Panel and photovoltaic module

By setting the coating area and the non-coating area on the visualization board of the photovoltaic module, and using transparent pearlescent ink, the problem of light transmittance loss and limited appearance of the photovoltaic module in the existing technology is solved, and efficient power generation and beautiful effects are achieved. .

CN221827898UActive Publication Date: 2024-10-11SHENZHEN HELLO TECH ENERGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420353654.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-26
Publication Date
2024-10-11
Estimated Expiration
2034-02-26

AI Technical Summary

Technical Problem

Existing screen-printed photovoltaic glass modules suffer from large light transmittance losses during the tempering process, low output power, and limited high-temperature ink options, making it difficult to meet the dual needs of appearance and power.

Method used

Partial screen printing technology is used to set coated areas and non-coated areas on the visualization board, and apply transparent pearlescent ink on the coated areas, adjust the number, spacing and thickness of the coated areas, and combine the curved surface structure and positioning holes to ensure The aesthetics and high light transmittance of photovoltaic modules.

Benefits of technology

It improves the power generation and aesthetics of photovoltaic modules, reduces the loss of light transmittance, avoids the problem of coating discoloration and distortion due to high temperature, and at the same time improves printing efficiency and mechanical strength.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221827898U_ABST
    Figure CN221827898U_ABST
Patent Text Reader

Abstract

The utility model provides a panel and a photovoltaic assembly, and relates to the field of photovoltaic technology, the panel comprises a visual plate, the visual plate comprises a coating area and a non-coating area defined by the coating area, and a coating is arranged on the coating area. According to the panel provided by the utility model, one side of the visual plate is provided with the coating area and the non-coating area, and the coating area is provided with the coating, so that the overall silk-screen printing is adjusted into partial silk-screen printing, the overall aesthetic property of the photovoltaic module panel is ensured, and the photovoltaic module is ensured to have higher light transmittance and higher power generation power; the poor light transmittance is avoided, and the power generation efficiency loss is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of photovoltaics, and in particular to a panel and a photovoltaic component. Background Art

[0002] With the development of photovoltaic technology, the application of photovoltaic modules is becoming an important sub-sector in the field of photovoltaic technology. At present, the market requires photovoltaic modules to provide good photoelectric performance, and also require beautiful appearance and bright colors. Therefore, silk-screen photovoltaic glass and its photovoltaic modules are favored by the market, and products such as curved roof tiles, roof-integrated photovoltaic modules, and glass curtain walls are promoted.

[0003] Most existing screen printing technologies are used to print or coat the entire glass surface. After screen printing, the glass has a large light transmittance loss, and the output power of the photovoltaic modules produced is low. Conventional inks are heated, dried and solidified after screen printing, and then tempered. During the tempering process, the ink is easily discolored and distorted after high temperature. If high-temperature ink screen printing is used, the available colors are limited, and it is difficult to meet customers' dual needs for appearance and power. Utility Model Content

[0004] A first aspect of the utility model is to provide a panel.

[0005] A second aspect of the utility model is to provide a photovoltaic module.

[0006] The panel provided by the first aspect of the utility model is used for a photovoltaic module, and the panel comprises: a visualization board, the visualization board comprises a coating area and a non-coating area defined by the coating area; and a coating arranged on the coating area.

[0007] The panel provided by the utility model includes a visualization panel, and the visualization panel includes a coating area and a non-coating area defined by the coating area; the coating is arranged on the coating area. The panel of the utility model is provided with a coating area and a non-coating area on one side of the visualization panel, and a coating is arranged on the coating area, so that the overall silk screen printing is adjusted to partial silk screen printing, which not only ensures the overall aesthetics of the photovoltaic module panel, but also ensures that the photovoltaic module has a higher light transmittance, and thus has a higher power generation capacity, avoiding poor light transmittance and reducing power generation efficiency loss. Among them, the visualization panel of the utility model can be a glass plate or other visual panel.

