Gallium nitride HEMT power devices and their fabrication methods
By setting a hot electron trapping suppression layer with a larger bandgap inside the AlGaN barrier layer of the GaNHEMT device, the problem of hot electrons being easily trapped by interface states under hard switching conditions is solved, thereby improving dynamic resistance and stabilizing electrical parameters, reducing production costs, and adapting to different device design requirements.
Patent Information
- Application Number
- CN202611248167.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-18
- Publication Date
- 2026-11-17
Smart Images

Figure CN123124387A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of semiconductor power device technology, specifically to a gallium nitride HEMT power device and its fabrication method. Background Technology
[0002] The description in this section provides only background information relevant to the disclosure of this application and does not constitute prior art.
[0003] Figure 1 The diagram illustrates a typical GaN HEMT device structure in the prior art, which mainly includes a barrier layer (AlGaN) / channel layer (GaN) heterojunction structure, source / drain ohmic contacts, and a gate.
[0004] Reference Figure 2 As shown, when the device is in a hard-switching scenario, the high field and high current allow some charge carriers to gain sufficient energy to form hot electrons. These hot electrons have a chance to cross the barrier layer and be captured by a large number of interface states at the barrier / passivation layer interface, leading to a significant degradation of the device's dynamic resistance. The drain is usually under high voltage in the off-state and half-on-state, while the source and gate voltages are lower. Therefore, the closer to the drain, the greater the kinetic energy of the electrons, and the easier it is to form hot electrons. Thus, the closer to the drain, the more severe this capture effect.
[0005] Both existing mainstream improvement solutions have inherent flaws: The first approach involves optimizing the passivation layer material and fabrication process. However, changes to the passivation layer composition and thickness will simultaneously alter several core electrical parameters of the device, such as parasitic capacitance, sheet resistance, and breakdown voltage. This makes it difficult to consider all device performance indicators simultaneously, resulting in significant challenges in parameter matching.
[0006] The second option is to add a field plate structure. The drain field plate introduces an additional electric field in the vertical direction, which further aggravates the hot electron trapping phenomenon in the drain region and worsens the dynamic resistance degradation problem; the fabrication of the gate field plate and the source field plate requires additional photolithography masks, which significantly increases the chip manufacturing cost and is not conducive to large-scale mass production.
[0007] In summary, the existing technology lacks a GaNHEMT device structure that can efficiently suppress hot electron trapping, without deteriorating the device's electrical parameters, and without increasing manufacturing costs.
[0008] It should be noted that the above introduction to the technical background is only for the purpose of providing a clear and complete explanation of the technical solutions of this application and facilitating understanding by those skilled in the art. It should not be assumed that these technical solutions are known to those skilled in the art simply because they have been described in the background section of this application. Summary of the Invention
[0009] This application aims to address the technical problems of existing GaNHEMT devices, such as the easy capture of hot electrons by interface states and severe degradation of dynamic resistance under hard switching conditions, as well as the poor parameter compatibility or high production cost of existing passivation layer optimization and field plate structure improvement schemes.
[0010] To achieve the above objectives, this application provides the following technical solution: a gallium nitride (GaN) HEMT power device, comprising a substrate, a buffer layer, a channel layer, and a barrier layer stacked sequentially from bottom to top. A source, a gate, and a drain are disposed above the barrier layer. The device also includes a hot electron trapping suppression layer, at least a portion of which is located inside the barrier layer. At least a portion of the hot electron trapping suppression layer is located directly below the drain and extends towards the gate to the region between the drain and the gate. The bandgap of the hot electron trapping suppression layer is greater than the bandgap of the barrier layer. The lower surface of the hot electron trapping suppression layer is located between the upper and lower surfaces of the barrier layer. The hot electron trapping suppression layer is made of a semiconductor material.
[0011] Preferably, the material of the hot electron trapping suppression layer is AlN or GaO. x AlGaON, AlInN, AlInGaN, diamond, and Al with an aluminum content higher than the barrier layer. x2 Ga1₋ x2 Any one of N.
[0012] Preferably, the band gap of the hot electron trapping suppression layer is greater than 3.5 eV.
[0013] Preferably, the thickness of the hot electron trapping suppression layer ranges from 0.1 nm to 200 nm.
[0014] Preferably, the distance between the boundary of the hot electron trapping suppression layer near the gate and the gate is 0.1 nm to 50 μm.
[0015] Preferably, the upper surface of the hot electron trapping suppression layer is flush with or higher than the upper surface of the barrier layer.
[0016] This application discloses a method for fabricating a gallium nitride HEMT power device as described above, including the following steps: Epitaxial growth of buffer layer, channel layer and barrier layer on substrate; A mask layer is fabricated on the barrier layer; A hot electron trapping suppression layer is fabricated in the region of the barrier layer that is not covered by the mask layer; After the hot electron trapping suppression layer is prepared, all mask layers are removed; A gate electrode is fabricated on the barrier layer, and a source electrode and a drain electrode are fabricated on the barrier layer and the hot electron trapping suppression layer, respectively.
