Alumite color layer resin coating device

By adopting a lifting roller and scraper structure in the anodized aluminum color layer resin coating equipment, the problem of poor coating uniformity is solved, the color layer resin on the anodized aluminum surface is evenly coated and smoothed, and the coating effect is improved. .

CN221789864UActive Publication Date: 2024-10-01JIANGSU LANYING PACKING MATERIAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420311633.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-20
Publication Date
2024-10-01
Estimated Expiration
2034-02-20

AI Technical Summary

Technical Problem

During the coating process of the existing anodized aluminum color layer resin coating equipment, due to the lack of a pressure roller cleaning structure, the coating effect gradually deteriorates and the uniformity is poor.

Method used

An anodized aluminum color layer resin coating device including a coating chamber and a drying chamber is designed. The first and second liftable pressure rollers are used to press the anodized aluminum on the coating roller and smoothing roller respectively. Use a scraper to scrape off the color layer resin on the smoothing roller to ensure uniform coating.

Benefits of technology

Through this device, the resin of the color layer on the surface of the anodized aluminum is evenly coated and smoothed, avoiding the deterioration of the coating effect and improving the uniformity of the coating process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221789864U_ABST
    Figure CN221789864U_ABST
Patent Text Reader

Abstract

The utility model discloses an alumite color layer resin coating device, which relates to the technical field of alumite hot stamping foil processing, and comprises a partition plate fixedly connected in a coating box, and the coating box is divided into a coating chamber and a drying chamber by the partition plate; an inlet / outlet penetrating through the coating chamber and the drying chamber is formed in the coating box; the coating structure and the uniform smearing structure are respectively arranged in the coating box; the air collecting box is fixedly connected into the drying chamber, a plurality of air outlet holes are formed in the face, corresponding to the alumite, of the air collecting box, and an air inlet pipe penetrating through the side wall of the drying chamber is arranged on the air collecting box; the alumite color layer resin coating device has the advantages of being convenient to use, improving the uniformity of alumite color layer resin coating, being more convenient and practical and the like.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of electrochemical aluminum hot stamping foil processing, in particular to an electrochemical aluminum color layer resin coating device. Background Art

[0002] Electrochemical aluminum hot stamping foil is mainly composed of PTE film layer, release layer, color layer, aluminum plating layer and glue layer. The main components of the color layer are film-forming, heat-resistant, transparent, suitable synthetic resin and dye. During production, the resin and dye are dissolved in organic solvent to form color paste, which is then coated and dried.

[0003] For example, patent application number CN202222843774.3 discloses a device for coating color layer resin on electroplated aluminum. The patent first spreads the electroplated aluminum on the upper end of the operating table 5, and evenly coats the color layer resin on the electroplated aluminum in a slender S shape. At this time, the electric telescopic rods 11 on both sides are simultaneously started to extend, and the connecting block 93 is pushed downward by the extension of the electric telescopic rods 11. The fixed rod 91 slides in the two slide grooves 71 to drive the pressure roller 92 to move downward, and the slider 94 slides in the corresponding connecting groove 72 to improve the stability of the pressure roller 92 during the adjustment process, thereby adjusting the distance between the pressure roller 92 and the electroplated aluminum to meet the color requirements of different thicknesses. The coating assembly 9 is driven by the mobile frame 7 to move forward and backward to evenly smooth the color layer resin, thereby realizing even coating of the color layer resin. Manual operation is not required, and the degree of automation is high, so that the color layer resin is suitable for large-scale and large-volume production.

[0004] In the coating method of the prior art, since the coating roller is at the top, during the coating process, the color layer resin needs to be evenly coated on the electroplated aluminum first, and then adjusted with a pressure roller. Then, when the pressure roller is evenly smoothing, the color layer resin will also stick to the surface of the pressure roller. Due to the lack of a pressure roller cleaning structure, the amount of color layer resin on the pressure roller will gradually increase, which will cause the subsequent coating method to be increasingly poor and uneven. Utility Model Content

[0005] The technical problem to be solved by the utility model is to provide a resin coating device for an electrochemical aluminum color layer, so as to solve the problem of poor coating uniformity of the coating equipment for the electrochemical aluminum color layer in the prior art described in the background technology.

