Pin-free semiconductor metal bonding wire packaging structure

By covering the side of the thermally conductive metal plate of the leadless semiconductor metal bonding wire package structure with solderable material, it ensures 100% soldering of the bare copper contacts on the side, solving the problem of difficulty in judging the quality of the solder points and oxidation during the welding process, and improving the welding efficiency. Stability and firmness simplify the inspection process and reduce costs.

CN221812091UActive Publication Date: 2024-10-08QIANGMAO ELECTRONICS WUXI CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420887677.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-26
Publication Date
2024-10-08
Estimated Expiration
2034-04-26

AI Technical Summary

Technical Problem

The existing leadless semiconductor metal bonding wire packaging structure makes it difficult to judge the quality of the solder points during the welding process. The bare copper contacts on the side are easily oxidized, causing solder rejection problems, and the tin creep is highly unstable, affecting the welding reliability.

Method used

Design a leadless semiconductor metal bonding wire packaging structure. The side of the thermally conductive metal plate is covered with solderable material to ensure 100% tin crawling of the bare copper contacts on the side. It is connected to the chip through metal leads and bonding wires, simplifying the welding process and improving welding. Firmness.

Benefits of technology

It achieves the stability and firmness of the welding process, simplifies welding quality inspection, reduces inspection time and cost, and improves product competitiveness.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221812091U_ABST
    Figure CN221812091U_ABST
Patent Text Reader

Abstract

The utility model discloses a pin-free semiconductor metal bonding wire packaging structure, which comprises a heat-conducting metal plate, a chip welding area for welding a chip is arranged in the middle area of the heat-conducting metal plate, and long connecting ribs for connecting the chip are arranged on the peripheral side of the heat-conducting metal plate; the left side and the right side of the chip welding area are respectively provided with four left side metal contact points and four right side metal contact points which are used for connecting an external circuit, the right side metal contact points are connected with the chip welding area, and the left side metal contact points are connected with the long connecting ribs; the back surface of the chip is welded on the chip welding area, and the front surface of the chip is connected with the left side metal welding point through a metal lead and a metal welding wire; and a plastic package material is encapsulated above the chip. According to the pin-free semiconductor metal bonding wire packaging structure provided by the utility model, the bare copper contact points on the side surfaces can realize 100% tin climbing, so that the stability of the welding process and the welding effect when a product is welded to a PCB (Printed Circuit Board) is ensured, the welding firmness of the product is improved, and a welding quality inspection method is simplified.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of semiconductor device production, and more specifically to a pinless semiconductor metal bonding wire packaging structure. Background Art

[0002] The leadless surface package structure DFN (Dual Flat No-lead Package) is a leadless package form that uses advanced double-sided or square flat leadless packaging. Only the bottom and two sides have pads. It has the advantages of small size, light weight, good heat dissipation, good electrical performance, and good reliability.

[0003] During the production process, the entire unit device is usually separated by cutting after the plastic encapsulation process. The separated device exposes the bare copper bottom surface and the bare copper contact points on the side flush with the device side wall. The existing production method can only make the bare copper on the bottom surface obtain a solderable coating. Therefore, when the product is soldered on the PCB, since the metal contact type package is used to replace the previous needle pins, this packaging form is difficult to judge its solder points from the appearance of the product, especially whether the solder condition of the bottom is good. It is necessary to use perspective methods such as X-RAY to judge the welding effect. At the same time, the bare copper contact points on the side are easily oxidized in the air, resulting in solder rejection problems.

[0004] In order to solve the above problems, the bare copper on the side is soaked with solder to further realize the tin creeping function of the metal contact points on the side of the product. The current conventional practice in the industry is to partially cut the lead frame first, and then use the electroplating process after cutting to achieve the bare copper contact points on the side covered with solder, and finally cut the lead frame into single materials. The purpose of partially cutting the metal frame is to ensure that the metal units are connected in series and there is a complete conduction circuit during electroplating. However, because the metal connecting ribs on the side of the product are partially cut or half-cut, when the subsequent product is welded on the circuit board, the tin creeping height depends on the cutting depth, and 100% tin creeping of the bare copper contact points on the side cannot be achieved; in addition, due to the half-cut state of the bare copper contact points on the side, the metal of the contact points is stepped. When the product is soldered on the PCB, there is a risk of insufficient tin creeping and residual air at the steps.

