Improved plywood / cladding
By combining a polyol-based polymer matrix with randomly oriented fiber segments, a high-strength, durable, and environmentally friendly self-supporting board is manufactured, solving the problems of brittleness and delamination in existing technologies and achieving excellent volume, strength, and natural appearance.
Patent Information
- Application Number
- CN202580016345.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2024-02-20
- Filing Date
- 2025-02-19
- Publication Date
- 2026-11-17
AI Technical Summary
Existing boards have problems with brittleness and insufficient overall strength in self-supporting structures, and are prone to delamination, making it difficult to achieve high integrity, excellent volume and strength, durability and natural appearance at the same time.
The board is manufactured by molding a combination of polyol-based polymer matrix and randomly oriented fiber segments, avoiding the use of traditional extrusion support beams. The mixture of elastomer and filler forms a multi-directional oriented core structure.
It improves the strength and durability of the sheet material, reduces the amount of plastic used, reduces the risk of delamination, provides a soft touch and anti-slip properties, and also has environmental advantages.
Smart Images

Figure CN123125092A_ABST
Abstract
Description
[0001] Invention Field This invention relates to sheet metal.
[0002] In this specification, the term "board" encompasses both "panel" and "clad board." "Panel" refers to a board material capable of being suspended from two or more support points and not significantly bending away from its natural plane when bearing the weight of a person, for example. It does not necessarily have to be laid flat on the floor to substantially maintain its shape. "Clad board" refers to a board material used for covering or coating (e.g., for decorative purposes) a material or structure (e.g., a house) without bending away from its natural plane. In other words, the board material in the sense of this invention is self-supporting.
[0003] Background technology and existing technology known to the applicant Many known "boards" in the prior art are unsuitable for use as flooring or cladding because they are designed to be laid flat on the ground to be adequately supported along their entire length. Therefore, these prior art "boards" are not self-supporting. However, to provide a self-supporting structure, a trade-off must be made between the rigidity of the component and the brittleness of the material. For example, the flooring must be able to withstand the forces generated by a user walking, sitting, lying, and / or standing. Therefore, the flooring must be flexible enough to ensure it does not break during use, while also possessing sufficient strength to be self-supporting and not bend off its natural plane. Equally important is that the materials used do not make the board too heavy to be suspended.
[0004] The closest prior art to this invention is the prior art published by the inventor in 2007, publication number WO2007060392A1.
[0005] Initially, among potentially available off-the-shelf support beams, extruded polymer-based support beams were considered the primary embodiment for producing pavers with sufficient volume and bending strength. Extruded beams are readily available and can therefore be covered with a layer of cushioning material and a top layer with appropriate embossing to achieve the appearance of natural wood, while being made entirely of plastic material.
[0006] Therefore, initial developments in this field focused on producing support beams, followed by adding subsequent overlays to these beams in separate manufacturing steps. In many prior art embodiments, brittleness and insufficient overall strength of the sheet material have been observed. Therefore, to strengthen the sheet material, a fiber pad layer is added to the core.
[0007] Therefore, existing embodiments consist of the following layered structure: 1) an extruded polymer beam; 2) a fiber pad layer located on one side of the extruded polymer beam; 3) a filler-containing polyurethane layer; and 4) a cover layer. It has been found that this structure is prone to delamination.
[0008] This invention proposes several improvements to the manufacturing method of the sheet material, and produces an improved sheet material accordingly.
[0009] Specifically, certain embodiments of the present invention seek one or more of the following objectives: • Provides a method for producing sheet materials with higher integrity to minimize the risk of delamination; • A method is provided that, while reducing the relative amount of plastic material used in the core, excellent volume and strength are still provided, enabling it to be used as a self-supporting sheet. • Provides a more durable and maintenance-free sheet material; It boasts a more natural appearance while providing a soft touch and excellent crack resistance. Summary of the Invention
[0010] In a first broad independent aspect, the present invention provides a method for producing sheet materials (e.g., veneer, cladding), comprising the following steps: • Provide a mold for a sheet material, the mold having an inner relief corresponding to the configuration of the relief to be formed on at least a portion of the outer surface of the sheet material; • Fill the mold with an elastomer portion; • The elastomer is fused with another composition comprising a filler dispersed in a polymer matrix; wherein the polymer matrix is formed of monomers, wherein at least one of the monomers is a polyol; the composition further comprises a foaming agent; and • Provide randomly oriented fiber segments to the other component; thereby the fiber segments are held in multiple directions within the foam of the resulting polymer and filler.
[0011] In some embodiments, this configuration is particularly advantageous because the core completely eliminates the requirement in the prior art to place separately manufactured, extruded support beams into the mold.
[0012] While providing a more efficient manufacturing method, in some embodiments, the method can produce sheets with improved strength and durability while occupying a larger volume, wherein the amount of plastic has been minimized relative to the relatively large volume and relatively large thickness associated with the type of sheet in question.
[0013] This improves the environmental friendliness of the board because the plastic material has a lower density than natural wood, which is prone to decay (which can be very fast in humid environments) and is particularly susceptible to cracking due to temperature fluctuations, while retaining the broad durability advantages of existing technologies.
[0014] Furthermore, in some embodiments, the elastomer and another component can form a better bond without the use of an adhesive, and the elastomer only partially fills the mold, and then another composition is poured onto the elastomer as the fiber segments are pushed into the mixture.
[0015] Furthermore, the present invention provides improved foot comfort, avoids the risk of splintering, and since adjacent layers are preferably fused together in a single process, there is almost no risk of delamination.
