High-reliability high-voltage GPP chip
By using a method that does not deepen the etching depth in the high-voltage GPP chip, a composite trench structure is formed, which solves the difficulties of traditional chips in improving voltage and reliability, and achieves the effects of voltage improvement and reliability enhancement.
Patent Information
- Application Number
- CN202420232439.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-31
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2034-01-31
AI Technical Summary
Traditional high-voltage GPP chips have difficulties in improving voltage and reliability, such as fragmentation caused by too deep trench depth, difficulty in achieving resistivity improvement, hidden cracks damaging the PN junction during cutting, and double-groove process reducing the effective area.
Using a method that does not deepen the etching depth, the arc-shaped components are connected in sequence from the P+ layer to the N layer, and the glass layer and Sipos film are wrapped on them. Three photolithography and two etchings are combined to form a composite trench structure to improve voltage and reliability. sex.
It effectively improves the voltage and reliability of the chip, increases the electric field width and mechanical stress resistance of the scribing track, reduces the risk of failure, and avoids the reduction of the effective area.
Smart Images

Figure CN221805435U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of semiconductors, in particular to a high-reliability and high-voltage GPP chip. Background Art
[0002] At present, the market has higher and higher requirements for the voltage and reliability of table semiconductor power device chips. The traditional methods for increasing voltage are generally:
[0003] 1) Deepening the groove depth can improve the product's pressure resistance, but too deep a groove can easily lead to fragmentation, which invisibly increases the failure cost;
[0004] 2) Select original wafers with higher resistivity for production. Since the production process requirements for high-resistivity original wafers are high, it is difficult for manufacturers to supply them. In addition, increasing the resistivity will lead to poor reverse capability of the product, increasing the risk of reliability failure.
[0005] In addition, this type of high-voltage chip generally uses the GPP passivation process. Since the bottom of the groove is close to the PN junction, it is easy for the cutting knife to hit the silicon when cutting the groove, causing hidden cracks and damaging the PN junction, resulting in product voltage attenuation and reliability failure. Traditional processes generally use the double-groove method (cutting the silicon between adjacent grooves) to avoid this problem, but the double-groove process will reduce the effective area of the chip, thereby reducing the surge capacity of the product. Utility Model Content
[0006] In view of the above problems, the utility model provides a high-reliability high-voltage GPP chip which does not increase the etching depth and improves the chip voltage and yield.
[0007] The technical solution of the utility model is:
[0008] High reliability high voltage GPP chip, including the lower metal layer, N + Layer, N layer, P + layer and upper metal layer;
[0009] The P + The edge of the layer is provided with an arc-shaped portion 1 extending downward;
[0010] An arc-shaped portion 2 is provided below the arc-shaped portion 1 and is connected thereto and extends downward to the Nth layer;
[0011] An arc-shaped portion 3 is provided below the arc-shaped portion 2 and is connected thereto and extends downward;
[0012] The P + A glass layer is provided on the top surface of the layer, which extends downward and wraps around the first arc portion, the second arc portion and the third arc portion.
[0013] Specifically, a Sipos film is provided between the glass layer and the connecting parts of the arc-shaped part 1, the arc-shaped part 2 and the arc-shaped part 3;
[0014] An LTO film is provided on the surface of the glass layer.
[0015] Specifically, the glass layer is from P + The top surface of the layer extends downward.
[0016] Specifically, the vertical height of the arc-shaped portion extending downward is half of the P+ junction depth.
[0017] Specifically, the second arc-shaped portion extends downward to the N layer.
[0018] Specifically, the arc portion three is located at the outer edge of the N layer.
[0019] Specifically, the upper and lower metal layers are Ni—Au layers respectively.
[0020] The vertical height of the arc portion 1 extending downward of the utility model is half of the depth of the P+ layer junction. This part can extend the electric field width of the P+ region, thereby increasing the voltage. Generally, the voltage can be increased by 100-200V; the arc portion 3 is located at the outer edge of the N layer. This part can increase the electric field widening distance between the dicing track and the N region, making the electric field widening area of the N region less affected by the mechanical stress of dicing, thereby improving the chip reliability; three photolithography and two etchings are performed to form the required groove morphology, thereby improving the voltage and product reliability. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 is a schematic diagram of the diffusion structure of step S100,
[0022] Figure 2 This is a schematic diagram of the structure of one-step photolithography + oxide film etching in step S200.
[0023] Figure 3 is a schematic diagram of a groove etching structure in step S300.
[0024] Figure 4 is a schematic diagram of the secondary photolithography structure in step S400,
[0025] Figure 5 is a schematic diagram of the secondary trench etching structure in step S500,
[0026] Figure 6 is a schematic diagram of the diffusion structure of step S100,
[0027] Figure 7 is a schematic diagram of the diffusion structure of step S100,
[0028] Figure 8 is a schematic diagram of the diffusion structure of step S100,
[0029] In the figure, 100 is the upper metal layer, 200 is the Sipos film, 300 is the glass layer, and 400 is the LTO film. DETAILED DESCRIPTION
[0030] The embodiments of the present invention are described in detail below, and examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.