[0017] Preferably, the step "preparing a hot electron trapping suppression layer in the region of the barrier layer not covered by the mask layer" includes: depositing aluminum metal in the region of the barrier layer not covered by the mask layer, followed by high-temperature thermal annealing, causing aluminum atoms to diffuse downwards into the interior of the barrier layer to form Al x2 Ga1₋ x2 N is a hot electron trapping suppression layer, wherein the aluminum content x2 in the hot electron trapping suppression layer is greater than the aluminum content x1 in the barrier layer.
[0018] Preferably, the step "preparing a hot electron trapping suppression layer in the region of the barrier layer not covered by the mask layer" includes: applying oxygen plasma or introducing oxygen at high temperature to the region of the barrier layer not covered by the mask layer, so that oxygen reacts with AlGaN to generate an AlGaON hot electron trapping suppression layer in situ.
[0019] Preferably, the step "preparing a hot electron trapping suppression layer in the area of the barrier layer not covered by the mask layer" includes: first etching away a portion of the barrier layer not covered by the mask layer, and then depositing a hot electron trapping suppression layer, wherein the deposition thickness is greater than or equal to the thickness of the barrier layer removed by etching.
[0020] The beneficial effects of this application, based on the above technical solutions, are as follows: (1) Effectively suppresses hot electron trapping and improves the dynamic resistance degradation characteristics of the device: This application incorporates a hot electron trapping suppression layer with a wider bandgap inside the AlGaN barrier layer. This raises the energy threshold required for hot electrons to overcome the barrier, significantly reducing the number of hot electrons that cross the AlGaN barrier and are trapped at the passivation interface, thus mitigating the dynamic resistance degradation effect from a physical mechanism perspective. The hot electron trapping suppression layer is only located in the region of concentrated electric field below the drain electrode between the gate and drain, precisely targeting the location where hot electron generation is most severe, resulting in higher suppression efficiency.
[0021] (2) Without altering the passivation layer structure, the device's electrical parameters exhibit high stability: The improved structure of this application is located inside the AlGaN barrier layer, which does not require adjustment of the material, thickness and fabrication process of the outer passivation layer. It does not simultaneously change the electrical parameters of the device such as parasitic capacitance, sheet resistance and breakdown voltage. The device has good static performance consistency and avoids the parameter coupling defects of the passivation layer optimization scheme.
[0022] (3) No need to add a field plate structure, reducing chip manufacturing costs: This application relies on a built-in wide bandgap thin layer to achieve electric field modulation and hot electron blocking, eliminating the need to fabricate gate, source, or drain field plates and adding additional photolithography masks, thus simplifying the chip process and reducing mass production costs; at the same time, it avoids the defect of the drain field plate introducing a vertical electric field that exacerbates hot electron trapping.
[0023] (4) Semiconductor material is used as the hot electron trapping suppression layer to balance conductivity compatibility and reliability: The hot electron trapping suppression layer uses a wide bandgap semiconductor material, which allows a small number of charge carriers to conduct laterally, avoiding the problems of charge accumulation and electric field distortion caused by pure insulating media; the semiconductor and AlGaN barrier layer have a higher lattice matching degree and a low heterojunction trap density, so no new electron trapping sites are added; at the same time, the weak conductivity can slowly dissipate high-energy hot electrons, avoiding long-term charge accumulation that could lead to dielectric breakdown, and improving the long-term switching reliability of the device.
[0024] (5) The fabrication process is flexible and adaptable to different device design requirements: This application provides three differentiated fabrication processes that can be flexibly selected according to the device power level, precision requirements, and production cost needs: the aluminum diffusion annealing process requires no etching and causes minimal damage to the epitaxial layer; the oxygen recombination process has simple steps and is compatible with mature oxidation production lines; the etching deposition process allows for free control of the thickness and material type of the hot electron trapping suppression layer, and is suitable for customized production of high-voltage, high-power devices.
[0025] Specific embodiments of this application are disclosed in detail with reference to the following description and accompanying drawings, illustrating how the principles of this application can be employed. It should be understood that the embodiments of this application are not limited in scope. Within the spirit and scope of the appended claims, the embodiments of this application include many changes, modifications, and equivalents.
[0026] Features described and / or illustrated for one embodiment may be used in the same or similar manner in one or more other embodiments, combined with features in other embodiments, or substituted for features in other embodiments.
[0027] It should be emphasized that the term "including / comprises" as used herein refers to the presence of a feature, whole, step, or component, but does not exclude the presence or addition of one or more other features, wholes, steps, or components. Attached Figure Description
[0028] The accompanying drawings described herein are for illustrative purposes only and are not intended to limit the scope of this application in any way. Furthermore, the shapes and scales of the components in the drawings are merely illustrative to aid in understanding this application and do not specifically limit the shapes and scales of the components. Those skilled in the art, guided by the teachings of this application, can select various possible shapes and scales to implement this application according to specific circumstances. In the drawings: Figure 1 This is a schematic diagram of the structure of a GaN HEMT device in the prior art. Figure 2This is a schematic diagram of the hot electron trapping effect under hard-switching conditions in GaN HEMT technology. Figure 3 This is a schematic diagram of the layered structure of the gallium nitride HEMT power device in this application; Figures 4A-4E This is a schematic diagram of the complete fabrication process of the gallium nitride HEMT power device in this application.