[0016] In a dependent aspect, the invention provides a step of penetrating fiber segments into another component while it is being sprayed or cast into a mold. This configuration is particularly advantageous because it allows the fiber segments to be multi-directionally oriented, thereby increasing the mechanical strength of the sheet without causing warping as is the case with fiber pads in the prior art.
[0017] In another subordinate aspect, fiber segments are incorporated into the airflow for injection into the other component. This configuration is particularly effective in promoting a favorable random orientation of the fiber segments within the core of the sheet, which provides additional strength and flexural strength while minimizing or completely avoiding undesirable breakage. Furthermore, this configuration delivers the fiber segments into the mixture in a clean and efficient manner.
[0018] In another aspect, the weight ratio of polyol to filler is less than 1:2.6. In other words, the weight of the filler is at most 2.6 times the weight of the polyol.
[0019] In another aspect, the weight ratio of polyol to filler is between 1:1.8 and 1:2.6. In other words, the filler weighs 1.8 to 2.6 times the weight of the polyol. These ranges are particularly advantageous because they further reduce the amount of plastic material required to produce the core reinforcement. Therefore, the plastic content in the core is minimized to facilitate the formation of a closed-cell structure containing gas, fiber segments, and particulate fillers. This effect is achieved by providing high toughness and high strength. From the perspective of replacing wood-based panels while minimizing plastic usage, this board offers environmental advantages.
[0020] In another aspect, the weight ratio of polyol to filler is greater than 1:1. In other words, the weight of the filler is less than the weight of the polyol.
[0021] In another aspect, the filler is a mineral filler. This configuration is particularly advantageous because it can further reduce the plastic content in the core while providing excellent mechanical properties.
[0022] In another subordinate aspect, the method also includes the step of selecting up to essentially 100% of the filler from the recycled material.
[0023] In another dependent aspect, the method also includes the step of mixing a polyol monomer with an isocyanate monomer used as a blowing agent to form a polymer matrix.
[0024] In another subordinate aspect, the method further includes the step of mixing the elastomer with the filler before casting and / or spraying the mixture of elastomer and filler into a mold.
[0025] In another subordinate aspect, the method also includes the step of placing a conduit into the mold. This configuration is particularly advantageous because it allows the conduit to be incorporated into the mold to facilitate fluid circulation, which is not possible in the support beams of prior art extrusions. It also further improves the connection strength between the conduit and the core without the need for adhesives.
[0026] In another subordinate aspect, the mold is sealed by a metal cap with vents to allow air to escape; the method also includes a step of applying pressure to the filled mold during the curing process before demolding. This configuration is particularly advantageous because it removes unwanted air bubbles.
[0027] In another subordinate aspect, the method also includes a step of removing the sheet material from the mold by suction. This configuration is particularly advantageous because it enables extremely efficient demolding while minimizing the risk of damage during the process.
[0028] In another broad, independent aspect, the invention provides a sheet material (e.g., a veneer, e.g., a cladding) comprising: a core serving as a support beam; one or more cushioning layers comprising an elastomer fixed to the core; and an upper surface comprising an exposed embossed surface, wherein the upper surface forms an anti-slip surface; wherein the core comprises a composition comprising filler dispersed in a polymer foam matrix; wherein the polymer foam matrix is formed of monomers, wherein at least one of the monomers is a polyol; and, in addition to the filler, the core comprises randomly oriented fiber segments.
[0029] This configuration overturns the traditional thinking of using fiber-woven mats, instead providing a stronger core to withstand bending stress, while in at least some embodiments, the core does not require the use of extruded support beams during production.
[0030] This configuration is particularly advantageous because it produces splinter-free flooring and, through its embossed surface, can achieve an appearance similar to real wood or natural stone, while also providing slip resistance and cushioning, making standing exceptionally comfortable and risk-free. Certain embodiments of the invention also exhibit a lower tendency for fungal growth on the flooring, especially when the layers are composed of polymer or plastic materials.
[0031] The material's anti-slip properties are particularly advantageous when the surface is wet. Preferably, the upper layer is homogeneous to prevent abrasion or discomfort, at least where the user's feet will contact the surface. This structure also allows the embossed design on the upper surface to present a natural-looking and soft-to-the-touch concavity and convexity.
[0032] In another aspect, the weight ratio of polyol to filler is less than 1:2.6.
[0033] In another aspect, the weight ratio of polyol to filler is between 1:1.8 and 1:2.6.
[0034] In another subordinate aspect, the weight ratio of polyol to filler is greater than 1:1.
[0035] In another subordinate aspect, the packing material is a mineral packing material.
[0036] On another aspect, up to 100% of the packing material is made from recycled materials.
[0037] In another aspect, the polymer matrix is composed of a mixture of polyol monomers and isocyanate monomers used as blowing agents.
[0038] In another aspect, the polymer matrix can be a polyurethane material.
[0039] In another aspect, the core has a fracture strength greater than 4.6 MPa.
[0040] In another subordinate aspect, at least one of the one or more buffer layers comprises an elastomer and a filler.
[0041] On another subordinate aspect, the core is fused together with one or more buffer layers without the use of adhesives.
[0042] In another aspect, the sheet material may also include conduits at least partially located within the core. In some embodiments, this may be particularly advantageous for securing the conduits within a single, efficient process.
