Packaging adhesive film and photovoltaic module thereof

By using an encapsulating adhesive film structure of non-cross-linked EVA and POE materials in photovoltaic modules, combined with an adhesive layer and an ion barrier layer, the defects of traditional adhesive films in water vapor barrier and battery stability are solved, achieving better water vapor barrier and battery stability while reducing cost.

CN221854494UActive Publication Date: 2024-10-18WUXI UTMOST LIGHT TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420456309.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-08
Publication Date
2024-10-18
Estimated Expiration
2034-03-08

AI Technical Summary

Technical Problem

The adhesive film structure of existing photovoltaic modules cannot meet the requirements of water vapor barrier performance, battery stability and cost at the same time. In particular, the traditional EPE adhesive film causes cross-linked EVA to be hydrolyzed to produce acetic acid after water vapor enters, affecting potential-induced attenuation and battery stability. , and the cost is higher.

Method used

An encapsulating adhesive film is used, including an adhesive layer, an intermediate layer and an ion barrier layer, which is prepared by melt co-extrusion. The intermediate layer is non-crosslinked EVA, the ion barrier layer is non-crosslinked POE, and the adhesive layer is POE. Or PVB, the thickness ratio is 1:1.25:1, ensuring water vapor barrier performance and battery stability while reducing costs.

Benefits of technology

It effectively improves the water vapor barrier performance, prevents polar substances from entering the battery, improves battery stability, and reduces costs by optimizing material and structural design, achieving a water vapor transmission rate of less than 5g/㎡·day and improving battery stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221854494U_ABST
    Figure CN221854494U_ABST
Patent Text Reader

Abstract

The utility model discloses a packaging adhesive film and a photovoltaic assembly thereof, and the packaging adhesive film comprises a bonding layer. The middle layer is used for blocking water vapor permeation; the ion barrier layer is used for blocking the polar material generated by the intermediate layer; the ion barrier layer is made of POE (Polyolefin Elastomer); the ion barrier layer, the middle layer and the bonding layer are sequentially stacked. The packaging adhesive film provided by the utility model has the advantages of good water vapor barrier property, high battery stability and low cost.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of packaging of photovoltaic modules, in particular to a packaging adhesive film and a photovoltaic module thereof. Background Art

[0002] The global photovoltaic market is growing steadily, and the market demand for adhesive films is also growing. At present, photovoltaic modules are generally encapsulated with EVA, POE or EPE films. In current battery encapsulation applications, most of them are encapsulated with EVA films or POE films. Among them, when using EVA films, water vapor enters the interior of the module and causes the cross-linked EVA to hydrolyze to produce acetic acid. The reaction of acetic acid with sodium salts in the glass can cause sodium ion migration, resulting in potential induced decay. In addition, acidic substances are not friendly to thin-film batteries themselves, which in turn affects battery stability. When pure POE film is used for encapsulation, although the encapsulation effect is better, the cost of the film is too high.

[0003] Among them, EPE film is a multilayer film made of POE resin and EVA resin through co-extrusion process. The traditional EPE film is a laminated structure formed by melt co-extrusion of cross-linked POE and cross-linked EVA, usually composed of two layers of EVA on the outside and a layer of POE in the middle; in terms of materials, POE resin accounts for 60% and EVA resin accounts for about 40%. EPE film is a compromise product in terms of performance and cost, which takes into account the good performance of POE film and the cost advantage of EVA film to a certain extent.

[0004] However, when water vapor enters the component, the laminated structure will cause the cross-linked EVA to hydrolyze and produce acetic acid. The reaction of acetic acid with sodium salt in the glass can cause sodium ions to migrate into the thin-film battery, resulting in potential induced decay. In addition, acidic substances are not friendly to the thin-film battery itself, which in turn affects the battery stability. At the same time, the water vapor barrier of traditional EPE co-extruded film is 20-40g / ㎡·day. For some thin-film batteries, such as perovskite batteries, its water vapor barrier performance does not meet the requirements at all. Utility Model Content

[0005] Therefore, the technical problem to be solved by the present invention is to overcome the defect that the film structure disclosed in the prior art cannot take into account water vapor barrier performance, battery stability and cost at the same time, thereby providing a packaging film and a photovoltaic module thereof that solve the above problems.

[0006] A packaging film, comprising:

[0007] Adhesive layer;

[0008] The middle layer is used to block water vapor penetration;

[0009] An ion blocking layer, used to block polar substances generated by the intermediate layer;

[0010] The material of the ion barrier layer is POE; the ion barrier layer, the intermediate layer and the bonding layer are stacked in sequence.

[0011] The packaging adhesive film in the utility model is prepared by melt co-extrusion.

