MOS (Metal Oxide Semiconductor) tube packaging structure with G-pole electrostatic shielding function
By introducing the design of magnetic attraction and anti-static materials into the MOS tube packaging structure, the problem of G being extremely susceptible to electrostatic interference is solved, and the stability and heat dissipation effect of the chip are improved through the improved heat dissipation structure.
Patent Information
- Application Number
- CN202420439493.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-07
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2034-03-07
AI Technical Summary
The G of the MOS tube is extremely susceptible to external electrostatic interference, causing damage. It is difficult for the existing packaging structure to provide effective electrostatic shielding.
A packaging structure including a package block, a chip body, a G-pole pin and an iron block is designed. The magnetic attraction and rubber material plug-in structure are used. The magnetic attraction between the iron block and the magnetic attraction block and the triangular limiting block are used. When plugged in, anti-static stainless steel is used to protect the G-pole pin, and the heat dissipation effect is improved through aluminum alloy heat sink plates and heat conduction rods.
It effectively prevents the G-pole pin from being interfered with by static electricity, improves the electrostatic shielding effect, and makes the main body of the chip run more stably through the improved heat dissipation structure.
Smart Images

Figure CN221861647U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of MOS tube packaging, in particular to a MOS tube packaging structure with a G-pole electrostatic shielding function. Background Art
[0002] MOS tube is a field effect tube, whose function is to modulate and decode the signal to be transmitted, and then directly couple the signal to the output end through a semiconductor field effect transistor. It is usually used as a switch in the circuit. The chip on the MOS tube is usually installed inside the package block with the pins exposed. The existing MOS tube packaging structure still has certain defects when used.
[0003] In the prior art, a MOS tube usually has three pins, namely a gate, a drain, and a source. The gate is also called a G-pole, which is a control pin of the MOS tube. Since the input resistance of the MOS tube itself is very high and the capacitance between the gate and the source is very small, the G-pole in the MOS tube is easily interfered by external static electricity during storage and transportation, causing damage to the MOS tube. Utility Model Content
[0004] The utility model aims to provide a MOS tube packaging structure with a G-pole electrostatic shielding function, so as to solve the problem that the G-pole of the MOS tube currently on the market is easily affected by electrostatic interference as mentioned in the above background technology.
[0005] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a MOS tube packaging structure with a G-pole electrostatic shielding function, comprising: a packaging block, a chip body, a G-pole pin and an iron block, the chip body is installed inside the packaging block, the G-pole pin is installed on the outside of the chip body, the iron block is installed on both sides of the packaging block, a first box body is arranged on the outside of the packaging block, a magnetic block is installed on the inner wall of the first box body close to the iron block, a connecting block is installed on the outside of the first box body, a second box body is arranged at the end of the first box body, plug-in blocks are installed on both sides of the second box body, and a triangular limit block is installed on the outside of the plug-in block.
[0006] Preferably, a plug-in structure is formed between the plug-in block and the connecting block, and the plug-in block is made of rubber material.
[0007] Preferably, a magnetic attraction structure is formed between the iron block and the magnetic attraction block.
[0008] Preferably, a through hole is opened inside the packaging block, a fixing block is installed on the surface of the packaging block, and a high-temperature resistant rubber block is installed on the inner wall of the fixing block.
[0009] Preferably, an aluminum alloy heat sink is provided at the end of the fixing block, and an aluminum alloy heat conducting rod is connected to a side of the aluminum alloy heat sink close to the through hole.
[0010] Preferably, a plug-in rod is connected to a side of the aluminum alloy heat sink close to the fixing block.
[0011] Compared with the prior art, the beneficial effects of the utility model are as follows: the MOS tube packaging structure with G-pole electrostatic shielding function can drive the G-pole pin and the iron block to move when the packaging block moves, and when the end of the packaging block moves to the inside of the first box body, the iron block can be magnetically attracted to the magnetic block, and when the end of the second box body is docked with the end of the first box body, the plug-in block can drive the triangular limit block to be plugged into the inside of the connecting block, and the high-temperature resistant rubber block can be reset by its own elasticity, so that the aluminum alloy heat sink can be installed on the outside of the packaging block, and the heat dissipation speed and heat dissipation effect of the chip body can be improved through the aluminum alloy heat sink and the aluminum alloy heat conducting rod, so that the operation of the chip body can be more stable.