[0008] In the above technical solution, optionally, the number of coating areas is at least two, at least two coating areas are distributed in an array, the interval between two adjacent coating areas is 5 mm to 10 mm, and / or the width and length of each coating area are 2 mm to 5 mm.

[0009] In this technical solution, the interval between two adjacent coating areas and the width and length of each coating area are limited, so that the coating areas and non-coating areas can be arranged alternately, avoiding the problem of the coating areas being too concentrated or too dispersed, and improving the overall effect.

[0010] In the above technical solution, optionally, the number of coating areas per square inch of the visualization board is greater than or equal to 10 and less than or equal to 1000.

[0011] In this technical solution, the number of coating areas per square inch on the visualization board is limited, which can avoid the problem of the coating areas being too concentrated or too dispersed, improve the aesthetics, and also improve the light transmittance.

[0012] In the above technical solution, optionally, the number of coating areas per square inch of the visualization board is greater than or equal to 150 and less than or equal to 250.

[0013] In this technical solution, the number of coating areas per square inch on the visualization board is limited to between 150 and 250, which further improves the aesthetics and light transmittance.

[0014] In the above technical solution, optionally, the panel further includes: at least two positioning holes, which are spaced apart on the visualization plate, and the positioning holes extend along the thickness direction of the visualization plate.

[0015] In this technical solution, by setting positioning holes on the panel, the visualization board and the screen mold can be well positioned, the visualization board and the screen mold can fit tightly, and precision printing can be completed continuously on the visualization board. It has the advantages of high printing efficiency and strong practicality, and no position deviation will occur during the printing process.

[0016] In the above technical solution, optionally, the maximum distance between any two points on the coating area is the first distance, the minimum distance between any two adjacent coating areas is the second distance, and the ratio of the first distance to the second distance is greater than or equal to 0.5 and less than or equal to 1.5.

[0017] In this technical solution, the length of the coating area is limited to be approximately the same as the spacing between the coating areas, so that the coating area and the non-coating area can be distributed more evenly, and the problem of the coating area being too concentrated or too dispersed will not occur, thereby improving the overall effect.

[0018] In the above technical solution, optionally, the coating is transparent pearlescent ink.

[0019] In this technical solution, the ordinary coating is adjusted to transparent pearlescent ink. During the tempering process, the transparent pearlescent ink is not prone to discoloration and distortion due to high temperature. High-temperature coating screen printing can be selected to improve printing efficiency.

[0020] In the above technical solution, optionally, the transparent pearlescent ink can absorb light with a wavelength greater than or equal to 100 nm and less than 300 nm, and the transparent pearlescent ink can transmit light with a wavelength greater than or equal to 300 nm and less than or equal to 1100 nm.

[0021] In this technical solution, transparent pearlescent ink has good light transmittance and can transmit visible light, part of ultraviolet light and part of near-infrared light. This can make the panel have good light transmittance and thus have higher power generation capacity, avoiding poor light transmittance and reducing power generation efficiency loss.

[0022] In the above technical solution, optionally, the light transmittance of the panel is greater than or equal to 85%.

[0023] In this technical solution, since the overall silk screen printing is adjusted to alternate silk screen printing in the coating area and the non-coating area, not only the overall aesthetics of the photovoltaic module panel is guaranteed, the light transmittance of the panel is greater than or equal to 85%, ensuring that the photovoltaic module has a higher power generation capacity.

[0024] In the above technical solution, optionally, the thickness of the coating is greater than or equal to 20 μm and less than or equal to 30 μm.

[0025] In this technical solution, the thickness of the coating should not be too thick, as too thick a coating will result in poor light transmittance and reduced power generation. The thickness of the coating should not be too thin, as too thin a coating will result in reduced overall aesthetics.

[0026] In the above technical solution, optionally, the visualization board includes a curved surface structure, and the radius of the curved surface structure is greater than or equal to 30 mm and less than or equal to 150 mm.

