A manufacturing process for a glass circuit board
By depositing aluminum and copper metal films on a glass substrate to form a copper-aluminum composite film, etching metal circuit patterns, and printing UV solder resist ink on the surface, the problem of high cost of traditional circuit boards is solved, achieving cost reduction and convenient electrical connection.
Patent Information
- Application Number
- CN202611520637.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-29
- Publication Date
- 2026-11-17
AI Technical Summary
Traditional printed circuit boards rely on pure copper foil as the conductive substrate, resulting in high production costs. The rising price of copper raw materials has exacerbated the business pressure on enterprises.
Using a glass substrate as the substrate, aluminum and copper metal films are sequentially deposited after laser drilling to form a copper-aluminum composite metal film. Metal circuit patterns are formed by laser etching, and finally UV solder resist ink is printed on the surface and cured with ultraviolet light.
It reduces circuit board production costs, saves copper resources, improves production efficiency, and facilitates electrical connection through through-holes, making it easy to connect to external circuits.
Smart Images

Figure CN123124203A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of circuit board manufacturing technology, and in particular to a manufacturing process for glass circuit boards. Background Technology
[0002] Traditional printed circuit boards (PCBs) use copper-clad laminates (CCLs) as the substrate. Their overall structure consists of an intermediate insulating substrate and conductive copper foil layers bonded to both sides of the insulating substrate. Conductive patterns are laid out on the copper foil layers, and the conductive copper foil layers on both sides of the intermediate insulating substrate are electrically connected via metallized vias. However, traditional PCBs rely on pure copper foil as the conductive substrate. In recent years, the price of copper raw materials has continued to rise, significantly increasing the production cost of PCBs and greatly exacerbating the operating pressure on manufacturing companies. Summary of the Invention
[0003] The present invention aims to at least partially improve one of the problems of the prior art. To this end, certain embodiments of the present invention provide a manufacturing process for glass circuit boards that helps to reduce the production cost of circuit boards.
[0004] A manufacturing process for a glass circuit board according to certain embodiments of the present invention includes the following steps: S1. Prepare materials: prepare a whole glass substrate, aluminum target and copper target. S2. Laser drilling: A laser device is used to drill holes in the glass substrate to form one or more through holes on the surface of the glass substrate, thereby obtaining a first glass substrate. The first glass substrate has a first surface and a second surface that are disposed opposite to each other. S3. Aluminum metal film layer: The first glass substrate and the aluminum target are placed into the vacuum coating chamber of the vacuum coating equipment, so that the first surface of the first glass substrate faces upward. Then the vacuum coating equipment is started and an aluminum metal film layer is deposited on the first surface to obtain the second glass substrate. S4. Copper metal film layer: The second glass substrate and the copper target are placed into the vacuum coating chamber of the vacuum coating equipment, with the aluminum metal film layer facing upward. Then the vacuum coating equipment is started and a copper metal film layer is formed on the surface of the aluminum metal film layer. The copper metal film layer and the aluminum metal film layer constitute a copper-aluminum composite metal film layer, and a third glass substrate is obtained. S5. Processing metal circuit patterns: Using a laser device to emit a laser to etch the copper-aluminum composite metal film layer of the third glass substrate, thereby etching the copper-aluminum composite metal film layer to form a preset metal circuit pattern, and obtaining the fourth glass substrate. S6. Printing and curing ink: UV solder resist ink is screen-printed on the first surface of the fourth glass substrate on which the metal circuit pattern is provided, and then UV curing equipment is used to cure the UV solder resist ink printed on the first surface to obtain a glass circuit board.
[0005] According to certain embodiments of the present invention, a manufacturing process for a glass circuit board has the following advantages: By using a glass substrate as the base, and then sequentially depositing an aluminum metal film and a copper metal film on one side of the glass substrate, forming a copper-aluminum composite metal film, and then using laser equipment to etch the copper-aluminum composite metal film to form a preset metal circuit pattern, UV solder resist ink is then screen-printed on the surface of the metal circuit pattern and ultraviolet curing is performed to obtain the desired glass circuit board. This manufacturing process is simple, reduces the production cost of glass circuit boards, and greatly reduces the production and operation pressure of enterprises. At the same time, the manufacturing process of this application, by sequentially depositing an aluminum metal film and a copper metal film on the surface of the glass substrate, with the aluminum metal film and the copper metal film working together to form a conductive copper-aluminum composite metal film, allows for an appropriate increase in the thickness of the aluminum metal film and an appropriate decrease in the thickness of the copper metal film, which helps to reduce the use of copper materials, thus saving copper resources and further reducing the production cost of glass circuit boards.