[0029] The meanings of the markings in the attached diagram are as follows: 1. Substrate; 2. Buffer layer; 3. Channel layer; 4. Barrier layer; 51. Source; 52. Gate; 53. Drain; 6. Passivation layer; 7. Hot electron trapping suppression layer; 8. Mask layer. Detailed Implementation
[0030] To enable those skilled in the art to better understand the technical solutions in this application, the technical solutions in the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments. Based on the embodiments of this application, all other embodiments obtained by those skilled in the art without creative effort should fall within the scope of protection of this application.
[0031] It should be noted that when an element is referred to as being "set on" another element, it can be directly on the other element or there may be an intervening element. When an element is referred to as being "connected to" another element, it can be directly connected to the other element or there may be an intervening element. The terms "vertical," "horizontal," "left," "right," and similar expressions used herein are for illustrative purposes only and do not represent the only embodiments.
[0032] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this application belongs. The terminology used herein is for the purpose of describing particular embodiments only and is not intended to be limiting of the application. The term "and / or" as used herein includes any and all combinations of one or more of the associated listed items.
[0033] The various embodiments in this specification are described in a progressive manner. Similar or identical parts between embodiments can be referred to interchangeably. Each embodiment focuses on describing the differences from other embodiments. In particular, the system embodiments are basically similar to the method embodiments, so the description is relatively simple; relevant parts can be referred to the descriptions in the method embodiments.
[0034] It should be noted that in the description of this application, the terms "first," "second," etc., are used only for descriptive purposes and to distinguish similar objects; there is no order between them, nor should they be construed as indicating or implying relative importance. Furthermore, in the description of this application, unless otherwise stated, "multiple" means two or more.
[0035] Reference Figure 3 As shown in the figure, this application discloses a gallium nitride HEMT power device, including a substrate 1, a buffer layer 2, a channel layer 3, and a barrier layer 4 stacked sequentially from bottom to top. A source 51, a gate 52, and a drain 53 are disposed above the barrier layer 4. The device also includes a hot electron trapping suppression layer 7, at least a portion of which is located directly below the drain 53 and extends toward the gate 52 to the region between the drain 53 and the gate 52. The bandgap of the hot electron trapping suppression layer 7 is greater than the bandgap of the barrier layer 4. The lower surface of the hot electron trapping suppression layer 7 is located between the upper and lower surfaces of the barrier layer 4.
[0036] Specifically, the substrate 1 serves as the underlying support structure of the device. The substrate 1 can be made of conventional substrate materials, such as silicon substrate 1, sapphire substrate 1, or silicon carbide substrate 1, or it can be a composite of several materials, such as silicon on insulator (SOI). The thickness of the substrate 1 is generally in the range of 300µm-3000µm. In this embodiment, a silicon substrate 1 is preferably used to reduce manufacturing costs and facilitate compatibility with existing semiconductor processes. When using a Si substrate 1, its resistivity ranges from 0.001 to 5000 Ω·cm.
[0037] The buffer layer 2 is located on the substrate 1. The function of the buffer layer 2 is to alleviate lattice and thermal mismatch between the substrate 1 and the upper epitaxial layer, reduce the extension of defects and dislocations into the epitaxial layer, and provide a transition layer for subsequent high-quality epitaxial growth. The buffer layer 2 can be composed of different materials depending on the substrate 110 and specific requirements. For example, when using a silicon substrate 1, it can be composed of an AlN nucleation layer, one or more AlGaN transition layers, a superlattice buffer layer 2 formed by alternating periods of AlN and AlGaN, and a high-carbon layer (carbon concentration greater than 10%). 18 cm -3 It can be composed of GaN layers, or sequentially of AlN nucleation layers, one or more AlGaN layers, and high carbon (carbon concentration greater than 10). 18 cm -3 It consists of GaN layers.
[0038] The channel layer 3 is located above the buffer layer 2. Channel layer 3 is the main region containing the two-dimensional electron gas (2DEG) conductive channel in this device. Channel layer 3 can be formed of a semiconductor material, for example, a low-carbon material (carbon concentration less than 10⁻⁶). 18 cm -3 GaN is a high-carrier-mobility and good-thermal-stability material, making it suitable as a channel layer for power devices.
[0039] The barrier layer 4 is located above the channel layer 3. The barrier layer 4 can be formed of a semiconductor material, such as a ternary or quaternary alloy compound based on gallium nitride, such as Al. x Ga 1x N, AlInGaN, In x Ga 1x N, Al x In 1x Al, AlScN. In this embodiment, barrier layer 4 is a barrier layer 4. An AlGaN / GaN heterojunction is formed between barrier layer 4 and the underlying GaN channel layer 3. Due to the spontaneous polarization and piezoelectric polarization effects between AlGaN and GaN materials, a high-concentration, high-mobility two-dimensional electron gas is formed at the heterojunction interface near the GaN channel layer 3. This two-dimensional electron gas serves as the conductive channel when the device is turned on. The function of barrier layer 4 includes providing polarization effects to form the two-dimensional electron gas and bearing reverse bias voltage in the off state.