[0027] In this technical solution, if the arc radius is too large, the wave crest position will be too flat, which is not conducive to the dispersion of light. If the arc radius is too small, it will be not conducive to the manufacture of the panel. Therefore, setting the radius of the curved surface structure between 30mm and 150mm can ensure the dispersion effect of light and facilitate the manufacture of the panel. For example, the radius of the curved surface structure is 40mm, 80mm or 120mm.

[0028] In the above technical solution, optionally, the thickness of the visualization board is greater than or equal to 3 mm and less than or equal to 8 mm.

[0029] In this technical solution, the thickness of the visualization board should not be too thick. If the thickness of the visualization board is too thick, it is not conducive to the dispersion of light and the manufacturing cost is high. If the thickness of the visualization board is too thin, the mechanical strength is reduced and it is easy to be damaged under the action of external force. Therefore, the thickness is controlled to be greater than or equal to 3mm and less than or equal to 8mm, for example, 4mm, 5mm or 6mm.

[0030] The technical solution of the second aspect of the utility model provides a photovoltaic assembly, including: a panel provided by any technical solution of the first aspect of the utility model.

[0031] Since the photovoltaic module provided by the utility model includes the panel provided by any technical solution of the first aspect of the utility model, it has all the beneficial effects of the panel provided by any technical solution of the first aspect of the utility model, which will not be repeated here.

[0032] In some technical solutions, optionally, the photovoltaic module also includes: a backplane layer, which is arranged on the side of the panel away from the coating; a battery layer, which is arranged between the backplane layer and the panel; a first adhesive layer, which is arranged between the panel and the battery layer; and a second adhesive layer, which is arranged between the backplane layer and the battery layer.

[0033] In this technical solution, the first adhesive layer can be a high-cutoff encapsulation film, preferably one of high-cutoff EVA, POE, EPE or PVB films, with a thickness of 0.5mm-0.8mm; the battery layer is preferably one of XBC, MWT, and shingled batteries without metal grid lines, and the positive and negative metal electrodes are both led out from the back, followed by a battery cell with grid lines on both sides, such as PERC, TOPCON, and HJT. The second adhesive layer can be a highly transparent encapsulation film, preferably one of high-cutoff EVA, POE, EPE or PVB films, with a thickness of 0.5mm-0.8mm; the backplane layer is a flexible polymer material, such as one of PET or CPC or HPC materials, with a thickness of 0.4mm to 0.8mm. The backplane layer of the utility model is a flexible polymer material, so it can be bent into different shapes and is suitable for different installation substrates. At the same time, the selection of the battery layer can further improve the power generation efficiency.

[0034] Additional aspects and advantages of the present invention will become apparent in the following description or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] The above and / or additional aspects and advantages of the embodiments of the present invention will become apparent and easily understood from the description of the embodiments in conjunction with the following drawings, in which:

[0036] Figure 1 A schematic diagram showing the structure of a panel in an embodiment of the utility model is shown;

[0037] Figure 2 A schematic diagram of the assembly structure of the screen mold and the panel of the embodiment of the utility model is shown;

[0038] Figure 3 A schematic diagram showing the structure of a photovoltaic assembly according to an embodiment of the utility model is shown;

[0039] Figure 4 A preparation flow chart of a method for preparing a panel according to an embodiment of the utility model is shown.

[0040] in, Figures 1 to 3 The corresponding relationship between the reference numerals and component names is as follows:

[0041] 1 photovoltaic module, 12 panel, 122 visualization board, 1222 coating area, 1224 non-coating area, 1226 curved surface structure, 124 positioning hole, 14 first glue layer, 16 battery layer, 18 second glue layer, 19 backboard layer, 2 screen mold, 22 mold hole, 3 scraper, 4 coating. DETAILED DESCRIPTION

[0042] In order to more clearly understand the above aspects, features and advantages of the embodiments of the present invention, the embodiments of the present invention are further described in detail below in conjunction with the accompanying drawings and specific implementation methods. It should be noted that the embodiments of the present application and the features in the embodiments can be combined with each other without conflict.

