Sample preparation mold for fiber reinforced material

By setting protrusions and through-holes in the fiber-reinforced material sample preparation mold, and using a compression plate to tension the fibers, the problem of incomplete fiber embedding is solved, simplifying the structure and improving the success rate of sample preparation.

CN221826595UActive Publication Date: 2024-10-11ZHONGFU SHENYING CARBON FIBER
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420271735.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-02
Publication Date
2024-10-11
Estimated Expiration
2034-02-02

AI Technical Summary

Technical Problem

The existing fiber-reinforced material sample preparation mold has the problem that the fibers are not completely embedded, resulting in low sample preparation success rate, complex mold structure, and high cost.

Method used

Design a fiber-reinforced material sample preparation mold that includes a first template and a second template. Protrusions are provided on the surface of the first template, and corresponding through holes are provided on the second template. The mold cavity is formed by fitting the templates, and a compression plate is used. The fibers are kept under tension, thereby completely embedding the fibers.

Benefits of technology

The mold structure is simplified, the success rate of sample preparation of fiber-reinforced materials is improved, the production cost is reduced, and the uniform distribution of fibers and material properties are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221826595U_ABST
    Figure CN221826595U_ABST
Patent Text Reader

Abstract

The utility model relates to a sample preparation mold for a fiber reinforced material. The sample preparation mold comprises a first mold plate, a second mold plate and two pressing plates, at least one group of lug bosses is arranged on the first surface of the first template, each group of lug bosses comprises at least two lug bosses which are arranged at intervals in the first direction, and the lug bosses are used for supporting fibers; at least one through hole is formed in the second template, and each through hole corresponds to one group of lug bosses; the two pressing plates are mounted on the two side faces, in the first direction, of the first template correspondingly and used for keeping the fibers in a tensioned state; the second template is attached to the first surface of the first template, the through holes and the first template are matched to define a cavity, a set of protruding parts corresponding to the through holes are located in the through holes, the protruding parts are lower than the second surface of the second template, and the second surface of the second template is the surface deviating from the first template. By means of the design, it is guaranteed that fibers are not exposed out of materials, meanwhile, a cavity does not need to be independently arranged, the structure is simplified, and production efficiency is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of fiber reinforced materials, and in particular to a sample making mold for fiber reinforced materials. Background Art

[0002] Fiber-reinforced materials have the advantages of high specific strength, large specific modulus, good corrosion resistance and durability, and are therefore increasingly widely used in various transportation equipment, building components, electronic equipment and other fields. The sample preparation method of fiber-reinforced materials includes pouring the material and a curing agent into a mold with fibers placed therein, and then demolding the mold after curing and molding.

[0003] However, in the fiber-reinforced materials currently made by sample making molds, the fibers are often not completely embedded and the material is exposed, which reduces the success rate of sample making of the fiber-reinforced materials. In addition, the cavity of the sample making mold needs to be set separately, which has a complex structure and high cost. Utility Model Content

[0004] In order to solve the above technical problems, the present application provides a sample making mold for fiber reinforced materials, which saves costs and improves production efficiency.

[0005] According to some embodiments, the present application provides a sample preparation mold for a fiber reinforced material, comprising:

[0006] A first template, wherein at least one group of protrusions is disposed on a first surface of the first template, each group of the protrusions includes at least two protrusions arranged at intervals along a first direction, and the protrusions are used to support fibers;

[0007] A second template, wherein the second template is provided with at least one through hole, and each of the through holes corresponds to a group of protrusions;

[0008] Two pressing plates, the two pressing plates are respectively installed on two side surfaces of the first template along the first direction, and the pressing plates are used to keep the fibers in a tensioned state;

[0009] The second template is fitted with the first surface of the first template, the through hole cooperates with the first template to enclose a molding cavity, a group of protrusions corresponding to the through hole are located in the through hole, and the height of the protrusions is lower than the second surface of the second template, and the second surface of the second template is the surface facing away from the first template.

[0010] In some embodiments of the present application, the protrusion is in the shape of a long strip extending along the second direction, and the length of the protrusion in the second direction is adapted to the length of the cavity in the second direction;

[0011] The first direction is perpendicular to the second direction.

[0012] In some embodiments of the present application, the protrusions are provided in multiple groups, and the multiple groups of protrusions are arranged at intervals along the second direction.

[0013] In some embodiments of the present application, in the first direction, two of the protrusions in each group of the protrusions are located at opposite ends of the cavity, respectively.

[0014] In some embodiments of the present application, the height of the protrusion in the vertical direction is one third to two thirds of the thickness of the second template in the vertical direction.

