Welding die
By designing a welding mold with a positioning plane and a limiting column, the problem of welding accuracy caused by the increase in the number of pins on the ceramic package base is solved, positional stability and accuracy during the welding process are achieved, and the problem of collision or solder deflection is avoided. Contact errors caused by shifting.
Patent Information
- Application Number
- CN202420289841.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-08
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2034-02-08
AI Technical Summary
During the chip packaging process, the increase in the number of pins of the ceramic packaging base leads to an increase in solder points. It is easy for the contact between the leads and the electrodes to deviate due to small collisions or solder melting, which affects the use of the product. Especially under the trend of miniaturization, it is difficult to achieve high accuracy. of welding.
Design a welding mold, including a carrier and a pressure block. The carrier is equipped with a positioning plane and a limiting column to fix the position of the package base through the cavity. The pressure block presses the leads and solder against the electrode on the welding side to limit the position. The posts limit the movement of the clamp, ensuring a stable hold of the leads and solder.
It effectively avoids the positional shift of the package base during the welding process, ensures that the leads and solder are accurately fixed on the welding side of the package base, improves welding accuracy and stability, and prevents position changes caused by external collisions.
Smart Images

Figure CN221809004U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of microelectronic device manufacturing, in particular to a welding mold. Background Art
[0002] During the application of chips, a shell is often required to protect them. Ceramic package base is one of the common packaging methods. At the same time, in order to ensure high utilization of chip packaging and stable operation on the circuit board, it is often necessary to weld metal leads on the electrodes of the ceramic package base to achieve internal and external conduction of the circuit. With the update and iteration of chips, the number of lead-in / lead-out terminals on the package base is increasing. The increase in the number of pins means that the number of welding points that need to be paid attention to is further increased. Minor collisions during assembly and movement of devices and melting of solder during welding may cause the contact between the lead and the electrode to shift, affecting the use of the product. In particular, the miniaturization trend of ceramic package bases makes this problem more obvious. This also poses a higher challenge to lead welding. Without reasonable fixing means, it is difficult to achieve high-precision welding. Utility Model Content
[0003] The technical problem to be solved by the utility model is: how to ensure the stability of the position of the product, lead and solder during the welding process. In order to solve the above technical problem, the utility model provides a welding mold, including a carrier and a pressing block, the carrier is provided with a positioning plane, the positioning plane is recessed to form a cavity for accommodating a limited package base, the carrier is provided with a limiting column, the limiting column forms a limited space, which is used to limit the movement of the pressing block in the extension direction of the positioning plane, the pressing block cooperates with the carrier by inserting the limiting space, and the pressing block is used to push the lead and solder against the electrode to be welded on the welding side of the package base; the positioning plane is provided with at least one limiting protrusion on the peripheral side of the cavity, and the limiting protrusion is used to limit the movement of the lead along the extension direction of the positioning plane. The distance between the limiting protrusion and the lead is controlled within 25μm to 50μm, and the limiting protrusion has a rounded corner.
[0004] Wherein, the extending direction of the positioning plane includes a first direction and a second direction which are perpendicular to each other.
[0005] Preferably, when the cavity accommodates the position-limiting packaging base, the dimensional tolerance between the length and width of the cavity and the length and width of the packaging base is 150 μm to 200 μm.
[0006] Preferably, the cavity includes a first cavity and a second cavity, the first cavity is formed by a depression of the positioning plane and matches the size of the packaging base, the second cavity is arranged on both sides of the first cavity along the second direction, and the depth of the second cavity is less than the depth of the first cavity.
[0007] Preferably, in the first direction, the length of the second cavity is smaller than the length of the first cavity, and both ends of the second cavity protrude toward the middle to form limiting portions relative to both ends of the first cavity.
[0008] Preferably, the side of the pressing block facing the cavity is provided with a protrusion corresponding to the welding side of the package base in the cavity, and the protrusion is used to press the lead and the solder against the electrode to be welded on the welding side of the package base.
[0009] Preferably, the depth of the cavity is h2, the distance between the side surface of the carrier opposite to the positioning plane and the bottom surface of the cavity is h1, and the range of h2 / h1 is 2 to 10.
[0010] Preferably, the carrier and the pressing block are both made of graphite, and the surfaces of the carrier and the pressing block are coated with silicon carbide coating.