[0006] In some embodiments of the present invention, in step S5, a laser device emits a laser to etch the copper-aluminum composite metal film layer of the third glass substrate, selectively removing a portion of the copper-aluminum composite metal film layer, thereby forming a metal circuit area, a pad area, and an insulating blank area; in step S6, UV solder resist ink is screen-printed on the first surface of the fourth glass substrate on which the metal circuit pattern is provided, such that the UV solder resist ink covers the metal circuit area and the insulating blank area, and the pad area is exposed.
[0007] In some embodiments of the present invention, in step S6, after UV curing the UV solder resist ink on the first surface of the fourth glass substrate using a UV curing device, UV solder resist ink is screen-printed on the second surface of the fourth glass substrate, and then UV curing the UV solder resist ink on the second surface of the fourth glass substrate is performed using a UV curing device.
[0008] In some embodiments of the present invention, in step S6, the ultraviolet curing equipment used is a UV curing tunnel oven, and the UV curing time of the UV solder resist ink on the first surface of the fourth glass substrate is 30 to 60 seconds.
[0009] In some embodiments of the present invention, in step S6, the UV curing tunnel oven cures the UV solder resist ink on the second surface of the fourth glass substrate for 30 to 60 seconds.
[0010] In some embodiments of the present invention, in step S6, the wavelength of the ultraviolet light generated when the UV curing tunnel oven starts working is 365nm, the UV curing tunnel oven cures the UV solder resist ink on the first surface of the fourth glass substrate for 40 seconds, and the UV curing tunnel oven cures the UV solder resist ink on the second surface of the fourth glass substrate for 50 seconds.
[0011] In some embodiments of the present invention, the thickness of the glass substrate prepared in step S1 is 1.0~3.0 mm.
[0012] In some embodiments of the present invention, the thickness of the glass substrate prepared in step S1 is 1.2 mm, 1.5 mm, 2.0 mm, or 2.5 mm.
[0013] In some embodiments of the present invention, in step S1, the length of the prepared glass substrate is 1250 mm and the width of the glass substrate is 700 mm.
[0014] In some embodiments of the present invention, after step S6, a laser device is used to cut the whole glass circuit board obtained in step S6 into multiple small glass circuit boards of a predetermined size. Attached Figure Description
[0015] Figure 1 This is a flowchart of a glass circuit board manufacturing process according to certain embodiments of the present invention. Detailed Implementation
[0016] The embodiments of this implementation are described in detail below. Examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals denote the same or similar elements or elements having the same or similar functions throughout. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain this implementation, and should not be construed as limiting this implementation.
[0017] The accompanying drawings used in this embodiment are schematic and principle-based, and are only for the purpose of facilitating and simplifying the description of this embodiment. Therefore, they should not be construed as limiting this embodiment.
[0018] In the description of this embodiment, "several" means one or more, "multiple" means two or more, "greater than," "less than," and "exceeding" are understood to exclude the stated number, while "above," "below," and "within" are understood to include the stated number. The use of "first" and "second" in the description is merely for distinguishing technical features and should not be construed as indicating or implying relative importance, or implicitly indicating the number of indicated technical features, or implicitly indicating the order of the indicated technical features.
[0019] In the description of this embodiment, unless otherwise explicitly limited, terms such as "set up," "install," and "connect" should be interpreted broadly, and those skilled in the art can reasonably determine the specific meaning of the above terms in this embodiment in conjunction with the specific content of the technical solution.