[0015] In some embodiments of the present application, the protrusion includes a curved surface for supporting the fiber.

[0016] In some embodiments of the present application, the protrusion is semi-cylindrical, and the cylindrical surface of the semi-cylindrical shape is used to support the fiber.

[0017] In some embodiments of the present application, the fiber-reinforced material sampling mold also includes a plurality of first fasteners, a plurality of first screw holes and a plurality of second screw holes, the first template is provided with a plurality of first screw holes arranged at intervals, the second template is provided with a plurality of second screw holes corresponding to the plurality of first screw holes, and the first fastener passes through the second screw holes and the first screw holes in sequence to fix the first template and the second template together.

[0018] In some embodiments of the present application, the fiber-reinforced material sampling mold also includes a plurality of second fasteners, a plurality of third screw holes and a plurality of fourth screw holes. The first template is provided with a plurality of third screw holes arranged at intervals, and the clamping plate is provided with a plurality of fourth screw holes corresponding to the plurality of third screw holes. The second fastener passes through the fourth screw holes and the third screw holes in sequence to detachably connect the clamping plate to the first template.

[0019] In some embodiments of the present application, the first template, the second template and the pressing plate are made of stainless steel.

[0020] The fiber reinforced material sample preparation mold provided in this application can achieve the following beneficial technical effects:

[0021] The fiber-reinforced material sampling mold provided in the present application is configured by arranging a protrusion on the first surface of the first template and correspondingly arranging a through hole on the second template. When the first template and the second template are bonded together, the through hole cooperates with the first template to enclose a molding cavity, and there is no need to set up a separate molding cavity, thereby simplifying the structure. In addition, the protrusion cooperates with the clamping plate to tension the fibers so that they are completely embedded in the material, thereby improving the success rate of sampling of the fiber-reinforced material. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] The drawings herein are incorporated into the specification and constitute a part of the specification to illustrate embodiments of the present application and are used together with the description to explain the principles of the present application. In these drawings, similar reference numerals are used to represent similar elements. The drawings described below are some embodiments of the present application, rather than all embodiments. For those of ordinary skill in the art, other drawings can be obtained based on these drawings without paying creative work.

[0023] Figure 1 It is a structural schematic diagram of a sample preparation mold for a fiber-reinforced material shown in one embodiment of the present application;

[0024] Figure 2 yes Figure 1 A schematic diagram of the structure of the first template;

[0025] Figure 3 yes Figure 1 Schematic diagram of the structure of the second template.

[0026] Reference numerals:

[0027] 100, first template; 110, first surface; 120, raised portion; 130, first screw hole; 140, third screw hole;

[0028] 200, second template; 210, second surface; 220, through hole; 230, second screw hole;

[0029] 300, pressing plate; 310, fourth screw hole;

[0030] 400, cavity;

[0031] 500, a first fastener;

[0032] 600. Second fastener. DETAILED DESCRIPTION

[0033] In order to make the purpose, technical scheme and advantages of the embodiments of the present application clearer, the technical scheme in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, rather than all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without making creative work are within the scope of protection of the present application. It should be noted that, in the absence of conflict, the embodiments in the present application and the features in the embodiments can be combined with each other arbitrarily.

[0034] In order to solve the problem that the fibers are not completely embedded and the material is exposed, an embodiment of the present application provides a sample making mold for a fiber-reinforced material, by setting a protrusion on the first surface of the first template and correspondingly setting a through hole on the second template. When the first template and the second template are fitted together, the through hole cooperates with the first template to enclose a molding cavity, and there is no need to set a separate molding cavity, thereby simplifying the structure. In addition, the protrusion cooperates with the clamping plate to completely embed the fibers in the material, thereby improving the success rate of sampling of the fiber-reinforced material.

[0035] The sample preparation mold of the fiber reinforced material provided in the present application is described in detail below in conjunction with the accompanying drawings.

[0036] An exemplary embodiment of the present application provides a sample preparation mold of a fiber reinforced material, such as Figures 1 to 3 As shown, the first direction is Figures 1 to 3 The x-axis direction in the second direction is Figures 1 to 3 The y-axis direction in the vertical direction is Figures 1 to 3 In the z-axis direction, the sample making mold of the fiber-reinforced material includes a first template 100, a second template 200 and two pressing plates 300, wherein at least one group of protrusions is arranged on the first surface 110 of the first template 100, and each group of protrusions includes two protrusions 120 arranged at intervals along the first direction, and the two protrusions 120 cooperate to support the fibers.