[0043] In another broad, independent aspect of the invention, a sheet material (e.g., a veneer, such as a laminate) is provided. The sheet material includes: a core serving as a support beam; one or more cushioning layers fixed to the core; and an upper layer including exposed embossing, wherein the upper layer forms an anti-slip layer that at least partially covers the one or more cushioning layers. The core is made of a polymeric material comprising fillers dispersed within a polymeric matrix. The polymeric matrix is formed of monomers, wherein at least one of the monomers is a polyol, and the weight ratio of the polyol to the filler is less than 1:2.6. Optionally, the weight ratio of the polyol to the filler is greater than 1:1.
[0044] In this text, the polymer matrix of any aspect of the embodiments of the present invention is referred to as a "polyol-based" polymer matrix. Therefore, according to the definition of the embodiments of the present invention, a polyol-based polymer matrix refers to a polymer matrix in which at least one monomer is a polyol.
[0045] Optionally, the board is a veneer. Optionally, the board is a cladding board.
[0046] Optionally, the cladding panel includes an edge portion, preferably located on an external and / or outward-facing surface (e.g., a surface visible when the cladding panel is installed). Preferably, the edge portion provides a decorative feature.
[0047] In a preferred embodiment, structural support is provided by a core that is stiffer than the outer layers (e.g., buffer layers and upper layers).
[0048] According to certain embodiments of the present invention, a polyol is a molecule having at least two hydroxyl groups. For example, a polyol may have two hydroxyl groups (e.g., diol), three hydroxyl groups (e.g., triol), four hydroxyl groups (e.g., tetraol), etc. Optionally, the polyol may be an aliphatic or aromatic polyol. Optionally, the polyol is an aromatic polyol. Optionally, the (e.g., aromatic) polyol is a low molecular weight (e.g., less than 2000) polyol.
[0049] Optionally, the polymer matrix is composed of a mixture of polyol monomers and isocyanate monomers. Optionally, the isocyanate monomer may be a diisocyanate monomer.
[0050] Optionally, the isocyanate monomer is added in excess (e.g., the polymerization process is limited by the amount of polyol used).
[0051] Optionally, the polymer matrix is polyurethane.
[0052] Optionally, the polymer matrix is foam. Optionally, the polymer matrix is polyurethane foam. Optionally, the polymer matrix according to any aspect further includes glass fibers for reinforcement.
[0053] According to the definitions of various embodiments of the present invention, a filler is a particulate material that can be dispersed in a polymer matrix to alter its physical properties. Generally, the addition of fillers typically increases the modulus (e.g., tensile modulus, such as elastic modulus) of the polymer and polymer material. Therefore, although fillers can increase volume by combining with the polymer material, thereby reducing the amount of polymer used, they also make the polymer material more brittle, thus reducing its fracture strength. This often makes it unsuitable for sheet metal structures, especially for components (e.g., cores) that achieve self-supporting structures.
[0054] However, the inventors unexpectedly discovered that, contrary to conventional wisdom, adding filler within a certain range does not decrease (and in some cases even increases) the breaking strength and breaking deflection. Therefore, the inventors unexpectedly discovered that polymer materials containing filler within the aforementioned specific range achieve an optimal trade-off between physical properties (e.g., ensuring the sheet can self-support the required stiffness) and the volume formed by the filler in the material.
[0055] As described above, the core acts as (for example,) a support beam for the sheet, eliminating the need for a separate extruded support beam. Therefore, the core itself serves to ensure the sheet's self-supporting properties.
[0056] It should be understood that the upper layer may be formed from any one of one or more cushioning layers. Therefore, in some embodiments, the board has a cushioning layer fixed to the core, wherein the cushioning layer includes exposed embossing and provides an anti-slip layer. This cushioning layer thus functions as both a cushioning layer and an upper layer. In some embodiments, the board has one (or more) cushioning layers and a separate upper layer, wherein the compositions of the cushioning layers and the upper layer are slightly different from each other (e.g., slightly different).
[0057] In some embodiments, the weight ratio of polyol to filler is between 1:1.8 and 1:2.6, for example, between 1:2 and 1:2.5. For example, at least 1800 grams of filler are added for every 1000 grams of polyol used to manufacture the polymer material (i.e., a ratio of 1:1.8). For example, no more than 2600 grams of filler material are added for every 1000 grams of polyol used to manufacture the polymer material. This allows the polymer material for the core to be manufactured with reduced plastic usage while providing a robust core that serves as the primary support for the sheet and can withstand the necessary bending moments when supported between two support beams.
[0058] As described above, the core is made of a polyol-based polymer matrix in which filler is dispersed. Optionally, the polymer material may also include other materials dispersed in the polyol-based polymer matrix, such as reinforcing fibers. However, the inventors of various embodiments of the present invention have unexpectedly discovered that when a “base” polymer material (e.g., in which other materials may be contained or dispersed) is used, the physical properties of the core (e.g., tensile strength, deflection at fracture) are significantly improved. In some embodiments, the base polymer material may be considered to consist of a polyol-based polymer matrix and filler dispersed therein, wherein the weight ratio between the polyol and the filler is less than 1:2.6, for example, between 1:1 and 1:2.6, for example, between 1:1.8 and 1:2.6.
[0059] Optionally, the tensile strength of the "base" polymer material is less than 150,000 N / m², for example less than 100,000 N / m², for example less than 90,000 N / m², for example less than 80,000 N / m², for example less than 70,000 N / m², for example less than 60,000 N / m². Optionally, the tensile strength of the core is between 30,000 N / m² and 150,000 N / m², for example between 40,000 N / m² and 100,000 N / m², for example between 50,000 N / m² and 80,000 N / m², for example between 60,000 N / m² and 70,000 N / m², for example about 64,000 N / m². It should be understood that tensile strength is an indicator used to measure the force required to break an object. Therefore, this allows the sheet material to withstand the expected forces during use without breaking.
