A heat dissipation device for heat-generating equipment

By combining a thermally conductive interface layer that converts to a viscoelastic state within the phase change temperature range with a phase change coolant, the heat dissipation problem of high-power chips is solved, achieving efficient, safe, and stable heat dissipation, and simplifying the structure and maintenance process of the heat dissipation device.

CN123124807APending Publication Date: 2026-11-17XIYUE TECHNOLOGY (CHENGDU) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611300306.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-26
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing heat dissipation technologies cannot meet the high-efficiency heat dissipation requirements of high-power chips. Traditional thermal interface materials have insufficient thermal conductivity, gallium-based liquid metals pose safety hazards, conventional liquid cooling plate systems have low heat dissipation efficiency, and traditional phase change cooling technologies are difficult to implement in engineering and have poor compatibility.

Method used

A heat dissipation device that uses a thermally conductive interface layer to transform from a solid state to a viscoelastic state within the phase change temperature range, combined with a phase change coolant and a metal cold plate, achieves high thermal conductivity and stability through the combination of thermally conductive materials and phase change materials, and simplifies structural design.

Benefits of technology

It improves thermal conductivity, reduces fabrication difficulty and cost, ensures high-power devices operate within a suitable temperature range, is compatible with various cooling media, has high safety and stability, is easy to deploy on a large scale, and simplifies maintenance procedures.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124807A_ABST
    Figure CN123124807A_ABST
Patent Text Reader

Abstract

This invention relates to a heat dissipation device for a heat-generating device, comprising: a coolant configured to absorb and dissipate heat from a cold plate; a cold plate having coolant channels for coolant flow and a heat dissipation surface for thermal contact with a thermally conductive interface layer; and a thermally conductive interface layer configured to be disposed between the heat dissipation surface of the cold plate and the heat-generating device and to allow heat exchange between the heat dissipation surface and the heat-generating device, wherein the thermally conductive interface layer transitions from a solid state to a viscoelastic state within a phase transition temperature range and remains in a viscoelastic state, wherein the phase transition temperature range overlaps with the operating temperature range of the heat-generating device, and the coolant and / or the cold plate are configured to maintain the thermally conductive interface layer within the phase transition temperature range after it transitions to a viscoelastic state.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of thermal management technology, and in particular to a heat dissipation device for heat-generating equipment. Background Technology

[0002] With the continuous iteration and upgrading of semiconductor manufacturing process nodes, the integration and computing performance of chips have been greatly improved, and the power density of devices has increased dramatically. At present, the heat flux density of mainstream high-performance computing chips has exceeded 100W / cm², and the heat generation per unit area of ​​the chip has increased significantly. This places higher demands on the thermal conductivity, stability and adaptability of the heat dissipation system, and traditional heat dissipation technologies can no longer meet the heat dissipation needs of high-power chips.

[0003] Currently, the industry's heat dissipation solutions for high-power chips mainly include traditional thermal interface materials, gallium-based liquid metal, conventional liquid cooling plates, and traditional phase change cooling. However, all of these technologies have inherent drawbacks that are difficult to avoid, as follows: First, traditional thermal interface materials have insufficient thermal conductivity, making it difficult to meet the heat dissipation requirements of high-power devices. Currently, the most widely used thermal interface materials in industrial applications, such as thermal grease and thermal pads, cannot quickly dissipate the large amount of heat generated by high-power chips during operation. This easily leads to heat buildup on the chip, causing the chip temperature to exceed the optimal operating temperature range, which is insufficient to meet the high-efficiency heat dissipation requirements of next-generation high-power semiconductor devices.

[0004] Secondly, gallium-based liquid metal heat dissipation solutions pose serious safety risks in engineering applications. To improve thermal conductivity, existing high-end heat dissipation solutions attempt to use gallium-based liquid metal as a thermal interface material. Although this material has excellent thermal conductivity, it is also electrically conductive, which can easily cause short circuits in chip circuits during application. At the same time, gallium-based liquid metal is highly corrosive to aluminum heat sinks, which will accelerate the aging and damage of the heat dissipation structure. Moreover, the difficulty in cleaning up material leaks is extremely high, which seriously affects the reliability and lifespan of chip devices and makes them unsuitable for large-scale mass production and long-term commercial applications.

[0005] Furthermore, conventional liquid-cooled cold plate systems have inherent bottlenecks in heat dissipation capacity. Current mainstream liquid-cooled cold plate systems generally use a water-glycol mixture or pure deionized water as the cooling medium. Under normal pressure, the medium undergoes no phase change, and heat exchange relies solely on sensible heat exchange. The heat dissipation efficiency is strictly limited by the sensible heat transfer formula Q=m·Cp·ΔT, where ΔT represents the temperature rise at the coolant inlet and outlet, Cp represents the specific heat capacity of the medium at constant pressure, m represents the mass of the cooling medium involved in heat exchange, and Q represents the heat absorbed / removed by the fluid through sensible heat. Under high-power, high-heat-flux-density operating conditions of the chip, the coolant temperature rise rate is too rapid, and the heat transfer efficiency cannot match the chip's heat generation rate, causing the chip's operating temperature to rapidly approach its thermal limit, posing a serious risk of overheating failure.

[0006] Finally, traditional phase change cooling technology faces significant challenges in engineering implementation and suffers from poor compatibility. Currently, most existing phase change cooling solutions employ structures such as vacuum chamber heat exchangers and closed two-phase flow loops, resulting in complex overall structural designs, high manufacturing costs, and low reliability. Furthermore, these phase change structures exhibit poor compatibility and adaptability with conventional liquid cooling plate systems, hindering large-scale deployment.

[0007] In summary, the current chip heat dissipation field lacks an integrated heat dissipation solution that combines ultra-high thermal conductivity, strong structural and process adaptability, high safety and stability, controllable cost, and efficient collaboration with phase change cooling cold plate systems. Summary of the Invention

[0008] To address at least some of the problems mentioned above in the prior art, the present invention provides a heat dissipation device for a heat-generating device, comprising: Coolant, which is configured to absorb and dissipate heat from the cold plate; A cold plate having coolant channels for coolant flow and a heat dissipation surface for thermal contact with a thermally conductive interface layer; and A thermally conductive interface layer is configured to be disposed between the heat dissipation surface of a cold plate and a heat-generating device and to allow heat exchange between the heat dissipation surface and the heat-generating device, wherein the thermally conductive interface layer transitions from a solid state to a viscoelastic state within a phase transition temperature range and remains in a viscoelastic state, wherein the phase transition temperature range overlaps with the operating temperature range of the heat-generating device, and the coolant and / or the cold plate is configured to maintain it within the phase transition temperature range after the thermally conductive interface layer transitions to a viscoelastic state.