[0043] In the following description, many specific details are set forth to facilitate a full understanding of the embodiments of the present invention. However, the embodiments of the present invention may also be implemented in other ways different from those described herein. Therefore, the protection scope of the embodiments of the present invention is not limited to the specific embodiments disclosed below.

[0044] like Figure 1 and Figure 2 As shown, the panel 12 provided in the first aspect of the utility model is used for the photovoltaic module 1, and the panel 12 includes: a visualization plate 122, the visualization plate 122 includes a coating area 1222 and a non-coating area 1224 defined by the coating area 1222; a coating 4 is arranged on the coating area 1222.

[0045] The panel 12 provided by the utility model includes a visualization board 122, and the visualization board 122 includes a coating area 1222 and a non-coating area 1224 defined by the coating area 1222; the coating 4 is arranged on the coating area 1222. The panel 12 of the utility model is provided with a coating area 1222 and a non-coating area 1224 on one side of the visualization board 122, and a coating 4 is arranged on the coating area 1222, so that the overall silk screen is adjusted to partial silk screen, which not only ensures the overall aesthetics of the panel 12, but also ensures that the photovoltaic module 1 has a higher light transmittance, and thus has a higher power generation power, avoids poor light transmittance, and reduces the loss of power generation efficiency. Among them, the visualization board 122 of the utility model can be a glass plate or other visual board.

[0046] In the above embodiment, optionally, the number of coating areas 1222 is at least two, at least two coating areas 1222 are distributed in an array, the interval between two adjacent coating areas 1222 is 5 mm to 10 mm, and / or the width and length of each coating area 1222 are 2 mm to 5 mm.

[0047] In this embodiment, by limiting the interval between two adjacent coating areas 1222 and the width and length of each coating area 1222, the coating areas 1222 and the non-coating areas 1224 can be arranged alternately, thereby avoiding the problem of the coating areas 1222 being too concentrated or too dispersed, and improving the overall effect.

[0048] In the above embodiment, optionally, the number of coating areas 1222 per square inch of the visualization board 122 is greater than or equal to 10 and less than or equal to 1000.

[0049] In this embodiment, limiting the number of coating areas 1222 per square inch on the visualization board 122 can avoid the problem of the coating areas 1222 being too concentrated or too dispersed, thereby improving the aesthetics and light transmittance.

[0050] In the above embodiment, optionally, the number of coating areas 1222 per square inch of the visualization board 122 is greater than or equal to 150 and less than or equal to 250.

[0051] In this embodiment, the number of coating areas 1222 per square inch of the visualization plate 122 is between 150 and 250, which further improves the aesthetics and light transmittance.

[0052] In the above embodiment, optionally, Figure 2 As shown, the panel 12 further includes: at least two positioning holes 124 , which are spaced apart on the visualization plate 122 , and the positioning holes 124 extend along the thickness direction of the visualization plate 122 .

[0053] In this embodiment, by setting the positioning hole 124 on the panel 12, the visualization board 122 and the screen mold 2 can be well positioned, the visualization board 122 and the screen mold 2 can fit tightly, and precision printing can be completed continuously on the visualization board 122. It has the advantages of high printing efficiency and strong practicality, and no position deviation will occur during the printing process.

[0054] In the above embodiment, optionally, the maximum distance between any two points on the coating area 1222 is the first distance, the minimum distance between any two adjacent coating areas 1222 is the second distance, and the ratio of the first distance to the second distance is greater than or equal to 0.5 and less than or equal to 1.5.

[0055] In this embodiment, the length of the coating area 1222 is limited to be approximately the same as the spacing between the coating areas 1222, so that the coating areas 1222 and the non-coating areas 1224 are distributed more evenly, and the problem of the coating areas 1222 being too concentrated or too dispersed will not occur, thereby improving the overall effect.

[0056] In the above embodiment, optionally, the coating 4 is transparent pearlescent ink.