[0040] The source 51, gate 52, and drain 53 are all disposed above the barrier layer 4. Specifically, the source 51 and drain 53 are electrically connected to the barrier layer 4 and the two-dimensional electron gas below it through ohmic contacts, serving as the current input and output terminals of the device, respectively. The gate 52 is disposed between the source 51 and the drain 53. By applying a bias voltage to the gate 52, the concentration of the two-dimensional electron gas in the channel below the gate 52 can be adjusted, thereby controlling the conduction and turn-off of the device.
[0041] The gallium nitride HEMT power device of this application also includes a hot electron trapping suppression layer 7. At least a portion of the hot electron trapping suppression layer 7 is located inside the barrier layer 4. In other words, at least a portion of the hot electron trapping suppression layer 7 is embedded inside the barrier layer 4. Vertically, the lower surface of the hot electron trapping suppression layer 7 is located between the upper and lower surfaces of the barrier layer 4. In an optional embodiment, the upper surface of the hot electron trapping suppression layer 7 is flush with the upper surface of the barrier layer 4. In this embodiment, the hot electron trapping suppression layer 7 is completely embedded inside the barrier layer 4, and its upper surface is coplanar with the upper surface of the barrier layer 4. This structure facilitates the uniform coverage and planarization of the subsequent passivation layer 6, and the process implementation is relatively simple. In another optional embodiment, the upper surface of the hot electron trapping suppression layer 7 is higher than or slightly higher than the upper surface of the barrier layer 4. This structure is easier to achieve when using the "etching + deposition" scheme (i.e., first etch away part of the barrier layer 4, and then deposit the hot electron trapping suppression layer 7 material, with the deposition thickness being greater than the etching depth). Its advantage is that it can increase the effective thickness of the hot electron trapping suppression layer 7 without deepening the extension depth below the barrier layer 4, thereby obtaining a thicker barrier region without affecting the two-dimensional electron gas in the channel.
[0042] At least a portion of the hot electron trapping suppression layer 7 is located directly below the drain 53. That is, from a top-down view, the horizontal projection area of the hot electron trapping suppression layer 7 overlaps at least partially with the horizontal projection area of the drain 53. This positional relationship allows the hot electron trapping suppression layer 7 to function directly in the region below the drain 53. As mentioned earlier, under hard-switching conditions, the drain 53 is under high voltage in both the off and half-on states. Therefore, the region near the drain 53 has the highest electric field strength, where electrons acquire the highest kinetic energy and are most likely to become hot electrons, crossing the barrier layer 4 as they move towards its upper surface. Placing the hot electron trapping suppression layer 7 directly below the drain 53 means that hot electrons will first encounter this layer on their path from the channel to the upper surface of the barrier layer 4, thus providing a blocking effect at the location where suppression is most needed.
[0043] Furthermore, another portion of the hot electron trapping suppression layer 7 extends horizontally from the drain 53 towards the gate 52, and is located in the region between the drain 53 and the gate 52. That is, the hot electron trapping suppression layer 7 starts directly below the drain 53 and extends laterally towards the gate 52, ending in the region between the drain 53 and the gate 52, without extending directly below the gate 52. This design is based on the following reasons: Firstly, the hot electron effect is most severe near the drain 53, but the electric field strength gradually decreases with distance from the drain 53, and the kinetic energy and density of hot electrons also gradually decrease. Therefore, the hot electron trapping suppression layer 7 does not need to extend below the gate 52. Secondly, extending the hot electron trapping suppression layer 7 directly below the gate 52 might affect the gate 52's ability to control the channel, altering key parameters such as the device's threshold voltage and transconductance. Therefore, by controlling the extension endpoint of the hot electron trapping suppression layer 7 to the region between the drain 53 and the gate 52, effective suppression can be implemented in the high-risk region of hot electrons, while avoiding affecting the channel control function of the gate 52 region.
[0044] Furthermore, the distance between the boundary of the hot electron trapping suppression layer 7 near the gate 52 and the gate 52 is 0.1 nm to 50 μm. This distance further clarifies the horizontal distance between the hot electron trapping suppression layer 7 and the gate 52. In this embodiment, the distance can be 0.1 nm, 1 nm, 10 nm, 100 nm, 1 μm, 10 μm, 50 μm, or any value between any two of the above. Preferably, the distance is 1 nm to 10 μm. The actual value of this distance can be adjusted according to factors such as the specific size of the device, the channel length, and the operating voltage of the drain 53.