[0009] Furthermore, the coolant does not undergo a phase change within the phase change temperature range of the thermally conductive interface layer.

[0010] Furthermore, the coolant includes water, an aqueous glycol solution, or a single-phase fluorinated liquid.

[0011] Furthermore, the coolant is a phase change coolant, and its bubble point is within the overlapping temperature range.

[0012] Furthermore, the coolant includes at least one of a fluorocarbon compound and dimethyl silicone oil.

[0013] Furthermore, the coolant contains 70-80% fluorocarbons by mass and 20-30% dimethyl silicone oil by mass; or The coolant is composed entirely of fluorocarbon compounds.

[0014] Furthermore, the fluorocarbon compound is one or more combinations of 1-chloro-trifluoropropene, 2-chloro-trifluoropropene, dichlorofluoroethane, perfluorohexanone, pentafluorobutane, and decafluoropentane.

[0015] Furthermore, the thermally conductive interface layer includes: A thermally conductive material configured to conduct heat between a heat sink and a heat-generating element, the thermally conductive material comprising diamond micron powder; A phase change material is configured to undergo a reversible phase change to enter a viscoelastic state within the operating temperature range of a heating device, wherein the phase change material in the viscoelastic state promotes an increase in the thermal conductivity of a thermally conductive material, such that the phase change material is maintained within the phase change temperature range; the phase change material and the thermally conductive material are mixed together.

[0016] Furthermore, the phase transition temperature range is 25°C to 60°C.

[0017] Furthermore, the thermally conductive material also includes one or more of the following: alumina, boron nitride, silicon carbide, zinc oxide, and aluminum powder.

[0018] Furthermore, the phase change material is a silicon-based binder, formed by an addition reaction of hydrogen-containing silicone oil and α-olefin-modified siloxane under the action of a catalyst: Hydrogen-containing silicone oil with the structure shown in Formula I: (Formula I), where 10≤a≤100, 2≤b≤50, 2≤c≤30, R1, R2, R3, R4, R7 are methyl, ethyl or C4~C8 straight-chain or branched alkyl, R6 is methyl, and R5 is C6~12 straight-chain or branched alkyl. α-olefin modified siloxanes with the structure shown in Formula II: (Formula II), R9, R10, R11, R13, and R14 are methyl, ethyl, or C6-C12 straight-chain or branched alkyl groups, R8 and R15 are alkenyl groups, R14 is methyl or C18-C30 straight-chain or branched alkyl groups, and 20 ≤ d ≤ 30.

[0019] Furthermore, R1, R2, R3, R4, R6, and R7 are methyl groups, and R5 is a C8 straight-chain or branched alkyl group; and / or R9, R10, R11, R13, and R14 are methyl, R8 is vinyl, R15 is vinyl, and R12 is a straight-chain or branched alkyl group of C24-C26 or C31-C39; and / or The molar ratio of hydrogen atoms in the Si-H of the hydrogen-containing silicone oil to the carbon-carbon double bond of the α-olefin-modified siloxane is 0.5 to 1.2; and / or The mass percentage of thermally conductive material in the thermal interface layer is greater than or equal to 90%; and / or The mass percentage of phase change material in the thermally conductive interface layer is 5%-8%; and / or The catalyst is one or more of chloroplatinic acid catalysts and platinum catalysts.

[0020] Furthermore, the cold plate is a metal cold plate, and the metal cold plate has a coolant flow channel inside, which includes one or more combinations of serpentine channels, parallel channels, microchannels or phase change cavities.

[0021] Furthermore, the material of the heat dissipation surface of the cold plate includes metal.

[0022] Furthermore, the heat dissipation surface of the cold plate is made of aluminum, aluminum alloy, or copper.

[0023] Furthermore, the thermally conductive interface layer is bonded to the cold plate through a chemical reaction.

[0024] Furthermore, the metal cold plate is an aluminum cold plate, and the thermally conductive interface layer is bonded to the aluminum cold plate through Si-O-Al chemical bonds.

[0025] Furthermore, the thermally conductive interface layer hardens at a hardening temperature below the phase change temperature range and liquefies at a liquefaction temperature above the phase change temperature range.

[0026] Furthermore, the hardening temperature of the thermally conductive interface layer is 25°C, and the thermal decomposition temperature of the thermally conductive interface layer is ≥155°C.

[0027] Furthermore, the heat-generating device includes a computer, an integrated circuit module, an energy storage battery, a photovoltaic module, a supercomputer node, a power electronic device, and a spaceborne unit.

[0028] The present invention also provides a method for operating a heat dissipation device, comprising: Operating the heating device causes the temperature of the thermally conductive interface layer to reach the phase transition temperature range and transform into a viscoelastic state, where the viscoelastic thermally conductive interface layer exhibits improved thermal conductivity; and The cold plate absorbs the heat conducted through the thermal interface, keeping the thermal interface layer within the phase change temperature range.

[0029] Furthermore, the heat absorbed by the cold plate from the thermal interface includes: The coolant in the cold plate undergoes a phase change; and The heat conducted through the thermal interface is absorbed by the coolant undergoing phase change.

[0030] Furthermore, the heat absorbed by the cold plate from the thermal interface includes: The coolant in the cold plate does not undergo a phase change; and The coolant absorbs the heat conducted through the thermal interface.

[0031] The present invention also provides a temperature gradient controller configured to control a heat dissipation device such that the thermally conductive interface layer is within the phase transition temperature range.

[0032] The present invention also provides a method for manufacturing a heat dissipation device, comprising the following steps: Plasma activation treatment is applied to the metal surface of the cold plate to form an oxide layer rich in hydroxyl groups. A thermally conductive paste is applied to the metal surface, the thermally conductive paste comprising a mixture of hydrogen-containing silicone oil, α-olefin-modified siloxane, platinum-based catalyst, and diamond micropowder; and The metal surface is heated to 60°C to 120°C, causing the thermally conductive paste to solidify and form a thermally conductive interface layer, wherein the thermally conductive interface layer is bonded to the metal surface by forming chemical bonds.