[0057] In this embodiment, the coating 4 can be ink, such as transparent pearlescent ink. The ordinary coating 4 is adjusted to transparent pearlescent ink. During the tempering process, the transparent pearlescent ink is not prone to discoloration and distortion due to high temperature. The high-temperature coating 4 can be selected for screen printing to improve printing efficiency.

[0058] In the above embodiment, optionally, the transparent pearlescent ink can absorb light with a wavelength greater than or equal to 100 nm and less than 300 nm, and the transparent pearlescent ink can transmit light with a wavelength greater than or equal to 300 nm and less than or equal to 1100 nm.

[0059] In this embodiment, the transparent pearlescent ink has good light transmittance and can transmit visible light, part of ultraviolet light and part of near infrared light, so that the panel 12 can have good light transmittance and thus have higher power generation, avoiding poor light transmittance and reducing power generation efficiency loss. In the above embodiment, optionally, the light transmittance of the panel 12 is greater than or equal to 85%.

[0060] In this embodiment, since the overall silk screen printing is adjusted to alternate silk screen printing in the coating area 1222 and the non-coating area 1224, not only the overall aesthetics of the panel 12 is guaranteed, the light transmittance of the panel 12 is greater than or equal to 85%, ensuring that the photovoltaic module 1 has a higher power generation capacity.

[0061] In the above embodiment, optionally, the thickness of the coating 4 is greater than or equal to 20 μm and less than or equal to 30 μm.

[0062] In this embodiment, the thickness of the coating 4 should not be too thick, as too thick a coating 4 will result in poor light transmittance and reduced power generation. The thickness of the coating 4 should not be too thin, as too thin a coating 4 will result in reduced overall aesthetics.

[0063] In the above embodiment, optionally, Figure 3 As shown, the visualization board 122 includes a curved surface structure 1226 , and the radius of the curved surface structure 1226 is greater than or equal to 30 mm and less than or equal to 150 mm.

[0064] In this embodiment, if the arc radius is too large, the wave crest position will be too flat, which is not conducive to the dispersion of light. If the arc radius is too small, it is not conducive to the manufacture of the panel 12. Therefore, the radius of the curved surface structure 1226 is set between 30 mm and 150 mm, which can ensure the dispersion effect of light and facilitate the manufacture of the panel 12. For example, the radius of the curved surface structure 1226 is 40 mm, 80 mm or 120 mm.

[0065] In the above embodiment, optionally, the thickness of the visualization board 122 is greater than or equal to 3 mm and less than or equal to 8 mm.

[0066] In this embodiment, the thickness of the visualization board 122 should not be too thick. If the thickness of the visualization board 122 is too thick, it is not conducive to the dispersion of light and the manufacturing cost is high. If the thickness of the visualization board 122 is too thin, the mechanical strength is reduced and it is easy to be damaged under the action of external force. Therefore, the thickness is controlled to be greater than or equal to 3mm and less than or equal to 8mm, for example, 4mm, 5mm or 6mm.

[0067] The second aspect of the present invention provides a photovoltaic assembly 1, comprising: a panel 12 provided in any one of the embodiments of the first aspect of the present invention.

[0068] Since the photovoltaic assembly 1 provided by the utility model includes the panel 12 provided by any embodiment of the first aspect of the utility model, it has all the beneficial effects of the panel 12 provided by any embodiment of the first aspect of the utility model, which will not be repeated here.

[0069] In some embodiments, optionally, Figure 3 As shown, the photovoltaic module 1 also includes: a backplane layer 19, which is arranged on the side of the panel 12 away from the coating 4; a battery layer 16, which is arranged between the backplane layer 19 and the panel 12; a first adhesive layer 14, which is arranged between the panel 12 and the battery layer 16; and a second adhesive layer 18, which is arranged between the backplane layer 19 and the battery layer 16.