[0012] The material of the middle layer is EVA.

[0013] The material of the bonding layer is POE or PVB. Preferably, the material of the bonding layer is non-cross-linked POE.

[0014] The material of the ion barrier layer is preferably non-cross-linked POE.

[0015] The material of the middle layer is non-cross-linked EVA.

[0016] The thickness of the adhesive layer is 150um-1.2mm; preferably, when the material of the adhesive layer is POE, the thickness of the adhesive layer is 150-250um; when the material of the adhesive layer is PVB, the thickness of the adhesive layer is 0.7-1.2mm;

[0017] And / or, the thickness of the intermediate layer is 200-400um;

[0018] And / or, the thickness of the ion blocking layer is 150-250 um.

[0019] The thickness ratio of the ion blocking layer, the intermediate layer and the bonding layer is 1:(1-2):(1-5).

[0020] The thickness ratio of the ion blocking layer, the intermediate layer and the bonding layer is 1:1.25:1.

[0021] The edges of the bonding layer and the ion blocking layer are bonded to each other so that the intermediate layer is wrapped between the bonding layer and the ion blocking layer.

[0022] A photovoltaic module comprises a thin film battery substrate, the above-mentioned packaging film and a battery back plate which are stacked in sequence, wherein the ion barrier layer is arranged corresponding to the thin film battery substrate, and the bonding layer is arranged corresponding to the battery back plate.

[0023] The non-crosslinked POE mentioned above refers to POE without a crosslinking agent, and the non-crosslinked EVA refers to EVA without a crosslinking agent.

[0024] The technical solution of the utility model has the following advantages:

[0025] 1. The utility model provides a packaging film, which adopts the method of stacking an ion barrier layer, an intermediate layer and an adhesive layer in sequence, which can effectively overcome the defects of the film structure disclosed in the prior art that it cannot take into account the water vapor barrier performance, battery stability and cost at the same time. The specific implementation mechanism is as follows: First, an intermediate layer is used to block water vapor penetration, which effectively achieves the purpose of water vapor barrier, and then its water vapor barrier performance fully meets the performance requirements of perovskite batteries; then an adhesive layer is set on the side of the intermediate layer close to the battery backplane, which effectively realizes the fixation of the packaging film of the utility model on the battery backplane; at the same time, since water vapor will hydrolyze to produce polar substances such as acetic acid when it contacts the intermediate layer, thereby affecting the battery stability, an ion barrier layer is set on the side of the intermediate layer close to the thin-film battery substrate to effectively block the polar substances generated by the intermediate layer from entering the thin-film battery substrate, effectively improving the battery stability; at the same time, since the POE content accounts for less than the amount of pure POE film, the cost can be effectively reduced. Therefore, the packaging film in the utility model has the advantages of good water vapor barrier performance, high battery stability and low cost.

[0026] 2. The packaging film provided by the utility model, the adhesive layer is preferably non-cross-linked POE, and the non-cross-linked POE has the effects of low water permeability and high adhesion. The water vapor barrier of the packaging film optimized by the above material is less than 5g / ㎡·day, and it will not release polar substances to damage the battery cells in a hot and humid environment. The effect is better than the existing EVA, POE or EPE films disclosed.

[0027] 3. The encapsulation film provided by the utility model is preferably a structure in which the edges of the bonding layer and the ion barrier layer are bonded to each other to wrap the middle layer between the bonding layer and the ion barrier layer, that is, the ion barrier layer and the adhesive layer completely wrap the middle layer, which helps to protect the middle layer in all directions. The above structure effectively prevents the middle layer from overflowing from the outer edge to the battery core during lamination and melting, and can also reduce the stratification phenomenon of the encapsulation film and the PID phenomenon of the component. The ion barrier layer contacts the thin film chip, plays a role in blocking water, blocking the polar substances released by the middle layer, and improving the photoelectric conversion efficiency of the photovoltaic component; the main purpose of the middle layer is to reduce costs, and when the middle layer is preferably non-cross-linked EVA, its water vapor permeability is low, so that the overall film has a cost advantage and improves the water barrier performance. The adhesive layer contacts the battery backplane or glass, on the one hand, the thin film battery substrate is tightly connected to the battery backplane, and the photovoltaic component is effectively formed; on the other hand, the closed space formed by the adhesive layer and the ion barrier layer can also protect the middle layer, so that it is not easy to yellow, and avoid affecting the overall transmittance. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] In order to more clearly illustrate the specific implementation methods of the utility model or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0029] Figure 1 This is a schematic diagram of the structure of a photovoltaic module in Example 1 of the utility model;

[0030] Figure 2 This is a schematic diagram of the structure of the packaging film in Example 2 of the utility model;

[0031] Figure 3 This is a schematic diagram of the structure of the photovoltaic module in Example 2 of the present utility model.

