Screw-in type continuous anode aluminum electrolysis structure based on short process
By using screw-in anodes in aluminum electrolytic production, the problems of heat loss and low current efficiency during anode replacement are solved, achieving more efficient electrolytic aluminum production and simplicity of anode replacement, reducing energy consumption and assembly costs.
Patent Information
- Application Number
- CN202323428739.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-15
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2033-12-15
AI Technical Summary
In existing aluminum electrolysis production, the anode replacement process has problems such as heat loss, low current efficiency, increased iron and phosphorus content, complex assembly, and high energy consumption, which affects the operating efficiency and product quality of the electrolytic cell.
The screw-in anode is used to replace the traditional assembled anode, and the screw-in anode is fixed by an electric brake to realize the continuous replenishment and replacement of the anode, simplify the replacement process, reduce heat loss and interference, and reduce energy consumption.
It improves the flue gas collection rate and current efficiency of the electrolyzer, reduces assembly workers and capital consumption, reduces energy consumption and replacement cycles, and makes it easy and economical to replace the anode.
Smart Images

Figure CN221854791U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to a screw-in continuous anode aluminum electrolysis structure based on a short process, belonging to the technical field of aluminum electrolysis. Background Art
[0002] Prebaked anodes are mostly used in modern electrolytic aluminum production. The anode assembly is mainly composed of an anode guide rod group and an anode carbon block. The anode guide rod group is welded in sequence by an anode guide rod, an explosive welding block, an anode transition steel beam, and an anode steel claw. Four circular grooves (i.e., carbon bowls) are provided on the top surface of the anode carbon block. The head end of the anode steel claw is cast by phosphorus pig iron to form a phosphorus iron ring embedded in the carbon bowl of the anode carbon block, thereby realizing the connection between the anode guide rod group and the anode carbon block.
[0003] After the anode assembly is used, the anode carbon block is consumed and the residual anode needs to be removed from the electrolytic cell and replaced with a newly assembled anode assembly. The residual anode will be transported to the anode assembly workshop and replaced with a new anode carbon block and anode guide rod group to cast a new anode assembly. There are several problems in the above link:
[0004] (1) The exhausted anode residues need to be removed from the electrolytic cell, and the cell cover needs to be opened to replace the anode. After a period of use, the anode residues are bonded to the covering material. Therefore, the anode replacement process requires the use of an electric pick on the electrolytic overhead crane to separate the anode residues from the covering material. This process will cause heat loss in the electrolytic cell and affect the fume collection rate of the electrolytic cell, resulting in an increase in the unorganized emission of harmful gases from the electrolytic cell.
[0005] (2) The newly replaced anode assembly is in a cold state and cannot directly participate in the reaction production process of electrolytic aluminum. It requires additional energy from the electrolytic cell to heat it. During this period, it has a great impact on the current efficiency of the entire electrolytic cell.
[0006] (3) The existing assembled anode is connected by anode carbon block and anode guide rod group through phosphorus iron casting. The steel claw head of the anode guide rod group will be corroded and dissolved in the electrolytic cell. When the repair quality of some anode steel claw heads is poor, the steel claw heads may fall into the electrolytic cell. The above situation increases the iron and phosphorus content in the aluminum liquid, thereby reducing the current efficiency and product quality.
[0007] (4) After the anode residue is replaced, it needs to be transported to the anode assembly workshop, where new anode carbon blocks and anode guide rod groups are cast into new anode components. The assembly process includes pressing off the anode residue, pressing off the phosphorus iron ring, cleaning, straightening the guide rod or steel claw, phosphorus iron casting, anode carbon block spraying and other links. In addition, in case of loss and damage of the steel claw, explosion welding block damage, etc., the anode guide rod group needs to be taken off the assembly line for welding repair, and then put back on the line for assembly after the repair is completed. This link consumes energy equivalent to 60-100kWh per ton of aluminum. At the same time, the entire assembly process has many processes and complex situations, consuming hundreds of people and tens of millions of yuan in funds. Utility Model Content
[0008] The purpose of the utility model is to provide a screw-in continuous anode aluminum electrolysis structure based on a short process. The structure adopts a screw-in anode to replace the original assembled anode, realizes the continuous production of aluminum electrolysis anodes, saves the anode assembly link, and simplifies the anode replacement link.
[0009] The technical solution of the utility model: a screw-in continuous anode aluminum electrolysis structure based on a short process, including an electrolytic cell, a plurality of screw-in anodes vertically arranged above the electrolytic cell, the bottom of the screw-in anode extends into the electrolyte solution of the electrolytic cell, the screw-in anode is a cylindrical carbon anode, one end of the screw-in anode is an external thread, and the other end is an internal thread, the screw-in anode is formed by connecting the threads of screw-in anode one and screw-in anode two, and the screw-in anode is fixed by an electric brake, and the other end of the electric brake is fixed to the anode busbar.