[0037] At least one through hole 220 is provided on the second template 200, and each through hole 220 corresponds to a group of protrusions; when the second template 200 is fitted with the first surface 110 of the first template 100, the through holes 220 located in the second template 200 cooperate with the first template 100 to enclose a molding cavity 400, and a group of protrusions are located in a corresponding through hole 220, that is, a group of protrusions are located in a corresponding molding cavity 400, and the surface of the second template 200 facing away from the first template 100 is the second surface 210, and the height of the protrusion 120 in the z-axis direction does not exceed the second surface 210 of the second template 200; two clamping plates 300 are installed on the two side surfaces of the first template 100 along the first direction.

[0038] The process of preparing the fiber-reinforced material using the sample preparation mold of the above fiber-reinforced material is as follows:

[0039] The fibers are placed on each group of raised portions 120 of the first template 100 along the first direction, and the fibers are fixed with two clamping plates 300 and kept in a tensioned state. At this time, two raised portions 120 in a group of raised portions support the fibers, so that the fibers located between the two raised portions 120 are away from the first surface 110 of the first template 100 in the z-axis direction; the second template 200 is fitted with the first surface 110 of the first template 100, and the through holes 220 and the first surface 110 cooperate to enclose a molding cavity 400. A group of raised portions corresponding to the through holes 220 are located in the molding cavity 400 enclosed by the through holes 220. Since the height of the raised portions 120 is lower than the second surface 210 of the second template 200, the fibers are located in the middle of the molding cavity 400 in the z-axis direction. Liquid raw materials are then poured into the molding cavity 400, and fiber-reinforced material can be obtained after solidification and demolding.

[0040] In the present embodiment, a protrusion 120 is provided on the first surface 110 of the first template 100, and a through hole 220 is correspondingly provided on the second template 200. When the first template 100 and the second template 200 are bonded together, the through hole 220 cooperates with the first surface 110 to enclose the molding cavity 400. There is no need to separately provide the molding cavity 400, thereby simplifying the structure. In addition, the protrusion 120 cooperates with the clamping plate 300 so that the fibers are located in the middle of the molding cavity 400 in the vertical direction and are in a tensioned state, and are thus completely embedded in the material, thereby avoiding the situation where the fibers sink to the bottom or float on the surface, thereby improving the success rate of sampling of fiber-reinforced materials.

[0041] In some embodiments, Figure 1 and Figure 2 As shown, the protrusion 120 is in the shape of an elongated strip and extends along the second direction. The length of the protrusion 120 in the second direction is adapted to the length of the cavity 400 in the second direction. "Adaptation" means that the length of the protrusion 120 in the second direction is equal to the length of the cavity 400 in the second direction or the length of the protrusion 120 in the second direction is slightly smaller than the length of the cavity 400 in the second direction.

[0042] Such a design ensures that fibers are distributed on the edges of the fiber reinforced material, and the fibers are distributed more evenly in the fiber reinforced material, which is beneficial to improving the specific strength and specific modulus of the fiber reinforced material, and is beneficial to the formation of the fiber cross section when the fiber reinforced material is brittlely fractured.

[0043] In some embodiments, continue to refer to Figure 1 and Figure 2 , a plurality of groups of protrusions 120 are provided on the first template 100, and the plurality of groups of protrusions 120 are arranged at intervals along the second direction, for example Figure 2Five groups of protrusions 120 are provided. By providing a plurality of groups of protrusions 120 on one first template 100, the consumption of raw materials for making the first template 100 can be reduced, thus saving costs.

[0044] In some embodiments, Figure 1 As shown, in the first direction, two protrusions 120 in each group of protrusions 120 are respectively located at opposite ends of the cavity 400. This arrangement can ensure that a larger portion of the fibers in the prepared fiber-reinforced material are located in the middle of the fiber-reinforced material, thereby improving the success rate of sample preparation and the utilization rate of raw materials.

[0045] In some embodiments, Figure 1 As shown, in the vertical direction, the height of the protrusion 120 is one-third to two-thirds of the thickness of the second template 200. For example, the height of the protrusion 120 is one-half of the thickness of the second template 200, the height of the protrusion 120 is three-eighths of the thickness of the second template 200, and so on. The thickness of the second template 200 is the height of the cavity 400. When the height of the protrusion 120 is within the above range, it can be ensured that the fiber is completely embedded in the material, thereby improving the success rate of sample preparation.

[0046] In some embodiments, reference Figure 2 The side of the protrusion 120 that contacts the fiber is set as an arc surface. For example, in some embodiments, the protrusion 120 is semi-cylindrical and extends along the second direction, and the cylindrical surface of the semi-cylindrical is used to support the fiber.