[0033] The present invention has at least the following beneficial effects: (1) The thermally conductive interface layer of the present invention can undergo a phase transition into a viscoelastic state within the operating temperature range of the heating device, thereby significantly increasing its thermal conductivity. This increased thermal conductivity, in turn, prevents or inhibits further temperature increases, thus maintaining the thermally conductive interface layer in a high thermal conductivity phase transition state. Moreover, since the thermally conductive interface can undergo a phase transition and soften under operating conditions, it does not need to be fabricated as a thin sheet with uniform thickness. Instead, it can automatically soften during use to achieve automatic flatness and eliminate gaps between the interface layer and the cold plate or the device to be cooled, thereby significantly reducing the manufacturing difficulty and cost while ensuring heat dissipation capacity. In short, the thermally conductive interface layer of the present invention is flat and easy to install in its solid state. After softening under heat, its fluidity is greatly improved, which can fill the micron-level uneven gaps between the chip and the heat sink, significantly reducing air thermal resistance (air has extremely poor thermal conductivity).

[0034] (2) The thermal interface layer of the present invention can react chemically with the metal surface to form a whole with the thermal interface layer and the cold plate, eliminating the thermal interface between the two and improving the thermal conductivity. Moreover, by providing the composite of the thermal interface layer and the cold plate as a finished product, the user is exempt from the need to install the thermal interface layer on the cold plate, and can directly install it on the device to be cooled for use.

[0035] (3) The thermal interface layer of the present invention has a high thermal conductivity and strong thermal conductivity, which enables high-power devices to operate within a suitable temperature range and meet the high-efficiency heat dissipation requirements of high-power devices.

[0036] (4) The phase change temperature range of the thermal interface layer of the present invention is precisely matched with the bubble point of the phase change coolant. The thermal interface layer and the phase change coolant form a closed-loop synergistic mechanism to regulate each other and keep the temperature of the heating device stable in the optimal range.

[0037] (5) The phase change coolant of the present invention can efficiently dissipate heat by utilizing the latent heat of vaporization under normal pressure, without the need for a vacuum cavity structure or a complex two-phase flow circuit. The heat dissipation device has a simple structure, high reliability, and is easy to deploy on a large scale.

[0038] (6) The heat dissipation device of the present invention is compatible with a variety of cooling working fluids such as phase change coolant, deionized water, and water glycol solution, and has a wide range of applications.

[0039] (7) The thermal interface layer of the present invention is insulated, and will not cause short circuit faults in semiconductor devices during application. It has high safety and stability and will not corrode metal cold plates.

[0040] (8) The thermal interface layer of the present invention is easy to use. After use, it can be manually peeled off when cooled to room temperature. The thermal interface layer can be removed without disassembly tools, which greatly simplifies the chip maintenance, replacement and reinstallation process. Attached Figure Description

[0041] To further illustrate the above and other advantages and features of the various embodiments of the present invention, a more specific description of the embodiments of the invention will be presented with reference to the accompanying drawings. It is to be understood that these drawings depict only typical embodiments of the invention and are therefore not intended to limit its scope. In the drawings, identical or corresponding parts will be indicated by identical or similar reference numerals for clarity.

[0042] Figure 1 A schematic diagram of a heat dissipation device for a heat-generating device according to the present invention is shown.

[0043] Figure 2 A cross-sectional structural diagram of a thermally conductive interface layer according to the present invention is shown.

[0044] Figure 3 A schematic diagram showing the contact between the bottom layer diamond and the cold plate after the thermally conductive interface layer of the present invention is shown. Detailed Implementation

[0045] It should be noted that the components in the accompanying drawings may be shown exaggerated for illustrative purposes and may not be to scale.

[0046] In this invention, the various embodiments are merely intended to illustrate the solutions of the invention and should not be construed as limiting.

[0047] In this invention, unless otherwise specified, the quantifiers “a” and “one” do not exclude scenarios involving multiple elements.

[0048] It should also be noted that, in the embodiments of the present invention, only a portion of the parts or components may be shown for clarity and simplicity. However, those skilled in the art will understand that, under the teachings of the present invention, the required parts or components can be added as needed for specific scenarios.

[0049] It should also be noted that within the scope of this invention, the terms "same", "equal", and "equal to" do not mean that the two values ​​are absolutely equal, but allow for a certain reasonable error. In other words, the terms also cover "substantially the same", "substantially equal", and "substantially equal to".

[0050] It should also be noted that in the description of this invention, the terms "center," "longitudinal," "lateral," "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are used only for the convenience of describing the invention and for simplifying the description, and do not explicitly or implicitly suggest that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on the invention. Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance.

[0051] Furthermore, the embodiments of the present invention describe the process steps in a specific order. However, this is only for the convenience of distinguishing each step, and is not a limitation on the order of each step. In different embodiments of the present invention, the order of each step can be adjusted according to the process.

[0052] Figure 1 A schematic diagram of a heat dissipation device for a heat-generating device according to the present invention is shown.

[0053] Figure 1 As shown, a heat dissipation device for a heat-generating device includes: Coolant, which is configured to absorb and dissipate heat from the cold plate; Cold plate 100, having coolant channels for coolant flow and a heat dissipation surface for thermal contact with thermally conductive interface layer 200; and A thermal interface layer 200 is configured to be disposed between the heat dissipation surface of the cold plate 100 and the heat-generating device 300 and to allow heat exchange between the heat dissipation surface and the heat-generating device 300. The thermal interface layer 200 changes from a solid state to a viscoelastic state within a phase change temperature range and remains in a viscoelastic state. The phase change temperature range overlaps with the operating temperature range of the heat-generating device 300. The coolant and / or the cold plate is configured to maintain the thermal interface layer within the phase change temperature range after it changes to a viscoelastic state.

[0054] The cold plate 100 can be a metal cold plate, such as an aluminum cold plate, an aluminum alloy cold plate, or a copper cold plate. The material of the heat dissipation surface of the cold plate is aluminum or an aluminum alloy. The metal cold plate 100 has coolant channels inside, which include one or more combinations of serpentine channels, parallel channels, microchannels, or phase change cavities.

[0055] The coolant can be deionized water, water-glycol solution, or single-phase fluorinated liquid. The combination of the thermally conductive interface layer and the above-mentioned coolant can meet the heat dissipation requirements of low to medium power (less than 400W).

[0056] The coolant may also be a phase change coolant with a bubble point within the aforementioned overlapping temperature range. The phase change coolant comprises at least one of a fluorocarbon compound and dimethyl silicone oil, with a viscosity of 0.5-2.0 mm² / s at 25°C, a density of 1.3-1.5 g / cm³, a breakdown voltage >20 kV, a freezing point <-30°C, and a first bubble point of 30°C to 100°C (preferably 30°C to 50°C).