[0010] In the aforementioned screw-in continuous anode aluminum electrolysis structure based on a short process, the screw-in anode 1 and the screw-in anode 2 are of the same structure, with an external thread at the lower end and an internal thread at the upper end.
[0011] In the aforementioned short-process-based screw-in continuous anode aluminum electrolysis structure, electric brakes are provided on both sides of the anode busbar, and multiple electric brakes are provided at intervals on the same side of the anode busbar.
[0012] In the aforementioned short-process screw-in continuous anode aluminum electrolysis structure, a covering material and a tank cover are arranged above the electrolytic cell, and the covering material and the tank cover are provided with notches adapted to the size of the screw-in anode.
[0013] Beneficial effects of the utility model: Compared with the prior art, the utility model has the following advantages:
[0014] (1) After the screw-in anode is consumed, a new screw-in anode can be screwed in at the rear end to complete the anode replenishment, and the slot cover plate does not need to be opened for pole change operation. This will reduce the heat loss caused by pole change by 40mv. Taking a 500kA electrolyzer as an example, it can save 128kWh / t-Al. In addition, the flue gas collection rate of the electrolyzer will be improved, which is expected to increase from 98% to more than 99%.
[0015] (2) Due to the use of screw-in anodes, the entire electrolytic aluminum production process becomes more continuous, reducing the interference of the pole-changing process, so that the current efficiency can be increased by more than 1% and the energy consumption can be reduced by more than 120 kWh / t-Al.
[0016] (3) Compared with the currently used assembled anodes, the screw-in anode is a pure carbon block anode, which greatly reduces the content of elements such as iron and phosphorus in the electrolytic aluminum production process.
[0017] (4) The screw-in anode replaces the currently used assembled anode. The anode no longer needs to be connected to the anode guide rod assembly. The anode assembly process is eliminated, which will save about 120 assembly workers and about 50 million yuan in funds. It can also avoid the increase in pressure drop caused by assembly and save more than 70kWh / t-Al in energy.
[0018] (5) Due to the use of screw-in anodes, all anode groups on the cell can be replaced at one time, which greatly reduces the load rate of the overhead crane. Taking 500kA as an example, traditionally, one pole-changing cycle requires 24 pole-changing operations. After using screw-in anodes, it only takes one time to complete, and the pole-changing load rate of the overhead crane can be reduced by more than 90%.
[0019] In summary, the use of screw-in anodes makes the process of replacing anodes simple, anode preparation is more economical, and electrolytic production is more continuous and efficient. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 It is a structural schematic diagram of this utility model;
[0021] Figure 2 It is a longitudinal schematic diagram of this utility model;
[0022] Figure 3 This is the first process of the screw-in continuous anode production of the utility model;
[0023] Figure 4 This is the second process of the screw-in continuous anode production of the utility model;
[0024] Figure 5 This is the front view of the traditionally assembled anode;
[0025] Figure 6 This is a top view of a traditionally assembled anode.
[0026] Figure numerals: 1-screw-in anode 1, 2-electric brake, 3-screw-in anode 2, 4-anode busbar, 5-slot cover, 6-covering material, 7-electrolyte solution, 8-liquid aluminum, 9-cathode carbon block, 10-anode guide rod, 11-explosive welding block, 12-anode transition steel beam, 13-anode steel claw, 14-anode carbon block, 15-ferrophosphorus ring. DETAILED DESCRIPTION
[0027] The present invention is further described below in conjunction with the accompanying drawings and embodiments, but they are not intended to limit the present invention.
[0028] See also Figure 5 , Figure 6The conventional assembled anode is shown, which includes an anode guide rod 10, an explosive welding block 11, an anode transition steel beam 12, an anode steel claw 13, an anode carbon block 14, and a phosphorus iron ring 15. During use, the conventional assembled anode needs to be replaced, a new anode carbon block 14 needs to be assembled, and the damaged anode steel claw 13, explosive welding block 11, etc. need to be welded and repaired. Various problems may occur during the assembly and repair process. In order to avoid these problems, the structure of the utility model is proposed.
[0029] Embodiment of the utility model: a screw-in continuous anode aluminum electrolysis structure based on a short process, such as Figure 1-4 As shown, an electrolytic cell is included, the bottom of the electrolytic cell is a cathode carbon block 9, above the cathode carbon block 9 is aluminum liquid 8, above the aluminum liquid 8 is an electrolyte solution 7, a plurality of screw-in anodes are vertically arranged above the electrolytic cell, the bottom of the screw-in anode extends into the electrolyte solution 7 of the electrolytic cell, the screw-in anode is a cylindrical carbon anode, one end of the screw-in anode is an external thread, and the other end is an internal thread, the screw-in anode is formed by threading a screw-in anode 1 and a screw-in anode 2 3, the screw-in anode is fixed by an electric brake 2, and the other end of the electric brake 2 is fixed to the anode bus 4.