[0011] Compared with the prior art, the welding mold provided in the embodiment of the utility model has the following beneficial effects:
[0012] The position of the package base is fixed by the cavity to prevent the position of the package base from shifting due to external factors such as collision during welding, and then a load is applied to the leads and solder through the pressing block, so that the leads and solder are fixed on the welding side of the package base to prevent the leads and solder from shifting relative to the package base due to collision. The limiting column can limit the position of the pressing block on the carrier to prevent the position of the pressing block from changing along the extension direction of the positioning plane, so that the pressing block can accurately and stably fix the leads and solder on the welding side of the package base, further avoiding the change and shift of the relative position between the leads, solder and package base caused by external collision. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 It is a schematic diagram of the installation of the welding mold, the packaging base, the lead wire and the solder of the utility model;
[0014] Figure 2 It is a three-dimensional view of the vehicle of the utility model;
[0015] Figure 3 It is a three-dimensional view of the pressing block of the utility model;
[0016] Figure 4 It is a three-dimensional diagram of the welding mold of the utility model;
[0017] Figure 5 It is a schematic diagram of the installation of the welding mold, the packaging base, the lead wire, and the solder when the pressing block is not placed in the utility model;
[0018] Figure 6 yes Figure 1 a top view of the illustrated embodiment;
[0019] Figure 7 yes Figure 7 Cross-sectional view at AA in the middle.
[0020] In the figure: 1, carrier; 11, cavity; 111, first cavity; 1111, limiting portion; 112, second cavity; 12, limiting column; 121, limiting space; 1211, limiting groove; 13, limiting protrusion; 14, positioning plane;
[0021] 2. briquetting; 21. protrusion;
[0022] 3. Lead wire;
[0023] 4. Solder;
[0024] 5. Package base. DETAILED DESCRIPTION
[0025] The following is a further detailed description of the specific implementation of the present invention in conjunction with the accompanying drawings and examples. The following examples are used to illustrate the present invention, but are not intended to limit the scope of the present invention.
[0026] like Figure 1 , Figure 3 and Figure 5 As shown, the preferred embodiment of the utility model provides a welding mold, which includes a carrier 1 and a pressing block 2. The carrier 1 is provided with a positioning plane 14, and the positioning plane 14 is recessed to form a cavity 11 for accommodating a limited packaging base 5. The carrier 1 is also provided with a limiting column 12, and the limiting column 12 forms a limited space 121 for limiting the movement of the pressing block 2 in the extension direction of the positioning plane. The pressing block 2 cooperates with the carrier 1 by inserting into the limiting space 121. The pressing block 2 is used to press the lead 3 and the solder 4 against the electrode to be welded on the welding side of the packaging base; wherein the extension direction of the positioning plane 14 includes a first direction B and a second direction C that are perpendicular to each other. It should be noted that Figure 6 The top view in the figure indicates that direction B is the first direction, direction C is the second direction, when the package base 5 is placed in the cavity 11, its welding edge faces the second direction, the solder 4 is arranged parallel to the first direction, and the lead 3 is arranged parallel to the second direction.
[0027] Specifically, during the brazing process, the position accuracy of the accessories will affect the welding quality of the finished product. When the position of the solder 4 is offset, the solder 4 may not spread properly after melting at high temperature, and the solder 4 may not be able to wet the electrode. When the position of the lead 3 is offset, it may cause the lead 3 to deform and warp during the melting process. The deformation and warping of the lead 3 will cause the connection between the lead 3 and the device to deviate, causing problems in the subsequent use of the device. During the transfer process and the brazing process, slight external collisions and other influences may cause the position of the lead 3 and solder 4, which have been placed correctly, to change and shift, resulting in the above problems. Before welding, the utility model first limits the position of the packaging base 5 through the cavity 11 on the carrier 1, so that the position of the packaging base 5 relative to the carrier 1 will not change during the transfer and welding process, and then fixes the lead 3 and the solder 4 to the packaging base 5 through the pressing block 2, and limits the movement of the pressing block 2 on the positioning plane 14 through the limiting column 12, so that the position of the pressing block 2 relative to the packaging base 5 will not change, thereby ensuring that during the transfer and welding process, the position of the lead 3 and the solder 4 relative to the packaging base 5 will not change or deviate, and the lead 3 and the solder 4 can also be firmly fixed on the welding side of the packaging base 5, ensuring the stability of the position of the packaging base 5, the lead 3 and the solder 4 during the welding process and the accuracy of the relative position, wherein the limiting column 12 can be set on the positioning plane 14, and can also be set on the side of the carrier 1, as long as it can meet the limit of the pressing block 2 and avoid the movement of the pressing block 2 on the positioning plane 14. In addition, the present solution reasonably designs the size of the pressing block 2 so that the pressing block 2 on the welding mold after assembly is slightly higher than the pressing block limiting column 12, so that it is convenient to continue to add other loads above the pressing block 2. If not, the load will be applied to the limiting column 12, and the effect of applying the load will not be achieved.
