Miniature chip inductor
By using L-shaped external electrodes and reinforcing block structures in miniature chip inductors, combined with optimized internal coil and marking layer designs, the problem of large parasitic capacitance and easy damage in the existing technology is solved, and small capacitance and high Q value are achieved. and structurally stable miniature chip inductors.
Patent Information
- Application Number
- CN202323647253.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-29
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2033-12-29
AI Technical Summary
Existing multi-layer laminated chip ceramic inductors have problems such as large parasitic capacitance at high frequencies, low Q value, and easy damage during detection.
The L-shaped external electrode and reinforcing block structure are used to reduce parasitic capacitance, improve the Q value, and protect the ceramic layer from damage through the reinforcing block. At the same time, the structure of the internal coil insulation layer and marking layer is optimized to improve material strength and ease of processing.
A miniature chip inductor with small parasitic capacitance, large Q value, stable structure, and not easily damaged is realized, which improves the material strength and provides protection during the detection process.
Smart Images

Figure CN221805274U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of multilayer ceramic chip inductors, in particular to a miniature chip inductor. Background Art
[0002] There are currently two product forms of multilayer laminated chip ceramic inductors. One is a full-terminal product form. Because the product pad needs to cover the entire product end, the parasitic capacitance formed at high frequencies is large, and the product Q value is low. However, the advantage of this structure is that the full-terminal product is protected by the external pad. During the current test, the test needle needs to be inserted into the product for testing. During the test, the metal probe contacts the soft tin plating and will not penetrate the ceramic layer. The tin plating acts as a buffer and will not cause damage to the product. Therefore, there is a need for a miniature chip inductor with small parasitic capacitance, large Q value, stable structure, and not easily damaged during testing. Utility Model Content
[0003] In order to solve the above problems, a miniature chip inductor with small parasitic capacitance, large Q value, stable structure and not easy to be damaged is provided. The utility model adopts the following technical solutions.
[0004] A miniature chip inductor comprises a marking layer, an upper substrate insulating layer, a lower substrate insulating layer, a plurality of internal coil insulating layers, and external electrodes, wherein the external electrodes comprise a first external electrode and a second external electrode, the internal coil insulating layer is located between the upper substrate insulating layer and the lower substrate insulating layer, the first external electrode and the second external electrode are respectively connected to the lower substrate insulating layer and the upper substrate insulating layer at both ends, the cross section of the external electrode is L-shaped, and a reinforcing block is provided at the bottom of the lower substrate insulating layer.
[0005] First, the utility model adopts an L-shaped external electrode, which is different from the full-terminal product form, which greatly reduces the parasitic capacitance and greatly improves the Q value. However, since the L-shaped external electrode cannot wrap the entire product, the metal probe can easily penetrate the ceramic layer during the detection process, causing damage to the product. Therefore, the utility model adopts a reinforcing block structure to play a protective role and prevent the utility model from being damaged during the detection process.
[0006] Preferably, the identification layer includes a first identification layer and a second identification layer, the first identification layer is disposed above the upper substrate insulation layer, and the second identification layer is disposed below the lower substrate insulation layer.
[0007] The utility model adopts a marking layer structure, which can distinguish the upper and lower parts of the utility model, and has the advantages of being easy to process and easy to identify.
[0008] Preferably, the reinforcement block includes a first reinforcement block, a second reinforcement block and a third reinforcement block, the first reinforcement block is located below the second reinforcement block, the second reinforcement block is located below the first external electrode and the second external electrode, and the third reinforcement block is connected to the first external electrode and the second external electrode, respectively.
[0009] The utility model adopts a three-layer reinforcement block structure, which can play a protective role to prevent the utility model from being damaged during the detection process, and can also play a role in preventing the metal detection needle from being deviated.
[0010] Preferably, the internal coil insulation layer comprises a first internal coil insulation layer and a second internal coil insulation layer, the first internal coil insulation layer and the second internal coil insulation layer are alternately arranged, a coil layer is provided on the first internal coil insulation layer, and a conductive through hole is provided on the second internal coil insulation layer.
[0011] The utility model has two structures including coils and excluding coils. When an internal coil layer is provided, under the same sintering conditions, the material strength of the product with the reinforcement block is at least 1.5 times that of the product without the reinforcement block, the dielectric constant is less than or equal to 8, and the dielectric loss is ≤0.005; when the internal coil 5 is not provided, the material strength of the product with the reinforcement block is at least 1.5 times that of the product without the reinforcement block, the dielectric constant is less than or equal to 8, and the dielectric loss is ≤0.005.