[0020] Reference Figure 1 A manufacturing process for a glass circuit board according to certain embodiments of the present invention includes the following steps: S1. Prepare materials: Prepare a whole glass substrate, aluminum target and copper target. In this embodiment, the glass substrate is a whole piece of inorganic glass plate. Specifically, the glass substrate is a flat plate made of borosilicate glass by cutting and polishing. Since aluminum target and copper target are known technologies in the art, they will not be described in detail here. S2. Laser drilling: A laser device is used to drill holes in the glass substrate prepared in step S1, forming one or more through holes on the surface of the glass substrate to obtain a first glass substrate. The first glass substrate has a first surface and a second surface that are disposed opposite to each other. S3. Aluminum metal film layer: The first glass substrate obtained in step S2 and the aluminum target material prepared in step S1 are placed into the vacuum coating chamber of the vacuum coating equipment, with the first surface of the first glass substrate facing upward. Then the vacuum coating equipment is started, and the vacuum coating equipment works to deposit an aluminum metal film layer on the first surface of the first glass substrate to obtain the second glass substrate. S4. Copper metal film layer: The second glass substrate obtained in step S2 and the copper target material prepared in step S1 are placed into the vacuum coating chamber of the vacuum coating equipment, with the aluminum metal film layer of the second glass substrate facing upward. Then the vacuum coating equipment is started, and the vacuum coating equipment works and deposits a copper metal film layer on the surface of the aluminum metal film layer. At this time, the copper metal film layer and the aluminum metal film layer constitute a copper-aluminum composite metal film layer, and the third glass substrate is obtained. S5. Process the metal circuit pattern by using a laser device to etch the copper-aluminum composite metal film layer of the third glass substrate obtained in step S4, thereby forming a preset metal circuit pattern in the copper-aluminum composite metal film layer to obtain the fourth glass substrate. S6. Printing and curing ink: UV solder resist ink is screen-printed on the first surface of the fourth glass substrate with metal circuit patterns obtained in step S5. Then, UV curing equipment is used to perform UV curing treatment on the UV solder resist ink printed on the first surface to obtain a glass circuit board.
[0021] One embodiment of the present invention discloses a manufacturing process for a glass circuit board. This process involves using a glass substrate as the base material, drilling holes in the glass substrate using a laser device, and then sequentially depositing an aluminum metal film and a copper metal film on one side of the drilled glass substrate. These aluminum and copper metal films constitute a copper-aluminum composite metal film. The copper-aluminum composite metal film is then etched using a laser device to form a pre-defined metal circuit pattern. Finally, UV solder resist ink is screen-printed onto the surface of the metal circuit pattern and cured using ultraviolet light to obtain the desired glass circuit board. This manufacturing process is simple, reduces production costs for glass circuit boards, and significantly lowers the operational pressure on enterprises. Furthermore, by sequentially depositing aluminum and copper metal films on the surface of the glass substrate, the aluminum and copper metal films work together to form a conductive copper-aluminum composite metal film. Therefore, the thickness of the aluminum metal film can be appropriately increased, while the thickness of the copper metal film can be appropriately decreased, which helps reduce the use of copper materials, saving copper resources and further reducing the production cost of the glass circuit board. In another embodiment, the manufacturing process of a glass circuit board involves using a laser device to drill holes in the glass substrate, resulting in through holes on the surface of the manufactured glass circuit board. This allows external electrical wires to pass through the through holes from one side of the second surface of the glass circuit board and electrically connect to the metal circuit pattern on the first surface, facilitating the electrical connection between the glass circuit board and external circuits.
[0022] In some embodiments of the present invention, in step S5, the laser device emits a laser to etch the copper-aluminum composite metal film layer of the third glass substrate, selectively removing a portion of the copper-aluminum composite metal film layer, thereby forming a metal circuit area, a pad area, and an insulating blank area. Specifically, in this embodiment, the laser emitted by the laser device moves according to a preset circuit pattern, selectively ablates and removes the copper-aluminum composite metal film in a designated area, and the area of the remaining copper-aluminum composite metal film forms the metal circuit area and the pad area. The metal circuit area constitutes a conductive circuit, and the pad area is subsequently used for soldering with components or electrical wires. The area of the copper-aluminum composite metal film removed by the laser is exposed on the glass substrate, forming an insulating blank area. In step S6, UV solder resist ink is screen-printed on the first surface of the fourth glass substrate where the metal circuit pattern is provided, so that the UV solder resist ink covers the metal circuit area and the insulating blank area, exposing the pad area. Specifically, a screen printing stencil is fabricated to match the metal circuit pattern on the first surface of the fourth glass substrate. The stencil has cutout areas corresponding to the pad areas. When UV solder resist ink is printed onto the first surface of the fourth glass substrate through the screen printing stencil, the UV solder resist ink is only transferred to the non-cutout areas of the stencil. The UV solder resist ink passes through the non-cutout areas and covers the metal circuit area and the insulating blank area. The pad areas of the metal circuit pattern correspond to the cutout areas of the stencil, and the UV solder resist ink does not adhere to these pad areas, leaving them completely exposed. After single-sided screen printing, the fourth glass substrate is placed in a UV curing device for UV irradiation and curing. The UV solder resist ink cures under UV light, ultimately forming a solder resist layer on the first surface of the fourth glass substrate. This solder resist layer covers the metal circuit area and the insulating blank area, leaving the pad areas exposed. This facilitates subsequent soldering of components or wires to the pad areas without easily causing short circuits in the metal circuit area. Since the aforementioned UV solder resist ink and UV curing device are known technologies in the art, they will not be described in detail here.