[0060] Optionally, the resulting core (i.e., made of the "base" polymer material and including other components or materials, such as reinforcing fibers) has a tensile strength greater than 3 MPa, for example greater than 3.5 MPa, for example greater than 4 MPa, for example greater than 4.6 MPa. Optionally, the tensile strength of the resulting core is from 3 MPa to 7 MPa, for example from 4 MPa to 6 MPa, for example from 4.6 MPa to 5.9 MPa.
[0061] Optionally, the filler material is selected as a mineral (e.g., limestone or calcium carbonate) filler material. Optionally, the filler material is high-purity (e.g., greater than 90%, greater than 95%, greater than 98%, greater than 99%, greater than 99.5%) carbonaceous limestone powder.
[0062] Optionally, at least 90% (e.g., at least 95%, at least 98%, at least 99%, or substantially 100%) of the filler material (e.g., limestone) is made from recycled materials. For example, Superlon™ L150 limestone filler made from 100% recycled materials can be used. This makes embodiments of the invention particularly environmentally friendly and allows for the responsible conservation and reuse of resources.
[0063] Optionally, the polymer material also includes reinforcing fibers. This strengthens the core to serve as the primary support for the sheet and enables it to withstand the necessary bending moments when supported between the two support beams.
[0064] Optionally, at least one of the one or more cushioning layers includes an elastomer and a filler (e.g., "filled elastomer"). The filler in the cushioning layer may be the same as or different from the filler dispersed in the core polymer material. Optionally, each (e.g., all) of the one or more cushioning layers includes an elastomer and a filler. In some embodiments, all (one or more) of the cushioning layers may have the same composition; for example, all (one or more) of the cushioning layers may be made of the same elastomer and the same concentration (or content) of filler material. In some embodiments, the composition of some of the cushioning layers may differ from each other. For example, some layers may be made of different elastomers and / or may have different fillers and / or different concentrations of filler. This allows the cushioning layers to be relatively soft and / or resilient, providing a soft feel underfoot when the user walks on the floor.
[0065] Optionally, the upper layer includes an elastomer. Optionally, the upper layer may include both an elastomer and a filler (e.g., "filled elastomer"). The filler in the upper layer may be the same as or different from the filler dispersed in the core polymer material. In some embodiments, the upper layer includes less filler than the filler in each of one or more cushioning layers. For example, the weight percentage of filler in the upper layer is lower than the weight percentage of filler in one of the cushioning layers. For example, the upper layer contains no filler, while the cushioning layer contains filler. This makes the upper layer softer than the cushioning layer, thus providing a better anti-slip surface (especially when wet) and a better feel underfoot when walking on the floor.
[0066] Optionally, the sheet comprises multiple cushioning layers and an upper layer covering at least part of the cushioning layers; one of the cushioning layers is a "filled elastomer," and the upper layer has greater abrasion resistance with less filler (or even no filler) than the cushioning layers. This configuration is particularly advantageous because it maximizes the abrasion resistance of the sheet and enhances its cushioning effect while reducing the material costs required for production.
[0067] Optionally, the buffer layer of the sheet has a Shore hardness (A) in the range of about 20 to about 90 Shore (A). Optionally, the upper layer of the sheet has a Shore hardness (A) in the range of about 15 to about 85 Shore (A).
[0068] Optionally, one or more cushioning layers comprise an elastic foam material. For example, the elastomer of the cushioning layer is polyurethane-based, such as polyurethane. Optionally, the elastomer of the upper layer is polyurethane-based, such as polyurethane. This optional feature helps to achieve a cushioned feel on the sheet while retaining the advantages discussed in the foregoing aspects. The fillers used in the cushioning layer and / or the upper layer may also include, for example, calcium carbonate or flame-retardant fillers.
[0069] Optionally, the board has at least a top surface and side surfaces, both of which are covered by at least one of one or more cushioning layers. For example, the core has at least a top surface and side surfaces, both of which are covered by at least one of one or more cushioning layers. This configuration is particularly advantageous because it protects not only the top surface but also the side surfaces, thereby minimizing the risk of edge slippage or splintering when handling the board.
[0070] Optionally, the core may be covered by at least one and / or the top of one or more cushioning layers. The advantage of this design is that it further enhances the versatility, ease of handling, and performance of the panel regardless of which side the installer chooses to install it from. This is particularly beneficial for user comfort and further reduces the risk of accidents.
[0071] Optionally, the upper layer covers at least the top surface of the slab. Therefore, the cushioning layer may be exposed on the sides of the slab. Optionally, the upper layer covers both the top surface and sides of the slab. Therefore, the cushioning layer on the top surface and sides of the slab is covered by the upper layer. Optionally, the cushioning layer and the core are covered by the slab.
[0072] Optionally, the plate also includes a plurality of lateral protrusions on at least one side and grooves on at least the opposite side for engaging with the lateral protrusions of another plate. This optional configuration is particularly advantageous because it not only secures adjacent plates to each other but also to their predetermined relative positions, thus eliminating the need for leveling adjustments.
[0073] Optionally, the panel has a groove on at least one side. This allows multiple panels to be assembled into a panel assembly surface (e.g., a panel). This design is particularly advantageous because it is suitable for concealed fixing.