[0012] 1. MOS tubes are usually used in inverters, switching power supplies and other equipment. Since it is difficult to protect the G-pole pin due to the MOS tube packaging structure, the G-pole pin is easily interfered by static electricity. When the packaging block moves, the G-pole pin and the iron block can be driven to move. When the end of the packaging block moves to the inside of the first box body, the iron block can be magnetically attracted to the magnetic block. When the end of the second box body is docked with the end of the first box body, the plug-in block can drive the triangular limit block to be plugged into the inside of the connecting block. When the second box body is completely docked with the first box body, the plug-in block can be reset in shape so that the triangular limit block can be stuck on the outside of the connecting block, so that the second box body is not easy to detach from the end of the first box body. The materials of the second box body and the first box body are both anti-static stainless steel. The G-pole pin on the packaging block can be protected by the second box body and the first box body, so that the G-pole pin is not easily interfered by external static electricity, thereby improving the electrostatic shielding effect of the G-pole pin.
[0013] 2. The traditional MOS tube packaging structure completely wraps the chip body, resulting in poor heat dissipation effect of the chip body. When the aluminum alloy heat sink moves, it can drive the aluminum alloy heat-conducting rod and the plug-in rod to move. When the aluminum alloy heat-conducting rod is inserted into the package block through the through hole, the plug-in rod can be plugged into the fixed block. The plug-in rod can squeeze the high-temperature resistant rubber block. When the plug-in rod is completely plugged into the fixed block, the high-temperature resistant rubber block can be reset by its own elasticity, so that the aluminum alloy heat sink can be installed on the outside of the package block. The aluminum alloy heat sink and the aluminum alloy heat-conducting rod can improve the heat dissipation speed and heat dissipation effect of the chip body, so that the operation of the chip body can be more stable. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 It is a schematic diagram of the cutaway structure of the main view of the utility model;
[0015] Figure 2It is a right view structural schematic diagram of the utility model;
[0016] Figure 3 It is a schematic diagram of the right side cutaway structure of the packaging block of the utility model.
[0017] In the figure: 1. packaging block; 2. chip body; 3. G-pole pin; 4. iron block; 5. first box body; 6. magnetic block; 7. connection block; 8. second box body; 9. plug-in block; 10. triangular limit block; 11. through hole; 12. fixing block; 13. high temperature resistant rubber block; 14. aluminum alloy heat sink; 15. aluminum alloy heat conducting rod; 16. plug-in rod. DETAILED DESCRIPTION
[0018] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0019] See also Figure 1 and Figure 2 It can be seen that the utility model provides a technical solution: a MOS tube packaging structure with a G-pole electrostatic shielding function, comprising: a packaging block 1, a chip body 2, a G-pole pin 3 and an iron block 4;
[0020] A chip body 2 is installed inside the package block 1, and a G-pole pin 3 is installed outside the chip body 2;
[0021] The iron block 4 is installed on both sides of the packaging block 1, and a first box body 5 is arranged on the outside of the packaging block 1. A magnetic block 6 is installed on the inner wall of the first box body 5 close to the iron block 4, and a connecting block 7 is installed on the outside of the first box body 5. A second box body 8 is arranged at the end of the first box body 5, and plug-in blocks 9 are installed on both sides of the second box body 8. A triangular limiting block 10 is installed on the outside of the plug-in block 9, and a plug-in structure is formed between the plug-in block 9 and the connecting block 7, and the plug-in block 9 is made of rubber material, and a magnetic attraction structure is formed between the iron block 4 and the magnetic block 6.
[0022] In specific implementation, MOS tubes are usually used in inverters, switching power supplies and other equipment. Since it is difficult for the MOS tube packaging structure to protect the G-pole pin 3, the G-pole pin 3 is easily interfered by electrostatics. For this reason, the packaging block 1 can be pushed. When the packaging block 1 moves, the G-pole pin 3 and the iron block 4 can be driven to move. When the end of the packaging block 1 moves into the first box body 5, the iron block 4 can be magnetically attracted to the magnetic block 6. At this time, the second box body 8 can be pushed. When the second box body 8 moves, the plug-in block 9 can be driven to move. When the end of the second box body 8 is docked with the end of the first box body 5, the plug-in block 9 can drive the triangular limit block 10 to be plugged into the inside of the connecting block 7. At this time, the plug-in block 9 can be deformed. When the second box body 8 is completely docked with the first box body 5, the plug-in block 9 can be reset in shape, so that the triangular limit block 10 can be stuck on the outside of the connecting block 7, so that the second box body 8 is not easy to detach from the end of the first box body 5. The materials of the second box body 8 and the first box body 5 are both anti-static stainless steel.
[0023] See also Figure 1 and Figure 2 It can be seen that the second box body 8 and the first box body 5 can protect the G-pole pin 3 on the package block 1, so that the G-pole pin 3 is not easily disturbed by external static electricity, thereby improving the electrostatic shielding effect of the G-pole pin 3.
