FPC (Flexible Printed Circuit) pressing die

By using a layer-by-layer laminated kraft paper and PE film structure in the FPC lamination mold, the problem of glue overflow in FPC products is solved, ensuring no glue overflow during the lamination process, and improving the aesthetics and usability of the product.

CN221863179UActive Publication Date: 2024-10-18CHUNHUA TECHNOLOGICAL KUSN
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323580546.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-27
Publication Date
2024-10-18
Estimated Expiration
2033-12-27

AI Technical Summary

Technical Problem

During the gluing process of FPC products, due to the small opening gap, the glue overflows and cannot be cleaned, which affects the appearance of the product and the customer's production. It is impossible to use conventional lamination pressure transmission and lamination.

Method used

An FPC pressing mold is designed, which adopts an upper mold and a lower mold structure. The upper mold includes a first kraft paper, a first PE film and a resist film that are layered layer by layer. The lower mold includes a second kraft paper that is set layer by layer. And the second PE film, through the combination of glue-resistant film and multi-layer kraft paper, prevents glue from overflowing.

Benefits of technology

It effectively prevents glue from overflowing, ensures that no glue overflow occurs during the lamination process, and improves the aesthetics and usability of the product.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221863179U_ABST
    Figure CN221863179U_ABST
Patent Text Reader

Abstract

The utility model discloses an FPC (Flexible Printed Circuit) pressing die, which comprises an upper die and a lower die, the upper die comprises an upper stacking plate group, the lower die comprises a lower stacking plate group and a matte film attached to the upper end surface of the lower stacking plate group, and the upper die comprises first kraft paper, a first PE (Poly Ethylene) film and a glue blocking film which are attached to the upper stacking plate group layer by layer from top to bottom. And through the arrangement of the glue blocking film, glue can be effectively prevented from overflowing from the uncovering opening, and through cooperation with buffering of the first kraft paper and blocking of the PE film, it is further ensured that glue overflowing cannot be generated in the pressing process.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to an FPC pressing die. Background Art

[0002] The client currently requires that the opening size of the cover on the FPC product should reach 0.9*0.9mm. When the FPC board is glued, some glue overflows into the opening. Due to the small opening gap, the glue in the opening cannot be cleaned after gluing. As a result, the presence of overflowed glue can be clearly observed in the opening after the product is formed, affecting the appearance of the product and the client's punching. Therefore, conventional stacking pressure transmission and pressing cannot be used. Summary of the invention

[0003] The utility model aims to provide an FPC pressing die which can prevent glue overflow from the FPC board during pressing.

[0004] To achieve the above-mentioned purpose, the technical solution adopted by the utility model is: an FPC pressing mold, which includes an upper mold and a lower mold, the upper mold includes an upper stacked plate group, the lower mold includes a lower stacked plate group and a matte film adhered to the upper end surface of the lower stacked plate group, and the upper mold includes a first kraft paper, a first PE film, and an adhesive-resistant film adhered to the upper stacked plate group layer by layer from top to bottom.

[0005] In another embodiment, a second kraft paper and a second PE film are provided layer by layer from bottom to top between the lower stacked plate group and the matte film.

[0006] In another embodiment, the first kraft paper has multiple layers.

[0007] In another embodiment, the second kraft paper has multiple layers.

[0008] In another embodiment, the upper stacking plate group includes a carrier plate, a buffer pad, and a steel plate from top to bottom.

[0009] In another embodiment, the lower stacked plate group includes a carrier plate, a buffer pad, and a steel plate from bottom to top.

[0010] In another embodiment, the first kraft paper specification is 160±5g / m 2 The thickness of the first PE film is 120±5um, and the thickness of the adhesive barrier film is 160um±5um.

[0011] In another embodiment, the second kraft paper specification is 160±5g / m 2 , the thickness of the second PE film is 120±5um.

[0012] Due to the application of the above technical solution, the utility model has the following advantages compared with the prior art: by setting the glue-blocking film, it can effectively prevent glue from overflowing from the cover opening, and with the buffering of the first kraft paper and the blocking of the PE film, it is further ensured that no glue overflow occurs during lamination. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Attached Figure 1 It is a structural schematic diagram of the utility model. DETAILED DESCRIPTION

[0014] The utility model is further described below in conjunction with the embodiments shown in the accompanying drawings.

[0015] like Figure 1 As shown, the FPC pressing mold includes an upper mold and a lower mold.

[0016] The upper mold includes an upper stacking plate group, the lower mold includes a lower stacking plate group and a matte film 7 attached to the upper end surface of the lower stacking plate group, and the upper mold includes a first kraft paper 4, a first PE film 5, and a glue-blocking film 6 attached to the upper stacking plate group layer by layer from top to bottom. The first kraft paper has multiple layers. The upper stacking plate group includes a carrier plate 1, a buffer pad 2, and a steel plate 3 from top to bottom.

[0017] The lower stacking plate group and the matte film are provided with second kraft paper 9 and second PE film 8 layer by layer from bottom to top. The second kraft paper has multiple layers. The lower stacking plate group includes a carrier plate 1, a buffer pad 2, and a steel plate 3 from bottom to top.

[0018] In this embodiment, the first kraft paper 4 has two layers and is stacked adjacent to each other, and the second kraft paper 9 has two layers and is stacked adjacent to each other.

[0019] By setting the adhesive blocking film, cooperating with the buffering of the first kraft paper and the second kraft paper and the blocking of the first PE film and the second PE film, it is ensured that no adhesive overflow occurs when the FPC board 0 is pressed.

[0020] The above embodiments are only for illustrating the technical concept and features of the utility model, and their purpose is to enable people familiar with the technology to understand the content of the utility model and implement it accordingly, and they cannot be used to limit the protection scope of the utility model. Any equivalent changes or modifications made according to the spirit of the utility model should be included in the protection scope of the utility model.

Claims

1. An FPC pressing mold, comprising an upper mold and a lower mold, wherein the upper mold comprises an upper stacked plate group, and the lower mold comprises a lower stacked plate group and a matte film attached to the upper end surface of the lower stacked plate group. Features: The upper mold includes a first kraft paper, a first PE film, and a glue-blocking film which are laminated on the upper stacked plate group layer by layer from top to bottom.

2. The FPC pressing mold according to claim 1, Features: A second kraft paper and a second PE film are arranged layer by layer from bottom to top between the lower stacking plate group and the matte film.

3. The FPC pressing mold according to claim 1, Features: The first kraft paper has multiple layers.

4. The FPC pressing mold according to claim 2, Features: The second kraft paper has multiple layers.

5. The FPC pressing mold according to claim 1, Features: The upper stacking plate group includes a carrier plate, a buffer pad, and a steel plate in order from top to bottom.

6. The FPC pressing mold according to claim 1, Features: The lower stacking plate group includes a carrier plate, a buffer pad, and a steel plate in order from bottom to top.

7. The FPC pressing mold according to claim 1, Features: The first kraft paper specification is 160±5g / m 2 The thickness of the first PE film is 120±5um, and the thickness of the adhesive barrier film is 160um±5um.