[0074] Alternatively, the core is fused together with one or more cushioning layers without the use of adhesives. This means that no removable fasteners are used. This configuration is particularly advantageous because the layers themselves act as adhesives when set together during manufacturing, eliminating the need for additional adhesives.
[0075] Optionally, the top surface of the upper panel has recessed areas to mark appropriate positions for inserting one or more screws or similar objects. This design prevents users from accidentally damaging the heating element during panel installation and eliminates the need for warning stickers to indicate unsuitable screw locations. Templates may also be provided. Attached Figure Description
[0076] Figure 1 A cross-sectional view of the sheet metal located in the mold when it is made entirely by the molding process is shown.
[0077] Figure 2A block diagram of a preferred embodiment of the method is shown.
[0078] Figure 3 shows cross-sectional views of different embodiments of the paving.
[0079] Figure 4 A cross-sectional view of a paving board according to another embodiment of the present invention is shown.
[0080] Figure 5 A cross-sectional view of a paving board according to another embodiment of the present invention is shown.
[0081] Figure 6 A cross-sectional view of a paving board according to another embodiment of the present invention is shown.
[0082] Figure 7 A cross-sectional view of a paving board according to another embodiment is shown.
[0083] Figure 8 shows a perspective view and a top view of the sheet metal according to another embodiment.
[0084] Figure 9 A perspective view of two pavers suitable for being connected to each other via a T-joint is shown.
[0085] Figure 10 A cross-sectional view of a paving material with channels that allow water / air circulation is shown.
[0086] Figure 11 shows two cross-sectional views of a paving with embedded pipes.
[0087] Figure 12 A first embodiment of a bonding mechanism for a water / air circulation paving is shown.
[0088] Figure 13 It shows the use of Figure 12 Side view of the threaded collar of the engagement mechanism.
[0089] Figure 14 A second embodiment of the engagement mechanism is shown.
[0090] Figure 15 A third embodiment of the engagement mechanism is shown.
[0091] Figure 16 A fourth embodiment of the engagement mechanism is shown.
[0092] Figure 17 A fifth embodiment of the engagement mechanism is shown.
[0093] Figure 18 The relationship between the core fracture strength and filler content according to an embodiment of the present invention is shown.
[0094] Figure 19The relationship between core fracture deflection and filler content according to an embodiment of the present invention is shown.
[0095] Detailed description of the attached figures Figure 1 A cross-sectional view of a sheet material made entirely by a molding process is shown.
[0096] The portion of the mold generally designated as 1 is composed of a mold surface layer of plastic material. A portion of the mold is shaped to introduce an embossing 2 inside the mold. This portion of the mold may have embossing with grooves and peaks reminiscent of wood grain on a wooden board. A portion of the mold's side 3 is smooth to provide a smooth surface to the corresponding portion of the board or sheet. While many layered embodiments are envisioned within the scope of the claims following the specification, in one embodiment, there is at least one elastomeric layer 4 and at least one substantially thicker main body layer serving as the core 5. These two layers are fused together during molding to avoid the use of adhesives. Unlike the layers disclosed in the prior art, which are separated by straight boundaries, the boundary between the two main layers of this sheet is not a perfectly straight line. This is clearly visible in the prior art, which discloses straight boundaries between previously separately produced extruded support beams and the outer layers of the sheet.
[0097] The elastomer layer 4 may be less than 5 mm, and preferably about 3 mm. In one embodiment, the elastomer is first cast or sprayed into a mold, followed by casting another component comprising particulate filler dispersed in a polymer matrix, preferably particulate filler; wherein the polymer matrix is formed of monomers, wherein at least one of the monomers is a polyol.
[0098] Furthermore, preferably, a foaming agent is also provided to the mixture as part of the other component. Additionally, it is envisioned during the molding process to provide randomly oriented fiber segments to the other component; thereby, these fiber segments are retained in a multi-directional manner within the resulting polymer and filler foam. In other words, at an appropriate time after the elastomer layer is completed, the other component is provided and bonded thereto, such that the entire layer 5 is formed of a polymer foam comprising particulate filler and fibers; the particulate filler and fibers, when bonded, provide advantageous volume and strength while simultaneously bonding with the elastomer layer. Therefore, layer 5 preferably includes environmentally friendly particulate filler, porosity resulting from the foam, and additional strength gained from advantageously dispersed fibers, which are preferably substantially omnidirectionally dispersed within layer 5.
[0099] In alternative embodiments, other layers are also conceivable. For example... Figure 2 As shown, in optional method step 401, the mold is preferably first treated with a release agent so that the material can be removed after curing and the mold can be reused subsequently.
[0100] It is also envisioned to provide one or more additional layers between the mold and the elastomer. These layers may include at least one coating layer, such as that provided in method step 402. In a further embodiment, two coating layers, as provided in method steps 402 and 403, may be provided, one being a relatively light color and the other a relatively dark color. This alternating arrangement of coating layers gives the embossed surface of the board a contrasting color, thereby producing a so-called shadow effect.
[0101] To ensure proper color results, this process envisions using a brush, either on the initial coating or after several coatings, such as... Figure 2 The method step 404 is shown in the figure.
[0102] As shown in step 405 of the method, another coating may be applied before the elastomer, the color of which may be selected as the main color of the sheet.
[0103] The coating thickness can be on the order of 100 micrometers or less.
[0104] Step 406 is provided to dry the coating and allow some of the moisture to evaporate.