[0057] In one embodiment, the coolant contains 70-80% by mass of fluorocarbons and 20-30% by mass of dimethyl silicone oil. In another embodiment, the coolant is composed entirely of fluorocarbons.

[0058] The fluorocarbon compound is one or more combinations of 1-chloro-trifluoropropene, 2-chloro-trifluoropropene, monofluorodichloroethane, perfluorohexanone, pentafluorobutane, and decafluoropentane.

[0059] The combination of phase change coolant and thermal interface layer can meet the heat dissipation requirements of high power greater than 500W.

[0060] The heat-generating device 300 can be a computer, integrated circuit module, energy storage battery, photovoltaic module, supercomputer node, power electronic equipment, or spaceborne single unit.

[0061] Figure 2 A cross-sectional structural diagram of a thermally conductive interface layer according to the present invention is shown.

[0062] like Figure 2 As shown, the thermal interface layer 200 includes: a thermally conductive material 201 configured to conduct heat between the heat sink and the heat-generating element; the thermally conductive material includes diamond micron powder and optionally one or more of alumina, boron nitride, and silicon carbide; and Phase change material 202 is configured to undergo a reversible phase transition to a viscoelastic state within the operating temperature range of the heating device 300. In this viscoelastic state, phase change material 202 promotes an increase in the thermal conductivity of the heat-conducting material 201, thereby maintaining phase change material 202 within the phase change temperature range. The phase change temperature range is 25°C to 60°C (preferably 35°C to 50°C, or 25°C to 45°C), and the operating temperature range of phase change material 202 is 25°C to 155°C. Phase change material 202 does not liquefy within the phase change temperature range, maintaining a viscoelastic state without flowing. The thermally conductive interface layer 200 hardens at a hardening temperature below the phase change temperature range and liquefies at a liquefaction temperature above the phase change temperature range. The thermally conductive interface layer 200 is in a hardened state below 25°C, with the hardening temperature being a temperature range below 25°C. The thermal decomposition temperature of the phase change material is above 155°C.

[0063] The phase change temperature range of the thermally conductive interface layer 200 of this invention is precisely matched with the bubble point of the phase change coolant. The thermally conductive interface layer 200 and the phase change coolant form a closed-loop synergistic mechanism, mutually regulating each other to stabilize the temperature of the heating device 300 within the optimal range. Specifically, the thermally conductive interface material controls the phase change rhythm of the coolant: when the coolant temperature approaches the bubble point, the thermally conductive interface layer undergoes a phase change precisely within that temperature range, causing a sharp drop in thermal resistance and a rapid transfer of a large amount of heat to the cold plate, precisely triggering the phase change vaporization of the phase change coolant. The coolant phase change, in turn, protects the thermal interface material: the strong latent heat absorption capacity of the coolant during vaporization stabilizes the cold plate temperature within the phase change temperature range of the thermally conductive interface layer, keeping the thermal interface material in its optimal operating range in a jelly-like (viscoelastic) state. When the power of the heating device fluctuates, the thermally conductive interface layer and the phase change coolant mutually regulate each other, allowing the temperature of the heating device to adaptively stabilize within the optimal range.

[0064] The phase change material 202 accounts for 5%-8% of the thermally conductive interface layer 200. The phase change material is a silicon-based binder, formed by an addition reaction between hydrogen-containing silicone oil and α-olefin-modified siloxane.

[0065] Hydrogen-containing silicone oil has the structure shown in Formula I: (Formula I), Where 10≤a≤100, 2≤b≤50, 2≤c≤30, R1, R2, R3, R4, and R7 can be methyl, ethyl, or C4~C8 straight-chain or branched alkyl groups, R6 can be methyl, and R5 can be C6~12 straight-chain or branched alkyl groups.

[0066] α-olefin-modified siloxanes have the structure shown in Formula II: (Formula II) R9, R10, R11, R13, and R14 can be methyl, ethyl, or C6-C12 straight-chain or branched alkyl groups, R8 and R15 are alkenyl groups, and R14 is methyl or C18-C30 straight-chain or branched alkyl groups, with 20 ≤ d ≤ 30.

[0067] The side chains of hydrogen-containing silicone oil contain Si-H bonds, and the two ends of α-olefin-modified siloxanes contain carbon-carbon double bonds, serving as crosslink acceptors for hydrosilylation reactions. Hydrogen-containing silicone oil and α-olefin-modified siloxanes can undergo an addition reaction catalyzed by a platinum-based catalyst to generate phase change materials. The molar ratio of hydrogen atoms in the Si-H chains of the hydrogen-containing silicone oil to the carbon-carbon double bonds in the α-olefin-modified siloxane is 0.5 to 1.2, for example, 0.8, 0.9, 1.0, 1.1, or 1.2, preferably 0.8 to 1.0.

[0068] In phase change materials, carbon chains with more than 18 carbon atoms directly bonded to silicon atoms undergo crystallization or decrystallization at the softening point (e.g., room temperature 25°C). When the temperature is above the softening point, the phase change material undergoes decrystallization and phase change to enter the viscoelastic state. When the temperature drops below the softening point, the phase change material undergoes crystallization and hardens into a solid state.

[0069] In hydrogen-containing silicone oil, the R5 group acts as a solvent for the long carbon chains (more than 18 carbon atoms) in α-olefin-modified siloxanes. The higher the R5 content, the more pronounced the solvent effect, and the lower the phase transition temperature. Therefore, by adjusting the ratio of a and b in the chemical formula (Formula I) of the hydrogen-containing silicone oil, the phase transition temperature of the phase change material can be precisely controlled: adjusting the ratio of a and b within the range of a and b values ​​can change the relative proportion of R5. When the relative proportion of R5 is larger, the phase transition temperature is relatively lower; when the relative proportion of R5 is smaller, the phase transition temperature is relatively higher. The value of a is between 10 and 100, and the value of b is between 2 and 50. When these values ​​are exceeded, the silicone-based binder does not exhibit a phase transition phenomenon.

[0070] The main difference between the phase change material (silicone binder) of the present invention and paraffin wax is that paraffin wax is in a liquid state after phase change, while the phase change material of the present invention is in a viscoelastic state after phase change. The two are fundamentally different.