[0006] To achieve the above purpose, the utility model provides the following technical solutions: an electrochemical aluminum color layer resin coating device, comprising

[0007] A partition is fixedly connected to the coating box, and the partition separates the coating box into a coating chamber and a drying chamber;

[0008] The coating box has an inlet and outlet that penetrates the coating chamber and the drying chamber;

[0009] A box cover, covering the open end of the coating box;

[0010] The coating structure and the spreading structure are respectively arranged in the coating box;

[0011] An air collecting box is fixedly connected to the drying chamber, and a plurality of air outlet holes are arranged on one side of the air collecting box corresponding to the anodized aluminum. The air collecting box has an air inlet pipe that passes through the side wall of the drying chamber;

[0012] The coating structure includes

[0013] A coating pool, fixedly connected to the bottom of the coating chamber;

[0014] A coating roller is rotatably disposed on the inner wall of the coating tank;

[0015] The baffle is fixedly connected to the inner wall of the coating tank and has a gap between it and the coating roller;

[0016] The first pressing roller is arranged in the coating chamber in a liftable manner and is located above the coating roller; it is used to press the anodized aluminum onto the coating roller;

[0017] The smearing structure includes

[0018] The material receiving pool is fixedly connected to the coating chamber;

[0019] A spreading roller is rotatably arranged on the inner wall of the material receiving pool;

[0020] A scraper is fixedly connected to the inner wall of the material receiving pool, and the scraper is in sliding contact with the outer wall of the smoothing roller;

[0021] The second pressing roller is arranged in the coating chamber in a liftable manner and is located above the spreading roller; it is used to press the electrochemical aluminum onto the spreading roller.

[0022] Preferably: the inner wall of the coating chamber is fixedly connected with a first cross beam plate, the first cross beam plate is fixedly connected with a first positioning plate through a plurality of springs, the first pressure roller is rotatably arranged on the first positioning plate, and the first positioning plate has a guide rod slidingly passing through the spring and the first cross beam plate.

[0023] Preferably: a lift plate which can be raised and lowered is arranged in the coating chamber, a pressure sensor is fixedly connected to the lift plate, a stress surface of the pressure sensor is fixedly connected to a second positioning plate, and the second pressure roller is rotatably arranged on the second positioning plate.

[0024] Preferably: the drying chamber has an exhaust hole on its side wall.

[0025] Preferably, the air outlet holes on the air collecting box face the upper surface of the anodized aluminum.

[0026] The beneficial effects of adopting the above technical solution are:

[0027] The present application can press the anodized aluminum onto the coating roller by setting up a first pressure roller, so that the color layer resin on the coating roller can be smeared on the anodized aluminum, and then press the anodized aluminum onto the smoothing roller by the second pressure roller, so that the color layer resin on the anodized aluminum is more uniform, and the scraper can scrape off the color layer resin on the smoothing roller, so that no color layer resin will remain on the smoothing roller. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 The utility model is a schematic diagram of an electrochemical aluminum color layer resin coating device.

[0029] Figure 2 The utility model is a cross-sectional view of an electrochemical aluminum color layer resin coating device.

[0030] Figure 3 This utility model Figure 2 Magnified view of the coating structure.

[0031] Figure 4 This utility model Figure 2 A magnified view of the smooth structure.

[0032] Figure 5 It is a schematic diagram of the coating structure of the utility model.

[0033] Figure 6 It is a schematic diagram of the smoothing structure of the utility model.

[0034] Among them: coating box 10, box cover 11, inlet and outlet 20, limiting roller 21, partition 30, coating chamber 31, drying chamber 32, coating structure 40, coating pool 41, coating roller 42, baffle 43, first pressure roller 44, first positioning plate 45, spring 46, first cross beam 47, guide rod 48, smoothing structure 50, material receiving pool 51, smoothing roller 52, hanging plate 53, second pressure roller 54, second positioning plate 55, pressure sensor 56, lifting plate 57, second cross beam 58, lifting cylinder 59, air collecting box 60, air outlet 61, air inlet pipe 62, exhaust hole 63. DETAILED DESCRIPTION

[0035] The embodiments of the present utility model are described in detail below with reference to the accompanying drawings.