[0047] Since the fiber is pressed by the pressing plate 300 to maintain a tensioned state when supported by the protrusion 120, there is a strong interaction force between the fiber and the protrusion 120. Setting the side of the protrusion 120 that contacts the fiber as an arc surface can effectively prevent the fiber from deforming or breaking, thereby improving production efficiency.

[0048] In some embodiments, Figures 1 to 3 As shown, the sample making mold of the fiber reinforced material also includes a plurality of first fasteners 500, a plurality of first screw holes 130 and a plurality of second screw holes 230. The first fasteners 500, the first screw holes 130 and the second screw holes 230 are arranged in a one-to-one correspondence. The first screw holes 130 are arranged on the first template 100, and the second screw holes 230 are arranged on the second template 200 and the second screw holes 230 correspond to the first screw holes 130. The first fasteners 500 pass through the second screw holes 230 and the first screw holes 130 in sequence to fix the first template 100 and the second template 200 in connection.

[0049] In this embodiment, in the second direction, the first screw hole 130 is also arranged between the two groups of protrusions 120, and correspondingly, the second screw hole 230 is also correspondingly arranged between the two through holes 220, and the first screw hole 130 is located in the middle of the first template 100 in the first direction, and the second screw hole 230 is located in the middle of the second template 200 in the first direction. Since the cavity 400 for containing liquid is surrounded by the first template 100 and the second template 200, the first template 100 and the second template 200 need to fit tightly, and through the cooperation of the first fastener 500 and the first screw hole 130 and the second screw hole 230 arranged in the middle of the template, a tighter fit between the first template 100 and the second template 200 can be achieved, reducing the possibility of leakage of the liquid raw material poured into the cavity 400.

[0050] In some embodiments, Figures 1 to 3 As shown, the sample making mold of the fiber reinforced material also includes a plurality of second fasteners 600, a plurality of third screw holes 140 and a plurality of fourth screw holes 310. The second fasteners 600, the third screw holes 140 and the fourth screw holes 310 are arranged in a one-to-one correspondence. The third screw hole 140 is arranged on the first template 100, and the fourth screw hole 310 is arranged on the clamping plate 300 and the fourth screw hole 310 corresponds to the third screw hole 140. The second fasteners 600 pass through the fourth screw hole 310 and the third screw hole 140 in sequence to detachably connect the first template 100 and the clamping plate 300. The simple structure can achieve the fixation of the fiber.

[0051] The first fastener 500 and the second fastener 600 may be, for example, bolts, screws, etc.

[0052] The process of preparing the fiber-reinforced material using the sample-preparing mold of the fiber-reinforced material is as follows:

[0053] The fiber is placed on each group of protrusions 120 of the first template 100 along the first direction, a clamping plate 300 is fixed to the side of the first template 100 with a second fastener 600 to clamp one end of the fiber, and after pulling the other end of the fiber, another clamping plate 300 is fixed to the first template 100 with the second fastener 600 to keep the fiber in a tensioned state and fixed on the arc surface of the protrusion 120. At this time, two protrusions 120 in a group of protrusions support the fiber, so that the fiber located between the two protrusions 120 is away from the first surface 110 of the first template 100 in the z-axis direction.

[0054] The second template 200 is aligned with the first template 100, and the second template 200 and the first surface 110 are tightly fitted by the cooperation of the first fastener 500, the first screw hole 130 and the second screw hole 230. The through hole 220 cooperates with the first surface 110 to enclose the cavity 400. A group of protrusions corresponding to the through hole 220 are located in the cavity 400 enclosed by the through hole 220, and in the first direction, two protrusions 120 in a group of protrusions are located at both ends of the cavity 400. Since in the vertical direction, the height of the protrusion 120 is one-third to two-thirds of the thickness of the second template 200, the fiber is located in the middle position of the cavity 400 in the z-axis direction. Liquid raw material is then poured into the cavity 400, and fiber-reinforced material can be obtained after curing and demolding.

[0055] The fiber-reinforced material sample making mold provided in the present embodiment is provided with a protrusion 120 on the first surface 110 of the first template 100, and a through hole 220 is correspondingly provided on the second template 200. When the first template 100 and the second template 200 are fixed and attached by the first fastener 500, the through hole 220 cooperates with the first surface 110 to enclose the molding cavity 400, and there is no need to set up the molding cavity 400 separately, thereby simplifying the structure and saving costs. In addition, the protrusion 120 cooperates with the clamping plate 300 to enable the fiber to be located in the middle of the molding cavity 400 in the vertical direction, and then be completely embedded in the material, thereby improving the success rate of fiber-reinforced material sample making.