[0071] Phase change materials (PCMs) also serve to bond diamond particles to metal surfaces and impart mechanical strength to the material. When heated, PCMs can chemically react with and bond to the metal surface of a cold plate. Specifically, PCMs contain Si-H bonds, and the metal surface includes hydroxyl groups (-OH). The Si-H bonds in the PCM react with the hydroxyl groups on the metal surface to form chemical bonds.

[0072] Platinum-based catalysts can be, for example, chloroplatinic acid catalysts, platinum catalysts, etc.

[0073] The main component of the thermally conductive material in the thermally conductive interface layer is diamond micropowder, and its content is greater than the sum of the contents of other thermally conductive materials in the interface layer. The particle size of the diamond micropowder is 10μm-100μm. When the thermally conductive material contains only diamond micropowder or diamond micropowder and nano-silver, the proportion of diamond micropowder can reach over 90%. The diamond particles in the thermally conductive interface layer have extremely high thermal conductivity (2000W / (m·K)), serving as the main framework of the thermal conduction pathway. The high filling ratio ensures the formation of a continuous heat conduction network, resulting in a high basic thermal conductivity of the thermally conductive interface layer, which can even reach over 12W / (m·K). The diamond particles are polyhedral in shape.

[0074] When the phase change material in the thermal interface layer undergoes a phase transition to a viscoelastic state upon heating, the volume of the thermal interface layer increases and its hardness decreases. This causes the diamond to tend to assemble into a closely packed configuration, thereby reducing free volume, lowering thermal resistance, and improving the thermal conductivity of the thermal interface layer.

[0075] Moreover, such as Figure 3 As shown, after the phase change material undergoes a phase change, a portion of the diamond adjacent to the cold plate naturally settles onto the metal surface of the cold plate. Furthermore, since the diamond is polyhedral, it forms surface contact with the metal surface, significantly increasing the heat conduction area. Because the material enters a viscoelastic state rather than a liquid state after the phase change, the diamond does not move significantly due to gravity. The amount of diamond in the upper half of the vertical path does not decrease due to settling, thus not affecting the vertical heat conduction path.

[0076] During use, a portion of the bottom layer of diamond sinks into the surface of the cold plate metal, further increasing the heat conduction surface.

[0077] When aluminum powder is included in the thermally conductive material in addition to diamond, an electronic heat transfer path is created between the aluminum atoms, which can further reduce the contact thermal resistance of the thermally conductive interface layer.

[0078] The aforementioned thermally conductive interface layer may also selectively include silver nanoparticles with a particle size of 1 nm to 100 nm, preferably 5 nm to 50 nm, which are dispersed in the phase change material to form additional thermally conductive pathways, further improving the thermal conductivity of the thermally conductive interface layer. The proportion of silver nanoparticles in the thermally conductive interface layer is 1% to 3%.

[0079] After the phase change material undergoes a phase change (viscoelastic state), the silver nanoparticles form a thermally conductive pathway in the micro-gap of the phase change material, which greatly reduces the contact thermal resistance of the thermally conductive interface layer.

[0080] Within the thermally conductive interface layer, electronic thermal conduction pathways are formed between silver particles or between silver particles and aluminum (optional). Between the thermally conductive interface layer and the cold plate, electronic thermal conduction pathways can also be formed between the silver particles and the cold plate metal. Electronic thermal conduction pathways have lower thermal resistance than phonon thermal conduction pathways, thus significantly reducing the contact thermal resistance of the thermally conductive interface layer.

[0081] The following describes the method for manufacturing a thermally conductive interface layer.

[0082] Step 1, preparing the thermally conductive material, includes: mixing diamond micro powder and one or more of the optional alumina, boron nitride, and silicon carbide according to the target filling ratio.

[0083] Step 2, preparing phase change material, includes: mixing hydrogen-containing silicone oil and α-olefin modified siloxane in a certain proportion, adding platinum-based catalyst, and stirring evenly under low temperature (50°C to 80°C) and light-protected conditions.

[0084] Step 3: Mix the thermally conductive material and the phase change material evenly to obtain a thermally conductive slurry.

[0085] Step 4: Perform plasma treatment on the surface of the metal cold plate to introduce hydroxyl groups.

[0086] In one embodiment, hydroxyl groups are introduced onto the surface of the metal cold plate by plasma cleaning or corona treatment (corona discharge).

[0087] Metal cold plates, such as aluminum cold plates, naturally have an oxide layer on their surface. Under normal temperature and natural conditions, aluminum oxide can slowly hydrate to generate hydroxyl groups, but the number of hydroxyl groups is small and easily masked by contaminants. Oxygen-containing plasma cleaning removes surface contaminants on the one hand, and generates a large number of oxygen dangling bond active sites on the aluminum oxide surface on the other hand. The interaction of these active sites with water vapor significantly increases the hydroxyl density on the aluminum surface.

[0088] The aluminum cold plate is surface activated by air corona discharge; the high-energy particles generated by the corona discharge remove organic pollutants from the surface of the cold plate and generate unsaturated active sites on the aluminum oxide layer; the active sites combine with the ambient water vapor to form high-density hydroxyl groups on the metal surface.

[0089] Step 5: Apply thermally conductive paste to the surface of the plasma-treated metal cold plate with a coating thickness of 150μm to 350μm, preferably 200-250μm.

[0090] Step 6: Heat the metal cold plate to 60°C~120°C to solidify the thermally conductive paste and form a thermally conductive interface layer, wherein the thermally conductive interface layer is bonded to the metal cold plate through chemical bonds.

[0091] The preferred metal cold plate is an aluminum cold plate or an aluminum alloy cold plate, and the thermally conductive interface layer is bonded to the aluminum cold plate through Si-O-Al chemical bonds.

[0092] In use, the thermally conductive interface layer is located between the heat sink (e.g., a metal cold plate) and the heating element. The heating element generates heat, which heats the thermally conductive interface layer. When the temperature reaches the phase change temperature range of the phase change material, the phase change material changes from a solid state to a viscoelastic state. Simultaneously, the heat sink absorbs the heat transferred by the thermally conductive material in the thermally conductive interface layer. The phase change material is maintained within the temperature range defined by the lower and upper limits of the temperature range, and remains in a viscoelastic state. The phase change temperature range is 25°C to 60°C (preferably 35°C to 50°C or 25°C to 45°C), and the operating temperature range is 25°C to 155°C.

[0093] After use, once cooled to 10°C below the softening temperature, the thermal interface layer can be peeled off without tools, greatly simplifying the chip maintenance, replacement, and reinstallation process.