[0031] Reference below Figure 1-8 Describe the embodiments of the utility model;
[0032] A method for preparing a high-voltage GPP chip with a composite groove comprises the following steps:
[0033] Step S100: Diffusion
[0034] Referring to Figure 1, a layer of phosphorus and boron is deposited on the surface of the silicon wafer to form P + —N—N + Structure, and grow a 2um thick silicon dioxide oxide film on both the upper and lower surfaces (the oxide layer in the figure);
[0035] Step S200: Photolithography and oxide film etching
[0036] Reference Figure 2 As shown, after the wafer is double-sidedly spin-coated with photoresist, the surface area of the P+ region is formed into grains, and the area to be etched is exposed on the surface of the grains. The mask is grooved with 12 mils, and the other areas are protected with photoresist. BOE etching acid is used to remove the oxide film to expose the silicon surface to be etched;
[0037] Step S300: first trench etching
[0038] Reference Figure 3 As shown, the exposed silicon is etched for the first time using KOH etching solution to form an arc-shaped groove 1;
[0039] The corrosion depth-to-width ratio is 1:1, and the corrosion depth condition is selected according to the diffusion structure of the product;
[0040] For example, the P+ junction depth of a 1200V rectifier chip is about 100um, so the total etching depth needs to be about 130-140um. The first KOH etching depth is 50% of the junction depth, about 50um. The mask slot is 12mil, the etching width is about 400um, and the bottom step width is about 360um.
[0041] The P+ junction depth of the 400V rectifier chip is about 60um, so the total etching depth needs to be about 90-100um. The first KOH etching depth is 50% of the junction depth, about 30um. The mask groove is 12mil, the etching width is about 360um, and the bottom step width is about 320um.
[0042] Step S400: secondary photolithography
[0043] Reference Figure 4 As shown, after the wafer is double-sidedly spin-coated with photoresist, the second etching area is photoetched at the bottom of the groove formed by the first etching, the mask is grooved with 5 mil, and the other areas are protected with photoresist;
[0044] Step S500: secondary trench etching
[0045] Reference Figure 5 As shown, a mixed acid is used to etch the etched silicon for a second time, and the etching depth needs to be etched to the depth of the P+ junction, to form an arc-shaped groove 2;
[0046] Through the actual depth and width design of the product, the depth-to-width ratio of the remaining silicon structure to be removed is calculated, and the operating conditions are selected according to the actual depth-to-width ratio requirements; for example, after the first KOH etching of the 1200V rectifier chip, the bottom step width is about 360um, and the second mixed acid etching width is about 50% of the bottom step width, that is, about 180um. The mask groove is 5mil (125um), that is, the depth to be etched is 50um, and the etching width on one side is (180-127) / 2=26.5um, that is, the etching depth-to-width ratio is 50 / 26.5=1.89.
[0047] Step S600, three-time photolithography
[0048] Reference Figure 6 As shown, after the wafer is double-sidedly spin-coated with photoresist, the area to be etched is photoetched three times at the bottom of the groove formed by the first and second etchings, the mask is grooved 8mil, and the other areas are protected with photoresist;
[0049] Step S700, three-time trench etching
[0050] The etched silicon is etched for the third time using mixed acid, and the etching depth is 30-40um below the P+ junction depth to form an arc-shaped groove three;
[0051] Through the actual depth and width design of the product, the depth and width ratio of the remaining silicon structure to be removed is calculated, and the operating conditions are selected according to the actual depth and width ratio requirements; for example, after the first KOH etching of the 1200V rectifier chip, the bottom step width is about 360um, the second mixed acid etching width is about 50% of the bottom step width, that is, about 180um, and the third mixed acid etching width is about 320um (KOU etching reserves a 20um width for the bottom step). The photolithography board is grooved 8mil (203um), that is, the depth to be etched is 40um, and the etching width on one side is (320-203) / 2=58.5um, that is, the etching depth and width ratio is 40 / 58.5=0.68.
[0052] Step S800, through the normal SIPOS-glass sintering-LTO-three yellow light-nickel gold plating process, the preparation is completed by segmentation. Figure 8 The product shown. Figure 1-7 This is a schematic diagram, in which only half of the chip is drawn. The two chips share one groove. After processing, they are cut from the middle of the groove.
[0053] It is further defined that the KOH etching solution in step S300 includes:
[0054] A 50% (wt) KOH solution is fully stirred in 8% (wt) IPA (isopropyl alcohol) to prepare a KOH etching solution;
[0055] It is further defined that the etching depth in step S300 is about 50% of the P+ junction depth.
