A silicon photonics process for self-aligned implantation and low contact resistance of asymmetric PN junctions

By forming an asymmetric PN junction through self-aligned implantation and pre-amorphization implantation, the problems of photolithographic alignment deviation and high contact resistance are solved, enabling the manufacturing of silicon photonic chips with high consistency and low power consumption, and improving modulation bandwidth and mass production yield.

CN123124686APending Publication Date: 2026-11-17ARROW (SHENZHEN) PHOTONICS TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611348663.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-02
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In existing technologies, photolithographic alignment deviations and high contact resistance limit the modulation bandwidth and yield of silicon-based high-speed electro-optic modulators, resulting in poor device performance consistency and making it difficult to achieve mass production of ultra-high-speed, low-power silicon photonic chips.

Method used

Asymmetric PN junctions are formed using a self-aligned implantation process. By combining pre-amorphization implantation and self-aligned metal silicide processes, the PN junctions are precisely assembled through tilted-angle ion implantation and high-precision photolithography. A low-resistivity metal silicide layer is formed in the contact area to eliminate photolithographic alignment deviations and reduce contact resistance.

Benefits of technology

It achieves zero alignment fluctuation, reduces contact resistivity, increases electro-optic modulation bandwidth, shortens manufacturing cycle, improves wafer mass production yield, and meets the requirements of ultra-high-speed transmission.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124686A_ABST
    Figure CN123124686A_ABST
Patent Text Reader

Abstract

This invention discloses a silicon photonics process for self-aligned implantation and low contact resistance of asymmetric PN junctions, relating to the field of semiconductor optoelectronic device manufacturing. The method first retains a hard mask layer on top of the ridge waveguide of the SOI substrate. Utilizing the photolithography window bias and the mesa shadow blocking effect of the hard mask layer, self-aligned implantation and precise splicing of the P-region and N-region are achieved through ion implantation at first and second tilt angles, respectively, completely eliminating photolithography errors. Furthermore, by combining pre-amorphization implantation (PAI), millisecond-level laser annealing, and self-aligned metal silicide (Salicide) technology, extremely low resistivity ohmic contacts are formed in the side contact areas; or a double-layer hard mask combined with multi-step stepped implantation and selective epitaxial growth (SEG) is used to construct steep junction depths and strained contact layers. This invention significantly improves the positional accuracy and electro-optic modulation bandwidth of the PN junction, reduces contact resistance and waveguide loss, and is suitable for mass production of high-speed silicon-based optical modules.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of semiconductor integrated circuit manufacturing technology and photonic integration technology, specifically relating to a process method for manufacturing asymmetric PN junction active region modulators with high precision and high consistency on silicon-based photonic wafers. Background Technology

[0002] In the industrial mass production of silicon-based high-speed electro-optic modulators (such as Mach-Zehnder modulators (MZM) and micro-ring modulators (MRM), overlay / alignment error of photomasks and contact resistance (Rc) are the two most critical factors limiting the modulation bandwidth of devices and reducing wafer yield.

[0003] Firstly, photolithographic alignment deviation and PN junction misalignment: Asymmetric PN junction modulators, by precisely positioning the physical boundary of the PN junction at a specific location tens of nanometers away from the geometric center of the waveguide (e.g., within a range of 100nm ± 10nm), can significantly improve modulation efficiency (reducing Vπ) while ensuring low insertion loss. However, if the conventional method of alternating exposure of P-injection masks and N-injection masks is used, the actual offset of the PN junction between different chips (dies) on the wafer, or even between different modulators within the same chip, will fluctuate greatly due to the inherent superposition alignment deviation of ±20nm to ±40nm in the scanner. This will cause characteristic impedance mismatch, junction capacitance detuning, and extremely uneven modulation efficiency, which will seriously reduce the consistency of device performance.

[0004] Secondly, high contact resistance and RC delay limitations: As single-wavelength rates evolve towards 200 Gbps (PAM4) and 1.6T optical modules, the 3dB electro-optic bandwidth requirement for modulators increases to over 50 GHz. In traditional silicon photonics processes, high-concentration doped regions (P... ++ / N ++ The contact resistance between the metal plug (Via) and the metal plug is relatively high (typically Rc > 100Ω). If the doping concentration is blindly increased to reduce resistance, it will be limited by the upper limit of impurity solid solubility in silicon and lead to severe lattice defects; if the contact hole area is increased, parasitic capacitance will be introduced, increasing RC delay, resulting in accelerated high-frequency attenuation and a significant increase in power consumption.