[0005] Therefore, there is an urgent need for a structure that can maximize the wetting area of ​​the side bare copper contact points to ensure product welding reliability. Summary of the invention

[0006] The technical problem to be solved by the utility model is to provide a pinless semiconductor metal wire packaging structure to ensure the stability of the welding process and welding effect when the product is welded to the PCB, improve the welding firmness of the product, simplify the welding quality inspection method, reduce the inspection time and financial costs, and thus enhance the product competitiveness.

[0007] In order to solve the above technical problems, the technical solutions adopted by the present utility model are as follows.

[0008] A leadless semiconductor metal wire bonding packaging structure comprises a heat-conducting metal plate, a chip bonding area for bonding a chip is arranged in the middle area of ​​the heat-conducting metal plate, and a long connecting rib for connecting the chip is arranged on the peripheral side of the heat-conducting metal plate; four left-side metal contact points and right-side metal contact points for connecting an external circuit are arranged on the left and right sides of the chip bonding area respectively, the right-side metal contact points are connected to the chip bonding area, and the left-side metal contact points are connected to the long connecting rib; the back side of the chip is welded to the chip bonding area, and the front side of the chip is connected to the left-side metal bonding points through metal leads and metal wires; and a plastic sealing material is potted on the top of the chip.

[0009] To further optimize the technical solution, the left metal contact point includes three interconnected left upper metal contact points and one left lower metal contact point, and the left upper metal contact point and the left lower metal contact point are respectively connected to the long connecting ribs through short connecting ribs.

[0010] To further optimize the technical solution, the upper metal contact point on the left side is connected to the front side of the chip through a metal lead, and the lower metal contact point on the left side is connected to the front side of the chip through a metal bonding wire.

[0011] To further optimize the technical solution, the upper left metal contact point, the lower left metal contact point and the right metal contact point are all covered with weldable materials that are easy to weld.

[0012] To further optimize the technical solution, the heat-conducting metal plate is a copper substrate.

[0013] To further optimize the technical solution, the metal lead wire is a copper wire or a gold wire, and the number is set to be single or multiple.

[0014] To further optimize the technical solution, the metal bonding wire is a copper wire, an aluminum wire or a gold wire.

[0015] Due to the adoption of the above technical scheme, the technical progress achieved by the present invention is as follows.

[0016] The utility model provides a pinless semiconductor metal wire packaging structure, in which the bare copper contact points on the side can achieve 100% tin creep, ensuring the stability of the welding process and welding effect when the product is welded to the PCB, improving the product welding firmness, and simplifying the welding quality inspection method. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is a schematic diagram of the structure of the utility model;

[0018] Figure 2 This is a schematic diagram of the structure of the internal pins of the utility model;

[0019] Figure 3 It is a schematic diagram of the structure of the utility model after packaging.

[0020] Among them: 101. chip, 102. heat-conducting metal plate, 103. metal lead, 104. metal welding wire, 105. plastic packaging material, 106. chip welding area, 201. long connecting rib, 202. short connecting rib, 203. upper metal contact point on the left, 204. lower metal contact point on the left, 205. metal contact point on the right. DETAILED DESCRIPTION

[0021] The present invention will be further described in detail below with reference to the accompanying drawings and specific embodiments.

[0022] A leadless semiconductor metal wire bonding package structure, combined with Figures 1 to 3 As shown, it includes a heat-conducting metal plate 102 , a chip welding area 106 is arranged in the middle area of ​​the heat-conducting metal plate 102 for welding the chip 101 , and a long connecting rib 201 is arranged on the peripheral side of the heat-conducting metal plate 102 for connecting the chip 101 .