[0105] After a suitable period of time, the elastomer layer can be applied over the coating by spraying or pouring. This can be done by spraying, as shown in step 407, which involves spraying an elastomer containing a flame retardant and smoothing the elastomer to ensure adequate coverage of the main contact surface areas of the sheet.
[0106] Subsequently, this method optionally envisions smoothing the elastomer surface, although an undulating upper surface may facilitate adhesion to another layer subsequently deposited thereon. Therefore, the smoothing step is primarily conceived to ensure that the surface is completely covered by the elastomer.
[0107] The elastomer may contain a suitable flame retardant. However, in a preferred embodiment, the elastomer layer does not contain fiber reinforcement, and the percentage of any particulate filler is much lower than the percentage of particulate filler in the core layer 5.
[0108] Another component forming the core layer 5 is prepared by mixing polyols, fillers, and foaming agents together, such as... Figure 2 The method step 409 is shown. Optionally, pigments may also be added to the mixture.
[0109] Essentially, while pouring the mixture into the mold, fiber segments, particularly single fiber bundles, are poured into or blown into the mixture according to method step 411. These fiber segments can be fiber bundles ranging from 10 to 50 millimeters in length. They can be chopped glass fiber segments cut from fiber bundles on a spool. These chopped fiber segments can be introduced into an airflow, where the turbulence causes the fiber orientation to become approximately random as it is injected into the liquid polymer mixture.
[0110] According to steps 412 and 413, the mold is then sealed on top with a metal plate or cap with vent holes to promote air escape and thus avoid unwanted bubbles.
[0111] The enclosed mold, along with its fixtures, is then transported or conveyed and subjected to high pressure to complete the molding process.
[0112] After a relatively short period of time under pressure, the mold is restored to atmospheric pressure, and the finished sheet is extracted from the mold by vacuum process according to method step 414 for demolding. Figure 2 The order of the steps in the method shown can be modified, and some steps are optional.
[0113] Figure 3a appears similar to the inventor's previously published documents cited in the background section, but due to the reference... Figure 1 The different production methods described result in fundamentally different final structures for each of these products.
[0114] When the above production method is applied, the cross-section of the paving plate 7 can be obtained, wherein the core 5 can be... Figure 1 The type described in [the text]. The paving has a substantially rectangular cross-section, with the core acting as a substantially rigid support beam, rather than a separate extruded component made of plastic material. Although Figure 1 The buffer layer 4 is shown to be primarily located at the bottom of the mold to form the upper surface of the sheet after curing, but... Figure 3A One embodiment is envisioned in which a buffer layer 6 (or multiple layers 4 and 6) completely covers the board material. On top of the buffer layer 6, an upper layer 4 is provided, which extends only across the top surface of the board material.
[0115] The embodiment shown in Figure 4 illustrates that the upper layer of the embodiment shown in Figure 3a extends at least partially to the sides and / or ends of the board. Alternatively, the upper layer may also extend completely to the sides and / or ends of the board.
[0116] The support beam forms a robust, rigid core to support foot loads. This support beam can be made of a polymer material in which filler is dispersed.
[0117] Figure 3a shows a core that is essentially completely filled except for the porosity of the foam polymer used. Because it is largely completely filled, screws can be screwed into and secured the buffer layer, the upper layer, and the support beams or core.
[0118] Referring back to the description of Figure 3a, the buffer layers (or multiple layers) 4 and 6 can be "filled elastomers". Preferably, the elastomer is polyurethane. The filler can be, for example, calcium carbonate or flame-retardant filler. The upper layer 4 can be made of a higher purity polyurethane material for better abrasion resistance.
[0119] The upper layer of this paving material includes a set of grooves and peaks (i.e., exposed embossed surfaces), which can also mimic the textures of antique wood, natural stone, terracotta, etc. The softer embossed surface also helps enhance the slip resistance of the upper layer. This "filled polyurethane" can be foamed.
[0120] As an alternative to the embodiment shown in FIG3a, FIG3b shows a paving 8 having a reference Figure 1 The reinforcing core 9 is of the type described, but now this reinforcing core is completely encapsulated within a single layer of homogeneous cushioning material 10, which may be a "foamed" type with "filled polyurethane". In this example, the single layer of cushioning 10 simultaneously constitutes the cushioning layer and the upper layer, providing the top surface of the board on which the user can walk.
[0121] Both the side portions 11 and 12 of the reinforcing core are covered with cushioning material. An embodiment of the invention is envisioned in which only the top surface and sides 11 and 12 of the supporting beam are covered with cushioning and / or an upper layer of material.
[0122] In another embodiment, Figure 3c shows a reinforced core 14 and a buffer / upper layer 15 on only the upper top surface, which together form a paving 13. The upper layer 15 may be cast onto the top of the support beam.
[0123] Figure 3d shows the reinforced core 16 covered by a buffer layer / upper layer 17, which completely encloses the reinforced core and includes an exposed embossed surface. In this embodiment, its upper surface can be a softer surface compared to conventional wood. Nevertheless, it will still retain the appearance of real wood and is classified as non-slip, especially due to the embossed structure. The plastic material used can be a material with fire-resistant / flame-retardant properties.
[0124] Figure 3e shows a paving material including a reinforcing core 18 and a buffer / upper layer 19, which is applied only to the top, sides and ends of the reinforcing core.
[0125] Figure 3f shows a panel in which the reinforcing core 20 has a buffer / upper layer 21 on the top surface of the panel.