[0045] The band gap of the hot electron trapping suppression layer 7 is larger than that of the barrier layer 4. This is the core physical principle behind the suppression of hot electron trapping in this application. Specifically, the band gap of a conventional barrier layer 4 typically varies with the aluminum composition; in the range of approximately 15% to 30%, the band gap can be approximately 3.5 eV to 4.2 eV. In this application, the hot electron trapping suppression layer 7 uses a material with a band gap larger than that of the barrier layer 4. When hot electrons gain energy from the channel and move towards the upper surface of the barrier layer 4, the region exhibits a higher barrier height in its band structure than the surrounding barrier layer 4 due to the larger band gap of the hot electron trapping suppression layer 7. In other words, the hot electron trapping suppression layer 7 is equivalent to adding an "energy barrier" to the barrier layer 4. Hot electrons must have higher energy to cross this additional energy barrier, thus a large number of hot electrons with insufficient energy will be blocked by this energy barrier and unable to reach the AlGaN / passivation layer 6 interface, thereby reducing the probability of being trapped by the interface state. The reduction in the number of trapped hot electrons means that the degradation of dynamic resistance is effectively suppressed.
[0046] In this embodiment, the hot electron trapping suppression layer 7 is made of a semiconductor material. More preferably, the material of the hot electron trapping suppression layer 7 is selected from AlN and GaO. x AlGaON, AlInN, AlInGaN, diamond, and aluminum composition higher than barrier layer 4. x2 Ga1₋ x2 Any one of N.
[0047] The thickness of the hot electron trapping suppression layer 7 ranges from 0.1 nm to 200 nm. This thickness refers to the vertical dimension of the hot electron trapping suppression layer 7, i.e., the distance from the lower surface to the upper surface of the hot electron trapping suppression layer 7. Specifically, in this embodiment, the thickness of the hot electron trapping suppression layer 7 can be 0.1 nm, 0.5 nm, 1 nm, 5 nm, 10 nm, 20 nm, 50 nm, 100 nm, 150 nm, 200 nm, or any value between any two of the above values. Preferably, the thickness is 1 nm to 100 nm. More preferably, the thickness is 1 nm to 30 nm. It should be noted that the thickness of the hot electron trapping suppression layer 7 cannot be too thin (e.g., less than 0.1 nm), otherwise it will be difficult to form a continuous and effective energy barrier, and hot electrons will still have the opportunity to reach the interface through tunneling or by crossing the thin layer. Meanwhile, the thickness of the hot electron trapping suppression layer 7 should not be too thick (e.g., exceeding 200 nm), otherwise it may adversely affect the overall stress state and lattice quality of the barrier layer 4, and may also excessively consume the effective thickness of the barrier layer 4, affecting the breakdown voltage and other performance characteristics of the device. Within the above preferred range, sufficient barrier height can be formed to effectively block hot electrons, while maintaining the overall structural integrity of the barrier layer 4.
[0048] When the device is in the on state, an on-state voltage is applied to the gate 52, the concentration of the two-dimensional electron gas below the gate 52 increases, the channel is turned on, and charge carriers (electrons) flow from the source 51 through the channel to the drain 53, and the device is in a low-resistance on state.
[0049] When the device switches from the on state to the off state (e.g., during a hard switching process), the voltage at the drain 53 rapidly rises to a high voltage, while the voltages at the source 51 and gate 52 remain at a low potential. This results in the channel region near the drain 53 experiencing an extremely high electric field. In this high-field region, electrons in the channel are accelerated by the strong electric field, gaining kinetic energy far exceeding that of the thermal equilibrium state, thus becoming "hot electrons".
[0050] Some of these hot electrons move towards the upper surface of barrier layer 4. In existing devices, due to the limited bandgap of barrier layer 4, these hot electrons have a certain probability of crossing barrier layer 4 and reaching the interface between barrier layer 4 and passivation layer 6, where they are captured by the large number of interface state energy levels present at the interface. Once captured, these electrons will form a fixed negative charge at the interface, depleting the two-dimensional electron gas in the channel, causing the on-resistance of the device to increase significantly in subsequent conduction cycles, i.e., dynamic resistance degradation occurs.
[0051] In the device of this application, when hot electrons move from the channel to the upper surface of the barrier layer 4, they first encounter a hot electron trapping suppression layer 7 with a larger bandgap when they reach the region of the barrier layer 4 below the drain 53. This hot electron trapping suppression layer 7 forms a higher barrier height than the surrounding barrier layer 4 in the band structure. Hot electrons need to have higher energy to overcome this additional barrier, and most hot electrons (especially those with insufficient energy) will be blocked by this additional barrier and cannot reach the barrier layer 4 (AlGaN) / passivation layer 6 interface. Therefore, the number of electrons trapped by the interface state is significantly reduced, and the degradation of dynamic resistance is effectively suppressed.
[0052] Furthermore, since the hot electron trapping suppression layer 7 is only disposed in the region below the drain 53 and extends towards the gate 52 to the space between the drain 53 and the gate 52, the original two-dimensional electron gas conductivity and electric field distribution are basically unaffected in regions of the channel far from the drain 53 (e.g., regions near the source 51). This ensures that while suppressing hot electron trapping, the device's key performance parameters such as on-resistance, threshold voltage, and breakdown voltage will not undergo unexpected changes.