[0028] like Figure 1 , Figure 5 and Figure 6 As shown, in some embodiments, at least one limiting column 12 is disposed on both sides of the cavity 11 along the first direction.
[0029] Specifically, the setting of the limiting column 12 should be based on the ability to limit the movement of the pressure block 2 along the direction extending along the positioning plane 14. In the present embodiment, two limiting columns 12 are provided, and a limited space 121 is formed between the two limiting columns 12 to limit the movement of the pressure block. In some other embodiments, the limiting columns 12 can be provided in three or four numbers and respectively limit the corners of the pressure block 2, thereby limiting the movement of the pressure block 2. In some other embodiments, the limiting columns 12 can also be two diagonally arranged numbers, and the positions of the two corners of the pressure block 2 are limited to limit the movement of the entire pressure block 2.
[0030] In some embodiments, such as Figure 2 As shown, a limiting groove 1211 which fits with the corner of the pressing block is provided on one side of the limiting column 12 facing the cavity 11. The limiting groove 1211 extends in a direction away from the positioning plane 14 and passes through the limiting column 12 to form an embedding opening. A limiting space 121 is formed between the limiting grooves 1211 provided on the limiting columns 12 on both sides of the cavity 11. Both ends of the pressing block 2 can be embedded in the limiting space 121 through the embedding opening.
[0031] Among them, the shape of the limiting groove 1211 fits with the shape of the corner of the pressing block 2, which can better limit the movement of the pressing block 2. For example, in another embodiment, when the corner of the pressing block 2 is set as a rounded corner, the limiting groove 1211 can be set as an arc structure that fits the rounded corner. The corner of the pressing block 2 corresponds to the limiting groove 1211, and then the pressing block 2 is embedded in the limiting space 121 through the embedding port and the lead 3 and the solder 4 are pressed against the electrode to be welded on the welding side of the package base 5.
[0032] In some embodiments, the dimensional tolerance between the length and width of the cavity 11 and the length and width of the package base 5 is 150 μm to 200 μm. By controlling the dimensional tolerance, it is ensured that the package base 5 and the cavity 11 have good contact and accurate relative position, and it is also convenient to remove the package base 5 after welding, avoiding the problem that the package base 5 cannot be removed from the cavity 11 after welding the lead 3 due to thermal expansion during the brazing process.
[0033] like Figure 2 As shown, in some embodiments, the cavity 11 includes a first cavity 111 and a second cavity 112. The first cavity 111 is formed by a depression of the positioning plane 14 and matches the size of the packaging base 5. The second cavity 112 is arranged on both sides of the first cavity 111 along the second direction, and the depth of the second cavity 112 is less than the depth of the first cavity 111.
[0034] Furthermore, in some embodiments, in the first direction, the length of the second cavity 112 is smaller than the length of the first cavity 111 , and both ends of the second cavity 112 protrude toward the middle to form limiting portions 1111 relative to both ends of the first cavity 111 .
[0035] Specifically, the first cavity 111 with a deeper depth is used to accommodate the limited package base 5, while the second cavity 112 with a smaller depth can adapt to the lead 3 with a bent structure, so that the lead 3 can avoid contact with the carrier 1 and can better contact with the electrode to be welded on the package base 5 for welding. In the first direction, the length of the second cavity 112 is less than the length of the first cavity 111, which can prevent the solder 4 in the first cavity 111 from moving toward the side of the first cavity 111 and leaving the package base 5. The movement of the solder 4 in the horizontal direction is limited to the package base 5, and the lead 3 can be better welded to the package base 5.
[0036] like Figure 3 As shown, in some embodiments, the side of the pressing block 2 facing the cavity 11 is provided with a protrusion 21 corresponding to the welding side of the package base 5 in the cavity 11, and the protrusion 21 is used to press the lead 3 and the solder 4 against the electrode to be welded on the welding side of the package base 5.