[0030] The screw-in anode 1 and the screw-in anode 2 3 have the same structure, with the lower end being an external thread and the upper end being an internal thread, so as to facilitate the threaded connection between the screw-in anode 1 and the screw-in anode 2 3 .
[0031] The electric brakes 2 are arranged on both sides of the anode bus bar 4 , and a plurality of electric brakes 2 are arranged at intervals on the same side of the anode bus bar 4 . A plurality of screw-in anodes can be lifted and fixed by one anode bus bar 4 .
[0032] A covering material 6 and a tank cover plate 5 are arranged above the electrolytic cell, and slots adapted to the size of the screw-in anodes are provided on the covering material 6 and the tank cover plate 5. A certain gap is left between the slots and the screw-in anode 1 and the screw-in anode 2 3. When the screw-in anode 1 and the screw-in anode 2 3 are consumed during electrolytic production, the anode bus bar 4 can be moved up and down to realize continuous replenishment of the anodes.
[0033] The screw-in anode 1 and the screw-in anode 2 3 of the utility model are both cylindrical carbon anodes, and one end of the screw-in anode 1 and the screw-in anode 2 3 is an external thread and the other end is an internal thread. Figure 3 As shown, when in use, the screw-in anode 1 is used to replace the existing assembled anode, with the external thread end of the screw-in anode 1 facing downward and the internal thread end facing upward. The screw-in anode 1 is directly inserted into the electrolyte solution 7 of the electrolytic cell for reaction. An electric brake 2 is installed on the anode bus 4 of the electrolytic cell, and the electric brake 2 holds the screw-in anode 1 tightly. After a part of the screw-in anode 1 is consumed in the reaction in the electrolytic cell, Figure 4 As shown, the anode busbar 4 is moved downward, driving the screw-in anode 1 to move downward to continue the reaction.
[0034] See also Figure 4 As shown, after most of the screw-in anode 1 is consumed by the reaction, a new screw-in anode 23 will be added above the screw-in anode 1, and the external thread of the screw-in anode 23 will be screwed into the internal thread at the tail of the screw-in anode 1, the electric brake 2 will loosen the screw-in anode 1, the anode busbar 4 will be lifted upward, and the electric brake 2 will clamp and fix the screw-in anode 23 to achieve the replenishment of the anode.
[0035] When the anode busbar 4 moves downward and reaches the lower position, the screw-in anode 2 3 is hoisted to the top of the screw-in anode 1 by the overhead crane, and then the external thread of the screw-in anode 2 3 is screwed into the internal thread at the tail of the screw-in anode 1 to replenish the anode. After replenishment, the screw-in anode is clamped and fixed briefly by the aluminum electrolysis overall lifting frame, and the electric brake 2 is opened at the same time. After the anode busbar 4 is lifted to a high position, the electric brake 2 is locked to clamp and fix the screw-in anode 2 3. The aluminum electrolysis overall lifting frame releases the screw-in anode and continues electrolysis production. During the process of extending the screw-in anode thread and moving the electric brake 2, the screw-in anode is lifted and fixed by the overhead crane to prevent the screw-in anode from falling into the electrolytic cell.
Claims
1. A short-process rotary continuous anode aluminum electrolysis structure, comprising an electrolytic cell, Features: A plurality of screw-in anodes are vertically arranged above the electrolytic cell, the bottom of the screw-in anode extends into the electrolyte solution (7) of the electrolytic cell, the screw-in anode is a cylindrical carbon anode, one end of the screw-in anode is an external thread, and the other end is an internal thread, the screw-in anode is formed by threading a screw-in anode 1 (1) and a screw-in anode 2 (3), and the screw-in anode is fixed by an electric brake (2), and the other end of the electric brake (2) is fixed on the anode busbar (4).
2. A short-process rotary continuous anode aluminum electrolysis structure according to claim 1, Features: The screw-in anode 1 (1) and the screw-in anode 2 (3) have the same structure, with the lower end being an external thread and the upper end being an internal thread.
3. A short-process rotary continuous anode aluminum electrolysis structure according to claim 1, Features: Electric brakes (2) are arranged on both the left and right sides of the anode busbar (4), and a plurality of electric brakes (2) are arranged at intervals on the same side of the anode busbar (4).
4. A short-process rotary continuous anode aluminum electrolysis structure according to claim 1, Features: A covering material (6) and a tank cover plate (5) are arranged above the electrolytic tank, and the covering material (6) and the tank cover plate (5) are provided with notches adapted to the size of the screw-in anode.