[0053] The following is combined with Figures 4A-4E This application provides a detailed description of the gallium nitride (GaN) HEMT power device fabrication method. The fabrication method provided in this application includes the following basic steps: Reference Figure 4A As shown, step S1: Epitaxially grow buffer layer 2, channel layer 3, and barrier layer 4 on substrate 1.
[0054] Specifically, a substrate 1 is provided, which may be a silicon substrate 1, a sapphire substrate 1, or a silicon carbide substrate 1, etc. In this embodiment, a silicon substrate 1 is preferably used. Using epitaxial growth techniques known in the art (e.g., metal-organic chemical vapor deposition, molecular beam epitaxy, etc.), a buffer layer 2, a GaN channel layer 3, and a barrier layer 4 are sequentially epitaxially grown on the substrate 1. The thickness of the buffer layer 2, the thickness of the GaN channel layer 3, and the thickness of the barrier layer 4, as well as the aluminum composition, can be selected and adjusted according to the performance requirements of the target device.
[0055] Reference Figure 4B As shown, step S2: prepare mask layer 8 on barrier layer 4.
[0056] Specifically, a mask layer 8 material is deposited or coated on the upper surface of the barrier layer 4. The mask layer 8 material can be a conventional photoresist or hard mask material (e.g., silicon oxide or silicon nitride). Subsequently, the mask layer 8 is patterned using a photolithography process, such that the mask layer 8 covers a portion of the area while exposing the area where the subsequent hot electron trapping suppression layer 7 needs to be fabricated. This exposed area corresponds to the region directly below the drain 53 in the final device and extends towards the gate 52 to the area between the drain 53 and the gate 52. In other words, the opening pattern of the mask layer 8 determines the position and extent of the hot electron trapping suppression layer 7 in the horizontal direction.
[0057] Reference Figure 4C As shown, step S3: a hot electron trapping suppression layer 7 is prepared in the region of the barrier layer 4 that is not covered by the mask layer 8.
[0058] In the exposed area not covered by the mask layer 8, a variety of processes can be used to form the hot electron trapping suppression layer 7.
[0059] Method 1: Deposit a metallic aluminum layer on the area of barrier layer 4 not covered by mask layer 8 (i.e., the exposed surface of barrier layer 4). The thickness of this aluminum layer can be selected according to the thickness of the target hot electron trapping suppression layer 7 and the aluminum diffusion depth, for example, it can be 0.5 nm to 10 nm.
[0060] Then, a high-temperature thermal annealing process is performed. During annealing, aluminum atoms gain sufficient kinetic energy to diffuse downwards from the deposited aluminum layer into the lower barrier layer 4. After entering the AlGaN lattice, aluminum atoms replace some of the lattice positions of Ga atoms, thereby increasing the aluminum content in that region. After annealing, the original AlGaN material with an aluminum content of 0.5% is transformed into Al material with an aluminum content of 0.5%. x2 Ga1₋ x2 Material N, wherein x2 is higher than the aluminum concentration x1 of barrier layer 4. As mentioned earlier, the higher the aluminum content, the larger the band gap, so this region forms a hot electron trapping suppression layer 7 with a band gap greater than that of barrier layer 4.
[0061] The advantages of this approach are as follows: aluminum atom diffusion propagates from the surface of barrier layer 4 inwards, therefore the lower surface of the formed hot electron trapping suppression layer 7 is located inside barrier layer 4 (determined by the diffusion depth), while the upper surface is flush with the upper surface of barrier layer 4 (because the modification is achieved through atomic doping on the original barrier layer 4 surface, without changing the surface height). This approach is simple to implement, has good compatibility with existing epitaxial and annealing processes, requires no additional etching steps, and causes minimal lattice damage to barrier layer 4. The specific temperature and time of high-temperature hot annealing can be adjusted according to the required diffusion depth and aluminum concentration distribution; for example, the annealing temperature can be 800℃~1200℃, and the annealing time can be 30 seconds~30 minutes.
[0062] Method 2: Oxygen Plasma / High-Temperature Oxygen Introduction Scheme In this scheme, step S3, "preparing a hot electron trapping suppression layer 7 in the region of the barrier layer 4 not covered by the mask layer 8", specifically includes: Oxygen plasma treatment is applied to the area of the barrier layer 4 that is not covered by the mask layer 8, or high-temperature heat treatment is performed in an oxygen atmosphere, so that oxygen reacts with AlGaN material to generate AlGaON (aluminum gallium oxynitride) composite hot electron trapping suppression layer 7 in situ.
[0063] Specifically, when using the oxygen plasma approach, a wafer with a mask layer 8 is placed in an oxygen plasma reaction chamber, and oxygen plasma is generated under radio frequency power excitation. The active oxygen radicals in the oxygen plasma react with the exposed AlGaN surface, and oxygen atoms partially replace nitrogen atom positions in the AlGaN lattice, forming an AlGaON complex. The introduction of oxygen broadens the bandgap in this region from approximately 3.5 eV to 4.2 eV for AlGaN to approximately 5 eV to 7 eV for AlGaON.