[0036] like Figure 1-6 In the first embodiment, a device for coating an electrochemical aluminum color layer with resin includes:

[0037] The partition 30 is fixedly connected to the coating box 10, and the partition 30 separates the coating box 10 into a coating chamber 31 and a drying chamber 32; the coating box 10 has an inlet and outlet 20 penetrating the coating chamber 31 and the drying chamber 32;

[0038] A box cover 11, covering the open end of the coating box 10;

[0039] The coating structure 40 and the spreading structure 50 are respectively disposed in the coating box 10;

[0040] The air collecting box 60 is fixedly connected to the drying chamber 32. A plurality of air outlet holes 20 are arranged on one side of the air collecting box 60 corresponding to the anodized aluminum. The air collecting box 60 has an air inlet pipe 62 that penetrates the side wall of the drying chamber 32.

[0041] The coating structure 40 includes

[0042] The coating pool 41 is fixedly connected to the bottom of the coating chamber 31;

[0043] A coating roller 42 is rotatably disposed on the inner wall of the coating pool 41;

[0044] The baffle plate 43 is fixedly connected to the inner wall of the coating tank 41 and has a gap between it and the coating roller 42;

[0045] The first pressing roller 44 is movably disposed in the coating chamber 31 and is located above the coating roller 42; it is used to press the electrochemical aluminum onto the coating roller 42;

[0046] The smearing structure 50 includes

[0047] The material receiving pool 51 is fixedly connected to the coating chamber 31;

[0048] A smoothing roller 52 is rotatably disposed on the inner wall of the material receiving pool 51;

[0049] The scraper 53 is fixedly connected to the inner wall of the material receiving pool 51, and the scraper 53 is in sliding contact with the outer wall of the smoothing roller 52;

[0050] The second pressing roller 54 is arranged in the coating chamber 31 in a liftable manner and is located above the smearing roller 52 ; it is used to press the electrochemical aluminum onto the smearing roller 52 .

[0051] This embodiment is implemented as follows:

[0052] When the present application is used, the electrochemical aluminum passes through the inlet and outlet 20, and the first pressing roller 44 presses the lower surface of the electrochemical aluminum onto the coating roller 42, and the second pressing roller 54 presses the lower surface of the electrochemical aluminum onto the smearing roller 52, and then the electrochemical aluminum moves, and the coating roller 42 rotates at the same time, and the coating roller 42 takes away the color layer resin in the receiving pool 41 and coats it on the moving electrochemical aluminum, and the gap between the baffle 43 and the coating roller 42 is the thickness of the color layer resin on the coating roller 42, so as to avoid excessive color layer resin on the coating roller 42;

[0053] The rotation of the smearing roller 52 will evenly spread the color layer resin on the anodized aluminum and take away a part of it, so that the color layer resin on the anodized aluminum is more uniform, and the scraper 53 can scrape off the color layer resin sticking on the smearing roller 52, so that it will not accumulate on the smearing roller 52, thereby improving the smearing effect;

[0054] Then the electroplated aluminum enters the drying chamber 32 and is connected to an external hot air blower through the air inlet pipe 62, so that the hot air flows out through the air outlet 61 on the air collecting box 60 and blows on the electroplated aluminum to dry the color layer resin on the electroplated aluminum.

[0055] The advantage of the present application over the prior art is that it makes the coating process more uniform.

[0056] See also Figure 2 , 3 5. The inner wall of the coating chamber 31 is fixedly connected with a first cross beam plate 47, which is fixedly connected with a first positioning plate 45 through a plurality of springs 46. The first pressing roller 44 is rotatably arranged on the first positioning plate 45, and the first positioning plate 45 has a guide rod 48 which slides through the spring 46 and the first cross beam plate 47;

[0057] The spring 46 is provided to make the first positioning plate 45 and the first cross beam plate 47 elastic, so that the first pressure roller 44 can elastically press the electroplated aluminum onto the coating roller 42, and the guide rod 48 can make the first positioning plate 45 move only in the vertical direction.