[0005] Therefore, developing a silicon photonics integration process that can completely eliminate the influence of photolithography alignment deviations and significantly reduce electrode contact resistance is an urgent need for the industry to achieve mass production of ultra-high-speed, low-power silicon photonics chips.

[0006] In summary, developing an integrated solution that can completely eliminate the influence of photolithography alignment deviations on asymmetric PN junction self-alignment and simultaneously achieve ultra-low contact resistance has become an urgent need for the mass production of ultra-high-speed, low-power silicon photonic chips. Summary of the Invention

[0007] The purpose of this invention is to overcome the problems of large junction position deviation and low device performance consistency in wafer-scale mass production of asymmetric PN junction modulators due to the limitation of alignment accuracy of photolithography exposure machines, and to provide a high-tolerance, self-aligned manufacturing process.

[0008] To achieve the above objectives, the present invention adopts the following technical solution: a silicon photonics process method for self-aligned injection and low contact resistance of asymmetric PN junctions, comprising the following steps: Step S1: Form a ridge waveguide on the SOI substrate and retain a hard mask layer on top of the ridge waveguide; Step S2: Perform P-region photolithography and self-aligned implantation: Form a P-region window biased on the left side of the ridge waveguide, with the right edge of the P-region window terminating at the middle of the hard mask layer; use a first ion beam to implant from left to right at a first tilt angle, and utilize the mesa shadow of the hard mask layer to form an acceptor distribution extending from the left side to the right side off from the geometric center within the waveguide. Step S3: Perform N-region photolithography and self-aligned implantation: form an N-region window biased on the right side of the ridge waveguide, and use a second ion beam to implant from right to left at a second tilt angle to complete the precise splicing of the PN junction. Step S4: Perform annealing to activate implanted ions and lock the PN junction interface.

[0009] The preferred embodiment is that the values ​​of the first tilt angle and the second tilt angle are both in the range of 5° to 10°; the material of the hard mask layer is SiO2 or Si3N4, and the thickness is 80nm to 100nm.

[0010] The preferred embodiment is that, in the P-region photolithography and self-aligned implantation steps, the first ion beam is boron (B). 11 The second ion beam is phosphorus (P) ions, implanted at an energy of 10 keV to 20 keV, with a dose of 1.0 × 10^13 cm^-2 to 1.5 × 10^13 cm^-2; in the N-region photolithography and self-aligned implantation steps, the second ion beam is phosphorus (P) ions. 31Ions were implanted at an energy of 30 keV to 40 keV and a dose of 1.5 × 10^13 cm^-2 to 2.5 × 10^13 cm^-2.

[0011] The preferred embodiment is as follows: in the annealing process, high-speed peak annealing is used, the annealing temperature is 950℃~1050℃, and the annealing time is 5 seconds~15 seconds.

[0012] The preferred embodiment is as follows: after completing the locking of the PN junction interface in step S4, an integrated process step with high bandwidth and low contact resistance is further included: Step S5: Perform pre-amorphization implantation in the side contact area away from the waveguide center to break the silicon surface layer into an amorphous silicon layer; Step S6: Perform extremely high concentration gradient implantation in the pre-amorphized implantation region, and then perform millisecond-level laser annealing to restore the amorphous silicon layer to a single crystal. Step S7: Deposit a metal alloy layer and perform rapid thermal annealing and selective wet etching to form a self-aligned metal silicide layer on the surface of the heavily doped region.

[0013] The preferred embodiment is that the pre-amorphization implantation in step S5 uses Ge 74 Ions implanted to a depth of 30 nm to 50 nm; the extremely high concentration gradient implantation uses BF2+ ions in the P-region and As ions in the N-region. 75 Ions; the millisecond-level laser annealing time is 0.5ms~2ms.

[0014] The preferred embodiment is as follows: the metal alloy layer in step S7 is a Ni-Pt alloy layer, and the rapid thermal annealing includes two steps: the first step temperature is 300℃~400℃, and the second step temperature is 450℃~500℃; the self-aligned metal silicide layer formed is a NiSi phase with a thickness of 20nm~25nm.