[0023] Four left metal contact points and four right metal contact points 205 are respectively arranged on the left and right sides of the chip welding area 106. The left metal contact points are connected to the long connecting ribs 201, and the right metal contact points 205 are connected to the chip welding area 106. The back of the chip 101 is welded to the chip welding area 106, and the front of the chip 101 is connected to the left metal welding points through the metal leads 103 and the metal welding wires 104. The top of the chip 101 is encapsulated with a plastic encapsulation material 105.

[0024] The left metal contact points include three interconnected left upper metal contact points 203 and one left lower metal contact point 204 . The left upper metal contact points 203 and the left lower metal contact points 204 are connected to the long connecting ribs 201 through the short connecting ribs 202 , respectively.

[0025] The upper metal contact point 203 on the left is connected to the front side of the chip 101 through the metal lead 103 , and the lower metal contact point 204 on the left is connected to the front side of the chip 101 through the metal bonding wire 104 .

[0026] The left upper metal contact point 203 , the left lower metal contact point 204 and the right metal contact point 205 are all covered with weldable materials to facilitate welding.

[0027] The heat-conducting metal plate 102 is a copper substrate, and the heat generated by the chip can be dissipated through the heat-conducting metal plate, thereby increasing the service life of the chip.

[0028] The metal lead 103 is a copper wire or a gold wire, and the number is set to be single or multiple. The specific number can be designed according to demand. The metal bonding wire 104 is a copper wire, an aluminum wire or a gold wire.

[0029] The bottom of the thermally conductive metal plate and the metal contact points on the two sides are covered with solderable materials, which can achieve 100% tin creepage and ensure the stability and firmness of the welding when the product is soldered on the PCB board.

Claims

1. A leadless semiconductor metal wire bonding package structure, characterized in that: The invention comprises a heat-conducting metal plate (102), wherein a chip welding area (106) for welding a chip (101) is arranged in the middle area of ​​the heat-conducting metal plate (102), and a long connecting rib (201) for connecting the chip (101) is arranged on the peripheral side of the heat-conducting metal plate (102); four left metal contact points and right metal contact points (205) for connecting to an external circuit are arranged on the left and right sides of the chip welding area (106), the right metal contact points (205) are connected to the chip welding area (106), and the left metal contact points are connected to the long connecting rib (201); the back side of the chip (101) is welded to the chip welding area (106), and the front side of the chip (101) is connected to the left metal welding points via metal leads (103) and metal welding wires (104); and a plastic encapsulation material (105) is encapsulated above the chip (101).

2. The leadless semiconductor metal bonding wire packaging structure according to claim 1, characterized in that: The left metal contact points include three mutually connected left upper metal contact points (203) and a left lower metal contact point (204), and the left upper metal contact points (203) and the left lower metal contact point (204) are respectively connected to the long connecting rib (201) via the short connecting rib (202).

3. The leadless semiconductor metal bonding wire packaging structure according to claim 2, characterized in that: The upper metal contact point (203) on the left side is connected to the front side of the chip (101) via a metal lead (103), and the lower metal contact point (204) on the left side is connected to the front side of the chip (101) via a metal bonding wire (104).

4. The leadless semiconductor metal bonding wire packaging structure according to claim 2, characterized in that: The left upper metal contact point (203), the left lower metal contact point (204) and the right metal contact point (205) are all covered with weldable material that facilitates welding.

5. The leadless semiconductor metal bonding wire packaging structure according to claim 1, characterized in that: The heat-conducting metal plate (102) is a copper substrate.

6. The leadless semiconductor metal bonding wire packaging structure according to claim 1, characterized in that: The metal lead wire (103) is a copper wire or a gold wire, and the number is set to be single or multiple.

7. The leadless semiconductor metal bonding wire packaging structure according to claim 1, characterized in that: The metal bonding wire (104) is a copper wire, an aluminum wire or a gold wire.