[0012] Preferably, two adjacent coil layers are connected to each other via conductive through holes, and multiple coil layers are connected to each other to form an internal coil, and both ends of the internal coil are respectively connected to the first external electrode and the second external electrode.
[0013] The utility model adopts the structure, has the advantages of small space occupation and easy processing.
[0014] Preferably, the reinforcement block also includes a fourth reinforcement block, a fifth reinforcement block and a sixth reinforcement block, the fourth reinforcement block is located above the fifth reinforcement block, the fifth reinforcement block is located above the first external electrode and the second external electrode, and the sixth reinforcement block is connected to the first external electrode and the second external electrode, respectively.
[0015] The utility model adopts the above structure, and the upper and lower surfaces of the utility model can play a protective role.
[0016] Preferably, the dielectric constant of the reinforcing block @15GHz≤8. Dielectric loss @15GHztanσ≤5×10 -4 .
[0017] The beneficial effects of the utility model are: 1. The parasitic capacitance of the utility model is small and the Q value is large; 2. The structure of the utility model is stable and easy to process; 3. The utility model is not easy to be damaged during the detection process. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 A structural schematic diagram of Example 1;
[0019] Figure 2 A structural schematic diagram of Example 2;
[0020] Figure 3 Schematic diagram of the stacking of Example 1
[0021] Figure 4 is a top view of Example 1;
[0022] Figure 5 This is a top view of Example 2. DETAILED DESCRIPTION
[0023] The utility model is further explained below in conjunction with specific implementation cases.
[0024] Example 1
[0025] A miniature chip inductor comprises a marking layer 1, an upper substrate insulating layer 2, a lower substrate insulating layer 3, several layers of internal coil insulating layers 4, and an external electrode 7. The external electrode 7 comprises a first external electrode 5 and a second external electrode 6. The internal coil insulating layer 4 is located between the upper substrate insulating layer 2 and the lower substrate insulating layer 3. The two ends of the first external electrode 5 and the second external electrode 6 are connected to the lower substrate insulating layer 3 and the upper substrate insulating layer 2, respectively. The cross section of the external electrode 7 is L-shaped. A reinforcing block 8 is provided at the bottom of the lower substrate insulating layer 3. The marking layer 1 comprises a first marking layer 12 and a second marking layer 13. The first marking layer 12 is provided above the upper substrate insulating layer 2, and the second marking layer 13 is provided below the lower substrate insulating layer 3. The reinforcing block 8 comprises a first reinforcing block 81, a second reinforcing block 82, and a third reinforcing block 83. The first reinforcing block 81 is located below the second reinforcing block 82. The second reinforcing block 82 is located below the first external electrode 5 and the second external electrode 6. The third reinforcing block 83 is connected to the first external electrode 5 and the second external electrode 6, respectively. The internal coil insulation layer 4 includes a first internal coil insulation layer 14 and a second internal coil insulation layer 15, the first internal coil insulation layer 14 and the second internal coil insulation layer 15 are arranged alternately, the first internal coil insulation layer 14 is provided with a coil layer 9, and the second internal coil insulation layer 15 is provided with a conductive through hole 10. Two adjacent coil layers 9 are connected to each other through the conductive through hole 10, and multiple layers of coil layers 9 are connected to each other to form an internal coil 11, and the two ends of the internal coil 11 are respectively connected to the first external electrode 5 and the second external electrode 6. The reinforcing block 8 also includes a fourth reinforcing block 84, a fifth reinforcing block 85 and a sixth reinforcing block 86, the fourth reinforcing block 84 is located above the fifth reinforcing block 85, the fifth reinforcing block 85 is located above the first external electrode 5 and the second external electrode 6, and the sixth reinforcing block 86 is respectively connected to the first external electrode 5 and the second external electrode 6. The dielectric constant of the reinforcing block 8 @15GHz≤8. Dielectric loss @15GHztanσ≤5×10 -4 .
[0026] First, the utility model adopts an L-shaped external electrode 7, which is different from the full-terminal product form, so that the parasitic capacitance is greatly reduced and the Q value is greatly improved. However, since the L-shaped external electrode 7 cannot wrap the entire product, during the detection process, the metal probe is easy to penetrate the ceramic layer and cause product damage. Therefore, the utility model adopts a reinforcing block 8 structure to play a protective role and prevent the utility model from being damaged during the detection process.
[0027] Under the same sintering conditions, the material strength of the product with the reinforcement block 8 is at least 1.5 times higher than that without the reinforcement block 8, the dielectric constant is less than or equal to 8, and the dielectric loss is ≤0.005.