[0023] In some embodiments of the present invention, in step S6, after UV curing the UV solder resist ink on the first surface of the fourth glass substrate using a UV curing device, UV solder resist ink is then screen-printed on the second surface of the fourth glass substrate, and then UV curing is performed on the UV solder resist ink on the second surface of the fourth glass substrate using a UV curing device. It should be noted that, since the second surface of the fourth glass substrate does not have any metal circuit patterns, in this embodiment, a second screen printing plate matching the second surface of the fourth glass substrate needs to be fabricated separately, and then the UV solder resist ink is printed onto the second surface of the fourth glass substrate using the second screen printing plate.
[0024] In some embodiments of the present invention, in step S6, the ultraviolet curing equipment used is a UV curing tunnel oven. The UV curing tunnel oven cures the UV solder resist ink on the first surface of the fourth glass substrate for 30-60 seconds, and cures the UV solder resist ink on the second surface of the fourth glass substrate for 30-60 seconds. Specifically, UV solder resist ink is printed on the first surface of the fourth glass substrate using a screen printing plate. Then, the fourth glass substrate is placed inside the UV curing tunnel oven, which starts operating and cures the UV solder resist ink printed on the first surface of the fourth glass substrate with ultraviolet light for 30-60 seconds. Afterward, the fourth glass substrate is removed from the UV curing tunnel oven, and then UV solder resist ink is printed on the second surface of the fourth glass substrate using a second screen printing plate. Then, the fourth glass substrate is placed back into the UV curing tunnel oven, which starts operating and cures the UV solder resist ink printed on the second surface of the fourth glass substrate with ultraviolet light for 30-60 seconds. Since the use of a UV curing tunnel oven for UV solder resist ink curing is a known technique in the art, it will not be described in detail here.
[0025] In some embodiments of the present invention, in step S6, the wavelength of the ultraviolet light generated when the UV curing tunnel oven starts working is 365nm, and the UV curing time for the UV solder resist ink on the first surface of the fourth glass substrate is 40 seconds; the UV curing time for the UV solder resist ink on the second surface of the fourth glass substrate is 50 seconds. By adopting the above method, the UV curing tunnel oven can better cure the UV solder resist ink printed on the first surface and the UV solder resist ink printed on the second surface, resulting in a better curing effect of the UV solder resist ink.
[0026] In some embodiments of the present invention, the thickness of the glass substrate prepared in step S1 is 1.0~3.0 mm. Specifically, the thickness of the glass substrate is 1.0 mm, 1.2 mm, 1.5 mm, 2.0 mm, 2.5 mm, or 3.0 mm. Therefore, glass circuit boards can be fabricated using glass substrates of different thicknesses, which can better meet the production needs of enterprises.
[0027] In some embodiments of the present invention, in step S1, the length of the prepared glass substrate is 1250 mm and the width is 700 mm. In some embodiments of the present invention, after step S6, a laser device is used to cut the whole glass circuit board obtained in step S6 into multiple small glass circuit boards of predetermined specifications. By using the above method, multiple small glass circuit boards can be produced at one time, thereby helping to improve production efficiency.
[0028] In some embodiments of the present invention, in step S2, before drilling holes in the glass substrate using a laser device, the glass substrate needs to be edge-ground, then cleaned to remove debris, and then dried. After drilling, the glass substrate needs to be cleaned again to remove debris or impurities generated during laser drilling. Since drilling the glass substrate using a laser device and drying the cleaned glass substrate using a dryer are both well-known techniques in the art, they will not be described in detail here.