[0032] Description of reference numerals:

[0033] 1-adhesive layer, 2-intermediate layer, 3-ion barrier layer, 4-thin film battery substrate, 5-battery backplane. DETAILED DESCRIPTION

[0034] The technical solution of the utility model will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0035] In the description of the present invention, it should be noted that the directions or positional relationships indicated by terms such as "upper", "lower", "left", "right", "inside" and "outside" are based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation on the present invention.

[0036] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection; it can be directly connected or indirectly connected through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0037] In addition, the technical features involved in the different embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.

[0038] Example 1

[0039] A packaging film includes an ion barrier layer 3, an intermediate layer 2 and an adhesive layer 1 which are sequentially stacked by melt coextrusion. Among them, the adhesive layer 1 can be any material that can be bonded and fixed to the battery backplane or glass, preferably POE or PVB. For thin film chips that are sensitive to crosslinking agents, non-crosslinked POE is the most preferred. The crosslinking agent contains peroxide, which has an impact on the thin film chip; the crosslinked film is mainly added with a crosslinking agent and an auxiliary crosslinking agent, and the inside of the film presents a three-dimensional network structure, which can obtain higher strength, hardness and heat resistance, but it will become more brittle over time. When the component is deformed, the film and the thin film chip are in hard contact, so it has an impact on the film layer of the thin film chip; the non-crosslinked film has a linear structure, has higher flexibility and plasticity, and has no release of polar substances. The intermediate layer 2 refers to a layered structure formed by a material that can be used to block water vapor penetration, such as EVA or PVB material. Since the intermediate layer is also required to achieve the effect of reducing costs, a non-POE material is used, such as EVA, preferably non-crosslinked EVA.

[0040] The non-cross-linked EVA can be a commercially available material or homemade. When homemade non-cross-linked EVA is selected, the content of acetate in the EVA can be greatly reduced by optimizing the formula, and the vinyl acetate content of the ethylene-vinyl acetate copolymer used is 5-15%. The water barrier performance can also be improved by modification, so that the water vapor barrier of the modified EVA is less than 4g / ㎡·day. At the same time, the residual acetate ions can be neutralized by additives to decompose as little polar substance as possible during the aging process of the film. Or the lamination temperature of the film can be lowered to make its process window consistent with that of the thin-film chip and low-temperature POE, so as to facilitate the molding of the encapsulation film by melt co-extrusion and facilitate the subsequent packaging of thin-film batteries.

[0041] The ion barrier layer 3 is used to block polar substances generated by the decomposition of the intermediate layer 2. The material of the ion barrier layer 3 is POE, preferably non-cross-linked POE.

[0042] In this embodiment, the encapsulation film comprises an ion barrier layer 3 composed of non-crosslinked POE, an intermediate layer 2 composed of non-crosslinked EVA, and an adhesive layer 1 composed of non-crosslinked POE, which are sequentially stacked by melt co-extrusion. Figure 1 shown.

[0043] In the above-mentioned encapsulation film, the thickness of the adhesive layer 1 is 150um-1.2mm; the thickness of the intermediate layer 2 is 200-400um; and the thickness of the ion barrier layer 3 is 150-250um. Since the material of the adhesive layer 1 is non-cross-linked POE, the thickness of the adhesive layer 1 in this embodiment is 150-250um. As a preferred setting, the thickness ratio of the ion barrier layer 3, the intermediate layer 2 and the adhesive layer 1 is 1:(1-2):(1-5); more preferably, the thickness ratio of the ion barrier layer 3, the intermediate layer 2 and the adhesive layer 1 is 1:1.25:1; specifically, in this embodiment, the thickness of the ion barrier layer 3, the intermediate layer 2 and the adhesive layer 1 are 200um, 250um, and 200um, respectively. By matching the thickness and material, the water vapor barrier of the co-extruded film can be reduced to less than 5g / ㎡·day, effectively meeting the water vapor barrier performance requirements of the perovskite battery.

[0044] This embodiment also provides a photovoltaic module, comprising a thin film battery substrate 4, the above-mentioned encapsulation film, and a battery back plate 5 stacked in sequence; wherein the ion barrier layer 3 is disposed adjacent to the thin film battery substrate 4, and the adhesive layer 1 is disposed adjacent to the battery back plate 5, such as Figure 1 shown.

