*200mm*4mm, wherein each electrode sheet has dimensions of 160mm*200mm*0.3mm.
[0033] The positive current collector uses 316L stainless steel, while the negative current collector directly uses a Zn electrode sheet. Each current collector measures 160mm*200mm*0.3mm. MnO2 is coated onto the 316L stainless steel current collector to form the positive electrode sheet, and a 316L stainless steel contact plate is pre-installed on the positive current collector. A 316L stainless steel contact plate is welded onto the Zn electrode sheet for the negative electrode. The contact plate on the positive electrode sheet is connected to the positive terminal 4, and the contact plate on the negative electrode sheet is connected to the negative terminal 5. The ends of the positive terminal 4 and the negative terminal 5 are connected to the outside via lead wires, forming internal and external electron channels. The lead wires are wrapped with an insulating protective cover 7.
[0034] The sealing insulation layer 6 is set on the outside of the concrete battery unit. At the same time, a 30mm high base is designed inside to fix the corrugated composite electrode concrete clamp plate. The outer shell material of the sealing insulation layer is PE100-RC. This material has good elastic-plastic deformation performance and can transfer the pressure from the upper part to the concrete plate inside the concrete battery for bearing. The electrolyte is a 2 mol / L KOH solution. The mixed solution presents an alkaline system. After placing the internal structure of the concrete battery unit, the electrolyte solution is added to 75%, leaving 25% space to reduce the sudden increase in lateral water pressure caused by container compression.
[0035] During the fabrication of concrete electrodes, a water-cement ratio of 0.6 is used in combination with different dosages of foaming agent to form a capillary network, so that the porosity of the conductive concrete reaches 25%-35% and forms interconnected channels.
[0036] In one embodiment, the mass fractions of each component in the porous organic conductive carbon black concrete mortar are: 200 parts cement, 110 parts water, 2 parts 30 wt% H2O2 solution foaming agent, and 10 parts organic conductive carbon black, with the porosity controlled at around 25%.
[0037] In one embodiment, the mass fractions of each component in the porous organic conductive carbon black concrete mortar are: 200 parts cement, 110 parts water, 5 parts 30 wt% H2O2 solution foaming agent, and 10 parts organic conductive carbon black, with the porosity controlled at around 30%.
[0038] In one embodiment, the mass fractions of each component in the porous organic conductive carbon black concrete mortar are: 200 parts cement, 110 parts water, 9 parts 30 wt% H2O2 solution foaming agent, and 10 parts organic conductive carbon black, with the porosity controlled at around 35%.
[0039] During the fabrication of the dense concrete diaphragm, a low water-cement ratio is adopted, and defoamers and S95 slag are added for filling, resulting in a low porosity of the dense concrete diaphragm. The effective water-cement ratio is 0.28–0.35. The internal porosity is reduced by adding S95 grade slag powder and defoamers, and by vibration compaction. The total porosity of the dense concrete diaphragm after 28 days of hardening is 5%–15%, preferably 8%–12%.
[0040] To verify the performance advantages of the concrete battery unit of this invention, and considering that actual energy storage building structures contain multiple concrete battery units combined together, this embodiment selects a single concrete battery unit in a low-voltage DC energy storage battery pack as the simulation object to simplify simulation calculations, improve simulation efficiency, and ensure the representativeness of the verification results. A realistic load-bearing simulation model is established using finite element simulation software to simulate and analyze the load-bearing performance of the concrete battery unit. The geometric dimensions, material parameters, and boundary conditions are kept completely consistent to ensure the objectivity and validity of the comparison results. In the simulation model, the concrete battery cells consist of two types of dense concrete membranes: a wavy, 160mm long, 200mm high, and 16mm wide membrane, and a flat, 160mm long, 200mm high, and 16mm wide membrane, arranged in a vertical parallel array of 13 units each. Because the wavy composite electrode concrete sandwich plate has weak load-bearing capacity, high porosity, and is a thin, porous concrete, the wavy composite electrode concrete sandwich plate model was omitted during the simulation. The isotropic material parameters of C30 plain concrete were used, and a concrete damage-plastic model capable of simulating stiffness recovery under cyclic loading was employed. The overall loading model is as follows: Figure 6 A rigid body is added to the upper and lower surfaces of the wavy dense concrete diaphragm. The contact surfaces between the rigid body and the two types of dense concrete diaphragms are bound together. The six-degree-of-freedom of the coupling point RP-2 at the center of the lower surface of the lower rigid body is completely fixed. A downward displacement of 1 mm is applied to the coupling point RP-1 at the center of the upper surface of the upper rigid body until the loading is completed.