[0015] The preferred embodiment is as follows: the hard mask layer in step S1 is a double-layer hard mask structure, including a pad oxide layer and a silicon nitride layer; the self-aligned implantation of the P region and N region adopts a stepped self-aligned implantation with a combination of multi-step tilt angle and energy, so that the vertical sidewalls of the PN junction exhibit a steep distribution.

[0016] The preferred embodiment is as follows: the stepped self-aligned injection includes: P-region deep implantation uses B++ ions with energies of 25keV~35keV, while shallow implantation uses BF2+ ions with energies of 8keV~12keV. N-region deep implantation uses As++ ions with energies of 55keV~65keV, while shallow implantation uses As+ ions with energies of 18keV~22keV. The tilt angle of the stepped self-aligned injection of the multi-step tilt angle and energy combination ranges from 10° to 15°.

[0017] The preferred embodiment is as follows: after completing the stepped self-aligned injection, selective epitaxial growth (SEG) is performed in the side contact area; a SiGe:B strained contact layer is epitaxially grown in the P region, a Si:C strained contact layer is epitaxially grown in the N region, and then a self-aligned metal silicide layer is formed.

[0018] The beneficial effects of this invention are as follows: 1. Zero Overlay Deviation: The PN junction injection boundary in steps 1-4 is determined by the high-precision waveguide physical stage and tilt angle geometry, completely eliminating the limitation of the exposure machine's alignment accuracy (±30nm), and reducing the standard deviation of the PN junction offset between chips to within ±1.5nm.

[0019] 2. Ultra-low contact resistance: After introducing pre-amorphization implantation and self-aligned NiSi silicide processes, the contact resistivity is reduced to 1.0 × 10⁻⁶. Below 8Ω·cm2, the contact resistance Rc drops to below 15Ω·μm, significantly reducing the RC time constant.

[0020] 3. Significantly improved high-frequency modulation bandwidth: While maintaining low insertion loss (<0.8dB / mm), the electro-optic modulation bandwidth is increased by more than 60% compared with traditional processes, fully meeting the 112Gbps / 220Gbps PAM4 transmission requirements.

[0021] 4. Simplified process and reduced costs: One to two high-precision photomask processes have been reduced, significantly shortening the manufacturing cycle and increasing the wafer mass production yield from the traditional <65% to >95%. Attached Figure Description

[0022] The preferred embodiment of the coplanar waveguide transmission line structure according to the present invention will now be described with reference to the accompanying drawings. In the drawings: Figure 1 A process flow diagram for PN junction self-aligned injection and low contact resistance according to the present invention; Figures 2a-2d This is a schematic diagram of the waveguide forming and hard mask retention in steps S1-S4 of Example 1; Figure 3a This is a schematic diagram of the integrated high-bandwidth self-aligned PN junction and low contact resistance (PAI + Salicide) process in step 5 of Example 2; Figure 3b This is a schematic diagram of the structure of the dielectric layer before the deposition of the metal in the complete electrode interconnect cross-section structure of Example 2; Figure 4 This is a schematic diagram of the structure formed by the double-layer hard mask and the double-sided stepped injection / epitaxy in Example 3. Detailed Implementation

[0023] To make the objectives, technical solutions, and advantages of this application clearer, the technical solutions of this application will be clearly and completely described below with reference to the accompanying drawings in the embodiments of this application. Obviously, the described embodiments are only some embodiments of this application, not all embodiments. Based on the embodiments in this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.

[0024] In the description of this invention, "several" means one or more, "multiple" means two or more, "greater than," "less than," and "exceeding" are understood to exclude the stated number, while "above," "below," and "within" are understood to include the stated number. The use of "first" and "second" in the description is merely for distinguishing technical features and should not be construed as indicating or implying relative importance, or implicitly indicating the number of indicated technical features, or implicitly indicating the order of the indicated technical features.

[0025] In the description of this invention, unless otherwise explicitly defined, terms such as "setup" should be interpreted broadly, and those skilled in the art can reasonably determine the specific meaning of the above terms in this invention in conjunction with the specific content of the technical solution.