[0070] In this embodiment, the first adhesive layer 14 can be a high-cutoff encapsulation film, preferably one of high-cutoff EVA, POE, EPE or PVB films, with a thickness of 0.5mm-0.8mm; the battery layer 16 is preferably one of XBC, MWT, and shingled batteries without metal grid lines, and the positive and negative metal electrodes are both led out from the back, followed by a battery cell with grid lines on both sides, such as PERC, TOPCON, and HJT. The second adhesive layer 18 can be a highly transparent encapsulation film, preferably one of high-cutoff EVA, POE, EPE or PVB films, with a thickness of 0.5mm-0.8mm; the backplane layer 19 is a flexible polymer material, such as one of PET or CPC or HPC materials, with a thickness of 0.4mm to 0.8mm. The backplane layer 19 of the utility model is a flexible polymer material, so it can be bent into different shapes and is suitable for different installation substrates. At the same time, the selection of the battery layer 16 can further improve the power generation efficiency.

[0071] like Figure 4 As shown, the third aspect of the present invention provides a method for preparing a panel, comprising the following steps:

[0072] S102: treating the visualization plate with a lipophilic treatment agent, wherein the visualization plate includes a coating area and a non-coating area defined by the coating area;

[0073] S104: A coating is prepared on the coating area by a screen mold to obtain a panel.

[0074] The preparation method of the panel of the utility model includes first treating the visualization plate 122 with an oleophilic treatment agent, so as to improve the bonding strength between the coating 4 and the visualization plate 122 after silk screen printing, the visualization plate 122 includes a coating area 1222 and a non-coating area 1224 defined by the coating area 1222, and then preparing the coating 4 on the coating area 1222 by a silk screen mold 2 to obtain the panel 12. The utility model adjusts the overall silk screen printing to partial silk screen printing, which not only ensures the overall aesthetics of the panel 12, but also ensures that the photovoltaic module 1 has a higher power generation power, avoids poor light transmittance, and reduces the loss of power generation efficiency.

[0075] In some embodiments, the lipophilic treatment agent optionally includes at least one of hexamethyldisiloxane, trimethylsiloxane, and dimethylchlorosilane.

[0076] In this embodiment, by selecting a lipophilic treatment agent, the bonding strength between the ink and the visualization board 122 can be further improved, thereby avoiding the problem of ink detachment.

[0077] In some embodiments, optionally, the screen mold 2 is provided with a through hole corresponding to each coating area 1222, and the number of through holes per square inch of the screen mold 2 is greater than or equal to 10 and less than or equal to 1000.

[0078] In this embodiment, limiting the number of through holes per square inch on the screen mold 2 can avoid the problem of the coating area 1222 being too concentrated or too dispersed, thereby improving the aesthetics of the panel 12 and the light transmittance.

[0079] In some embodiments, optionally, the number of through holes per square inch of the screen mold 2 is greater than or equal to 150 and less than or equal to 250.

[0080] In this embodiment, the number of through holes per square inch on the screen mold 2 is limited to between 150 and 250, which further improves the aesthetics and light transmittance.

[0081] The fourth aspect of the present invention provides a panel 12, which is prepared by the panel preparation method of any one of the third aspects of the present invention.

[0082] The fifth embodiment of the utility model provides a photovoltaic assembly 1, including: a panel 12 provided in the fourth embodiment of the utility model.

[0083] like Figure 2 and Figure 3 As shown, another embodiment of the utility model provides a preparation process of a photovoltaic module 1, which mainly addresses the defects of existing curved panel silk screen printing, and can conveniently bend the silk screen mold 2 to obtain the desired curved shape, thereby meeting the precision printing requirements for curved panel products.

[0084] The equipment involved includes:

[0085] The scraper 3 is made of a flexible material. The scraper 3 is made of polyurethane rubber with good wear resistance and resilience. Its hardness is between 60 and 80 Shore A, and its width should be smaller than the width of the screen mold 2.