[0058] See also Figure 2 , 4 6. A lifting plate 57 is provided in the coating chamber 31. A pressure sensor 56 is fixedly connected to the lifting plate 57. A stress surface of the pressure sensor 56 is fixedly connected to a second positioning plate 55. The second pressure roller 54 is rotatably provided on the second positioning plate 55.

[0059] When the second pressure roller 54 presses the electroplated aluminum onto the smoothing roller 52 , it will be subjected to a reaction force. At this time, the reaction force will be transmitted to the pressure sensor 56 through the second positioning plate 55 . Therefore, the pressure sensed by the pressure sensor 56 can control the lifting range of the lifting plate 57 .

[0060] See also Figure 2 , 4 6. A second cross beam plate 58 is fixedly connected in the coating chamber 31, a lifting cylinder 59 is fixedly connected to the second cross beam plate 58, and an output end of the lifting cylinder 59 is fixedly connected to the lifting plate 57;

[0061] The lifting plate 57 can be driven to move vertically on the second cross beam plate 58 by the lifting cylinder 59 .

[0062] See also Figure 2 , the side wall of the drying chamber 32 is provided with an exhaust hole 63;

[0063] The exhaust holes 63 can more conveniently discharge the dried water vapor out of the drying chamber.

[0064] See also Figure 2 , the air outlet 61 on the air collecting box 60 faces the upper surface of the anodized aluminum;

[0065] The air outlet 61 on the air collecting box 60 is not directly facing the color layer resin on the electroplated aluminum, which can avoid the influence of wind force on the uniformity of the color layer resin.

[0066] The above are only preferred implementations of the present invention. It should be pointed out that, for ordinary technicians in this field, several modifications and improvements can be made without departing from the creative concept of the present invention, which all belong to the protection scope of the present invention.

Claims

1. A device for coating an electrochemical aluminum color layer with resin, comprising: A partition is fixedly connected to the coating box, and the partition separates the coating box into a coating chamber and a drying chamber; The coating box has an inlet and outlet that penetrates the coating chamber and the drying chamber; A box cover, covering the open end of the coating box; The coating structure and the spreading structure are respectively arranged in the coating box; An air collecting box is fixedly connected to the drying chamber, and a plurality of air outlet holes are arranged on one side of the air collecting box corresponding to the anodized aluminum. The air collecting box has an air inlet pipe that passes through the side wall of the drying chamber; The coating structure includes A coating pool, fixedly connected to the bottom of the coating chamber; A coating roller is rotatably disposed on the inner wall of the coating tank; The baffle is fixedly connected to the inner wall of the coating tank and has a gap between it and the coating roller; The first pressing roller is arranged in the coating chamber in a liftable manner and is located above the coating roller; it is used to press the anodized aluminum onto the coating roller; The smearing structure includes The material receiving pool is fixedly connected to the coating chamber; A spreading roller is rotatably arranged on the inner wall of the material receiving pool; A scraper is fixedly connected to the inner wall of the material receiving pool, and the scraper is in sliding contact with the outer wall of the smoothing roller; The second pressing roller is arranged in the coating chamber in a liftable manner and is located above the spreading roller; it is used to press the electrochemical aluminum onto the spreading roller.

2. The device for coating an electrochemical aluminum color layer with resin according to claim 1, characterized in that: The inner wall of the coating chamber is fixedly connected with a first cross beam plate, and the first cross beam plate is fixedly connected with a first positioning plate through a plurality of springs. The first pressure roller is rotatably arranged on the first positioning plate, and the first positioning plate has a guide rod which slides through the spring and the first cross beam plate.

3. The device for coating an electrochemical aluminum color layer with resin according to claim 1, characterized in that: A lifting plate that can be raised and lowered is arranged in the coating chamber, a pressure sensor is fixedly connected to the lifting plate, a stress surface of the pressure sensor is fixedly connected to a second positioning plate, and the second pressure roller is rotatably arranged on the second positioning plate.

4. The electrochemical aluminum color layer resin coating device according to claim 1, characterized in that: The side wall of the drying chamber is provided with an exhaust hole.

5. The electrochemical aluminum color layer resin coating device according to claim 1, characterized in that: The air outlet on the air collecting box faces the upper surface of the anodized aluminum.