[0026] In the description of this invention, the terms "one embodiment," "some embodiments," "illustrative embodiment," "example," "specific example," or "some examples," etc., refer to specific features or characteristics described in connection with that embodiment or example, which are included in at least one embodiment or example of the invention. In this specification, the illustrative expressions of the above terms do not necessarily refer to the same embodiment or example. Furthermore, the specific features or characteristics described may be combined in any suitable manner in one or more embodiments or examples.

[0027] like Figure 1 As shown: The process of self-aligned implantation of an asymmetric PN junction includes the following steps: Step S1: Form a ridge waveguide on the SOI substrate and retain a hard mask layer on top of the ridge waveguide; Step S2: Perform P-region photolithography and self-aligned implantation: Form a P-region window biased on the left side of the ridge waveguide, with the right edge of the P-region window terminating at the middle of the hard mask layer; use a first ion beam to implant from left to right at a first tilt angle, and utilize the mesa shadow of the hard mask layer to form an acceptor distribution extending from the left side to the right side off from the geometric center within the waveguide. Step S3: Perform N-region photolithography and self-aligned implantation: form an N-region window biased on the right side of the ridge waveguide, and use a second ion beam to implant from right to left at a second tilt angle to complete the precise splicing of the PN junction. Step S4: Perform annealing to activate implanted ions and lock the PN junction interface.

[0028] It also includes an integrated process step that combines high bandwidth and low contact resistance: Step S5: Perform pre-amorphization implantation in the side contact area away from the waveguide center to break the silicon surface layer into an amorphous silicon layer; Step S6: Perform extremely high concentration gradient implantation in the pre-amorphized implantation region, and then perform millisecond-level laser annealing to restore the amorphous silicon layer to a single crystal. Step S7: Deposit a metal alloy layer and perform rapid thermal annealing and selective wet etching to form a self-aligned metal silicide layer on the surface of the heavily doped region.

[0029] Example 1, Figures 2a to 2d are schematic diagrams of the formation process of the off-angle self-aligned asymmetric PN junction based on 220nm SOI according to Embodiment 1 of the present invention.

[0030] First, step S1, waveguide shaping and hard mask retention: as follows Figure 2a As shown: On a 220 nm SOI (Top Si 220 nm, BOX 2.0 μm) substrate, SiO2 with a thickness of 80 nm was deposited as a hard mask (HM) using plasma enhanced chemical vapor deposition (PECVD).

[0031] By utilizing immersion lithography and dry etching (ICP-RIE, which stands for Inductively Coupled Plasma - Reactive Ion Etching, where ICP is responsible for "chemical etching" and RIE is responsible for "physical bombardment and ensuring perpendicularity," the combination of the two can achieve high etching rate and extremely high anisotropy) with an etching width of 193 nm and an etching depth of 150 nm, a ridge waveguide with a ridge height of 220 nm, a plate thickness of 70 nm, and a width of 500 nm is formed. After etching, the top of the waveguide retains an 80 nm thick SiO2 hard mask intact.

[0032] Secondly, step S2, as follows Figure 2bAs shown in the table: Photolithography and self-aligned implantation are performed in the P-region, photoresist is coated, and a P-region window is created through exposure. Since the P-region window is offset to the left side of the waveguide, the right edge of the window terminates in the middle of the SiO2 hard mask at the top of the waveguide. Boron (B) is used. 11 Ion implantation was performed at an energy of 15 keV and a dose of 1.2 × 10⁻⁶. 13 cm -2 With an injection angle of θ = 7°, the ion beam is tilted from left to right. Due to the obstruction of the platform shadow, the injected material forms an acceptor distribution that extends from the left side of the waveguide to the right side, 100 nm away from the geometric center.

[0033] Furthermore, in step S3, as... Figure 2c As shown: N-region photolithography and implantation: Similarly, an N-region window is opened on the right, and phosphorus (P) is implanted at an energy of 35 keV. 31 ) ions, dose 2.0 × 10 13 cm -2 The ion beam is injected at an angle of θ=7° and tilted from right to left to complete the precise splicing.

[0034] Finally, step S4, as follows Figure 2d As shown: Annealing lock: High-speed spike annealing at 1000℃ for 10 seconds activates dopant ions, suppresses impurity lateral diffusion, and locks the PN junction interface.