[0094] A method for manufacturing a heat dissipation device includes the following steps: Plasma activation treatment is applied to the metal surface of the cold plate to form an oxide layer rich in hydroxyl groups (-OH). A thermally conductive paste is applied to a metal surface. The thermally conductive paste comprises a mixture of hydrogen-containing silicone oil, α-olefin-modified siloxane, platinum-based catalyst, and diamond micropowder; and The metal surface is heated to 60°C to 120°C, which causes the thermally conductive paste to solidify and form a thermally conductive interface layer, wherein the thermally conductive interface layer is bonded to the metal surface by forming chemical bonds.

[0095] The thermally conductive paste may also selectively contain one or more of alumina, boron nitride, and silicon carbide.

[0096] The method of operating the above-mentioned heat dissipation device includes: The operation of the heating device causes the temperature of the thermal interface layer to reach the phase change temperature range and transform into a viscoelastic state, wherein the viscoelastic thermal interface layer has improved thermal conductivity; and the heat conducted by the thermal interface is absorbed by the cold plate, so that the thermal interface layer is kept within the phase change temperature range.

[0097] When the coolant in the cold plate is a phase change coolant, the coolant in the cold plate undergoes a phase change. The phase change coolant absorbs the heat conducted by the thermal interface, so that the thermal interface layer is kept within the phase change temperature range.

[0098] This invention also provides a temperature gradient controller configured to control a heat dissipation device, ensuring that the thermal interface layer remains within the phase transition temperature range. For example, when the temperature is too high, the initial temperature of the coolant entering the cold plate can be reduced by optimizing the control of the front-end cold source, or the circulation pump speed can be increased / the pipeline valves can be opened wider to increase the total amount of coolant flowing through the liquid cooling plate per unit time, thus ensuring that the thermal interface layer remains within the phase transition temperature range. When the temperature is too low, the initial temperature of the coolant entering the cold plate can be increased by optimizing the control of the front-end cold source, or the circulation pump speed can be reduced / the pipeline valves can be opened narrower to reduce the total amount of coolant flowing through the liquid cooling plate per unit time, thus ensuring that the thermal interface layer remains within the phase transition temperature range. The embodiments of the present invention will be described in detail below. These embodiments are implemented based on the technical solution of the present invention, and detailed implementation methods and specific operation processes are given. However, the scope of protection of the present invention is not limited to the following embodiments.

[0099] The components used in the examples and comparative examples are described below.

[0100] Components used in the examples: Hydrogen-containing silicone oil: Mixtures represented by general formula A-1: (A-1), a: 10~20, b: 0~20; c: 5~10.

[0101] α-Olefin-modified siloxanes: mixtures based on general formulas B-1 and B-2: (B-1), R9, R10, R11, R13, and R14 are methyl, R8 is vinyl, R15 is vinyl, R12 is a C24-C26 straight-chain alkyl group, and d = 20~40.

[0102] (B-2), R9, R10, R11, R13, and R14 are methyl, R8 is vinyl, R15 is vinyl, and R12 is a straight-chain or branched alkyl group with 30 or more carbon atoms, such as a straight-chain alkyl group with C31 to C39 and d = 20 to 40.

[0103] Diamond micron powder C-1 has a particle size of 20μm-50μm.

[0104] Diamond micron powder C-2 has a particle size of 50μm-80μm.

[0105] Chloroplatinic acid catalyst.

[0106] Nano-silver particles with a particle size of 5nm-50nm.

[0107] Zinc oxide particles with a particle size of 0.2μm-0.4μm.

[0108] Aluminum powder with a particle size of 1μm~10μm.

[0109] The following table shows a description of the components used in the examples, expressed as a percentage by mass.

[0110] Hydrogen-containing silicone oil (A-1 or A-2) and α-olefin-modified siloxane (B-1 or B-2) are mixed in a specific ratio, and a chloroplatinic acid catalyst is added. The mixture is stirred evenly under light conditions at 50°C-80°C to form a phase change material. The thermally conductive material and the phase change material listed in the table are mixed evenly in a specific ratio to obtain a thermally conductive slurry. The surface of the aluminum cold plate is subjected to plasma treatment to introduce hydroxyl groups. The thermally conductive slurry is coated onto the plasma-treated surface of the aluminum cold plate to a thickness of 200 μm. The aluminum cold plate is heated to 60°C-120°C to allow the thermally conductive slurry to form a thermally conductive interface layer.

[0111] Comparative Example 1 Silicone grease thermal conductive materials consist of components in the following table with the indicated mass percentages.

[0112] Comparative Example 2 The high-temperature phase change thermal conductive material comprises the components shown in the table below by mass percentage.

[0113] Comparative Example 3 The high-temperature phase change thermal conductive material comprises the components shown in the table below by mass percentage.

[0114] Comparative Example 4 The thermally conductive gel comprises the components in the mass percentages shown in the table below.

[0115] The following describes the methods for thermal conductivity testing, phase transition testing, electrical conductivity testing (breakdown voltage), and stability verification.

[0116] Thermal conductivity was tested according to ISO 22007.

[0117] The thermal conductivity test method includes: placing the thermally conductive interface layer of Examples 1-5 and the thermally conductive material of Comparative Examples 1-4 between the chip and the cold plate, respectively, testing the chip temperature under 100% load for 1000 hours, and recording the highest temperature of the chip as the thermal conductivity test data.

[0118] Differential thermal analysis (DTA) was used to test the phase transition temperature of the material using a differential thermal analyzer.

[0119] Thermogravimetric analysis (TGA) was used to test the stability of the thermally conductive interface layers of Examples 1-5 and the thermally conductive materials of Comparative Examples 1-4, and to examine their thermal weight loss at 200 degrees Celsius.

[0120] The breakdown voltage of the material is tested according to GBT1408.

[0121] The test results of the embodiments and comparative examples are shown below.

[0122] When the thermal weight loss exceeds 1%, it is considered unqualified. The thermally conductive interface layer of Example 3 does not contain hydrogen-containing silicone oil, and its thermal weight loss is as high as 4%, far exceeding that of Examples 1, 2, 4, and 5, and its breakdown voltage is also lower than that of Examples 1, 2, 4, and 5. This indicates that hydrogen-containing silicone oil is crucial to the thermal stability of the thermally conductive interface layer and also affects its electrical conductivity.