[0064] When using the oxygen atmosphere high-temperature processing method, the wafer with mask layer 8 is placed in a high-temperature furnace tube and subjected to high-temperature heat treatment in an oxygen atmosphere. Under high-temperature conditions, oxygen undergoes a thermal oxidation reaction with the exposed AlGaN surface, and an AlGaON composite is also formed in the surface region of barrier layer 4.
[0065] The advantages of this approach are: the AlGaON hot electron trapping suppression layer 7 is generated in situ by introducing oxygen atoms onto the original barrier layer 4. Therefore, the interface between the hot electron trapping suppression layer 7 and the barrier layer 4 is a continuous transition interface, without significant lattice mismatch issues. This approach also offers a wide process window, allowing for precise control of the thickness and oxygen content of the AlGaON hot electron trapping suppression layer 7 by adjusting the oxygen plasma treatment time / power or the oxygen atmosphere concentration / temperature / time, thereby controlling its bandgap value.
[0066] Method 3: In this scheme, step S3, "preparing a hot electron trapping suppression layer 7 in the region of the barrier layer 4 not covered by the mask layer 8", specifically includes: First, an etching process is performed on the area of barrier layer 4 not covered by mask layer 8 to remove a portion of the AlGaN material in that area. Etching can be performed using conventional dry etching methods (e.g., reactive ion etching, inductively coupled plasma etching, etc.) or wet etching processes. The etching depth determines the position of the lower surface of the subsequent suppression layer; that is, the lower surface of the suppression layer is the depth at which the bottom of the pit formed after etching is located. To ensure that the lower surface of the suppression layer is located between the upper and lower surfaces of barrier layer 4, the etching depth should be less than the total thickness of barrier layer 4.
[0067] Then, a hot electron trapping suppression layer 7 is deposited in the etched pit region. The deposited material can be AlN, GaOx, diamond, AlInN, AlInGaN, etc., all of which have a band gap greater than that of the AlGaN barrier layer 4.
[0068] Deposition can be performed using conventional thin film deposition techniques in the field, such as atomic layer deposition (ALD), chemical vapor deposition (CVD), physical vapor deposition (PVD), or pulsed laser deposition (PLD), depending on the type of material being deposited.
[0069] In this scheme, the deposition thickness is greater than or equal to the thickness of the barrier layer 4 removed by etching. When the deposition thickness is equal to the thickness of the barrier layer 4 removed by etching, the upper surface of the deposited suppression layer is flush with the upper surface of the barrier layer 4. When the deposition thickness is greater than the thickness of the barrier layer 4 removed by etching, the upper surface of the deposited suppression layer is higher than the upper surface of the barrier layer 4, that is, the suppression layer protrudes upward from the upper surface of the barrier layer 4 by a certain height. In this case, the protruding portion of the suppression layer is located outside the barrier layer 4 (i.e., above the upper surface of the barrier layer 4), while the pit filling portion remains inside the barrier layer 4.
[0070] The advantages of this approach are: the most flexible material selection, allowing the use of ultra-wide bandgap materials such as AlN and diamond to achieve the highest energy barrier; and the ability to flexibly adjust the total thickness of the suppression layer by controlling the deposition thickness to achieve the best blocking effect. This approach is particularly suitable for applications requiring ultra-high energy barriers to cope with extreme high-voltage / high-frequency operating conditions.
[0071] Reference Figure 4D As shown, step S4: After the hot electron trapping suppression layer 7 is prepared, remove all the mask layers 8.
[0072] Specifically, the mask layer 8 is completely removed from the surface of the barrier layer 4 using conventional removal processes in the art (e.g., wet stripping or dry ashing). After removing the mask layer 8, the upper surface of the barrier layer 4 is re-exposed in the area previously covered by the mask layer 8. At this point, the hot electron trapping suppression layer 7 has been formed in a predetermined area within the barrier layer 4, and its upper surface may be flush with or higher than the upper surface of the barrier layer 4 (depending on the specific method used in step S3).
[0073] Reference Figure 4E As shown, step S5 involves fabricating a gate electrode 52 on the barrier layer 4, and fabricating a source electrode 51 and a drain electrode 53 on the barrier layer 4 and the hot electron trapping suppression layer 7, respectively. Specifically, a metal deposition and patterning process is used to form the source electrode 51, the gate electrode 52, and the drain electrode 53 on the upper surface of the barrier layer 4. The gate electrode 52 is disposed on the upper surface of the barrier layer 4 and located between the source electrode 51 and the drain electrode 53. The position of the gate electrode 52 should satisfy the following condition: the boundary of the hot electron trapping suppression layer 7 near the gate electrode 52 should maintain a spacing of 0.1 nm to 50 μm between the gate electrode 52 and the gate electrode 52.
[0074] The source electrode 51 and the drain electrode 53 are respectively disposed at predetermined positions. The location of the drain electrode 53 satisfies the following condition: the drain electrode 53 overlaps with at least a portion of the hot electron trapping and suppression layer 7 in the horizontal direction, that is, at least part or all of the drain electrode 53 is located directly above the hot electron trapping and suppression layer 7 in the vertical direction. The source electrode 51 is disposed on the side away from the drain electrode 53. Both the source electrode 51 and the drain electrode 53 form ohmic contacts with the barrier layer 4, thereby forming an electrical connection with the two-dimensional electron gas below.