[0035] Example 2 High-bandwidth self-aligned PN junction with low contact resistance (PAI + Salicide) integrated process.

[0036] Step S5, as follows Figure 3a As shown: After completing the self-aligned implantation of the PN active region through pre-amorphization implantation (PAI) in the flank contact region, Ge is implanted in the contact region 1.2 μm away from the waveguide center. 74 Ions break down the 40 nm silicon surface layer into an amorphous silicon layer (a-Si).

[0037] Step S6, extremely high concentration gradient injection (P ++ / N ++ BF was injected into the left PAI region after laser annealing. 2+ As injected into the right PAI region 75 After 1 ms laser annealing, the amorphous silicon layer was restored to a high-quality single crystal, and the activity concentration increased to 1.2 × 10²⁰ cm⁻¹. 3.

[0038] In step S7, a Ni-Pt alloy layer is selectively grown and deposited using self-aligned metal silicide (Salicide). After two-step rapid thermal annealing (RTA-1: 350°, RTA-2: 480°) and selective wet etching, an ultrathin NiSi phase with low resistivity is formed only on the surface of the heavily doped region, with a thickness of 22 nm.

[0039] like Figure 3b As shown: Finally, it also includes depositing a pre-metal dielectric (PMD) layer on the cross-sectional structure of the complete electrode interconnect (including tungsten plugs and metal layers), filling the openings with tungsten plugs (W Plugs), and fabricating anode and cathode electrodes.

[0040] Example 3 This embodiment is formed by a double-layer hard mask facing the 1.6T module and double-sided step injection / epitaxy.

[0041] As shown in Figure 4: The dual-layer hard mask (Si3N4 / SiO2) structure and waveguide shaping: 30 nm SiO2 (pad oxide layer) and 70 nm Si3N4 (total hard mask thickness 100 nm) are deposited on a 300 nm Top-Si wafer, and a 550 nm wide waveguide is etched out.

[0042] The multi-step tilt / energy combined ladder self-aligned injection system has an angle of θ=12°, where the deep region uses a 30 keV B-type laser. ++ Injection, shallow zone using 10 keV BF 2+ Injection, with an injection angle of θ=12°, and 60 keV As in the deep region. ++ Injection was performed, with the shallow region using 20 keV As. + The injection process creates a near-right-angled, steep distribution on the vertical sidewalls of the PN junction, with an approximate offset of 90 nm.

[0043] Selective epitaxial growth (SEG) and in-situ silicide contact ultimately result in the selective epitaxial growth of 15 nm SiGe:B (P-region) and Si:C (N-region) strained contact layers in the flank contact area, followed by the formation of a self-aligned NiSi layer, achieving the ultimate high-frequency electro-optic response performance.

[0044] To verify the technical superiority of the present invention, performance tests were conducted on 800G / 1.6T silicon-based Mach-Zehnder modulators manufactured using the traditional dual-mask alternating exposure process and the self-aligned low contact resistance process of the present invention on 12-inch SOI wafers of the same product.

[0045] Table 1 shows a comparison of the star energy between the traditional dual-mask exposure injection process and the self-aligned low-contact-resistance process.

[0046] As can be seen from Table 1, by utilizing the self-aligned + low contact resistance process of this application to improve chip performance, the standard deviation of the PN junction offset is reduced to within ±1.8nm, the contact resistance Rc is reduced to below 15Ω·μm, and the RC time constant is significantly reduced; the electro-optic modulation bandwidth is increased by more than 60% compared with the traditional process, fully meeting the 112Gbps / 220Gbps PAM4 transmission requirements, and the wafer mass production yield is improved from the traditional <65% to >95%. Those skilled in the art will understand that, without conflict, the above-mentioned preferred solutions can be freely combined and superimposed.

[0047] It should be understood that the above embodiments are merely exemplary and not restrictive. Various obvious or equivalent modifications or substitutions that can be made by those skilled in the art regarding the above details without departing from the basic principles of the present invention will be included within the scope of the claims of the present invention.