[0123] The phase transition of the thermally conductive interface layer in Examples 1-5 is determined by the α-olefin-modified siloxane, specifically by the R12 group of the α-olefin-modified siloxane. Example 2 uses a different α-olefin-modified siloxane than Examples 1, 3, 4, and 5, specifically in the R12 group. Changing the number of carbon atoms in the R12 group alters the phase transition temperature of the thermally conductive interface layer. The phase transition temperature affects heat dissipation from the chip. The phase transition temperature in Example 2 is 40-42°C, higher than the 30-35°C in other examples. Correspondingly, the highest chip temperature in Example 2 is 68°C, higher than the 59-63°C in other examples.

[0124] During the thermal conductivity test of Comparative Example 1, the chip temperature gradually increased from 63°C to 73°C after 500 hours. The highest chip temperatures measured in the thermal conductivity experiments of Comparative Examples 1 to 5 all exceeded the preferred chip operating temperature range. The highest chip temperatures corresponding to Examples 1-5 were all lower than those of the Comparative Examples, and the highest chip temperatures of Examples 1, 3, 4, and 5 were within the preferred chip operating temperature range, indicating that the thermally conductive interface layer of the present invention has good thermal conductivity.

[0125] The phase change material of the present invention forms a more stable electrical-thermal conduction path (electronic thermal conduction path and phonon thermal conduction path) during long-term use. It is not easily degraded by aging overflow during long-term use, and therefore has better long-term thermal conductivity.

[0126] The breakdown voltages tested in Examples 1-5 were 5-7KV / mm, indicating that the thermally conductive interface layer of the present invention is a weakly insulating medium that can be adapted to chip heat dissipation and will not cause short circuit faults in the chip circuit during use.

[0127] Example 6 Phase change coolant C1 contains the following components by mass percentage: 1-Chlorotrifluoropropylene + 2-Chlorotrifluoropropylene 70% 30% dimethyl silicone oil The phase change coolant C1 has a bubble point of 38-39°C, a viscosity of 5 mm² / s at 25°C, a density of 1.5 g / cm³, and a breakdown voltage greater than 7 kV.

[0128] Example 7 Phase change coolant C2 comprises the following components by mass percentage: 80% of monofluorodichloroethane 20% dimethyl silicone oil The phase change coolant C2 has a bubble point of 33°C, a viscosity of 4 mm² / s at 25°C, a density of 1.6 g / cm³, and a breakdown voltage greater than 7 kV.

[0129] Example 8 Phase change coolant C3 contains the following components by mass percentage: Perfluorohexanone 30% 70% pentafluorobutane The phase change coolant C3 has a bubble point of 40.5°C, a viscosity of less than 2 mm² / s at 25°C, a density of approximately 1.7 g / cm³, and a breakdown voltage greater than 7 kV.

[0130] Example 9 Phase change coolant C4 comprises the following components by mass percentage: 30% decafluoropentane 70% pentafluorobutane The phase change coolant C4 has a bubble point of 40.5°C, a viscosity of less than 2 mm² / s at 25°C, a density of approximately 1.7 g / cm³, and a breakdown voltage greater than 7 kV.

[0131] Example 10 100% perfluorohexanone in phase change coolant C5.

[0132] The phase change coolant C5 has a bubble point of 49°C, a viscosity of less than 2 mm² / s at 25°C, a density of 1.6 g / cm³, and a breakdown voltage greater than 7 kV.

[0133] Example 11 100% decafluoropentane in phase change coolant C6.

[0134] The phase change coolant C6 has a bubble point of 55°C, a viscosity of less than 2 mm² / s at 25°C, a density of 1.6 g / cm³, and a breakdown voltage greater than 7 kV.

[0135] The thermal conductivity of the phase change coolant in Examples 5-10 was tested. The specific test method included: injecting the phase change coolant of Examples 5-10 into the cold plate respectively, directly attaching and fixing the chip and the cold plate with the thermal interface layer, testing the chip temperature under 100% load for 1000 hours, and recording the highest temperature of the chip as the thermal conductivity test data.

[0136] The test results of the thermal conductivity of the phase change coolant in Examples 5-10 are shown in the table below.

[0137] The phase change coolant in Example 5 has the highest bubble point temperature, corresponding to the highest chip temperature and the worst thermal conductivity. The phase change coolant in Example 2 has the lowest bubble point temperature, corresponding to the lowest chip temperature and the best thermal conductivity.

[0138] The highest chip temperature corresponding to Examples 5-8 is within the preferred operating range of the chip. The highest chip temperature corresponding to Example 9 is close to the maximum value of the chip's optimal operating temperature range, while Example 10 exceeds the optimal operating temperature range.

[0139] The bubble points of the phase change coolants in Examples 6, 9, and 10 match the phase change temperature of the thermally conductive interface layer in Example 2; the bubble points of the phase change coolants in Examples 7 and 8 match the phase change temperature of the thermally conductive interface layer in Examples 1, 3, 4, and 5.

[0140] While some embodiments of the present invention have been described in this application, those skilled in the art will understand that these embodiments are merely illustrative. Numerous variations, alternatives, and improvements will arise in those skilled in the art under the teachings of this invention without departing from its scope. The appended claims are intended to define the scope of the invention and thereby cover methods and structures within the scope of the claims themselves and their equivalents.

Claims

1. A heat dissipation device for a heat-generating equipment, characterized in that, include: Coolant, which is configured to absorb and dissipate heat from the cold plate; Cold plate, which has coolant channels for coolant flow and a heat dissipation surface for thermal contact with the thermally conductive interface layer; as well as A thermally conductive interface layer is configured to be disposed between the heat dissipation surface of a cold plate and a heat-generating device and to allow heat exchange between the heat dissipation surface and the heat-generating device, wherein the thermally conductive interface layer transitions from a solid state to a viscoelastic state within a phase transition temperature range and remains in a viscoelastic state, wherein the phase transition temperature range overlaps with the operating temperature range of the heat-generating device, and the coolant and / or the cold plate is configured to maintain it within the phase transition temperature range after the thermally conductive interface layer transitions to a viscoelastic state.

2. The heat dissipation device according to claim 1, characterized in that, The coolant does not undergo a phase change within the phase change temperature range of the thermally conductive interface layer.

3. The heat dissipation device according to claim 2, characterized in that, Coolants include water, aqueous glycol solution, or single-phase fluorinated liquid.

4. The heat dissipation device according to claim 1, characterized in that, The coolant is a phase change coolant, and its bubble point is within the overlapping temperature range.