[0126] The polymer material used can be a material with fire-resistant / flame-retardant properties.
[0127] Figure 5 A paving material, generally designated 204, is shown, having a rigid reinforcing core 205, which can be manufactured according to... Figure 1 The method shown involves forming the core in a mold and adding multiple longitudinal grooves 206. A softer travel surface 207 is provided on the top and side surfaces of the rigid reinforced core. The harder core can be molded onto the softer "surface".
[0128] like Figure 6 As shown, the groove 206 is closed near the end—for example, end 208. Figure 5 It is also shown that, in this embodiment, the upper layer 207 covers both the ends and the sides.
[0129] Figure 7 Another type of decking is shown, generally designated 209, which has side grooves 210 and 211. These grooves can be located on one side of the two sides to accommodate concealed fasteners. This embodiment may include references... Figure 1 The type of reinforced core.
[0130] Furthermore, preferably, the Shore hardness (A) of the overlay of the paving is in the range of about 20 to about 90 Shore (A).
[0131] Because the reinforcing core is positioned behind the elastomer layer, electrical components or conduits can also be embedded within it, not only enhancing the strength of the reinforcing core but also providing protection for the components effectively embedded within it. The mold can be designed in a suitable shape to mimic antique wood, stone, or terracotta, and to indicate the screw insertion position. Other suitable mold configurations are conceivable.
[0132] In addition, it is conceivable to cast conduits or pipes—such as hollow tubes—along with a plastic cover layer so that heating cables can be slid into them after the slab is formed.
[0133] Figures 8a and 8b show two portions of two panels, wherein the protrusions of panel 212, such as protrusions 213 and 214, are sized and shaped to fit into corresponding grooves 215 and 216 located on the side of panel 217. Protrusions such as protrusion 213 are provided with side wings 218 and 219, which allow the protrusion to be locked in place when pressed into grooves such as groove 216, which have corresponding lateral cutouts such as cutout 220. In this embodiment, panel 217 comprises a polyurethane cushioning / upper layer 221 with a thickness selected in the range of 2 to 7 mm.
[0134] Figure 9 Two plates of the type shown in Figure 8a are illustrated, along with a T-shaped member for insertion into holes on the sides of the plates to secure them together in a so-called "invisible" manner.
[0135] While the foregoing embodiments specifically envision the use of resistance heating, the use of fluid-heated panels, such as water-heated or hot-air-heated panels, is also envisioned. The panel is envisioned to include pipes or extruded hollow supports that not only support the panel but also function as water / air distributors.
[0136] Figure 10A plate 301 is shown, which has as follows Figure 1 The enhanced core region 302 of this type has multiple tunnels to guide the flow of liquid or air, enabling the plate to function as a heat exchanger. The core region is encapsulated in a buffer layer 303 made of resin, which includes a relatively soft upper layer 304.
[0137] Figures 11a and 11b illustrate two additional embodiments of the heated liner, wherein the conduit is cast or molded into the resin of a reinforcing core, which may be... Figure 1 The described type, and according to Figure 2 The plate is manufactured using the method shown in Figure 11a, which illustrates a circular tube 305, while the plate in Figure 11b contains a square tube 306.
[0138] Various joining mechanisms can be used between adjacent pipes or plates. For example, Figure 12 shows two plates 307 and 308 supported on a support beam within a joining area, where a threaded collar 309 is embedded. Figure 13 As shown, the threaded collar includes a flange 310, with threads on both sides of the flange 310. These threads on both sides of the flange can simultaneously engage with the hollow cores of two adjacent plates. The flange can be multi-faceted to allow for easy screwing in with a wrench.
[0139] Figure 14 Another embodiment of the joining mechanism between adjacent plates 311 and 312 is shown. Each plate is provided with cast-in connectors 313 and 314, which can form a waterproof connection with a short tube inserted between the connectors.
[0140] Figure 15 shows another joining mechanism in which an encapsulated tubing or hollow extruded support is used, with a connector in the form of a tube 315 and equipped with O-rings, such as O-rings 316, the size and shape of which are designed to ensure a waterproof connection between the two panels.
[0141] Figure 16 Two adjacent panels 317 and 318 are shown, along with a tube 319 that simply needs to be glued into the channel provided in each panel.
[0142] Figure 17 The end of the manifold is shown, with a larger diameter connecting end to facilitate positioning of the adhesive-secured tube 320.
[0143] It is conceivable that the connecting pipe may or may not be flexible.
[0144] The present invention also envisions that the fluid flowing through the paving board can be heated or cooled to function as a heater or cooler. The present invention envisions, optionally, that in summer, the paving board be installed around the swimming pool, with a pump placed between the paving board and the pool water to cool the paving board while simultaneously heating the pool water.
[0145] The plastic tubes (possibly two) cast into the buffer layer can simultaneously serve as support beams and fluid conduits.
[0146] Figure 18 The relationship between the fracture strength of a polymer core comprising limestone filler dispersed therein and the amount of filler added per 1000 grams of polyol used to form the polymer material is shown. Similarly, Figure 19 The relationship between the fracture deflection of a polymer core comprising limestone filler dispersed therein and the amount of filler added per 1000 grams of polyol used to form the polymer material is shown.
[0147] The data points shown in Figures 18 and 19 represent the average of multiple repeated measurements. All measurements were performed using a Mecmesin MultiTest-i dual-column force gauge on a core sample measuring 250 mm × 32 mm × 50 mm (length × height × width).