[0028] Example 2
[0029] A miniature chip inductor comprises a marking layer 1, an upper substrate insulating layer 2, a lower substrate insulating layer 3, a plurality of layers of internal coil insulating layers 4, a first external electrode 5 and a second external electrode 6, wherein the internal coil insulating layer 4 is located between the upper substrate insulating layer 2 and the lower substrate insulating layer 3, the two ends of the first external electrode 5 and the second external electrode 6 are connected to the lower substrate insulating layer 3 and the upper substrate insulating layer 2 respectively, the cross section of the external electrode 7 is L-shaped, and a reinforcing block 8 is provided at the bottom of the lower substrate insulating layer 3. The marking layer 1 comprises a first marking layer 12 and a second marking layer 13, the first marking layer 12 is provided above the upper substrate insulating layer 2, and the second marking layer 13 is provided below the lower substrate insulating layer 3. The reinforcing block 8 comprises a first reinforcing block 81, a second reinforcing block 82 and a third reinforcing block 83, wherein the first reinforcing block 81 is located below the second reinforcing block 82, the second reinforcing block 82 is located below the first external electrode 5 and the second external electrode 6, and the third reinforcing block 83 is connected to the first external electrode 5 and the second external electrode 6 respectively. The reinforcing block 8 further includes a fourth reinforcing block 84, a fifth reinforcing block 85 and a sixth reinforcing block 86. The fourth reinforcing block 84 is located above the fifth reinforcing block 85. The fifth reinforcing block 85 is located above the first external electrode 5 and the second external electrode 6. The sixth reinforcing block 86 is connected to the first external electrode 5 and the second external electrode 6, respectively. The dielectric constant of the reinforcing block 8 @ 15 GHz is ≤ 8. The dielectric loss @ 15 GHz is tanσ ≤ 5×10 -4 .
[0030] The material strength of the product with the reinforcement block 8 added in this embodiment is at least 1.5 times higher than that without the reinforcement block 8 added, the dielectric constant is less than or equal to 8, and the dielectric loss is ≤0.005.
[0031] Example 1 and Example 2 were tested with reference to GB / T 6569-2006 fine ceramic bending strength test method.
[0032] The comparative solution is the technical solution of Example 1 without the reinforcement block 8 installed.
[0033] The following are the test results of the utility model:
[0034]
Claims
1. A miniature chip inductor, Features: It includes a marking layer, an upper substrate insulating layer, a lower substrate insulating layer, several layers of internal coil insulating layers, and external electrodes. The external electrodes include a first external electrode and a second external electrode. The internal coil insulating layer is located between the upper substrate insulating layer and the lower substrate insulating layer. Both ends of the first external electrode and the second external electrode are respectively connected to the lower substrate insulating layer and the upper substrate insulating layer. The cross-section of the external electrode is L-shaped. A reinforcing block is provided at the bottom of the lower substrate insulating layer.
2. The microchip inductor according to claim 1, Features: The identification layer comprises a first identification layer and a second identification layer. The first identification layer is arranged above the upper substrate insulation layer, and the second identification layer is arranged below the lower substrate insulation layer.
3. The microchip inductor according to claim 2, Features: The reinforcement block includes a first reinforcement block, a second reinforcement block and a third reinforcement block, the first reinforcement block is located below the second reinforcement block, the second reinforcement block is located below the first external electrode and the second external electrode, and the third reinforcement block is connected to the first external electrode and the second external electrode respectively.
4. The micro-chip inductor according to claim 3, Features: The internal coil insulation layer includes a first internal coil insulation layer and a second internal coil insulation layer, the first internal coil insulation layer and the second internal coil insulation layer are alternately arranged, a coil layer is arranged on the first internal coil insulation layer, and a conductive through hole is arranged on the second internal coil insulation layer.
5. The microchip inductor according to claim 4, Features: Two adjacent coil layers are connected to each other through conductive through holes, and multiple coil layers are connected to each other to form an internal coil, and two ends of the internal coil are respectively connected to the first external electrode and the second external electrode.
6. A miniature chip inductor according to claim 3 or 5, Features: The reinforcement block also includes a fourth reinforcement block, a fifth reinforcement block and a sixth reinforcement block, the fourth reinforcement block is located above the fifth reinforcement block, the fifth reinforcement block is located above the first external electrode and the second external electrode, and the sixth reinforcement block is connected to the first external electrode and the second external electrode respectively.
7. The micro-chip inductor according to claim 6, Features: The dielectric constant of the reinforcement block is ≤8 @15GHz; the dielectric loss @15GHztanσ is ≤5×10 -4 .