[0056] It is further defined that in step S300, the temperature of the etching solution is 80-90° C., the etching rate is 5-8 um / min, and the etching time is 6.5-10 min.
[0057] It is further defined that the acid mixture in step S500 includes:
[0058] Composition and concentration: nitric acid 39.68%, glacial acetic acid 19.96%, hydrofluoric acid 11.44%
[0059] It is further defined that in step S500, the temperature of the etching solution is 0°C to 2°C, the etching rate is 15-18um / min, and the etching time is 100-200S.
[0060] It is further defined that the etching depth in step S500 is about 50% of the P+ junction depth.
[0061] It is further defined that in step S700, the temperature of the etching solution is: -5°C~-3°C, the etching rate is 6-8um / min, and the etching time is: 200-400S.
[0062] It is further defined that the etching depth in step S700 is 50% of the junction depth + 30-40 um.
[0063] A high-voltage GPP chip with a composite groove includes a lower metal layer, an N + Layer, N layer, P + layer and an upper metal layer 100;
[0064] The P + The edge of the layer is provided with an arc-shaped portion 1 extending downward, which is a part of the arc-shaped groove 1;
[0065] The arc-shaped portion 1 is provided below the arc-shaped portion 1 and connected thereto and extending downward to the N layer, which is a part of the arc-shaped groove 2;
[0066] An arc-shaped portion 3 is provided below the arc-shaped portion 2 and is connected thereto and extends downward, which is a part of the arc-shaped groove 3;
[0067] The P + The top surface of the layer is provided with a glass layer 300 (or referred to as Glass) extending downward and wrapping around the arc portion 1, the arc portion 2 and the arc portion 3;
[0068] A Sipos film 200 is provided between the glass layer 300 and the connecting parts of the arc portion 1, the arc portion 2 and the arc portion 3; the full name of the Sipos film 200 is oxygen-doped semi-insulating polycrystalline silicon, which is a commonly used passivation layer for semiconductor devices, especially some high-voltage devices. It can not only improve the reverse breakdown voltage of the device, but also greatly improve the reliability of the device.
[0069] The surface of the glass layer 300 is provided with an LTO film 400. The LTO film 400 is a silicon dioxide film, which is a common passivation layer for isolating glass from packaging solder, and protects the glass layer 300 from being damaged by solder.
[0070] Further defined, the glass layer 300 is formed from P + The top surface of the layer extends downward.
[0071] It is further defined that the vertical height of the arc-shaped portion extending downward is half of the P+ junction depth.
[0072] It is further defined that the second arc-shaped portion extends downward to the Nth layer.
[0073] It is further defined that the arc portion is located at the outer edge of the N layer.
[0074] It is further defined that the upper and lower metal layers are Ni—Au layers respectively.
[0075] Regarding the contents disclosed in this case, there are a few points that need to be explained:
[0076] (1) The drawings of the embodiments disclosed in this case only involve the structures involved in the embodiments disclosed in this case. Other structures can refer to the general design;
[0077] (2) In the absence of conflict, the embodiments and features of the embodiments disclosed in this case may be combined with each other to obtain new embodiments;
[0078] The above are only specific implementation methods disclosed in this case, but the protection scope of the present disclosure is not limited thereto. The protection scope disclosed in this case should be based on the protection scope of the claims.
Claims
1. High reliability and high voltage GPP chip, It is characterized in that Including the lower metal layer, N + Layer, N layer, P + layer and upper metal layer; The P + The edge of the layer is provided with an arc-shaped portion 1 extending downward; An arc-shaped portion 2 is provided below the arc-shaped portion 1 and is connected thereto and extends downward to the Nth layer; An arc-shaped portion 3 is provided below the arc-shaped portion 2 and is connected thereto and extends downward; The P + A glass layer is provided on the top surface of the layer, which extends downward and wraps around the first arc portion, the second arc portion and the third arc portion.
2. The high reliability and high voltage GPP chip according to claim 1, It is characterized in that A Sipos film is provided between the glass layer and the connecting parts of the arc-shaped part 1, the arc-shaped part 2 and the arc-shaped part 3; An LTO film is provided on the surface of the glass layer.
3. The high reliability and high voltage GPP chip according to claim 1, It is characterized in that The glass layer is from P + The top surface of the layer extends downward.
4. The high reliability and high voltage GPP chip according to claim 1, It is characterized in that The vertical height of the arc portion extending downward is half of the depth of the P+ junction.
5. The high reliability and high voltage GPP chip according to claim 1, It is characterized in that The second arc portion extends downward to the N layer.
6. The high reliability and high voltage GPP chip according to claim 1, It is characterized in that The arc portion three is located at the outer edge of the N layer.
7. The high reliability and high voltage GPP chip according to claim 1, It is characterized in that The upper and lower metal layers are Ni—Au layers respectively.