[0148] In order to obtain Figure 18 To obtain fracture strength data, the sample was placed in a Mecmesin Multi-Test 25-i tester, and a point load was positioned at the midpoint (100 mm) between two support points (e.g., a distance of 200 mm between the support points). The point load was located on the top surface of the sample, while the two support points were located on the bottom surface. The tester was then run at a speed of 250 mm / min (i.e., moving the point load downwards (e.g., towards the center of the support points) by 250 mm per minute). Therefore, the fracture strength was determined as the point where the load reached its peak value, i.e., the maximum force causing the sample to fracture.
[0149] To obtain the fracture deflection data shown in Figure 19, a three-point bending test was conducted with a center-to-center distance of 200 mm between the two support points. Therefore, the fracture deflection corresponds to the maximum load (i.e., force) applied that caused the sample to fracture.
[0150] It can be seen that as the filler content in the polymer material increases, the core tends to fracture at lower force values and exhibit less deflection. This is consistent with the conventional understanding that adding fillers to polymer materials increases their brittleness (leading to reduced flexibility and thus reduced bending) and reduces their strength (e.g., fracture at lower force values).
[0151] However, as the data shows, the inventors unexpectedly discovered a range of filler content within which the fracture strength and deflection were essentially unaffected. In fact, the fracture strength was even improved.
[0152] Therefore, the inventors discovered that, advantageously, 1800 grams (per 1000 grams of polyol) to 2600 grams (per 1000 grams of polyol) of filler can be incorporated into the reinforcing core without reducing the physical properties of the plywood to a usable level. Thus, the reinforcing core possesses excellent overall strength and does not need to be entirely composed of polyurethane. Therefore, while providing excellent physical properties, the plastic content can be reduced.
Claims
1. A method for producing sheet metal, comprising the following steps: • A mold for a sheet material is provided, the mold having an inner relief corresponding to the configuration of the relief to be formed on at least a portion of the outer surface of the sheet material; • The mold is partially filled with an elastomer; • The elastomer is fused with another composition comprising a filler dispersed in a polymer matrix; wherein the polymer matrix is formed of monomers, wherein at least one of the monomers is a polyol; the composition further comprises a foaming agent; and • Provide randomly oriented fiber segments to the other component; thereby, the fiber segments are held in a multi-directional manner in the resulting polymer and filler foam.
2. The method of claim 1, further comprising the step of: injecting fiber segments into the other component while injecting or casting the other component into the mold.
3. The method according to claim 1 or 2, wherein, The fiber segments are mixed into the airflow to be sprayed into the other component.
4. The method according to any one of the preceding claims, wherein, The weight ratio of the polyol to the filler is less than 1:2.
6.
5. The method according to claim 4, wherein the weight ratio of the polyol to the filler is between 1:1.8 and 1:2.
6.
6. The method according to any one of claims 1 to 3, wherein, The weight ratio of the polyol to the filler is greater than 1:
1.
7. The method according to any one of the preceding claims, wherein, The packing material is a mineral packing material.
8. The method according to any one of the preceding claims further comprises the step of selecting up to substantially 100% of the filler from the recycled material.
9. The method according to any one of the preceding claims further comprises the step of: forming the polymer matrix by mixing a polyol monomer with an isocyanate monomer used as a blowing agent.
10. The method according to any one of the preceding claims further includes the step of mixing the elastomer with the filler.
11. The method according to any one of the preceding claims further includes the step of: placing a pipe into the mold.
12. The method according to any one of the preceding claims, wherein, The mold is sealed by a metal cap with vent holes to allow air to escape; the method also includes the step of applying pressure to the filled mold during the curing process before demolding.
13. The method according to any one of the preceding claims further includes the step of: removing the sheet material from the mold by suction.
14. A type of board material, comprising: The core used to support the beam; One or more buffer layers, the one or more buffer layers including an elastomer, the elastomer being held on the core; as well as The upper surface includes exposed relief, wherein the upper surface forms a non-slip surface; The core comprises a composition including filler dispersed within a polymer foam matrix; The polymer foam matrix is formed from monomers, wherein at least one of the monomers is a polyol; and the core comprises randomly oriented fiber segments, which are other components besides the filler.
15. The sheet metal according to claim 14, wherein, The weight ratio of the polyol to the filler is less than 1:2.
6.
16. The sheet metal according to claim 15, wherein, The weight ratio of the polyol to the filler is between 1:1.8 and 1:2.
6.
17. The sheet metal according to claim 14, wherein, The weight ratio of the polyol to the filler is greater than 1:
1.
18. The sheet metal according to any one of claims 14 to 17, wherein, The packing material is a mineral packing material.
19. The plate according to any one of claims 14 to 18, wherein, Up to 100% of the filler is made from recycled materials.
20. The plate according to any one of claims 14 to 19, wherein, The polymer matrix is formed by mixing polyol monomers with isocyanate monomers used as foaming agents.
21. The plate according to any one of claims 14 to 20, wherein, The polymer matrix is a polyurethane material.
22. The plate according to any one of claims 14 to 21, wherein, The core has a fracture strength greater than 4.6 MPa.
23. The sheet metal according to any one of claims 14 to 22, wherein, At least one of the one or more buffer layers includes an elastomer and a filler.
24. The sheet metal according to any one of claims 14 to 23, wherein, The core is fused together with the one or more buffer layers without the use of adhesives.
25. The sheet material according to any one of claims 14 to 24, further comprising a conduit at least partially located inside the core.
Citation Information
Patent Citations
Decking plank
WO2007060392A1