[0056] In some embodiments, the first template 100 , the second template 200 , and the pressing plate 300 may be made of stainless steel or the like.

[0057] In some embodiments, the fiber can be carbon fiber, glass fiber or organic fiber, etc., and the liquid raw material can be resin, that is, the mold can be used to produce resin-based carbon fiber reinforced materials, resin-based glass fiber reinforced materials, etc., which are not limited here.

[0058] In some embodiments, the shape of the through hole 220 may be adjusted according to the actual shape of the fiber-reinforced material, such as a rectangle, an ellipse, etc., which is also within the protection scope of the present application.

[0059] The contents described above may be implemented individually or in combination in various ways, and these variations are all within the protection scope of this application.

[0060] It should be noted that, in the description of the present application, the terms "upper", "lower", "front", "back", etc., indicating directions or positional relationships are based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore should not be understood as a limitation on the present application.

[0061] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of this application, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.

[0062] In this application, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0063] In the present application, unless otherwise clearly specified and limited, a first feature being “above” or “below” a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being “above”, “above”, and “above” a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being “below”, “below”, and “below” a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.

[0064] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present application. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, without contradiction.

[0065] Although the embodiments of the present application have been shown and described above, it can be understood that the above embodiments are exemplary and cannot be understood as limitations on the present application. Ordinary technicians in the field can change, modify, replace and modify the above embodiments within the scope of the present application.

Claims

1. A sample making mold for a fiber reinforced material, characterized in that: The sample preparation mold of the fiber reinforced material comprises: A first template, wherein at least one group of protrusions is disposed on a first surface of the first template, each group of the protrusions includes at least two protrusions arranged at intervals along a first direction, and the protrusions are used to support fibers; A second template, wherein at least one through hole is provided on the second template, and each of the through holes corresponds to a group of the protrusions; Two pressing plates, the two pressing plates are respectively installed on two side surfaces of the first template along the first direction, and the pressing plates are used to keep the fibers in a tensioned state; The second template is fitted with the first surface of the first template, the through hole cooperates with the first template to enclose a molding cavity, a group of protrusions corresponding to the through hole are located in the through hole, and the height of the protrusions is lower than the second surface of the second template, and the second surface of the second template is the surface facing away from the first template.

2. The sample preparation mold for fiber reinforced materials according to claim 1, characterized in that: The protrusion is in the shape of a long strip extending along the second direction, and the length of the protrusion in the second direction is adapted to the length of the cavity in the second direction; The first direction is perpendicular to the second direction.

3. The sample preparation mold for fiber reinforced materials according to claim 2, characterized in that: The protrusions are provided in a plurality of groups, and the plurality of groups of protrusions are arranged at intervals along the second direction.

4. The sample preparation mold for fiber reinforced materials according to claim 1, characterized in that: In the first direction, two protrusions in each group of protrusions are located at opposite ends of the cavity.

5. The sample preparation mold for fiber reinforced materials according to claim 1, characterized in that: The height of the protrusion in the vertical direction is one third to two thirds of the thickness of the second template in the vertical direction.

6. The sample preparation mold for fiber reinforced materials according to claim 1, characterized in that: The protrusion includes a curved surface for supporting the fiber.

7. The sample preparation mold for fiber reinforced materials according to claim 6, characterized in that: The protrusion is in a semi-cylindrical shape, and the cylindrical surface of the semi-cylindrical shape is used to support the fiber.

8. The sample preparation mold for fiber reinforced materials according to claim 1, characterized in that: The fiber-reinforced material sampling mold also includes multiple first fasteners, multiple first screw holes and multiple second screw holes. The first template is provided with multiple first screw holes arranged at intervals, and the second template is provided with multiple second screw holes corresponding to the multiple first screw holes. The first fastener passes through the second screw holes and the first screw holes in sequence to fix the first template and the second template together.

9. The sample preparation mold for fiber reinforced materials according to claim 1, characterized in that: The fiber-reinforced material sampling mold also includes multiple second fasteners, multiple third screw holes and multiple fourth screw holes. The first template is provided with multiple third screw holes arranged at intervals, and the clamping plate is provided with multiple fourth screw holes corresponding to the multiple third screw holes. The second fastener passes through the fourth screw holes and the third screw holes in sequence to detachably connect the clamping plate to the first template.

10. The sample preparation mold for fiber reinforced materials according to claim 1, characterized in that: The first template, the second template and the pressing plate are made of stainless steel.