[0037] Specifically, the protrusion 21 can more tightly fix the lead 3 and the solder 4 on the package base 5, while also avoiding the influence of the pressure block 2 on the middle part of the package base 5. It can also increase the load applied by the pressure block 2 to the lead 3 and the solder 4 by reducing the contact area, so that the lead 3 and the solder 4 can be pressed more tightly on the package base 5, and the lead 3 and the solder 4 are fixed more securely. The load applied by the pressure block 2 can also be evenly applied to the contact points between each lead 3 and the solder 4 and the package base 5, avoiding the problem of uneven pressure.
[0038] In some embodiments, the protrusion 21 is a strip-shaped protrusion extending along the first direction. The strip-shaped protrusion corresponds to the shape of the welding side of the package base 5, and its length does not exceed the length of the first cavity 111 in the first direction. The protrusion 21 can extend into the first cavity 111 and better apply pressure to the lead 3, so that the multiple leads 3 and the solder 4 are better fixed on the electrodes on the welding side of the package base 5, and the force on the leads 3 and the solder 4 will be more uniform.
[0039] In some embodiments, in the second direction, the width of the pressing block 2 is smaller than the width of the package base 5 and the first cavity 111. By setting it in this way, a gap can be exposed for observing the relative positions of the assembled leads 3, solder 4 and package base 5, so as to adjust the position of the offset leads 3 or solder 4 in time and ensure the accuracy during the welding process.
[0040] In some embodiments, the pressure applied by the pressing block 2 to the lead 3 is controlled within a range of 1 kPa to 8 kPa. By setting the pressure, the lead 3 can be well fixed. When the pressure is too high, the lead 3 will be deformed by pressure, while when the pressure is too low, the lead 3 will not be pressed in place and will be easy to loosen, resulting in the problem of the lead 3 being offset or warping.
[0041] like Figure 1 , Figure 2 , Figure 4 and Figure 5 As shown, in some embodiments, the positioning plane 14 is provided with at least one limiting protrusion 13 on the peripheral side of the cavity 11 along the second direction, and the limiting protrusion 13 is used to limit the movement of the lead 3 along the extending direction of the positioning plane 14 .
[0042] Specifically, according to the number of pins that need to be welded on the package base 5, multiple leads 3 are provided, and the ends of the multiple leads 3 away from the welding side of the package base 5 can be connected together to form a lead group, and the limiting protrusion 13 on the positioning plane 14 can cooperate with the lead group by embedding into the gap between the leads 3, thereby limiting the position of the leads 3 and the lead group on the positioning plane 14 to prevent the leads 3 from moving; the limiting protrusion 13 on the positioning plane 14 can be provided in multiples according to the number of leads 3 to better limit the movement of the leads 3. In one embodiment, four limiting protrusions 13 are symmetrically provided on the positioning plane 14, and the four limiting protrusions 13 are respectively provided at the four corners of the lead group to limit the position of the lead group and the leads 3. In addition, a triangular protrusion is additionally provided, and the triangular protrusion cooperates with one of the limiting protrusions 13 and is respectively provided on the inner and outer sides of the lead group to further limit the movement of the lead group and each lead 3.
[0043] Furthermore, the distance between the limiting protrusion 13 and the lead 3 is controlled within 25μm to 50μm, and the limiting protrusion 13 is rounded to form a rounded corner. The setting of the distance between the limiting protrusion 13 and the lead 3 and the rounding of the limiting protrusion 13 are both to ensure that the limiting protrusion 13 can limit the lead 3 while not affecting the removal of the lead 3 after welding due to thermal expansion during the soldering process. When multiple leads 3 form a lead group, the setting of the fillet only needs to set a fillet on a corner of the limiting protrusion 13 close to the corner of the lead group so that the lead group can be easily removed after welding, simplifying the processing procedures of the carrier.
[0044] In addition, see Figure 7 The main body of the lead 3 to be welded does not contact the outer plane of the cavity 11, but is higher by a certain distance. Because the melting of the solder 4 during brazing will cause the height of the lead 3 to drop, if the height drop causes the main body of the lead 3 to contact the outer plane of the cavity 11, it will affect the contact between the pin and the electrode to be welded.
[0045] See also Figure 7 In some embodiments, the depth of the cavity 11 is h2, the distance between the side surface of the carrier 1 opposite to the positioning plane 14 and the bottom surface of the cavity 11 is h1, and the range of h2 / h1 is 2 to 10.