[0086] Curved panel: Choose customized tempered glass with multiple peaks and valleys, with a radius of 30mm to 150mm and a thickness of 3mm to 8mm;

[0087] Screen mold 2: It can be a dot matrix screen mold 2, that is, the printing holes on the screen mold 2 are arranged in the form of a dot matrix, the curved shape is designed to match the curved panel, the length is slightly longer than the curved panel, and the width is consistent with the curved panel. The material of the dot matrix screen mold 2 can be high-strength low-shrinkage nylon, polyester or polyester fiber material, or stainless steel. The mesh number is selected between 150 and 250 meshes, the dot matrix diameter is 2 mm to 5 mm, and the dot matrix spacing is between 5 mm and 10 mm. The screen mold 2 is positioned through the mold hole 22 and the positioning hole 124 at the upper end of the curved panel;

[0088] Coating 4: Coating 4 can be ink, the ink color is a translucent pearlescent ink in the color number PANTONE 1645CP or 1625CP in the Pantone color card, the ink has selective permeability, can selectively absorb ultraviolet light and transmit visible light, and the transmittance T of the panel 12 after screen printing is greater than 85%.

[0089] During the preparation process, the curved panel is first turned over and the inner surface of the curved panel is cleaned. The treatment agent can be one of hexamethyldisiloxane, trimethylsiloxane, and dimethylchlorosilane to enhance the lipophilicity of the inner surface of the curved panel and improve the bonding strength between the ink and the panel 12 after screen printing. After the screen mold 2 is fixed to the curved panel, it is placed in a screen printing machine and the ink is injected into the screen mold 2. The screen printing speed is 20m / min to 30m / min. The ink on the screen mold 2 is evenly scraped with the scraper 3, and the ink thickness is 20μm to 30μm.

[0090] The curved panel after silk screen printing is sintered at a high temperature of 140°C to 150°C and a drying time of 45min to 60min, so that the ink is quickly solidified and formed, and stably combined with the surface of the panel 12 to obtain a printed curved panel, which is used as the panel 12 of the photovoltaic module 1.

[0091] After curing, the ink layer appears in circular stripes, and the overall shape follows the curved shape of the curved panel. It appears as star-shaped dots when viewed from close up, with bright colors and a translucent effect. From a distance, the overall color appears to be a consistent bright golden red or brick red.

[0092] After the panel 12 is prepared, the photovoltaic module 1 is prepared by using the printed panel 12. The structure of the photovoltaic module 1 includes:

[0093] A curved panel prepared by the above method;

[0094] The first adhesive layer 14 may be a high-cutoff encapsulation adhesive film, for example, one of high-cutoff EVA, POE, EPE or PVB adhesive films, with a thickness of 0.5 mm to 0.8 mm;

[0095] The battery layer 16 may be a battery without metal grid lines in XBC, MWT, or shingled cells, where both positive and negative metal electrodes are led out from the back, or a battery cell with grid lines on both the front and back sides, such as PERC, TOPCON, or HJT.

[0096] The second adhesive layer 18 may be a highly transparent encapsulation adhesive film, such as a high-cutoff EVA, POE, EPE or PVB adhesive film, with a thickness of 0.5 mm to 0.8 mm;

[0097] The backplane layer 19 may be a flexible polymer backplane material, such as PET, CPC or HPC material, with a thickness of 0.4 mm to 0.8 mm.

[0098] The photovoltaic module 1 prepared by the method of the utility model can selectively screen print the entire inner surface of the curved panel by adjusting the dot diameter size, dot spacing and mesh number of the screen mold 2, thereby improving the overall aesthetics of the curved photovoltaic module 1, ensuring that the curved photovoltaic module 1 has a higher power generation capacity, and reducing the loss of power generation efficiency. Semi-transparent pearlescent ink is selected. Since the ink has selective permeability, it absorbs ultraviolet light and selectively transmits visible light, ensuring that the power generation efficiency loss of the curved screen-printed photovoltaic module 1 is less than 10%, while highlighting the translucent visual effect of the product and the consistency of the overall bright appearance. This solution designs a customized dot matrix screen mold 2, which fits tightly with the curved panel through the mold hole 22, and can continuously complete precision printing on the curved panel, with the advantages of high printing efficiency and strong practicality.