[0029] Although embodiments of this implementation have been shown and described, those skilled in the art will understand that various changes, modifications, substitutions and variations can be made to these embodiments without departing from the principles and spirit of this implementation, the scope of which is defined by the claims and their equivalents.
Claims
1. A manufacturing process for a glass circuit board, characterized in that, Includes the following steps: S1. Prepare materials: prepare a whole glass substrate, aluminum target and copper target. S2. Laser drilling: A laser device is used to drill holes in the glass substrate to form one or more through holes on the surface of the glass substrate, thereby obtaining a first glass substrate. The first glass substrate has a first surface and a second surface that are disposed opposite to each other. S3. Aluminum metal film layer: The first glass substrate and the aluminum target are placed into the vacuum coating chamber of the vacuum coating equipment, so that the first surface of the first glass substrate faces upward. Then the vacuum coating equipment is started and an aluminum metal film layer is deposited on the first surface to obtain the second glass substrate. S4. Copper metal film layer: The second glass substrate and the copper target are placed into the vacuum coating chamber of the vacuum coating equipment, with the aluminum metal film layer facing upward. Then the vacuum coating equipment is started and a copper metal film layer is formed on the surface of the aluminum metal film layer. The copper metal film layer and the aluminum metal film layer constitute a copper-aluminum composite metal film layer, and a third glass substrate is obtained. S5. Processing metal circuit patterns: Using a laser device to emit a laser to etch the copper-aluminum composite metal film layer of the third glass substrate, thereby etching the copper-aluminum composite metal film layer to form a preset metal circuit pattern, and obtaining the fourth glass substrate. S6. Printing and curing ink: UV solder resist ink is screen-printed on the first surface of the fourth glass substrate on which the metal circuit pattern is provided, and then UV curing equipment is used to cure the UV solder resist ink printed on the first surface to obtain a glass circuit board.
2. The manufacturing process of a glass circuit board according to claim 1, characterized in that, In step S5, the laser device emits a laser to etch the copper-aluminum composite metal film layer on the third glass substrate, selectively removing part of the copper-aluminum composite metal film layer, thereby forming a metal circuit area, a pad area and an insulating blank area. In step S6, UV solder resist ink is screen-printed on the first surface of the fourth glass substrate where the metal circuit pattern is provided, so that the UV solder resist ink covers the metal circuit area and the insulating blank area, and the solder pad area is exposed.
3. The manufacturing process of a glass circuit board according to claim 2, characterized in that, In step S6, after UV curing the UV solder resist ink on the first surface of the fourth glass substrate using a UV curing device, UV solder resist ink is screen-printed on the second surface of the fourth glass substrate, and then UV curing the UV solder resist ink on the second surface of the fourth glass substrate is performed using a UV curing device.
4. The manufacturing process of a glass circuit board according to claim 3, characterized in that, In step S6, the ultraviolet curing equipment used is a UV curing tunnel oven, and the UV curing tunnel oven cures the UV solder resist ink on the first surface of the fourth glass substrate for 30 to 60 seconds.
5. The manufacturing process of a glass circuit board according to claim 4, characterized in that, In step S6, the UV curing tunnel oven cures the UV solder resist ink on the second surface of the fourth glass substrate for 30 to 60 seconds.
6. The manufacturing process of a glass circuit board according to claim 5, characterized in that, In step S6, the wavelength of the ultraviolet light generated when the UV curing tunnel oven starts working is 365nm. The UV curing tunnel oven cures the UV solder resist ink on the first surface of the fourth glass substrate for 40 seconds. The UV curing tunnel oven cures the UV solder resist ink on the second surface of the fourth glass substrate for 50 seconds.
7. The manufacturing process of a glass circuit board according to claim 1, characterized in that, The thickness of the glass substrate prepared in step S1 is 1.0~3.0 mm.
8. The manufacturing process of a glass circuit board according to claim 7, characterized in that, The thickness of the glass substrate prepared in step S1 is 1.2 mm, 1.5 mm, 2.0 mm, or 2.5 mm.
9. The manufacturing process of a glass circuit board according to claim 1, characterized in that, In step S1, the length of the prepared glass substrate is 1250 mm and the width of the glass substrate is 700 mm.
10. The manufacturing process of a glass circuit board according to claim 1, characterized in that, After step S6, a laser device is used to cut the entire glass circuit board obtained in step S6 into multiple small glass circuit boards of a predetermined size.