[0075] Reference Figure 3 As shown, in step S6, passivation layer 6 is prepared. After forming the gate 52, drain 53 and source 51, passivation layer 6 can be deposited, thereby completing the basic fabrication of the gallium nitride HEMT power device of this application.
[0076] In summary, this application, by introducing the hot electron trapping suppression layer 7, forms a localized energy barrier region inside the barrier layer 4, which precisely blocks high-energy hot electrons near the drain 53 from reaching the interface in a physical manner, fundamentally suppressing dynamic resistance degradation, without introducing various side effects and additional costs as in existing technical solutions.
[0077] It should be understood that the above description is for illustrative purposes and not for limitation. Many embodiments and applications beyond the provided examples will be apparent to those skilled in the art upon reading the above description. Therefore, the scope of this teaching should not be determined by reference to the above description, but rather by reference to the foregoing claims and the full scope of their equivalents. For purposes of completeness, all articles and references, including patent applications and publications, are incorporated herein by reference. The omission of any aspect of the subject matter disclosed herein in the foregoing claims is not intended as a waiver of that subject matter, nor should it be construed as an indication that the applicant has not considered that subject matter as part of the disclosed application subject matter.
Claims
1. A gallium nitride HEMT power device, comprising a substrate, a buffer layer, a channel layer, and a barrier layer stacked sequentially from bottom to top, wherein a source, a gate, and a drain are disposed above the barrier layer, characterized in that, It also includes a hot electron trapping suppression layer, at least a portion of which is located inside the barrier layer; At least a portion of the hot electron trapping suppression layer is located directly below the drain and extends toward the gate into the region between the drain and the gate; the bandgap of the hot electron trapping suppression layer is greater than the bandgap of the barrier layer; The lower surface of the hot electron trapping suppression layer is located between the upper and lower surfaces of the barrier layer, and the hot electron trapping suppression layer is a semiconductor material.
2. The gallium nitride HEMT power device according to claim 1, characterized in that, The material of the hot electron trapping suppression layer is AlN or GaO. x AlGaON, AlInN, AlInGaN, diamond, and Al with an aluminum content higher than the barrier layer. x2 Ga1₋ x2 Any one of N.
3. The gallium nitride HEMT power device according to claim 1, characterized in that, The band gap of the hot electron trapping suppression layer is greater than 3.5 eV.
4. The gallium nitride HEMT power device according to claim 1, characterized in that, The thickness of the hot electron trapping suppression layer ranges from 0.1 nm to 200 nm.
5. The gallium nitride HEMT power device according to claim 1, characterized in that, The distance between the boundary of the hot electron trapping suppression layer near the gate and the gate is 0.1 nm to 50 μm.
6. The gallium nitride HEMT power device according to claim 1, characterized in that, The upper surface of the hot electron trapping suppression layer is flush with or higher than the upper surface of the barrier layer.
7. A method for fabricating a gallium nitride HEMT power device according to any one of claims 1 to 6, characterized in that, Includes the following steps: Epitaxial growth of buffer layer, channel layer and barrier layer on substrate; A mask layer is fabricated on the barrier layer; A hot electron trapping suppression layer is fabricated in the region of the barrier layer that is not covered by the mask layer; After the hot electron trapping suppression layer is prepared, all mask layers are removed; A gate electrode is fabricated on the barrier layer, and a source electrode and a drain electrode are fabricated on the barrier layer and the hot electron trapping suppression layer, respectively.
8. The method for fabricating a gallium nitride HEMT power device according to claim 7, characterized in that, The step "Preparing a hot electron trapping suppression layer in the region of the barrier layer not covered by the mask layer" includes: depositing aluminum metal in the region of the barrier layer not covered by the mask layer, followed by high-temperature thermal annealing to allow aluminum atoms to diffuse downwards into the interior of the barrier layer, forming Al x2 Ga1₋ x2 N is a hot electron trapping suppression layer, wherein the aluminum content x2 in the hot electron trapping suppression layer is greater than the aluminum content x1 in the barrier layer.
9. The method for fabricating a gallium nitride HEMT power device according to claim 7, characterized in that, The step "preparing a hot electron trapping suppression layer in the region of the barrier layer not covered by the masking layer" includes: applying oxygen plasma or introducing oxygen at high temperature to the region of the barrier layer not covered by the masking layer, so that oxygen reacts with AlGaN to generate an AlGaON hot electron trapping suppression layer in situ.
10. The method for fabricating a gallium nitride HEMT power device according to claim 7, characterized in that, The step "preparing a hot electron trapping suppression layer in the region of the barrier layer not covered by the mask layer" includes: first etching away a portion of the barrier layer not covered by the mask layer, and then depositing a hot electron trapping suppression layer, wherein the deposition thickness is greater than or equal to the thickness of the barrier layer removed by etching.