Claims

1. A silicon photonics process for self-aligned implantation and low contact resistance of asymmetric PN junctions, characterized in that, Includes the following steps: Step S1: Form a ridge waveguide on the SOI substrate and retain a hard mask layer on top of the ridge waveguide; Step S2: Perform P-region photolithography and self-aligned implantation: Form a P-region window biased on the left side of the ridge waveguide, with the right edge of the P-region window terminating at the middle of the hard mask layer; use a first ion beam to implant from left to right at a first tilt angle, and utilize the mesa shadow of the hard mask layer to form an acceptor distribution extending from the left side to the right side off from the geometric center within the waveguide. Step S3: Perform N-region photolithography and self-aligned implantation: form an N-region window biased on the right side of the ridge waveguide, and use a second ion beam to implant from right to left at a second tilt angle to complete the precise splicing of the PN junction. Step S4: Perform annealing to activate implanted ions and lock the PN junction interface.

2. The method according to claim 1, characterized in that, The first tilt angle and the second tilt angle both range from 5° to 10°; the hard mask layer is made of SiO2 or Si3N4 and has a thickness of 80nm to 100nm.

3. The method according to claim 1, characterized in that, In the P-region photolithography and self-aligned implantation step of step S2, the first ion beam is boron (B). 11 The second ion beam is phosphorus (P) ions, implanted at an energy of 10 keV to 20 keV, with a dose of 1.0 × 10^13 cm^-2 to 1.5 × 10^13 cm^-2; in the N-region photolithography and self-aligned implantation step of step S3, the second ion beam is phosphorus (P) ions. 31 Ions were implanted at an energy of 30 keV to 40 keV and a dose of 1.5 × 10^13 cm^-2 to 2.5 × 10^13 cm^-2.

4. The method according to claim 1, characterized in that, In the annealing process of step S4, high-speed peak annealing is used, the annealing temperature is 950℃~1050℃, and the annealing time is 5 seconds~15 seconds.

5. The method according to any one of claims 1 to 4, characterized in that, After completing step 4 of locking the PN junction interface, the process also includes an integrated process step that achieves high bandwidth and low contact resistance: Step S5: Perform pre-amorphization implantation in the side contact area away from the waveguide center to break the silicon surface layer into an amorphous silicon layer; Step S6: Perform extremely high concentration gradient implantation in the pre-amorphized implantation region, and then perform millisecond-level laser annealing to restore the amorphous silicon layer to a single crystal. Step S7: Deposit a metal alloy layer and perform rapid thermal annealing and selective wet etching to form a self-aligned metal silicide layer on the surface of the heavily doped region.

6. The method according to claim 5, characterized in that, The pre-amorphization implantation in step S5 uses Ge 74 Ions implanted to a depth of 30 nm to 50 nm; the extremely high concentration gradient implantation uses BF2+ ions in the P-region and As ions in the N-region. 75 Ions; the millisecond-level laser annealing time is 0.5ms~2ms.

7. The method according to claim 5, characterized in that, The metal alloy layer in step S7 is a Ni-Pt alloy layer. The rapid thermal annealing includes two steps: the first step temperature is 300℃~400℃, and the second step temperature is 450℃~500℃. The self-aligned metal silicide layer formed is a NiSi phase with a thickness of 20nm~25nm.

8. The method according to any one of claims 1 to 4, characterized in that, The hard mask layer in step S1 is a double-layer hard mask structure, including a pad oxide layer and a silicon nitride layer; the self-aligned implantation of the P region and N region adopts a stepped self-aligned implantation with a combination of multi-step tilt angle and energy, so that the vertical sidewalls of the PN junction exhibit a steep distribution.

9. The method according to claim 8, characterized in that, The stepped self-aligned injection includes: P-area deep injection uses B ++ Ions with energies of 25keV~35keV were implanted in the shallow region using BF. 2+ Ions with energies of 8keV to 12keV; N-zone deep injection uses As ++ Ions with energies of 55keV~65keV, shallow implantation using As + Ions with energies of 18keV to 22keV; The tilt angle of the stepped self-aligned injection of the multi-step tilt angle and energy combination ranges from 10° to 15°.

10. The method according to claim 8, characterized in that, After completing the stepped self-aligned injection, selective epitaxial growth is also performed in the flank contact region: a SiGe:B strained contact layer is epitaxially grown in the P region, a Si:C strained contact layer is epitaxially grown in the N region, and then a self-aligned metal silicide layer is formed.