[0024] See also Figure 1 and Figure 3 It can be seen that a through hole 11 is opened inside the packaging block 1, a fixing block 12 is installed on the surface of the packaging block 1, a high temperature resistant rubber block 13 is installed on the inner wall of the fixing block 12, an aluminum alloy heat sink 14 is arranged at the end of the fixing block 12, an aluminum alloy heat sink 14 is connected to the side of the aluminum alloy heat sink 14 close to the through hole 11, a plug-in rod 16 is connected to the side of the aluminum alloy heat sink 14 close to the fixing block 12, and the aluminum alloy heat sink 14 is evenly spaced.
[0025] In specific implementation, the traditional MOS tube packaging structure completely wraps the chip body 2, resulting in poor heat dissipation effect of the chip body 2. For this reason, the aluminum alloy heat sink 14 can be pushed. When the aluminum alloy heat sink 14 moves, it can drive the aluminum alloy heat conducting rod 15 and the plug-in rod 16 to move. When the aluminum alloy heat conducting rod 15 is inserted into the packaging block 1 through the through hole 11, the plug-in rod 16 can be plugged into the fixed block 12. When the plug-in rod 16 is plugged into the fixed block 12, the plug-in rod 16 can squeeze the high-temperature resistant rubber block 13. When the plug-in rod 16 is completely plugged into the fixed block 12, the high-temperature resistant rubber block 13 can be reset by its own elasticity, so that the aluminum alloy heat sink 14 can be installed on the outside of the packaging block 1.
[0026] See also Figure 1 and Figure 3It can be seen that the aluminum alloy heat sink 14 and the aluminum alloy heat conducting rod 15 can improve the heat dissipation speed and heat dissipation effect of the chip body 2, so that the chip body 2 can operate more stably.
[0027] In summary, when the MOS tube packaging structure with the G-pole electrostatic shielding function is used, the MOS tube works by utilizing the metal oxide semiconductor field effect. The MOS tube packaging structure is used to install the chip body 2 and the G-pole pin 3. The MOS tube controls the current on and off by controlling the voltage of the G-pole pin 3. The MOS tube packaging structure is a prior art and will not be described in detail herein. The second box body 8 and the first box body 5 are both made of antistatic stainless steel. The G-pole pin 3 on the packaging block 1 can be protected by the second box body 8 and the first box body 5, so that the G-pole pin 3 is not easily interfered by external static electricity, thereby improving the electrostatic shielding effect of the G-pole pin 3. The high-temperature resistant rubber block 13 can be reset by its own elasticity, so that the aluminum alloy heat sink 14 can be installed on the outside of the packaging block 1. The aluminum alloy heat sink 14 and the aluminum alloy heat conducting rod 15 can improve the heat dissipation speed and heat dissipation effect of the chip body 2, so that the chip body 2 can run more stably. The contents not described in detail in this description belong to the prior art known to professional and technical personnel in this field.
[0028] Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art may still modify the technical solutions described in the aforementioned embodiments, or make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention shall be included in the protection scope of the present invention.
Claims
1. A MOS tube packaging structure with G-pole electrostatic shielding function, include: The packaging block (1), the chip body (2), the G-pole pin (3) and the iron block (4) are characterized by: A chip body (2) is installed inside the packaging block (1), and a G-pole pin (3) is installed outside the chip body (2); An iron block (4) is mounted on both sides of the packaging block (1); a first box body (5) is arranged on the outer side of the packaging block (1); a magnetic attraction block (6) is installed on the inner wall of the first box body (5) close to the iron block (4); a connecting block (7) is installed on the outer side of the first box body (5); a second box body (8) is arranged at the end of the first box body (5); plug-in blocks (9) are installed on both sides of the second box body (8); and a triangular limit block (10) is installed on the outer side of the plug-in block (9).
2. A MOS tube packaging structure with G-pole electrostatic shielding function according to claim 1, Features: The plug-in block (9) and the connecting block (7) form a plug-in structure, and the plug-in block (9) is made of rubber material.
3. The MOS tube packaging structure with G-pole electrostatic shielding function according to claim 1, Features: A magnetic attraction structure is formed between the iron block (4) and the magnetic attraction block (6).
4. The MOS tube packaging structure with G-pole electrostatic shielding function according to claim 1, Features: A through hole (11) is provided inside the packaging block (1), a fixing block (12) is mounted on the surface of the packaging block (1), and a high temperature resistant rubber block (13) is mounted on the inner wall of the fixing block (12).
5. The MOS tube packaging structure with G-pole electrostatic shielding function according to claim 4, Features: An aluminum alloy heat dissipation plate (14) is provided at the end of the fixing block (12), and an aluminum alloy heat conduction rod (15) is connected to a side of the aluminum alloy heat dissipation plate (14) close to the through hole (11).
6. A MOS tube packaging structure with G-pole electrostatic shielding function according to claim 5, Features: The aluminum alloy heat sink (14) is connected to a plug-in rod (16) on one side close to the fixing block (12).