5. The heat dissipation device according to claim 4, characterized in that, The coolant includes at least one of fluorocarbon compounds and dimethyl silicone oil.

6. The heat dissipation device according to claim 5, characterized in that, The coolant contains 70-80% fluorocarbons by mass and 20-30% dimethyl silicone oil by mass; or The coolant is composed entirely of fluorocarbon compounds.

7. The heat dissipation device according to claim 5, characterized in that, The fluorocarbon compound is one or more combinations of 1-chloro-trifluoropropene, 2-chloro-trifluoropropene, monofluorodichloroethane, perfluorohexanone, pentafluorobutane, and decafluoropentane.

8. The heat dissipation device according to claim 1, characterized in that, The thermally conductive interface layer includes: A thermally conductive material configured to conduct heat between a cold plate and a heating device, the thermally conductive material comprising diamond micron powder; A phase change material is configured to undergo a reversible phase change to enter a viscoelastic state within the operating temperature range of a heating device, wherein the phase change material in the viscoelastic state promotes an increase in the thermal conductivity of a thermally conductive material, such that the phase change material is maintained within the phase change temperature range; the phase change material and the thermally conductive material are mixed together.

9. The heat dissipation device according to claim 8, characterized in that, The phase transition temperature range is 25°C to 60°C.

10. The heat dissipation device according to claim 8, characterized in that, The thermally conductive material also includes one or more of the following: alumina, boron nitride, silicon carbide, zinc oxide, and aluminum powder.

11. The heat dissipation device according to claim 8, characterized in that, The phase change material is a silicon-based binder, formed by an addition reaction of hydrogen-containing silicone oil and α-olefin-modified siloxane under the action of a catalyst. Hydrogen-containing silicone oil with the structure shown in Formula I: (Formula I), where 10≤a≤100, 2≤b≤50, 2≤c≤30, R1, R2, R3, R4, R7 are methyl, ethyl or C4~C8 straight-chain or branched alkyl, R6 is methyl, and R5 is C6~12 straight-chain or branched alkyl. α-olefin modified siloxanes with the structure shown in Formula II: (Formula II), R9, R10, R11, R13, and R14 are methyl, ethyl, or C6-C12 straight-chain or branched alkyl groups, R8 and R15 are alkenyl groups, R14 is methyl or C18-C30 straight-chain or branched alkyl groups, and 20 ≤ d ≤ 30.

12. The heat dissipation device according to claim 11, characterized in that, R1, R2, R3, R4, R6, and R7 are methyl groups, and R5 is a C8 straight-chain or branched alkyl group; and / or R9, R10, R11, R13, and R14 are methyl, R8 is vinyl, R15 is vinyl, and R12 is a straight-chain or branched alkyl group of C24-C26 or C31-C39; and / or The molar ratio of hydrogen atoms in the Si-H of the hydrogen-containing silicone oil to the carbon-carbon double bond of the α-olefin-modified siloxane is 0.5 to 1.2; and / or The mass percentage of thermally conductive material in the thermal interface layer is greater than or equal to 90%; and / or The mass percentage of phase change material in the thermally conductive interface layer is 5%-8%; and / or The catalyst is one or more of chloroplatinic acid catalysts and platinum catalysts.

13. The heat dissipation device according to claim 1, characterized in that, The cold plate is a metal cold plate, and the metal cold plate has a coolant flow channel inside. The coolant flow channel includes one or more combinations of serpentine channels, parallel channels, microchannels or phase change cavities.

14. The heat dissipation device according to any one of claims 1 to 13, characterized in that, The heat dissipation surface of the cold plate is made of metal.

15. The heat dissipation device according to claim 14, characterized in that, The heat dissipation surface of the cold plate is made of aluminum, aluminum alloy, or copper.

16. The heat dissipation device according to any one of claims 1 to 13, characterized in that, The thermally conductive interface layer is bonded to the cold plate through a chemical reaction.

17. The heat dissipation device according to claim 16, characterized in that, The metal cold plate is an aluminum cold plate, and the thermally conductive interface layer is bonded to the aluminum cold plate through Si-O-Al chemical bonds.

18. The heat dissipation device according to any one of claims 1 to 13, characterized in that, The thermally conductive interface layer hardens at a hardening temperature below the phase change temperature range and liquefies at a liquefaction temperature above the phase change temperature range.

19. The heat dissipation device according to any one of claims 1 to 13, characterized in that, The hardening temperature of the thermally conductive interface layer is 25°C, and the thermal decomposition temperature of the thermally conductive interface layer is ≥155°C.

20. The heat dissipation device according to any one of claims 1 to 13, characterized in that, The heat-generating devices include computers, integrated circuit modules, energy storage batteries, photovoltaic modules, supercomputer nodes, power electronic equipment, and spaceborne single units.

21. A method of operating a heat dissipation device according to any one of claims 1 to 13, characterized in that, include: The heat-generating equipment is operated so that the temperature of the heat-conducting interface layer reaches the phase transition temperature range and transforms into a viscoelastic state, in which the viscoelastic heat-conducting interface layer has improved thermal conductivity. as well as The cold plate absorbs the heat conducted through the thermal interface, keeping the thermal interface layer within the phase change temperature range.

22. The method according to claim 21, characterized in that, The heat absorbed by the cold plate through the thermal interface includes: The coolant in the cold plate undergoes a phase change; and The heat conducted through the thermal interface is absorbed by the coolant undergoing phase change.

23. The method according to claim 21, characterized in that, The heat absorbed by the cold plate through the thermal interface includes: The coolant in the cold plate does not undergo a phase change; and The coolant absorbs the heat conducted through the thermal interface.

24. A temperature gradient controller, characterized in that, Configured to control the heat dissipation device according to any one of claims 1 to 13, such that the thermally conductive interface layer is within the phase transition temperature range.

25. A method for manufacturing a heat dissipation device according to any one of claims 1 to 13, characterized in that, Includes the following steps: Plasma activation treatment is applied to the metal surface of the cold plate to form an oxide layer rich in hydroxyl groups. A thermally conductive paste is applied to the metal surface, the thermally conductive paste comprising a mixture of hydrogen-containing silicone oil, α-olefin-modified siloxane, platinum-based catalyst and diamond micron powder; as well as The metal surface is heated to 60°C to 120°C, causing the thermally conductive paste to solidify and form a thermally conductive interface layer, wherein the thermally conductive interface layer is bonded to the metal surface by forming chemical bonds.