[0041] like Figure 7 Upon completion of the final loading, the high-damage area was mainly concentrated in the middle layer of the specimen. The damage levels between the high-damage zones and in the upper and lower parts of the specimen were relatively low. The maximum compressive damage variable was approximately 0.926, indicating that significant compressive stiffness degradation occurred in the local concrete. The results are as follows... Figure 8 The results show that, under C30 concrete parameters, the finite element model of a straight, dense concrete diaphragm exhibits the following performance when the loading displacement is 0.44 mm: Figure 7When the load reached a certain level, some elements began to show damage, and the overall load-bearing stress of the concrete battery unit reached a peak stress of 12.17 MPa. Under the same material and size, the finite element model of the corrugated dense concrete diaphragm reached its peak stress of 14.69 MPa at a loading displacement of 0.41 mm, and then began to decrease. The analysis results show that when using C30 material, the load-bearing capacity of the corrugated dense concrete diaphragm is 1.2 times that of the straight dense concrete diaphragm. In actual engineering, the concrete grade of the dense concrete diaphragm in the concrete battery unit can be increased to enable the corrugated dense concrete diaphragm to achieve better load-bearing performance in applications. Meanwhile, the energy storage density of the concrete battery cell was investigated. Because the electrode plates are located within a porous concrete electrode, the concrete electrode has a high porosity and forms interconnected channels, allowing the electrolyte solution to directly enter the interior of the concrete electrode and undergo electrochemical reactions with the electrode plates. Furthermore, the weight-bearing capacity of the corrugated, dense concrete diaphragm has minimal impact on the redox reactions of the electrode plates. A simplified energy storage density test was conducted using a 2mm*2mm MnO2 sheet as the positive electrode and a 2mm*2mm Zn sheet as the negative electrode. Constant current charge-discharge tests were performed in a 2mol / L KOH solution with a current of 0.8mA and a voltage range of 1.0-1.65V. The experimental results are as follows: Figure 9 As shown, the five-cycle constant current charge-discharge test revealed similar curve shapes in each cycle, with no sudden shortening, abnormal voltage fluctuations, or inability to reach the cutoff voltage. Furthermore, the curve gradually widened to the right in the later stages, indicating capacity activation. Energy density calculations were performed using the third cycle, yielding an area energy density of 1.1 mWh / cm² for the electrode. 2 This indicates that the battery not only serves a load-bearing function but also possesses a high energy storage density. Furthermore, regarding the total energy storage capacity, the use of a 30-degree wave-interlocked electrode allows for an electrode area approximately 1.21 times that of a flat electrode per unit volume. Therefore, the total energy storage capacity of the wave-interlocked electrode is also 1.21 times that of the flat electrode. This method provides a new approach to increasing the total energy storage capacity of concrete batteries.
[0042] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, and are not intended to limit the scope of protection of the present invention. Those skilled in the art can make equivalent substitutions or improvements to the electrode materials, concrete formulations, monomer dimensions, terminal arrangements, sealing materials, and test loads without departing from the essential concept of the present invention.
Claims
1. A concrete battery cell, characterized in that, include: Sealing insulation layer; An electrode body, disposed within the sealed insulating layer, comprises a corrugated composite electrode concrete clamping plate, a corrugated dense concrete diaphragm, a positive terminal, and a negative terminal. The corrugated composite electrode concrete clamping plates are arranged parallel to each other at intervals within the sealed insulating layer, each plate being divided into a positive electrode plate and a negative electrode plate, which are arranged alternately. The corrugated dense concrete diaphragm is disposed between two adjacent corrugated composite electrode concrete clamping plates. The positive terminal is connected to the positive electrode plate, and the negative terminal is connected to the negative electrode plate. An electrolyte solution is added to the insulating layer and comes into contact with the electrode body.
2. The concrete battery unit according to claim 1, characterized in that, The corrugated composite electrode concrete sandwich plate is formed by assembling electrode sheets and concrete electrodes, and the concrete electrodes are composed of porous organic conductive carbon black concrete mortar.
3. The concrete battery unit according to claim 2, characterized in that, Porous organic conductive carbon black concrete mortar includes cement, water, foaming agent, and organic conductive carbon black. The mass fractions of each component are: cement 180-200 parts, foaming agent 2-9 parts, organic conductive carbon black 5-10 parts, and the water-cement ratio is controlled at 0.4-0.
6.
4. The concrete battery cell according to claim 3, characterized in that, In porous organic conductive carbon black concrete mortar, there are 200 parts of cement, 9 parts of foaming agent, and 10 parts of organic conductive carbon black.
5. The concrete battery unit according to claim 3, characterized in that, In porous organic conductive carbon black concrete mortar, the water-cement ratio is controlled at 0.
6.
6. The concrete battery unit according to claim 2, characterized in that, The electrode sheet comprises a metal conductor or a carbon-based conductor; the metal conductor comprises one or more of the following: metal mesh, metal sheet, metal rod, and foam metal structure; the material of the metal conductor comprises manganese dioxide, nickel hydroxyl oxide, nickel hydroxide, iron oxide, and ferrooxy hydroxyl; the carbon-based conductor comprises one or more of the following: graphite felt, carbon fiber felt, carbon cloth, carbon black coating, biochar coating, carbon nanotube coating, and graphene coating.
7. The concrete battery cell according to claim 3, characterized in that, The foaming agent includes chemical foaming agents and physical foaming agents.
8. The concrete battery unit according to claim 1, characterized in that, The corrugated dense concrete diaphragm is formed by pouring dense concrete mortar between corrugated composite electrode concrete sandwich plates; the total porosity of the corrugated dense concrete diaphragm after hardening is 5% to 15%.
9. The concrete battery unit according to claim 1, characterized in that, The angle between the line segment formed by the highest point of the wave crest and the lowest point of the wave trough of the wave-shaped composite electrode concrete sandwich plate and the horizontal line is 15-40 degrees.
10. A method for preparing a concrete battery cell according to any one of claims 1-9, characterized in that, include: Preparation of positive and negative electrode plates; The prepared positive and negative electrode sheets are alternately arranged in the sealed insulating layer; Pouring a corrugated, dense concrete diaphragm; Connect the positive and negative extremes; Add an electrolyte solution inside the sealed insulation layer.