[0046] Specifically, the thickness of the bottom of the carrier 1 should be as thin as possible, while meeting the mechanical strength requirements of the carrier 1, it can also meet the heat transfer requirements during the brazing process, so that the solder 4 can fully melt and spread, and then completely infiltrate the electrodes to be welded on the welding side of the packaging base 5; when the thickness of the bottom of the carrier 1 is too large, heat is not easily transferred to the solder 4, and incomplete melting of the solder 4 will seriously affect the welding quality.
[0047] In some embodiments, the carrier 1 and the pressing block 2 are both made of graphite, and the surfaces of the carrier 1 and the pressing block 2 are coated with a silicon carbide coating.
[0048] Specifically, graphite has stable chemical properties and good thermal conductivity, and can transfer heat to the solder 4 very well, so that the solder 4 can fully melt and spread to infiltrate the electrode. Graphite is also resistant to high temperatures and easy to shape, with lower costs and is more conducive to use in welding. The silicon carbide coating can protect the graphite and prevent carbon particles dropped from the graphite during friction from contaminating the packaging base 5 and other accessories.
[0049] In addition, the utility model also provides a welding method, which adopts the welding mold described above, and the method also includes the following steps:
[0050] S1, placing the package base 5 into the cavity 11 of the carrier 1 and placing the solder 4 on the electrode to be welded of the package base 5, and then placing the lead 3 on the solder 4 and applying a load to the lead 3, the solder 4 and the package base 5 through the pressing block 2;
[0051] S2. Place the soldering mold with the lead 3, solder 4 and package base 5 in a soldering furnace, and set a heating program to complete the soldering.
[0052] In summary, the embodiment of the utility model provides a welding mold, which first limits and fixes the position of the packaging base 5 through the cavity 11, and then fixes the lead 3 and the solder 4 on the packaging base 5 by applying a load through the pressure block 2, and finally limits the position of the pressure block 2 through the limiting column 12, thereby ensuring that the relative positions of the packaging base 5, the solder 4 and the lead 3 are stable and reliable during the welding process, and the relative positions of the three are not easily shifted due to external collisions, thereby causing a decrease in the quality of the finished welding product.
[0053] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and substitutions can be made without departing from the technical principle of the present invention. These improvements and substitutions should also be regarded as the protection scope of the present invention.
Claims
1. A welding mold, characterized in that: The invention comprises a carrier and a pressing block, wherein the carrier is provided with a positioning plane, the positioning plane is recessed to form a cavity for accommodating a limited packaging base, the carrier is provided with a limiting column, the limiting column forms a limited space for limiting the movement of the pressing block in the extension direction of the positioning plane, the pressing block cooperates with the carrier by being inserted into the limiting space, and the pressing block is used to press the lead and the solder against the electrode to be welded on the welding side of the packaging base; the positioning plane is provided with at least one limiting protrusion on the peripheral side of the cavity, and the limiting protrusion is used to limit the movement of the lead along the extension direction of the positioning plane; the distance between the limiting protrusion and the lead is controlled within 25μm to 50μm, and the limiting protrusion has a rounded corner; Wherein, the extending direction of the positioning plane includes a first direction and a second direction which are perpendicular to each other.
2. The welding mold according to claim 1, characterized in that: When the cavity accommodates the position-limiting packaging base, the dimensional tolerance between the length and width of the cavity and the length and width of the packaging base is 150 μm to 200 μm.
3. The welding mold according to claim 1, characterized in that: The cavity includes a first cavity and a second cavity, the first cavity is formed by the depression of the positioning plane and matches the size of the packaging base, the second cavity is arranged on both sides of the first cavity along the second direction, and the depth of the second cavity is less than the depth of the first cavity.
4. The welding mold according to claim 3, characterized in that: In the first direction, the length of the second cavity is smaller than that of the first cavity, and both ends of the second cavity protrude toward the middle to form limiting portions relative to both ends of the first cavity.
5. The welding mold according to claim 1, characterized in that: The side of the pressing block facing the cavity is provided with a protrusion corresponding to the welding side of the package base in the cavity, and the protrusion is used to press the lead and the solder against the electrode to be welded on the welding side of the package base.
6. The welding mold according to claim 1, characterized in that: The depth of the cavity is h2, the distance between the side surface of the carrier opposite to the positioning plane and the bottom surface of the cavity is h1, and the range of h2 / h1 is 2 to 10.
7. The welding mold according to claim 1, characterized in that: The carrier and the pressing block are both made of graphite, and the surfaces of the carrier and the pressing block are coated with silicon carbide coatings.
Citation Information
Cited By
Welding die and welding method
CN117921128A