[0099] In the embodiments according to the present invention, the terms "first", "second", and "third" are only used for descriptive purposes and are not to be understood as indicating or implying relative importance; the term "plurality" refers to two or more, unless otherwise clearly defined. The terms "installed", "connected", "connected", "fixed", etc. should be understood in a broad sense. For example, "connected" can be a fixed connection, a detachable connection, or an integral connection; "connected" can be a direct connection or an indirect connection through an intermediate medium. For those of ordinary skill in the art, the specific meanings of the above terms in the embodiments according to the present invention can be understood according to specific circumstances.

[0100] In addition, although each operation is described in a specific order, this should be understood as requiring such operation to be performed in a specific order or in a sequential order, or requiring that all illustrated operations should be performed to obtain desired results. Under certain circumstances, multitasking and parallel processing may be advantageous. Similarly, although some specific implementation details are included in the above discussion, these should not be interpreted as limiting the scope of the present utility model. Some features described in the context of a separate embodiment can also be implemented in a single implementation in combination. On the contrary, the various features described in the context of a single implementation can also be implemented in multiple implementations individually or in any suitable sub-combination.

[0101] Although the subject matter has been described in the language of specific structural features and / or method logical actions, it should be understood that the subject matter defined in the appended claims is not necessarily limited to the specific features or actions described above. On the contrary, the specific features and actions described above are merely example forms of implementing the claims.

[0102] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. For those skilled in the art, various modifications and changes can be made to the present invention. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A panel, characterized in that: For a photovoltaic module, the panel comprises: a visualization plate, the visualization plate comprising a coating area and a non-coating area defined by the coating area; A coating is disposed on the coating area, the number of the coating areas is at least two, and the at least two coating areas are distributed in an array; At least two positioning holes are arranged at intervals on the visualization plate, and the positioning holes extend along the thickness direction of the visualization plate.

2. The panel according to claim 1, characterized in that The interval between two adjacent coating areas is 5 mm to 10 mm, and / or the width and length of each coating area are 2 mm to 5 mm.

3. The panel according to claim 1, characterized in that The number of the coating areas per square inch of the visualization board is greater than or equal to 10 and less than or equal to 1000.

4. The panel according to claim 3, characterized in that The number of the coating areas per square inch of the visualization board is greater than or equal to 150 and less than or equal to 250.

5. The panel according to claim 1, characterized in that The maximum distance between any two points on the coating area is a first distance, the minimum distance between any two adjacent coating areas is a second distance, and the ratio of the first distance to the second distance is greater than or equal to 0.5 and less than or equal to 1.

5.

6. The panel according to any one of claims 1 to 5, characterized in that The coating is transparent pearlescent ink.

7. The panel according to claim 6, characterized in that The transparent pearlescent ink can absorb light with a wavelength greater than or equal to 100 nm and less than 300 nm, and the transparent pearlescent ink can transmit light with a wavelength greater than or equal to 300 nm and less than or equal to 1100 nm.

8. The panel according to any one of claims 1 to 5, characterized in that The light transmittance of the panel is greater than or equal to 85%.

9. The panel according to any one of claims 1 to 5, characterized in that The thickness of the coating is greater than or equal to 20 μm and less than or equal to 30 μm.

10. The panel according to any one of claims 1 to 5, characterized in that The visualization board comprises a curved surface structure, the radius of the curved surface structure is greater than or equal to 30 mm and less than or equal to 150 mm, and / or The thickness of the visualization board is greater than or equal to 3 mm and less than or equal to 8 mm.

11. A photovoltaic module, characterized in that: include: A panel as claimed in any one of claims 1 to 10.

12. The photovoltaic module according to claim 11, characterized in that: Also includes: A backing layer, arranged on a side of the panel away from the coating; A battery layer, the battery layer is arranged between the back plate layer and the panel; A first adhesive layer, disposed between the panel and the battery layer; The second adhesive layer is arranged between the back plate layer and the battery layer.