[0045] Example 2

[0046] This embodiment also provides another photovoltaic module, such as Figure 2 and Figure 3 As shown, the ion blocking layer 3, the intermediate layer 2 and the bonding layer 1 are not merely stacked in sequence, but the edges of the bonding layer 1 and the ion blocking layer 3 are bonded to each other to wrap the intermediate layer 2 between the bonding layer 1 and the ion blocking layer 3. Figure 2 As shown. The middle layer is completely wrapped by the ion barrier layer and the adhesive layer, which helps to protect the middle layer in all directions. When the above structure is laminated and melted, it can effectively prevent the middle layer from overflowing from the outer edge to the battery cell. At the same time, it can also reduce the stratification phenomenon of the encapsulation film and the PID phenomenon of the component. The ion barrier layer is in contact with the thin film chip, which plays a role in blocking water, blocking the polar substances released by the middle layer, and improving the stability of the photoelectric conversion of the photovoltaic component; the main purpose of the middle layer is to reduce costs, and when the middle layer is preferably non-cross-linked EVA, its water vapor permeability is low, so that the overall film has a cost advantage and improves the water barrier performance. The adhesive layer is in contact with the battery backplane glass. On the one hand, it tightly connects the thin-film battery substrate and the battery backplane to effectively form a photovoltaic component; on the other hand, the closed space formed by the adhesive layer and the ion barrier layer can also protect the middle layer, making it less likely to yellow and avoid affecting the overall transmittance.

[0047] The structure of the photovoltaic module in this embodiment is as follows Figure 3 shown.

[0048] Example 3

[0049] The difference between this embodiment and embodiment 1 is that the structure of the encapsulation film is an ion barrier layer 3 composed of non-cross-linked POE, an intermediate layer 2 composed of non-cross-linked EVA and an adhesive layer 1 composed of PVB / PET; wherein the thickness of the adhesive layer 1 composed of PVB / PET is 0.7-1.2 mm, preferably 0.76-1.14 mm, and is selected as 1 mm in this embodiment, and the rest is the same as in embodiment 1.

[0050] In this embodiment, PVB / PET is used to contact the battery back plate, which has higher safety performance, and the encapsulation film in this embodiment can be used in construction and has a wider range of applications.

[0051] Example 4

[0052] The difference between this embodiment and embodiment 1 is that the structure of the encapsulation film is an ion barrier layer 3 composed of non-cross-linked POE, an intermediate layer 2 composed of non-cross-linked EVA and an adhesive layer 1 composed of cross-linked POE; in this embodiment, the non-cross-linked side is in contact with the thin-film battery substrate, and the cross-linked side is in contact with the battery backplane, which is suitable for thin-film chips that are insensitive to cross-linking agents. The other structures of this embodiment are the same as those of embodiment 1.

[0053] Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the invention.

Claims

1. A packaging film, characterized in that: include: Adhesive layer (1); An intermediate layer (2) for preventing water vapor penetration; An ion blocking layer (3) for blocking polar substances generated by decomposition of the intermediate layer (2); The material of the ion blocking layer (3) is POE; the ion blocking layer (3), the intermediate layer (2) and the bonding layer (1) are stacked in sequence.

2. The packaging film according to claim 1, characterized in that: The material of the middle layer (2) is EVA.

3. The packaging film according to claim 1, characterized in that: The material of the adhesive layer (1) includes POE or PVB.

4. The packaging film according to any one of claims 1 to 3, characterized in that: The material of the ion barrier layer (3) is non-cross-linked POE.

5. The packaging film according to any one of claims 1 to 3, characterized in that: The material of the middle layer (2) is non-cross-linked EVA.

6. The packaging film according to any one of claims 1 to 3, characterized in that: The thickness of the adhesive layer (1) is 150um-1.2mm; And / or, the thickness of the intermediate layer (2) is 200-400 um; And / or, the thickness of the ion blocking layer (3) is 150-250 um.

7. The packaging film according to any one of claims 1 to 3, characterized in that: The thickness ratio of the ion blocking layer (3), the intermediate layer (2) and the bonding layer (1) is 1:(1-2):(1-5).

8. The packaging film according to claim 7, characterized in that: The thickness ratio of the ion blocking layer (3), the intermediate layer (2) and the bonding layer (1) is 1:1.25:

1.

9. The packaging film according to any one of claims 1 to 3, characterized in that: The edges of the bonding layer (1) and the ion blocking layer (3) are bonded to each other so that the intermediate layer (2) is wrapped between the bonding layer (1) and the ion blocking layer (3).

10. A photovoltaic module, characterized in that: Comprising a thin film battery substrate stacked in sequence (4) The packaging film and battery backplane (5) as described in any one of claims 1 to 9, wherein the ion barrier layer (3) is arranged corresponding to the thin-film battery substrate, and the adhesive layer (1) is arranged corresponding to the battery backplane.